Crystallizer liquid level fluctuation suppression device and continuous casting equipment
By arranging long side and short side baffles under the liquid level of the mold, the flow direction of the molten steel is changed, the problem of liquid level fluctuation in high-speed continuous casting is solved, and the quality of the slab and the efficiency of slag removal are improved.
Patent Information
- Application Number
- CN202410908672.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2024-10-22
AI Technical Summary
In high-speed continuous casting technology, frequent fluctuations in the steel slag liquid level lead to slag entrainment and cracks on the surface of the cast slab, which affects the quality of the cast slab.
A pair of long side baffles and a pair of short side baffles are installed at the lower part of the crystallizer liquid level to change the flow direction of the upward return flow of molten steel, suppress the impact of molten steel on the steel slag interface, and prevent liquid level fluctuations.
It effectively avoids violent fluctuations in the liquid level, improves the uniformity of the steel slag interface flow rate, improves the slag removal efficiency and the quality of the cast slab.
Smart Images

Figure CN118808581A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of metal casting, and specifically relates to a device for suppressing liquid level fluctuation of a crystallizer and a continuous casting device. Background Art
[0002] High-speed continuous casting technology can achieve higher production efficiency and lower energy consumption, and is a concrete manifestation of the efficiency and greenness of the steel production process. However, the biggest challenge facing high-speed continuous casting technology is the frequent fluctuations in the slag level and the frequent cracks on the surface of the ingot. The violent fluctuations in the slag level can cause slag curling, which in turn affects the normal consumption of the protective slag and causes quality problems such as cracks on the edges, corners and surfaces of the ingot.
[0003] The crystallizer, as the "heart" of continuous casting, is a continuous casting device that receives the molten steel injected from the tundish and solidifies it into a solid shell according to a specific cross-sectional shape. The flow state of the molten steel in the crystallizer and the consumption of protective slag have a huge impact on the quality of the ingot. Under high-speed continuous casting conditions, the molten steel stream flows out from the submerged nozzle at high speed, and forms upper and lower refluxes after impacting the inner wall of the crystallizer. The upper reflux impacts the steel-slag interface, causing violent fluctuations in the interface, resulting in slag rolling, affecting the normal consumption of protective slag, and causing defects in the ingot. Therefore, how to ensure the stability of the liquid level in the slab continuous casting crystallizer under high-speed conditions is the key to achieving high-speed continuous casting. Summary of the invention
[0004] Therefore, the technical problem to be solved by the present application is to provide a device for suppressing the liquid level fluctuation of the crystallizer and a continuous casting equipment. By arranging a pair of long side baffles and a pair of short side baffles at the lower part of the liquid level of the crystallizer, the flow direction of the molten steel flowing back upward can be changed, thereby suppressing the molten steel flowing back upward from impacting the steel-slag interface and preventing the occurrence of crystallizer liquid level fluctuations.
[0005] In order to solve the above-mentioned problems, one aspect of the present application provides a crystallizer liquid level fluctuation suppression device for resisting the impact of molten steel on the crystallizer liquid level. The crystallizer liquid level fluctuation suppression device includes a pair of long side baffles and a pair of short side baffles. The pair of long side baffles and the pair of short side baffles can be raised and lowered at the lower part of the crystallizer liquid level so that the molten steel flowing back upward is located in the projection area of the pair of long side baffles and the pair of short side baffles. The pair of long side baffles and the pair of short side baffles are used to change the flow direction of the molten steel flowing back upward.
[0006] Optionally, the bottom surfaces of the long side baffles and the short side baffles are arc-shaped, and the central angle corresponding to the arc is α, 10°≤α≤30°.
[0007] Optionally, the long side baffles and the short side baffles are inclined in a direction away from the protective slag layer, and an inclination angle of the long side baffles and the short side baffles relative to a horizontal plane is β, 3°≤β≤10°.
[0008] Optionally, the tail ends of the long side baffles and the short side baffles are rounded structures, and the radius of the rounded structures is R, 3mm≤R≤7mm.
[0009] Optionally, the length of the long side baffle is n, 3 / 4N≤n≤N, N is the width of the casting billet;
[0010] The length of the short side baffle is d, 1 / 2D≤d≤D, and D is the thickness of the casting.
[0011] Optionally, the width of the long side baffle and the short side baffle is k, 15mm≤k≤300mm;
[0012] The thickness of the long side baffles and the short side baffles is h, 5mm≤h≤30mm.
