Waveform energy characteristic-based guided wave reference-damage-free imaging method

By arranging sparse array sensors on the aluminum plate, calculating the root mean square error of the signal and selecting pseudo-reference signals, combined with the probabilistic damage detection reconstruction imaging algorithm, reference-free damage detection is achieved, which solves the problem of reduced reliability of reference data in traditional technology and improves improve detection accuracy and efficiency.

CN118817845APending Publication Date: 2024-10-22CHANGSHA UNIVERSITY OF SCIENCE AND TECHNOLOGY
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410836764.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-26
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

Traditional ultrasonic guided wave detection technology relies on reference data, which is affected by the environment and working conditions, resulting in reduced reliability of the reference data and unable to effectively implement reference-free damage detection.

Method used

By arranging a circular sparse array sensor on an aluminum plate, calculating the root mean square error between signals, adaptively selecting a pseudo-reference signal, and using the full-path waveform energy characteristics to fuse the damage index and probabilistic damage detection reconstruction imaging algorithm to achieve no reference damage detection.

Benefits of technology

There is no need to rely on the response signal in the healthy state of the component as the benchmark, which reduces the workload of the detection process, improves the accuracy and efficiency of damage detection, and effectively avoids the interference of environmental changes on the detection results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118817845A_ABST
    Figure CN118817845A_ABST
Patent Text Reader

Abstract

The invention discloses a guided wave reference-damage-free imaging method based on waveform energy characteristics. The method comprises the following steps: acquiring a response signal on each path of a circular array sensor in a detection area; grouping all path signals, ensuring that each group has the same distance, and obtaining a signal matrix of each group; cutting off each group of signals according to the distance, retaining S0 modal signals, and calculating a root-mean-square error between response signals in each group of signal matrixes; determining two response signals with the maximum root-mean-square error in each group according to the root-mean-square error, and adaptively selecting the signal with the larger amplitude as a pseudo reference signal; calculating a root-mean-square error damage index and an energy damage index of each signal and the pseudo reference signal in each group of signal matrixes so as to obtain a full-path waveform energy feature fusion damage index; and imaging the damage in the detection area by using the fusion damage index and a probability damage detection reconstruction imaging algorithm, and determining the position of a damage point in an imaging image by using the position of a probability maximum value.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of nondestructive testing of materials, and in particular to a guided wave non-reference damage imaging method based on waveform energy characteristics. Background Art

[0002] With the vigorous development of aerospace, rail transportation, chemical manufacturing, and shipbuilding industries, thin plate components have become the preferred components for industrial equipment and high-end manufacturing equipment. During the manufacturing and service process of thin plate components, they often face harsh working environments and may suffer various damages such as bumps, scratches, fatigue cracks, and corrosion. Therefore, in order to ensure the safety and reliability of industrial equipment, it is necessary to develop non-destructive testing technology for thin plate components.

[0003] The field of nondestructive testing includes various technologies, such as thermal imaging, laser and ultrasonic testing. Among them, the detection method based on ultrasonic guided waves has become a research hotspot in the field of structural nondestructive testing due to its advantages such as low cost, long-distance propagation and high sensitivity. In particular, the application of ultrasonic guided waves is particularly prominent in the detection of thin plate structure damage. Traditional ultrasonic guided wave detection technology usually relies on benchmark data to determine the existence and location characteristics of damage by comparing the difference between the detection signal and the benchmark signal. However, in actual engineering detection, the coupling between the sensor and the detection component and the characteristics of the component itself are often affected by factors such as the environment and working conditions. Therefore, the reliability of the previously acquired benchmark data as a reference value will be significantly reduced. Existing benchmark-free guided wave damage detection technologies include time reversal method, sparse reconstruction method and symmetric excitation method. The time reversal method uses the guided wave signal recorded by the sensor array to locate and image the damage in the structure by propagating the signal back to the source point. The sparse reconstruction method uses the guided wave propagation model to build a dictionary and combines the sparsity of component damage to identify and locate damage. Symmetrical excitation methods use specially arranged sensors to analyze the differences in damage scattering wave packets or symmetrical response signals in single-mode guided wave signals to accurately locate damage. Although these methods have made significant progress in ultrasonic guided wave detection technology, they mainly rely on the study of scattered signals or signal changes, and usually ignore the differences in signal characteristics between different sensors.

