Ethylene acrylate rubber with high wear resistance, high impact and low resonance
Through a specific formula of ethylene acrylate rubber, the problems of slow vulcanization speed, poor cold resistance and insufficient wear resistance are solved, achieving high wear resistance, high impact and low resonance performance, meeting the high temperature and wear resistance requirements of automotive shock absorbing products, and reducing Reduce costs and improve production efficiency.
Patent Information
- Application Number
- CN202411164905.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-10-22
AI Technical Summary
Existing ethylene acrylate rubber has slow vulcanization speed during the production process, poor cold resistance, insufficient elasticity and wear resistance, and has problems with poor electrical insulation in power engineering.
Made of AEM three-element rubber, N774 semi-reinforced furnace black, TP-795 plasticizer, stearic acid SA, internal release agent, antioxidant, microcrystalline wax, potassium stearate, sodium stearate, accelerator DOTG The specific formula of raw materials such as whitening agent KB-1 improves vulcanization speed and wear resistance, and enhances elasticity and durability.
The produced high-wear-resistant, high-impact, low-resonance ethylene acrylate rubber has good compression permanent deformation and shock-absorbing properties at high temperatures, which reduces material costs, improves production efficiency, expands the scope of use, and meets the high temperature requirements of automotive shock-absorbing products. and wear resistance requirements.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of rubber, in particular to high-wear-resistant, high-impact, low-resonance ethylene acrylate rubber. Background Art
[0002] Ethylene acrylate rubber is a rubber material commonly used in the current manufacturing industry. It has the characteristics of good heat resistance and oil resistance, and stable performance in lubricating oils containing sulfur, phosphorus, and chlorine additives. It is also resistant to aging, oxygen and ozone, UV rays, and has excellent air tightness.
[0003] However, the existing ethylene acrylate rubber still has some inevitable problems. First, due to the problem of raw material formula used in production, the vulcanization speed is slow, which increases the production cost. In addition, the ethylene acrylate rubber produced by the existing formula has poor cold resistance, and there are certain deficiencies in elasticity and wear resistance. In addition, the electrical insulation is generally poor in power engineering applications, which seriously affects the use of ethylene acrylate rubber. Summary of the invention
[0004] In view of the above-mentioned shortcomings of the prior art, the present invention provides a high-wear-resistant, high-impact, low-resonance ethylene acrylate rubber, which can effectively solve the problem of insufficient wear resistance of the ethylene acrylate rubber in the prior art.
[0005] To achieve the above objectives, the present invention is implemented through the following technical solutions: The invention provides a high-wear-resistant, high-impact, low-resonance ethylene acrylate rubber, which comprises the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 40-60 parts of N774 semi-reinforced furnace black; 2-5 parts of TP-795 plasticizer; 0.5-1 parts of stearic acid SA; 1-2 parts of internal mold release agent; 1-2 parts of antioxidant RD; 1-3 parts of antioxidant 445; 1-3 parts of microcrystalline wax; 1-5 parts of potassium stearate; 1-3 parts of sodium stearate; 1-5 parts of accelerator DOTG; and 1-2 parts of brightener KB-1.
[0006] The technical solution provided by the present invention has the following beneficial effects compared with the known prior art: the ethylene acrylate rubber produced by the present invention is characterized by high temperature resistance, low compression permanent deformation, high wear resistance and high fatigue durability. The ethylene acrylate rubber achieves good compression permanent deformation at high temperature, meets the high requirements of the bearing bracket for shock absorption performance, and compared with previous products of this type, the price of the mixed rubber and the production efficiency are greatly improved; and the present invention improves the processing technology, vulcanization speed, and reduces the material cost, meets the requirements of rubber products for both high temperature resistance and improved elasticity and wear resistance and durability in automobile shock absorption products, and expands the application scope of ethylene acrylate. DETAILED DESCRIPTION
[0007] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0008] The present invention will be further described below in conjunction with the embodiments.
[0009] Embodiment 1: High wear-resistant, high-impact, low-resonance ethylene acrylate rubber comprises the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 40 parts of N774 semi-reinforced furnace black; 2 parts of TP-795 plasticizer; 0.5 parts of stearic acid SA; 1 part of internal mold release agent; 1 part of antioxidant RD; 1 part of antioxidant 445; 1 part of microcrystalline wax; 1 part of potassium stearate; 1 part of sodium stearate; 1 part of accelerator DOTG; 1 part of brightener KB-1.
