Integral forming method of heat shield
Simplifying the processing process of heat shields through the integral molding method, using automatic argon arc welding and internal expansion and external expansion molds to solve the problems of long processing cycle and low efficiency in traditional methods, and achieve high-quality, low-cost thermal insulation Screen mass production.
Patent Information
- Application Number
- CN202411145313.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-10-18
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional heat shield processing methods have problems such as long processing cycle, low efficiency, high occupancy rate of personnel and equipment, and poor welding and grinding quality, making it difficult to achieve mass production.
The overall forming method is adopted, including material preparation, punching and blanking, deburring, automatic argon arc welding, integral expansion, end face cutting and other steps. The process flow is simplified through high-speed punching, automatic argon arc welding and internal expansion and external expansion molds. , improve processing efficiency and quality.
The high-quality integral molding of the heat shield is achieved, and the air film holes are accurately positioned, which reduces the turnover cycle and processing costs, improves the efficiency and quality of mass production, and reduces the occupancy of personnel and equipment.
Smart Images

Figure CN118789233A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of aerospace technology, and relates to the forming of a cylindrical sheet metal with a wavy surface, mold design and manufacturing, precise calculation of rough materials and plane development, and sheet metal simulation application. Background Art
[0002] Figure 1 and Figure 2 A heat shield part was displayed. The structure of the part is a thin-walled cylindrical part with annular corrugated ribs, and the overall shape is a circular cylinder with a diameter of more than 1 meter. The heat shield is formed by processing 0.8mm thick alloy sheet. Since the cross-section of the heat shield is a wavy ring structure and the part is large in size, the traditional processing method uses 1 / 3 section forming and then manual argon arc welding to form a cylinder. The part diameter and surface size are corrected by the correction mold, and then the air film holes on the heat shield are processed by laser drilling. Finally, the heat shield is finally processed by expanding the hole, removing burrs, and cutting the two ends. However, the traditional processing method is difficult to process, and has the disadvantages of long processing cycle, low processing efficiency, high personnel and equipment occupancy rate, poor welding and grinding quality, etc., which makes it difficult to achieve mass production of parts. Summary of the invention
[0003] In response to the problems recorded in the background technology, the present invention aims to provide a method for integrally forming a heat insulation screen, which has high surface forming quality, accurate positioning of air film holes, simple forming process, reduced turnover cycle between different processes, saving processing costs in the development process, low personnel and equipment occupancy rate, and can accelerate the progress of mass production.
[0004] To achieve the above object, the present invention adopts the following technical solutions:
[0005] The heat shield integral forming method comprises the following steps:
[0006] Step 1, material preparation: select plates of the same thickness as the thickness requirements of the heat shield in the heat shield parts drawing, take the cylindrical surface coaxial with the heat shield in the heat shield parts drawing as the basis, take the generatrix length of the cylindrical surface plus a margin as the width of the plate, and take the circumferential development length of the cylindrical surface plus a margin as the length of the plate;
[0007] Step 2, punching and cutting: according to the position relationship and size of the air film holes in the heat insulation screen parts diagram and the plate size determined in step 1, a high-speed punch is used to punch and cut the plate to obtain two plates with holes and a width equal to the width of the plate in step 1 and a length half the length of the plate in step 1;
[0008] Step 3: Deburring: remove the burrs at the punching holes and the burrs on the edges of the sheet;
[0009] Step 4: Automatic argon arc welding: butt the two plates after deburring at both ends in the length direction, and then perform automatic argon arc welding to weld the two plates into a cylinder;
[0010] Step 5: Overall bulging: Place the cylinder into a bulging mold, and use the bulging mold to perform overall bulging molding on the cylinder to obtain a surface including a corrugated surface on the heat insulation screen.
[0011] Step 6, end face cutting: Cut the two axial end faces of the cylinder after expansion so that the cylinder's profile height is consistent with the heat shield part drawing. At the same time, the distance from the cylinder hole to the end face is consistent with the distance from the air film hole to the end face in the heat shield part drawing.
[0012] As an option, in step 1, the cylindrical surface is selected so that the distance from its generatrix to the crest of the heat insulation screen is equal to the distance to the trough.
[0013] As an option, in step 1, the margin is 10 to 15 mm.