[0013] Optionally, the crystallizer liquid level fluctuation suppression device further includes a long side lifting assembly and a short side lifting assembly;
[0014] The long side lifting assembly comprises a long side screw, a long side nut and a long side connecting plate, wherein the long side screw is arranged at the upper opening of the crystallizer, at least two long side nuts are arranged, at least two of the long side nuts are sleeved on the long side screw and are threadedly connected with the long side screw, one end of the long side connecting plate is arranged between at least two of the long side nuts, and the other end of the long side connecting plate is relatively fixed to the long side baffle;
[0015] The short side lifting assembly includes a short side screw, a short side nut and a short side connecting plate. The short side screw is arranged at the upper mouth of the crystallizer. At least two short side nuts are arranged. At least two short side nuts are sleeved on the short side screw and threadedly connected to the short side screw. One end of the short side connecting plate is arranged between at least two short side nuts, and the other end of the short side connecting plate is relatively fixed to the short side baffle.
[0016] Optionally, at least two long side lifting assemblies are provided, and at least two long side lifting assemblies are arranged relatively along the length direction of the long side baffle.
[0017] Optionally, the long side baffle and the short side baffle are made of niobium-based high-temperature alloy.
[0018] Another aspect of the present application provides a continuous casting device, comprising the device for suppressing the liquid level fluctuation of the crystallizer as described in any one of the above.
[0019] Beneficial Effects
[0020] An embodiment of the present invention provides a crystallizer liquid level fluctuation suppression device and a continuous casting device, wherein the crystallizer liquid level fluctuation suppression device can change the flow direction of the molten steel flowing back upward by arranging a pair of long side baffles and a pair of short side baffles at the lower part of the crystallizer liquid level, thereby suppressing the upwardly flowing molten steel from impacting the slag interface and preventing the occurrence of crystallizer liquid level fluctuations; at the same time, changing the flow direction of the upwardly flowing molten steel can avoid slag rolling caused by violent fluctuations of the liquid level, improve the uniformity of the flow velocity at the slag interface, thereby improving the slag-melting efficiency, which is beneficial to improving the quality of the ingot. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 This is a schematic structural diagram of a device for suppressing liquid level fluctuations in a crystallizer according to an optional embodiment of the present application;
[0022] Figure 2 A top view of a device for suppressing liquid level fluctuation of a crystallizer according to an optional embodiment of the present application;
[0023] Figure 3 This is a schematic structural diagram of a long side baffle of an optional embodiment of the present application;
[0024] Figure 4 A side view of a long side baffle of an optional embodiment of the present application;
[0025] Figure 5 This is a schematic structural diagram of a short side baffle of an optional embodiment of the present application;
[0026] Figure 6 A side view of a short side baffle of an optional embodiment of the present application;
[0027] Figure 7 This is the internal flow field diagram of a traditional crystallizer;
[0028] Figure 8 This is the slag interface velocity cloud diagram of the traditional crystallizer;
[0029] Fig. 9 This is a cloud diagram of the liquid level fluctuation amplitude of a traditional crystallizer;
[0030] Fig.10 For application Figure 1 The internal flow field diagram of the crystallizer of the crystallizer liquid level fluctuation suppression device shown;
[0031] Fig.11 For application Figure 1 The slag interface velocity cloud diagram of the crystallizer of the crystallizer liquid level fluctuation suppression device shown;
[0032] Fig.12 For application Figure 1 The cloud diagram of the liquid level fluctuation amplitude of the crystallizer of the crystallizer liquid level fluctuation suppression device is shown.
[0033] The reference numerals are:
[0034] 1. Long side baffle; 2. Short side baffle; 3. Long side lifting assembly; 31. Long side screw rod; 32. Long side nut; 33. Long side connecting plate; 4. Short side lifting assembly; 41. Short side screw rod; 42. Short side nut; 43. Short side connecting plate; 5. Long side working plate; 6. Long side cooling plate; 7. Short side working plate; 8. Short side cooling plate. DETAILED DESCRIPTION
[0035] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0036] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0037] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0038] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0039] See also Figures 1 to 12As shown, according to one aspect of an embodiment of the present application, a device for suppressing liquid level fluctuations in a crystallizer is provided, which is used to resist the impact of molten steel on the protective slag layer. The device for suppressing liquid level fluctuations in a crystallizer includes a pair of long side baffles 1 and a pair of short side baffles 2. The pair of long side baffles 1 and the pair of short side baffles 2 can be raised and lowered at the lower part of the crystallizer liquid surface, so that the molten steel flowing back upward is located within the projection area of the pair of long side baffles 1 and the pair of short side baffles 2. The pair of long side baffles 1 and the pair of short side baffles 2 are used to change the flow direction of the molten steel flowing back upward.
