SVM (Support Vector Machine) algorithm-based method for detecting void defect of pressure steel pipe of pumped storage power station
Through an intelligent identification model based on the SVM algorithm, finite element numerical simulation and elastic wave detection experiments are used to establish a void defect sample database, which solves the problem of low detection accuracy of pressure steel pipes in pumped storage power stations and achieves efficient and automatic void defect detection. Detection improves the safety of the water delivery system.
Patent Information
- Application Number
- CN202410770013.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-14
- Publication Date
- 2024-10-18
AI Technical Summary
In the existing technology, the voiding defect detection method of penstock pressure steel pipes in pumped storage power stations has low accuracy and low efficiency, and lacks a fast and effective non-destructive testing method, resulting in potential safety hazards under high internal water pressure.
Using an intelligent identification model based on the SVM algorithm, through finite element numerical simulation and elastic wave detection tests, a void defect sample database was established, the waveform characteristics were analyzed, and the machine learning model was trained to achieve automatic identification of void defects in pressure steel pipes.
It improves the accuracy and efficiency of detection, can quickly and automatically identify voiding defects in pressure steel pipes, and enhances the safety and stability of the water delivery system.
Smart Images

Figure CN118795036A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on an SVM algorithm. The method is mainly applicable to quickly detecting the quality of backfill concrete grouting between the steel pipe wall and the surrounding rock after the installation of the water supply pressure steel pipe is completed, so as to ensure the compactness of the concrete backfill and the construction quality of the pressure steel pipe. Background Art
[0002] Pumped storage power stations use the height difference between the upper and lower reservoirs to generate electricity. The greater the water head, the smaller the required storage capacity, which can greatly save the overall investment of the project. Therefore, the average height difference between the upper and lower reservoirs of many large pumped storage power stations that have been built and are under construction is more than 500m. Under such high internal water pressure, if the water transfer tunnel adopts ordinary reinforced concrete lining structure, it is very easy to crack, causing high-pressure water to enter the surrounding rock through the cracks, which poses a great threat to the stability of the surrounding rock. At the same time, it will also cause a large amount of water loss and affect the power generation efficiency of the power station. Therefore, high-strength pressure steel pipes with many advantages are widely used in large and medium-sized pumped storage power stations. On the one hand, the steel lining is an impermeable material that isolates the high water pressure from the surrounding rock, and there is no need to consider leakage. On the other hand, after the pressure steel pipe is installed, it is necessary to backfill concrete grouting between the steel pipe and the surrounding rock to form a close combination of "steel pipe-backfill concrete-external surrounding rock", which greatly enhances the joint bearing capacity of the pressure steel pipe and the surrounding rock. Existing research results and engineering practices have shown that when the backfill concrete is densely filled, the pressure steel pipe, backfill concrete and surrounding rock can work well together and bear the load together, and the surrounding rock has a large load sharing ratio. Even for relatively soft surrounding rock, as long as the steel lining, backfill concrete and surrounding rock are in good contact, the surrounding rock can also share a certain load.
[0003] During the backfill concrete construction process, due to the large cross-sectional size of the pressure steel pipe, the narrow working space between the steel pipe wall and the surrounding rock, the poor fluidity of the concrete itself, the obstruction of the stiffening ribs on the outside of the steel pipe and the difficulty in vibration, it is very easy to cause the backfill concrete to be loose. When a cavity appears between the outer wall of the steel pipe and the concrete or between the concrete and the surrounding rock, it will destroy the joint bearing state between the steel pipe-backfill concrete-surrounding rock. Under the action of high internal water pressure and pulsating pressure, stress concentration is prone to occur in the vacated part. If local deformation and buckling occur, it will bring great safety hazards to the safe and stable operation of the entire water supply system. Therefore, after the backfill concrete construction is completed, the filling quality must be tested to detect the vacated phenomenon in time, and backfill grouting reinforcement treatment must be carried out.
