Method for adding dosage of catalyst for efficiently preparing N-oxide

By heating the catalyst and adding it at multiple positions, as well as shaking and stirring in the reactor and slowly dripping hydrogen peroxide, the problem of prolonged catalyst diffusion time is solved and the efficiency of N-oxide preparation and reaction effect are improved.

CN118807616APending Publication Date: 2024-10-22CHONGQING ZENGCHENG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310352765.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-04
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

In the prior art, the catalyst takes time to diffuse when injected, which results in prolonged chemical reaction time and reduces the efficiency of N-oxide preparation.

Method used

Use a heater to heat the catalyst and add it at multiple positions, combined with shaking and stirring in the reactor and slowly and evenly dripping hydrogen peroxide, and control the temperature and dripping time to speed up the catalyst diffusion and reaction rate.

Benefits of technology

The catalyst activity and reaction efficiency are improved, the N-oxide preparation time is shortened, and the reaction effect is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118807616A_ABST
    Figure CN118807616A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of N-oxide processing methods, and provides a method for adding a catalyst for efficiently preparing N-oxide, which comprises the following steps: S1, adding 1200kg of 3-cyanopyridine dissolving solution, water and sulfuric acid into a reaction kettle; s2, preparing to add 10kg of a catalyst, heating the catalyst by using a heater, and then adding the heated catalyst into the reaction kettle at multiple positions; the catalyst is heated to 37 DEG C through the heater, the activity of the catalyst can be enhanced to the maximum extent, follow-up operation is facilitated, meanwhile, the heated catalyst is added at multiple positions, the catalyst is fully diffused, the follow-up reaction effect is enhanced, and then the N-oxide preparation efficiency is improved; meanwhile, the inside of the reaction kettle is oscillated and stirred when the hydrogen peroxide is added twice, so that the hydrogen peroxide can be quickly diffused, the reaction of the hydrogen peroxide and the raw materials in the reaction kettle is accelerated, the oxidation reaction effect is enhanced, and the N-oxide preparation efficiency is further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of N-oxide processing methods, and in particular is a method for adding a catalyst dosage for efficiently preparing N-oxide. Background Art

[0002] N-oxide is a metal oxide that conducts electricity using electrons as carriers. There are two types of structural defects in N-oxide, one is interstitial metal ions and the other is oxygen ion vacancies. Catalysts are required for the preparation of N-oxide.

[0003] In the existing preparation of N-oxide, raw materials such as catalysts are added into a reactor, and then heated to react, and finally N-oxide is obtained;

[0004] However, when adding existing catalysts, most of them are injected at one position, so that the catalyst needs a certain amount of time to diffuse, resulting in an increase in the time required for the chemical reaction, thereby reducing the efficiency of N-oxide preparation. In view of this, a method for adding a catalyst dosage for efficiently preparing N-oxide is provided. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a method for adding a catalyst for efficiently preparing N-oxides, so as to solve the problem that the catalyst is injected at a single position in the prior art, so that the catalyst needs a certain amount of time to diffuse, resulting in an increase in the time required for the chemical reaction, thereby reducing the efficiency of N-oxide preparation.

[0006] A method for efficiently adding a catalyst for preparing N-oxides comprises the following steps:

[0007] S1, first add 1200kg 3-cyanopyridine solution, water and sulfuric acid into a reactor;

[0008] S2, then prepare to add 10kg of catalyst, the catalyst is a titanium silicon molecular sieve prepared with ZSM-5 as a carrier, and use a heater to heat the catalyst to increase the catalyst activity, and then add the heated catalyst into the reactor from multiple positions to fully diffuse the catalyst and enhance the subsequent reaction effect;

[0009] S3, then the reactor is heated to 77°C-80°C by a heater, and hydrogen peroxide is slowly and evenly dripped into the reactor, and the reactor is shaken and stirred at the same time. The time for dripping hydrogen peroxide is controlled within 6 hours, and the temperature of the reactor is controlled at 77°C-80°C, and kept warm for 1 hour;

[0010] S4, continue to drip hydrogen peroxide into S3, and at the same time, shake and stir the reactor. The dripping time of hydrogen peroxide is 5 hours, and the temperature in the reactor is controlled at 77°C-80°C, and kept warm for 11 hours;

[0011] S5, central control sampling, to obtain the finished product.

[0012] Preferably, in step S1, the solvent for dissolving 3-cyanopyridine is chloroform, which is also called chloroform. It is an organic compound with a chemical formula of CHCl3. It is a colorless, transparent liquid with a special smell, sweet taste, high refractive index, non-flammable, heavy, and volatile.

[0013] Preferably, in step S1, the sulfuric acid is 35% dilute sulfuric acid.

[0014] Preferably, in step S2, the heater needs to heat the catalyst to 37°C.

[0015] Preferably, in step S3, the hydrogen peroxide is an oxidant, and the hydrogen peroxide is 35% hydrogen peroxide, and the amount of hydrogen peroxide dripped in is 55% of the total amount of hydrogen peroxide to be dripped in.

[0016] Preferably, in step S4, the amount of hydrogen peroxide added is 45% of the total amount of hydrogen peroxide added.

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] 1. The present invention heats the catalyst to 37° C. by a heater, which can maximize the activity of the catalyst and facilitate subsequent operations. At the same time, the heated catalyst is added to multiple positions to allow the catalyst to fully diffuse, enhance the subsequent reaction effect, and thus improve the efficiency of N-oxide preparation.

