Defect inspection device and defect inspection method
By using specific optical systems and image processing technology in SiC epitaxial wafers, we can accurately distinguish the location of BPD in SiC epitaxial wafers, solve the problems of low detection efficiency and complexity in the existing technology, and realize the detection of BPD in SiC epitaxial wafers. Efficient and accurate detection.
Patent Information
- Application Number
- CN202410403484.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-05
- Filing Date
- 2024-04-03
- Publication Date
- 2024-10-15
AI Technical Summary
It is difficult for existing defect inspection devices to accurately distinguish whether basal plane dislocations (BPD) in SiC epitaxial wafers are continuous from the buffer layer to the drift layer, or only exist in the buffer layer, and the existing methods are complex or have low detection efficiency.
A defect inspection device including an irradiation optical system, a filter part and a detection optical system is used. By controlling the photoluminescence band and image processing, a specific wavelength range and offset angle are used to calculate the length of the defect and distinguish between the buffer layer and the detection optical system. BPD in the drift layer and improve discrimination accuracy through machine learning algorithms.
It achieves accurate identification of BPD in SiC epitaxial wafers, improves detection efficiency and accuracy, can distinguish defects in the buffer layer and drift layer, and enhances the long-term reliability of the device.
Smart Images

Figure CN118777302A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a defect inspection device and a defect inspection method. Background Art
[0002] Silicon carbide (hereinafter referred to as SiC) has excellent physical and thermal properties and is therefore useful for the manufacture of semiconductor devices with high withstand voltage and low loss. A SiC epitaxial wafer is a wafer having an epitaxial layer containing SiC formed on a SiC substrate. In the manufacturing process of semiconductor devices using SiC epitaxial wafers, it is extremely important to detect defects present in the epitaxial layer and classify the detected defects in order to improve the manufacturing yield. In particular, basal plane dislocation (hereinafter referred to as BPD) becomes a fatal defect that has a fatal adverse effect on the performance of semiconductor devices when semiconductor devices are manufactured on SiC epitaxial wafers. Therefore, it is strongly desired to detect BPD separately from other defects.
[0003] In a SiC epitaxial wafer in which a drift layer including SiC is formed on a SiC substrate, in order to prevent the occurrence of BPD in the drift layer, a structure in which a buffer layer doped with impurities at a high concentration is sandwiched between the drift layer and the SiC substrate is sometimes adopted. By adopting such a structure, the BPD in the buffer layer can be converted into a threading edge dislocation (TED) at the interface between the buffer layer and the drift layer. The fatal defect is usually the BPD in the drift layer. Therefore, by converting the BPD in the buffer layer into a TED in the drift layer, the occurrence of fatal defects in the drift layer can be suppressed.
[0004] However, when long-term reliability is taken into consideration, it is desirable to also detect BPDs present only in the buffer layer that are converted into TEDs at the interface between the buffer layer and the drift layer.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2015-119056;
[0008] Patent document 2: Japanese Patent No. 6999212;
[0009] Patent document 3: Japanese Patent Application Publication No. 2019-099438.
[0010] Problem that the invention aims to solve
[0011] Patent Document 1 describes a defect inspection device that irradiates ultraviolet light onto a SiC epitaxial wafer and detects defects based on the generated photoluminescence. The defect inspection device of Patent Document 1 detects BPD in the drift layer based on an image of the near-infrared light band in the photoluminescence. However, the defect inspection device of Patent Document 1 has difficulty in detecting BPD in the buffer layer.
[0012] Patent Document 2 describes converting BPD in the drift layer and the buffer layer into a Shockley type stacking fault (SSF) and detecting BPD based on the photoluminescence from the converted SSF. Although the method of Patent Document 2 can detect BPD in the buffer layer, it requires converting BPD into SSF, and the inspection process is very complicated.
[0013] Patent document 3 describes detecting BPD in a high-concentration epitaxial layer by transmitting photoluminescence in a wavelength band below 430 nm. The defect inspection device of Patent document 3 can detect BPD in a high-concentration epitaxial layer as a linear defect that is darker than the surrounding area. However, there is no description of the relationship between the detected BPD and the TED in the drift layer.
[0014] It is desirable to discriminate in a SiC epitaxial wafer whether the BPD extends from the buffer layer to the drift layer or exists only in the buffer layer. Summary of the invention
[0015] The present invention has been made in view of such problems, and provides a defect inspection device and a defect inspection method capable of identifying BPD in a SiC epitaxial wafer.