[0014] As an option, in step 2,
[0015] Based on the cylindrical surface coaxial with the heat insulation shield in the heat insulation shield parts drawing, take the generatrix of the cylindrical surface as the coordinate axis, take the vertical projection point of the midpoint of the axial length of the heat insulation shield in the heat insulation shield parts drawing on the aforementioned coordinate axis as the coordinate origin, take the arc length of the heat insulation shield corrugation between the origin and the air film hole as the coordinate of the air film hole on the coordinate axis, and take the coordinate as the first processing position of the air film hole;
[0016] The first heat insulation shield is trial-produced with the initial processing position of the above-mentioned air film holes plus the reserved margins at both ends of the axial direction of the heat insulation shield when designing the expansion mold. Then, the positions of the air film holes in the trial-produced parts are compared with the positions of the air film holes in the heat insulation shield parts drawing, the initial processing position of the above-mentioned air film holes is corrected, and the corrected values are used as the correct processing positions of subsequent air film holes.
[0017] As an option, in step 2, when a high-speed punch is used to punch holes in the plate, the tolerance of the hole is the positive tolerance of the air film hole in the heat insulation shield part drawing.
[0018] As an option,
[0019] In the step 2, when the high-speed punching machine is used to punch the plates, a length region is reserved at both ends of the two plates in the length direction without punching;
[0020] The step six also includes a supplementary drilling step, in which holes are drilled in the non-punching area reserved in step two near the two welds on the cylinder, so that the holes in this area are consistent with the air film holes in the same area in the heat insulation shield parts diagram in terms of number, size and position.
[0021] As an option, in step three, a drill press is used to remove burrs on the edge of the punching hole, and an abrasive belt is used to remove burrs on the edge of the plate.
[0022] As an option, in step 4, during automatic argon arc welding, the punched holes on the plate are used as welding positioning references.
[0023] As an option, a heat treatment step is further included between step four and step five to remove welding stress generated during the automatic argon arc welding of the cylinder.
[0024] As an option, the bulging die used in step 5 includes:
[0025] An upper template and a lower template, wherein the upper template and the lower template are arranged in parallel and spaced apart in a vertical direction;
[0026] An inclined guide rail, wherein two inclined guide rails are arranged relative to each other at intervals to form a group of guide rails, and multiple groups of guide rails are evenly distributed on the same circumference of the upper end surface of the lower template, and the spacing between the lower ends of the two inclined guide rails in the same group of guide rails is smaller than the spacing between the upper ends;
[0027] Inner expansion flaps and outer expansion flaps, the inner expansion flaps and the outer expansion flaps are respectively slidably connected to different inclined guide rails in the same set of guide rails;
[0028] The ejector block is arranged between the inner expansion flap, the outer expansion flap and the lower template, and can move in the vertical direction relative to the lower template.
[0029] As an option, in step six, laser alignment of holes and profiles is first performed before end face cutting, specifically including:
[0030] Laser alignment hole: select any hole on the cylinder after bulging, align the laser beam with the edge of the hole, keep the height of the laser beam unchanged, rotate the cylinder for one circle, observe the height position deviation of the other holes in the same row with the hole relative to the laser beam, and then adjust the clamping height of the cylinder relative to the laser beam so that the holes in the same row are at the same height;
[0031] Laser alignment of the profile, use a profile clamp to check whether the profile height dimension of the cylinder is qualified, and use the profile clamp to draw multiple measuring points along the circumferential surface of the cylinder corresponding to the end face positions at both axial ends. Then aim the laser beam at one of the measuring points, keep the laser beam height unchanged, rotate the cylinder for one circle, observe the height offset of multiple measuring points relative to the laser beam, and then adjust the clamping height of the cylinder relative to the laser beam so that multiple measuring points corresponding to the same end face position are at the same height.
[0032] Compared with the prior art, the present invention has the following characteristics:
[0033] 1. The forming method of the present invention is simple. Compared with the traditional forming process, the processing route of the present invention is simple, the hole is processed first and then the wavy surface is formed, the processing process has fewer turnover times and higher processing efficiency; 2. The present invention adopts an overall bulging method. The part profile formed by the bulging mold used in the overall bulging forming method is more in line with the design drawings. The bulging mold design with an inner bulging and outer contracting structure has certain advantages for parts that are difficult to remove from the mold after bulging (cylinders with wavy or annular rib structures); 3. The processing quality of the present invention is higher. The present invention uses automatic argon arc welding to process two perforated plates. Compared with the existing manual argon arc welding of the profiled surface, it is easier to operate, has better welding quality, high processing efficiency, and lower personnel and equipment occupancy rate.
