Novel ether-amide ashless additive and preparation method thereof

By developing sulfur-free and phosphorus-free ether-amide ashless additives, we have solved the problems of poor compatibility between lubricating oil additives and synthetic base oils and environmental pollution, and achieved the effects of reducing friction coefficient and resisting sulfur corrosion in low-viscosity oils. Significantly improved lubrication performance and environmental friendliness.

CN118772007APending Publication Date: 2024-10-15SHANGHAI INST OF ORGANIC CHEM CHINESE ACAD OF SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310382294.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing lubricating oil additives have poor compatibility with synthetic base oils and are not effective in reducing the friction coefficient in low-viscosity oils. At the same time, they have adverse effects on the environment. In particular, metal friction modifiers can poison the catalysts of automobile exhaust purification devices and increase oil quality. Sediment content during thermal oxidation.

Method used

Develop a sulfur-free, phosphorus-free ether-amide ashless additive. Polyethylene glycol reacts with sulfonylation reagents and diamine alcohol to form ether-amine compounds, and reacts with acid chloride to form ether-amide compounds. Friction modifier and anti-sulfur corrosion agent for use in synthetic base oils.

Benefits of technology

The ether-amide compound significantly reduces the friction coefficient of low-viscosity oils, improves lubrication performance, and effectively prevents corrosion of copper sheets by active sulfur without containing metal, providing a wider scope of application and higher durability. Simplicity of synthetic route.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004172755750000021
    Figure BDA0004172755750000021
  • Figure BDA0004172755750000023
    Figure BDA0004172755750000023
  • Figure BDA0004172755750000031
    Figure BDA0004172755750000031
Patent Text Reader

Abstract

The invention provides a novel ether-amide ash-free friction modifier and a preparation method thereof. Specifically, the invention provides a metal-free, sulfur-free and phosphorus-free environment-friendly base oil friction improvement additive, which takes cheap and easily available diamine alcohol or diol amine as a raw material and reacts with acyl chloride with different structures to generate a corresponding amide-ester compound. The reaction synthesis route is simple, the yield is considerable, and the tribological properties can be effectively regulated and controlled by adjusting the number, length and branched structure of amide chains and ester chains.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of lubricating oil additives, and in particular relates to a novel ether-amide ashless friction modifier and a preparation method thereof. Background Art

[0002] With increasingly stringent environmental regulations and people's demand for increasing energy efficiency of mechanical equipment, low-viscosity oil products have become the main development trend. Among them, the low viscosity of oil products requires the combination of more effective lubricant additives to effectively improve the durability of the oil film protection of low-viscosity oil products. Generally, lubricant additives form a strong adsorption film on the surface of the friction pair through van der Waals force or chemical bonds, increasing the adsorption and wedging ability of the lubricant, which not only reduces the risk of dry friction, but also reduces kinetic energy consumption, achieving the purpose of energy saving.

[0003] At present, lubricating oil additives that improve the durability of oil film protection of low-viscosity oil products are mainly divided into metal friction modifiers (zinc dialkyl dithiophosphate ZDDP and organic molybdenum, etc.) and organic friction modifiers. The former will not only poison the catalyst of automobile exhaust purification devices due to the sulfur, phosphorus and metal elements in the compounds, but also increase the sediment content during the thermal oxidation process of oil products. In order to protect the engine and emission control system from harmful substances such as sulfate ash, phosphorus and sulfur (SAPS) generated during the use of oil products, it is urgent to develop new sulfur-free and phosphorus-free ash-free additives.

[0004] In terms of performance, synthetic base oils have better heat and oxidation resistance, better viscosity and low temperature performance, and a wider operating temperature range than traditional mineral base oils, making them the preferred choice for developing high-performance lubricants.

[0005] In view of the improvement of mechanical precision and the upgrading of lubricant technology, accompanied by the steady growth of high-end market demand, the study of the application of lubricant additives in synthetic base oils is of great significance to the development of high-performance lubricants. Summary of the invention

[0006] In order to overcome the deficiencies of the prior art, the present invention provides a novel ether-amide ashless additive and a preparation method thereof, aiming to solve the problems that the existing lubricating oil additives have poor compatibility with synthetic base oils, poor effect in reducing friction coefficient in low-viscosity base oils, and adverse effects on the environment.

