Method for exploring seepage characteristics of EICP solidified sandy soil
Through the long sand column model device and various analysis methods, the seepage characteristics and slurry diffusion rules of EICP solidified sand are studied, which solves the deficiencies in the current research on the seepage characteristics and slurry diffusion rules of EICP solidified sand and provides detailed information. The data supports the application of EICP technology.
Patent Information
- Application Number
- CN202410998121.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-18
AI Technical Summary
It is difficult to study the seepage characteristics and slurry diffusion rules of EICP-solidified sand with existing technology, especially the changing rules of ion concentration, calcium carbonate content, and pH value along the seepage path during the EICP mineralization reaction, and the real-time monitoring and analysis capabilities are limited.
Using a long sand column model device combined with conductivity method, EDTA titration method and UV spectrophotometer, the urease activity, pH value, calcium ion concentration, and ammonium ion concentration at different positions and reaction times were measured to indirectly study the EICP solidified sand. The seepage characteristics and slurry diffusion of the soil were measured, and the calcium carbonate content, permeability coefficient and porosity were measured.
It achieved in-depth research on the seepage characteristics and slurry diffusion rules of EICP solidified sand, provided detailed data at different locations and reaction times, and improved the understanding and application prospects of EICP technology.
Smart Images

Figure CN118794858A_ABST
Abstract
Description
Technical field:
[0001] The invention belongs to the interdisciplinary scientific and technical field of microorganisms and civil engineering, and specifically relates to a method for preparing an EICP solution and a method for exploring the seepage characteristics of EICP-solidified sand. Background technology:
[0002] Enzyme-induced calcium carbonate precipitation (EICP) technology can cement loose soil into stone with a certain strength. It has broad application prospects in the reinforcement of poor soil due to its environmental friendliness, simple reaction mechanism and reactants, and controllable process. EICP soil solidification tests usually adopt a cyclic grouting method, that is, the bacterial solution and cementing liquid are circulated into the soil to induce calcium carbonate to precipitate and continue to grow between soil particles. The generated calcium carbonate can not only fill the soil pores, but also act as a "bridge" to connect loose minerals together under the premise of large-volume calcium carbonate crystals cemented with two or more soil particles.
[0003] However, there are currently few experimental studies on the seepage characteristics of EICP-solidified sand, and there are few studies on the changing laws of ion concentration, calcium carbonate content, pH value, and calcium carbonate content along the seepage path during the EICP mineralization reaction. In addition, the real-time monitoring and accurate analysis capabilities of the seepage path and slurry diffusion are limited. In order to better promote EICP technology to actual projects, it is necessary to study the seepage characteristics and slurry diffusion laws of EICP-solidified sand.
[0004] At present, a Chinese patent "A device for visually simulating and measuring the seepage characteristics of sand using tracer image velocimetry technology" has been retrieved, with publication number CN116380747A, which includes a computer, a CCD camera and an injection pump. The device also includes a porous medium component, which is made of a transparent material; the porous medium component includes two flat plates, which are arranged in parallel along the vertical direction; a number of glass columns are arranged between the two flat plates, and the two ends of the axial direction of each glass column are fixedly connected to the two flat plates respectively; a glass panel for sealing the four sides of the two flat plates is arranged between the two flat plates, and the glass panel is fixed to the two flat plates, and a test cavity is reserved between the two flat plates; a liquid inlet pipe and a liquid outlet pipe are fixed on the two opposite glass panels, respectively, and the liquid inlet pipe and the liquid outlet pipe are both connected to the test cavity, and the liquid inlet pipe is connected to the injection pump. Although the device can replace sand for permeability test and improve visualization ability, it is impossible to conduct experimental research on the seepage characteristics of EICP-solidified sand, and it is impossible to study the changing law of ion concentration, urease activity, pH value, and calcium carbonate content along the seepage path during the EICP mineralization reaction. Summary of the invention:
[0005] In view of the above-mentioned problems, the purpose of the present invention is to propose a method that can systematically and deeply study the seepage characteristics and slurry diffusion laws of EICP-solidified sand. The method can measure the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the test liquid at different positions and different reaction times to indirectly reflect the seepage characteristics and slurry diffusion laws of EICP-solidified sand, and can also measure the calcium carbonate content, permeability coefficient and porosity index of the sample after solidification.
