Method for stabilizing relative lateral position of two components
By arranging protrusions on the interface surface of the attached object and using pre-dried sintered materials, the problem of stability and shape matching of the attached object on the base component is solved, efficient fixation without alignment of the frame structure is achieved, and manufacturing complexity is reduced performance and risk of failure.
Patent Information
- Application Number
- CN202410428065.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-12
- Filing Date
- 2024-04-10
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-04-10
AI Technical Summary
The existing technology has problems such as poor stability, mismatched shapes, and complex alignment frame structures when fixing attached objects to base components, resulting in increased manufacturing time and cost, and the alignment frame structure is too complex in mass production. High risk of failure.
By providing stabilizing means, such as protrusions, on the interface surface of the attached object, protruding into the sintered layer to stabilize its lateral position, and using pre-dried sintered material and wire bonding structures during the curing step, ensuring that the attached object is in the correct position and Shape fixation.
No additional alignment frame structure is required to maintain the correct position of the attached object, reducing manufacturing complexity and energy consumption, improving the stability of the attached object and the reliability of the curing process, and reducing the risk of failure.
Smart Images

Figure CN118800664A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for sintering an interface surface of an attachment object (eg a semiconductor power module) to an attachment side of a base component, such as to a heat dissipator, a heat sink and / or a cooler (part for a cooler). Background Art
[0002] The method is applicable to the manufacture of a power module assembly. Such a power module assembly (hereinafter referred to as an "assembly") may include several attached objects fixed to a base component. Typically, the assembly is configured to form a part of an electrical circuit, such as a powertrain circuit of an electric vehicle. Nowadays, the demand for electric vehicles (especially electric vehicles) is growing rapidly.
[0003] The power module, and in particular the objects to which it is attached, is adapted to exhibit the required electrical functions. At least some of the attached objects may be semiconductor power modules. These may include insulated gate bipolar transistors (IGBTs) and / or metal oxide semiconductor field effect transistors (MOSFETs).
[0004] During the operation of the circuit, the attached object generates heat, in particular due to the current. In order to avoid overheating and damage to the attached object, it is fixed to the base component. Usually, the base component is a heat dissipator, a heat sink and / or a cooler (a part for a cooler). The base component receives a considerable part of the heat generated by the attached object and further dissipates it. For example, the base component further releases the heat to the ambient air via a heat sink.
[0005] The attachment object should be fixed to the base component in a manner that allows sufficient heat transfer from the attachment object to the base component. In particular, the attachment object can be fixed to the base component by pressure sintering. A sintering layer consisting of a sintering material is arranged between the attachment object and the base component. During the subsequent curing step, the sintering material is heated to a maximum sintering temperature. In addition, the attachment object and the base component are pressed together, for example along a normal direction, which can be perpendicular to the attachment side. The curing step densifies and solidifies the sintering material. A sintered body layer is formed between the attachment object and the base component by the sintering layer. The sintered body layer permanently fixes the attachment object to the base component.
[0006] The curing step can be a bottleneck in component production. It requires the use of a pressure sintering tool to press the attachment object and the base component against each other while heating the sintering material.
[0007] Each attachment object should be fixed to the base part at the correct position, i.e. at its respective predetermined position and with its respective predetermined spatial orientation. In order to use the maximum production capacity of the pressure sintering tool, before the curing step begins, the sintering layer is applied to the base part and the attachment objects are positioned on top of the sintering layer and outside the pressure sintering tool. The matching parts to be sintered are put together and then moved into the pressure sintering tool. In this matching part, the attachment objects are correctly positioned on the sintering layer. Their interface surfaces face the sintering layer.
[0008] When the pair is brought together, the pressure sintering tool is not occupied and a curing step for another component can be performed.
[0009] It is not enough to simply place the attachment object onto the sintered layer. The upper surface of the sintered layer is not very sticky, especially after some pre-drying (if any). In this pairing, the attachment object has no significant adhesion to the sintered layer.
[0010] Furthermore, at the attachment side where the attachment object is fixed, a mismatch between the shape of the interface surface of the attachment object and the shape of the base component occurs. When the attachment object is placed on the sintered layer before the curing step, its interface surface does not fit or rest snugly against the sintered layer. This may result in an unstable support of the attachment object on the sintered layer. For example, the shape of the interface surface of the attachment object may be convex. Therefore, there is only a small contact area between the interface surface and the sintered layer. The attachment object may wobble. Of course, other shape mismatches may also occur.
[0011] Without additional measures, in these cases, there is a high risk that the attached objects move away from their respective predetermined positions and / or deviate from their respective predetermined spatial orientation when the mating parts are moved into the press tool. The attached objects may wobble and easily lose their correct position. When moving the mating parts (for example, moving them into a pressure sintering tool), something is needed to keep them exactly in place. Additionally or alternatively, in the early stages of the curing step, when the attached objects are pressed against the base part and the raised interface surfaces are flattened due to the pressure increase, unintentional deflection and lateral displacement of the attached objects relative to the base part may still occur.
[0012] The current method uses an alignment frame structure that holds the attached objects in the matching parts in their correct positions, in particular during the transfer of the matching parts into the pressure sintering tool and during the curing step performed in the pressure sintering tool. The alignment frame structure includes a frame that circumferentially surrounds the base component, for example, at least in a plane perpendicular to the normal direction. The alignment frame structure may include a recess for receiving the attached object at the correct position of the attached object. Additionally or alternatively, it may include a pin that engages with a corresponding hole in the base component and / or the attached object.
[0013] The use of alignment frames, especially during transfer into the pressure sintering tool and during the curing step, increases manufacturing time, manufacturing cost and manufacturing complexity. The alignment frames are only used temporarily. They are removed from the assembly after the curing step. An appropriate alignment frame must be designed specifically for each assembly layout. Current methods are suitable for small batch production, but are too complex for large batch production.
[0014] Furthermore, the alignment frame structure is complex and delicate in design, which results in a considerable risk of failure. Summary of the invention
[0015] The invention aims to facilitate the manufacture of an assembly as described above.
[0016] This problem is solved by a method according to claim 1 .
[0017] The method is used to sinter a first surface of a first component to a second surface of a second component. It comprises the following steps:
[0018] - applying a sintered layer onto the second surface;
[0019] - providing a stabilizing device on the first surface; and
[0020] - placing the first component directly onto the sintering layer, wherein the first surface faces the sintering layer and wherein the stabilizing means protrude into the sintering layer for stabilizing the lateral position of the first component relative to the second component, thereby forming a companion piece to be sintered.