[0007] In a first aspect of the present invention, an ether-amide ashless additive is provided, wherein the ashless additive comprises one or more components selected from the following formulas (I)-(V):

[0008]

[0009] Wherein, n is an integer from 1 to 8; R is -C mH 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

[0010] In another preferred embodiment, n is an integer of 2 to 5; R is -C m H 2m+1 , m is an integer from 1 to 9; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 6; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 5 to 17.

[0011] In another preferred embodiment, the ashless additive is selected from

[0012]

[0013] In the second aspect of the present invention, an ashless additive-base oil complex is provided, the complex comprising the ashless additive as described in the first aspect of the present invention; preferably, in the complex, the friction modifier is added in an amount of 0.1 to 10.0 wt% of the base oil weight; preferably 0.1 to 5.0 wt%.

[0014] In another preferred embodiment, the base oil is selected from the following group: synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.

[0015] In a third aspect of the present invention, there is provided a method for preparing the ashless additive according to the first aspect of the present invention, comprising the following steps:

[0016]

[0017] Polyethylene glycol (monoether) reacts with a sulfonylating agent, and then reacts with a diamine alcohol to generate an ether-amine compound, and the ether-amine compound reacts with R2-COCl acyl chloride to obtain an ether-amide compound;

[0018] Wherein, n is an integer from 1 to 8; R is -C m H 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -Cj H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

[0019] In another preferred embodiment, the sulfonylating agent is selected from TsCl or MsCl.

[0020] In another preferred embodiment, the molecular weight Mw of the polyethylene glycol (monoether) is 100 to 10000 g / mol; preferably 100 to 1000 g / mol.

[0021] In another preferred embodiment, the polyethylene glycol (monoether) is polyethylene glycol, polyethylene glycol monoalkyl ether, polyethylene glycol monoaryl ether, or a combination thereof.

[0022] In another preferred embodiment, the diamino alcohol is 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-diamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, or a combination thereof; preferably 1,3-di(methylamino)-2-propanol.

[0023] In another preferred embodiment, the R2-COCl acyl chloride is selected from the group consisting of butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, dodecanoyl chloride, tetradecanoyl chloride, hexadecanoyl chloride, octadecanoyl chloride, oleic acid chloride, or a combination thereof; preferably hexanoyl chloride and oleic acid chloride.

[0024] In a fourth aspect of the present invention, there is provided a use of the ashless additive as described in the first aspect of the present invention, which is used as a friction modifier in a base oil to reduce the friction coefficient of the base oil.

[0025] In a fifth aspect of the present invention, there is provided a use of the ashless additive according to the first aspect of the present invention, which is used as an anti-sulfur corrosion agent in a base oil.

[0026] It should be understood that within the scope of the present invention, the above-mentioned technical features of the present invention and the technical features specifically described below (such as embodiments) can be combined with each other to form a new or preferred technical solution. Due to space limitations, they will not be described one by one here. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 The friction curves of the sample oils containing the ether-amide compounds in Examples 1 and 2 of the present invention and the base oil are compared.

[0028] Figure 2 The friction reduction and anti-wear performance of the sample oils containing the ether-amide compounds in Examples 1 and 2 of the present invention are compared with the base oil.

[0029] Figure 3 The ether-amide compounds prepared in Examples 1 and 2 of the present invention inhibit the corrosion of active sulfur on copper sheets. DETAILED DESCRIPTION

[0030] After extensive and in-depth research and a large number of experiments, the inventors have developed for the first time an ashless, sulfur-free and phosphorus-free ether-amide ashless additive. The ashless additive is obtained by grafting polyether chains and amide chains using cheap and readily available diamine alcohol as a raw material. The tribological properties of the ether-amide compound can be effectively regulated by adjusting the grafted polyether structure and the amide chain structure. The synthetic route of the additive is simple and has a high yield. On this basis, the inventors have completed the present invention.