[0006] The method for exploring the seepage characteristics of EICP-solidified sand soil of the present invention is characterized by comprising the following steps:
[0007] Step S1: baking the soybeans in an oven at 40°C for 6 hours, crushing the soybeans with a grinder after they are completely dried, filtering with a 60-mesh sieve to obtain soybean powder, grinding and sieving the remaining coarse powder again, and storing the obtained soybean fine powder in a dry environment at 4°C for later use;
[0008] Step S2: weighing the required mass of soybean powder, adding it to 30% alcohol at a solid-liquid ratio of 1:10, and stirring it with a magnetic stirrer at a speed of 1000 rpm for not less than 30 minutes; after sufficient stirring, placing the solution in a refrigerator at 4°C for more than 12 hours to allow impurities in the liquid to fully precipitate;
[0009] Step S3: taking the supernatant of the solution after standing still and placing it in a refrigerated centrifuge, setting the ambient temperature to 4° C., centrifuging at 10,000 rpm for 10 min, and collecting the supernatant after centrifugation as the soybean urease solution;
[0010] Step S4: mixing a 1 mol / L calcium chloride solution and a 1 mol / L urea solution at a volume ratio of 1:1 to obtain a binder solution, and then mixing the above-obtained soybean urease solution with the binder solution at a volume ratio of 1:2 to obtain an EICP treatment solution;
[0011] Step S5: Pour the EICP treatment liquid into a long sand column model device to study the seepage characteristics of the EICP-solidified sand, wait for the EICP treatment liquid to react for a certain time (0, 6, 12, 24, 36 h), and measure the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the liquid at different positions in the long sand column model device (0, 10, 20, 30, 40, 50 mm);
[0012] Step S6: The activity of urease is determined by the conductivity method. The conductivity of the reaction system is increased by a large amount of urease-catalyzed hydrolysis of urea, thereby indirectly determining the activity of urease. 1 mL of the urease to be tested is added to 9 mL of 1.1 mol / L urea solution to start the reaction. The conductivity changes rapidly over time and gradually stabilizes after 20 minutes. Therefore, after 20 minutes of the reaction, the conductivity change value of the reaction solution within 1 minute is measured using a conductivity sensor, and the conductivity change value is converted into urease activity using the following formula:
[0013] S=11.11KC
[0014] In the formula, 11.11 means that every change of 1mS / min in conductivity corresponds to 11.11mM / min of urea hydrolysis; K represents the dilution factor, which is 10 in this test; C is the change in conductivity per minute;
[0015] Step S7: Calcium ion concentration is determined by EDTA titration. Prepare 100 mL of deionized water, add 0.2 g of calcium carboxylate indicator, take 0.5 mL of the solution to be tested after the reaction into the above 100 mL of deionized water and shake well, titrate with EDTA standard solution until the solution color changes to bright blue, which is the titration end point, record the volume of EDTA standard solution consumed at this time, and the concentration calculation formula is as follows:
[0016] C M (Ca 2+ )=00.1×V EDTA / 0.5
[0017] Where V EDTA is the volume of EDTA standard solution consumed;
[0018] Step S8: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value;
[0019] Step S9: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by using an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value. Determine the pH value of the liquid to be tested by using a pH meter;
[0020] Step S10: indirectly reacting the seepage characteristics and slurry diffusion of the EICP-solidified sand according to the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the liquid to be tested at different positions and different reaction times.
[0021] The long sand column model device includes a long cylindrical mold and a base threadedly connected to the lower part of the long cylindrical mold. The long cylindrical mold is a hollow cylinder with an external thread at the lower part. A plurality of holes are arranged in the length direction of the long cylindrical mold, and rubber plugs are arranged on the holes. The base is a short cylinder, and a countersunk hole threadedly connected to the external thread at the lower part of the long cylindrical mold is opened on its upper surface. A through hole is arranged below the countersunk hole, and both the countersunk hole and the through hole are provided with internal threads. A bolt is connected inside the through hole, and a through hole is arranged in the center of the bolt, and a plug is inserted into the through hole.
[0022] A rubber ring is arranged on the edge between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold.
[0023] A hard gasket and a soft gasket are arranged between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold, and a plurality of holes for filtering are arranged on the hard gasket and the soft gasket.