[0004] The present invention utilizes the root mean square error of signals between full-path sensor pairs to determine a pseudo-reference signal. The pseudo-reference signal is directly and adaptively selected from the current response signal without relying on a pre-acquired reference signal. The full-path waveform energy feature fusion damage index is calculated using the pseudo-reference signal and the response signal, and combined with a probabilistic damage detection reconstruction imaging algorithm, precise positioning of guided wave non-reference damage detection is achieved. Summary of the invention

[0005] The purpose of the present invention is to provide a waveguide-based reference-free damage imaging method based on waveform energy characteristics, which can not only realize reference-free damage detection and reduce dependence on reference signals, but also significantly reduce the workload of the detection process.

[0006] In order to achieve the above object, the present invention is implemented by the following technical solutions, including:

[0007] Circular sparse array sensors are evenly arranged on the selected aluminum plate, each sensor in the circular sparse array sensor is used as an excitation end in turn to send an excitation signal, and the remaining sensors receive response signals to obtain the response signal on each path of the circular array sensor in the detection area;

[0008] Group all path signals so that each group has the same distance, and obtain the signal matrix of each group;

[0009] Each group performs signal truncation according to the distance, retains the S0 modal signal, calculates the root mean square error between the response signals in each group of signal matrices, determines the two response signals with the largest root mean square error, and adaptively selects the signal with the larger amplitude as the pseudo reference signal;

[0010] Calculate the root mean square error damage index and energy damage index between each signal and the pseudo reference signal in each group of signal matrices to obtain the full path waveform energy feature fusion damage index;

[0011] The damage in the detection area is imaged using the fusion damage index and probabilistic damage detection reconstruction imaging algorithm, and the position of the damage point in the imaging image is determined using the maximum probability position;

[0012] A further technical solution is to obtain the response signal on each path of the circular array sensor in the detection area, including:

[0013] A circular array sensor is arranged in the detection area, and a 5-cycle Hanning window modulated sine wave signal is selected for excitation to obtain the response signal on each path;

[0014] The 5-cycle Hanning window modulated sine wave signal is defined as:

[0015]

[0016] Where V0 is the amplitude of the signal, f is the frequency of the excitation signal, which is also the center frequency of the response signal, N is the number of cycles of the excitation signal, and the response signal on the acquisition path is y(t).

[0017] A further technical solution is to group all path signals, each group having the same distance, and obtain a signal matrix for each group, including:

[0018] M=[Y1 Y2 … Y p … Yq ] Τ (2)

[0019] Y p =[y p1 (t) y p2 (t) … y ps (t)] (3)

[0020] Among them, M is the total path signal, which is divided into q groups, Y p is the p-th group of signal matrix whose sensor path distance is D, including s response signals.

[0021] Further technical solutions, in the following technical solutions, the response signal is truncated to retain only the S0 modal signal, including:

[0022]

[0023] Among them, t L is the left position time point of the S0 modal signal, t R is the right position time point of the S0 modal signal, is the S0 modal group velocity, is the A0 modal group velocity.

[0024] A further technical solution is to calculate the root mean square error between the response signals in each group of signal matrices, determine the two response signals with the largest root mean square error, and adaptively select the signal with the larger amplitude as the pseudo reference signal;

[0025] Calculate the root mean square error between the response signals in each group of signal matrices to obtain the root mean square error matrix RMSE p ,include:

[0026]

[0027] Where N is the number of signal sampling points, s is the number of response signals; calculate max(RMSE p ), get the corresponding i-th response signal and j-th response signal, compare the amplitudes of the two, and select the signal with the larger amplitude as the pseudo reference signal, denoted by y B (t).

[0028] A further technical solution is to calculate the root mean square error damage index and energy damage index between each signal in each group of signal matrices and the pseudo-reference signal to obtain the full-path waveform energy feature fusion damage index;

[0029] The root mean square error damage index between each signal and the pseudo reference signal is calculated as follows:

[0030]

[0031] Among them, DI R (m,n) is the root mean square error damage index calculated by obtaining the response signal when the mth sensor is used as the excitation end and the nth sensor is used as the receiving end, y B is the pseudo reference signal, y p (m,n) is the response signal;

[0032] The energy damage index of each signal and the pseudo-reference signal is calculated as follows:

[0033]

[0034] Among them, DI E (m,n) is the energy damage index calculated by obtaining the response signal when the mth sensor is used as the excitation end and the nth sensor is used as the receiving end. Indicates that Hilbert transform envelope processing is performed on the signal;

[0035] Full path waveform energy feature fusion damage index DI F (m,n) is expressed as:

[0036]

[0037] Among them, max means taking the maximum value of the damage index.