[0031] the term

[0032] As used herein, the term "base oil" refers to lubricating oil used for mechanical equipment and industrial equipment, including mineral-based lubricating oils and synthetic-based lubricating oils.

[0033] As used herein, the term "friction modifier" refers to a type of lubricant additive that enhances boundary lubrication, increases the adsorption and wedging capabilities of lubricating oil, prevents dry friction, reduces the coefficient of friction, enhances oil film strength, and reduces kinetic energy consumption.

[0034] As used herein, the term "synthetic hydrocarbon base oil" is obtained by polymerization of α-olefins under the action of a catalyst and has excellent comprehensive properties.

[0035] As used herein, the term "synthetic ester base oil" is prepared by dehydration of fatty acids and fatty alcohols by esterification reaction under the action of a catalyst. Depending on the types of fatty acids and fatty alcohols in the reaction, synthetic esters can be divided into: polyol esters, diesters and monoesters, etc.

[0036] As used herein, the term "polyether base oil" is the most widely used synthetic base oil, which is made from raw materials such as ethylene oxide (EO), propylene oxide (PO), and butylene oxide (DB) through ring-opening homopolymerization or copolymerization, and can be divided into water-soluble polyethers, water-insoluble polyethers, and oil-soluble polyethers.

[0037] Ether-amide ashless additives

[0038] The invention provides an ashless additive which has good compatibility with base oil, can reduce friction coefficient and resist active sulfur corrosion, and the ashless additive does not contain metal, sulfur or phosphorus.

[0039] Specifically, the ether-amide ashless additive includes one or more structures shown in the following formulas (I) to (V):

[0040]

[0041] Wherein, n is an integer from 1 to 8; R is -C m H 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

[0042] Preferably, n is an integer of 2 to 5; R is -C m H 2m+1 , m is an integer from 1 to 9; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 6; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 5 to 17.

[0043] Preferably, the ashless additive is selected from

[0044]

[0045] In a preferred embodiment, the ashless additive is added to the base oil for use as a compound, and the amount of the ashless additive added is 0.1-10.0wt% of the base oil, preferably 0.1-5.0wt%; more preferably 0.1-1.0wt%.

[0046] In a preferred embodiment, the base oil is a synthetic base oil or a mineral base oil.

[0047] In a preferred embodiment, the base oil is selected from the group consisting of synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.

[0048] In one embodiment, the ashless additive is used in a base oil as a friction modifier.

[0049] In another embodiment, the ashless additive is used in base oil as an anti-sulfur corrosion agent.

[0050] Preparation method of ether-amide ashless additive

[0051] The present invention also provides a method for preparing an ether-amide ashless additive, which specifically comprises the following steps:

[0052] After the alcoholic hydroxyl group in polyethylene glycol (monoether) is activated by a sulfonylating agent, it first reacts with diamine alcohol to generate an ether-amine compound, and then reacts with R2-COCl acyl chloride to obtain the corresponding unilateral ether-amide compound or bilateral ether-amide compound.

[0053]

[0054] Wherein, n is an integer from 1 to 8; R is -C m H 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

[0055] Preferably, the molecular weight Mw of the polyethylene glycol (monoether) is 100-10000 g / mol; more preferably 100-1000 g / mol; specifically, the polyethylene glycol (monoether) is polyethylene glycol, polyethylene glycol monoalkyl ether, polyethylene glycol monoaryl ether, or a combination thereof.

[0056] In the present invention, a sulfonylating agent is used to activate the alcoholic hydroxyl group in the polyethylene glycol (monoether), and the sulfonylating agent is a common sulfonylating agent in the art, for example, TsCl or MsCl.

[0057] Preferably, the diamino alcohol is 1,3-diamino-2-propanol, 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, or a combination thereof; preferably 1,3-di(methylamino)-2-propanol.

[0058] Preferably, the R2-COCl acyl chloride is selected from the group consisting of butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, dodecanoyl chloride, tetradecanoyl chloride, hexadecanoyl chloride, octadecanoyl chloride, oleic acid chloride, or a combination thereof; preferably hexanoyl chloride and oleic acid chloride.