[0004] The thickness of the pressure steel pipe in the pumped storage is generally 30mm-40mm. With such a high steel plate thickness, it is very difficult to accurately detect the empty position under the steel plate. The traditional detection methods are manual knocking and elastic wave method. Manual knocking judges whether there is a hollowing out by the sound after hitting the steel plate. The detection accuracy is poor and basically relies on the experience and judgment of the inspector; the elastic wave method judges whether there is a hollowing out by analyzing the waveform and frequency, but the interpretation of the waveform is also overly dependent on the judgment of the technicians, and the detection accuracy is not high. At present, there is no fast and effective non-destructive detection method for the hollowing out of the pressure steel pipe of pumped storage. Therefore, based on the impact elastic wave method, numerical simulation and artificial intelligence algorithm, by establishing an intelligent recognition model of hollowing defects based on the SVM algorithm, studying an intelligent non-destructive detection technology for pressure steel pipe hollowing defects with fast detection efficiency, high accuracy, and automatic judgment is a technical problem that urgently needs to be solved in the construction of pumped storage pressure steel pipes. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on a SVM algorithm, so as to solve the problems of low accuracy and low detection efficiency of existing conventional detection methods.
[0006] To this end, the present invention adopts the following technical solutions:
[0007] A method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on a SVM algorithm comprises the following steps:
[0008] Step S1, hollow defect model test: a plurality of different hollow defects are preset to establish a hollow defect test model for a pressure steel pipe, and an elastic wave detection test is performed based on the model to obtain measured wave field data;
[0009] Step S2, simulation analysis and calculation of hollow defect: a calculation model under various hollow defect working conditions is established through a finite element numerical simulation platform, and the wave field changes of the impact elastic wave in the defect area and the corresponding dense area under different working conditions are calculated;
[0010] Step S3, establishing a void defect sample database: extracting waveform time history curves and spectrum curves of the above numerical simulation calculation results according to different defect types, and establishing a waveform database of defect samples under various working conditions and corresponding dense samples;
[0011] Step S4, wave field characteristic analysis and evaluation index establishment: Based on the established defect sample database, analyze the factors affecting the waveform characteristics, analyze various factors affecting the waveform characteristics such as different steel plate thicknesses, different defect sizes, and different distances from the earthquake source, clarify the change rules of the wave field characteristics under different defect models, and formulate sensitivity evaluation indicators;
[0012] Step S5, establishing an SVM defect intelligent recognition model: extracting feature vectors from the waveform data in the sample database, incorporating a machine learning SVM algorithm to train and analyze the sample data, establishing a mapping relationship between feature vectors and hollow defects, and forming an intelligent recognition model for hollow defects in pressure steel pipes;
[0013] Step S6, accuracy verification and algorithm optimization: normalize and denoise the defect detection data of the preset hollow defect model, and apply the above-established defect intelligent recognition model to perform defect recognition on the processed detection data. By verifying the accuracy of the prediction model and analyzing the causes of errors, the recognition model is further optimized to improve its accuracy in actual detection work.
[0014] Further, step S2 includes the following steps:
[0015] Step S201, establishing a geometric model for simulation analysis: according to the thickness, diameter, defect area and defect depth parameters of the pressure steel pipe in each test model, respectively establish a geometric model for numerical calculation;
[0016] Step S202, meshing the geometric model: determine the meshing size based on the relationship between wavelength, mesh density and calculation accuracy, and mesh the geometric model.
[0017] The grid size can be calculated as follows:
[0018]
[0019] Where l is the grid size, λ is the wavelength of the elastic wave;
[0020] Step S203, establishing boundary conditions: deriving and determining boundary parameters according to viscoelastic boundary condition calculation theory, where:
[0021] Normal boundary parameters: C BN =ρC P
[0022] Tangent boundary parameters: C BT =ρC S
[0023] In the formula, K BN ,K BT are the normal and tangential stiffness of the spring unit, E is the elastic modulus of the dielectric material, μ is the Poisson's ratio of the dielectric material, R is the distance from the wave source to the artificial boundary point, C BN , C BT is the damping coefficient of the boundary condition, ρ is the mass density of the medium, C P , C Sare the P-wave and S-wave velocities in dielectric materials, respectively;
[0024] Step S204, elastic wave excitation and iterative solution: setting the test waveform data of the impact hammer to determine the width of the elastic wave excitation pulse load, constructing the function of the excitation load in the numerical simulation calculation and performing iterative solution of the finite element elastic wave field;
[0025] Step S205, wave field comparison and parameter optimization: extract the elastic wave field results of the finite element simulation, compare and analyze them with the test waveform in step S1, adjust and optimize the simulation parameters according to the analysis results, and establish a corresponding relationship between the wave field characteristics of the theoretical signal and the measured signal;
[0026] Step S206, classify and establish analysis models: according to the optimization parameters of step S205, construct analysis models under various working conditions reflecting different defect sizes and steel plate thicknesses, and repeat the above simulation analysis process of S201 to S204.
