Production process of aluminum alloy section
By embedding an organic-coated steel pipe in the groove of the aluminum alloy profile and processing the honing pattern, combined with nano-graphite powder, the problem of deformation and stress concentration of the aluminum alloy profile when carrying external loads is solved, and its strength and stability are significantly improved. Improved material match and fatigue resistance.
Patent Information
- Application Number
- CN202410898021.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-07-05
AI Technical Summary
Traditional aluminum alloy profiles are prone to deformation and warping when bearing external loads, and there are stress concentrations at corners and connection points, leading to breakage and failure. Existing composite molding solutions suffer from poor material matching and thermal expansion stress problems.
By embedding a steel pipe with an organic coating on the surface in the groove of the aluminum alloy profile, and fitting it with the bottom surface of the groove through a stamping mechanism, a core tube is formed. At the same time, honing patterns are processed in the groove and coated with nano-graphite powder. Enhance material adhesion and stress dispersion capabilities.
Significantly improves the strength and rigidity of aluminum alloy profiles, enhances resistance to deformation, improves matching between materials, avoids friction and looseness, and extends service life.
Smart Images

Figure CN118808367A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum profile processing, and in particular to a production process of aluminum alloy profiles. Background Art
[0002] Aluminum alloy profiles are widely used in door and window structures due to their advantages such as light weight, corrosion resistance and good processability. However, traditional aluminum alloy profiles still have the following shortcomings in practical applications: Although aluminum alloy profiles have excellent lightweight characteristics, their strength and rigidity are relatively weak. When bearing external loads (such as wind pressure, opening and closing forces), they are prone to deformation and warping, affecting the stability and sealing of doors and windows. In addition, stress concentration often occurs at the corners, connection points and stress-bearing wall thickness areas of aluminum alloy profiles, resulting in damage and failure of these parts in long-term use.
[0003] In response to the above defects, the prior art includes combining the aluminum alloy profile with other high-strength materials at the parts that need to be strengthened by composite molding, such as Chinese patent CN116809679A, which discloses a method of processing a steel pipe that interferes with the aluminum profile by stamping on the oblique side arm of the aluminum profile, thereby enhancing the impact resistance of the aluminum profile. However, this solution provides a new idea for improving the performance of aluminum profiles, but the solution still has some application difficulties, such as the poor matching effect between the surface of the steel pipe and the surface of the aluminum alloy profile. At the same time, the thermal expansion coefficients of aluminum alloy and steel are different, which may cause stress problems when the temperature changes, loose deformation between materials, electrochemical corrosion problems, etc.
[0004] In view of this, how to overcome the above problems and provide an aluminum alloy profile with better mechanical properties, good matching performance and good stability has become one of the technical problems that need to be solved urgently. Summary of the invention
[0005] In view of this, the present invention proposes a production process for aluminum alloy profiles, aiming to improve the structural strength and stability of the aluminum profiles through process improvement.
[0006] The technical solution of the present invention is achieved as follows: The present invention provides a production process of aluminum alloy profiles, and the process steps include:
[0007] Step 1: Extrusion mold the aluminum alloy ingot to obtain a long strip profile, wherein at least one side of the long strip profile has a groove along the length direction, and the width of the bottom of the groove is greater than the width of the groove opening;
[0008] Step 2: Cut the long strip profile obtained in step 1 according to the required length to obtain a single-segment profile;
[0009] Step three, insert a steel pipe with an organic coating on the surface into the groove of the single-section profile, and make the steel pipe fit with the bottom surface of the groove after being squeezed and deformed by a stamping mechanism to form a core tube inside the single-section profile, thereby obtaining an aluminum alloy profile.
[0010] In some embodiments, the organic coating layer includes a polyurethane layer, and the thickness of the organic coating layer is 100-400 μm.
[0011] In some embodiments, the organic coating further includes an epoxy layer, wherein the epoxy layer is located at the bottom of the polyurethane layer, and the thickness of the epoxy layer is 30-50 μm.