[0059] Compared with the prior art, the main advantages of the present invention are as follows:

[0060] (1) The present invention uses cheap and readily available diamine alcohol as a raw material, and obtains a novel sulfur-free and phosphorus-free ashless additive by grafting polyether chains and amide chains.

[0061] (2) The ash-free additive of the present application has a simple synthesis route and a high yield. The tribological properties of the ether-amide compound can be effectively regulated by adjusting the grafted polyether structure and the amide chain structure, and has a wider range of applications.

[0062] (3) The nitrogen atoms and oxygen atoms in the structure of the ether-amide compound of the present invention can provide electrons for the electron-deficient orbits of the metal, and can form an ordered protective film on the surface of the friction pair through a strong adsorption effect, which can significantly reduce the friction coefficient of low-viscosity oil products and effectively improve the anti-friction performance of the oil products.

[0063] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are only used to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples without specifying specific conditions are usually based on conventional conditions or the conditions recommended by the manufacturer. Unless otherwise stated, percentages and parts are calculated by weight.

[0064] Example 1: Preparation of unilateral ether-amide compounds

[0065]

[0066] First, 1-diethylene glycol-4-nonylphenol ether (1-1, 3.09 g, 10 mmol) and Et3N (1.52 g, 15 mmol) were dissolved in 50 mL DCM in a 250 mL reaction bottle, and TsCl (2.10 g, 11 mmol) was added at 0°C. After 10 min, the ice-water bath was removed, and the reaction solution was stirred at room temperature for 2 h until the reaction of compound 1-1 was complete as monitored by TLC. Water was added to quench the reaction, and DCM was extracted, washed with saturated NaHCO3 and NaCl solutions in turn, dried with anhydrous Na2SO4, and separated by column chromatography (developing solvent was PE:EA=5:1) to obtain 4.92 g of white solid, namely compound 1-2 (yield 90.7%).

[0067] Secondly, compound 1-2 (3.70 g, 8 mmol) was weighed and dissolved in 50 mL of ultra-dry THF, and NaH (0.60 g, 15 mmol) was slowly added in an ice-water bath and stirred for 2 h. Subsequently, 1,3-dimethylamino-2-propanol (0.99 g, 8.4 mmol) was added, and the mixture was refluxed at 80°C until the reaction of compound 1-2 was complete as monitored by TLC. Water was added to quench the reaction, EA was extracted, and the mixture was washed with saturated NaHCO3 and NaCl solutions in turn. After drying with anhydrous Na2SO4, column chromatography was performed (developing solvent was PE:EA:MeOH=10:5:1) to obtain 2.86 g of white solid, namely compound 1-3 (yield 87.5%).

[0068] Then, compound 1-3 (2.86 g, 7 mmol), K2CO3 (2.90 g, 21 mmol) and DMAP (0.17 g, 1.4 mmol) were placed in a reaction flask, and 80 mL of DCM was added and stirred at 50 ° C for 0.5 h. Hexanoyl chloride (2.36 g, 17.5 mmol) was dissolved in 20 mL of DCM and slowly added to the reaction flask via a constant pressure addition funnel. The mixed solution continued to reflux until TLC monitored that compound 1-3 was completely reacted. Water was added to quench the reaction, DCM was extracted, saturated NaHCO3 and NaCl solutions were washed, anhydrous Na2SO4 was dried, and column chromatography was performed (developing solvent was DCM: MeOH = 15: 1) to obtain 3.02 g of light yellow liquid, i.e., monolateral ether-amide compound 1-4 (yield 71.4%).

[0069] 1 H NMR(400MHz, CDCl3)δ=7.13(d,2H),6.86(d,2H),4.54(m,1H),4.31(t,2H),3.77(t,2H),3.52~3.55(m,4H),3.31(d, 4H),2.94(s,6H),2.64(t,2H),2.27(t,4H),2.64(t,2H),1.63~1.53(m,6H),1.29~1.26(m,20H),0.99~0.82(m,9H).