[0016] Solutions for solving problems
[0017] A defect inspection device according to one mode of the present embodiment comprises: an irradiation optical system for irradiating excitation light to a sample, wherein the sample includes a silicon carbide substrate, a buffer layer formed on the silicon carbide substrate, and a drift layer formed on the buffer layer; a filter section for controlling a wavelength band through which photoluminescence generated by the sample is transmitted; a detection optical system for detecting the photoluminescence transmitted from the filter section; and an image processing section for forming an image based on the detected photoluminescence and discriminating defects captured in the formed image, wherein the filter section transmits the wavelength band including a wavelength of not less than 420 nm and not more than 430 nm in the photoluminescence, and when the thickness of the drift layer is set to D1, the thickness of the buffer layer is set to D2, the offset angle is set to θ, and the first length and the second length are set to L1 and L2 respectively as shown below,
[0018] L1=(D1+D2) / tanθ
[0019] L2=D2 / tanθ
[0020] When the length of the defect belongs to a prescribed first range including the first length, the image processing unit determines the defect as the defect including a basal plane dislocation extending from the buffer layer to the drift layer. When the length of the defect belongs to a prescribed second range including the second length, and the second range is different from the first range, the image processing unit determines the defect as the defect including the basal plane dislocation in the buffer layer and the edge dislocation in the drift layer.
[0021] In the above-mentioned defect inspection device, the filter section can change the transmitted wavelength band from the wavelength band including more than 420nm and less than 430nm to the wavelength band including near-infrared light, the detection optical system can detect the near-infrared light transmitted from the changed filter section, and the image processing section can form a near-infrared image based on the detected near-infrared light, and when the defect photographed in the formed near-infrared image is determined, when the third length is set to L3 expressed below,
[0022] L3=D1 / tanθ
[0023] When the length of the defect belongs to a predetermined third range including the third length and the third range is different from the first range and the second range, the image processing unit determines the defect as the defect including the basal plane dislocation in the drift layer.
[0024] In the above-mentioned defect inspection device, the image processing unit may calculate the accuracy of the identified defects by comparing the number of the defects having the length belonging to the first range and the number of the defects having the length belonging to the third range.
[0025] In the above-mentioned defect inspection device, the image processing unit can identify the defects captured in the image by using an algorithm that has previously performed machine learning using the plurality of defects belonging to the first range and the plurality of defects belonging to the second range as learning data.
[0026] In the above defect inspection device, the impurity concentration of the drift layer may be 1×10 15 cm -3 More than and less than 5×10 17 cm -3 , the impurity concentration of the buffer layer may be 5×10 17 cm -3 Above and 1×10 19 cm -3 the following.
[0027] A defect inspection method according to one mode of the present embodiment includes: a step of irradiating an excitation light onto a sample, the sample including a silicon carbide substrate, a buffer layer formed on the silicon carbide substrate, and a drift layer formed on the buffer layer; a step of allowing photoluminescence generated by the sample to pass through a filter, the filter controlling a wavelength band of transmission; a step of detecting the photoluminescence transmitted from the filter; a step of forming an image based on the detected photoluminescence; and a step of distinguishing a defect captured in the formed image, wherein in the step of allowing the photoluminescence to pass, the filter allows the wavelength band of the photoluminescence to pass, which is greater than or equal to 420 nm and less than or equal to 430 nm, and in the step of distinguishing the defect, when the thickness of the drift layer is set to D1, the thickness of the buffer layer is set to D2, the offset angle is θ, and the first length and the second length are set to L1 and L2 respectively as shown below,
[0028] L1=(D1+D2) / tanθ
[0029] L2=D2 / tanθ
[0030] When the length of the defect belongs to a prescribed first range including the first length, the defect is judged as the defect including a basal plane dislocation extending from the buffer layer to the drift layer. When the length of the defect belongs to a prescribed second range including the second length, and the second range is different from the first range, the defect is judged as the defect including the basal plane dislocation in the buffer layer and the edge dislocation in the drift layer.
[0031] The defect inspection method may further include: after the step of determining the defect, changing the wavelength band transmitted from the filter portion from the wavelength band including more than 420nm and less than 430nm to the wavelength band including near-infrared light; detecting the near-infrared light transmitted from the changed filter portion; forming a near-infrared image based on the detected near-infrared light; and determining the defect captured in the formed near-infrared image. In the step of determining the defect captured in the near-infrared image, when the third length is set to L3 represented below,
[0032] L3=D1 / tanθ
[0033] When the length of the defect captured in the near-infrared image belongs to a prescribed third range including the third length, and the third range is different from the first range and the second range, the defect is determined to be the defect including the basal plane dislocation in the drift layer.
[0034] The defect inspection method described above may further include a step of calculating the accuracy of the identified defects by comparing the number of the defects having the length belonging to the first range with the number of the defects having the length belonging to the third range.
[0035] In the above-mentioned defect inspection method, the defects captured in the image can be identified by using an algorithm that has previously performed machine learning using the plurality of defects belonging to the first range and the plurality of defects belonging to the second range as learning data.
[0036] In the above defect inspection method, the impurity concentration of the drift layer may be 1×10 15 cm -3 More than and less than 5×10 17 cm -3 , the impurity concentration of the buffer layer may be 5×10 17 cm -3 Above and 1×10 19 cm -3 the following.