[0024] The diameter of the countersunk groove is 60mm, the diameter of the hard gasket is 48mm, the thickness is 5mm, the diameter of the hole is 3mm, the diameter of the soft gasket is 48mm, the thickness is 1mm, and the diameter of the hole is 1mm.
[0025] The invention explores a method for the seepage characteristics of EICP-solidified sand. In the experiment, transparent sand is used as a reinforcement object, purple pigment is added into a soybean urease extract, the seepage path of the slurry is observed, holes are set at different positions of a long cylindrical mold for collecting a liquid to be tested, and the method is used to analyze the change characteristics of urease activity, pH value, calcium ion concentration, ammonium ion concentration and calcium carbonate generation along the seepage direction at different positions (0, 10, 20, 30, 40, 50 mm) and different reaction times (0, 6, 12, 24, 36 h). The seepage characteristics of the EICP-solidified sand and the diffusion of the slurry are indirectly reflected according to the urease activity, pH value, calcium ion concentration and ammonium ion concentration of the liquid to be tested at different positions and different reaction times. The invention can also measure the calcium carbonate content, permeability coefficient, porosity and other indicators of the EICP solidified body at different positions to reflect its seepage characteristics. Description of the drawings:
[0026] The present invention is further described below in conjunction with the accompanying drawings;
[0027] Figure 1 This is an exploded view of the long sand column model device;
[0028] Figure 2 This is the front view of the PVC hard gasket.
[0029] In the figure: 1—long cylindrical mold, 2—PVC hard gasket, 3—base, 4—bolt, 5—plug, 6—rubber ring, 7—plastic soft gasket, 8—rubber plug. Specific implementation method:
[0030] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.
[0031] The method for exploring the seepage characteristics of EICP-solidified sand soil comprises the following steps:
[0032] Step S1: baking the soybeans in an oven at 40°C for 6 hours, crushing the soybeans with a grinder after they are completely dried, filtering with a 60-mesh sieve to obtain soybean powder, grinding and sieving the remaining coarse powder again, and storing the obtained soybean fine powder in a dry environment at 4°C for later use;
[0033] Step S2: weighing the required mass of soybean powder, adding it to 30% alcohol at a solid-liquid ratio of 1:10, and stirring it with a magnetic stirrer at a speed of 1000 rpm for not less than 30 minutes; after sufficient stirring, placing the solution in a refrigerator at 4°C for more than 12 hours to allow impurities in the liquid to fully precipitate;
[0034] Step S3: taking the supernatant of the solution after standing still and placing it in a refrigerated centrifuge, setting the ambient temperature to 4° C., centrifuging at 10,000 rpm for 10 min, and collecting the supernatant after centrifugation as the soybean urease solution;
[0035] Step S4: mixing a 1 mol / L calcium chloride solution and a 1 mol / L urea solution at a volume ratio of 1:1 to obtain a binder solution, and then mixing the above-obtained soybean urease solution with the binder solution at a volume ratio of 1:2 to obtain an EICP treatment solution;
[0036] Step S5: Pour the EICP treatment liquid into a long sand column model device to study the seepage characteristics of the EICP-solidified sand, wait for the EICP treatment liquid to react for a certain time (0, 6, 12, 24, 36 h), and measure the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the liquid at different positions in the long sand column model device (0, 10, 20, 30, 40, 50 mm);
[0037] Step S6: The activity of urease is determined by the conductivity method. The conductivity of the reaction system is increased by a large amount of urease-catalyzed hydrolysis of urea, thereby indirectly determining the activity of urease. 1 mL of the urease to be tested is added to 9 mL of 1.1 mol / L urea solution to start the reaction. The conductivity changes rapidly over time and gradually stabilizes after 20 minutes. Therefore, after 20 minutes of the reaction, the conductivity change value of the reaction solution within 1 minute is measured using a conductivity sensor, and the conductivity change value is converted into urease activity using the following formula:
[0038] S=11.11KC
[0039] In the formula, 11.11 means that every change of 1mS / min in conductivity corresponds to 11.11mM / min of urea hydrolysis; K represents the dilution factor, which is 10 in this test; C is the change in conductivity per minute;
[0040] Step S7: Calcium ion concentration is determined by EDTA titration. Prepare 100 mL of deionized water, add 0.2 g of calcium carboxylate indicator, take 0.5 mL of the solution to be tested after the reaction into the above 100 mL of deionized water and shake well, titrate with EDTA standard solution until the solution color changes to bright blue, which is the titration end point, record the volume of EDTA standard solution consumed at this time, and the concentration calculation formula is as follows:
[0041] C M (Ca 2+ )=00.1×V EDTA / 0.5
[0042] Where V EDTA is the volume of EDTA standard solution consumed;
[0043] Step S8: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value;
[0044] Step S9: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by using an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value, and use a pH meter to determine the pH value of the liquid to be tested;
[0045] Step S10: indirectly reacting the seepage characteristics and slurry diffusion of the EICP-solidified sand according to the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the liquid to be tested at different positions and different reaction times.