[0038] A further technical solution is to image the damage in the detection area by using the full-path waveform energy feature fusion damage index and probabilistic damage detection reconstruction imaging algorithm, including:

[0039]

[0040] Where L is the number of sensors, P(x, y) is the damage probability value of the point (x, y) in the detection area, and β is a shape parameter greater than 1.

[0041] In some embodiments, calculating a weight distribution function in a probabilistic damage detection reconstruction imaging algorithm includes:

[0042]

[0043] Where R(x,y,m,n) is the weight distribution function, RD(x,y,m,n) is the relative distance from point (x,y) to the path formed by the excitation sensor m and the receiving sensor n, (x,y) is the pixel coordinate in the detection area, (x m ,y m ) is the position coordinate of the excitation sensor m, (x n ,y n ) is the position coordinate of the receiving sensor n.

[0044] A further technical solution is to use the position of the maximum probability as the predicted damage point after damage imaging.

[0045] Compared with the prior art, the present invention has the following beneficial effects:

[0046] The present invention does not need to rely on the response signal of the component in a healthy state as a reference, effectively avoids the interference of environmental changes on the detection results, and reduces the workload of the detection process.

[0047] The present invention utilizes waveform energy characteristics to more accurately describe damage characteristics, thereby achieving rapid and accurate positioning of damage points within the detected target, thereby improving detection efficiency and accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] The accompanying drawings constituting a part of the present disclosure are used to provide a further understanding of the present disclosure. The illustrative embodiments of the present disclosure and their descriptions are used to explain the present disclosure and do not constitute an improper limitation on the present disclosure.

[0049] Figure 1 A schematic diagram of a method flow in an embodiment of the present invention;

[0050] Figure 2 A piezoelectric chip position coordinate table in an embodiment of the present invention;

[0051] Figure 3 Schematic diagram of single damage and double damage arrangement in an embodiment of the present invention;

[0052] Figure 4 A table of single damage and double damage position coordinates in an embodiment of the present invention;

[0053] Figure 5 It is a time domain waveform diagram of a damage signal in an embodiment of the present invention;

[0054] Figure 6 The excitation signal time domain waveform and spectrum diagram in the embodiment of the present invention;

[0055] Figure 7 Path diagrams of sensors with different propagation distances in an embodiment of the present invention;

[0056] Figure 8 Root mean square error matrix diagram in an embodiment of the present invention;

[0057] Fig. 9 A three-dimensional bar graph of waveform energy characteristics fused with damage index in an embodiment of the present invention;

[0058] Fig.10 These are single-lesion and double-lesion imaging images in the embodiments of the present invention. DETAILED DESCRIPTION

[0059] It should be noted that the following detailed descriptions are all illustrative and are intended to provide further explanation of the present disclosure. Unless otherwise specified, all technical and scientific terms used herein have the same meanings as those commonly understood by those skilled in the art to which the present disclosure belongs.

[0060] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present disclosure. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprising" and / or "including" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.

[0061] The present invention is further described below in conjunction with the accompanying drawings.

[0062] like Figure 1 As shown, this embodiment provides a waveguide non-reference damage imaging method based on waveform energy characteristics, the method comprising the following steps:

[0063] Circular sparse array sensors are evenly arranged on the selected aluminum plate, each sensor in the circular sparse array sensor is used as an excitation end in turn to send an excitation signal, and the remaining sensors receive response signals to obtain the response signal on each path of the circular array sensor in the detection area;

[0064] Group all path signals so that each group has the same distance and obtain the signal matrix of each group;

[0065] Each group performs signal truncation according to the distance, retains the S0 modal signal, calculates the root mean square error between the response signals in each group of signal matrices, determines the two response signals with the largest root mean square error, and selects the signal with the larger amplitude as the pseudo reference signal;

[0066] Calculate the root mean square error damage index and energy damage index between each signal and the pseudo reference signal in each group of signal matrices to obtain the full path waveform energy feature fusion damage index;

[0067] The damage in the detection area is imaged using the fusion damage index and probabilistic damage detection reconstruction imaging algorithm, and the position of the damage point in the imaging image is determined using the maximum probability position.

[0068] A waveguide non-reference damage imaging method based on waveform energy characteristics disclosed in this embodiment is described in detail.

