Crosstalk mitigation in multi-core optical fibers under micro-bending
By applying a torsion period of less than 9.1 cm in the multi-core fiber to form a spiral core, the crosstalk problem between the cores of the multi-core fiber under micro-bending conditions is solved, the signal quality and data capacity are improved, and the PMD is reduced coefficient.
Patent Information
- Application Number
- CN202280070801.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-12
- Publication Date
- 2024-10-22
AI Technical Summary
Crosstalk problems between cores in multi-core optical fibers under micro-bending conditions lead to signal quality degradation and data capacity limitations, and it is difficult for existing technologies to effectively mitigate the crosstalk effect caused by micro-bending.
By applying a twist with a twist period (τ) less than 9.1 cm in the multi-core fiber, a spiral core is formed to reduce crosstalk caused by microbending, and while maintaining fiber density, limiting the number of twists between cores and improving the rotation rate of the fiber to reduce crosstalk.
It effectively reduces crosstalk caused by micro-bending, lowers the PMD coefficient, improves signal quality and data capacity, and improves the mechanical strength and production convenience of the optical fiber without damaging other transmission parameters.
Smart Images

Figure CN118829918A_ABST
Abstract
Description
background Technical Field
[0002] The present invention relates generally to optical fibers and, more particularly, to multi-core optical fibers. Background Art
[0003] Those skilled in the art of optical fiber understand that there is a significant difference between macrobending effects and microbending effects. This is because the principles governing macrobending are different from those governing microbending. Also, because different types of optical fibers are affected by various design parameters, sometimes unpredictably, the design considerations for single-core optical fibers are sometimes different from those for multi-core optical fibers. Summary of the invention
[0004] The present disclosure teaches optical fibers having multiple cores (also referred to as multi-core fibers, or simply multi-core fibers (MCFs)). For some embodiments, the optical fiber includes a central axis (arbitrarily designated as the z-axis, or simply z), along which the optical signal is transmitted. The optical fiber also includes a cladding extending along z. The cladding includes a substantially circular axial cross-section (having a cladding center and a cladding outer diameter (ODclad)). For some embodiments, ODclad is between about eighty (80) microns (μm) and about 300 μm (also expressed as 80 μm≤ODclad≤300 μm). Preferably, 100 μm≤ODclad≤240 μm, and in more preferred embodiments, 125 μm≤ODclad≤200 μm or 125 μm≤ODclad≤150 μm. In some preferred embodiments, ODclad is approximately 100 μm or 125 μm (meaning ODclad≈100 μm, or ODclad≈125 μm).
[0005] The optical fiber also includes a coating disposed around the cladding. The coating has an outer diameter (ODcoat) that depends on ODclad. Preferably, the coating has a thickness ranging from 0 μm (meaning no coating) to about 200 μm, such that an acceptable range of ODcoat is between about 80 μm and about 700 μm (meaning 80 μm ≤ ODcoat ≤ 700 μm). For some embodiments (e.g., when ODclad ≈ 125 μm), ODcoat ≈ 245 μm or ODcoat ≈ 200 μm, while for other embodiments (e.g., when ODclad ≈ 100 μm), ODcoat ≈ 200 μm, or the coating thickness is further reduced, such that ODcoat ≈ 180 μm or even ODcoat ≈ 160 μm. It should be noted that as ODcoat decreases or ODclad decreases, the optical fiber becomes more sensitive to microbending effects.
[0006] Because the optical fiber is an MCF, the optical fiber also includes at least a first core arranged in the cladding and a second core arranged in the cladding. In order to meet the industrial standard of single-mode fiber (SMF), each core of MCF 100 (e.g., the first core, the second core, etc.) has a maximum polarization mode dispersion (PMD) coefficient of 0.1 picoseconds per square root kilometer (ps / √km). Preferably, the maximum PMD coefficient is 0.04ps / √km (e.g., when the minimum length of the optical fiber removed from the spool is ~500 meters (m) or greater). More preferably, the maximum PMD coefficient is 0.02ps / √km (when the minimum length of the optical fiber removed from the spool is ~500m).