[0021] The stabilizing device engages with the sintered layer and helps to fix the first component in its correct position in the companion piece. It stabilizes the position of the first component relative to the sintered layer and thus the position of the first component relative to the second component. No additional alignment frame structure is required to ensure the correct position of the first component in the companion piece, for example during the transfer of the companion piece into a pressure sintering tool or during the curing step of curing the sintered material of the sintered layer to the sintered body layer. This facilitates manufacturing.
[0022] Since no alignment frame structure is inserted into the pressure sintering tool together with the partner, the pressure sintering tool can be smaller. Since no heat is wasted to at least partially heat the material of such an alignment frame structure in the pressure sintering tool during the curing step, energy is saved.
[0023] When the first component is placed on top of the sintered layer in its correct position, its first surface faces the sintered layer. The first surface may at least partially directly abut the sintered layer. The stabilizing device protruding into the sintered layer exhibits a form fit between the stabilizing device and the sintered layer. Naturally, this stabilizes the first component to remain in its correct position. The stabilizing device engages the sintered layer, and the sintered layer ultimately exhibits a predetermined mechanical stability. This engagement reduces the risk of the first component moving and / or deviating from its correct position in the companion piece.
[0024] Of course, the method may involve sintering the first surface of multiple first components, such as the first surface of at least two first components, to the second surface of the second component. The disclosures related to "first component" and its fixation to the second component may each relate to one, multiple or all first components in the first components. According to the present disclosure, the fixation of different first components may include different modifications. Preferably, the fixation of multiple first components is performed by the same curing step. According to one aspect, all first components can be fixed to the second component in the same manner. The first components can be positioned spaced apart from each other in the matching piece to be sintered (and correspondingly in the resulting assembly).
[0025] According to one aspect, the mating parts to be sintered are placed together outside the pressure sintering tool and then moved into the pressure sintering tool. The mating parts to be sintered can be moved into the pressure sintering tool without using an alignment frame device that engages the second component and the first component. In particular, while the mating parts (to be sintered) are moved into the pressure sintering tool, the first component can be mechanically engaged with the second component only by:
[0026] ·Through sintered layer
[0027] and, optionally, in addition, directly through a stabilizing device partner protruding through the sintered layer and directly adjoining the second surface.
[0028] It has been found that by applying the sintered layer to the first surface of the first component or the second surface of the second component the same stability can be obtained in the companion piece, provided that the stabilizing means is applied to the surface opposite to the surface to which the sintered layer has been applied.
[0029] Thus, in one embodiment, the first component may be an attachment object and the first surface may be an interface surface of the attachment object, and the second component is a base component and the second surface is an attachment side of the base component.
[0030] In an alternative embodiment, the first component may be a base component and the first surface may be an attachment side of the base component, and the second component is an attachment object and the second surface is an interface surface of the attachment object.
[0031] In one embodiment, the stabilizing means comprises at least one protrusion protruding from the interface surface. Without considering the additional stabilizing means, after the curing step, the interface surface is at least substantially flat. However, due to the convex shape of the interface surface before the curing step (particularly in the partner), at least a portion of the interface surface may not directly abut the sintered layer (non-abutting portion) in the partner to be sintered, while at least another portion of the interface surface directly abuts the sintered layer (abutting portion). When at least one protrusion protrudes from the interface surface, it protrudes towards the base component in the partner to be sintered.
[0032] If several protrusions are provided, the disclosure related to "a protrusion" may relate individually to at least one, several or all protrusions, respectively. Different protrusions may be realized according to different disclosed modifications.
[0033] The protrusions may protrude from the interface surface, for example by at least 125 μm in the normal direction. Taking into account the expected maximum convexity of the interface surface, this ensures an acceptable probability that the protrusions protrude into the sintered layer even if they are arranged in non-adjoining portions.
[0034] If the at least one protrusion is located in the abutment portion, it protrudes deeply into the sintered layer. This results in a relatively strong bond with the sintered layer.
[0035] If the at least one protrusion is located in the non-adjacent portion, it must not protrude partially into the sintered layer. Thus, there are now at least two different locations showing the engagement between the attached object and the sintered layer: the at least one adjacent portion and the at least one protrusion. This reduces the risk of the attached object deviating from its respective intended spatial orientation, for example, when the partner is moved and / or the partner is subjected to pressure sintering. Of course, this also further reduces the risk of the attached object being displaced from its respective intended position relative to the base part.
[0036] In one embodiment, the stabilizing device comprises at least two protrusions protruding from the interface surface, wherein the at least two protrusions are spaced apart from one another. When the protrusions protrude from the interface surface, they protrude towards the base part in the partner. Since the at least two protrusions protrude into the sintered layer in the partner, the individually intended positioning and the individually intended alignment of the attachment object in the partner to be sintered are ensured particularly reliably even in the case of particularly low adhesion of the interface surface to the sintered body layer (not taking into account the stabilizing device).
[0037] The stabilizing means may comprise a plurality of protrusions protruding from the interface surface. The risk that the attached object will not remain in the correct position is further reduced as the number of protrusions increases. For example, there may be at least 3 protrusions or even at least 24 protrusions.
[0038] In one embodiment, the stabilizing means comprises at least three protrusions protruding from the interface surface. The at least three protrusions may be spaced apart from each other. This ensures that the attached object rests at at least three different positions on the sintered layer. In other words, the attached object is supported on the sintered layer by at least three points of support. This prevents the attached object from swinging on top of the sintered layer, even if the shape of the interface surface is convex.
[0039] According to another aspect, at least one protrusion is respectively arranged at each corner portion of the interface surface.For example, the interface surface may be rectangular in shape and have four corner portions.
[0040] According to one aspect, parts of the stabilizing device (e.g., protrusions) can be concentrated at and / or near at least one area where the risk of cracks in the sintered body layer is expected to increase. These locations are, for example, edges and corners of the attached object and the sintered body layer, such as lateral ends (edges), especially corners, of the sintered body layer in a plane perpendicular to the normal direction, or areas of lateral ends (especially corners) of the interface surface of the sintered body layer adjacent to the attached object. In the final assembly, the combination of the sintered layer and the stabilizing device (and, if applicable, its remainder) at least partially forms a composite material remainder. This inhibits the formation and / or propagation of cracks in the sintered body layer.
[0041] For example, the stabilizing means may comprise a plurality of protrusions protruding from the interface surface, which are arranged along the circumferential outer portion of the interface surface. The protrusions may be equidistantly spaced apart along the circumference. It is also possible that the spatial density of the protrusions is increased in at least one region where the risk of crack formation in the sintered body layer is particularly high. For example, the protrusions are arranged substantially equidistantly along the edge of the sintered body layer and / or the edge of the adjacent interface surface, but with a denser spatial (narrower) arrangement at the corners of the sintered body layer and / or the corners of the adjacent interface surface.
