Fractured rock mass fluid seepage visualization device based on resistivity and monitoring method
Through resistivity-based methods, the resistivity and permeability of fractured rock masses are measured and simulated, and visual images are generated, which solves the problem of difficulty in monitoring fluid seepage inside fractured rock masses with traditional devices and achieves real-time and accurate seepage analysis and monitoring.
Patent Information
- Application Number
- CN202410847804.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-27
- Publication Date
- 2024-10-18
AI Technical Summary
It is difficult for traditional rock mass visualization devices to achieve comprehensive observation and analysis of fluid seepage inside fractured rock masses. The operation is complex and costly, and it is difficult to achieve real-time monitoring and feedback.
A method of visualizing fluid seepage in fractured rock mass based on resistivity is adopted. By measuring the three-dimensional resistivity tensor and converting it into a permeability tensor, a theoretical mathematical model is used for simulation, and a visual image is generated to reflect the seepage channels and paths inside the rock mass. .
Real-time monitoring and analysis of fluid seepage inside fractured rock mass is achieved, reducing testing costs and destructiveness, improving detection efficiency and accuracy, enabling timely acquisition of seepage information, and supporting scientific engineering applications.
Smart Images

Figure CN118794856A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of fractured rock mass seepage visualization, and in particular to a fractured rock mass fluid seepage visualization device and a monitoring method based on resistivity. Background Art
[0002] In the field of geological engineering, fluid seepage in fractured rock mass is an important research topic. Fluid migration in fractured rock mass has an important impact on groundwater resource development, groundwater pollution prevention and control, geotechnical engineering stability, etc. Traditional rock mass visualization devices can usually only provide monitoring of the surface of fractured rock mass or local areas of the surface, and it is difficult to achieve comprehensive observation and analysis of fluid seepage inside fractured rock mass.
[0003] In addition, traditional rock visualization devices require complex equipment and professional technical support, are costly, and complex to operate, which is not conducive to their promotion and use in field surveys. Data collection and processing take a long time, making it difficult to achieve real-time monitoring and feedback of the fluid seepage process, and also limits the timely grasp of the dynamic changes of fractured rock masses.
[0004] Therefore, based on the above technical problems, it is necessary to improve the current monitoring methods and monitoring devices for fractured rock masses in order to achieve comprehensive observation and analysis of fluid seepage inside fractured rock masses. Summary of the invention
[0005] The purpose of the present invention is to provide a resistivity-based fractured rock mass fluid seepage visualization device and monitoring method, so as to solve the technical problem that traditional rock mass visualization devices can usually only provide monitoring of the fractured rock mass surface or a local area of the surface, and it is difficult to achieve comprehensive observation and analysis of the fluid seepage inside the fractured rock mass.
[0006] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0007] In a first aspect, the present invention discloses a method for visually monitoring fluid seepage in a fractured rock mass based on resistivity, comprising the following steps:
[0008] S1. Sampling from the fractured rock mass to obtain fractured rock mass samples;
[0009] S2, measuring the three-dimensional resistivity of the fractured rock mass sample to obtain the three-dimensional fractured rock mass resistivity tensor;
[0010] S3, constructing a theoretical mathematical model of the entire fractured rock mass, and converting the three-dimensional fractured rock mass resistivity tensor obtained in step S2 into a three-dimensional fractured rock mass permeability tensor;
[0011] S4, simulating the fluid seepage condition of the entire fractured rock mass in a theoretical mathematical model using the three-dimensional fractured rock mass resistivity tensor obtained in step S2 and the three-dimensional fractured rock mass permeability tensor obtained in step S3, and converting them into a visual image.
[0012] The basic principle used by the visualization monitoring method of the present invention is that the resistivity characteristics of fractured rock mass are sensitive to fluid seepage. In fractured rock mass, fluid seepage will change the resistivity distribution in the fractures. By using this characteristic, the fluid migration in the fractured rock mass can be indirectly monitored and visualized by measuring the resistivity change. Then, this scheme first needs to monitor the measured resistance value of the fractured rock mass sample and convert it into a resistivity tensor, and then simulate and analyze it through a theoretical mathematical model to obtain a permeability tensor, which can then be converted into image data after computer display, so as to realize the visualization operation of fluid seepage in fractured rock mass; this scheme combines the resistivity tensor with the three-dimensional fractured rock mass permeability tensor, and can more accurately reflect the real seepage channel and path of the fractured rock mass through visualized image simulation, so as to realize the automation of fractured rock mass seepage visualization test.
[0013] Preferably, in step S2, the three-dimensional resistivity of the fractured rock sample is measured by the following method:
[0014] S2.1. Install multiple positive electrodes and multiple negative electrodes on the surface of the fractured rock sample, each positive electrode corresponds to a negative electrode, and connect each positive electrode and each negative electrode to the current output terminal and current input terminal of the LCR digital bridge respectively;
[0015] S2.2. Power on the LCR digital bridge, use the LCR digital bridge to measure the real-time resistance value of the fractured rock sample from multiple directions, and convert the real-time resistance value into three-dimensional fractured rock resistivity.
[0016] Preferably, in step S2.1, each of the positive electrodes and each of the negative electrodes are flexible electrodes, and each of the positive electrodes and each of the negative electrodes are respectively installed with a position adjustment member for adjusting the position of each of the positive electrodes and each of the negative electrodes on the surface of the fractured rock sample, so that each of the positive electrodes and each of the negative electrodes are enclosed to form an internal space, and the fractured rock sample can be enclosed in the internal space.
[0017] Preferably, in step S2.1, a stress sensor and a stress regulating device are respectively provided on two adjacent negative electrodes, and the stress sensor can sense the stress magnitude of the negative electrode on the fractured rock sample;
[0018] In step S2.2, after the LCR digital bridge is powered on, first observe whether the resistivity value on the LCR digital bridge is within a reasonable range, where the reasonable range refers to the resistivity value corresponding to when the stress value applied by the electrode to the surface of the fractured rock sample is ≤1 kPa;
[0019] If it is not within the reasonable range, the error caused by the contact resistivity is too large. At this time, the stress adjustment device should be adjusted so that the stress value of the electrode on the surface of the fractured rock sample is ≤1kPa to reduce the error caused by the contact resistivity.
[0020] Preferably, in step S2.2, the stress value applied by the electrode to the surface of the fractured rock sample is 1 kPa, at which time the influence of the contact resistivity can be minimized.