[0046] The long sand column model device comprises a long cylindrical mold 1 and a base 3 threadedly connected to the lower part of the long cylindrical mold 1. The long cylindrical mold 1 is a hollow cylinder with an external thread at the lower part. A plurality of holes are arranged in the length direction of the long cylindrical mold 1, and rubber plugs 8 are plugged in the holes. The base 3 is a short cylinder with a countersunk hole threadedly connected to the external thread at the lower part of the long cylindrical mold 1 on its upper surface. A through hole is arranged below the countersunk hole, and both the countersunk hole and the through hole are provided with internal threads. A bolt 4 is connected in the through hole, and a through hole is arranged at the center of the bolt 4, and a plug 5 is inserted into the through hole.
[0047] A rubber ring 6 is provided at the edge between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold.
[0048] A hard gasket 2 and a soft gasket 7 are arranged between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold, and a plurality of holes for filtering are arranged on the hard gasket 2 and the soft gasket 7.
[0049] The diameter of the countersunk groove is 60 mm, the diameter of the hard gasket 2 is 48 mm, the thickness is 5 mm, the hole diameter is 3 mm, the diameter of the soft gasket 7 is 48 mm, the thickness is 1 mm, and the hole diameter is 1 mm.
[0050] Specifically, the long cylindrical mold 1 is composed of a hollow cylinder made of PVC material, with an outer diameter of 60mm, an inner diameter of 50mm, a thickness of 5mm and a length of 500mm. A 10mm thread is set on the outer periphery of the bottom of the long sand column mold for connecting the lower base. Five holes of 3mm in size are opened on the long cylindrical mold, which are distributed at 0, 10, 20, 30, 40 and 50mm from the top of the column, and are used for liquid samples at different positions and different reaction times, so as to facilitate the study of the seepage characteristics and slurry diffusion law of EICP-solidified sand. A rubber stopper 8 is provided on the hole, so that when necessary, a needle of a syringe can be used to pass through the rubber stopper 8 to extract the EICP treatment liquid at the corresponding position.
[0051] Base 3: A short cylinder made of PVC material, with a height of 20 mm and an outer diameter of 70 mm. A countersunk hole with a diameter of 60 mm is opened on the upper surface of the short cylinder and a customized thread is provided to be threadedly connected with the thread on the outer periphery of the bottom of the long sand column mold 1. A through hole with a diameter of 8 mm is opened at the bottom of the countersunk hole and a customized thread is provided. The function of the base is to connect the long cylindrical mold 1 to prevent the EICP treatment liquid from leaking from the bottom.
[0052] Rubber ring 6: It is set at the edge between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold. When the base and the long cylindrical mold rotate, the rubber ring plays a role in increasing the sealing performance to prevent the slurry from leaking from the base and the long cylindrical mold during the subsequent grouting process.
[0053] Hard gasket 2: Made of PVC material, located at the bottom of the base countersunk groove, with a diameter of 48mm and a thickness of 5mm. It has several holes with a diameter of 3mm. Its main function is to prevent the unreinforced sand and soil from flowing out along the water flow when discharging the waste liquid, and to block the flow of sand and soil along the water flow, while facilitating the discharge of waste liquid from the bottom.
[0054] Soft gasket 7: Located below the hard gasket, it has a diameter of 48mm and a thickness of 1mm. It is provided with a number of holes with a diameter of 1mm. Its function is similar to that of the hard gasket. It prevents unreinforced sand and soil from flowing out along the water flow when discharging waste liquid, plays a role in blocking the flow of sand and soil along the water flow, and facilitates the discharge of waste liquid from the bottom.