[0027] Further, step S4 includes the following steps:
[0028] Step S401, source offset distance analysis: extract the waveform signals at different distances (5cm, 10cm, 15cm, 20cm, 25cm, 30cm) from the load excitation position, analyze the influence of the source offset distance on the waveform characteristics, and determine the optimal offset distance between the detector and the source during the detection process;
[0029] Step S402, steel plate thickness influence analysis: waveform characteristic analysis is performed on models of different steel plate thicknesses with the same defect size to determine the maximum steel plate thickness applicable to the detection method;
[0030] Step S403, defect size recognition capability analysis: waveform characteristic analysis is performed on models with the same steel plate thickness and different defect sizes to determine the minimum defect size that can be recognized by the detection method;
[0031] Step S404, waveform and spectrum comparison analysis: compare the waveform time history curve and spectrum curve of the defect area and the dense area, perform statistical analysis on the waveform amplitude, vibration duration, spectrum peak size and occurrence interval, summarize the similarities and differences between the two, and formulate sensitivity evaluation indicators.
[0032] Further, step S5 includes the following steps:
[0033] Step S501, feature vector extraction: according to the sensitivity evaluation index formulated in step S4, feature vectors of waveform curves and spectrum curves are extracted from the waveform data in the waveform database established in step S3;
[0034] Step S502, model training: Apply the SVM algorithm to train and analyze the extracted sample data, and analyze and select different kernel functions to establish a mapping relationship between the feature vector and the void defect, that is, by adjusting the values of w and b, solve the minimum ||w|| 2 Values, where:
[0035]
[0036] sty i (w T x i +b)≥+1,i=1,2,...n (5-2)
[0037] Where, w=(w1;w2;...;w d ) represents the normal vector of the hyperplane, which determines the direction of the hyperplane, b represents the displacement term, which determines the offset distance of the hyperplane, (x i ,y i ) is the coordinate position of any data point in the sample space;
[0038] Step S503, model training: optimizing the penalty coefficient C of the established SVM intelligent defect recognition model and the Gamma parameter of the RBF kernel function, and using the grid search function (GridSearchCV) method to adjust the parameters;
[0039] Step S504, verification and iteration: randomly select samples from the sample data set as the verification set, and perform multiple repeated tests to verify the accuracy and robustness of the model. If the accuracy does not meet the requirements, repeat steps S502 to S504 until the performance of the intelligent recognition model meets the requirements.
[0040] Furthermore, according to the method for detecting hollowing defects of pressure steel pipes in pumped-storage power stations based on the SVM algorithm according to claim 1, it is characterized in that, in actual engineering applications, step S6 allows repeated loop execution, and the accuracy and applicability of the intelligent defect recognition model are continuously improved by continuously expanding the sample data of the hollowing defect sample database and retraining the intelligent defect recognition model.
[0041] The beneficial effect of the above further scheme is: based on a rich defect sample database, an intelligent recognition model for hollowing defects in pressure steel pipes is established and optimized, so as to realize automatic recognition of hollowing defects in detection work. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] Figure 1 It is a flow chart of the method in the present invention.
[0043] Figure 2 This is a flow chart of the numerical simulation model test in the present invention.
[0044] Figure 3 A flow chart is established for the SVM intelligent recognition model in the present invention. DETAILED DESCRIPTION
[0045] In combination with specific embodiments and drawings, a method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm is described in detail below so that those skilled in the art can understand the present invention. However, it should be clear that the technical features of the present invention are not limited to this specific implementation case, and any changes or modifications made by those skilled in the relevant field within the scope of the present invention are all included in the protection scope of the present invention.
[0046] The present invention provides a method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm, and its flow chart is as follows: Figure 1 As shown, the specific steps include:
[0047] Step S1, hollow defect model test: a plurality of different hollow defects are preset to establish a hollow defect test model for a pressure steel pipe, and an elastic wave detection test is performed based on the model to obtain measured wave field data.
[0048] In this example, in order to construct various typical types of void defects in actual engineering, different defects with void areas of 10 cm×10 cm, 15 cm×15 cm, and 20 cm×20 cm were preset in the model test, and elastic wave data were collected after the detection area was divided into grids.
[0049] Step S2, hollow defect simulation analysis and calculation: a calculation model under various hollow defect working conditions is established through a finite element numerical simulation platform, and the wave field changes of the impact elastic wave in the defect area and the corresponding dense area under different working conditions are calculated.
