Novel amide-ester ash-free friction modifier and preparation method thereof
By developing amide-ester ashless friction modifiers, we have solved the problems of poor compatibility between existing friction modifiers and synthetic base oils and poor performance in low-viscosity oils, achieving environmentally friendly and efficient friction reduction and anti-wear performance improvement.
Patent Information
- Application Number
- CN202310371048.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-15
AI Technical Summary
Existing friction modifiers have poor compatibility with synthetic base oils and are not effective in reducing the friction coefficient in low-viscosity base oils, while causing adverse effects on the environment.
Develop an ashless amide-ester ashless friction modifier. The amide-ester compound is prepared by reacting diamine alcohol or glycol amine with acid chloride in the presence of a catalyst and an acid binding agent to form a metal-free, sulfur- and phosphorus-free compound. An environmentally friendly friction modifier that can be well compatible with synthetic base oils and regulate its tribological properties.
It achieves good compatibility with synthetic base oil, significantly reduces friction coefficient and wear, improves the friction reduction and anti-wear performance of lubricating oil, and is environmentally friendly and harmless.
Smart Images

Figure CN118772009A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of lubricating oil additives, and in particular relates to a novel amide-ester ashless friction modifier and a preparation method thereof. Background Art
[0002] Additives are an effective way to improve the performance of lubricants. In recent years, increasingly stringent environmental regulations and people's demand for improving the energy efficiency of automobile engines have made low-viscosity engine oils a major development trend. However, low-viscosity oils require more effective friction modifiers, which are additives that reduce the friction coefficient of oils. Friction modifiers form a strong adsorption film on the surface of the friction pair through van der Waals forces or chemical bonds, thereby increasing the adsorption and wedging ability of the lubricant, preventing dry friction, and reducing friction and kinetic energy consumption, thereby achieving energy saving.
[0003] At present, the friction modifiers used in engine oil formulations are mainly metal friction modifiers (zinc dialkyl dithiophosphate ZDDP and organic molybdenum, etc.) and organic friction modifiers. The former, due to the sulfur, phosphorus and metal elements in the compound, will not only poison the catalyst of the automobile exhaust purification device, but also increase the sediment content during the thermal oxidation process of the oil. In order to protect the engine and emission control system from harmful substances such as sulfated ash, phosphorus and sulfur (SAPS) generated during the use of oil products, it is urgent to develop new sulfur-free and phosphorus-free organic friction modifiers.
[0004] In terms of performance, synthetic base oils have better heat and oxidation resistance, better viscosity and low temperature performance, and a wider operating temperature range than traditional mineral base oils, making them the preferred choice for developing high-performance lubricants.
[0005] In view of the improvement of mechanical precision and the upgrading of lubricant technology, accompanied by the steady growth of high-end market demand, the study of the application of friction modifiers in synthetic base oils is of great significance to the development of high-performance lubricants. Summary of the invention
[0006] In order to overcome the deficiencies of the prior art, the present invention provides a novel amide-ester ashless friction modifier and a preparation method thereof, aiming to solve the problems that the existing friction modifiers have poor compatibility with synthetic base oils, poor effect of reducing friction coefficient in low-viscosity base oils, and adverse effects on the environment.
[0007] In a first aspect of the present invention, an ashless friction modifier is provided, wherein the friction modifier comprises one or more components selected from the following formulas (A) to (D):
[0008]
[0009] Among them, each R 1Each independently selected from H, -C m H 2m+1 or -C m H 2m-1 , R 2 Each independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 30;
[0010] In the friction modifier, the content of the component represented by Formula A, Formula B, Formula C or Formula D is ≥50%, preferably ≥70%, more preferably ≥90%, and most preferably ≥95%.
[0011] In another preferred embodiment, the friction modifier comprises one or more components selected from the following formulas (I)-(VIII):
[0012]
[0013] Among them, each R 1 , R 2 Each independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 22;
[0014] In the friction modifier, the content of the component represented by Formula I, Formula II, Formula III, Formula IV, Formula V, Formula VI, Formula VII or Formula VIII is ≥50%, preferably ≥70%, more preferably ≥90%, and most preferably ≥95%.
[0015] In another preferred embodiment, m is an integer of 1-17.
[0016] In another preferred embodiment, the friction modifier is 1,3-bis(palmitamide)-2-propyl palmitate
[0017]
[0018] In the second aspect of the present invention, a friction modifier-base oil composite is provided, wherein the composite comprises the friction modifier as described in the first aspect of the present invention; preferably, in the composite, the friction modifier is added in an amount of 0.1-10.0 wt % of the base oil, more preferably 0.1-5.0 wt %.