[0034] 4. The hole position confirmation method of the present invention is easier to operate, and the obtained hole processing position is accurate. Combined with the subsequent cutting end processing, the correct position of the air film hole on the heat insulation screen can be ensured.
[0035] 5. The present invention adopts a method of laser alignment of holes and molded surfaces to correct the slight position deviation between the air film hole and the end surface of the cylinder generated during the expansion process.
[0036] Through the molding method of the present invention, not only the rapid molding (integral molding) method of the heat insulation screen with annular ribs or wave structure is mastered, but also the method of determining the position of the holes before molding of such parts and the design and manufacture of the bulging mold with internal expansion and external contraction are mastered, which effectively improves the processing efficiency and processing quality of such parts, saves the processing cost in the process of parts development, accelerates the progress of mass production, and provides technical guarantee for the mass production of such parts.
[0037] At present, the processing method of the present invention has been used on site and has achieved the purpose of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 It is a three-dimensional schematic diagram of the heat shield parts;
[0039] Figure 2 It is a two-dimensional schematic diagram of the heat shield parts;
[0040] Figure 3 It is a schematic diagram of sheet metal punching material;
[0041] Figure 4 It is a schematic diagram of the structure of the bulging die with the outer contraction and the inner expansion;
[0042] Figure 5 It is the hole processing position confirmation drawing during the first trial production;
[0043] Figure 6 It is to confirm the rough material size schematic diagram according to the heat shield parts drawing;
[0044] In the figure, 1-lower template; 4-ejection block; 5-inclined guide rail; 6-outer expansion flap; 7-upper template; 9-inner expansion flap. DETAILED DESCRIPTION
[0045] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments, but it should not be understood that the scope of the subject matter described in the present invention is limited to the following embodiments. Without departing from the above-mentioned technical ideas of the present invention, various modifications, substitutions and changes made according to the common technical knowledge and customary means in the field are included in the scope of the present invention.
[0046] against Figure 1 and Figure 2 The heat shield shown in the figure adopts a combination of reasonable process arrangement and sheet metal simulation, and finally processes a qualified heat shield that meets the requirements of the drawing through field tests. The processing steps of the present invention are as follows:
[0047] Step 1: Prepare the required thickness of the plate according to the drawing requirements. The plate thickness requirement is consistent with the final material thickness requirement of the heat insulation screen in the heat insulation screen drawing. The plate length ( Figure 3 L 长 ),Width( Figure 3 H 宽 ) must exceed the required length and width by (10-15) mm. The required length and width here refer to Figure 2 The circumferential length and axial length H of the cylindrical surface coaxial with the heat shield after expansion in the heat shield parts drawing are as follows, for example Figure 2 ΦD1 and ΦD2 are the diameters at both ends of the heat insulation screen, and both can be used as cylindrical surfaces coaxial with the heat insulation screen.
[0048] Step 2: Determine the size of the rough material: To ensure a better surface after forming the part, the sheet metal simulation software PAM-STAMP is used to perform forming simulation to confirm that the final rough material is the rough material between the crest and the trough, which is the best for forming the part surface. That is, the cylindrical surface located between the crest and the trough is selected, corresponding to Figure 2 The cylindrical surface with a distance of L in the interval of length 2L is then unfolded, and the circumference of the unfolded cylindrical surface plus (10-15) mm is obtained to obtain L 长 , the axial length of the unfolded cylinder plus (10-15) mm to obtain H 宽 .