[0050] In this step, the calculation flow chart of typical defect numerical simulation analysis is shown in Figure 2 , specifically including the following steps:
[0051] S201. Establishment of the geometric model for simulation analysis. According to the different parameters such as thickness, diameter, defect area, defect depth, etc. of the pressure steel pipe in the test model, the geometric model for numerical calculation is established. Figure 3 .
[0052] Step S201, establishing a geometric model for simulation analysis: according to the thickness, diameter, defect area and defect depth parameters of the pressure steel pipe in each test model, respectively establish a geometric model for numerical calculation;
[0053] Step S202, meshing the geometric model: determine the meshing size based on the relationship between wavelength, mesh density and calculation accuracy, and mesh the geometric model.
[0054] The grid size can be calculated as follows:
[0055]
[0056] Where l is the grid size, λ is the wavelength of the elastic wave;
[0057] Step S203, establishing boundary conditions: deriving and determining boundary parameters according to viscoelastic boundary condition calculation theory, where:
[0058] Normal boundary parameters: C BN =ρC P
[0059] Tangent boundary parameters: C BT =ρC S
[0060] In the formula, K BN ,K BT are the normal and tangential stiffness of the spring unit, E is the elastic modulus of the dielectric material, μ is the Poisson's ratio of the dielectric material, R is the distance from the wave source to the artificial boundary point, C BN , C BT is the damping coefficient of the boundary condition, ρ is the mass density of the medium, C P , C S are the P-wave and S-wave velocities in dielectric materials, respectively;
[0061] Step S204, elastic wave excitation and iterative solution: setting the test waveform data of the impact hammer to determine the width of the elastic wave excitation pulse load, constructing the function of the excitation load in the numerical simulation calculation and performing iterative solution of the finite element elastic wave field;
[0062] Step S205, wave field comparison and parameter optimization: extract the elastic wave field results of the finite element simulation, compare and analyze them with the test waveform in step S1, adjust and optimize the simulation parameters according to the analysis results, and establish a corresponding relationship between the wave field characteristics of the theoretical signal and the measured signal;
[0063] Step S206, classify and establish analysis models: according to the optimization parameters of step S205, construct analysis models under various working conditions reflecting different defect sizes and steel plate thicknesses, and repeat the above simulation analysis process of S201 to S204.
[0064] In this example, models of adequate-sized pressure steel pipes, backfill concrete layers and part of the surrounding rock are established to complete the construction of the geometric model. The elastic wave velocity is deduced based on the model material parameters, and the finite element mesh density is determined. By applying triangular impact loads to simulate the elastic wave field excited by the earthquake source, numerical simulation analysis of different defect conditions is achieved.
[0065] Step S3, establishing a void defect sample database: extracting waveform time history curves and spectrum curves of the above numerical simulation calculation results according to different defect types, and establishing a waveform database of defect samples under various working conditions and corresponding dense samples.
[0066] In this example, the node displacement and node velocity information at different positions above the defect are extracted according to the finite element node numbering, and the large number of extracted calculation results are numbered and labeled according to attribute information such as working condition type and extraction position to establish a defect sample database.
[0067] Step S4, wave field characteristic analysis and evaluation index establishment: Based on the established defect sample database, analyze the factors affecting the waveform characteristics, analyze various factors affecting the waveform characteristics such as different steel plate thicknesses, different defect sizes, and different distances from the earthquake source, clarify the change rules of the wave field characteristics under different defect models, and formulate sensitivity evaluation indicators.
[0068] In this step, the following steps are specifically included:
[0069] Step S401, source offset distance analysis: extract the waveform signals at different distances (5cm, 10cm, 15cm, 20cm, 25cm, 30cm) from the load excitation position, analyze the influence of the source offset distance on the waveform characteristics, and determine the optimal offset distance between the detector and the source during the detection process;
[0070] Step S402, steel plate thickness influence analysis: waveform characteristic analysis is performed on models of different steel plate thicknesses with the same defect size to determine the maximum steel plate thickness applicable to the detection method;
[0071] Step S403, defect size recognition capability analysis: waveform characteristic analysis is performed on models with the same steel plate thickness and different defect sizes to determine the minimum defect size that can be recognized by the detection method;
[0072] Step S404, waveform and spectrum comparison analysis: compare the waveform time history curve and spectrum curve of the defect area and the dense area, perform statistical analysis on the waveform amplitude, vibration duration, spectrum peak size and occurrence interval, summarize the similarities and differences between the two, and formulate sensitivity evaluation indicators.