[0021] As a preferred embodiment, specifically, in step S2.2, the center point of the fractured rock sample is taken as the coordinate origin O, and a z coordinate system of the fractured rock fluid seepage visualization monitoring method based on resistivity is established, in which the coordinate axes are perpendicular to each other, and the three-dimensional fractured rock resistivity tensor ρ ij It is expressed as:
[0022]
[0023] In the formula, i∈{x,y,z}, j∈{x,y,z};
[0024] In step S3, the resistivity tensor ρ of the three-dimensional fractured rock mass ij and the permeability tensor k of three-dimensional fractured rock mass ij The relationship is:
[0025]
[0026] Where H is the correction coefficient of the crack resistivity concentration tensor, f is the crack connectivity coefficient; δ ij is the Kronecker function; η is the fracture permeability tensor correction coefficient, r is the crack radius, A is the crack shape factor, which is π2; ρ ij is the resistivity tensor of fractured rock mass;
[0027] in,
[0028]
[0029] In the formula, τ represents the average number of intersections of each crack; τ c represents the permeation threshold; β represents the crack shape factor;
[0030] Then, the permeability tensor k of three-dimensional fractured rock mass is ij It can be expressed as:
[0031]
[0032] In the formula, i∈{x,y,z}, j∈{x,y,z}.
[0033] Preferably, in step S4, the visualization image is a three-dimensional visualization model, which is used to display the spatial distribution and connectivity of cracks inside the rock mass, and the spatial variation of permeability, and can also display multi-level permeability distribution by adjusting the transparency of different rock layers or cracks;
[0034] Alternatively, the visualization image is a color-coded image, which is used to represent different components of the permeability tensor by different colors, and to reflect the magnitude or change trend of the permeability by using the depth or gradient of the colors;
[0035] Or, the visual image is a flow diagram, which is used to show the potential flow path of the fluid in the rock mass, using arrows or streamlines to indicate the direction and speed of the fluid flow;
[0036] Or, the visualization image is a fracture network diagram, which is used to highlight and represent the fracture network through different visual elements, including the width, length and aperture of the fractures, and to provide quantitative information on parameters such as fracture density, fracture directionality, and permeability anisotropy;
[0037] Or, the visualization image is a contour map, which is used to represent the equal distribution of permeability in the rock mass through contour lines (such as isopreservability lines);
[0038] Or, the visualization image is an interactive view for rotating, zooming or slicing the three-dimensional model through interactive tools to view the permeability distribution from different angles and depths;
[0039] Alternatively, the visualization image is a dynamic simulation diagram, which is used to display the dynamic changes of the seepage process according to the changes in time.
[0040] In a second aspect, the present invention discloses a device for visualizing fluid seepage in a fractured rock mass based on resistivity, which is used to monitor a fractured rock mass sample using the method for visualizing fluid seepage in a fractured rock mass based on resistivity as described above, and includes a positive electrode and a negative electrode, wherein the positive electrode and the negative electrode are respectively attached to the surface or the inside of the fractured rock mass sample;
[0041] Also included is an LCR digital bridge, which is electrically connected to the positive electrode and the negative electrode respectively and can provide an input current to the positive electrode, and the input current flows out from the negative electrode and returns to the LCR digital bridge;
[0042] It also includes a data processing system, wherein the data output end of the LCR digital bridge is connected to the data input end of the data processing system, and the data processing system stores a theoretical mathematical model for transmitting the measured resistivity to the data processing system for data calculation and analysis;
[0043] The data processing system also includes a display screen for displaying the fluid seepage conditions of the entire fractured rock mass after conversion into a visual image on the display screen.
[0044] This scheme arranges electrodes on the surface or deep inside the fractured rock mass, and uses the transmission path of the current in the rock mass and the resistivity change in the path to infer the fluid seepage situation. This scheme first needs to monitor the measured resistance value of the fractured rock mass sample and convert it into a resistivity tensor, then simulate and analyze it through a theoretical mathematical model to obtain a permeability tensor, and then after computer display, it can be converted into image data, so as to realize the visualization operation of fluid seepage in the fractured rock mass; this scheme combines the resistivity tensor with the three-dimensional fractured rock mass permeability tensor, and through the visualization image simulation, it can more accurately reflect the real seepage channel and path of the fractured rock mass, and can realize the automation of the visualization test of fractured rock mass seepage.
[0045] Preferably, the fractured rock sample is in the shape of a parallelepiped; specifically, the parallelepiped has six faces, every two opposite faces are parallel, and each face is a parallelogram, and the areas of the two opposite parallelograms are equal.
[0046] Preferably, the fractured rock sample is in the shape of a cube, and the positive electrode and the negative electrode are respectively attached to the surface of the fractured rock sample; the negative electrode includes three independent negative electrode sheets, namely a first negative electrode sheet, a second negative electrode sheet, and a third negative electrode sheet;
[0047] The first negative electrode sheet is located at the bottom of the fractured rock sample, the extension directions of the second and third negative electrode sheets are respectively perpendicular to the first negative electrode sheet, the third negative electrode sheet is located on the right side facing the second negative electrode sheet, and the extension directions of the second and third negative electrode sheets are perpendicular.
[0048] The positive electrode includes three independent positive electrode sheets, namely a first positive electrode sheet, a second positive electrode sheet, and a third positive electrode sheet, and the first positive electrode sheet, the second positive electrode sheet, and the third positive electrode sheet are respectively located on the opposite sides of the first negative electrode sheet, the second negative electrode sheet, and the third negative electrode sheet in a one-to-one correspondence;
[0049] A stress regulating device is installed on the side of the third negative electrode sheet away from the fractured rock sample, which is used to adjust the stress value of the fractured rock sample; a stress sensor is correspondingly installed on the second negative electrode sheet, which is used to monitor the stress value actually applied by the third negative electrode sheet to the fractured rock sample; this is used to ensure that the stress applied to the test reduces the error caused by the contact resistance as much as possible without destroying the structure of the fractured rock sample. The reason is that in the resistivity test process, contact resistivity, as the most important influencing factor of accuracy, often causes the measured data to be several orders of magnitude higher, which greatly affects the authenticity of the entire test. Therefore, installing a stress sensor and a stress regulating device can monitor the contact stress between the electrode sheet and the fractured rock sample in real time, and the stress regulating device can control the stress value, so that the resistivity data is closer to the actual value.
[0050] This solution can deal with the technical problem that since fractured rock masses usually have well-developed joints and their internal structures are relatively broken under the action of tectonic movements, there are certain difficulties in sample preparation and the expected size may not be achieved. It uses 6 independent electrode sheets that can be assembled and disassembled, which has considerable flexibility.
[0051] The present invention has the following beneficial effects: the present invention adopts a non-destructive detection method, which will not cause damage to the rock mass, while reducing the damage to the rock mass sample during the test experiment, and can more truly reflect the distribution of cracks inside the rock mass. The present invention can realize real-time monitoring of the seepage of the fluid inside the fractured rock mass, and intuitively display it through images in a visual way, so that researchers can obtain the seepage information inside the fractured rock mass in time, which is helpful to more clearly study the internal damage mechanism of the fractured rock mass caused by seepage, and can realize comprehensive observation and analysis of the seepage of the fluid inside the fractured rock mass. Moreover, since the data can be transmitted in real time, it can also realize real-time monitoring and feedback of the fluid seepage process, and can grasp the dynamic changes of the fractured rock mass in time. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] In order to make the purpose, technical solution and advantages of the invention more clear, the present invention will be further described in detail below with reference to the accompanying drawings, in which:
[0053] Figure 1 Schematic diagram of the structure of a resistivity-based fractured rock fluid seepage visualization device in an embodiment of the present invention.