[0069] Example 1: Single lesion imaging.

[0070] Eight piezoelectric chips are bonded and arranged on an aluminum plate with a thickness of 1 mm and a length and width of 1000 mm. The diameter of the uniform circular sparse array is 200 mm. The center of the array is taken as the origin. The coordinate table of the piezoelectric chip position is as follows: Figure 2 shown.

[0071] Arrange a hole damage with a diameter of 10mm. The schematic diagram of single damage arrangement is as follows Figure 3 (a) shows that the coordinate table of a single damage position is as follows: Figure 4 shown.

[0072] One of the sensors is used to stimulate the signal, and the other sensors receive the signal. The eight sensors are stimulated counterclockwise in turn, and a total of 56 groups of signals are obtained. The response signal under a single damage state is collected. The time domain waveform is as follows Figure 5 shown.

[0073] According to formula (1), a 5-cycle Hanning window modulated sine wave signal with a center frequency of 300KHz is selected to excite the waveguide response signal dominated by a single S0 mode. The time domain waveform and its spectrum are as follows: Figure 6 shown.

[0074] According to formulas (2) and (3), the 56 groups of signals are grouped according to different propagation distance paths, and are divided into 4 groups in total, such as Figure 7 As shown, each group of signal matrices is truncated according to formulas (4) and (5) to obtain a matrix containing only the S0 mode signal.

[0075] According to formula (6), the root mean square error between the response signals in each group of signal matrices is calculated to obtain the root mean square error matrix, and the max(RMSE D ), and obtain the corresponding i-th response signal and j-th response signal, such as Figure 8 As shown, the dotted box is the maximum value position. Compare the amplitudes of the two and select the signal with the larger amplitude as the pseudo reference signal, denoted by y B (t).

[0076] According to formulas (7), (8) and (9), the root mean square error damage index and energy damage index of each signal in each signal matrix and the pseudo reference signal are calculated to obtain the full path waveform energy feature fusion damage index. Its three-dimensional bar graph is shown as follows: Fig. 9 shown.

[0077] According to formulas (10), (11) and (12), the damage in the detection area is imaged by using the full path waveform energy feature fusion damage index and probabilistic damage detection reconstruction imaging algorithm. In the present invention, β is set to 1.06, and a single damage is imaged. The imaging results are shown in Fig.10 As shown in (a), the position of the maximum probability is represented by the symbol ×, the black circle is the actual damage location, and the center of the circle is the center of the hole damage circle.

[0078] Fig.10 In (a), the single damage imaging result shows that the predicted damage point position is (-36.5, 14), the relative distance from the actual damage point position (-40, 20) is 6.95 mm, and the position error is 0.0347, indicating that the present invention can achieve accurate positioning imaging of a single damage.

[0079] Embodiment 2: Double lesion imaging.

[0080] The arrangement of the piezoelectric chip, the signal excitation method and the calculation formula are consistent with those in the first embodiment. The diameter of the double damage is a hole damage of 10 mm. The arrangement diagram is as follows: Figure 3 (b) shows the coordinate table of the double damage positions. Figure 4 shown.

[0081] The double lesions were imaged, and the imaging results were as follows Fig.10 As shown in (b), the position of the maximum probability is represented by the symbol ×, the black circle is the actual damage location, and the center of the circle is the center of the hole damage circle.

[0082] Fig.10 In (b), the dual damage imaging results show that the predicted damage points are at (-40, -15) and (26, 64), and the relative distances from the actual damage point positions (-40, -20) and (20, 60) are 5 mm and 7.21 mm, respectively. The position errors are 0.025 and 0.0361, respectively. Considering the influence of the actual size of the damage, the present invention can also achieve high-precision positioning imaging in the case of dual damage, providing an effective solution for structural damage detection.

[0083] It is understood that, in the description of this specification, the description with reference to the terms "an embodiment", "another embodiment", "other embodiments", or "first to Nth embodiments" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, and material characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0084] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A guided wave non-reference damage imaging method based on waveform energy characteristics, characterized in that: include: Circular sparse array sensors are evenly arranged on the selected aluminum plate, each sensor in the circular sparse array sensor is used as an excitation end in turn to send an excitation signal, and the remaining sensors receive response signals to obtain the response signal on each path of the circular array sensor in the detection area; Group all path signals so that each group has the same distance, and obtain the signal matrix of each group; Each group performs signal truncation according to the distance, retains the S0 modal signal, calculates the root mean square error between the response signals in each group of signal matrices, determines the two response signals with the largest root mean square error, and adaptively selects the signal with the larger amplitude as the pseudo reference signal; Calculate the root mean square error damage index and energy damage index between each signal and the pseudo reference signal in each group of signal matrices to obtain the full path waveform energy feature fusion damage index; The damage in the detection area is imaged using the fusion damage index and probabilistic damage detection reconstruction imaging algorithm, and the position of the damage point in the imaging image is determined using the maximum probability position.