[0073] In this example, by classifying and comparing the waveform data in the sample database, the influence of different factors on the wave field characteristics was clarified, and sensitivity evaluation indicators were proposed, laying the foundation for the establishment of the subsequent recognition model.
[0074] Step S5, establishing an SVM defect intelligent recognition model: extracting feature vectors from the waveform data in the sample database, incorporating a machine learning SVM algorithm to train and analyze the sample data, establishing a mapping relationship between feature vectors and hollow defects, and forming an intelligent recognition model for hollow defects in pressure steel pipes.
[0075] In this step, the SVM defect intelligent recognition model is established. Figure 3 , specifically including the following steps:
[0076] Step S501, feature vector extraction: according to the sensitivity evaluation index formulated in step S4, feature vectors of waveform curves and spectrum curves are extracted from the waveform data in the waveform database established in step S3;
[0077] Step S502, model training: applying the SVM algorithm to perform training analysis on the extracted sample data, and performing analysis and selection of different kernel functions to establish a mapping relationship between feature vectors and void defects;
[0078] Step S503, model training: optimizing the penalty coefficient C of the established SVM intelligent defect recognition model and the Gamma parameter of the RBF kernel function, and using the grid search function (GridSearchCV) method to adjust the parameters;
[0079] Step S504, verification and iteration: randomly select samples from the sample data set as the verification set, and perform multiple repeated tests to verify the accuracy and robustness of the model. If the accuracy does not meet the requirements, repeat steps S502 to S504 until the performance of the intelligent recognition model meets the requirements.
[0080] In this example, feature vectors are extracted from the waveform and spectrum data in the sample database to complete the coupling preparation of data dimensions before model training and form a feature vector data set. Secondly, 80% of the feature vector data set is randomly selected and input into the SVM intelligent recognition model to establish a mapping relationship, and the remaining 20% of the data is used as a validation set to verify the accuracy of the intelligent recognition model. If the accuracy does not meet the requirements, the above process is repeated until the performance of the intelligent recognition model meets the requirements.
[0081] Step S6, accuracy verification and algorithm optimization: normalize and denoise the defect detection data of the preset hollow defect model, and apply the above-established defect intelligent recognition model to perform defect recognition on the processed detection data. By verifying the accuracy of the prediction model and analyzing the causes of errors, the recognition model is further optimized to improve its accuracy in actual detection work.
[0082] In this example, the measured waveform data collected in the model test are normalized and feature vectors are extracted. Then, the established intelligent defect recognition model is used to identify defects in the measured waveform data, and the effectiveness of the model is verified based on the recognition results.
Claims
1. A method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on SVM algorithm, characterized in that: The following steps are involved: Step S1, hollow defect model test: a plurality of different hollow defects are preset to establish a hollow defect test model for a pressure steel pipe, and an elastic wave detection test is performed based on the model to obtain measured wave field data; Step S2, simulation analysis and calculation of hollow defect: a calculation model under various hollow defect working conditions is established through a finite element numerical simulation platform, and the wave field changes of the impact elastic wave in the defect area and the corresponding dense area under different working conditions are calculated; Step S3, establishing a void defect sample database: extracting waveform time history curves and spectrum curves of the above numerical simulation calculation results according to different defect types, and establishing a waveform database of defect samples under various working conditions and corresponding dense samples; Step S4, wave field characteristic analysis and evaluation index establishment: Based on the established defect sample database, analyze the factors affecting the waveform characteristics, analyze various factors affecting the waveform characteristics such as different steel plate thicknesses, different defect sizes, and different distances from the earthquake source, clarify the change rules of the wave field characteristics under different defect models, and formulate sensitivity evaluation indicators; Step S5, establishing an SVM defect intelligent recognition model: extracting feature vectors from the waveform data in the sample database, incorporating a machine learning SVM algorithm to train and analyze the sample data, establishing a mapping relationship between feature vectors and hollow defects, and forming an intelligent recognition model for hollow defects in pressure steel pipes; Step S6, accuracy verification and algorithm optimization: normalize and denoise the defect detection data of the preset hollow defect model, and apply the above-established defect intelligent recognition model to perform defect recognition on the processed detection data. By verifying the accuracy of the prediction model and analyzing the causes of errors, the recognition model is further optimized to improve its accuracy in actual detection work.