[0012] In some embodiments, in step 2, after obtaining the single-segment profile, the step further includes machining a honing pattern in the groove.
[0013] In some embodiments, the honing texture has a depth of 5-50 μm, a texture pitch of 50-100 μm, and a crossing angle of 20-45°.
[0014] In some embodiments, after the honing pattern is machined, the method further includes coating nano-graphite powder into the groove, wherein the particle size of the nano-graphite powder is 5-20 μm.
[0015] In some embodiments, the angle between the two side walls of the groove and the bottom surface is less than 90°.
[0016] In some embodiments, flanges are provided on both side walls of the groove, the distance between the flanges on both sides is smaller than the width of the groove opening, and the angle between the lower surface of the flange and the bottom surface of the groove is 30-45°.
[0017] In some embodiments, the cross-section of the steel pipe is circular, the outer diameter of the steel pipe does not exceed the distance between the flanges on both sides, and the distance between the end of the flange and the bottom surface of the groove is 1 / 2 of the radius of the steel pipe.
[0018] In some embodiments, the wall thickness of the steel tube does not exceed 1 mm.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] The present invention embeds a steel pipe inside the aluminum profile, thereby significantly improving the strength and rigidity of the profile, enhancing its ability to resist deformation when subjected to external loads, and improving the stability and load-bearing capacity of the aluminum profile. At the same time, an organic coating is applied to the surface of the steel pipe, effectively solving a new matching problem between the aluminum alloy and the steel pipe, and avoiding friction and looseness between the two materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0022] Figure 1 A cross-sectional view of an aluminum alloy profile according to one embodiment of the present invention;
[0023] Figure 2 A cross-sectional view of an aluminum alloy profile according to one embodiment of the present invention;
[0024] Figure 3 A schematic diagram of an aluminum alloy profile forming process according to one embodiment of the present invention;
[0025] Figure 4 This is a cross-sectional view of a steel pipe used in an aluminum alloy profile according to one embodiment of the present invention.
[0026] In the figure: 1-long strip profile, 11-groove, 2-steel pipe, 3-organic coating, 31-polyurethane layer, 32-epoxy layer, 12-flange. DETAILED DESCRIPTION
[0027] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0029] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0030] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those of ordinary skill in the art to which the embodiments of the present invention belong. If the definitions set forth in this section are contrary to or otherwise inconsistent with the definitions set forth in the patents, patent applications, published patent applications, and other publications incorporated herein by reference, the definitions listed in this section take precedence over the definitions incorporated herein by reference.
[0031] Unless otherwise specified, the methods used in the following examples are all conventional methods. Unless otherwise specified, the materials, reagents and instruments used are all conventional materials, reagents and instruments in the art, and can be obtained by those skilled in the art through commercial channels.
[0032] When an amount, concentration or other value or parameter is expressed as a range, a preferred range or a range defined by a series of upper preferred values and lower preferred values, this should be understood as specifically disclosing all ranges formed by any pairing of any range upper limit or preferred value with any range lower limit or preferred value, regardless of whether the range is disclosed separately. For example, when a range of "1 to 5" is disclosed, the described range should be interpreted as including the range "1 to 4", "1 to 3", "1 to 2", "1 to 2 and 4 to 5", "1 to 3 and 5", etc. When a numerical range is described herein, unless otherwise stated, the range is intended to include its end values and all integers and fractions within the range. In the present specification and claims, range definitions can be combined and / or interchanged, and if not otherwise stated, these ranges include all subranges contained therein.
[0033] like Figure 1 As shown, combined Figure 2-4 The production process of an aluminum alloy profile according to one embodiment of the present invention comprises the following steps:
[0034] S1, processing an aluminum alloy ingot by extrusion die molding to obtain a long strip profile 1, wherein at least one side surface of the long strip profile 1 is provided with a groove 11 along the length direction, and the width of the bottom surface of the groove 11 is greater than the opening width of the groove 11;
[0035] S2, cutting the long strip profile 1 obtained in S1 according to the required length to obtain a single-segment profile;
[0036] S3. A steel tube 2 having an organic coating 3 on its surface is inserted into the groove 11 of the single-section profile, and is deformed by extrusion by a punching mechanism, so that the steel tube 2 is attached to the bottom surface of the groove 11 and remains relatively fixed, thereby forming a core tube inside the single-section profile and obtaining an aluminum alloy profile.