[0054] Figure 2 Schematic diagram of the installation positions of various electrodes and fractured rock samples in an embodiment of the present invention.
[0055] Figure 3 Schematic diagram of the connection structure of each electrode in an embodiment of the present invention.
[0056] Figure 4 Schematic diagram of the installation position of the stress sensor in an embodiment of the present invention.
[0057] Explanation of the accompanying reference numerals: 101, first positive electrode sheet; 102, second positive electrode sheet; 103, third positive electrode sheet; 104, first negative electrode sheet; 105, second negative electrode sheet; 106, third negative electrode sheet; 107, stress adjustment device; 108, position adjustment member; 109, stress sensor; 2, data processing system; 3, display; 4, LCR digital bridge; 5, fractured rock sample. DETAILED DESCRIPTION
[0058] To make the purpose, technical solution and advantages of the embodiments of the present invention more clear, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0059] It should be noted that similar numbers and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings. In the description of the present invention, it should be noted that the orientation or position relationship indicated by the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. is based on the orientation or position relationship shown in the drawings, or the orientation or position relationship in which the invention product is usually placed when used, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance. In addition, the terms "horizontal", "vertical", etc. do not mean that the components are absolutely horizontal or suspended, but can be slightly tilted. For example, "horizontal" only means that its direction is more horizontal than "vertical", and does not mean that the structure must be completely horizontal, but can be slightly tilted. In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0060] The present invention can be applied to the monitoring and analysis of internal fluid seepage in fractured rock masses, solving the technical problem that traditional rock mass visualization devices can usually only provide monitoring of the surface of fractured rock masses or local areas of the surface, and it is difficult to achieve comprehensive observation and analysis of internal fluid seepage in fractured rock masses.
[0061] In the first aspect, based on the technical problems solved above, the present invention discloses a method for visual monitoring of fluid seepage in fractured rock mass based on resistivity, comprising the following steps:
[0062] S1. Sampling from the fractured rock mass to obtain fractured rock mass samples;
[0063] S2, measuring the three-dimensional resistivity of the fractured rock mass sample to obtain the three-dimensional fractured rock mass resistivity tensor;
[0064] S3, constructing a theoretical mathematical model of the entire fractured rock mass, and converting the three-dimensional fractured rock mass resistivity tensor obtained in step S2 into a three-dimensional fractured rock mass permeability tensor;
[0065] S4, simulating the fluid seepage condition of the entire fractured rock mass in a theoretical mathematical model using the three-dimensional fractured rock mass resistivity tensor obtained in step S2 and the three-dimensional fractured rock mass permeability tensor obtained in step S3, and converting them into a visual image.
[0066] The basic principle used by the visualization monitoring method of the present invention is that the resistivity characteristics of fractured rock mass are sensitive to fluid seepage. In fractured rock mass, fluid seepage will change the resistivity distribution in the fractures. By using this characteristic, the fluid migration in the fractured rock mass can be indirectly monitored and visualized by measuring the resistivity change. Then, this scheme first needs to monitor the measured resistance value of the fractured rock mass sample and convert it into a resistivity tensor, and then simulate and analyze it through a theoretical mathematical model to obtain a permeability tensor, which can then be converted into image data after computer display, so as to realize the visualization operation of fluid seepage in fractured rock mass; this scheme combines the resistivity tensor with the three-dimensional fractured rock mass permeability tensor, and can more accurately reflect the real seepage channel and path of the fractured rock mass through visualized image simulation, so as to realize the automation of fractured rock mass seepage visualization test.
[0067] This program will also combine mathematical models and computer simulation technology to achieve quantitative analysis and visualization of fluid seepage in fractured rock masses. Through model establishment and simulation calculation, the fluid migration path and seepage velocity in fractured rock masses can be predicted more accurately. Based on real-time resistivity data, mathematical models are used to convert resistivity into a visualized seepage path, thereby providing researchers with an effective tool to monitor and analyze fluid migration in fractured rock masses, providing important technical support for geological engineering research on fluid migration and seepage damage in fractured rock masses.
[0068] Preferably, in step S2, the three-dimensional resistivity of the fractured rock sample is measured by the following method:
[0069] S2.1. Install multiple positive electrodes and multiple negative electrodes on the surface of the fractured rock sample, each positive electrode corresponds to a negative electrode, and connect each positive electrode and each negative electrode to the current output terminal and current input terminal of the LCR digital bridge respectively;
[0070] S2.2. Power on the LCR digital bridge, use the LCR digital bridge to measure the real-time resistance value of the fractured rock sample from multiple directions, and convert the real-time resistance value into three-dimensional fractured rock resistivity.
[0071] Preferably, in step S2.1, each of the positive electrodes and each of the negative electrodes are flexible electrodes, and each of the positive electrodes and each of the negative electrodes are respectively installed with a position adjustment member for adjusting the position of each of the positive electrodes and each of the negative electrodes on the surface of the fractured rock sample, so that each of the positive electrodes and each of the negative electrodes are enclosed to form an internal space, and the fractured rock sample can be enclosed in the internal space.
[0072] Preferably, in step S2.1, a stress sensor and a stress regulating device are respectively provided on two adjacent negative electrodes, and the stress sensor can sense the stress magnitude of the negative electrode on the fractured rock sample;
[0073] In step S2.2, after the LCR digital bridge is powered on, first observe whether the resistivity value on the LCR digital bridge is within a reasonable range, where the reasonable range refers to the resistivity value corresponding to when the stress value applied by the electrode to the surface of the fractured rock sample is ≤1 kPa;
[0074] If it is not within the reasonable range, the error caused by the contact resistivity is too large. At this time, the stress adjustment device should be adjusted so that the stress value of the electrode on the surface of the fractured rock sample is ≤1kPa to reduce the error caused by the contact resistivity.
[0075] Preferably, in step S2.2, the stress value applied by the electrode to the surface of the fractured rock sample is 1 kPa, at which time the influence of the contact resistivity can be minimized.
[0076] Preferably, in step S2.2, the seepage of the three-dimensional fractures of the fractured rock sample is considered, and the center point of the fractured rock sample is taken as the coordinate origin O, and a z coordinate system of the fractured rock fluid seepage visualization monitoring method based on resistivity is established. The coordinate axes in the coordinate system are perpendicular to each other, so the data in six different directions can be collected by combining three positive electrodes and three negative electrodes, which are ρ xx , xy , xz , yx , yy , yz , zx , zy , zz, these six resistivity data together constitute the resistivity tensor ρ ij , where i∈{x,y,z}, j∈{x,y,z}, the three-dimensional fractured rock resistivity tensor ρ ij It is expressed as:
[0077]
[0078] Specifically, in step S3, when constructing the theoretical mathematical model of the entire fractured rock mass, the three-dimensional fracture is first regarded as a disc-shaped structure with a certain thickness, and then on this basis, the theoretical mathematical model of the entire fractured rock mass is constructed.