2. The method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm according to claim 1 is characterized in that: Step S2 includes the following steps: Step S201, establishing a geometric model for simulation analysis: according to the thickness, diameter, defect area and defect depth parameters of the pressure steel pipe in each test model, respectively establish a geometric model for numerical calculation; Step S202, meshing the geometric model: determine the meshing size based on the relationship between wavelength, mesh density and calculation accuracy, and mesh the geometric model. The grid size can be calculated as follows: Where l is the grid size, λ is the wavelength of the elastic wave; Step S203, establishing boundary conditions: deriving and determining boundary parameters according to viscoelastic boundary condition calculation theory, where: Normal boundary parameters: C BN =ρC P Tangent boundary parameters: C BT =ρC S In the formula, K BN ,K BT are the normal and tangential stiffness of the spring unit, E is the elastic modulus of the dielectric material, μ is the Poisson's ratio of the dielectric material, R is the distance from the wave source to the artificial boundary point, C BN , C BT is the damping coefficient of the boundary condition, ρ is the mass density of the medium, C p , C S are the P-wave and S-wave velocities in dielectric materials, respectively; Step S204, elastic wave excitation and iterative solution: setting the test waveform data of the impact hammer to determine the width of the elastic wave excitation pulse load, constructing the function of the excitation load in the numerical simulation calculation and performing iterative solution of the finite element elastic wave field; Step S205, wave field comparison and parameter optimization: extract the elastic wave field results of the finite element simulation, compare and analyze them with the test waveform in step S1, adjust and optimize the simulation parameters according to the analysis results, and establish a corresponding relationship between the wave field characteristics of the theoretical signal and the measured signal; Step S206, classify and establish analysis models: according to the optimization parameters of step S205, construct analysis models under various working conditions reflecting different defect sizes and steel plate thicknesses, and repeat the above simulation analysis process of S201 to S204.
3. The method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm according to claim 1 is characterized in that: Step S4 includes the following steps: Step S401, source offset distance analysis: extracting waveform signals at different distances from the load excitation position, analyzing the influence of the source offset distance on the waveform characteristics, and determining the optimal offset distance between the detector and the source during the detection process; Step S402, steel plate thickness influence analysis: waveform characteristic analysis is performed on models of different steel plate thicknesses with the same defect size to determine the maximum steel plate thickness applicable to the detection method; Step S403, defect size recognition capability analysis: waveform characteristic analysis is performed on models with the same steel plate thickness and different defect sizes to determine the minimum defect size that can be recognized by the detection method; Step S404, waveform and spectrum comparison analysis: compare the waveform time history curve and spectrum curve of the defect area and the dense area, perform statistical analysis on the waveform amplitude, vibration duration, spectrum peak size and occurrence interval, summarize the similarities and differences between the two, and formulate sensitivity evaluation indicators.
4. The method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm according to claim 1 is characterized in that: Step S5 includes the following steps: Step S501, feature vector extraction: according to the sensitivity evaluation index formulated in step S4, feature vectors of waveform curves and spectrum curves are extracted from the waveform data in the waveform database established in step S3; Step S502, model training: Apply the SVM algorithm to train and analyze the extracted sample data, and analyze and select different kernel functions to establish a mapping relationship between the feature vector and the void defect, that is, by adjusting the values of w and b, solve the minimum w 2 Values, where: s.t.y i (w T x i +b)≥+1,i=1,2,...n(5-2) Where, w=(w1;w2;...;w d ) represents the normal vector of the hyperplane, which determines the direction of the hyperplane, b represents the displacement term, which determines the offset distance of the hyperplane, (x i ,y i ) is the coordinate position of any data point in the sample space; Step S503, model training: optimizing the penalty coefficient C of the established SVM intelligent defect recognition model and the Gamma parameter of the RBF kernel function, and using the grid search function (GridSearchCV) method to adjust the parameters; Step S504, verification and iteration: randomly select samples from the sample data set as the verification set, and perform multiple repeated tests to verify the accuracy and robustness of the model. If the accuracy does not meet the requirements, repeat steps S502 to S504 until the performance of the intelligent recognition model meets the requirements.
5. The method for detecting hollowing defects of pressure steel pipes in pumped storage power stations based on the SVM algorithm according to claim 1 is characterized in that: In actual engineering applications, step S6 allows repeated loop execution, and the accuracy and applicability of the intelligent defect recognition model can be continuously improved by continuously expanding the sample data of the hollow defect sample database and retraining the intelligent defect recognition model.
Citation Information
Cited By
Physical modeling method for verifying steel shell concrete void detection mapping model