[0019] In another preferred embodiment, the base oil is selected from the following group: synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.
[0020] In a third aspect of the present invention, there is provided a method for preparing the friction modifier as described in the first aspect of the present invention, comprising the following steps:
[0021]
[0022] In an inert solvent, in the presence of a catalyst and an acid binder, diamine alcohol or diol amine is reacted with R 2 -COCl acyl chloride reaction to obtain amide-ester compounds;
[0023] Each R 1 Each independently selected from H, -C m H 2m+1 or -C m H 2m-1 , R 2 Each independently selected from -C m H 2m+1 or -C m H 2m-1 , wherein m is an integer from 1 to 30.
[0024] In another preferred embodiment, the method comprises the steps of: mixing diamine alcohol or diol amine and an acid binding agent in an inert solvent, adding a mixed solution of acyl chloride and a catalyst to react to obtain an amide-ester compound.
[0025] In another preferred embodiment, the inert solvent is selected from the following group: C1-C6 alkane solvents, C2-C6 ester solvents, C2-C6 ether solvents, or a combination thereof.
[0026] In another preferred embodiment, the inert solvent is DCM.
[0027] In another preferred embodiment, the diamine alcohol or diolamine is selected from the following group: 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, 2-amino-1,3-propanediol, 2-amino-2-methyl-1,3-propanediol, 2-amino-2-ethyl-1,3-propanediol, 3-methylamino-1,2-propanediol, 3-amino-1,2-propanediol, 3-methylamino-1,2-propanediol, 3-isopropylamino-1,2-propanediol, 3-butylamino-1,2-propanediol, or a combination thereof.
[0028] In another preferred embodiment, the acid binding agent is selected from the group consisting of triethylamine, pyridine, Na 2 CO 3 、NaHCO 3 , K 2 CO 3 , NaOH, KOH, or a combination thereof.
[0029] In another preferred embodiment, the catalyst is selected from the following group: 4-dimethylaminopyridine (DMAP), 4-pyrrolidinopyridine (4-PPY), 4,5-dicyanoimidazole (DCI), N,N'-dicyclohexylcarbodiimide (DCC), 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide hydrochloride (EDCI), 1-hydroxybenzotriazole (HOBt), benzotriazole-N,N,N',N'-tetramethyluronium hexafluorophosphate (HBTU), or a combination thereof.
[0030] In another preferred embodiment, the R 2 The -COCl acyl chloride is selected from the group consisting of butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, lauroyl chloride, myristoyl chloride, palmitoyl chloride, stearoyl chloride, oleoyl chloride, or a combination thereof.
[0031] It should be understood that within the scope of the present invention, the above-mentioned technical features of the present invention and the technical features specifically described below (such as embodiments) can be combined with each other to form a new or preferred technical solution. Due to space limitations, they will not be described one by one here. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a comparison diagram of the friction curves of the sample oil to which the amide-ester compound prepared in Example 1 of the present invention is added and the blank base oil.
[0033] Figure 2 The friction reduction performance of the sample oil to which 0.5 wt.% of the amide-ester compound prepared in Example 1 of the present invention is added is compared with that of a blank base oil.
[0034] Figure 3 The anti-wear properties of the sample oil to which 0.5 wt.% of the amide-ester compound prepared in Example 1 of the present invention is added are compared with those of the blank base oil. DETAILED DESCRIPTION
[0035] After extensive and in-depth research and a large number of experiments, the inventors have developed for the first time an ashless, sulfur-free and phosphorus-free amide-ester ashless friction modifier. The ashless friction modifier uses diamine alcohol or diolamine and acyl chloride as raw materials to obtain an amide-ester compound. The tribological properties can be effectively regulated by adjusting the number, length, and branched structure of the amide chain and the ester chain. The friction modifier does not contain metal and is sulfur-free and phosphorus-free and environmentally friendly. On this basis, the inventors have completed the present invention.
[0036] the term
[0037] As used herein, the term "base oil" refers to lubricating oil used for mechanical equipment and industrial equipment, including mineral-based lubricating oils and synthetic-based lubricating oils.
[0038] As used herein, the term "friction modifier" refers to a type of lubricant additive that enhances boundary lubrication, increases the adsorption and wedging capabilities of lubricating oil, prevents dry friction, reduces the coefficient of friction, enhances oil film strength, and reduces kinetic energy consumption.