[0049] Step 3, confirm the hole position size: because the height direction of the material cannot be clearly seen during the part forming process, the confirmation of the hole position size (the position information of the hole on the rough material) is one of the difficulties of the present invention. In order to ensure that the hole position of the final overall forming meets the requirements of the final drawing of the part, it is proved through simulation and experiments that the part is formed by moving the material from both ends to the middle position. Therefore, the center position of the final size of the part is taken as the 0 point (origin), and the arc length is calculated or measured from the 0 point to both ends to fix the hole position of the first processing (such as Figure 5 , the 0 point is drawn at the midpoint of the axial length of the heat shield, and the positions of the air film holes are marked along the arrow direction. The specific distance of the air film holes relative to the 0 point is indicated by Figure 5 The value of R in Figure 2 The R3 value in the calculation is used to calculate the arc length of the wave arc, and the arc length is used as the coordinate distance. It should be noted that the straight-line distance from the air film hole to the 0 point is not calculated, but the arc length of the wave arc is calculated as the distance from the 0 point, which is equivalent to straightening the wave arc). After confirming the coordinate size of each row of holes, add the margins reserved at both ends when designing the bulging mold ( Figure 4 L1 and L2 in it are the margins reserved for bulging. The length retained by cutting at both ends after bulging is h. During bulging, relatively excess sheet material must be left at both ends to ensure that there is no shortage of material at both ends of the part after final forming). This is the first test size (hole position information on the sheet material). This size is the closest to the drawing requirements during forming. The size can be adjusted through actual measurement after the test (including the distance between holes and the distance between the hole and the end face of the cylinder) to obtain the hole position size that meets the final drawing requirements.
[0050] Step 4: Punching and cutting: According to the hole position size determined in step 3, use high-speed punching machine programming to punch and cut the plate rough material determined in step 2 to ensure the processed hole size ( Figure 2 The Φd) and the length and width of the sheet material meet the requirements of the drawing (because the hole has a certain deformation during the forming process, in order to make the final formed hole meet the tolerance requirements of the drawing, the hole diameter tolerance is between +0.05 and +0.1 when punching, and negative tolerance cannot be used). When punching, since the two ends of the sheet material need to be welded, the holes that interfere with the edge of the sheet material are not processed, and the holes are drilled after the final forming.
[0051] Step 5. Deburring: Use a drill press (or hand drill) to remove burrs on the edge of the hole, and use an abrasive belt to remove burrs around the parts.
[0052] Step 6: Automatic argon arc welding: Automatic argon arc welding is performed on the raw material of the plate, and the welding becomes Figure 6The straight-cylinder structure shown. When welding, the two ends of the rough material need to be aligned, and the misalignment should not exceed 0.3mm (in order to ensure the longitudinal position size of the hole on the plate rough material, it is best to use the hole on the plate rough material for positioning during automatic argon arc welding to ensure the consistency of the longitudinal position of the hole). Automatic argon arc welding is used to improve the welding quality and efficiency of parts (the traditional forming method is to perform manual argon arc welding on 1 / 3 rough material with a corrugated surface, which has poor welding quality and requires 3 people to complete the welding, and the welding efficiency is low).
[0053] Step 7, heat treatment: heat treatment is performed on the welded cylinder parts to remove welding stress (because there is a certain welding stress after welding, and the parts are subsequently formed by the overall expansion method. There is extension of the raw material during forming. If the welding stress at the weld is not removed, weld cracks are easily caused during the forming process).
[0054] Step 8: Overall bulging: Use a bulging mold to bulge the heat-treated cylinder, and obtain the required surface and diameter size of the heat insulation screen through bulging. Figure 4 As shown, the structure of the bulging mold is an inner-expanding and outer-contracting structure. Since the cylinder after heat treatment is smaller than the size of the final mold surface of the heat shield, there is a situation where the cylinder cannot be placed into the bulging mold. When designing the bulging mold, multiple sets of inclined guide rails 5 distributed on the same circumference and installed on the lower mold plate 1 are designed to cooperate with the sliding of the inner expansion flap 9 and the outer expansion flap 6, so that the inner expansion flap 9 and the outer expansion flap 6 move outward and inward respectively under the action of the ejection block 4, and finally the cylinder is placed. Finally, the upper mold plate 7 moves downward to press the inner expansion flap 9 and the outer expansion flap 6 downward while moving them outward and inward respectively, thereby realizing the forming of the cylinder surface (satisfying the Figure 2 Medium dimensions α°, H3, 2L, R1, R2 and R3).
