Polyethylene film with high peeling strength and preparation method thereof
By using monodispersed mesoporous silica hollow sphere composites as inorganic additives in the polyethylene film, the peeling strength of the polyethylene film is improved and the appropriate bending properties are maintained, solving the problem of insufficient peeling strength of the polyethylene film and expanding the Its scope of application.
Patent Information
- Application Number
- CN202310446661.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-04-24
AI Technical Summary
The low surface energy and hydrophobicity of polyethylene film result in low peeling strength, limiting its application range.
Monodisperse mesoporous silica hollow sphere composite is used as an inorganic additive, and is mixed with polyethylene through microwave stirring and ultrasonic dispersion technology to form a polyethylene film with high peeling strength.
The peeling strength of the polyethylene film is significantly improved, while the amount of inorganic additives is controlled to maintain appropriate bending properties and expand its application scope.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of polyethylene films, and in particular relates to a polyethylene film with high peeling strength and a preparation method thereof. Background Art
[0002] Polyethylene (PE) is a linear alkane with high relative molecular mass formed by the polymerization of ethylene monomers. Polyethylene is the resin variety with the simplest molecular composition and molecular structure. Due to its wide source, non-toxicity, easy processing, reproducible processing, cold resistance, moisture resistance and other advantages, it has a wide range of uses in food, daily necessities packaging, and agricultural production. Polyethylene is the largest plastic variety in today's production, and the amount of polyethylene film is also increasing year by year. However, due to the presence of non-polar groups in the polyethylene chain, its cohesive energy density is low among plastic materials, and its surface energy is relatively low (30-32 dynes / cm). Its surface is inert and hydrophobic, so it is not easy to compound or mix with other materials, resulting in its low peel strength, which leads to certain limitations on the application range of polyethylene film.
[0003] For example, a Chinese invention patent discloses a polyethylene film having high peel strength with a non-aluminum-plated surface of VMPET and a preparation method thereof [application number: 201710990655.1]. The invention patent is composed of the following substances calculated by weight percentage: 5-15% hydrogenated dimer acid / rosin-based polyester polyamide, 2-5% maleic anhydride grafted polyethylene, and 80-93% polyethylene; the hydrogenated dimer acid / rosin-based polyester polyamide is prepared by reacting a carboxyl-terminated polyamide and a diol, and the carboxyl-terminated polyamide is prepared by reacting a hydrogenated dimer acid, maleic rosin acid, and a diamine, and the weight ratio of the hydrogenated dimer acid to the maleic rosin acid is 5:5-3:7, the ratio of the sum of the molar numbers of carboxyl groups of the hydrogenated dimer acid and the maleic rosin acid to the molar number of amino groups of the diamine is 1:0.6-0.8, and the ratio of the molar number of hydroxyl groups of the diol to the molar number of carboxyl groups of the carboxyl-terminated polyamide is greater than or equal to 1.8:1.
[0004] The improvement made in this invention patent lies in the peel strength of the polyethylene film, and is limited to the peel strength between the non-aluminum-plated surface of the VMPET film, and does not involve improvements in the peel strength performance. Summary of the invention
[0005] The object of the present invention is to provide a polyethylene film with high peel strength in view of the above problems.
[0006] Another object of the present invention is to provide a method for preparing a polyethylene film with high peel strength in view of the above problems.
[0007] In order to achieve the above object, the present invention adopts the following technical solutions: A polyethylene film with high peel strength, characterized in that the raw materials of the polyethylene film include polyethylene and an inorganic additive; the inorganic additive is a monodisperse mesoporous hollow silica sphere composite; the monodisperse mesoporous hollow silica sphere composite is a monodisperse mesoporous hollow silica sphere loaded with barium sulfate; The peel strength F of the polyethylene film is greater than 1.5N.
[0008] The mass fraction of the inorganic additive in the raw material of the polyethylene film (a mixture of polyethylene and the inorganic additive) is 5 to 9%.
[0009] The mass fraction of inorganic additives in the raw materials of polyethylene film is 5-7%.
[0010] The mass fraction of inorganic additives in the raw materials of polyethylene film is 7-9%.
[0011] The peel strength F of the polyethylene film is greater than 2.5N.
[0012] The peel strength F of the polyethylene film is greater than 3.5N.
[0013] The peel strength F of the polyethylene film is greater than 4.5N.
[0014] The peel strength F of the polyethylene film is greater than 5.5N.
[0015] A method for preparing a polyethylene film with high peel strength, comprising the following technical steps: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 8:1 to 12:1; The mass fraction of the aqueous sulfuric acid solution is 10% to 25%, and the sulfuric acid is kept in excess.
[0016] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere complex in hexanediol is 20 to 30 g / L; the monodisperse mesoporous hollow silica sphere complex is added to hexanediol, mainly using hexanediol, one of the spinning solvents of the present application, to surface treat the monodisperse mesoporous hollow silica sphere complex to improve its compatibility in polyethylene and make it evenly dispersed in polyethylene.