[0039] As used herein, the term "synthetic hydrocarbon base oil" is obtained by polymerization of α-olefins under the action of a catalyst and has excellent comprehensive properties.
[0040] As used herein, the term "synthetic ester base oil" is prepared by dehydration of fatty acids and fatty alcohols by esterification reaction under the action of a catalyst. Depending on the types of fatty acids and fatty alcohols in the reaction, synthetic esters can be divided into: polyol esters, diesters and monoesters, etc.
[0041] As used herein, the term "polyether base oil" is the most widely used synthetic base oil, which is made from raw materials such as ethylene oxide (EO), propylene oxide (PO), and butylene oxide (DB) through ring-opening homopolymerization or copolymerization, and can be divided into water-soluble polyethers, water-insoluble polyethers, and oil-soluble polyethers.
[0042] Amide-ester ashless friction modifier
[0043] The present invention provides an amide-ester ashless friction modifier that has good compatibility with various synthetic base oils and can reduce friction and wear. Specifically, the amide-ester ashless friction modifier includes one or more structures as shown below:
[0044]
[0045] Among them, each R 1 Each independently selected from H, -C m H 2m+1 or -C m H 2m-1 , R 2 Each independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 30;
[0046] In the friction modifier, the content of the component represented by Formula A, Formula B, Formula C or Formula D is ≥50%, preferably ≥70%, more preferably ≥90%, and most preferably ≥95%.
[0047] Preferably, the amide-ester ashless friction modifier comprises one or more structures as shown below:
[0048]
[0049] Among them, each R 1 , R2 Each independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 22.
[0050] Preferably, m is an integer of 1-17.
[0051] More preferably, the amide-ester ashless friction modifier is 1,3-bis(palmitamide)-2-palmitic acid propyl ester.
[0052] In a preferred embodiment, when used in a base oil, the friction modifier is added in an amount of 0.1-10.0 wt % of the base oil, preferably 0.1-5.0 wt %; more preferably 0.1-1.0 wt %.
[0053] In a preferred embodiment, the base oil is a synthetic base oil or a mineral base oil.
[0054] In a preferred embodiment, the base oil is selected from the group consisting of synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.
[0055] Preparation method of amide-ester ashless friction modifier
[0056] The present invention also provides a method for preparing an amide-ester ashless friction modifier, which specifically comprises the following steps:
[0057]
[0058] First, diamine alcohol or diolamine and an acid-binding agent are mixed with a solvent in a reactor; then, the acyl chloride and the catalyst are dissolved in a solvent and slowly added dropwise to the reactor; subsequently, the mixed solution is heated and stirred continuously until the reaction of the raw material diamine alcohol or diolamine is complete as monitored by TLC, water is added to quench the reaction, and the corresponding diamide monoester compound or monoamide diester compound is obtained after extraction, washing, drying and purification.
[0059] Preferably, the diamine alcohol or diolamine is any one or more mixtures of 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, 2-amino-1,3-propanediol, 2-amino-2-methyl-1,3-propanediol, 2-amino-2-ethyl-1,3-propanediol, 3-methylamino-1,2-propanediol, 3-amino-1,2-propanediol, 3-methylamino-1,2-propanediol, 3-isopropylamino-1,2-propanediol and 3-butylamino-1,2-propanediol.
[0060] Preferably, the inert solvent is selected from the following group: C1-C6 alkane solvents, C2-C6 ester solvents, C2-C6 ether solvents, or a combination thereof; more preferably, dichloromethane.
[0061] Preferably, the acid binding agent is an acid binding agent commonly used in the art, such as triethylamine, pyridine, Na 2 CO 3 、NaHCO 3 , K 2 CO 3 , NaOH or KOH.
[0062] Preferably, the catalyst is any one or more of 4-dimethylaminopyridine (DMAP), 4-pyrrolidinopyridine (4-PPY), 4,5-dicyanoimidazole (DCI), N,N'-dicyclohexylcarbodiimide (DCC), 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide hydrochloride (EDCI), 1-hydroxybenzotriazole (HOBt), and benzotriazole-N,N,N',N'-tetramethyluronium hexafluorophosphate (HBTU).
[0063] Preferably, the R 2 The -COCl acyl chloride is a common aliphatic hydrocarbon acyl chloride in the art, for example, any one of butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, lauroyl chloride, myristoyl chloride, palmitoyl chloride, stearyl chloride, and oleic acid chloride.