[0037] Effects of the Invention
[0038] According to the present invention, it is possible to provide a defect inspection apparatus and a defect inspection method capable of identifying BPD in a SiC epitaxial wafer. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 This is a structural diagram illustrating a defect inspection device according to the first embodiment.
[0040] Figure 2 This is a cross-sectional view illustrating a sample to be inspected in the defect inspection apparatus according to the first embodiment.
[0041] Figure 3 This is a schematic diagram illustrating an image formed by the image processing unit in the defect inspection device according to the first embodiment.
[0042] Figure 4 This is a flowchart illustrating the defect inspection method according to the first embodiment.
[0043] Figure 5 This is a structural diagram of a defect inspection device according to the second embodiment.
[0044] Figure 6 This is a schematic diagram illustrating an image formed by the image processing unit in the defect inspection device according to the second embodiment.
[0045] Figure 7The diagram illustrates the appearance of the BPD in the defect captured by the defect inspection apparatus according to the first embodiment and the defect inspection apparatus according to the second embodiment.
[0046] Figure 8 This is a flowchart illustrating the defect inspection method according to the second embodiment. DETAILED DESCRIPTION
[0047] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. The following description shows preferred embodiments of the present invention, and the scope of the present invention is not limited to the following embodiments. In the following description, the contents marked with the same reference numerals represent substantially the same contents.
[0048] (Implementation Method 1)
[0049] The defect inspection device and defect inspection method according to the first embodiment are described. Figure 1 FIG. 1 is a structural diagram illustrating a defect inspection device 1 according to Embodiment 1. Figure 1 As shown, the defect inspection device 1 of the present embodiment includes an irradiation optical system 10 , a filter unit 20 , a detection optical system 30 , and an image processing unit 40 .
[0050] The irradiation optical system 10 irradiates the excitation light EL to the sample 50 placed on the workbench 60. The irradiation optical system 10 may include a light source 11. In addition, the irradiation optical system 10 may also include optical components such as filters, reflectors, and lenses. The irradiation optical system 10 irradiates the excitation light EL toward the SiC epitaxial wafer as the sample 50. The excitation light EL may include, for example, ultraviolet light that generates photoluminescence PL from the SiC epitaxial wafer. That is, the excitation light EL has energy greater than the energy of the bandgap of SiC.
[0051] For example, the excitation light EL may be a laser with a wavelength of 320 nm generated by a He-Cd laser, or a fourth harmonic laser with a wavelength of 266 nm generated by a YAG laser. In addition, the excitation light EL may be ultraviolet light generated by a mercury-xenon lamp. The irradiation optical system 10 may also transmit a specified wavelength band in the excitation light EL through a filter. For example, when the light source 11 is a mercury-xenon lamp, the excitation light EL may include a light beam with a wavelength of 313 nm transmitted through the filter. The irradiation optical system 10 may have optical components such as reflectors and lenses on the optical path of the excitation light EL emitted by the light source 11 to the sample 50. For example, the inspection surface of the sample 50 may be scanned with the excitation light EL by using a galvanometer mirror or the like. Alternatively, the inspection surface of the sample 50 may be scanned with the excitation light EL by moving the workbench 60.
[0052] Here, in order to facilitate the description of the defect inspection device 1, an XYZ orthogonal coordinate axis system is introduced. The direction orthogonal to the upper surface of the workbench 60 is set as the Z-axis direction, and the surface parallel to the upper surface of the workbench 60 is set as the XY surface. For example, the +Z-axis direction is set as the top, and the -Z-axis direction is set as the bottom. In addition, the top and the bottom are used to facilitate the description of the defect inspection device 1, and do not represent the actual configuration direction of the defect inspection device 1.
[0053] The filter unit 20 controls the wavelength band that transmits the photoluminescence PL generated by the sample 50. Specifically, for example, the filter unit 20 may include a filter 21 that transmits a wavelength band including 420 nm or more and 430 nm or less in the photoluminescence PL. The filter 21 transmits a wavelength band including 420 nm or more and 430 nm or less in the photoluminescence PL. For example, the filter 21 may transmit a wavelength band including a central wavelength of 425±13 nm, or may transmit a wavelength band including a central wavelength of 425±5 nm.
[0054] In addition, the optical filter unit 20 may include an optical filter 22 that transmits a wavelength band including near infrared light. The optical filter 22 transmits, for example, a wavelength band including 700 nm to 1100 nm. The optical filter unit 20 may select the optical filter 21 or the optical filter 22 according to the wavelength band to be detected.
[0055] The detection optical system 30 includes a detector 31. The detection optical system 30 detects the photoluminescence PL transmitted from the filter section 20. In addition to the detector 31, the detection optical system 30 may include optical components such as a lens and a reflective mirror that guide the photoluminescence PL transmitted from the filter section 20 to the detector 31.