[0040] The crystallizer liquid level fluctuation suppression device provided in the embodiment of the present application can change the flow direction of the upwardly reflowing molten steel by arranging a pair of long side baffles 1 and a pair of short side baffles 2 at the lower part of the crystallizer liquid level, thereby suppressing the upwardly reflowing molten steel from impacting the slag interface and preventing the occurrence of crystallizer liquid level fluctuations; at the same time, changing the flow direction of the upwardly reflowing molten steel can avoid slag rolling caused by violent fluctuations of the liquid level, improve the uniformity of the flow velocity at the slag interface, thereby improving the slag-melting efficiency, which is beneficial to improving the quality of the ingot.
[0041] Among them, the crystallizer liquid level fluctuation suppression device includes a pair of long side baffles 1, which each extend in one direction and are spaced apart from each other in a direction intersecting or perpendicular to the extension direction; and a pair of short side baffles 2, which each extend in a direction intersecting or perpendicular to the long side baffles 1 and are spaced apart from each other in a direction intersecting or perpendicular to the extension direction.
[0042] Specifically, in the embodiment of the present application, the extension direction of the pair of long side baffles 1 is perpendicular to the extension direction of the pair of short side baffles 2. For example, the extension direction of the pair of long side baffles 1 is defined as the X-axis direction, and the extension direction of the pair of short side baffles 2 is the Y-axis direction. At this time, the pair of long side members are spaced apart in the Y-axis direction, and the pair of short side members are spaced apart in the X-axis direction.
[0043] As an embodiment, a pair of long side baffles 1 is located between a pair of spaced short side baffles 2; as another embodiment, a pair of short side baffles 2 is located between a pair of spaced long side baffles 1. In the embodiment of the present application, a pair of long side baffles 1 is located between a pair of spaced short side baffles 2.
[0044] The inner cavity of the crystallizer has a protective slag layer, which is a slag layer formed by powdered or granular slag added to the surface of the molten steel in the crystallizer during the continuous casting process. The protective slag layer can insulate heat, prevent secondary oxidation of molten steel, absorb and dissolve inclusions, reduce billet drawing resistance and improve heat transfer in the crystallizer.
[0045] The contact surface between the protective slag layer and the molten steel is the slag interface, and a pair of long side baffles 1 and a pair of short side baffles 2 are arranged at the slag interface or below the slag interface to resist the impact of the molten steel on the crystallizer liquid surface. Figure 7 As shown, as the continuous casting speed increases, the flow rate of the molten steel flowing into the inner cavity of the crystallizer from the submerged water inlet increases, and part of the molten steel flowing back upward will impact the steel-slag interface, resulting in frequent liquid level fluctuations and causing slag rolling.
[0046] Specifically, a pair of long side baffles 1 and a pair of short side baffles 2 are arranged on the flow path of the upwardly reflowing molten steel to intercept the upwardly reflowing molten steel, thereby inhibiting the upwardly reflowing molten steel from impacting the slag interface and preventing the occurrence of crystallizer liquid level fluctuations.
[0047] As an embodiment, a pair of long side baffles 1 and a pair of short side baffles 2 are perpendicular to the flow direction of the molten steel flowing back upwards; as another embodiment, a pair of long side baffles 1 and a pair of short side baffles 2 intersect with the flow direction of the molten steel flowing back upwards. In the embodiment of the present application, a pair of long side baffles 1 and a pair of short side baffles 2 intersect with the flow direction of the molten steel flowing back upwards, and a pair of long side baffles 1 and a pair of short side baffles 2 can change the flow direction of the molten steel flowing back upwards.
[0048] Among them, a pair of long side baffles 1 and a pair of short side baffles 2 are arranged in a liftable manner in the inner cavity of the crystallizer. By arranging a pair of long side baffles 1 and a pair of short side baffles 2 to be liftable in the inner cavity of the crystallizer, the height of the pair of long side baffles 1 and the pair of short side baffles 2 can be adjusted to meet the requirements of different crystallizers for different heights of the pair of long side baffles 1 and the pair of short side baffles 2, thereby improving the user experience.
[0049] The inner cavity of the crystallizer may be formed by a pair of long side working plates 5 and a pair of short side working plates 7. The long side working plates 5 may be wide copper plates in contact with the solidified shell, and the short side working plates 7 may be narrow copper plates in contact with the solidified shell.