[0037] In the above embodiment scheme, the opening width of the groove 11 is smaller than the bottom width. After extrusion and deformation by the stamping mechanism, the steel pipe 2 adapts to the shape of the bottom surface of the groove 11, and is thereby limited to the bottom surface of the groove 11. After stamping, the surface of the steel pipe 2 can be completely fitted with the bottom surface of the groove 11, thereby forming a composite structure to achieve the purpose of enhancing the mechanical strength of the aluminum alloy profile. Moreover, compared with the scheme of directly using a steel pipe in the prior art, the surface of the steel pipe 2 in the scheme of the present application has an organic coating 3. On the one hand, the organic coating 3 can play a role of elastic buffering to avoid stress concentration and loosening or over-tightening problems caused by thermal expansion. At the same time, it can also avoid friction between the two materials, extend the service life, and improve stability.
[0038] In some embodiments, the organic coating 3 includes a polyurethane layer 31 , and the thickness of the organic coating 3 is 100-400 μm.
[0039] In the above embodiment, the organic coating 3 not only increases the adhesion between the steel pipe and the aluminum alloy profile, but also provides a buffer layer, effectively solving the stress problem caused by the different thermal expansion coefficients of the two materials. The coating thickness of 100-400 μm ensures sufficient buffering and protection.
[0040] In some embodiments, the organic coating 3 further includes an epoxy layer 32 , and the epoxy layer 32 is located at the bottom of the polyurethane layer 31 . The thickness of the epoxy layer 32 is 30-50 μm.
[0041] In the above embodiments, the epoxy layer 32 is used to provide a transition structure. The bonding force between the epoxy layer 32 and the steel is stronger. As a base layer, the bonding force between the organic coating 3 and the steel pipe 2 can be higher, and the adhesion effect of the organic coating 3 is better and more stable.
[0042] In some embodiments, in step 2, after obtaining the single-segment profile, the process further includes machining a honing pattern in the groove 11 .
[0043] In the above embodiments, by processing the honing texture on the inner surface of the groove 11, stress concentration can be significantly reduced, and the contact strength and fatigue resistance of the material surface can be improved. These honing textures can significantly increase the surface area of the inner surface of the groove 11, thereby expanding the stress distribution area and reducing the stress value in the local stress concentration area. Moreover, by processing the honing texture, regular texture paths can be formed on the inner surface of the groove 11. These texture paths can change the stress path and reduce the peak stress at the stress concentration point. Moreover, the textured surface provides more adhesion points, thereby improving the bonding strength between the organic coating 3 and the groove 11. This adhesion effect will also reduce the destructive effect of the stamping deformation on the organic coating 3 in step S3. Moreover, the honing texture can also eliminate the tiny defects on the inner surface of the groove 11 after extrusion molding, thereby reducing the stress concentration points. Moreover, the complex surface morphology brought by the honing texture requires more energy to be consumed during the subsequent crack expansion process, thereby slowing down the crack expansion rate.
[0044] In some embodiments, the honing texture has a depth of 5-50 μm, a texture pitch of 50-100 μm, and a crossing angle of 20-45°.
[0045] After optimizing the process parameters of the honing pattern, the above-mentioned preferred parameter values are obtained. The depth of 5-50μm is suitable for surface processing and can provide obvious stress dispersion effect. The texture spacing of 50-100μm is more suitable for the use conditions of aluminum profiles; the cross angle of 20-45° brings a certain complexity and stress dispersion effect to the texture, which is conducive to enhancing fatigue resistance.