[0079] In step S3, the three-dimensional fractured rock mass resistivity tensor obtained in step S2.2 is converted into a three-dimensional fractured rock mass permeability tensor using the following method:
[0080] Considering that the connectivity between fractures will affect the actual permeability tensor, thus leading to the inaccuracy of the visualization image, a fracture connectivity correction coefficient f is proposed to provide data correction for the conversion between the resistivity tensor and the permeability tensor, so as to eliminate the inaccuracy of the visualization image caused by the influence of the connectivity between fractures on the calculated value of the permeability tensor. The calculation formula of the fracture connectivity correction coefficient f is given below:
[0081]
[0082] In formula (2), τ represents the average number of intersections of each crack; τ c represents the permeation threshold; β represents the crack shape factor; where, according to the assumptions of this theoretical mathematical model, when the three-dimensional crack shape is compared to a disk, τ c Take 2.41 and β as 0.18.
[0083] Then the resistivity tensor ρ ij With the permeability tensor k ij Establish a calculation relationship, the calculation formula is as follows:
[0084]
[0085] In formula (3), H represents the correction coefficient of the crack resistivity concentration tensor, f is the fracture connectivity coefficient, and the calculation formula has been given above; δ ij is the Kronecker function; η is the fracture permeability tensor correction coefficient, A is the shape factor of the crack. In this invention, the crack is regarded as a disk with a certain thickness, so π2 is taken; ρ ij is the resistivity tensor of fractured rock mass.
[0086] Then, for the z coordinate system of the established resistivity-based fractured rock fluid seepage visualization monitoring method, the three-dimensional fractured rock permeability tensor can be expressed as:
[0087]
[0088] In formula (4), k ij is the permeability tensor of three-dimensional fractured rock mass, where i∈{x,y,z}, j∈{x,y,z}.
[0089] Preferably, in step S4, the visualization image is a three-dimensional visualization model, which is used to display the spatial distribution and connectivity of cracks inside the rock mass, and the spatial variation of permeability, and can also display multi-level permeability distribution by adjusting the transparency of different rock layers or cracks;
[0090] Alternatively, the visualization image is a color-coded image, which is used to represent different components of the permeability tensor by different colors, and to reflect the magnitude or change trend of the permeability by using the depth or gradient of the colors;
[0091] Or, the visual image is a flow diagram, which is used to show the potential flow path of the fluid in the rock mass, using arrows or streamlines to indicate the direction and speed of the fluid flow;
[0092] Or, the visualization image is a fracture network diagram, which is used to highlight and represent the fracture network through different visual elements, including the width, length and aperture of the fractures, and to provide quantitative information on parameters such as fracture density, fracture directionality, and permeability anisotropy;
[0093] Or, the visualization image is a contour map, which is used to represent the equal distribution of permeability in the rock mass through contour lines (such as isopreservability lines);
[0094] Or, the visualization image is an interactive view for rotating, zooming or slicing the three-dimensional model through interactive tools to view the permeability distribution from different angles and depths;
[0095] Alternatively, the visualization image is a dynamic simulation diagram, which is used to display the dynamic changes of the seepage process according to the changes in time.
[0096] Specifically, the present invention also provides the resistivity tensor ρ ij With the permeability tensor k ij Theoretical derivation was carried out to facilitate comparison and verification of measured values and converted values in practical applications.
[0097] (1) Resistivity tensor ρ ij Theoretical calculations
[0098] In formula (1), the resistivity of three-dimensional fractured rock mass is calculated using the improved asymmetric self-consistent theory of rock mass resistivity (ASC), and the resistivity tensor ρ is ij The calculation formula is as follows:
[0099]
[0100] In formula (5), ρ ij is the resistivity tensor of fractured rock mass; σ ij is the conductivity tensor of fractured rock mass; σ m is the matrix conductivity of fractured rock mass.
[0101] Among them, the conductivity tensor of fractured rock mass σ ij The expression is:
[0102]
[0103] In formula (6), δ ij is the Kronecker function; α, β, λ are all related parameters; ε is the density of cracks without cause; n ij represents the normal unit vector of the disk-shaped crack in the ij plane, and N is the number of conductive cracks.
[0104] Specifically, the Kronecker function is defined as follows: when i = j, δ ij =1; when i≠j, δ ij =0. In tensor analysis, the Kronecker function can be used to represent the contraction of a tensor or the increase or decrease of an index, and can be used to simplify the expression of a tensor.
[0105] In formula (6), the solution equations and calculation formulas of the relevant parameters α, β, ε, and λ are as follows:
[0106]
[0107]
[0108] In formulas (7), (8), (9), and (10), ξ is the number of cracks per unit volume; r is the crack radius; σ f is the saturated fracture conductivity; ω represents the aspect ratio of the fracture (fracture aperture / fracture diameter), σ m is the matrix conductivity of fractured rock mass. The values of parameters α and β can be determined by solving equations (7) and (8). The values of ε and λ are calculated by formulas (9) and (10).
[0109] Considering that the presence of fillings in the cracks of the fractured rock mass will affect the permeability and hydraulic properties of the rock mass, it is easy to have abnormal values of the crack resistivity, which makes it impossible to truly reflect the internal seepage path. At this time, the crack is a resistive crack and may be mistaken for not being a seepage path, thus affecting the presentation of the correct seepage image. Therefore, it is also necessary to calculate the accurate resistivity value through the following formula to eliminate the error:
[0110] The calculation formula of resistive crack conductivity is:
[0111]
[0112] In formula (11), δ ij is the Kronecker function; ρ ij is the resistivity tensor of fractured rock mass; σ ij is the conductivity tensor of fractured rock mass; σ m is the matrix conductivity of fractured rock mass; δ ij is the Kronecker function; β and λ are related parameters; ε is the density of causal cracks, where the expressions of β, λ, and ε are shown in equations (8), (9), and (10).
[0113] The resistive crack conductivity Substituting the resistivity tensor ρ ij The resistivity is calculated in the calculation formula.
[0114] (1) Permeability tensor k ij Theoretical calculation:
[0115] Without considering the connectivity between fractures, the permeability tensor k ij Calculate according to the following formula:
[0116]
[0117] In formulas (12) and (13), k ij represents the permeability tensor; M ij represents the basic crack tensor; V e represents the unit volume; D represents the crack diameter; b represents the crack aperture; n i represents the normal unit vector of the disk-shaped crack.
[0118] Among them, it is used to calculate the basic crack tensor M ij The various parameters of can be obtained through the theoretical mathematical model, which includes the geometric model and distribution characteristics of the crack, and can derive the crack tensor M through the theory of mathematics and mechanics. ij In addition, numerical simulation methods, such as finite element analysis (FEA) or discrete element method (DEM), can also be used to simulate the distribution of cracks and the influence of cracks on the properties of the rock mass, thereby obtaining the crack tensor Mij .