[0055] Bolt 4: The upper part has a stud with a length of 10 mm and a diameter of 8 mm. The upper stud of the bolt is connected to the threaded hole at the lower part of the base. The center of the bolt has a through hole, which is combined with a plug to block the liquid outlet and control the discharge of slurry.
[0056] Plug 5: can be inserted into the through hole of bolt 4, used to block the EICP treatment liquid. When the EICP treatment liquid is grouted multiple times, the plug needs to be removed, and the waste liquid of the previous grouting is drained and then new EICP treatment liquid is poured in.
[0057] Rubber plug 8: used to seal the 3mm hole opened on the long cylindrical mold to prevent the slurry from flowing out of the hole.
[0058] One embodiment: The preparation process of the grouting liquid is as follows: the soybean seed coat powder that meets the requirements is mixed with clean water in a sedimentation barrel, and each 100g of soybean powder is mixed with 1L of distilled water containing 30% ethanol. The mixed solution is stirred at 800rpm for 30 minutes, and the mixed solution suspension is placed in a 4℃ refrigerator for 12 hours, centrifuged at 40000rpm for 25min, and the supernatant is the soybean urease solution. The cementing solution is composed of urea with a concentration of 1.0M and calcium chloride with a concentration of 0.75M, and is mainly used to provide Ca in the EICP process. 2+ and CO 3 2- (The EICP solution used for grouting is made of soybean urease solution and binder in a ratio of 1:1).
[0059] The experiment used transparent sand as the reinforcement object to facilitate the observation of the flow path of the fluid. Purple pigment was added to the soybean urease extract to observe its seepage path and explore the changing rules of the EICP mineralization reaction along the seepage path.
[0060] The reinforced object was set in a long sand column mold, and the grouting liquid was injected. The waste liquid was extracted through the holes on the cylindrical groove. The change characteristics of urease activity, pH value, calcium ion concentration, ammonium ion concentration and calcium carbonate production along the seepage direction at different positions (0, 10, 20, 30, 40, 50 mm) and different reaction times (0, 6, 12, 24, 36 h) were analyzed. A fitting formula along the seepage direction was established to study the seepage path and slurry diffusion during the EICP mineralization reaction.
[0061] The invention explores a method for the seepage characteristics of EICP-solidified sand. In the experiment, transparent sand is used as a reinforcement object, purple pigment is added into a soybean urease extract, the seepage path of the slurry is observed, holes are set at different positions of a long cylindrical mold for collecting a liquid to be tested, and the method is used to analyze the change characteristics of urease activity, pH value, calcium ion concentration, ammonium ion concentration and calcium carbonate generation along the seepage direction at different positions (0, 10, 20, 30, 40, 50 mm) and different reaction times (0, 6, 12, 24, 36 h). The seepage characteristics of the EICP-solidified sand and the diffusion of the slurry are indirectly reflected according to the urease activity, pH value, calcium ion concentration and ammonium ion concentration of the liquid to be tested at different positions and different reaction times. The invention can also measure the calcium carbonate content, permeability coefficient, porosity and other indicators of the EICP solidified body at different positions to reflect its seepage characteristics.
[0062] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the specific implementation methods of the present invention can still be modified or some technical features can be replaced by equivalents without departing from the spirit of the technical solution of the present invention, which should be included in the scope of the technical solution for protection of the present invention.