[0046] In some embodiments, after the honing lines are machined, the process further includes coating nano graphite powder into the groove 11, wherein the particle size of the nano graphite powder is 5-20 μm, and after coating, the nano graphite powder on the surface is purged and removed.
[0047] In the above embodiments, nano-graphite powder is mainly used to fill the texture grooves of the honing lines. This operation can make the grooves 11 still have a relatively smooth appearance surface after the honing lines are processed, thereby reducing the wear between the organic coating 3 and the honing lines due to deformation or load. At the same time, the nano-graphite powder has a certain self-lubricating effect, further reducing the friction loss. During the relative sliding process between the organic coating 3 and the grooves 11, the nano-graphite powder helps to form a uniform base coating film at the interface, which can not only further improve the adaptive stress dispersion, but also protect the aluminum alloy surface.
[0048] In some embodiments, the angle formed between the two side walls and the bottom surface of the groove 11 is less than 90°.
[0049] In the above embodiments, the angles of the two side walls of the groove 11 are limited to acute angles, so that the steel pipe 2 after extrusion and bonding can be closely attached to the bottom surface of the groove 11 after the size is determined in advance, so as to maintain structural stability.
[0050] In some embodiments, flanges 12 are provided on both side walls of the groove 11, the distance between the flanges 12 on both sides is smaller than the opening width of the groove 11, and the angle between the lower surface of the flange 12 and the bottom surface of the groove 11 is 30-45°.
[0051] In the above embodiments, the function of the flange 12 is to limit and guide the extrusion forming of the steel pipe 2 , and further limit the position of the extruded steel pipe 2 to maintain the stability of the steel pipe 2 .
[0052] In some embodiments, the cross-section of the steel pipe 2 is circular, the outer diameter of the steel pipe 2 does not exceed the distance between the flanges 12 on both sides, and the distance between the end of the flange 12 and the bottom surface of the groove is 1 / 2 of the radius of the steel pipe.
[0053] The flange size and position of the above embodiment are conducive to filling the space between the bottom of the flange 12 and the bottom surface of the groove 11 during the extrusion of the steel pipe 2, thereby avoiding unexpected deformation of the steel pipe 2 during extrusion.
[0054] In some embodiments, the wall thickness of the steel pipe 2 does not exceed 1 mm.
[0055] In the above embodiments, the steel pipe 2 needs to have a relatively stable and predictable deformation ability, so the thickness should not be too large. At the same time, the strength improvement effect of the steel pipe 2 mainly depends on its structure. Too much thickness is not conducive to the lightweight of the aluminum alloy. Therefore, the optimal thickness does not exceed 1 mm, preferably 0.1-0.8 mm, and more preferably 0.4 mm.
[0056] Example 1
[0057] This embodiment provides an aluminum alloy profile, the structure of which is as follows Figure 1 shown.
[0058] The organic coating 3 prepared by the above method includes a 30 μm epoxy layer 32 and a 70 μm polyurethane layer 31 , and does not include honing marks and graphite powder.
[0059] Example 2
[0060] This embodiment provides an aluminum alloy profile, the structure of which is as follows Figure 1 shown.
[0061] The organic coating 3 prepared by the above method includes a 30 μm epoxy layer 32 and a 70 μm polyurethane layer 31, and also includes honing textures. The honing texture parameters are: depth of 30 μm, texture spacing of 60 μm, and intersection angle of 30°.
[0062] Example 3
[0063] This embodiment provides an aluminum alloy profile, the structure of which is as follows Figure 1 shown.
[0064] The method is used to prepare an organic coating 3, which includes a 30μm epoxy layer 32 and a 70μm polyurethane layer 31, and also includes honing textures. The honing texture parameters are: depth of 30μm, texture spacing of 60μm, and intersection angle of 30°. At the same time, the texture is rich in nano-graphite powder with a particle size of 15μm.
[0065] Example 4
[0066] This embodiment provides an aluminum alloy profile, the structure of which is as follows Figure 2 shown.