[0019] 2. The present invention performs oscillation and stirring inside the reactor when adding hydrogen peroxide twice, so that the hydrogen peroxide can diffuse quickly, thereby accelerating the reaction between the hydrogen peroxide and the raw materials in the reactor, enhancing the effect of the oxidation reaction, and thus improving the efficiency of the preparation of N-oxides. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 The process flow chart of the preparation of N-oxide of the present invention is shown in FIG. DETAILED DESCRIPTION

[0021] The following embodiments of the present invention are described in further detail in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0022] As attached Figure 1 As shown:

[0023] A method for efficiently adding a catalyst for preparing N-oxides comprises the following steps:

[0024] S1, first add 1200kg 3-cyanopyridine solution, water and sulfuric acid into a reactor;

[0025] S2, then prepare to add 10kg of catalyst, and use a heater to heat the catalyst to increase the catalyst activity, and then add the heated catalyst into the reactor from multiple positions to allow the catalyst to fully diffuse and enhance the subsequent reaction effect;

[0026] S3, then the reactor is heated to 77°C-80°C by a heater, and hydrogen peroxide is slowly and evenly dripped into the reactor, and the reactor is shaken and stirred at the same time. The time for dripping hydrogen peroxide is controlled within 6 hours, and the temperature of the reactor is controlled at 77°C-80°C, and kept warm for 1 hour;

[0027] S4, continue to drip hydrogen peroxide into S3, and at the same time, shake and stir the reactor. The dripping time of hydrogen peroxide is 5 hours, and the temperature in the reactor is controlled at 77°C-80°C, and kept warm for 11 hours;

[0028] S5, central control sampling, to obtain the finished product.

[0029] Furthermore, in step S1, the solvent for dissolving 3-cyanopyridine is chloroform.

[0030] Furthermore, in step S1, the sulfuric acid is 35% dilute sulfuric acid.

[0031] Furthermore, in step S2, the heater needs to heat the catalyst to 37°C.

[0032] Further, in step S3, hydrogen peroxide is used as the oxidant, and the hydrogen peroxide is 35% hydrogen peroxide, and the amount of hydrogen peroxide dripped in is 55% of the total amount of hydrogen peroxide that needs to be dripped in.

[0033] Furthermore, in step S4, the amount of hydrogen peroxide added is 45% of the total amount of hydrogen peroxide added.

[0034] In summary, first, 1200 kg of 3-cyanopyridine solution, water and sulfuric acid are added to the reactor, and then 10 kg of the catalyst is heated by a heater to make the catalyst temperature reach 37°C, which can maximize the activity of the catalyst and facilitate subsequent operations. The heated catalyst is then added to the reactor at multiple positions to allow the catalyst to fully diffuse and enhance the subsequent reaction effect, thereby improving the efficiency of N-oxide preparation. The reactor is then heated to 77°C-80°C by a heater, and hydrogen peroxide is slowly and evenly dripped into the reactor, wherein the hydrogen peroxide is an oxidant and the hydrogen peroxide is 35%. The reactor is shaken and stirred at the same time, and the time for dripping the hydrogen peroxide is controlled at 6 hours, and the amount of hydrogen peroxide dripped is 55% of the total amount of hydrogen peroxide to be dripped, and the temperature of the reactor is controlled at 77°C-80°C, and kept warm for 1 hour, and then hydrogen peroxide is continued to be dripped into the reactor, and the amount of hydrogen peroxide dripped is 45% of the total amount of hydrogen peroxide dripped, and the reactor is shaken and stirred at the same time, the hydrogen peroxide is added for 5 hours, and the temperature in the reactor is controlled at 77°C-80°C, and kept warm for 11 hours. By shaking and stirring the inside of the reactor when adding hydrogen peroxide twice, the hydrogen peroxide can be quickly diffused, thereby accelerating the reaction of hydrogen peroxide with the raw materials in the reactor, enhancing the effect of the oxidation reaction, and thereby improving the efficiency of N-oxide preparation. Finally, central control sampling is performed to obtain a finished product.

[0035] The embodiments of the present invention are provided for the purpose of illustration and description. Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A method for adding a catalyst dosage for the efficient and effective preparation of N-oxides, characterized in that: The following steps are included: S1, first add 1200kg 3-cyanopyridine solution, water and sulfuric acid into a reactor; S2, then prepare to add 10 kg of catalyst, and use a heater to heat the catalyst, and then add the heated catalyst into the reactor from multiple positions; S3, then the reactor is heated to 77°C-80°C by a heater, and hydrogen peroxide is slowly and evenly dripped into the reactor, and the reactor is shaken and stirred at the same time. The time for dripping hydrogen peroxide is controlled within 6 hours, and the temperature of the reactor is controlled at 77°C-80°C, and kept warm for 1 hour; S4, continue to drip hydrogen peroxide into S3, and at the same time, shake and stir the reactor. The dripping time of hydrogen peroxide is 5 hours, and the temperature in the reactor is controlled at 77°C-80°C, and kept warm for 11 hours; S5, central control sampling, to obtain the finished product.

2. The method for efficiently preparing N-oxide according to claim 1, characterized in that: In step S1, the solvent for dissolving 3-cyanopyridine is chloroform.

3. The method for efficiently preparing N-oxide according to claim 1, characterized in that: In step S1, the sulfuric acid is 35% dilute sulfuric acid.

4. The method for efficiently preparing N-oxide according to claim 1, characterized in that: In step S2, the heater needs to heat the catalyst to 37°C.

5. The method for efficiently preparing N-oxide according to claim 1, characterized in that: In step S3, the hydrogen peroxide is an oxidant, and the hydrogen peroxide is 35% hydrogen peroxide, and the amount of hydrogen peroxide dripped in is 55% of the total amount of hydrogen peroxide to be dripped in.

6. The method for efficiently preparing N-oxide according to claim 1, characterized in that: In step S4, the amount of hydrogen peroxide added is 45% of the total amount of hydrogen peroxide added.