[0056] The detector 31 may include an image sensor in which solid-state imaging elements such as CCD (Charged-coupled devices) and CMOS (Complementary metal-oxide-semiconductors) are arranged in a two-dimensional array, or may include a line sensor in which a plurality of imaging elements are arranged in a row.
[0057] The image processing unit 40 forms an image based on the photoluminescence PL detected by the detection optical system 30. In addition, the image processing unit 40 determines the defect captured in the formed image. The image processing unit 40 is a computer having, for example, a CPU, a memory, a storage, etc. The image processing unit 40 may also have an input and output unit including a display for displaying an image.
[0058] Figure 2 FIG. 2 is a cross-sectional view showing a sample 50 to be inspected in the defect inspection apparatus 1 according to the first embodiment. Figure 2As shown, the sample 50 includes a SiC substrate 51, a buffer layer 52, and a drift layer 53. The sample 50 has a structure in which the SiC substrate 51, the buffer layer 52, and the drift layer 53 are stacked. The buffer layer 52 is formed on the SiC substrate 51, and the drift layer 53 is formed on the buffer layer 52. Therefore, the buffer layer 52 is arranged between the SiC substrate 51 and the drift layer 53.
[0059] The SiC substrate 51 is a base for manufacturing a thin film of a buffer layer 52 and a drift layer 53 by an epitaxial growth method. The SiC substrate 51 is a substrate containing a SiC single crystal (4H-SiC). The method for manufacturing the SiC substrate 51 is not particularly limited. For example, the SiC substrate 51 is obtained by slicing a SiC ingot obtained by a sublimation method or the like. On the SiC substrate 51, the BPD may exist along the (0001) plane (c-plane).
[0060] The buffer layer 52 and the drift layer 53 are thin films containing SiC single crystal (4H-SiC) deposited on the SiC substrate 51 by epitaxial growth. Specifically, the epitaxial layer containing the buffer layer 52 and the drift layer 53 can be formed on the SiC substrate 51, and the SiC substrate 51, for example, uses the surface with an offset angle from the (0001) surface to the <11-20> direction as the growth surface. The epitaxial layer can also be 4H-SiC grown by step flow growth (lateral growth from atomic steps) on the SiC substrate 51.
[0061] The buffer layer 52 is a layer formed by epitaxially growing an epitaxial layer containing a high concentration of impurities on the SiC substrate 51. The doped impurities may be nitrogen, boron, titanium, vanadium, aluminum, gallium, phosphorus, etc. The buffer layer 52 functions, for example, in a power device to suppress minority carriers from reaching the drift layer 53. By stacking the buffer layer 52, when a current is caused to flow in the positive direction of a bipolar device having a BPD, the minority carriers can be prevented from reaching the BPD present in the SiC substrate 51.
[0062] The drift layer 53 is a layer obtained by epitaxially growing an epitaxial layer containing low-concentration impurities on the buffer layer 52. As for the doped impurities, nitrogen, boron, titanium, vanadium, aluminum, gallium, phosphorus, etc. can be used as in the aforementioned buffer layer 52. The drift layer 53 is doped with impurities at a lower concentration than the buffer layer 52, and functions as a drift layer of a SiC-MOSFET, for example.
[0063] The impurity concentration of the buffer layer 52 is preferably 1×10 18 cm -3 For example, the impurity concentration of the buffer layer 52 is preferably 5×10 17 cm -3 Above and 1×10 19 cm -3 The impurity concentration of the drift layer is preferably 1×1016 cm -3 For example, the impurity concentration of the drift layer is 1×10 15 cm -3 More than and less than 5×10 17 cm -3 .
[0064] The thickness D2 of the buffer layer 52 is, for example, 1 μm. In addition, the thickness D2 of the buffer layer 52 is not limited to 1 μm. The thickness D1 of the drift layer 53 is, for example, 10 μm. In addition, the thickness D1 of the drift layer 53 is not limited to 10 μm. The thickness D1 of the drift layer 53 is preferably different from the thickness D2 of the buffer layer 52. For example, the thickness D1 of the drift layer 53 is preferably greater than the thickness D2 of the buffer layer 52, but is not limited thereto.
[0065] In the sample 50, a part of the BPD is inherited to the drift layer 53. That is, the defect K1 formed in the sample 50 includes, for example, a BPD that is continuous from the buffer layer 52 to the drift layer 53. Specifically, the defect K1 includes a BPD that reaches the drift layer 53 from the SiC substrate 51 through the buffer layer 52. In such a defect K1, the angle formed by the direction in which the BPD extends and the upper surface of the SiC substrate 51 (called the base surface) is the offset angle θ. That is, the BPD extends in the direction of the offset angle θ relative to the base surface. The BPD inherited to the drift layer 53 emits photoluminescence PL with a wavelength of 710nm through the recombination of carriers generated by irradiating the sample 50 with the excitation light EL.