[0007] The optical fiber exhibits crosstalk from cross coupling between the first core and the second core. Under microbending conditions, the crosstalk increases. In order to mitigate the increased crosstalk due to microbending, the optical fiber is twisted about the z-axis and thereby exhibits a twist (including a twist period of τ). Due to this twist, at least one core (e.g., the first core) becomes helically arranged about z to form a helical core with a helical pitch (p). Because the MCF is twisted about the z-axis, and because the first core is arranged within the cladding, p is approximately equal to τ, meaning p≈τ. For some embodiments, the second core is a central core that extends substantially along z and includes a rotation (due to the twist on the optical fiber) with a period of τ. For other embodiments, the second core is a second helical core that has a pitch p≈τ similar to the first helical core.
[0008] The twist limits the maximum amount of added crosstalk. In some embodiments, in the wavelength (λ) range between about 1260 nanometers (nm) and 1360 nanometers (nm) (1260nm < λ < 1360nm), which is referred to in the industry as the O-band (for the original band), the maximum amount of added crosstalk is limited to less than about ten decibels (~10dB). In other embodiments, for 1530nm < λ < 1565nm, which is referred to in the industry as the C-band (for the legacy band), the maximum amount of added crosstalk is limited to less than ~6dB.
[0009] To limit the maximum amount of added crosstalk, some embodiments twist the optical fiber such that τ is less than 9.1 centimeters (meaning τ < 9.1 cm). In other words, the optical fiber exhibits more than eleven (> 11) twists per meter (or rotations per meter (rotations / meter)), which is higher than previously identified twist rates (or rotation rates). This is because high rotation rates (or high twist rates), such as fifty (50) rotations / meter (translating to τ ≤ 2 cm), lead to rapid degradation of the optical fiber quality and subsequent breakage during the optical fiber drawing process.
[0010] To this end, preferred embodiments of the disclosed optical fiber have a rotation rate of τ>2.5 cm (translating to less than forty (<40) rotations / meter), with a preferred range of 2.9 cm<τ<6.7 cm (translating to ~15≤rotations / meter≤35). More preferred embodiments include 3.3 cm<τ<5.0 cm (translating to ~20≤rotations / meter≤30). Several embodiments of the disclosed torsional MCF were tested with 3.4 cm<τ<4.0 cm (implying a narrow range of ~25≤rotations / meter≤~29), which showed successful mitigation of microbending induced crosstalk.
[0011] In summary, a twist having a twist period (τ) is applied to the optical fiber about z. The twist mitigates crosstalk caused by microbending. The cladding includes a substantially circular axial cross section. The substantially circular axial cross section includes a cladding center and a cladding outer diameter (ODclad). A plurality of cores (e.g., a first core, a second core, etc.) are disposed within the cladding. At least one core is helically disposed about z to form a helical core, wherein the helical core includes a helical pitch (p) such that p≈τ and τ<9.1 cm.
[0012] Other systems, devices, methods, features and advantages will be or will become apparent to one skilled in the art after studying the following drawings and detailed description. All such additional systems, methods, features and advantages are intended to be included within this description, within the scope of the present disclosure, and protected by the accompanying claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Many aspects of the present disclosure may be better understood with reference to the following drawings. The components in the drawings are not necessarily drawn to scale, but emphasis is placed on clearly illustrating the principles of the present disclosure. In addition, in the drawings, similar reference numerals represent corresponding components throughout the drawings.
[0014] Figure 1A is an axial cross-sectional view of one embodiment of a multi-core optical fiber, wherein the axes are designated as the x-axis (horizontal) and the y-axis (vertical).
[0015] Figure 1B yes Figure 1A A transverse view of a multi-core optical fiber is shown, with the axes designated as the y-axis (vertical) and the z-axis (along the transmission path). Specific embodiments
[0016] As the demand for fiber optic transmission capacity increases with global data traffic, efforts are being made to deploy more and more optical fibers in fiber optic cables. For example, by reducing the outer diameter (OD) of the optical fiber, the fiber optic cable can carry more optical fibers, thereby increasing the fiber density within the cable duct.