[0050] Among them, a long side cooling plate 6 can be provided on the side of the long side working plate 5 away from the solidified blank shell, and the long side cooling plate 6 can be fixed to the back of the long side working plate 5 by bolt connection, and a long side cooling water trough is formed between the long side cooling plate 6 and the long side working plate 5 for passing cooling water to bring out the heat of the long side working plate 5; a short side cooling plate 8 can be provided on the side of the short side working plate 7 away from the solidified blank shell, and the short side cooling plate 8 can also be fixed to the back of the short side working plate 7 by bolt connection, and a short side cooling water trough is formed between the short side cooling plate 8 and the short side working plate 7 for passing cooling water to bring out the heat of the short side working plate 7.
[0051] Specifically, the long side baffle plate 1 is arranged close to the working surface of the long side working plate 5, which can prevent the molten steel from flowing back upwards and impacting the steel-slag interface along the long side working plate 5; the short side baffle plate 2 is arranged close to the working surface of the short side working plate 7, which can prevent the molten steel from flowing back upwards and impacting the steel-slag interface along the short side working plate 7.
[0052] Among them, the long side baffle 1 is connected to the long side working plate 5 and / or the long side cooling plate 6 through a lifting assembly, so that the height of the long side baffle 1 in the inner cavity of the crystallizer is adjustable; the short side baffle 2 is connected to the short side working plate 7 and / or the short side cooling plate 8 through a lifting assembly, so that the height of the short side baffle 2 in the inner cavity of the crystallizer is adjustable.
[0053] Specifically, the lifting assembly can be a hydraulic lifting assembly, which drives the movement of the piston or plunger through the pressure of hydraulic oil to achieve the lifting function; or, a screw-nut lifting assembly, which is composed of a screw and a nut matching it, and the rotation of the screw drives the nut to move along the axial direction of the screw, thereby achieving lifting; or, a gear and rack lifting assembly, which utilizes the meshing transmission of the gear and the rack to convert the rotational motion of the gear into the linear motion of the rack to achieve lifting; or, a chain and sprocket lifting assembly, which relies on the transmission of the chain on the sprocket to drive the movement of the lifting component.
[0054] Among them, in the embodiment of the present application, the lifting assembly is a screw nut lifting assembly. By setting the lifting assembly as a screw nut lifting assembly, it is convenient to assemble and disassemble the long side baffle 1 and the short side baffle 2; at the same time, there is no need to carry out large-scale transformation of the original crystallizer, and only bolt holes need to be opened at the top surface of the crystallizer. The equipment transformation cost is low and it is suitable for slab blanks of full cross-sectional size.
[0055] For details, see Figures 1 to 6As shown, the lifting assembly includes a long side lifting assembly 3 and a short side lifting assembly 4; the long side lifting assembly 3 includes a long side screw rod 31, a long side nut 32 and a long side connecting plate 33, the long side screw rod 31 is arranged on the top of the long side cooling plate 6, two long side nuts 32 are arranged, the two long side nuts 32 are sleeved on the long side screw rod 31 and are screwed with the long side screw rod 31, the long side connecting plate 33 is L-shaped, one end of the long side connecting plate 33 is arranged between the two long side nuts 32, and the other end of the long side connecting plate 33 is L-shaped. One end is relatively fixed to the long side baffle 1; the short side lifting assembly 4 includes a short side screw rod 41, a short side nut 42 and a short side connecting plate 43. The short side screw rod 41 is arranged on the top of the short side cooling plate 8. Two short side nuts 42 are arranged. The two short side nuts 42 are sleeved on the short side screw rod 41 and are screwed with the short side screw rod 41. The short side connecting plate 43 is L-shaped. One end of the short side connecting plate 43 is arranged between the two short side nuts 42, and the other end of the short side connecting plate 43 is relatively fixed to the short side baffle 2.
[0056] In some possible implementations provided in this application, see Figures 1 to 3 As shown, at least two long side lifting assemblies 3 are provided, and at least two long side lifting assemblies 3 are arranged opposite to each other along the length direction of the long side baffle 1. By providing at least two long side lifting assemblies 3, the height of the long side baffle 1 can be stably adjusted, and the long side baffle 1 can be prevented from shaking during operation, thereby improving the stability of the crystallizer liquid level.
[0057] Among them, two, three or four long side lifting assemblies 3 can be provided, and this application does not make further limitations. It can be understood that when more than two long side lifting assemblies 3 are provided, the production cost of the crystallizer liquid level fluctuation suppression device will increase.