[0017] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 6% to 18%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 5-9%; With the addition of inorganic additives, the peel strength of the polyethylene film continues to increase and eventually tends to balance. However, if too much inorganic additives are added, the bending performance of the polyethylene film will deteriorate, that is, the feel will deteriorate, affecting the use of the product. Therefore, it is necessary to select a better range between peel strength and bending performance to meet the actual use of the product.
[0018] (4) Preparation of waterproof polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the temperature of flash spinning is 160°C to 230°C; The hot pressing temperature is 110℃~120℃.
[0019] Test standards for this application: Peel strength: Industry standard FZ / T 80007.1-2006 uses the peel strength test method for adhesive interlining garments.
[0020] Bending length: in accordance with GB / T 18318-2001 (Determination of bending length of textile fabrics).
[0021] Compared with the prior art, the present invention has the following positive effects: 1. The present invention improves the peeling strength of the polyethylene film by adding an inorganic additive with monodisperse mesoporous hollow silica spheres, thereby expanding the application range of the polyethylene film.
[0022] 2. The present invention controls the amount of inorganic additives containing monodisperse mesoporous hollow silica spheres added so that the polyethylene film has a smaller bending length, thereby allowing the polyethylene film to maintain its proper feel. DETAILED DESCRIPTION
[0024] The present invention is further described in detail below in conjunction with specific implementation methods.
[0025] Example 1 This embodiment provides a method for preparing a polyethylene film with high peel strength, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 8:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0026] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 20 g / L.
[0027] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 8%; The mass fraction of the inorganic additive in the raw material of the polyethylene film (a mixture of polyethylene and the inorganic additive) is 5%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 190°C; The hot pressing temperature is 110°C.
[0028] The test results of the polyethylene film prepared in this example are shown in Table 1. Example 2 This embodiment provides a method for preparing a polyethylene film with high peel strength, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 10:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0030] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 25 g / L.
[0031] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 11%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 7%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0032] The test results of the polyethylene film prepared in this example are shown in Table 1. Example 3 This embodiment provides a method for preparing a polyethylene film with high peel strength, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 12:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0034] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 30 g / L.
[0035] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 14%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 9%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 220°C; The hot pressing temperature is 118°C.
[0036] The test results of the polyethylene film prepared in this example are shown in Table 1. Comparative Example 1 This comparative example provides a method for preparing a polyethylene film, and the specific steps are as follows: (1) Preparation of spinning solution: polyethylene is added to a spinning solvent for dispersion to obtain a spinning solution; In step (1), the mass fraction of polyethylene in the spinning solution is 11%; The spinning solvent was dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane in a mass ratio of 7:2:1; (2) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (2), and then hot pressing to obtain a polyethylene film; In step (2), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0038] The test results of the polyethylene film prepared in this comparative example are shown in Table 1. Comparative Example 2 This comparative example provides a method for preparing a polyethylene film, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 10:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0040] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 25 g / L.
[0041] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 11%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 2%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0042] The test results of the polyethylene film prepared in this comparative example are shown in Table 1. Comparative Example 3 This comparative example provides a method for preparing a polyethylene film, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 10:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0044] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 25 g / L.
[0045] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 11%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 11%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0046] The test results of the polyethylene film prepared in this comparative example are shown in Table 1. Comparative Example 4 This comparative example provides a method for preparing a polyethylene film, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium chloride are dispersed in a sulfuric acid aqueous solution, stirred by microwaves for reaction, filtered, and the filtrate is dried to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), The mass ratio of monodisperse mesoporous hollow silica spheres to barium chloride is 10:1; The mass fraction of the aqueous sulfuric acid solution is 15%, and the sulfuric acid is kept in excess.
[0048] (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 25 g / L.
[0049] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 11%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 13%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0050] The test results of the polyethylene film prepared in this comparative example are shown in Table 1. Comparative Example 5 This comparative example provides a method for preparing a polyethylene film, and the specific steps are as follows: (1) Preparation of inorganic additives: Monodisperse mesoporous hollow silica spheres and barium sulfate are dispersed and directly mixed to obtain a monodisperse mesoporous hollow silica sphere composite; In step (1), the mass ratio of monodisperse mesoporous hollow silica spheres to barium sulfate is 10:1; (2) Preparation of a spinning solvent containing an inorganic auxiliary agent: dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step (1) in hexylene glycol, stirring at high speed and ultrasonically dispersing the mixture, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic auxiliary agent; In step (2), the mass ratio of dichloromethane, hexanediol, and 1,1,1,3,3-pentafluorobutane is 7:2:1; The mass concentration of the monodisperse mesoporous hollow silica sphere composite in hexanediol is 25 g / L.