[0119] Considering that the connectivity between fractures will affect the actual permeability tensor, thus leading to the inaccuracy of the visualization image, the fracture connectivity correction coefficient f is proposed to correct the permeability tensor. The calculation formula of the corrected permeability tensor is as follows:
[0120]
[0121] In formula (14), k i ' j represents the corrected permeability tensor; f represents the fracture connectivity correction coefficient; M ij represents the basic crack tensor; δ ij is the Kronecker function, and N is the number of conductive cracks.
[0122] Then the resistivity tensor ρ ij With the permeability tensor k ij A calculation relationship is established, such as the relationship shown in the above formula (3).
[0123] The resistivity-based visualization monitoring method for fluid seepage in fractured rock mass disclosed in the present invention has the following technical effects:
[0124] 1. Traditional fractured rock mass seepage detection methods usually require destructive sampling, which is complex, time-consuming and costly. The present invention adopts a non-destructive detection method, which will not damage the rock mass, and at the same time reduces the damage to the rock mass sample during the test experiment, and can more truly reflect the distribution of fractures inside the rock mass.
[0125] 2. This visualization monitoring method can realize real-time monitoring of the seepage of fluid inside the fractured rock mass, and intuitively display it through images in a visualized way, so that researchers can obtain the seepage information inside the fractured rock mass in time, which is helpful to more clearly study the internal damage mechanism of the fractured rock mass caused by seepage.
[0126] 3. Compared with traditional destructive core sampling and expensive laboratory testing methods, this visual monitoring method has higher detection efficiency and lower cost, can save time and labor costs, improve work efficiency, and can provide more effective technical means and data support for fractured rock seepage research and engineering applications.
[0127] 4. The resistivity-based method can be used to observe the fluid seepage at different locations inside the fractured rock mass in a three-dimensional manner, so as to have a more comprehensive understanding of the seepage distribution and characteristics of the fractured rock mass. And through resistivity measurement, the permeability, seepage rate and seepage path of the fluid inside the fractured rock mass can be quantitatively analyzed, providing quantitative data support for engineering construction and geological disaster prevention and control, which is helpful to scientifically and rationally formulate engineering plans and take corresponding disaster prevention measures.
[0128] In a second aspect, the present invention discloses a device for visualizing fluid seepage in a fractured rock mass based on resistivity, which is used to monitor a fractured rock mass sample using the method for visualizing fluid seepage in a fractured rock mass based on resistivity as described above, and includes a positive electrode and a negative electrode, wherein the positive electrode and the negative electrode are respectively attached to the surface or the inside of the fractured rock mass sample;
[0129] Also included is an LCR digital bridge, which is electrically connected to the positive electrode and the negative electrode respectively and can provide an input current to the positive electrode, and the input current flows out from the negative electrode and returns to the LCR digital bridge;
[0130] It also includes a data processing system, wherein the data output end of the LCR digital bridge is connected to the data input end of the data processing system, and the data processing system stores a theoretical mathematical model for transmitting the measured resistivity to the data processing system for data calculation and analysis;
[0131] The data processing system also includes a display screen for displaying the fluid seepage conditions of the entire fractured rock mass after conversion into a visual image on the display screen.
[0132] This scheme arranges electrodes on the surface or deep inside the fractured rock mass, and uses the transmission path of the current in the rock mass and the resistivity change in the path to infer the fluid seepage situation. This scheme first needs to monitor the measured resistance value of the fractured rock mass sample and convert it into a resistivity tensor, then simulate and analyze it through a theoretical mathematical model to obtain a permeability tensor, and then after computer display, it can be converted into image data, so as to realize the visualization operation of fluid seepage in the fractured rock mass; this scheme combines the resistivity tensor with the three-dimensional fractured rock mass permeability tensor, and through the visualization image simulation, it can more accurately reflect the real seepage channel and path of the fractured rock mass, and can realize the automation of the visualization test of fractured rock mass seepage.
[0133] Preferably, the fractured rock sample is in the shape of a parallelepiped; specifically, the parallelepiped has six faces, every two opposite faces are parallel, and each face is a parallelogram, and the areas of the two opposite parallelograms are equal.
[0134] Preferably, the fractured rock sample is a cube or a cuboid specimen. Specifically, the side length of the fractured rock sample ranges from 10 to 50 cm.
[0135] As a preference, see Figures 1 to 4 The fractured rock sample 5 is in the shape of a cube, and the positive electrode and the negative electrode are respectively attached to the surface of the fractured rock sample 5; the negative electrode includes three independent negative electrode sheets, namely a first negative electrode sheet 104, a second negative electrode sheet 105, and a third negative electrode sheet 106;
[0136] The first negative electrode sheet 104 is located at the bottom of the fractured rock sample 5, the extension directions of the second negative electrode sheet 105 and the third negative electrode sheet 106 are respectively perpendicular to the first negative electrode sheet 104, the third negative electrode sheet 106 is located in the right direction facing the second negative electrode sheet 105, and the extension directions of the second negative electrode sheet 105 and the third negative electrode sheet 106 are perpendicular.
[0137] The positive electrode includes three independent positive electrode sheets, namely a first positive electrode sheet 101, a second positive electrode sheet 102, and a third positive electrode sheet 103. The first positive electrode sheet 101, the second positive electrode sheet 102, and the third positive electrode sheet 103 are respectively located on the opposite sides of the first negative electrode sheet 104, the second negative electrode sheet 105, and the third negative electrode sheet 106 in a one-to-one correspondence;
[0138] A stress regulating device 107 is installed on the side of the third negative electrode sheet 106 facing away from the fractured rock sample 5, which is used to adjust the stress value on the fractured rock sample 5; a stress sensor 109 is correspondingly installed on the second negative electrode sheet 105, which is used to monitor the stress value actually applied by the third negative electrode sheet 106 to the fractured rock sample 5; this is used to ensure that the stress applied to the test reduces the error caused by the contact resistance as much as possible without destroying the structure of the fractured rock sample 5. The reason is that in the resistivity test process, contact resistivity, as the most important influencing factor of accuracy, often causes the measured data to be several orders of magnitude higher, which greatly affects the authenticity of the entire test. Therefore, installing the stress sensor 109 and the stress regulating device 107 can monitor the contact stress between the electrode sheet and the fractured rock sample 5 in real time, and the stress regulating device 107 can control the stress value, so that the resistivity data is closer to the actual value.
[0139] This solution can deal with the technical problem that since fractured rock masses usually have well-developed joints and their internal structures are relatively broken under the action of tectonic movements, there are certain difficulties in sample preparation and the expected size may not be achieved. It uses 6 independent electrode sheets that can be assembled and disassembled, which has considerable flexibility.
[0140] Specifically, the data output end of the stress sensor is connected to the data input end of the data processing system. After the data acquisition end of the stress sensor acquires the stress value, the stress value is transmitted to the display screen and displayed on the display screen, so that the operator can adjust the stress value conveniently.
[0141] Specifically, a connector is installed between each adjacent electrode, and the connector is detachable, so that each electrode sheet can be detached, and assembly, disassembly and carrying are convenient.
[0142] Specifically, each positive electrode sheet and each negative electrode sheet includes two layers, namely a conductive material layer and an insulating layer, wherein the conductive layer faces one side of the fractured rock sample.