[0070] Example 2: Preparation of Bilateral Ether-Amide Compounds

[0071]

[0072] Diethylene glycol bis-p-toluenesulfonate (2-1, 4.15 g, 10 mmol) and 100 mL of ultra-dry THF were mixed, and NaH (0.60 g, 15 mmol) was slowly added in an ice-water bath and stirred for 2 h. Subsequently, 1,3-dimethylamino-2-propanol (2.48 g, 21 mmol) was added, and the mixture was refluxed at 80 ° C until the compound 2-1 was completely consumed as monitored by TLC. Water was added to quench the reaction, EA was extracted, and the mixture was washed with saturated NaHCO3 and NaCl solutions in turn. After drying with anhydrous Na2SO4, column chromatography was performed (developing solvent was PE:EA:MeOH=10:5:2) to obtain 2.58 g of white solid, namely compound 2-2 (yield 84.2%). Subsequently, compound 2-1 (2.15 g, 7 mmol), K2CO3 (2.90 g, 21 mmol) and DMAP (0.17 g, 1.4 mmol) were placed in a reaction flask, and 80 mL of DCM was added and stirred at 50 ° C for 0.5 h. Oleoyl chloride (5.27 g, 17.5 mmol) was dissolved in 50 mL of DCM and slowly added to the reaction flask via a constant pressure addition funnel. The mixed solution continued to reflux until the reaction of compound 2-2 was complete as monitored by TLC. Water was added to quench the reaction, DCM was extracted, saturated NaHCO3 and NaCl solutions were washed, anhydrous Na2SO4 was dried, and column chromatography was performed (developing solvent was DCM: MeOH = 10: 1) to obtain 5.45 g of a nearly colorless liquid, namely, bilateral ether-amide compound 2-3 (yield 57.1%).

[0073] 1 H NMR(400MHz, CDCl3)δ=5.27(td,4H),4.54(m,2H),3.64~3.52(m,8H),3.31(d,8 H), 2.94 (s, 6H), 2.27 (t, 8H), 2.24 (q, 16H), 1.32 ~ 1.22 (m, 48H), 0.81 (t, 12H).

[0074] Example 3: Friction reduction performance test

[0075] The unilateral ether-amide compound 1-4 prepared in Example 1 and the bilateral ether-amide compound 2-3 prepared in Example 2 were added to the low-viscosity synthetic hydrocarbon base oil PAO6 in an amount of 1.0 wt.% (mass percentage), and stirred and mixed at 60°C for 1 hour to obtain nearly colorless and transparent sample oils.

[0076] The friction coefficient and wear spot diameter of the blank base oil PAO6, the sample oil in Example 1 and the sample oil in Example 2 were tested by a four-ball friction and wear tester. The test conditions were: load 392N, spindle speed 1200r / min, oil temperature 75°C, test time 60min, and the test results were as follows: Figure 1 and Figure 2 .

[0077] Depend on Figure 1 It can be seen from the friction curve that the friction coefficient of PAO6 base oil fluctuates greatly during the friction process, indicating that its oil film is unstable. When 1.0wt.% of the ether-amide compound of the present invention is added, the fluctuation of the friction curve is improved. Among them, the bilateral ether-amide compound 2-3 prepared in Example 2 can greatly shorten the running-in period and reduce the friction coefficient. Figure 2 It was found from the tribological properties that adding 1.0 wt.% of the ether-amide compounds prepared in Examples 1 and 2 of the present invention can reduce the average friction coefficient by 14.5% and 28.9%, respectively, and the average wear spot diameter by 13.2% and 34.8%, respectively, indicating that the ether-amide compounds of the present application can effectively improve the lubrication performance of synthetic hydrocarbon base oils.

[0078] Example 4: Antioxidant performance test

[0079] In order to study the effect of ether-amide compounds on the antioxidant properties of oil products, referring to ASTM E2009-08 (2014) "Standard Method for Determination of Initial Oxidation Temperature of Hydrocarbons by Differential Scanning Calorimetry", a high pressure differential scanning calorimeter (PDSC) was used to test the initial oxidation temperatures of base oil PAO6, and the sample oils in Example 1 and Example 2. The results are shown in Table 1.