[0052] The high-speed stirring speed is 2000-3000 rpm; the dispersion time is 2-3h; (3) Preparation of spinning solution: adding polyethylene to the spinning solvent containing inorganic additives prepared in step (2) for dispersion to obtain a spinning solution; In step (3), the mass fraction of polyethylene in the spinning solution is 11%; The mass fraction of inorganic additives in the raw material of polyethylene film (mixture of polyethylene and inorganic additives) is 7%; (4) Preparation of polyethylene film: flash spinning the spinning solution prepared in step (3), and then hot pressing to obtain a polyethylene film; In step (4), the flash spinning temperature is 206°C; The hot pressing temperature was 114°C.
[0053] The test results of the polyethylene film prepared in this comparative example are shown in Table 1. Table 1 Test data table of this application Peel strength N Bending length cm Example 1 2.8 6.2 Example 2 3.9 6.8 Example 3 5.3 7.6 Comparative Example 1 0.8 4.5 Comparative Example 2 1.3 5.2 Comparative Example 3 5.9 10.0 Comparative Example 4 6.2 11.0 Comparative Example 5 1.1 4.9 Result analysis: It can be seen from the above experimental results that with the addition of inorganic additives, the peel strength of the polyethylene film is increased simultaneously, while the bending length is reduced. Therefore, the inorganic additive provided by the present invention is limited to the value range of 5-9% by mass fraction in the raw material of the polyethylene film, and the polyethylene film prepared can take into account the properties of both peel strength and bending length, achieving the intended purpose of the present invention.
[0055] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
Claims
1. A polyethylene film with high peel strength, characterized in that: The raw materials of the polyethylene film include polyethylene and inorganic additives, wherein the inorganic additives include a monodisperse mesoporous hollow silica sphere composite, and the peeling strength F of the polyethylene film is greater than 1.5N; the monodisperse mesoporous hollow silica sphere composite is a monodisperse mesoporous hollow silica sphere loaded with barium sulfate.
2. A polyethylene film with high peel strength as claimed in claim 1, characterized in that: The mass fraction of the inorganic additive in the raw material of the polyethylene film is 5-9%.
3. A polyethylene film with high peel strength as claimed in claim 2, characterized in that: The mass fraction of the inorganic additive in the raw material of the polyethylene film is 5-7%.
4. A polyethylene film with high peel strength as claimed in claim 2, characterized in that: The mass fraction of the inorganic additive in the raw material of the polyethylene film is 7-9%.
5. A polyethylene film with high peel strength as claimed in claim 1, characterized in that: The peel strength F of the polyethylene film is greater than 2.5N.
6. A polyethylene film with high peel strength as claimed in claim 1, characterized in that: The peel strength F of the polyethylene film is greater than 3.5N.
7. A polyethylene film with high peel strength as claimed in claim 1, characterized in that: The peel strength F of the polyethylene film is greater than 4.5N.
8. A polyethylene film with high peel strength as claimed in claim 1, characterized in that: The peel strength F of the polyethylene film is greater than 5.5N.
9. A method for preparing a polyethylene film with high peel strength as claimed in any one of claims 1 to 8, characterized in that: The following steps are involved: Step 1: Preparation of inorganic additives, dispersing monodisperse mesoporous hollow silica spheres and barium chloride in a sulfuric acid aqueous solution, stirring with microwaves for reaction, filtering and drying the filtrate to obtain a monodisperse mesoporous hollow silica sphere composite; Step 2: Preparation of a spinning solvent containing an inorganic additive, dispersing the monodisperse mesoporous hollow silica sphere composite obtained in step 1 in hexylene glycol, stirring at high speed and ultrasonically dispersing, and finally adding dichloromethane and 1,1,1,3,3-pentafluorobutane to obtain a spinning solvent containing an inorganic additive; Step 3: preparing a spinning solution, adding polyethylene into the spinning solvent containing an inorganic auxiliary agent prepared in step 2 and dispersing the polyethylene to obtain a spinning solution; Step 4: Preparation of polyethylene film: flash spinning the spinning solution prepared in step 3, and then hot pressing to obtain a polyethylene film.
10. The preparation method according to claim 9, characterized in that: The stirring speed in the step 2 is 2000-3000 rpm, and the dispersion time is 2-3 hours; the mass ratio of dichloromethane, hexylene glycol and 1,1,1,3,3-pentafluorobutane is 7:2:1.
Citation Information
Patent Citations
Label for in-mold molding, in-mold molded article and method for molding same
CN102576502A
Thin film material for processing use
CN104968720A
Laminated porous film, and production method therefor
CN105992691A
Composition
CN110573673A
Microwave heat sealing flash evaporation spinning non-woven fabric process method, microwave heat sealing device and non-woven fabric preparation equipment
CN114657701A
Cited By
Flash spinning sheet material with better single stripping degree and application of flash spinning sheet material