[0066] On the other hand, sometimes BPD is converted into TED at the interface 54 between the buffer layer 52 and the drift layer 53. In this case, the defect K2 formed in the sample 50 includes BPD in the buffer layer 52 and TED in the drift layer 53. Specifically, the defect K2 includes BPD in the buffer layer 52 and TED converted from BPD at the interface 54 between the buffer layer 52 and the drift layer 53. In the defect K2, the angle between the direction in which the BPD in the buffer layer 52 extends and the substrate surface is the offset angle θ. The BPD in the buffer layer 52 before being converted at the interface 54 does not emit photoluminescence PL even if the sample 50 is irradiated with the excitation light EL because the carrier lifetime in the buffer layer 52 is short.
[0067] Figure 3 Schematic diagram illustrating an image formed by the image processing unit 40 in the defect inspection device 1 according to the first embodiment. Figure 3 is an image taken from the +Z axis direction by the photoluminescence PL of the sample 50. For example, Figure 3 A field of view during the examination is shown, which is 1.75 mm square or 1.5 mm square.
[0068] like Figure 3As shown in FIG. 1 , when an image is formed by transmitting photoluminescence PL including a wavelength band of 420 nm to 430 nm, a linear defect that is darker (black) than the surrounding and longer and a short linear defect are observed in the image. For example, a black linear defect extends in the Y-axis direction. In the Y-axis direction, the length of the long linear defect is referred to as a first length L1. The length of the short linear defect is referred to as a second length L2.
[0069] Here, the thickness of the drift layer 53 is set to D1, the thickness of the buffer layer 52 is set to D2, the offset angle is set to θ, and the first length and the second length are set to L1 and L2 represented by the following equations (1) and (2), respectively. In addition, the thickness D1 of the drift layer 53 and the thickness D2 of the buffer layer 52 are preferably different, but they may be the same thickness.
[0070] L1=(D1+D2) / tanθ (1)
[0071] L2=D2 / tanθ (2)
[0072] Thus, a defect having a length of the first length L1 corresponds to a defect K1 including a BPD that continues from the buffer layer 52 to the drift layer 53. A defect having a length of the second length L2 corresponds to a defect K2 including a BPD in the buffer layer 52 and a TED in the drift layer 53. Therefore, when the length of the defect captured in the image is the first length L1, the image processing unit 40 determines the defect as the defect K1 including a BPD that continues from the buffer layer 52 to the drift layer 53. On the other hand, when the length of the defect captured in the image is the second length L2, the image processing unit 40 determines the defect as the defect K2 including a BPD in the buffer layer 52 and a TED in the drift layer 53.
[0073] In addition, the length of the defect K1 is not limited to the first length L1, and may include the first length L1 including an inevitable error caused by the deviation of the thickness generated when the buffer layer 52 and the drift layer 53 are formed. The length of the defect K2 is also not limited to the second length L2, and may include the second length L2 including an inevitable error. The inevitable error depends on the conditions such as the thickness when the buffer layer 52 and the drift layer 53 are formed, and may be, for example, ±10% of the first length L1 and the second length L2, or ±5%.
[0074] Therefore, when the length of the defect captured in the image belongs to a predetermined first range including the first length L1, the image processing unit 40 determines the defect as a defect K1 including a BPD extending from the buffer layer 52 to the drift layer 53. In addition, when the length of the defect captured in the image belongs to a predetermined second range including the second length L2, and the second range is different from the first range, the image processing unit 40 determines the defect as a defect K2 including a BPD in the buffer layer 52 and a TED in the drift layer 53. The first range is a range of the first length L1 including an inevitable error, for example, a range from (first length L1-unavoidable error) to (first length L1+unavoidable error). The second range is a range of the second length L2 including an inevitable error, for example, a range from (second length L2-unavoidable error) to (second length L2+unavoidable error).
[0075] The length of the defect can be calculated based on the number of pixels in the area detected as a defect by the image processing unit 40. In addition, the image processing unit 40 can also identify the defect captured in the image by using an algorithm that uses a plurality of defects K1 belonging to the first range and a plurality of defects K2 belonging to the second range as learning data and performs machine learning in advance.
[0076] Next, the defect inspection method according to the present embodiment will be described. Figure 4 FIG. 1 is a flowchart illustrating a defect inspection method according to Embodiment 1. Figure 4 As shown, the defect inspection method of this embodiment includes: step S11, irradiating the sample 50 with excitation light EL; step S12, allowing the photoluminescence PL to pass through the filter 20; step S13, detecting the photoluminescence PL; step S14, forming an image based on the photoluminescence PL; and step S15, determining the defects captured in the image.