[0017] One way to increase transmission capacity is to employ space division multiplexing (SDM) in multi-core optical fiber, or multi-core fiber (MCF). Unlike single-core optical fiber, or single-mode fiber (SMF), MCF has multiple cores within the same cladding. Because the cores in MCF are very close together, cross-coupling between adjacent cores can cause inter-core crosstalk, an impairment that is not present in SMF. Inter-core crosstalk degrades signal quality, thus limiting the reach or data capacity of the MCF.
[0018] As one can appreciate, inter-core crosstalk can be reduced by increasing the spacing between adjacent cores. However, increasing the spacing while keeping the outer cladding thickness (OCT) constant increases the OD of the MCF, thereby reducing the fiber density. In other words, in an MCF, there is a tradeoff between reducing the OD and increasing the spacing between the cores. Alternatively, if the core spacing is increased without increasing the OD, the OCT will decrease, thereby increasing additional losses between the cores and creating a tradeoff between crosstalk and fiber loss. For improved crosstalk, there are additional tradeoffs, such as attenuation, mode field diameter (MFD), cutoff wavelength, and manufacturing cost (in addition to fiber density).
[0019] One of the many confounding factors in inter-core crosstalk is the effect of macrobending and microbending on the crosstalk. Fiber cabling and actual field deployment conditions can have a strong impact on the actual crosstalk due to both macrobending and microbending.
[0020] As will be appreciated by those skilled in the art, the industry standard for optical fiber includes macrobending losses as part of the optical fiber specification. Therefore, macrobending losses are routinely and easily tested during factory optical fiber qualification. Unlike macrobending, microbending is not addressed in the optical fiber specification. In addition, the characterization of microbending losses is more difficult and time-consuming than the characterization of macrobending losses. In addition, unlike macrobending tests (which are performed by wrapping the optical fiber around a mandrel of various diameters or bending the optical fiber in some other way), microbending tests are typically performed on nominally straight optical fibers, in a state without bending. Some examples of measuring microbending sensitivity are described in the International Electrotechnical Commission (IEC) Technical Report (TR) 62221 Ed 2.0: 2012, entitled "Optical Fibres-Measurement Methods-Microbending Sensitivity", which is familiar to those skilled in the art. Due to these differences between macrobending and microbending, methods for mitigating macrobending losses cannot be directly converted to microbending.
[0021] Due to the trade-offs between attenuation, MFD, cut-off wavelength, manufacturing cost, number of fibers (or fiber density), macrobending effects on crosstalk and microbending effects on crosstalk, as well as many other effects (e.g., polarization mode dispersion (PMD)), mitigating microbending crosstalk effects without negatively affecting other transmission influencing parameters is not a simple or trivial task.
[0022] The disclosed embodiments attempt to mitigate microbending effects on crosstalk by applying a twist (or rotation) to the MCF. Specifically, the twist period (τ) applied to the MCF is less than 9.1 centimeters (cm), which translates to more than eleven (11) twists per meter. Such a small τ < 9.1 cm is much smaller than the rotation rates conventionally used to mitigate macrobending losses. This is because higher rotation rates (or higher twist rates) increase the likelihood of breakage during fiber drawing or increase the likelihood of undesirable mechanical twisting when handling the fiber off the spool.
[0023] Having provided a broad technical solution to the technical problem, reference is now made in detail to the description of the embodiments as shown in the accompanying drawings. Although several embodiments are described in conjunction with these drawings, it is not intended to limit the present disclosure to one or more embodiments disclosed herein. On the contrary, it is intended to cover all alternatives, modifications and equivalents. It should be understood that, unless otherwise expressly or indicated by the context, rotation and torsion are used interchangeably in the present disclosure, and similarly, rotation rate and torsion rate are used interchangeably in the present disclosure.