[0058] Specifically, in the embodiment of the present application, two long side lifting assemblies 3 are provided, the two long side lifting assemblies 3 are arranged opposite to each other along the length direction of the long side baffle 1, and the two long side lifting assemblies 3 are at the same distance from the symmetry center of the long side baffle 1.
[0059] In some possible implementations provided in this application, see Figure 4 and Figure 6As shown, the long side baffle 1 and the short side baffle 2 are inclined in the direction away from the protective slag layer, and the inclination angle of the long side baffle 1 and the short side baffle 2 relative to the horizontal plane is β, 3°≤β≤10°. By setting the long side baffle 1 and the short side baffle 2 to be inclined in the direction away from the protective slag layer, the molten steel flowing back upward can be guided away from the protective slag layer, which can effectively prevent the molten steel flowing back upward from impacting the slag interface, causing the liquid level to fluctuate violently and cause slag rolling, and improve the stability of the crystallizer liquid level fluctuation; at the same time, the design of the long side baffle 1 and the short side baffle 2 being inclined in the direction away from the protective slag layer can avoid the occurrence of shear slag rolling at the slag interface, and after the flow stream changes direction, the uniformity of the flow velocity at the slag interface can be improved, which is beneficial to the melting of the protective slag and improves the slag melting efficiency. It can be understood that the improvement of the slag melting efficiency can promote the consumption of protective slag, improve the lubrication and heat transfer effects of the protective slag, and improve the uniformity and quality of the solidified shell.
[0060] Wherein, when the protective slag layer is a horizontal plane, the inclination angle β of the long side baffle 1 and the short side baffle 2 relative to the protective slag layer can be 3° to 10°. For example, the inclination angle of the long side baffle 1 and the short side baffle 2 relative to the protective slag layer is 3°, or 4°, or 5°, or 6°, or 7°, or 8°, or 9°, or 10°. It can be understood that the inclination angle of the long side baffle 1 and the short side baffle 2 relative to the protective slag layer can also be other values in addition to the above values, as long as the inclination angle of the long side baffle 1 and the short side baffle 2 relative to the protective slag layer is 3° to 10°.
[0061] In some possible implementations provided in this application, see Figure 4 and Figure 6 As shown, the bottom surfaces of the long side baffle 1 and the short side baffle 2 are arc-shaped, and the central angle corresponding to the arc is α, 10°≤α≤30°. By setting the bottom surfaces of the long side baffle 1 and the short side baffle 2 to be arc-shaped, the flow direction of the molten steel flowing back upward can be smoothly changed, and the fluctuation of the liquid level can be reduced.
[0062] Among them, the central angle of the arc-shaped bottom surface of the long side baffle 1 and the short side baffle 2 is 10° to 30°. For example, the central angle of the arc-shaped bottom surface of the long side baffle 1 and the short side baffle 2 is 10°, or 11°, or 12°, or 13°, or 14°, or 15°, or 16°, or 17°, or 18°, or 19°, or 20°, or 21°, or 22°, or 23°, or 24°, or 25°, or 26°, or 27°, or 28°, or 29°, or 30°. It can be understood that the central angle of the arc-shaped bottom surface of the long side baffle 1 and the short side baffle 2 can also be other values in addition to the above values, as long as the central angle of the arc-shaped bottom surface of the long side baffle 1 and the short side baffle 2 is 10° to 30°.
[0063] In some possible implementations provided in this application, see Figure 4 and Figure 6 As shown, the tail ends of the long side baffle 1 and the short side baffle 2 are rounded structures, and the radius of the rounded structure is R, 3mm≤R≤7mm. By setting the tail ends of the long side baffle 1 and the short side baffle 2 as rounded structures, the flow direction of the molten steel flowing back upward can be smoothly changed, so that the molten steel flow field is stable.
[0064] The tail ends of the long side baffle 1 and the short side baffle 2 may be ends away from the installation position.
[0065] The radius of the rounded corner structure at the tail end of the long side baffle 1 and the short side baffle 2 is 3mm to 7mm. For example, the radius of the rounded corner structure at the tail end of the long side baffle 1 and the short side baffle 2 is 3mm, or 4mm, or 5mm, or 6mm, or 7mm. It can be understood that the radius of the rounded corner structure at the tail end of the long side baffle 1 and the short side baffle 2 can also be other values besides the above values, as long as the radius of the rounded corner structure at the tail end of the long side baffle 1 and the short side baffle 2 is 3mm to 7mm.