[0042] The protrusion (or its remaining part) locally increases the thermal cycle resistance (TC resistance) of the sintered body layer. TC resistance refers to the resistance to damage by thermal cycling. During the operation of the component, the attached object (for example, in the form of a molded semiconductor power module) can generate heat. The temperature of the attached object, the sintered layer and the attached side can change during operation. This leads to thermal cycling of the sintered body layer between the attached object and the attached side. Thermally induced stresses are higher at the edges of the sintered body layer and / or the interface surface, and are particularly high at the corners of the sintered body layer and / or the interface surface. Thermal cycling can lead to crack formation and crack propagation in the sintered body layer.
[0043] Arranging many protrusions around the edge of an attached object, such as a molded module with a DCB structure (see below), such as a wire bonding structure, inhibits the propagation of cracks from the edge (where the probability of crack formation occurring is expected to increase) in a manner similar to the case of composite materials such as fiber-reinforced plastics (such as glass fibers). In homogeneous materials, cracks generally propagate more easily. In materials rich in items exhibiting different physical properties (such as protrusions or their remaining parts in this case, or glass fibers in the case of glass fibers), the tips of the cracks are repeatedly blunted, which slows down the propagation of the cracks.
[0044] According to one aspect, the lateral distance between adjacent protrusions may be less than 0.5 mm.The lateral distance may be measured where the protrusions are fixed to the interface surface.
[0045] The protrusions can locally influence the heat conduction in the sintered layer and / or the sintered body layer.
[0046] The stabilization means may comprise elements that are fixed to the interface surface and / or elements that are directly integrated with the interface surface.
[0047] The method may include forming at least a portion of the stabilizer on the interface surface by wire bonding, for example by a wire-bonder. The positions of the portions of the stabilizer formed by this technique can be controlled very precisely. The technique can be easily implemented in existing manufacturing practices. It is particularly suitable for gathering portions of the stabilizer (e.g., protrusions) at specific locations in a very precise manner. This is a cost-effective and time-effective method of securing the stabilizer to the interface surface. The bonding wires used for wire bonding are compatible with the sintering process. They do not affect the sintering process.
[0048] The thickness of the bonding wires used may be in the range of 90 μm to 200 μm, for example in the range of 100 μm to 140 μm. This allows the creation of very fine structures.
[0049] In one embodiment, the stabilizing means comprises at least one wire bonding structure. As described above, the wire bonding structure may be formed by wire bonding. It may be fixed to the interface surface by ultrasonic welding.
[0050] For example, the at least one protrusion may be a wire bonding structure formed by a wire bonder.
[0051] Therefore, the at least two protrusions may be formed into wire bonding structures by wire bonders, respectively.
[0052] In particular, the at least one wire bonding structure may be a bond. The bond is a wire bonding structure fixed to the interface surface by the free end portion of the bonding wire. In other words, the free end portion of the bonding wire is not directly fixed to the interface surface, but another portion of the bonding wire, such as at least the other end of the bonding wire, is fixed to the interface surface by melting, for example, by an ultrasonic welding process. Even after the pre-drying of the sintered layer has been completed, the sharp bond can easily penetrate the sintered layer.
[0053] At least one, several or all of the wire bonding structures may be bonds. At least one, several or all of the protrusions may be bonds.
[0054] In one embodiment, the at least one wire bond structure may be a ball bond. Typically, at least one, several or all of the wire bond structures may be ball bonds.
[0055] In one embodiment, the stabilizing device is made of a sinterable material. "Sinterable material" may refer to a material that bonds well with the sintered body layer during the curing step. For example, (multiple) wire bonding structures can be manufactured by using wires of (multiple) sinterable materials such as copper, silver and / or aluminum (including alloys based on at least one of these materials). In particular, the stabilizing device can be made of a material that is sintered together with the sintered material during the curing step. In one embodiment, the stabilizing device is made of a material that can be sintered together with the sintered layer during the curing step but has a different metal ratio from the sintered material. On the one hand, this is conducive to firmly and permanently fixing the attached object to the base component after the curing step, but on the other hand, it is conducive to suppressing the formation and / or propagation of cracks in the sintered body layer.
[0056] In one embodiment, at least one, several or all of the protrusions may include drops of glue. According to another aspect, at least one, several or all of the protrusions may include sharp burrs at the interface surface. The sharp burrs may be formed by cutting and / or scraping into the interface surface. According to another aspect, at least one, several or all of the protrusions are produced by fixing a solid protruding object, such as made of metal, to the interface surface.
[0057] The stabilizing means may comprise different types of protrusions.
[0058] According to another aspect, the method may comprise applying a sintering material onto the attachment side to form a sintering layer.
[0059] If the partner comprises a plurality of attachment objects, the sintered layer may comprise a plurality of portions, for example one portion per attachment object.The different portions of the sintered layer may be spaced apart from each other.
[0060] The sintering material may include (particularly be formed of) a sintering paste and / or a sintering slurry (alternatively referred to as a sintering preform).
[0061] The sintered material may include metal particles and at least one volatile component. The metal particles may include silver particles and / or copper particles, or may be silver particles and / or copper particles. The volatile component(s) may be organic. The density of the sintered material may be 2.5 g / cm 3 Up to 3.5g / cm 3 within the range.
[0062] The sintering material (sintering paste and / or sintering slurry) may be pre-dried. In particular, the method may include a step of pre-drying the sintering material, for example after application and before placing the attachment object on the attachment side, wherein the sintering layer is between the attachment object and the attachment side. At least a portion of the volatile organic components may evaporate during the pre-drying.
[0063] The sintering material can be applied in a wet state in an application step prior to predrying.
[0064] By pre-drying, the sintered material becomes more like a solid material compared to the wet state. The sintered slurry can adhere to the attachment surface because it is a slurry. The pre-dried sintered layer can be firmly attached to the attachment side. As the sintered material becomes more like a solid material by pre-drying, it exhibits greater resistance to resisting dragging the stabilizer parallel to the attachment side.
[0065] After evaporation of the volatile component(s), the predried sintered layer may be porous. Thus, the stabilizing means may penetrate the sintered layer even after predrying has been completed.
[0066] The thickness (along the normal direction) of the sintered layer may be in the range of 80 μm to 200 μm, for example 100 μm.
[0067] The method may include the step of placing the attachment object onto the applied sintered layer by a robot. This allows cost-effective production with high throughput and high precision. It is much easier to use a robot to perform this task since no complex alignment frame structures are required.