[0024] Go to Figure 1A and Figure 1B (collectively shown as FIG. 1 ), the present disclosure teaches an optical fiber 100 (shown as an MCF) having a central axis (arbitrarily shown as the z-axis, or simply z) along which an optical signal is transmitted. Specifically, Figure 1A An axial cross-sectional view of one embodiment of the MCF 100 is shown, and Figure 1B A transverse view of the MCF 100 is shown. The optical fiber 100 includes a cladding 110 extending along z. The cladding 110 includes a substantially circular axial cross-section (having a cladding center and a cladding outer diameter (ODclad)). For some embodiments, the ODclad is between about eighty (80) microns (μm) and about 300 μm (also expressed as 80 μm≤ODclad≤300 μm). Preferably 100 μm≤ODclad≤240 μm, and more preferred embodiments have 125 μm≤ODclad≤200 μm or 125 μm≤ODclad≤150 μm. In some preferred embodiments, the ODclad is about 100 μm or 125 μm (meaning ODclad≈100 μm, or ODclad≈125 μm).
[0025] Because the optical fiber 100 is an MCF, the optical fiber 100 also includes a plurality of cores 120, 130a, 130b. In the embodiment of FIG. 1 , the MCF includes a central core 120 and peripheral cores (e.g., a first peripheral core 130a and a second peripheral core 130b). The central core 120, the first peripheral core 130a and the second peripheral core 130b are disposed within the cladding 110. In order to comply with industry standards, each core (e.g., the central core 120 and the peripheral cores 130a, 130b (collectively represented as 130)) has a maximum polarization mode dispersion (PMD) coefficient of 0.1 picoseconds per square root kilometer (ps / √km). Preferably, the maximum PMD coefficient is 0.04ps / √km (e.g., when the minimum length of the optical fiber removed from the spool is ~500 meters (m) or greater). For the preferred embodiment, the maximum PMD coefficient is 0.02 ps / √km (when the minimum length of fiber removed from the spool is ~500m).
[0026] The optical fiber 100 also includes a coating 140 disposed around the cladding 110. The coating 140 has an outer diameter (ODcoat). Preferably, the thickness of the coating ranges from 0 μm (meaning no coating) to about 200 μm, such that an acceptable range of ODcoat is between about 80 μm and about 700 μm (meaning 80 μm ≤ ODcoat ≤ 700 μm). For some embodiments (e.g., when ODclad ≈ 125 μm), ODcoat ≈ 245 μm, while for other embodiments (e.g., when ODclad ≈ 100 μm), ODcoat ≈ 200 μm. It should be noted that as ODcoat decreases or ODclad decreases, the optical fiber becomes more sensitive to microbending effects.
[0027] The optical fiber 100 exhibits crosstalk (whether central core to peripheral core crosstalk or peripheral core to peripheral core crosstalk) from cross coupling between the first core 130a and the second core. Under microbending conditions, the crosstalk increases. To mitigate the increased crosstalk due to microbending, the optical fiber 100 is twisted about the z-axis and thus exhibits a twist (including a twist period of τ). Due to this twist, at least one core (e.g., the first core 130a) becomes helically arranged about z to form a helical core having a helical pitch (p), such as Figure 1B shown.
[0028] Because the MCF 100 is twisted about the z-axis, and because the first core 130a is disposed within the cladding 110, p is approximately equal to τ, which means p≈τ. For some embodiments, the second core is the central core 120 that extends substantially along z and includes a rotation (due to the twist on the fiber) with a period of τ. For other embodiments, the second core is a second helical core 130b that has a pitch p≈τ similar to the first helical core 130a.
[0029] The twist limits the maximum amount of added crosstalk between adjacent cores. In some embodiments, in the wavelength (λ) range between about 1260 nanometers (nm) and 1360 nanometers (nm) (1260nm < λ < 1360nm), which is referred to in the industry as the O-band (for the original band), the maximum amount of added crosstalk is limited to less than about ten decibels (~10 dB). In other embodiments, for 1530nm < λ < 1565nm, which is referred to in the industry as the C-band (for the legacy band), the maximum amount of added crosstalk is limited to less than ~6 dB.
[0030] To limit the maximum amount of added crosstalk, some embodiments twist the optical fiber 100 such that τ is less than 9.1 centimeters (meaning τ < 9.1 cm). In other words, the optical fiber 100 exhibits more than eleven (> 11) twists per meter (or rotations per meter (rotations / meter)), which is higher than previously identified twist rates (or rotation rates). This is because high rotation rates (or high twist rates), such as fifty (50) rotations / meter (translating to τ ≤ 2 cm), lead to rapid degradation of the optical fiber quality and subsequent breakage during the optical fiber drawing process.