[0066] In some possible embodiments provided in the present application, the length of the long side baffle 1 is n, 3 / 4N≤n≤N, N is the width of the ingot; the length of the short side baffle 2 is d, 1 / 2D≤d≤D, D is the thickness of the ingot.
[0067] The width of the ingot is the width of the inner cavity of the crystallizer.
[0068] Among them, the thickness of the ingot is also the thickness of the inner cavity of the crystallizer.
[0069] Specifically, taking the case where the width of the ingot is 1100 mm and the thickness of the ingot is 240 mm as an example, the length of the long side baffle 1 is 825 mm to 1100 mm, and the length of the short side baffle 2 is 120 mm to 240 mm.
[0070] In some possible embodiments provided in the present application, the width of the long side baffle 1 and the short side baffle 2 is k, 15mm≤k≤300mm; the thickness of the long side baffle 1 and the short side baffle 2 is h, 5mm≤h≤30mm.
[0071] The width of the long side baffle 1 is 15 mm to 300 mm. For example, the width of the long side baffle 1 is 15 mm, or 34 mm, or 53 mm, or 72 mm, or 91 mm, or 110 mm, or 129 mm, or 148 mm, or 167 mm, or 186 mm, or 105 mm, or 224 mm, or 243 mm, or 262 mm, or 281 mm, or 300 mm. It can be understood that the width of the long side baffle 1 can also be other values besides the above values, as long as the width of the long side baffle 1 is 15 mm to 300 mm.
[0072] The width of the short side baffle 2 is 15 mm to 300 mm. For example, the width of the short side baffle 2 is 15 mm, or 34 mm, or 53 mm, or 72 mm, or 91 mm, or 110 mm, or 129 mm, or 148 mm, or 167 mm, or 186 mm, or 105 mm, or 224 mm, or 243 mm, or 262 mm, or 281 mm, or 300 mm. It can be understood that the width of the short side baffle 2 can also be other values in addition to the above values, as long as the width of the short side baffle 2 is 15 mm to 300 mm.
[0073] Specifically, as an embodiment, the width of the short side baffle 2 is greater than the width of the long side baffle 1; as another embodiment, the width of the short side baffle 2 is less than the width of the long side baffle 1; as yet another embodiment, the width of the short side baffle 2 is the same as the width of the long side baffle 1. In the embodiment of the present application, the width of the short side baffle 2 is greater than the width of the long side baffle 1, which is conducive to resisting the large flow of molten steel flowing back upward along the short side working plate 7.
[0074] The thickness of the long side baffle 1 is 5 mm to 30 mm. For example, the width of the long side baffle 1 is 5 mm, or 6 mm, or 7 mm, or 8 mm, or 9 mm, or 10 mm, or 11 mm, or 12 mm, or 13 mm, or 14 mm, or 15 mm, or 16 mm, or 17 mm, or 18 mm, or 19 mm, or 20 mm, or 21 mm, or 22 mm, or 23 mm, or 24 mm, or 25 mm, or 26 mm, or 27 mm, or 28 mm, or 29 mm, or 30 mm. It can be understood that the thickness of the long side baffle 1 can also be other values besides the above values, as long as the thickness of the long side baffle 1 is 5 mm to 30 mm.
[0075] The thickness of the short side baffle 2 is 5 mm to 30 mm. For example, the width of the short side baffle 2 is 5 mm, or 6 mm, or 7 mm, or 8 mm, or 9 mm, or 10 mm, or 11 mm, or 12 mm, or 13 mm, or 14 mm, or 15 mm, or 16 mm, or 17 mm, or 18 mm, or 19 mm, or 20 mm, or 21 mm, or 22 mm, or 23 mm, or 24 mm, or 25 mm, or 26 mm, or 27 mm, or 28 mm, or 29 mm, or 30 mm. It can be understood that the thickness of the short side baffle 2 can also be other values besides the above values, as long as the thickness of the short side baffle 2 is 5 mm to 30 mm.
[0076] Specifically, as an embodiment, the thickness of the short side baffle 2 is greater than the thickness of the long side baffle 1; as another embodiment, the thickness of the short side baffle 2 is less than the thickness of the long side baffle 1; as yet another embodiment, the thickness of the short side baffle 2 is the same as the thickness of the long side baffle 1. In the embodiment of the present application, the thickness of the short side baffle 2 is greater than the thickness of the long side baffle 1, which is conducive to resisting the large flow of molten steel flowing back upward along the short side working plate 7.