[0010] Example 2: Highly wear-resistant, high-impact, low-resonance ethylene acrylate rubber, comprising the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 50 parts of N774 semi-reinforced furnace black; 3 parts of TP-795 plasticizer; 0.5 parts of stearic acid SA; 1 part of internal mold release agent; 2 parts of antioxidant RD; 2 parts of antioxidant 445; 2 parts of microcrystalline wax; 2 parts of potassium stearate; 2 parts of sodium stearate; 3 parts of accelerator DOTG; 1 part of brightener KB-1.
[0011] Example 3: Highly wear-resistant, high-impact, low-resonance ethylene acrylate rubber, comprising the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 50 parts of N774 semi-reinforced furnace black; 3 parts of TP-795 plasticizer; 1 part of stearic acid SA; 2 parts of internal mold release agent; 2 parts of antioxidant RD; 2 parts of antioxidant 445; 2 parts of microcrystalline wax; 3 parts of potassium stearate; 3 parts of sodium stearate; 3 parts of accelerator DOTG; 2 parts of brightener KB-1.
[0012] Example 4: Highly wear-resistant, high-impact, low-resonance ethylene acrylate rubber, comprising the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 60 parts of N774 semi-reinforced furnace black; 4 parts of TP-795 plasticizer; 1 part of stearic acid SA; 2 parts of internal mold release agent; 2 parts of antioxidant RD; 1 part of antioxidant 445; 1 part of microcrystalline wax; 4 parts of potassium stearate; 3 parts of sodium stearate; 3 parts of accelerator DOTG; 2 parts of brightener KB-1.
[0013] Example 5: Highly wear-resistant, high-impact, low-resonance ethylene acrylate rubber, comprising the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 40 parts of N774 semi-reinforced furnace black; 5 parts of TP-795 plasticizer; 1 part of stearic acid SA; 2 parts of internal mold release agent; 2 parts of antioxidant RD; 3 parts of antioxidant 445; 3 parts of microcrystalline wax; 5 parts of potassium stearate; 3 parts of sodium stearate; 5 parts of accelerator DOTG; 2 parts of brightener KB-1.
[0014] Example 6: Highly wear-resistant, high-impact, low-resonance ethylene acrylate rubber, comprising the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 60 parts of N774 semi-reinforced furnace black; 5 parts of TP-795 plasticizer; 1 part of stearic acid SA; 2 parts of internal mold release agent; 2 parts of antioxidant RD; 3 parts of antioxidant 445; 3 parts of microcrystalline wax; 5 parts of potassium stearate; 3 parts of sodium stearate; 5 parts of accelerator DOTG; 2 parts of brightener KB-1.
[0015] The following table can be obtained by conducting various experiments on the ethylene acrylate rubber produced in the above examples 1-6: From the above examples, it can be seen that the ethylene acrylate rubber produced by the present invention has the characteristics of high temperature resistance, low compression permanent deformation, high wear resistance and high fatigue durability. The ethylene acrylate rubber achieves good compression permanent deformation at high temperature, meets the high requirements of the bearing bracket for shock absorption performance, and compared with previous products of this type, the price and production efficiency of the mixed rubber are greatly improved. Moreover, it can be used continuously for 18 months at 120°C and 6 weeks at 170°C, and the compression permanent deformation at high temperature is less than 20. The present invention improves the processing technology, vulcanization speed, and reduces the material cost, meets the requirements of rubber products for both high temperature resistance and improved elasticity and wear resistance and durability in automotive shock absorption products, and expands the scope of use of ethylene acrylate.
[0016] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the protection scope of the technical solutions of the embodiments of the present invention.
Claims
1. High wear resistance, high impact and low resonance ethylene acrylate rubber, It is characterized in that The invention comprises the following raw materials in parts by weight: 100 parts of AEM ternary rubber; 40-60 parts of N774 semi-reinforced furnace black; 2-5 parts of TP-795 plasticizer; 0.5-1 parts of stearic acid SA; 1-2 parts of internal mold release agent; 1-2 parts of antioxidant RD; 1-3 parts of antioxidant 445; 1-3 parts of microcrystalline wax; 1-5 parts of potassium stearate; 1-3 parts of sodium stearate; 1-5 parts of accelerator DOTG; and 1-2 parts of brightener KB-1.