[0068] Pre-drying can be performed before, during and / or after placing the attachment object on the sintering layer. Pre-drying can be completed at the latest before the partner is inserted into the pressure sintering tool, in particular before the partner is moved for insertion into the pressure sintering tool. For example, pre-drying can be considered to be completed when at least 70% by weight of the volatile compounds have evaporated.
[0069] For example, the attachment object may be placed onto the pre-dried sintered material. In particular, placing the attachment object onto the applied sintered layer is performed after pre-drying is complete (eg at least 70% by weight of volatile compounds have been evaporated).
[0070] The curing step may be carried out with pre-dried sintered material.
[0071] According to one aspect, the method comprises inserting the partner to be sintered into a pressure sintering tool, wherein placing the attachment object onto the sintering layer occurs before the partner to be sintered is inserted into the pressure sintering tool. In other words, the method may comprise moving the partner to be sintered into the pressure sintering tool. In particular, the partner to be sintered may be inserted into the pressure sintering tool without the need for an alignment frame structure for holding the attachment object in the partner in its correct position.
[0072] According to another aspect, the method comprises a curing step for curing the sintered layer in the partner to be sintered. Thereby, the attached object becomes rigidly and permanently fixed to the base part.
[0073] The curing step may include sintering the sintering layer (for permanently fixing at least one attachment object to the base component) at a maximum sintering temperature in the range of 200° C. to 300° C. and / or at a maximum sintering pressure in the range of 10 MPa to 40 MPa. This ensures proper sintering and therefore ensures that the attachment object is rigidly and firmly fixed to the base component.
[0074] The curing step may be performed using a pressure sintering tool.
[0075] In one embodiment, the thickness of the sintered layer (e.g., along the normal direction) is at most 70 μm. Additionally or alternatively, the thickness of the sintered layer may be at least 20 μm. The thickness of the sintered layer may be 50 μm ± V. For example, V may be 10 μm or 6 μm. The thickness of the sintered layer may be less than the width of the previous sintered layer. The density of the sintered layer may be higher than the density of the previous sintered layer. The sintered layer may be made of at least 90% by weight (possibly at least 96% by weight) of metal, for example resulting from the metal material proportion of the sintered material. The density of the sintered layer may at least substantially correspond to the density of the metal material proportion of the sintered material.
[0076] The stabilizing device can become at least partially permanently compressed (at least partially reduced in height) during the curing step. As described above, the stabilizing device can include a protrusion formed by a bonding wire with a diameter of 125 μm. In addition, the sintered layer should be thin to allow good heat transfer from the attached object to the base component, for example, its thickness is at most 70 μm. Even in the case where the interface surface of the attached object is initially convex in shape, it has become flat in the later stages of the curing step. The force of pressing the attached object to the base component and the resulting reaction force from the sintered layer and the stabilizing device squeezed between the interface surface and the base component flatten the interface surface. In addition, due to the relative friction between the attached object, the sintered layer and the base component and due to the later curing (hardening) of the sintered layer, a stabilizing device is no longer needed to keep the attached object in its correct position. Therefore, there is no problem causing the stabilizing device to become at least partially permanently compressed during the curing step. It was also found that this does not damage the sintering process.
[0077] According to one aspect, the stabilizing device may be made of a different material than the interface surface. For example, the hardness and / or yield strength of (the material of) the stabilizing device may be less than the hardness and / or yield strength of (the material of) the interface surface. This reduces the risk of the interface surface being damaged if the stabilizing device is compressed during the curing step.
[0078] According to another aspect, the attachment object is or includes at least one of the following:
[0079] -Heating components,
[0080] - electronic components, such as semiconductor components, and
[0081] -Semiconductor power modules.
[0082] In particular, the attachment object may be a semiconductor power module.A semiconductor power module may include at least one semiconductor component.
[0083] Electronic components and semiconductor power modules generate heat during operation; therefore, they can also be considered as heat-generating components.
[0084] The semiconductor component may include or consist of a semiconductor switch, an insulated gate bipolar transistor (IGBT), a metal oxide semiconductor field effect transistor (MOSFET), etc.
[0085] In particular, the attached object may include a molded module or consist of a molded module. The molded module may be a semiconductor power module including a resin cover. The resin cover may be manufactured by transfer resin molding. If a plurality of attached objects are fixed to the patterned object, at least one of them, a portion of them, or all of them may include a molded module or consist of a molded module, respectively.
[0086] The semiconductor power module itself may include different layers and / or components.
[0087] Semiconductor power modules may include any, some or all of the following:
[0088] - Integrated heat spreader,
[0089] - insulating layer,
[0090] - (internal) circuit layer,
[0091] - a fixing layer (e.g. an inner sintering layer) for fixing the semiconductor component to the insulating layer and / or the circuit layer,
[0092] - semiconductor components,
[0093] -bonding wires, and
[0094] - Resin cover ("molded module").
[0095] The insulating layer may be made of a ceramic material. The (internal) circuit layer may be fixed to the insulating layer. Additionally or alternatively, an integrated heat sink may be fixed to the insulating layer. The integrated heat sink may be arranged at the interface surface. In particular, it may constitute the interface surface. The insulating layer may be arranged between the integrated heat sink and the (internal) circuit layer.
[0096] In one embodiment, the attached object (e.g., a semiconductor power module) includes a direct copper bond (DCB) structure. It may include a substrate, such as a ceramic substrate, forming an insulating layer. In addition, the DCB structure may include an insulating layer, and one or both of an (internal) circuit layer and an integrated heat sink.
[0097] According to another aspect, the patterned object is or comprises a heat dissipator, a heat sink and / or a cooler (part of a cooler).
[0098] In one embodiment, the attachment side of the base component is made of metal. Additionally or alternatively, the interface surface is made of metal. This allows for good transfer and dissipation of heat generated in the attached object.
[0099] The above problem is further solved by an assembly comprising a base component and an attachment object, wherein a sintered layer between an interface surface of the attachment object and an attachment side of the base component secures the attachment object to the base component, wherein the stabilization device formed on the interface surface or at least its remaining part protrudes into the sintered layer.
[0100] Features and advantages described with respect to the method apply correspondingly to the assembly, and vice versa.For example, as described above, the stabilizing means (eg, the protrusions, or the remainder thereof) may inhibit the formation and / or propagation of cracks.
[0101] According to one aspect, the attachment object may have been (permanently) fixed to the base object using the methods disclosed herein.
[0102] The component may be adapted to exhibit an electrical function. For example, it may be adapted to switch an electric current.
[0103] The assembly may be configured to be electrically connected to other electrical and / or electronic components.
[0104] In one embodiment, the component is configured to form part of an electrical circuit.