[0077] First, as shown in step S11, the excitation light EL is irradiated to the sample 50. The sample 50 includes a SiC substrate 51, a buffer layer 52 formed on the SiC substrate 51, and a drift layer 53 formed on the buffer layer 52. The impurity concentration of the drift layer is, for example, 1×10 15 cm -3 More than and less than 5×10 17 cm -3 , the impurity concentration of the buffer layer is, for example, 5×10 17 cm -3 More than and less than 1×10 19 cm -3Therefore, the impurity concentration of the buffer layer 52 is greater than the impurity concentration of the drift layer 53. The excitation light EL is irradiated by the irradiation optical system 10. The irradiation optical system 10 can also scan the sample 50 with the excitation light EL. The sample 50 can also be scanned with the excitation light EL by moving the workbench 60. The sample 50 irradiated with the excitation light EL generates photoluminescence PL.
[0078] Next, as shown in step S12, the photoluminescence PL generated by the sample 50 is transmitted through the filter 20. Specifically, the photoluminescence PL generated by the sample 50 is transmitted through the filter 20, and the filter 20 controls the wavelength band to be transmitted. For example, the filter 20 transmits the wavelength band including 420 nm or more and 430 nm or less in the photoluminescence PL through the filter 21.
[0079] Next, as shown in step S13, the photoluminescence PL transmitted from the optical filter 20 is detected. For example, the detector 31 in the detection optical system 30 detects the photoluminescence PL transmitted from the optical filter 21.
[0080] Next, as shown in step S14 , an image is formed based on the detected photoluminescence PL. Specifically, the image processing unit 40 forms an image based on the photoluminescence PL detected by the detection optical system 30 including the detector 31 .
[0081] Next, as shown in step S15, the defect captured in the formed image is determined. For example, when the length of the defect captured in the image belongs to a prescribed first range including the first length L1, the image processing unit 40 can determine the defect as a defect K1 including a BPD that continues from the buffer layer 52 to the drift layer 53. In addition, when the length of the defect captured in the image belongs to a prescribed second range including the second length L2, and the second range is different from the first range, the image processing unit 40 can determine the defect as a defect K2 including a BPD in the buffer layer 52 and a TED in the drift layer 53. In this way, defects of SiC epitaxial wafers can be inspected.
[0082] Next, the effects of this embodiment are described. The defect inspection device 1 of this embodiment forms an image based on the photoluminescence PL having a wavelength band of 420 nm or more and 430 nm or less transmitted through the filter 21. Therefore, the image processing unit 40 can detect the BPD formed in the epitaxial layer as a black linear defect in the formed image. In addition, the image processing unit 40 can distinguish the defect based on the length of the defect captured in the image. Thus, the defect of the SiC epitaxial wafer can be distinguished.
[0083] Furthermore, the defect inspection apparatus 1 can identify BPD of the buffer layer 52 . Therefore, BPD existing only in the buffer layer 52 and converted into TED at the interface 54 between the buffer layer 52 and the drift layer 53 can also be identified, and the device characteristics of the drift layer 53 can be improved.
[0084] (Implementation Method 2)
[0085] Next, a description will be given of a defect inspection apparatus according to Embodiment 2. The defect inspection apparatus according to this embodiment changes the wavelength band of the photoluminescence PL transmitted through the filter 20 from a wavelength band including 420 nm to 430 nm to a wavelength band including near infrared light. Figure 5 FIG. 2 is a structural diagram of a defect inspection device according to an exemplary embodiment 2. Figure 5 As shown, the defect inspection device 2 of this embodiment is different from the defect inspection device 1 described above in that the filter 21 of the filter unit 20 is replaced by a filter 22 .
[0086] The detection optical system 30 detects the photoluminescence PL including the near-infrared light transmitted from the changed filter unit 20. The image processing unit 40 forms an image based on the detected photoluminescence PL including the near-infrared light. The image formed based on the photoluminescence PL including the near-infrared light is called a near-infrared image. The image processing unit 40 determines the defect captured in the near-infrared image.
[0087] Figure 6 Schematic diagram illustrating an image formed by the image processing unit 40 in the defect inspection device 2 according to the second embodiment. Figure 6 To photograph the sample 50 Figure 3 Figure of the same location. Figure 6 As shown, the image processing unit 40 forms a near-infrared image based on the photoluminescence PL that transmits the wavelength band including near-infrared light. In this case, a linear defect is observed in the near-infrared image. The length of the linear defect is referred to as a third length L3. Figure 6 In order to facilitate the explanation, Figure 3 The same black lines are used to illustrate linear defects in the near-infrared image.
[0088] The BPD in the buffer layer 52 is not captured in the near-infrared image. The TED in the drift layer 53 is not captured in the near-infrared image. On the other hand, the BPD in the drift layer 53 is captured in the near-infrared image.
[0089] Here, the thickness of the drift layer 53 is D1, the thickness of the buffer layer 52 is D2, the offset angle is θ, and the third length is L3 represented by the following formula (3). In addition, the thickness D1 of the drift layer 53 and the thickness D2 of the buffer layer 52 are preferably different.