[0031] To this end, preferred embodiments of the disclosed optical fiber 100 have a rotation rate of τ>2.5 cm (translating to less than forty (<40) rotations / meter), with a preferred range of 2.9 cm<τ<6.7 cm (translating to ~15≤ rotations / meter≤~35). More preferred embodiments include 3.3 cm<τ<5.0 cm (translating to ~20≤ rotations / meter≤~30). Several embodiments of the disclosed torsional MCF were tested with 3.4 cm<τ<4.0 cm (implying a narrow range of ~25≤ rotations / meter≤~29), which showed successful mitigation of microbending induced crosstalk.
[0032] The rotation or torsion of optical fiber 100 produces additional benefits, such as further reduction and stabilization of PMD. Because MCF has an asymmetric structure, the cladding 110 around core 120, 130 always shows sizable frozen thermal stress from the drawing process. This is usually an order of magnitude higher than the thermal stress in standard SCF. This stress causes optical birefringence, which is the reason for PMD. Under the state where the rotation period is less than 9.1cm, the microbend effect on crosstalk can be reduced, while reducing PMD.
[0033] Experimentally, embodiments of the disclosed MCF 100 were tested at 3.4 cm < τ < 4.0 cm (implying a narrow range of ~25 ≤ rotations / meter ≤ ~29) and compared with unrotated (or untwisted) optical fibers. Under microbending conditions (compared to no microbending), the unrotated (or untwisted) optical fiber exhibited an increase in core-to-core crosstalk of ~17 dB / km in the O-band and an increase in core-to-core crosstalk of ~6 dB / km in the L-band (for the long-wave band, which is 1565 nm ≤ λ ≤ 1625 nm). Unlike unrotated (or untwisted) optical fibers, under microbending conditions (compared to no microbending), the twisted optical fiber 100 exhibited an increase in core-to-core crosstalk of only ~7 dB / km in the O-band and an increase in core-to-core crosstalk of ~4 dB / km in the L-band. Therefore, the experimental results show that for τ between ~25 rotations / meter and ~29 rotations / meter, the O-band improves by ~10 dB / km and the L-band improves by ~2 dB / km.
[0034] In other embodiments, the microbending losses of the optical fiber 100 are reduced by about 0.04 dB / km averaged across all the cores 120 , 130 .
[0035] Measure the PMD coefficient value in twisted and untwisted optical fiber, twisted to ~ 30 turns / meter (or τ ≈ 3.3cm) optical fiber improves PMD. For example, untwisted optical fiber shows the PMD coefficient of measurement up to ~ 0.3ps / √km (for example ~ 0.28ps / √km) when tested on the spool, and shows the PMD coefficient of measurement up to ~ 4.8ps / √km (for example ~ 4.33ps / √km) when removed from the spool. The latter value continues to increase proportionally with longer unwound optical fiber length. This shows that cable deployment can increase the signal damage related to PMD.
[0036] To compare untwisted fiber and twisted fiber, at a rotation rate of ~30 rotations / meter (τ≈3.3cm), the PMD coefficient changes from 0.28ps / √km (for untwisted fiber on the spool) to 0.028ps / √km (for twisted fiber on the spool), which is an improvement of one (1) order of magnitude. The off-spool comparison results in an even greater improvement, with the off-spool PMD coefficient dropping from ~4.33ps / √km (for untwisted fiber) to ~0.03ps / √km (for twisted fiber, τ≈3.3cm), which is an improvement of more than two (2) orders of magnitude. It is noteworthy that the on-spool and off-spool PMD values become essentially the same, indicating that the low PMD in twisted fiber can be fully maintained during MCF cabling and field deployment. In addition, unlike most current transmission fibers, the PMD on a twisted MCF can be accurately measured on the spool, which no longer requires the low-mode coupling method commonly used in production.