[0105] The component may be configured to form part of a powertrain circuit, such as in an electric vehicle. Electric vehicles may include electric cars, trucks, electric trains, marine vehicles (e.g., ships and boats), aircraft, and the like. The powertrain circuit may be a circuit for an electric motor, an electric powertrain, a hybrid electric powertrain, a battery electric powertrain, and / or the like. For example, the component may be a multi-chip automotive traction power module. Typically, the powertrain circuit may be configured for mobile, semi-mobile, and / or fixed applications. For example, powertrain circuits for compressors, cableways, stationary cranes, pumps, and the like may also be considered.
[0106] According to one aspect, the assembly is configured to form part of an inverter circuit.The assembly may be used in an inverter, for example in a power train circuit.
[0107] According to one aspect, the assembly is a half-bridge power assembly.
[0108] The above mentioned problems are further solved by a to-be-sintered partner for fixing an interface surface of an attachment object to an attachment side of a base component by sintering, the partner comprising:
[0109] Base components;
[0110] Attaching objects; and
[0111] a sintered layer disposed between the attachment side and the interface surface;
[0112] Wherein, a stabilizing device for stabilizing the lateral position of the attached object relative to the base component is formed on the interface surface, wherein the stabilizing device protrudes into the sintered layer to stabilize the lateral position of the attached object relative to the base component.
[0113] The features and advantages described with regard to the method and the assembly apply correspondingly to the counterpart to be sintered, and vice versa.
[0114] The companion piece to be sintered may be suitable for producing the component.
[0115] Additional features, advantages and possible applications of the invention result from the following description of exemplary embodiments and the accompanying drawings. All features described and / or illustrated graphically herein form the subject matter of the invention individually or in any desired combination, regardless of how they are combined in the claims or in their reference to preceding claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0116] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings, in which:
[0117] Figure 1 shows a cross-sectional view of a base component, wherein a sintered layer is applied to an attachment side of the base component and a semiconductor power module is placed onto the sintered layer, wherein the semiconductor power module comprises stabilization means protruding from an interface surface of the semiconductor power module for engaging the sintered layer, in particular for being penetrated into the sintered layer;
[0118] Figure 2 A cross-sectional view of a matching part to be sintered is shown, including Figure 1 A base component with a sintered layer and a semiconductor power module as shown in , wherein the semiconductor power module is placed on the sintered layer, wherein the stabilizing device protrudes into the sintered layer, thereby stabilizing the lateral position of the semiconductor power module relative to the base component;
[0119] Figure 3 Shown by Figure 2 A cross-sectional view of an assembly formed by pressure sintering of a matching part to be sintered as shown in FIG.
[0120] Figure 4 Shows Figure 1 A view on the interface surface of a semiconductor power module;
[0121] Figure 5 A flow chart showing a method for sintering an interface surface of a semiconductor power module to an attachment side of a base component; and
[0122] Figures 6A to 6E Various embodiments of protrusions of the stabilizing device are shown.
[0123] Figure 7 A cross-sectional view of an embodiment of two components to be joined using the method of the present invention is shown.
[0124] Figure 8 Shown by Figure 7 A cross-sectional view of a matching piece formed by the components shown in FIG. DETAILED DESCRIPTION
[0125] Figure 11 is a cross-sectional view showing a base member 10 and an attached object, which should be fixed to the attachment side 11 of the base member 10 by pressure sintering to finally produce a Figure 3 Component 60 is shown.
[0126] In this example, the attached module is a semiconductor power module 30 , more specifically, a semiconductor power module 30 having a resin cover 40 (which may be referred to as a molded semiconductor power module).
[0127] The semiconductor power module 30 includes a direct copper bonding (DCB) structure having a ceramic insulating layer 34, an integrated heat sink 33, and an internal circuit layer 35. The side of the integrated heat sink 33 facing away from the insulating layer 34 constitutes an interface surface 31. The integrated heat sink 33 is formed on one side of the insulating layer 34 and fixed to the insulating layer 34. The internal circuit layer 35 is formed on the opposite side of the insulating layer 34 (e.g., Figure 1 The semiconductor component 37 is fixed to the internal circuit layer 35 by the internal sintered body layer 36. The internal sintered body layer 36 may include separate parts for some or each of the semiconductor components 37. The semiconductor element 37 includes, for example, an IGBT and / or a MOSFET. The semiconductor power module 30 may also include internal wiring 38, for example, for forming an electrical connection between the semiconductor component 37 and the internal circuit layer 35. In addition, the semiconductor power module 30 may include an electrical connector 39. The electrical connector 39 can be used to establish an electrical connection with other attached objects (not shown), such as establishing an electrical connection with other semiconductor power modules, which become fixed to the same base component 30 and / or fixed to other electrical components.
[0128] The optional resin cover 40 covers the entire semiconductor power module 30 except for the integrated heat sink 33 at the interface surface 31. The resin cover 40 has electrical insulation, moisture resistance, and protection against mechanical and chemical damage.
[0129] The semiconductor power module 30 is adapted to provide at least one electrical function in the final assembly 60, for example for switching current. In operation, the semiconductor power module 30 generates heat. By fixing the semiconductor power module 30 to the base member 10, heat dissipation is improved and overheating of the semiconductor power module 30 during operation is prevented.
[0130] In the assembly 60, the base component 10 is used to dissipate the heat generated by the semiconductor power module 30. For example, the base component 10 may be a heat sink having fins, such as rectangular fins and / or pin fins (not shown). Additionally or alternatively, the base component 10 may be a cooler or a part for forming a cooler. The base component 10 may include a channel structure for guiding a fluid (e.g., a coolant).
[0131] The base component 10 can be made of aluminum and / or copper (including corresponding alloys). In a variant (not shown), the base component 10 is made of aluminum (including aluminum alloys) and includes an inlay at the contact area, wherein the inlay is made of copper (including copper alloys).
[0132] The attachment object is rigidly and permanently fixed to the base member 10 by pressure sintering.
[0133] The attachment side 11 of the base object 10 is substantially flat at least in the contact area where the attachment object (semiconductor power module 30) becomes fixed. The normal direction N is perpendicular to the contact area. In this example, the entire attachment side 11 is flat and the normal direction N is perpendicular to the entire attachment side 11.
[0134] The following references Figure 5 and other figures describe in more detail an example of a corresponding method for (pressure) sintering an interface surface 31 of an attachment object (eg, a semiconductor power module 30 ) to an attachment side 11 of a base component 10 .