[0090] L3=D1 / tanθ (3)
[0091] Therefore, the defect having the third length L3 corresponds to the defect K3 including the BPD in the drift layer 53. When the length of the defect is the third length L3, the image processing unit 40 determines the defect as the defect K3 including the BPD in the drift layer 53. The length of the defect K3 is not limited to the third length L3, and may include the third length L3 including an inevitable error caused by the thickness deviation generated when the buffer layer 52 and the drift layer 53 are formed. Therefore, when the length of the defect captured in the near-infrared image belongs to the prescribed third range including the third length L3, and the third range is different from the first range and the second range, the image processing unit 40 determines the defect as the defect K3 including the BPD in the drift layer 53.
[0092] Figure 7 1 is a diagram illustrating the appearance of BPD in defects K1 to K3 captured by the defect inspection apparatus 1 of embodiment 1 and the defect inspection apparatus 2 of embodiment 2. Figure 3 and Figure 7 As shown in FIG. 1 , when the wavelength band including 420 nm and above and 430 nm is transmitted, both defect K1 and defect K2 are captured in the image. Figure 6 and Figure 7 As shown, when the band containing near-infrared light is transmitted, defect K3 is captured in the near-infrared image. Defects K1 and K2 are not captured in the near-infrared image. In addition, defect K3 is obtained by subtracting the portion of defect K2 from defect K1. Therefore, the third length L3 becomes the difference between the first length L1 and the second length L2.
[0093] In addition, the image processing unit 40 may also calculate the accuracy of the identified defects by comparing the number of defects K1 of the first range of lengths with the number of defects K3 of the third range of lengths. The closer the number of defects K1 is to the number of defects K3, the higher the accuracy of defect identification.
[0094] Next, the defect inspection method according to the present embodiment will be described. Figure 8 FIG. 2 is a flowchart illustrating a defect inspection method according to Embodiment 2. Figure 8 As shown, the defect inspection method of this embodiment, in addition to the aforementioned steps S11 to S15, also includes: step S16, changing the wavelength band transmitted from the filter part 20 to near-infrared light; step S17, detecting the near-infrared light; step S18, forming a near-infrared image based on the near-infrared light; and step S19, determining the defects displayed in the image.
[0095] As shown in step S16 , after step S15 of determining a defect, the wavelength band transmitted by the filter unit 20 is changed from the wavelength band including 420 nm to 430 nm to the wavelength band including near infrared light. Specifically, in the filter unit 20 , the filter 21 is changed to the filter 22 .
[0096] Next, as shown in step S17, the near infrared light transmitted through the changed filter unit 20 is detected. Specifically, the detector 31 in the detection optical system 30 detects the near infrared light transmitted through the filter 22 in the filter unit 20.
[0097] Next, as shown in step S18 , the image processing unit 40 forms a near-infrared image based on the near-infrared light detected by the detection optical system 30 .
[0098] Next, as shown in step S19, the image processing unit 40 determines the defect captured in the near-infrared image. Specifically, when the length of the defect captured in the near-infrared image belongs to the third range including the third length L3, the image processing unit 40 determines the defect as a defect K3 including BPD in the drift layer 53. By determining the defect in this way, the SiC epitaxial wafer can be inspected.
[0099] In addition, after step S19, the method may further include a step of calculating the accuracy of the identified defects by comparing the number of defects K1 having a length belonging to the first range and the number of defects K3 having a length belonging to the third range.
[0100] According to this embodiment, the defect inspection device 2 can identify the defect K3 captured in the near-infrared image. Thus, the BPD in the drift layer 53 can be detected. In addition, the defect K1 captured in the image that transmits the wavelength band of 420 nm or more and 430 nm or less can be compared with the defect K3 captured in the near-infrared image, which can improve the defect detection rate. Other structures and effects are included in the description of the first embodiment.
[0101] The embodiments of the present invention have been described above, but the present invention includes appropriate modifications that do not impair its objects and advantages, and is not limited to the above embodiments. In addition, the combination of the structures of Embodiments 1 and 2 is also within the scope of the technical concept of the present invention.
[0102] Description of Reference Numerals
[0103] 1, 2: Defect inspection device;
[0104] 10: Illumination optical system;
[0105] 11: Light source;
[0106] 20: filter unit;
[0107] 21, 22: filter;
[0108] 30: Detection optical system;
[0109] 31: detector;
[0110] 40: Image processing unit;
[0111] 50: sample;
[0112] 51: SiC substrate;
[0113] 52: buffer layer;
[0114] 53: drift layer;
[0115] 54: Interface;
[0116] 60: workbench;
[0117] D1, D2: thickness;
[0118] EL: excitation light;
[0119] K1, K2, K3: defects;
[0120] L1: first length;
[0121] L2: second length;
[0122] PL: photoluminescence.