[0037] It should also be noted that the high rotation rates described above do not cause significant detriment to other critical parameters such as core density, cutoff wavelength, MFD, attenuation, coating quality, fiber strength, etc. Additionally, imparting such a twist or rotation on the MCF does not require any specialized equipment and is accomplished with standard draw tower equipment.
[0038] Finally, depending on the degree of birefringence in the MCF, the rotation conditions may require additional optimization or adjustment (compared to SMF). However, the maximum rotation rate (eg, τ≈2.5 cm) can be achieved with standard pull tower equipment.
[0039] Although exemplary embodiments have been shown and described, it will be apparent to those skilled in the art that many changes, modifications or variations may be made to the disclosed subject matter described. Therefore, all such changes, modifications and variations should be considered within the scope of the disclosed subject matter.
Claims
1. An optical fiber, comprising: Central axis z; a cladding extending along z, the cladding comprising a substantially circular axial cross-section, the substantially circular axial cross-section comprising a cladding center, the substantially circular axial cross-section further comprising a cladding outer diameter ODclad; a torsion about z, the torsion having a period τ less than 9.1 centimeters (τ<9.1 cm); a first core disposed within the cladding, the first core being disposed helically about z to form a helical core, the helical core comprising a pitch p approximately equal to τ (p≈τ); as well as a second core disposed in the cladding; crosstalk from cross coupling between the first core and the second core, the crosstalk increasing under microbending conditions to a maximum amount of increased crosstalk, the maximum amount of increased crosstalk being limited by the torsion; as well as A coating is disposed around the cladding, the coating comprising a coating outer diameter ODcoat.
2. The optical fiber according to claim 1, wherein The second core is a central core extending substantially along z, the central core comprising a rotation with a period τ.
3. The optical fiber according to claim 1: in, The first core is a first helical core; and The second fiber core is arranged helically around z to form a second helical fiber core.
4. The optical fiber according to claim 1: in, The first core includes a maximum polarization mode dispersion (PMD) coefficient of 0.1 picoseconds per square root kilometer (ps / √km).
5. The optical fiber according to claim 4, wherein: The maximum PMD coefficient is 0.04ps / √km.
6. The optical fiber according to claim 4, wherein: The maximum PMD coefficient is 0.02ps / √km.
7. The optical fiber according to claim 1: in, The second core includes a maximum polarization mode dispersion (PMD) coefficient of 0.1 picoseconds per square root kilometer (ps / √km).
8. The optical fiber according to claim 7, wherein: The maximum PMD coefficient is 0.04ps / √km.
9. The optical fiber according to claim 7, wherein: The maximum PMD coefficient is 0.02ps / √km.
10. The optical fiber according to claim 1, wherein In the wavelength (λ) range between about 1260 nanometers nm and 1360 nm (1260 nm < λ < 1360 nm), the maximum amount of added crosstalk is limited to less than about ten decibels (-10 dB).
11. The optical fiber according to claim 1, wherein: The maximum amount of increased crosstalk is limited to less than about six decibels (~6 dB) within a wavelength (λ) range of about 1530 nanometers to 1565 nm (1530 nm < λ < 1565 nm).
12. The optical fiber according to claim 1, wherein: ODclad is between about eighty (80) microns μm and about 300 μm (-80 μm ≤ ODclad ≤ -300 μm).
13. The optical fiber according to claim 12, wherein: ODclad is approximately equal to 125 μm (ODclad≈125 μm).
14. The optical fiber of claim 1, wherein: ODcoat is between about 80 micrometers μm and about 700 μm (80 μm≤ODcoat≤700 μm).
15. The optical fiber of claim 14, wherein: ODcoat≈245μm.
16. The optical fiber of claim 14, wherein: ODcoat≈200μm.
17. The optical fiber of claim 1, wherein: τ is greater than 2.5cm (τ>2.5cm).
18. The optical fiber of claim 17, wherein: τ is between 2.9 cm and 6.7 cm (2.9 cm < τ < 6.7 cm).
19. The optical fiber of claim 18, wherein: 3.3cm<τ<5.0cm.
20. The optical fiber of claim 19, wherein: 3.4cm<τ<4.0cm.