[0143] Specifically, the stress sensor is a flexible contact stress sensor.
[0144] Specifically, when choosing electrode materials and stress sensors, for problems such as the rough and uneven surface of rock samples, materials with certain deformation ability and wear resistance should be selected. This can not only significantly reduce the contact resistivity error, but also improve the durability of the entire device.
[0145] Specifically, in terms of electrode materials, both the positive electrode and the negative electrode of the present invention are polyaniline-based flexible electrodes (FCC@PANI). The polyaniline-based flexible electrodes can be designed to be flexible and plastic by regulating the preparation method and material composition to adapt to the needs of different shapes and surfaces. The polyaniline-based flexible electrodes have good electrical conductivity, can achieve stable current transmission on a flexible substrate, maintain good electrochemical properties, and have good chemical stability. They can work stably for a long time under different environmental conditions, have certain corrosion resistance, and are suitable for applications in various corrosive media, etc.
[0146] The area ratio of the electrodes (C A ,F cm -2 ) and mass specific capacitance (C m ,F g -1 ) is an important indicator for evaluating capacitor performance, which can directly affect the storage energy and charge density of the capacitor. The calculation formula is as follows:
[0147]
[0148]
[0149] In equations (15) and (16), △V (V) is the voltage window to remove the voltage drop during the discharge process; s (cm 2 ) is the actual working area of the electrode; I(A) is the discharge current; ∫Vdt is the integrated area of the discharge curve; The square (absolute value) of the voltage window (V·V); m(g) is the mass of the active material.
[0150] The area energy density (E A , mWh cm-2) and power density (PA ,mW cm-2) can be calculated by the following formula:
[0151]
[0152] In formula (17) and formula (18), C de (F cm-2) is the area specific capacitance of the flexible electrode; △V (V) is the actual discharge voltage window; Δt (s) is the discharge time.
[0153] The flexible contact stress sensor of the present invention is made of polydimethylsiloxane as the base material. The total thickness of the flexible contact stress sensor made of polydimethylsiloxane (PDMS) as the base material is about 1.5mm, which is highly flexible. The flexible pressure sensor has excellent performance, a monitoring range of 0-1kPa, and a high sensitivity (0.34kPa -1 ), short response time (﹤200ms), strong stability and other advantages.
[0154] Sensitivity (S n ) is the ratio of the sensor's output change to the input change in steady state. The sensitivity of the pressure sensor means how fast the output signal changes under a unit pressure change, so that the pressure change can be detected and measured more accurately. Therefore, a high-sensitivity pressure sensor has higher measurement precision and accuracy. The sensitivity calculation formula is as follows:
[0155]
[0156] In equations (19) and (20), C0 is the initial capacitance; P is the pressure; ε0 is the vacuum dielectric constant; ε r is the relative dielectric constant of the medium between the plates, A is the area covered by the two parallel plates; d is the distance between the two parallel plates.
[0157] The resistivity-based fractured rock fluid seepage visualization device disclosed in the present invention has the following technical effects:
[0158] 1. The resistivity-based fractured rock fluid seepage visualization device can realize the above-mentioned fractured rock fluid seepage visualization method, can monitor the resistivity of fractured rock samples in real time, and convert the permeability, and can also realize timely image visualization processing. In the data processing system, the resistivity tensor is combined with the three-dimensional fractured rock permeability tensor by using the constructed theoretical mathematical model. Through the visualized image simulation, the real seepage channel and path of the fractured rock can be more accurately reflected, and the automation of fractured rock seepage visualization test can be realized.
[0159] 2. The resistivity-based fractured rock fluid seepage visualization device does not require destructive sampling of fractured rock samples. It has a simple process, easy operation, low cost, and can truly reflect the distribution of fractures inside the rock mass.
[0160] 3. The electrodes in the resistivity-based fractured rock fluid seepage visualization device are detachable, easy to assemble and carry.
[0161] In order to further illustrate the resistivity-based fractured rock fluid seepage visualization device and monitoring method of the present invention, the present invention discloses the following application embodiments.
[0162] See also Figures 1 to 4 The resistivity-based fractured rock fluid seepage visualization device used in this embodiment is used to monitor the fractured rock sample 5, and includes a positive electrode, a negative electrode and an LCR digital bridge 4, wherein the positive electrode and the negative electrode are respectively attached to the surface of the fractured rock sample 5; the positive electrode and the negative electrode are both flexible electrodes.
[0163] The shape of the fractured rock sample 5 in this embodiment is a cube.
[0164] See also Figure 2 The negative electrode includes three independent negative electrode sheets, namely a first negative electrode sheet 104, a second negative electrode sheet 105, and a third negative electrode sheet 106;
[0165] The first negative electrode sheet 104 is located at the bottom of the fractured rock sample 5, the extension directions of the second negative electrode sheet 105 and the third negative electrode sheet 106 are respectively perpendicular to the first negative electrode sheet 104, the third negative electrode sheet 106 is located in the right direction facing the second negative electrode sheet 105, and the extension directions of the second negative electrode sheet 105 and the third negative electrode sheet 106 are perpendicular.
[0166] The positive electrode includes three independent positive electrode sheets, namely a first positive electrode sheet 101, a second positive electrode sheet 102, and a third positive electrode sheet 103. The first positive electrode sheet 101, the second positive electrode sheet 102, and the third positive electrode sheet 103 are respectively located on the opposite sides of the first negative electrode sheet 104, the second negative electrode sheet 105, and the third negative electrode sheet 106.
[0167] Specifically, a connector is installed between each adjacent electrode, and the connector is detachable, so that each electrode sheet can be detached, and assembly, disassembly and carrying are convenient.
[0168] Specifically, each electrode sheet in this embodiment adopts a polyaniline-based flexible electrode (FCC@PANI), where FCC refers to a flexible conductive substrate and PANI refers to polyaniline, wherein polyaniline is a conductive polymer with a conjugated structure and has good conductive properties and chemical stability; the polyaniline-based flexible electrode means that polyaniline is compounded or coated on a flexible conductive substrate to form a composite conductive material with good flexibility, conductivity, chemical stability, plasticity and durability.
[0169] Specifically, each positive electrode sheet and each negative electrode sheet includes two layers, namely a conductive material layer and an insulating layer, wherein the conductive layer faces one side of the fractured rock sample.
[0170] See also Figure 3 and Figure 4 A stress regulating device 107 is installed on the side of the third negative electrode sheet 106 facing away from the fractured rock sample 5, which is used to adjust the stress value of the fractured rock sample 5; a stress sensor 109 is correspondingly installed on the second negative electrode sheet 105, which is used to monitor the stress value actually applied by the third negative electrode sheet 106 to the fractured rock sample 5; this is used to ensure that the stress applied during the test reduces the error caused by the contact resistance as little as possible without destroying the structure of the fractured rock sample 5.