[0064] Compared with the prior art, the main advantages of the present invention are as follows:
[0065] (1) The present invention uses cheap and readily available diamine alcohol or diol amine as raw materials, and reacts them with aliphatic hydrocarbon acyl chlorides to obtain a type of environmentally friendly ashless friction modifier that does not contain metal, sulfur, or phosphorus.
[0066] (2) The preparation method of the ashless friction modifier of the present application has a simple synthesis route and a considerable yield, and its tribological properties can be effectively controlled by adjusting the number, length, and branching structure of the amide chains and ester chains.
[0067] (3) When the amide-ester compound of the present invention is used as an ashless friction modifier, it can synergistically act on the friction pair surface through polar amide bonds, ester bonds and non-polar chain alkanes to form a dense and orderly lubricating film to reduce friction and resist wear, and the friction reduction effect in synthetic base oil is significant.
[0068] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are only used to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples without specifying specific conditions are usually based on conventional conditions or the conditions recommended by the manufacturer. Unless otherwise stated, percentages and parts are calculated by weight.
[0069] Example 1: Preparation of ashless friction modifier 1,3-bis(palmitamide)-2-propyl palmitate
[0070]
[0071] Weigh 0.50 g 1,3-diamino-2-propanol (5.55 mmol) and 5.33 g K 2 CO 3 (11.11mmol) was placed in a three-necked flask, and 30mL of DCM was added to mix. At the same time, 6.88mL of palmitoyl chloride (22.22mmol) and 0.203g of DMAP (1.66mmol) were added to 20mL of DCM and heated to dissolve at 50°C for 0.5h, and then slowly added to the three-necked flask through a constant pressure addition funnel. The mixture was heated to reflux at 50°C for 2h until the reaction of the raw material 1,3-diamino-2-propanol was complete as monitored by TLC. Then water was added to quench the reaction, and the organic phase was extracted with DCM. The organic phase was washed with saturated sodium bicarbonate solution and saturated sodium chloride solution in turn, and anhydrous Na 2 SO 4 The mixture was dried and filtered, and the solvent was removed by rotary evaporation. The mixture was separated by column chromatography (developing solvent: DCM:MeOH=25:1) to obtain 3.71 g of a white solid, namely 1,3-di(palmitamide)-2-palmitic acid propyl ester, with a yield of 71.0%.
[0072] 1 H NMR (400 MHz, CDCl 3 )δ=6.20(s,2H),4.83(s,1H),3.49(s,2H),3.34(s,2H),2.29(s,2H),2.20(t,J=7.4Hz,4H),1.62(s,6H),1.25(s,72H),0.87(d,J=6.7Hz,9H).
[0073] Example 2: Evaluation of tribological properties of ashless friction modifier 1,3-bis(palmitamide)-2-propyl palmitate
[0074] 1,3-bis(palmitamide)-2-palmitic acid propyl ester prepared in Example 1 was added to a mixed base oil of low-viscosity synthetic hydrocarbon PAO4 and saturated polyol ester 3970 (the mass ratio of PAO4 to 3970 was 90:10) at an additive amount of 0.5wt.%, and the mixture was stirred at 60°C for 30min to obtain a nearly colorless and transparent sample oil. The friction coefficient and wear spot diameter of the blank base oil (i.e., the mixed base oil with a weight ratio of PAO4 to 3970 of 90:10) and the sample oil were tested by a four-ball friction and wear tester. The test conditions were: load 392N, spindle speed 1200r / min, oil temperature 75°C, test time 60min, and the test results are shown in Figure 1-3 .
[0075] from Figure 1 It can be seen from the friction curve comparison that the friction coefficient of the blank base oil fluctuates greatly during the friction process, indicating that its oil film is unstable, while the friction curve of 1,3-di(palmitamide)-2-palmitic acid propyl ester prepared by adding 0.5wt.% of Example 1 is more stable, indicating that the amide-ester compound of the example can effectively improve the stability of the oil film.
[0076] contrast Figure 2 and Figure 3 From the results, it can be seen that adding 0.5wt.% of 1,3-di(palmitamide)-2-palmitic acid propyl ester prepared in Example 1 can reduce the average friction coefficient and wear spot diameter by 12.5% and 24.7%, respectively, that is, the friction reduction and anti-wear properties of the oil are improved by 12.5% and 24.7%, respectively, indicating that it has good compatibility with low-viscosity synthetic base oils and can significantly improve the tribological properties of low-viscosity hydrocarbons and synthetic esters.