2. The waveguide imaging method without reference damage based on waveform energy characteristics according to claim 1, characterized in that: Acquiring a response signal on each path of the circular array sensor in the detection area, including: arranging the circular array sensor in the detection area, selecting and using a 5-cycle Hanning window modulated sine wave signal for excitation, and acquiring a response signal on each path; The 5-cycle Hanning window modulated sine wave signal is defined as: Where V0 is the amplitude of the signal, f is the frequency of the excitation signal, which is also the center frequency of the response signal, N is the number of cycles of the excitation signal, and the response signal on the acquisition path is y(t).

3. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 1, characterized in that: All path signals are grouped, each group has the same distance, and the signal matrix of each group is obtained, including: M=[Y1 Y2 … Y p …Y q ] Τ (2) AND p =[and p1 (t) and p2 (t) … and ps (t)] (3) Among them, M is the total path signal, which is divided into q groups, Y p is the p-th group of signal matrix whose sensor path distance is D, including s response signals.

4. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 1, characterized in that: Each group performs signal truncation according to the distance, retains the S0 modal signal, calculates the root mean square error between the response signals in each group of signal matrices, determines the two response signals with the largest root mean square error, and adaptively selects the signal with the larger amplitude as the pseudo reference signal; The response signal is truncated to retain only the S0 modal signal, including: Among them, t L is the left position time point of the S0 modal signal, t R is the right position time point of the S0 modal signal, is the S0 modal group velocity, is the A0 modal group velocity; Calculate the root mean square error between the response signals in each group of signal matrices to obtain the root mean square error matrix RMSE p ,include: Where N is the number of signal sampling points, s is the number of response signals; calculate max(RMSE p ), get the corresponding i-th response signal and j-th response signal, compare the amplitudes of the two, and select the signal with the larger amplitude as the pseudo reference signal, denoted by y B (t).

5. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 1, characterized in that: Calculate the root mean square error damage index and energy damage index between each signal and the pseudo reference signal in each group of signal matrices to obtain the full path waveform energy feature fusion damage index; The root mean square error damage index between each signal and the pseudo reference signal is calculated as follows: Among them, DI R (m,n) is the root mean square error damage index calculated by obtaining the response signal when the mth sensor is used as the excitation end and the nth sensor is used as the receiving end, y B is the pseudo reference signal, y p (m,n) is the response signal; The energy damage index of each signal and the pseudo-reference signal is calculated as follows: Among them, DI E (m,n) is the energy damage index calculated by obtaining the response signal when the mth sensor is used as the excitation end and the nth sensor is used as the receiving end. Indicates that Hilbert transform envelope processing is performed on the signal; Full path waveform energy feature fusion damage index DI F (m,n) is expressed as: Among them, max means taking the maximum value of the damage index.

6. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 1, characterized in that: The damage in the detection area is imaged using the full-path waveform energy feature fusion damage index and probabilistic damage detection reconstruction imaging algorithm, including: Where L is the number of sensors, p(x,y,m,n) is the damage probability value of the point (x,y) in the detection area, and β is a shape parameter greater than 1.

7. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 6, characterized in that: Calculate the weight distribution function in the probabilistic damage detection reconstruction imaging algorithm, including: Among them, R(x,y,m,n) is the weight distribution function, RD(x,y,m,n) is the relative distance from point (x,y) to the path formed by the excitation sensor m and the receiving sensor n, (x,y) is the coordinate of the pixel point in the detection area, (x m ,y m ) is the position coordinate of the excitation sensor m, (x n ,y n ) is the position coordinate of the receiving sensor n.

8. The waveguide imaging method without reference damage based on waveform energy characteristics as claimed in claim 1, characterized in that: The position with the maximum probability is taken as the predicted damage point.

Citation Information

Cited By

  • No-reference guided wave damage positioning method based on path time domain self-matching

    CN120102724A