[0135] In the sintering layer applying step S20, a sintering material is applied to the attachment side 11 of the base component 10 to form a sintering layer 20 that will be pressure-sintered in the subsequent curing step S60. The sintering layer 20 is formed at least at the contact area of the attachment side 11 for attaching the attachment object. In this example, the sintering layer 20 is formed by using a sintering paste. The sintering paste is spread on the attachment side 11, at least on the contact area. It includes finely divided metals, such as silver, copper and / or another metal. In this example, silver and / or copper are used as metals (including corresponding alloys). In the sintering layer applying step S20, a sintering paste in a wet state is applied. The sintering paste includes a liquid organic volatile compound. This is conducive to the correct application of the sintering paste. The density of the sintering paste can be 2.5g / cm 3 Up to 3.5g / cm 3 within the range.
[0136] Figure 1 A base component 10 is shown in which one portion (one patch) of the sintering layer 20 is applied on the attachment side 11. Of course, the portion may be larger, in particular if several attachment objects are to be pressure-sintered to the base component 10 via the same portion. Additionally or alternatively, the sintering layer 20 may comprise a plurality of portions (patches) for pressure-sintering different attachment objects to the base component 10.
[0137] The sintered layer 20 may be subjected to a pre-drying step S30. In the pre-drying step S30, at least a portion of the volatile components evaporate. In other words, the sintered layer 20 is at least partially dried during the pre-drying step S30. The pre-drying step S20 may include allowing the base component 10 with the applied sintered layer 20 to rest for at least a predetermined time. When the sintered layer 20 dries, it becomes more like a solid but spongy material (with voids therein). The sintered layer 20 also becomes firmly attached to the attachment side 11.
[0138] The thickness of the (pre-dried) sintered layer 20 (in the normal direction N) may be in the range of 80 μm to 200 μm. The thickness may not be affected, at least substantially, by the pre-drying step S30. For example, the thickness after pre-drying may differ from the thickness before pre-drying by less than 20%.
[0139] Figure 2 A companion piece 50 to be sintered is shown. The companion piece 50 comprises a base component 10, a sintering layer 20 applied to an attachment side 11, and an attachment object (here in the form of a semiconductor power module 30) placed onto (on top of) the sintering layer 20 in its correct position.
[0140] The interface surface 31 of the attached module (in this case the semiconductor power module 30) is usually convex. Figure 1 and Figure 2 The shape of the protrusion may be caused by different thermal expansion coefficients of the elements constituting the semiconductor power module 30 .
[0141] In a conventional embodiment (not shown), the interface surface 31 of the semiconductor power module 30 is flat and smooth except for the raised curved portion. Due to the raised curved portion, only a small portion of the interface surface 31 (only a small portion of the underside of the integrated heat sink 33) directly abuts the top of the sintered layer 20. Therefore, the semiconductor power module can easily swing, twist and / or shift laterally relative to the base component 10. This will impair proper manufacturing. Therefore, conventionally, the matching component 50 excludes a specially designed connecting frame structure to keep the semiconductor power module 30 in its correct lateral position intended for the final assembly 60. "Lateral" can refer to a direction perpendicular to the normal direction N (parallel to Figure 2 Attachment side 11).
[0142] According to the present invention, the method comprises a step S10 of providing a stabilizing device on the interface surface 31. If the attachment object (i.e., the semiconductor power module 30) is placed on the sintering layer 20 (which may have been pre-dried before), the stabilizing device is configured to protrude into the sintering layer 20 and stabilize the lateral position of the attachment object relative to the base component 10. Therefore, there is no need to use an additional alignment frame structure to stabilize the attachment object in its correct lateral position relative to the base component 10. The partner 50 to be sintered does not include such an additional alignment frame structure and is processed without such an additional alignment frame structure.
[0143] In this example, step S10 includes providing a plurality of protrusions 32 at the interface surface 31. The protrusions 32 protrude from the interface surface 31 (in this example, from the underside of the integrated heat sink 33).
[0144] The protrusions 32 can be produced by means of an ultrasonic wire bonder. The protrusions 32 can be wire bond structures. In particular, they can be formed as so-called bond-offs. In order to produce such a bond-off, the wire bonder fixes the end of the bonding wire to the interface surface 31 (fixed to the integrated heat sink 33) by ultrasonic waves. Then, the bonding wire is cut to separate the bonding wire segments fixed to the interface surface 31.
[0145] The diameter of the bonding wire and thus the diameter of the bonding wire segment forming the protrusion 32 (stabilizing means) may be, for example, 125 μm.
[0146] The stabilizing means may be made of a sinterable material. It may be made of a sinterable metal, such as copper, silver and / or gold (including alloys based on one or more of these metals). The bonding wires may be made of corresponding materials.
[0147] In the placing step S40, the attachment object is placed on the sintered layer 20. The placing step S40 may include automatically aligning the attachment object relative to the base member 10. For example, the attachment object may be placed at a correct position on the sintered layer 20 by at least one robot. The correct position is Figure 3 The desired lateral position in the final assembly 60 is shown.
[0148] The placing step S40 may include placing several attachment objects at their respective correct locations on the sintered layer 20 .
[0149] The placing step S40 results in the formation of Figure 2 A component 50 to be sintered is shown.
[0150] In the fitting 50, the stabilizing means (in this example, the protrusions 32) protrude deeply into the sintered layer 20. In more detail, in this example, the sharp engaging objects are pushed into the pre-dried sintered layer 20. They are pierced into the sintered layer 20.
[0151] The pre-dried sintered layer 20 is similar to snow in that it can be further compressed and it resists the dragging of the stabilizing device transversely to the normal direction N, ie parallel to the attachment side 11 .
[0152] The stabilizing means protruding into the sintering layer 20 stabilizes the correct position of the attached object relative to the sintering layer 20, and thus stabilizes the correct position of the attached object relative to the base member 10. This allows the fitting 50 to be sintered to be handled without the use of an additional alignment frame structure without laterally shifting or twisting the attached object out of its correct position. Since a plurality of protrusions 32 are provided in this example, the attached object also cannot swing.
[0153] In the transfer step S50, the partner 50 to be sintered is moved and inserted into a pressure sintering tool. The transfer step S50 is performed without an additional alignment frame structure.
[0154] In the curing step S60, the sintered layer 20 is transformed into a sintered body layer 20a. Thereby, the attached object (in this example, the semiconductor power module 30) becomes firmly, rigidly and permanently fixed to the base component 10. The curing step 60 is performed in a pressure sintering tool. The curing step 60 includes, for example, pressing the attached object and the base component 10 toward each other along the normal direction N. The sintered layer 20 is pressed between the interface surface 31 and the attachment side 11. In addition, heat is provided, for example, by a pressure sintering tool, for heating the sintered layer 20. Due to the combined application of pressure and heat to the sintered layer 20, the sintered layer 20 is transformed into a sintered body layer 20a. The stabilizing device does not impair the sintering process.