[0077] In addition, by Figure 3 From the wear spot morphology, it can be seen that the friction pair surface lubricated with the blank base oil has more plowing grooves caused by abrasive wear. After adding 0.5wt.% of 1,3-di(palmitamide)-2-palmitic acid propyl ester prepared in the embodiment, the plowing grooves are reduced, indicating that the amide-ester compound provided by the present invention can effectively improve the lubrication durability of low-viscosity oil.
[0078] All documents mentioned in the present invention are cited as references in this application, just as each document is cited as reference individually. In addition, it should be understood that after reading the above teachings of the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.
Claims
1. An ashless friction modifier, characterized in that: The friction modifier comprises one or more components selected from the following formulas (A)-(D): Wherein, each R1 is independently selected from H, -C m H 2m+1 or -C m H 2m-1 , R2 are each independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 30; In the friction modifier, the content of the component represented by Formula A, Formula B, Formula C or Formula D is ≥50%, preferably ≥70%, more preferably ≥90%, and most preferably ≥95%.
2. The friction modifier according to claim 1, characterized in that The friction modifier comprises one or more components selected from the following formulas (I)-(VIII): Wherein, each R1 and R2 are independently selected from -C m H 2m+1 or -C m H 2m-1 , where m is an integer from 1 to 22; In the friction modifier, the content of the component represented by Formula I, Formula II, Formula III, Formula IV, Formula V, Formula VI, Formula VII or Formula VIII is ≥50%, preferably ≥70%, more preferably ≥90%, and most preferably ≥95%.
3. The friction modifier according to claim 1, characterized in that The friction modifier is 1,3-bis(palmitamide)-2-propyl palmitate 4. A friction modifier-base oil composite, characterized in that: The composite comprises the friction modifier as claimed in claim 1; preferably, in the composite, the friction modifier is added in an amount of 0.1-10.0 wt % of the base oil, more preferably 0.1-5.0 wt %.
5. The composite according to claim 4, characterized in that The base oil is selected from the group consisting of synthetic hydrocarbon base oil, synthetic ester base oil, polyether base oil, alkyl naphthalene base oil, or a combination thereof.
6. A method for preparing a friction modifier as claimed in claim 1, characterized in that: The steps include: In an inert solvent, in the presence of a catalyst and an acid binding agent, a diamine alcohol or a diol amine reacts with R2-COCl acyl chloride to obtain an amide-ester compound; Each R1 is independently selected from H, -C m H 2m+1 or -C m H 2m-1 , R2 are each independently selected from -C m H 2m+1 or -C m H 2m-1 , wherein m is an integer from 1 to 30.
7. The preparation method according to claim 6, characterized in that: The diamine alcohol or diolamine is selected from the following group: 1,3-diamino-2-propanol, 1-amino-3-methylamino-2-propanol, 1,3-di(methylamino)-2-propanol, 1,3-di(isopropylamino)-2-propanol, 2-amino-1,3-propanediol, 2-amino-2-methyl-1,3-propanediol, 2-amino-2-ethyl-1,3-propanediol, 3-methylamino-1,2-propanediol, 3-amino-1,2-propanediol, 3-methylamino-1,2-propanediol, 3-isopropylamino-1,2-propanediol, 3-butylamino-1,2-propanediol, or a combination thereof.
8. The preparation method according to claim 6, characterized in that: The acid binding agent is selected from the group consisting of triethylamine, pyridine, Na2CO3, NaHCO3, K2CO3, NaOH, KOH, or a combination thereof.
9. The preparation method according to claim 6, characterized in that: The catalyst is selected from the following group: 4-dimethylaminopyridine (DMAP), 4-pyrrolidinopyridine (4-PPY), 4,5-dicyanoimidazole (DCI), N,N'-dicyclohexylcarbodiimide (DCC), 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide hydrochloride (EDCI), 1-hydroxybenzotriazole (HOBt), benzotriazole-N,N,N',N'-tetramethyluronium hexafluorophosphate (HBTU), or a combination thereof.
10. The preparation method according to claim 6, characterized in that: The R2-COCl acyl chloride is selected from the group consisting of butyryl chloride, hexanoyl chloride, octanoyl chloride, isooctanoyl chloride, 2-ethylhexanoyl chloride, nonanoyl chloride, decanoyl chloride, lauroyl chloride, myristoyl chloride, palmitoyl chloride, stearoyl chloride, oleic acid chloride, or a combination thereof.