[0077] In some possible embodiments provided in the present application, the long side baffle 1 and the short side baffle 2 are made of niobium-based high-temperature alloy. By making the long side baffle 1 and the short side baffle 2 of niobium-based high-temperature alloy, the heat resistance of the long side baffle 1 and the short side baffle 2 can be improved, so that they maintain good mechanical properties in a high-temperature environment, thereby improving the stability of the crystallizer liquid level.
[0078] The long side connecting plate 33 and the short side connecting plate 43 may also be made of niobium-based high temperature alloy.
[0079] Another aspect of an embodiment of the present application provides a continuous casting device, comprising any one of the above-mentioned crystallizer liquid level fluctuation suppression devices.
[0080] Among them, the continuous casting equipment includes: a ladle, which stores molten steel refined in the steelmaking process; a tundish, which receives the molten steel through an injection nozzle connected to the ladle and temporarily stores the molten steel; a crystallizer, which receives the molten steel stored in the tundish and preliminarily solidifies the molten steel into a predetermined shape; and an immersion nozzle, which supplies the molten steel in the tundish to the crystallizer.
[0081] Specifically, the device for suppressing the crystallizer liquid level fluctuation can be applied to the crystallizer in the continuous casting equipment.
[0082] The structure and effect of the crystallizer liquid level fluctuation suppression device are further described below in combination with specific numerical values and drawings.
[0083] Taking low carbon steel as the object, the casting speed is 2.0m / min, the casting section is 1100mm×240mm, and the superheat of the molten steel is 25℃. Figures 1 to 6 The molten steel flow field and liquid level fluctuation of the crystallizer of the crystallizer liquid level fluctuation suppression device shown.
[0084] See also Figures 1 to 6 As shown, the length of the long side baffle 1 is 780mm, the width of the long side baffle 1 is 30mm, the thickness of the long side baffle 1 is 5mm, the radius of the rounded corner structure at the tail end of the long side baffle 1 is 5mm, the central angle corresponding to the arc-shaped bottom surface of the long side baffle 1 is 30°, and the inclination angle of the long side baffle 1 is 5°; the length of the short side baffle 2 is 245mm, the width of the short side baffle 2 is 105mm, the thickness of the short side baffle 2 is 15mm, the radius of the rounded corner structure at the tail end of the short side baffle 2 is 5mm, the central angle corresponding to the arc-shaped bottom surface of the short side baffle 2 is 12°, and the inclination angle of the short side baffle 2 is 3°.
[0085] Through numerical simulation analysis, application Figures 1 to 6 The crystallizer of the crystallizer liquid level fluctuation suppression device shown in the figure is compared with the traditional crystallizer, and the results show that: under the same process parameters, Fig.11 As shown, application Figures 1 to 6 After the crystallizer with the crystallizer liquid level fluctuation suppression device shown in the figure, the flow velocity distribution at the slag interface is more uniform, and the area with the largest flow velocity becomes smaller, which is conducive to uniform slag on the crystallizer surface. Figure 8 As shown in the figure, the area with higher velocity is mainly distributed in the corner of the short side working plate, while the velocity near the nozzle is relatively low, which is not conducive to the uniform melting of the mold slag. Figures 1 to 6 After the crystallizer liquid level fluctuation suppression device is installed, the uniformity of the slag interface flow velocity is improved, which is beneficial to improving the slag reduction efficiency and slag reduction uniformity; see Fig.12 As shown, application Figures 1 to 6 After the crystallizer liquid level fluctuation suppression device is installed, the liquid level fluctuation amplitude of the crystallizer is 2.5 mm, while the conventional crystallizer, see Fig. 9 As shown in the figure, the liquid level fluctuation amplitude of the crystallizer is 5.0mm. Figures 1 to 6 After the crystallizer liquid level fluctuation suppression device is installed, the liquid level fluctuation amplitude can be reduced by 50%.
[0086] According to the numerical simulation results of the embodiments of the present application, under the condition of a pulling speed of 2.0 m / min, after the crystallizer is equipped with a crystallizer liquid level fluctuation suppression device, the liquid level fluctuation of the crystallizer is weakened within ±3 mm, effectively reducing the liquid level fluctuation frequency and amplitude height, while also increasing the uniformity of the slag interface flow velocity and improving the slag-melting efficiency.