Claims
1. A defect inspection device, comprising: an irradiation optical system that irradiates excitation light to a sample, the sample including a silicon carbide substrate, a buffer layer formed on the silicon carbide substrate, and a drift layer formed on the buffer layer; A filter part for controlling the wavelength band in which the photoluminescence generated by the sample is transmitted; a detection optical system that detects the photoluminescence transmitted from the filter portion; as well as an image processing unit that forms an image based on the detected photoluminescence and identifies defects captured in the formed image, The filter unit transmits the wavelength band including 420 nm or more and 430 nm or less in the photoluminescence. When the thickness of the drift layer is set to D1, the thickness of the buffer layer is set to D2, the offset angle is set to θ, and the first length and the second length are set to L1 and L2 respectively as shown below, L1=(D1+D2) / tanθ L2=D2 / tanθ When the length of the defect is within a predetermined first range including the first length, the image processing unit determines the defect as the defect including a basal plane dislocation extending from the buffer layer to the drift layer. When the length of the defect belongs to a prescribed second range including the second length, and the second range is different from the first range, the image processing unit determines the defect as the defect including the basal plane dislocation in the buffer layer and the edge dislocation in the drift layer.
2. The defect inspection device according to claim 1, wherein: The filter unit changes the wavelength band transmitted from the wavelength band including 420 nm or more and 430 nm or less to the wavelength band including near infrared light, The detection optical system detects the near infrared light transmitted through the changed filter section, When the image processing unit forms a near-infrared image based on the detected near-infrared light and identifies the defect photographed in the formed near-infrared image, when the third length is set to L3 represented as follows: L3=D1 / tanθ When the length of the defect belongs to a predetermined third range including the third length and the third range is different from the first range and the second range, the image processing unit determines the defect as the defect including the basal plane dislocation in the drift layer.
3. The defect inspection device according to claim 2, wherein: The image processing unit calculates the accuracy of the identified defects by comparing the number of the defects having the length belonging to the first range and the number of the defects having the length belonging to the third range.
4. The defect inspection device according to claim 1, wherein: The image processing unit discriminates the defect captured in the image by using an algorithm that has previously performed machine learning using the plurality of defects belonging to the first range and the plurality of defects belonging to the second range as learning data.
5. The defect inspection device according to claim 1, wherein: The impurity concentration of the drift layer is 1×10 15 cm -3 More than and less than 5×10 17 cm -3 , The impurity concentration of the buffer layer is 5×10 17 cm -3 Above and 1×10 19 cm -3 the following.
6. A defect inspection method, comprising: a step of irradiating an excitation light to a sample, wherein the sample includes a silicon carbide substrate, a buffer layer formed on the silicon carbide substrate, and a drift layer formed on the buffer layer; A step of allowing the photoluminescence generated by the sample to transmit through a filter portion, wherein the filter portion controls a transmission wavelength band; a step of detecting the photoluminescence transmitted from the filter portion; a step of forming an image based on the detected photoluminescence; as well as a step of identifying defects captured in the formed image, In the step of transmitting the photoluminescence, The filter unit transmits the wavelength band including 420 nm or more and 430 nm or less in the photoluminescence. In the step of identifying the defect, When the thickness of the drift layer is set to D1, the thickness of the buffer layer is set to D2, the offset angle is set to θ, and the first length and the second length are set to L1 and L2 respectively as shown below, L1=(D1+D2) / tanθ L2=D2 / tanθ When the length of the defect is within a predetermined first range including the first length, the defect is determined to be the defect including a basal plane dislocation extending from the buffer layer to the drift layer. When the length of the defect belongs to a predetermined second range including the second length and the second range is different from the first range, the defect is determined to be the defect including the basal plane dislocation in the buffer layer and the edge dislocation in the drift layer.
7. The defect inspection method according to claim 6, further comprising: After the step of determining the defect, the step of changing the wavelength band transmitted through the filter portion from the wavelength band including 420 nm or more and 430 nm or less to the wavelength band including near infrared light; a step of detecting near infrared light transmitted through the changed filter portion; A step of forming a near-infrared image according to the detected near-infrared light; as well as a step of identifying the defect captured in the formed near-infrared image, In the step of determining the defect captured in the near infrared image, When the third length is set to L3 represented as follows, L3=D1 / tanθ When the length of the defect captured in the near-infrared image belongs to a prescribed third range including the third length, and the third range is different from the first range and the second range, the defect is determined to be the defect including the basal plane dislocation in the drift layer.
8. The defect inspection method according to claim 7, further comprising: A step of calculating the accuracy of the identified defects by comparing the number of the defects of the length belonging to the first range with the number of the defects of the length belonging to the third range.
9. The defect inspection method according to claim 6, wherein: In the step of identifying the defect, The defect captured in the image is identified by using an algorithm that has previously performed machine learning using the plurality of defects belonging to the first range and the plurality of defects belonging to the second range as learning data.