Claims
1. A method for exploring the seepage characteristics of EICP-solidified sand, characterized by: The following steps are involved: Step S1: baking the soybeans in an oven at 40°C for 6 hours, crushing the soybeans with a grinder after they are completely dried, filtering with a 60-mesh sieve to obtain soybean powder, grinding and sieving the remaining coarse powder again, and storing the obtained soybean fine powder in a dry environment at 4°C for later use; Step S2: weighing the required mass of soybean powder, adding it to 30% alcohol at a solid-liquid ratio of 1:10, and stirring it with a magnetic stirrer at a speed of 1000 rpm for not less than 30 minutes; after sufficient stirring, placing the solution in a refrigerator at 4°C for more than 12 hours to allow impurities in the liquid to fully precipitate; Step S3: taking the supernatant of the solution after standing still and placing it in a refrigerated centrifuge, setting the ambient temperature to 4° C., centrifuging at 10,000 rpm for 10 min, and collecting the supernatant after centrifugation as the soybean urease solution; Step S4: mixing a 1 mol / L calcium chloride solution and a 1 mol / L urea solution at a volume ratio of 1:1 to obtain a binder solution, and then mixing the above-obtained soybean urease solution with the binder solution at a volume ratio of 1:2 to obtain an EICP treatment solution; Step S5: pouring the EICP treatment liquid into a long sand column model device to study the seepage characteristics of the EICP-solidified sand, after the EICP treatment liquid reacts for a certain time (0, 6, 12, 24, 36 h), measuring the urease activity, pH value, calcium ion concentration and ammonium ion concentration of the liquid at different positions in the long sand column model device (0, 10, 20, 30, 40, 50 mm); Step S6: The activity of urease is determined by the conductivity method. The conductivity of the reaction system is increased by a large amount of urease-catalyzed hydrolysis of urea, thereby indirectly determining the activity of urease. 1 mL of the urease to be tested is added to 9 mL of 1.1 mol / L urea solution to start the reaction. The conductivity changes rapidly over time and gradually stabilizes after 20 minutes. Therefore, after 20 minutes of the reaction, the conductivity change value of the reaction solution within 1 minute is measured using a conductivity sensor, and the conductivity change value is converted into urease activity using the following formula: S=11.11KC In the formula, 11.11 means that every change of 1mS / min in conductivity corresponds to 11.11mM / min of urea hydrolysis; K represents the dilution factor, which is 10 in this test; C is the change in conductivity per minute; Step S7: Calcium ion concentration is determined by EDTA titration. Prepare 100 mL of deionized water, add 0.2 g of calcium carboxylate indicator, take 0.5 mL of the solution to be tested after the reaction into the above 100 mL of deionized water and shake well, titrate with EDTA standard solution until the solution color changes to bright blue, which is the titration end point, record the volume of EDTA standard solution consumed at this time, and the concentration calculation formula is as follows: C M (That 2+ )=00.1×V EDTA / 0.5 Where V EDTA is the volume of EDTA standard solution consumed; Step S8: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value; Step S9: Determine the concentration of ammonium ions by utilizing the characteristic that the concentration of ammonium ions reacts with Nessler's reagent in an alkaline environment to generate orange-yellow ammonium iodide, and determine the concentration of ammonium ions in the liquid to be tested by using an ultraviolet spectrophotometer. The higher the concentration of ammonium ions, the greater the absorbance value, and use a pH meter to determine the pH value of the liquid to be tested; Step S10: indirectly reacting the seepage characteristics and slurry diffusion of the EICP-solidified sand according to the urease activity, pH value, calcium ion concentration, and ammonium ion concentration of the liquid to be tested at different positions and different reaction times.
2. The method for exploring the seepage characteristics of EICP-solidified sand according to claim 1, characterized in that: The long sand column model device comprises a long cylindrical mold (1) and a base (3) threadedly connected to the lower part of the long cylindrical mold (1); the long cylindrical mold (1) is a hollow cylinder, the lower part of which has an external thread, and a plurality of holes are arranged in the length direction of the long cylindrical mold (1), and rubber plugs (8) are arranged on the holes; the base (3) is a short cylinder, and a countersunk hole threadedly connected to the external thread of the lower part of the long cylindrical mold (1) is opened on its upper surface, and a through hole is arranged below the countersunk hole, and both the countersunk hole and the through hole are provided with internal threads, and a bolt (4) is connected inside the through hole, and a through hole is arranged at the center of the bolt (4), and a plug (5) is inserted into the through hole.
3. The method for exploring the seepage characteristics of EICP-solidified sand according to claim 2, characterized in that: A rubber ring (6) is arranged at the edge between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold.
4. The method for exploring the seepage characteristics of EICP-solidified sand according to claim 3, characterized in that: A hard gasket (2) and a soft gasket (7) are arranged between the bottom of the countersunk groove of the base and the lower end surface of the long cylindrical mold, and a plurality of holes for filtering are arranged on the hard gasket (2) and the soft gasket (7).
5. The method for exploring the seepage characteristics of EICP-solidified sand according to claim 4, characterized in that: The diameter of the countersunk hole groove is 60mm, the diameter of the hard gasket (2) is 48mm, the thickness is 5mm, the hole diameter is 3mm, and the diameter of the soft gasket (7) is 48mm, the thickness is 1mm, and the hole diameter is 1mm.