[0155] During the curing step S60, the sintered layer 20 is heated to a maximum sintering temperature in the range of 200° C. to 300° C. The pressure applied to the sintered layer 20 may be in the range of 10 MPa to 40 MPa. In the curing step S60, the temperature may be maintained in the sintering temperature range and / or the pressure applied to the sintered layer 20 may be maintained in the sintering pressure range for a duration in the range of 2 minutes to 10 minutes.
[0156] The thickness of the sintered body layer 20a (in the normal direction N) may be smaller than the thickness of the previous sintered layer 20. For example, the thickness of the sintered body layer 20a may be in the range of 40 μm to 60 μm, for example, 50 μm.
[0157] Such a sintered body layer 20a (ignoring the stabilizing device or its remaining part 32a) consists of the metal proportion contained in the original sintering paste. The density of the sintered body layer 20a is higher than the density of the earlier (pre-dried) sintered layer 20. For example, the density of the sintered body layer 20a is similar to the density of the metal proportion (for example, if the metal proportion is silver, then about 10.5 g / cm 3 If it is copper, it is about 9g / cm 3 ).
[0158] Figure 3 Shown by Figure 2 The assembly 50 to be sintered is shown to produce a final assembly 60 , wherein the production includes a curing step S60 .
[0159] In this example, the original diameter of the bonding wire (and therefore the protrusion 32) is larger than the thickness of the sintered body layer 20a. Therefore, the stabilizing means (protrusion 32) is deformed during the curing step S60. The remaining part 32a of the stabilizing means is embedded in the final sintered body 20a.
[0160] The material of the stabilizing device may be softer (e.g., lower hardness and / or yield strength) than the material of the integrated heat sink 33 and / or the material of the base component 10 at the attachment surface. This allows the stabilizing device to deform during the curing step S60 without damaging the attachment module and / or the base component 10.
[0161] The material of the stabilizing device and its remaining part 32a on the one hand and the material of the sintered body layer 20a on the other hand may be different. Therefore, the stabilizing device or the remaining part 32a (in the case of significant deformation of the stabilizing device during the curing step S60) may be different. Figure 3 The final assembly 60 is shown as at least partially formed of a composite material.
[0162] The stabilizing means or remaining portion 32 a in the sintered body layer 20 a may locally influence the thermal conductivity between the attached object and the base member 10 .
[0163] As described above, the attached object may generate heat during operation, for example, when the assembly 60 switches current. The amount of heat generated per time unit and therefore the temperature of the attached object (e.g., at the integrated heat sink 33) varies depending on the operating state. Due to the difference in thermal expansion coefficients, the rigid connection between the attached object and the base component 10 via the sintered body layer 20a is subject to stress generated by thermal cycles. This may lead to the formation and expansion (growth) of cracks in the sintered body layer 20a.
[0164] The local composite structure in the sintered body layer 20a created by the embedded stabilizing device or its remaining portion 32a locally inhibits the formation and propagation of cracks in the sintered body layer 20a. The boundary between different materials can redistribute local stress and strain and play a role in preventing crack propagation.
[0165] According to one aspect, stabilizing means, for example provided in the form of protrusions 32 made as joints, are gathered at and / or near areas in the sintered body layer 20a where the risk of cracking is expected to increase. These areas are, for example, areas in the sintered body layer 20a below the peripheral area of the integrated heat sink 33 (in a plane parallel to the normal direction N), i.e. below the edge area of the integrated heat sink 33, in particular below the corner area. Thus, the stabilizing means can be gathered at corresponding areas at the integrated heat sink 33.
[0166] Figure 4 FIG. 3 is a view of the underside of the attachment module 30 before the curing step S60 is performed. The protrusions 32 are provided at the underside of the integrated heat sink 33. In more detail, they are arranged equidistantly along the circumferential outer portion 31a of the underside of the integrated heat sink 33. Figure 3 In the final assembly 60 shown, the protrusions 32 or at least their remaining portions 32 are located in the areas of the sintered body layer 20a where the risk of cracking is highest. This improves the resistance of the assembly 60 (and in particular the sintered layer 20) to thermal cycling and therefore improves the reliability of the assembly 60. Figure 4 As shown, the lower portion of the resin cover 40 may laterally bypass the peripheral area of the integrated heat sink 33. It is believed that the lower portion of the resin cover 40 does not form a part of the interface surface 31 because the resin material does not form a strong connection with the sintered body layer 20a.
[0167] Of course, the method may include pressure sintering the interface surfaces of several attachment objects (eg, several semiconductor power modules 30) to the attachment side 11 of the base component. Accordingly, the partner 50 may include several attachment objects.
[0168] Assembly 60 is configured to form part of an electrical circuit, such as a powertrain circuit for mobile, semi-mobile and / or stationary applications. Electrical connector 39 may be used to integrate assembly 60 in the electrical circuit.
[0169] Figures 6A to 6E Different embodiments of the projections 32 provided at the interface side 31 are shown.
[0170] exist Fig. 6A In the embodiment, as described above, a single protrusion 32 is formed as a short wire bond (bond).
[0171] Figure 6BAn embodiment of a protrusion 32 formed by ball bonding is shown. In this case, the protrusion 32 includes a ball portion 321 fixed to the interface surface 31 and an appendage 322 further protruding from the ball portion 321 away from the interface surface 31. In the first step, the ball portion 321 is formed at the interface side 31. To this end, the bonding wire is supplied by the capillary of the bonding tool and is subjected to a high voltage charge. Therefore, one end of the bonding wire metal melts at the tip of the capillary. Due to the surface tension of the molten metal, the ball portion 321 is preformed at the end of the bonding wire. The preformed ball portion 321 cools and solidifies at least partially. The preformed spherical portion 321 is pushed against the interface surface 31 and fixed to the interface surface 31, for example, by ultrasonic welding. In the second step, the capillary is lifted off the interface surface 31 while the bonding wire is further supplied by the capillary. Then, the bonding wire is cut. This results in an additional appendage 322 on the top of the spherical portion 321.
[0172] exist Figure 6C In the embodiment shown, the protrusion 32 is formed by a solid (metal) object 323 that is fixed to the interface surface 31. This ensures that the protrusion 32 has a very precise shape. The solid object 323 may have a sharp peak (e.g. Figure 6C ). The solid object 323 is provided (eg, prefabricated) as a separate element and then welded, glued and / or brazed to the interface surface 31. For example, the solid object 323 may be fixed by an ultrasonic welding process.