[0055] Step 9: Laser cutting: Process the end surface of the formed cylinder parts to make the hole-to-edge size and profile height meet the requirements of the drawing (such as Figure 2As shown, the requirements of ΦD1, ΦD2, H, H1, H2, L1 and 2L1 are met). This step can also be achieved by turning the end face, but the efficiency is lower than laser processing. When laser cutting the end, laser alignment of the hole and the profile is required. The laser alignment of the hole is because the part is punched on a flat plate. After forming, the position of the hole relative to the part profile is fixed. When the final height of the part is ensured at both ends of the laser processed part, the position distance from the hole to the edge is also generated at the same time. In order to ensure that the position size of the hole at this time also meets the requirements of the drawing, and at the same time, it is necessary to ensure that the distance of a whole circle of holes relative to the end face of the part can meet the drawing size, so before processing the end face, it is necessary to use a laser beam to align the edge of one of the holes, and adjust the height by rotating one circle to ensure that the holes are at the same height. This method is to keep the laser beam at the height of one of the holes The edge of the height keeps the beam height unchanged. , by rotating the part for one circle, check the distance between the edge of the same row of holes and the laser beam, and by fine-tuning the clamping height of the part, ensure that the positions of the holes in the same row are at the same height, so that the distance from the same row of holes to the edge can be guaranteed after the cutting end; Regarding laser alignment of the profile, it means that before the end of the part is cut, the clamped part is passed through a profile clamp (the profile clamp is a measuring tool whose size conforms to the outer profile and height size of the part) to draw the upper and lower points on the outer surface of the part (4 to 8 pairs can be drawn symmetrically), and then the laser beam is aimed at one of the points, and the height of the remaining points relative to the laser beam is checked by rotating one circle, and the clamping height of the part is fine-tuned to ensure that the profile and end face meet the requirements of the drawing.
[0056] Step 10: Drill additional holes: Re-drill the holes at the weld positions in step 6 to ensure the final hole quantity and position size required by the heat shield drawing.
[0057] The contents not described in detail in the specification of the present invention belong to the prior art known to the professional and technical personnel in the field. Although the illustrative specific embodiments of the present invention are described above to facilitate the understanding of the present invention by the technical personnel in the field, it should be clear that the present invention is not limited to the scope of the specific embodiments. For ordinary technicians in the field of this technology, as long as various changes are within the spirit and scope of the present invention defined and determined by the attached claims, these changes are obvious, and all inventions and creations using the concept of the present invention are protected.
Claims
1. A method for integrally forming a heat shield, characterized in that: The following steps are involved: Step 1, material preparation: select plates of the same thickness as the thickness requirements of the heat shield in the heat shield parts drawing, take the cylindrical surface coaxial with the heat shield in the heat shield parts drawing as the basis, take the generatrix length of the cylindrical surface plus a margin as the width of the plate, and take the circumferential development length of the cylindrical surface plus a margin as the length of the plate; Step 2, punching and cutting: according to the position relationship and size of the air film holes in the heat insulation screen parts diagram and the plate size determined in step 1, a high-speed punch is used to punch and cut the plate to obtain two plates with holes and a width equal to the width of the plate in step 1 and a length half the length of the plate in step 1; Step 3: Deburring: remove the burrs at the punching holes and the burrs on the edges of the sheet; Step 4: Automatic argon arc welding: butt the two plates after deburring at both ends in the length direction, and then perform automatic argon arc welding to weld the two plates into a cylinder; Step 5: Overall bulging: Place the cylinder into a bulging mold, and use the bulging mold to perform overall bulging molding on the cylinder to obtain a surface including a corrugated surface on the heat insulation screen. Step 6, end face cutting: Cut the two axial end faces of the cylinder after expansion so that the cylinder's profile height is consistent with the heat shield part drawing. At the same time, the distance from the cylinder hole to the end face is consistent with the distance from the air film hole to the end face in the heat shield part drawing.
2. The heat shield integral forming method according to claim 1, characterized in that: In the step 1, the cylindrical surface is selected so that the distance from its generatrix to the crest of the heat insulation screen is equal to the distance to the trough.