[0171] It should be emphasized that the relative positions of the second negative electrode sheet and the third negative electrode sheet cannot be swapped, while the positions of the first positive electrode sheet 101 , the second positive electrode sheet 102 , the third positive electrode sheet 103 , and the first negative electrode sheet 104 , as well as the positive and negative electrode properties can be adjusted.
[0172] The stress sensor adopts a flexible contact stress sensor and is attached to the second negative electrode sheet. The flexible contact stress sensor made of polydimethylsiloxane (PDMS) as the substrate is preferred, which has extremely high flexibility and can be bent and stretched without breaking, so that the PDMS-based stress sensor can adapt to surfaces of various shapes and sizes; it also has good transparency, chemical stability, acid resistance, alkali resistance, organic solvent resistance, thermal stability, sensitivity, fast response, easy processing, and low cost.
[0173] See also Figure 1 and Figure 3Each positive electrode sheet and each negative electrode sheet is provided with a corresponding position adjustment member 108 and a connector, each connector is used to connect to the LCR digital bridge 4, each electrode sheet can adjust its own physical position and contact area with the fractured rock sample 5, and can conveniently deal with fractured rock samples 5 of different sizes; the LCR digital bridge 4 can provide input current to each positive electrode sheet respectively, and the input current flows out from each corresponding negative electrode sheet and returns to the LCR digital bridge 4.
[0174] See also Figure 1 Considering the anisotropy of fractures in fractured rock mass, the current is transferred from the positive electrode ( Figure 1 The top, back, and left side of the front view of the device flow in, and the samples pass through the inside of the device from ( Figure 1 The device is viewed from the bottom, front, and right side of the device.
[0175] See also Figure 1 The resistivity-based fractured rock fluid seepage visualization device further includes a data processing system 2, wherein the data output end of the LCR digital bridge 4 is connected to the data input end of the data processing system 2, and is used to transmit the measured resistivity to the data processing system 2 for data calculation and analysis;
[0176] Specifically, the data acquisition end of the stress sensor 109 is used to collect the stress value, and the data output end of the stress sensor 109 is connected to the data input end of the data processing system 2;
[0177] The data processing system 2 also includes a display screen, which can display the real-time stress value collected by the stress sensor 109 and the data results after data calculation and analysis on the display screen.
[0178] Specifically, the construction and monitoring process of the resistivity-based fractured rock fluid seepage visualization device of this embodiment includes the following steps:
[0179] D1. First, place the first negative electrode sheet on a stable place, and then fix the second negative electrode sheet with the stress sensor to the corresponding position on the fractured rock sample through the corresponding position adjusting member;
[0180] D2. Fix the electrode sheet with the stress adjustment device to the third negative electrode sheet facing the right side of the second negative electrode sheet through the position adjustment member. After assembly, align the vertex of the fractured rock sample close to the intersection of the second negative electrode sheet and the third negative electrode sheet with the intersection, and keep the position of the fractured rock sample unchanged;
[0181] D3. Subsequently, the positive electrode sheets are assembled according to the size of the fractured rock sample, and the positive electrode sheets and the negative electrode sheets are closely fitted to the surface of the fractured rock sample through their respective position adjustment parts, and the stress size regulator is preliminarily adjusted;
[0182] D4, connecting the LCR digital bridge to the connectors on each positive electrode sheet and each negative electrode sheet, so that the LCR digital bridge is powered on and the measured resistance value of the fractured rock sample is collected;
[0183] D5, transmitting the measured resistance value of the fractured rock sample obtained in step D4 to the data processing system, wherein a theoretical mathematical model of the fractured rock sample is pre-built in the data processing system, and data calculation and analysis can be performed through the theoretical mathematical model according to the measured resistance value of the fractured rock sample, and the measured resistance value of the fractured rock sample can be converted into multiple characterization parameters such as resistivity tensor and permeability tensor;
[0184] D6. After converting each characterization parameter into an image, transmit it to the display screen for visual display and realize visual monitoring.
[0185] Specifically, in step D4, after the LCR digital bridge is powered on, first observe whether the resistivity value on the LCR digital bridge is within a reasonable range. If the resistivity value is not within a reasonable range, it means that the error caused by the contact resistivity is too large. At this time, the error caused by the contact resistivity should be reduced by adjusting the stress regulator.
[0186] Specifically, the reasonable region range refers to the resistivity value corresponding to when the stress value generated by each positive electrode sheet and each negative electrode sheet on the surface of the fractured rock sample is ≤1 kPa, and preferably 1 kPa, at which time the influence of the contact resistivity can be minimized.
[0187] Specifically, in step D5, in the data processing system, it is necessary to construct a theoretical mathematical model of the fractured rock sample in advance, and the subsequent data calculation and analysis process and visual simulation are all performed on this theoretical mathematical model. In this embodiment, the three-dimensional fracture is regarded as a disc-shaped structure with a certain thickness, and the theoretical mathematical model is constructed based on this.
[0188] According to the theoretical mathematical model, the initial resistivity and initial permeability tensors of the fractured rock samples are first detected as a comparison benchmark for subsequent visualization. The subsequently measured resistivity and permeability tensors can be subtracted from the initial values to show the changing trends of resistivity and permeability.
[0189] In the specific implementation, the above calculation formulas are entered into the data processing system in advance through programming. The data processing system automatically matches the formula and calculates the corresponding parameters according to the input parameter values or the parameter values transmitted through the LCR digital bridge, and finally obtains the three-dimensional fractured rock mass permeability tensor k ij , and displayed on the display.
[0190] The monitoring principle of the resistivity-based fractured rock fluid seepage visualization device in this embodiment is as follows:
[0191] By monitoring the measured resistance value of the fractured rock sample and converting it into a real-time resistivity tensor, the permeability tensor is then calculated through mathematical conversion using the resistivity tensor and related geological models. This process does not require direct measurement of the permeability, but indirectly infers the permeability of the fluid through electrical properties. The rock matrix and the fracture can be distinguished according to the permeability in different directions. By combining and comparing the permeability values in different directions, the size of the fracture opening and the filling condition inside the fracture can be obtained. Finally, the permeability tensor obtained through software analysis and calculation can be converted into image data, and then the image data can be transmitted to the fractured rock seepage image display through a data transmission line to realize the visualization of the fractured rock fluid seepage.
[0192] This embodiment combines the resistivity tensor with the three-dimensional fractured rock permeability tensor, and can more accurately reflect the real seepage channels and paths of the fractured rock through visual image simulation, and can realize the automation of fractured rock seepage visualization testing. It is also equipped with a data collection system composed of an LCR digital bridge, a data processing system capable of data calculation and analysis, and a display screen capable of displaying results, which can greatly improve the accuracy and data image processing capabilities of the entire fractured rock seepage visualization device.
[0193] It is understood that the present invention is described by some embodiments, and those skilled in the art are aware that various changes or equivalent substitutions may be made to these features and embodiments without departing from the spirit and scope of the present invention. Under the teachings of the present invention, these features and embodiments may be modified to adapt to specific circumstances and materials without departing from the spirit and scope of the present invention. The embodiments described in the present invention are part of the embodiments of the present invention, rather than all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings herein may be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed herein, and all other embodiments obtained by ordinary technicians in the art without creative work based on the embodiments in the present invention belong to the scope of protection of the present invention.