[0087] The embodiments of the present application provide a device for suppressing liquid level fluctuation in a crystallizer and a continuous casting device, wherein the device for suppressing liquid level fluctuation in a crystallizer can change the flow direction of the molten steel flowing back upward by arranging a pair of long side baffles 1 and a pair of short side baffles 2 at the lower part of the liquid level in the crystallizer, thereby suppressing the impact of the molten steel flowing back upward on the slag interface and preventing the occurrence of liquid level fluctuation in the crystallizer; at the same time, changing the flow direction of the molten steel flowing back upward can avoid slag rolling caused by violent fluctuation of the liquid level, improve the uniformity of the flow velocity at the slag interface, thereby improving the slag-melting efficiency, which is beneficial to improving the quality of the ingot.
[0088] It is easy for those skilled in the art to understand that, under the premise of no conflict, the above-mentioned advantageous methods can be freely combined and superimposed.
[0089] The above are only preferred embodiments of the present application and are not intended to limit the present application. Any modifications, equivalent replacements and improvements made within the spirit and principles of the present application shall be included in the protection scope of the present application. The above are only preferred implementations of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and variations can be made without departing from the technical principles of the present application, and these improvements and variations should also be regarded as the protection scope of the present application.
Claims
1. A device for suppressing mold liquid level fluctuations, characterized in that: Used to resist the impact of molten steel on the liquid surface of the crystallizer, the crystallizer liquid surface fluctuation suppression device comprises a pair of long side baffles (1) and a pair of short side baffles (2), the pair of long side baffles (1) and the pair of short side baffles (2) are arranged in a liftable manner at the lower part of the liquid surface of the crystallizer, so that the molten steel flowing back upward is located within the projection area of the pair of long side baffles (1) and the pair of short side baffles (2), and the pair of long side baffles (1) and the pair of short side baffles (2) are used to change the flow direction of the molten steel flowing back upward.
2. The device for suppressing mold liquid level fluctuation according to claim 1, characterized in that: The bottom surfaces of the long side baffle (1) and the short side baffle (2) are arc-shaped, and the central angle corresponding to the arc is α, 10°≤α≤30°.
3. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The long side baffle (1) and the short side baffle (2) are inclined in a direction away from the protective slag layer, and the inclination angle of the long side baffle (1) and the short side baffle (2) relative to the horizontal plane is β, 3°≤β≤10°.
4. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The tail ends of the long side baffle (1) and the short side baffle (2) are rounded structures, the radius of the rounded structure is R, and 3mm≤R≤7mm.
5. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The length of the long side baffle (1) is n, 3 / 4N≤n≤N, N is the width of the casting billet; The length of the short side baffle (2) is d, 1 / 2D≤d≤D, and D is the thickness of the casting.
6. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The width of the long side baffle (1) and the short side baffle (2) is k, 15 mm ≤ k ≤ 300 mm; The thickness of the long side baffle (1) and the short side baffle (2) is h, 5mm≤h≤30mm.
7. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The crystallizer liquid level fluctuation suppression device further comprises a long side lifting assembly (3) and a short side lifting assembly (4); The long side lifting assembly (3) comprises a long side screw rod (31), a long side nut (32) and a long side connecting plate (33); the long side screw rod (31) is arranged at the upper opening of the crystallizer; at least two long side nuts (32) are arranged; at least two long side nuts (32) are sleeved on the long side screw rod (31) and are screwed to the long side screw rod (31); one end of the long side connecting plate (33) is arranged between at least two long side nuts (32); the other end of the long side connecting plate (33) is fixed relative to the long side baffle (1); The short side lifting assembly (4) comprises a short side screw (41), a short side nut (42) and a short side connecting plate (43); the short side screw (41) is arranged at the upper opening of the crystallizer; at least two short side nuts (42) are arranged; at least two short side nuts (42) are sleeved on the short side screw (41) and are threadedly connected to the short side screw (41); one end of the short side connecting plate (43) is arranged between at least two short side nuts (42); and the other end of the short side connecting plate (43) is relatively fixed to the short side baffle (2).
8. The device for suppressing mold level fluctuation according to claim 7, characterized in that: At least two of the long side lifting assemblies (3) are provided, and at least two of the long side lifting assemblies (3) are arranged opposite to each other along the length direction of the long side baffle (1).
9. The device for suppressing mold level fluctuation according to claim 1, characterized in that: The long side baffle (1) and the short side baffle (2) are made of niobium-based high-temperature alloy.
10. A continuous casting device, characterized in that: The invention comprises a crystallizer liquid level fluctuation suppression device as described in any one of claims 1 to 9.