3. The heat shield integral forming method according to claim 1, characterized in that: In the step 2, Based on the cylindrical surface coaxial with the heat insulation shield in the heat insulation shield parts drawing, take the generatrix of the cylindrical surface as the coordinate axis, take the vertical projection point of the midpoint of the axial length of the heat insulation shield in the heat insulation shield parts drawing on the aforementioned coordinate axis as the coordinate origin, take the arc length of the heat insulation shield corrugation between the origin and the air film hole as the coordinate of the air film hole on the coordinate axis, and take the coordinate as the first processing position of the air film hole; The first heat insulation shield is trial-produced with the initial processing position of the above-mentioned air film holes plus the reserved margins at both ends of the axial direction of the heat insulation shield when designing the expansion mold. Then, the positions of the air film holes in the trial-produced parts are compared with the positions of the air film holes in the heat insulation shield parts drawing, the initial processing position of the above-mentioned air film holes is corrected, and the corrected values are used as the correct processing positions of subsequent air film holes.
4. The heat shield integral forming method according to claim 1, characterized in that: In the step 2, when a high-speed punching machine is used to punch holes in the plate, the tolerance of the hole is the positive tolerance of the air film hole in the heat insulation shield part drawing.
5. The heat shield integral forming method according to claim 1, characterized in that: In the step 2, when the high-speed punching machine is used to punch the plates, a length region is reserved at both ends of the two plates in the length direction without punching; The step six also includes a supplementary drilling step, in which holes are drilled in the non-punching area reserved in step two near the two welds on the cylinder, so that the holes in this area are consistent with the air film holes in the same area in the heat insulation shield parts diagram in terms of number, size and position.
6. The heat shield integral forming method according to claim 1, characterized in that: In the step three, a drilling machine is used to remove burrs on the edge of the punching hole, and an abrasive belt is used to remove burrs on the edge of the plate.
7. The heat shield integral forming method according to claim 1, characterized in that: In the step 4, during automatic argon arc welding, the punched holes on the plate are used as welding positioning references.
8. The heat shield integral forming method according to claim 1, characterized in that: A heat treatment step is also included between step 4 and step 5 to remove the welding stress generated during the automatic argon arc welding of the cylinder.
9. The heat shield integral forming method according to claim 1, characterized in that: The bulging die used in step 5 includes: An upper template (7) and a lower template (1), wherein the upper template (7) and the lower template (1) are arranged in parallel and spaced apart in a vertical direction; An inclined guide rail (5), wherein two inclined guide rails (5) are arranged relative to each other at intervals to form a group of guide rails, and the multiple groups of guide rails are evenly distributed on the same circumference of the upper end surface of the lower template (1), and the spacing between the lower ends of the two inclined guide rails (5) in the same group of guide rails is smaller than the spacing between the upper ends; Inner expansion flaps (9) and outer expansion flaps (6), wherein the inner expansion flaps (9) and the outer expansion flaps (6) are respectively slidably connected to different inclined guide rails (5) in the same set of guide rails; An ejector block (4) is arranged between the inner expansion flap (9), the outer expansion flap (6) and the lower template (1), and is capable of moving in a vertical direction relative to the lower template (1).
10. The heat shield integral forming method according to claim 1, characterized in that: In the step 6, laser alignment of holes and profiles is first used before end face cutting, specifically including: Laser alignment hole: select any hole on the cylinder after bulging, align the laser beam with the edge of the hole, keep the height of the laser beam unchanged, rotate the cylinder for one circle, observe the height position deviation of the other holes in the same row with the hole relative to the laser beam, and then adjust the clamping height of the cylinder relative to the laser beam so that the holes in the same row are at the same height; Laser alignment of the profile, use a profile clamp to check whether the profile height dimension of the cylinder is qualified, and use the profile clamp to draw multiple measuring points along the circumferential surface of the cylinder corresponding to the end face positions at both axial ends. Then aim the laser beam at one of the measuring points, keep the laser beam height unchanged, rotate the cylinder for one circle, observe the height offset of multiple measuring points relative to the laser beam, and then adjust the clamping height of the cylinder relative to the laser beam so that multiple measuring points corresponding to the same end face position are at the same height.
Citation Information
Patent Citations
Machining method for special-shaped wall of aero-engine
CN117260197A
Aero-engine lobe mixer machining method and bulging die
CN117260278A
Thermal forming method for titanium alloy conical cylinder
CN118357680A
Laser / arc hybrid welding method and method for producing welded member using same
US20120325787A1