Claims
1. A method for visual monitoring of fluid seepage in fractured rock mass based on resistivity, characterized in that: The following steps are involved: S1. Sampling from the fractured rock mass to obtain fractured rock mass samples; S2, measuring the three-dimensional resistivity of the fractured rock mass sample to obtain the three-dimensional fractured rock mass resistivity tensor; S3, constructing a theoretical mathematical model of the entire fractured rock mass, and converting the three-dimensional fractured rock mass resistivity tensor obtained in step S2 into a three-dimensional fractured rock mass permeability tensor; S4, simulating the fluid seepage condition of the entire fractured rock mass in a theoretical mathematical model using the three-dimensional fractured rock mass resistivity tensor obtained in step S2 and the three-dimensional fractured rock mass permeability tensor obtained in step S3, and converting them into a visual image.
2. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 1, characterized in that: In step S2, the three-dimensional resistivity of the fractured rock sample is measured using the following method: S2.
1. Install multiple positive electrodes and multiple negative electrodes on the surface of the fractured rock sample, each positive electrode corresponds to a negative electrode, and connect each positive electrode and each negative electrode to the current output terminal and current input terminal of the LCR digital bridge respectively; S2.
2. Power on the LCR digital bridge, use the LCR digital bridge to measure the real-time resistance value of the fractured rock sample from multiple directions, and convert the real-time resistance value into three-dimensional fractured rock resistivity.
3. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 2, characterized in that: In step S2.1, each of the positive electrodes and each of the negative electrodes are flexible electrodes, and each of the positive electrodes and each of the negative electrodes are respectively installed with a position adjustment member for adjusting the position of each of the positive electrodes and each of the negative electrodes on the surface of the fractured rock sample, so that each of the positive electrodes and each of the negative electrodes are enclosed to form an internal space, and the fractured rock sample can be enclosed in the internal space.
4. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 3 is characterized in that: In step S2.1, a stress sensor and a stress regulating device are respectively provided on two adjacent negative electrodes, and the stress sensor can sense the stress magnitude of the negative electrode on the fractured rock sample; In step S2.2, after the LCR digital bridge is powered on, first observe whether the resistivity value on the LCR digital bridge is within a reasonable range, where the reasonable range refers to the resistivity value corresponding to when the stress value applied by the electrode to the surface of the fractured rock sample is ≤1 kPa; If it is not within the reasonable range, the error caused by the contact resistivity is too large. At this time, the stress adjustment device should be adjusted so that the stress value of the electrode on the surface of the fractured rock sample is ≤1kPa to reduce the error caused by the contact resistivity.
5. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 4, characterized in that: In step S2.2, the stress value applied by the electrode to the surface of the fractured rock sample is 1 kPa, at which the influence of the contact resistivity can be minimized.
6. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 5, characterized in that: In step S2.2, the center point of the fractured rock sample is taken as the coordinate origin O, and a z coordinate system of the fractured rock fluid seepage visualization monitoring method based on resistivity is established. The coordinate axes in the coordinate system are perpendicular to each other, and the three-dimensional fractured rock resistivity tensor ρ ij It is expressed as: In the formula, i∈{x,y,z}, j∈{x,y,z}; In step S3, the resistivity tensor ρ of the three-dimensional fractured rock mass is ij and the permeability tensor k of three-dimensional fractured rock mass ij The relationship is: Where H is the correction coefficient of the crack resistivity concentration tensor, f is the crack connectivity coefficient; δ ij is the Kronecker function; η is the fracture permeability tensor correction coefficient, r is the crack radius, A is the crack shape factor, which is π2; ρ ij is the resistivity tensor of fractured rock mass; in, In the formula, τ represents the average number of intersections of each crack; τ c represents the permeation threshold; β represents the crack shape factor; Then, the permeability tensor k of three-dimensional fractured rock mass is ij It can be expressed as: In the formula, i∈{x,y,z}, j∈{x,y,z}.
7. The method for visual monitoring of fluid seepage in fractured rock mass based on resistivity according to claim 1, characterized in that: In step S4, the visualization image is one of a three-dimensional visualization model, a color coding map, a flow map, a fracture network map, a contour map, an interactive view, and a dynamic simulation map.
8. A device for visualizing fluid seepage in fractured rock mass based on resistivity, which is used to monitor fractured rock mass samples using the method for visualizing fluid seepage in fractured rock mass based on resistivity as claimed in claim 2, and is characterized in that: It includes a positive electrode and a negative electrode, wherein the positive electrode and the negative electrode are respectively attached to the surface or the inside of the fractured rock sample; Also included is an LCR digital bridge, which is electrically connected to the positive electrode and the negative electrode respectively and can provide an input current to the positive electrode, and the input current flows out from the negative electrode and returns to the LCR digital bridge; It also includes a data processing system, wherein the data output end of the LCR digital bridge is connected to the data input end of the data processing system, and the data processing system stores a theoretical mathematical model for transmitting the measured resistivity to the data processing system for data calculation and analysis; The data processing system also includes a display screen for displaying the fluid seepage conditions of the entire fractured rock mass after conversion into a visual image on the display screen.
9. The resistivity-based fractured rock fluid seepage visualization device according to claim 8, characterized in that: The fractured rock mass sample is in the shape of a parallelepiped.
10. The resistivity-based fractured rock fluid seepage visualization device according to claim 9, characterized in that: The fractured rock sample is in the shape of a cube, and the positive electrode and the negative electrode are respectively attached to the surface of the fractured rock sample; the negative electrode includes three independent negative electrode sheets, namely a first negative electrode sheet, a second negative electrode sheet, and a third negative electrode sheet; The first negative electrode sheet is located at the bottom of the fractured rock sample, the extension directions of the second and third negative electrode sheets are respectively perpendicular to the first negative electrode sheet, the third negative electrode sheet is located on the right side facing the second negative electrode sheet, and the extension directions of the second and third negative electrode sheets are perpendicular. The positive electrode includes three independent positive electrode sheets, namely a first positive electrode sheet, a second positive electrode sheet, and a third positive electrode sheet, and the first positive electrode sheet, the second positive electrode sheet, and the third positive electrode sheet are respectively located on the opposite sides of the first negative electrode sheet, the second negative electrode sheet, and the third negative electrode sheet in a one-to-one correspondence; A stress adjustment device is installed on the side of the third negative electrode sheet facing away from the fractured rock sample, which is used to adjust the stress value of the fractured rock sample; a stress sensor is correspondingly installed on the second negative electrode sheet, which is used to monitor the stress value actually applied by the third negative electrode sheet to the fractured rock sample.
Citation Information
Cited By
Layer fracture dynamic monitoring method and system based on three-dimensional resistivity imaging
CN120652554A
Shale reservoir artificial fracture relative permeability testing method based on resistivity
CN121933416A
A method for testing relative permeability of artificial fractures in shale reservoirs based on resistivity
CN121933416B