[0067] The organic coating 3 prepared by the above method includes a 30 μm epoxy layer 32 and a 70 μm polyurethane layer 31 , and does not include honing marks and graphite powder.
[0068] Comparative Example
[0069] The difference from Example 1 is that the surface of the steel pipe 2 does not have the organic coating 3 .
[0070] The above-mentioned embodiment and comparative example were subjected to bending modulus and bending fatigue tests respectively, and the test results of the embodiment were compared with the results of the comparative example, and the data shown in the following table were obtained:
[0071] Grouping Comparative Example Example 1 Example 2 Example 3 Example 4 Flexural modulus increment / % 0 1.5 6.6 6.5 2.4 Bending fatigue increment / % 0 10.8 18.4 22.9 10.6
[0072] It is not difficult to see that the present application uses an organic coated steel pipe for extrusion and compounding, which significantly improves the bending fatigue effect of the profile, and the bending modulus is also improved to a certain extent. While adding the organic coating, processing the honing pattern on the inner surface of the groove 11 can significantly improve the bending of the wooden beam and the bending fatigue effect. After being combined with nano-graphite powder, the effect is even better. After setting the flange, it also brings a certain improvement in the mechanical effect.
[0073] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A production process for aluminum alloy profiles, characterized in that: The steps include: Step 1: Extrusion mold the aluminum alloy ingot to obtain a long strip profile, wherein at least one side of the long strip profile has a groove along the length direction, and the width of the bottom of the groove is greater than the width of the groove opening; Step 2: Cut the long strip profile obtained in step 1 according to the required length to obtain a single-segment profile; Step three, insert a steel pipe with an organic coating on the surface into the groove of the single-section profile, and make the steel pipe fit with the bottom surface of the groove after being squeezed and deformed by a stamping mechanism to form a core tube inside the single-section profile, thereby obtaining an aluminum alloy profile.
2. The production process of aluminum alloy profiles according to claim 1, characterized in that: The organic coating layer comprises a polyurethane layer, and the thickness of the organic coating layer is 100-400 μm.
3. The production process of aluminum alloy profiles according to claim 2, characterized in that: The organic coating layer also includes an epoxy layer, which is located at the bottom of the polyurethane layer and has a thickness of 30-50 μm.
4. The production process of the aluminum alloy profile according to claim 2, characterized in that: In step 2, after obtaining the single-segment profile, the step further includes machining a honing pattern in the groove.
5. The production process of the aluminum alloy profile according to claim 4, characterized in that: The depth of the honing pattern is 5-50 μm, the texture spacing is 50-100 μm, and the crossing angle is 20-45°.
6. The production process of the aluminum alloy profile according to claim 4, characterized in that: After the honing lines are machined, the method further includes coating nano graphite powder into the grooves, wherein the particle size of the nano graphite powder is 5-20 μm.
7. The production process of the aluminum alloy profile according to claim 1, characterized in that: The angle formed between the two side walls of the groove and the bottom surface is less than 90°.
8. The production process of the aluminum alloy profile according to claim 7, characterized in that: Both side walls of the groove are provided with flanges, the distance between the flanges on both sides is smaller than the opening width of the groove, and the angle between the lower surface of the flange and the bottom surface of the groove is 30-45°.
9. The production process of the aluminum alloy profile according to claim 8, characterized in that: The cross section of the steel pipe is circular, the outer diameter of the steel pipe does not exceed the distance between the flanges on both sides, and the distance between the end of the flange and the bottom surface of the groove is 1 / 2 of the radius of the steel pipe.
10. The production process of aluminum alloy profiles according to claim 1, characterized in that: The wall thickness of the steel pipe does not exceed 1 mm.
Citation Information
Patent Citations
Production process of reinforced aluminum alloy section
CN116809679A
Bimetal composite radiator capable of reducing friction abnormal sound and preparation method thereof
CN113108642A
Aluminum-steel composite profile and processing technology thereof
CN113843296A
High-strength building aluminum alloy
CN212866604U
Aluminum alloy member for different material joining, different material joining member, and different material joining method