[0080] Table 1

[0081] Base oil PAO6 Sample oil in Example 1 Example 2 Sample oil Initial oxidation temperature(℃) 198.9 210.0 200.3

[0082] It can be seen from the data in the table that the initial oxidation temperature of the sample oil in Example 1 is significantly higher than that of the base oil PAO6, while the initial oxidation temperature of the sample oil in Example 2 is slightly higher, indicating that ether-amide compounds 1-4 and 2-3 have certain antioxidant properties, and the antioxidant property of compound 1-4 is better than that of compound 2-3.

[0083] In addition, the active sulfur element in conventional extreme pressure anti-wear agents often corrodes metals when used. Therefore, the unilateral etheramide compounds 1-4 prepared in Example 1 and the bilateral etheramide compounds 2-3 prepared in Example 2 were added at an amount of 1.0wt.% to a blank oil composed of 0.1wt.% extreme pressure anti-wear agent GS-440L (sulfur content ~40%) and 99.9wt.% polyethylene oil LPE4, and the corrosion inhibition performance of the etheramide compounds was tested in accordance with GB / T 5096-2017 "Petroleum Products Copper Strip Corrosion Test Method". Figure 3The results of the copper sheet corrosion test show that the blank copper sheet corrosion level is 3b. After adding 1.0wt.% of the ether-amide compound prepared in Example 1 and Example 2 of the present invention, the copper sheet corrosion level is reduced to 1a and 1b respectively, indicating that the ether-amide compound can effectively inhibit the strong corrosion of GS-440L containing active sulfur on the copper sheet.

[0084] All documents mentioned in the present invention are cited as references in this application, just as each document is cited as reference individually. In addition, it should be understood that after reading the above teachings of the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.

Claims

1. An ether-amide ashless additive, characterized in that: The ashless additive comprises one or more components selected from the following formulas (I)-(V): Wherein, n is an integer from 1 to 8; R is -C m H 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

2. The ashless additive according to claim 1, characterized in that n is an integer of 2 to 5; R is -C m H 2m+1 , m is an integer from 1 to 9; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 6; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 5 to 17.

3. The ashless additive according to claim 1, characterized in that The ash-free additive is selected from 4. An ashless additive-base oil composite, characterized in that: The composite comprises the ashless additive as claimed in claim 1; preferably, in the composite, the friction modifier is added in an amount of 0.1 to 10.0 wt % of the base oil; preferably 0.1 to 5.0 wt %.

5. The composite according to claim 4, characterized in that The base oil is selected from the group consisting of synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.

6. A method for preparing the ashless additive according to claim 1, characterized in that: The steps include: Polyethylene glycol (monoether) reacts with a sulfonylating agent, and then reacts with a diamine alcohol to generate an ether-amine compound, and the ether-amine compound reacts with R2-COCl acyl chloride to obtain an ether-amide compound; Wherein, n is an integer from 1 to 8; R is -C m H 2m+1 or m is an integer of 1 to 15; R1 is selected from H or -C i H 2i+1 , i is an integer from 1 to 8; R2 is selected from -C j H 2j+1 or -C j H 2j-1 , j is an integer from 3 to 20.

7. The method according to claim 6, characterized in that The molecular weight Mw of the polyethylene glycol (monoether) is 100-10000 g / mol, preferably 100-1000 g / mol.

8. The method according to claim 6, characterized in that The polyethylene glycol (monoether) is polyethylene glycol, polyethylene glycol monoalkyl ether, polyethylene glycol monoaryl ether, or a combination thereof.

9. The method according to claim 6, characterized in that The diamino alcohol is 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-diamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, or a combination thereof; preferably 1,3-di(methylamino)-2-propanol.

10. The method according to claim 6, characterized in that The R2-COCl acyl chloride is selected from the following group: butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, dodecanoyl chloride, tetradecanoyl chloride, hexadecanoyl chloride, octadecanoyl chloride, oleic acid chloride, or a combination thereof; preferably hexanoyl chloride or oleic acid chloride.