[0173] Another method is Fig.6D As shown. In this case, the protrusion 32 is a glue drop 324. The glue drop 324 has a sharp peak. To produce the glue drop 324, the material can be applied to the interface surface 31 as a viscous liquid and then cured. In one embodiment, the glue drop 324 is formed by hot melt glue.
[0174] Fig. 6E Another embodiment of a protrusion 32 is shown. In this case, the protrusion 32 is a sharp burr 325. An exemplary sharp tool 326 for forming the burr 325 is shown by a dashed line. The sharp tool 326 is pushed into the interface surface 31 of the attachment object 30 so that a small portion of the interface surface 31 is raised as a sharp protrusion 32.
[0175] Figure 7 The first and second components 130 and 110 are shown ready to be sintered using the method of the present invention to the first surface 131 of the first component 130 to the second surface 111 of the second component 110. The sintering layer 20 has been applied to the second surface 111 of the second component 110, and the stabilizing device 32 has been provided on the first surface 131 of the first component.
[0176] Figure 8 A fitting 50 is shown which is formed by placing a first component 130 directly onto a sintering layer 20, wherein a first surface 131 of the first component faces the sintering layer 20, and wherein stabilizing means 32 protrude into the sintering layer 20 for stabilizing the lateral position of the first component 130 relative to the second component 110. The fitting 50 thus formed is suitable for being moved and inserted into a pressure sintering tool without any additional alignment frame structure.
[0177] List of reference numerals:
[0178] 10 Base components
[0179] 11 Attachment side
[0180] 20 Sintering layer
[0181] 20a Sintered body layer
[0182] 30Semiconductor power module (attached object)
[0183] 31 Interface surface
[0184] 31a Circumferential outer
[0185] 32 Stabilizer
[0186] 32a Remaining part (of the stabilizing device)
[0187] 33 Integrated heat sink
[0188] 34 Insulation layer
[0189] 35 Internal circuit layer
[0190] 36 Internal sintered body layer
[0191] 37 Semiconductor components
[0192] 38 Internal connections
[0193] 39 Electrical connector
[0194] 40 Resin cover
[0195] 50 (to be sintered) matching parts
[0196] 60 Components
[0197] 110 Second Part
[0198] 111 Second Surface
[0199] 130 First Part
[0200] 131 First Surface
[0201] 321 Spherical part
[0202] 322 Addendum
[0203] 323 Solid metal object
[0204] 324 Glue Drops
[0205] 325 Burr
[0206] 326 Tools
[0207] N Normal direction
[0208] S10 provides a stabilization device (step)
[0209] S20 Sintering layer application step
[0210] S30 Pre-drying step
[0211] S40 placement steps
[0212] S50 Transfer Steps
[0213] S60 Curing Steps
Claims
1. A method for sintering a first surface (131) of a first component (130) to a second surface (111) of a second component (110), the method comprising the following steps: Applying a sintered layer (20) to the second surface (111); · providing a stabilizing device (32) on the first surface (131); and Placing the first component (130) directly onto the sintering layer (20), wherein the first surface (131) faces the sintering layer (20), and wherein the stabilizing device (32) protrudes into the sintering layer (20) for stabilizing the lateral position of the first component (130) relative to the second component (110), thereby forming a matching piece (50) to be sintered.
2. The method according to any one of the preceding claims, characterized in that The stabilizing means comprises at least one protrusion (32) protruding from the first surface (131).
3. The method according to claim 2, characterized in that The stabilizing device comprises at least two protrusions (32) protruding from the first surface (131), wherein the at least two protrusions (32) are spaced apart from each other.
4. The method according to claim 3, characterized in that: The stabilizing device includes a plurality of protrusions (32) protruding from the first surface (131), and the plurality of protrusions are arranged along a circumferential outer portion (31a) of the first surface (131).
5. A method according to any one of the preceding claims, characterised in that At least a portion of the stabilizing device (32) is formed on the first surface (131) by wire bonding.
6. The method according to claim 5, characterized in that The stabilizing device (32) includes at least one wire bonding structure.
7. A method according to any one of the preceding claims, characterised in that The step of inserting the partner (50) to be sintered into a pressure sintering tool, wherein placing the first component (130) onto the sintering layer (20) occurs before inserting the partner (50) to be sintered into the pressure sintering tool.
8. The method according to any one of the preceding claims, characterized in that The first component (130) is an attachment object (30), the first surface (131) is an interface surface (31) of the attachment object (30), and the second component (110) is a base component (10), the second surface (111) is an attachment side (11) of the base component (10).
9. The method according to any one of claims 1 to 7, characterized in that The first component (130) is a base component (10), the first surface (131) is an attachment side (11) of the base component (10), and the second component (110) is an attachment object (30), the second surface (111) is an interface surface (31) of the attachment object (30).
10. The method according to any one of the preceding claims, characterized in that A curing step (S60) for curing the sintered layer (20) in the companion piece (50) to be sintered.
11. The method according to claim 10, characterized in that The solidification step (S60) includes sintering the sintered layer (20) at a maximum sintering temperature in the range of 200°C to 300°C and / or at a maximum sintering pressure in the range of 10 MPa to 40 MPa.
12. The method according to claim 10 or 11, characterized in that: The stabilizing device (32) becomes at least partially permanently compressed during the curing step (S60).
13. The method according to any one of the preceding claims, characterized in that The stabilizing device (32) is made of a different material than the first surface (131).
14. The method according to any one of claims 10 to 13, characterized in that The attachment object is or includes at least one of the following: -Heating components (30, 35, 37, 38, 39); - electronic components (30, 37); and - A semiconductor power module (30).
15. The method according to any one of claims 10 to 14, characterized in that The base component (10) is a heat dissipator, a heat sink and / or a cooler.
16. The method according to any one of claims 10 to 15, characterized in that The attachment side (11) of the base component (10) is made of metal, and / or the interface surface (31) is made of metal.
17. An assembly (60) comprising a base member (10) and an attachment object (30), wherein: A sintered body layer (20a) located between an interface surface (31a) of the attachment object (10) and an attachment side (11) of the base component (10) secures the attachment object (30) to the base component (10), It is characterized in that the stabilizing device (32) formed on the interface surface (31) or at least the remaining part (32a) of the stabilizing device (32) protrudes into the sintered body layer (20a).
Citation Information
Patent Citations
Method for low-temperature pressure sintering
CN101952960A
Pressure sintering method and pressure transmission device therefor
CN109285790A
Power module and power conversion device
CN114846598A
Method for fastening microtool components to objects
US20050277244A1
Fastening objects to each other
US20190168463A1