CrSi thin-film resistor preparation method and CrSi thin-film resistor

The dry etching process simplifies the preparation process of CrSi thin film resistors, solves the problem of complex processes in large-size wafers, achieves morphology control and structural simplification, and is suitable for mass production.

CN118843391AInactive Publication Date: 2024-10-25GUANGZHOU CANSEMI TECH INC

Patent Information

Application Number
CN202411321824.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-23
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The process of preparing CrSi thin film resistors in large-size wafers is complex and involves many procedures, making it difficult to accurately control the morphology and simplify the structure.

Method used

The dry etching process is used to simplify the process flow and control the resistance morphology by depositing a dielectric layer on the substrate, embedding metal wires, forming through holes, filling metal compounds, depositing CrSi films and performing high-temperature annealing, and finally wrapping the insulating layer.

Benefits of technology

The preparation process of simplifying the CRSI film resistance on large -scale wafers, improving the appearance control accuracy and simplicity of structure, shortening the research and development cycle, saving the cost of processing raw materials, and suitable for large quantities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118843391A_ABST
    Figure CN118843391A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a CrSi thin-film resistor and the CrSi thin-film resistor, relates to the technical field of semiconductors, and solves the problem that the preparation process of the CrSi thin-film resistor in the related technology is complicated. The CrSi thin-film resistor is etched by adopting a dry etching process, so that the morphology of the thin-film resistor can be well controlled, and the quality of the thin-film resistor is improved. And the CrSi thin-film resistor in the scheme is simpler in structure. For large-scale production of large-size wafers, the preparation process of the CrSi thin-film resistor is simple and convenient, and the morphology of the thin-film resistor can be effectively controlled, so that the CrSi thin-film resistor has great advantages, and the production efficiency can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a method for preparing a CrSi thin film resistor and a CrSi thin film resistor. Background Art

[0002] In circuit applications, thin film resistors play a very important role, such as CrSi (chrome silicon) thin film resistors. CrSi thin film resistors are a commonly used high-resistance thin film material with the characteristics of high resistivity, good stability, and small temperature coefficient. Correspondingly, thin film resistors can protect circuits, adjust signals, and oscillate. However, in related technologies, thin film resistors are usually prepared in small-sized wafers such as 8-inch wafers. The preparation of thin film resistors mainly uses a dry etching process to etch and remove the film layer. Although compared with the wet etching process, this solution can more accurately control the removal changes of the film layer. However, in large-sized wafers such as 12-inch wafers, the preparation process is relatively more complicated and involves more processing steps. Summary of the invention

[0003] The present application provides a CrSi thin film resistor preparation method and a CrSi thin film resistor, which solves the problem of complex preparation process of CrSi thin film resistors in related technologies. The preparation process of the present application is simple, the morphology of the thin film resistor can be well controlled, and the structure is simpler.

[0004] In a first aspect, the present application provides a method for preparing a CrSi thin film resistor, the method comprising: Providing a substrate, and depositing a first dielectric layer on the substrate; embedding a metal wire on the first dielectric layer; Depositing a second dielectric layer on the first dielectric layer, and etching the second dielectric layer to form a through hole connected to the metal wire; Filling the vias with metallic compounds; A CrSi thin film resistor having a preset length is deposited on the second dielectric layer; A third dielectric layer is deposited on the CrSi thin film resistor to wrap the CrSi thin film resistor.

[0005] In some embodiments, depositing a second dielectric layer on the first dielectric layer, and etching the second dielectric layer to form a through hole connected to the metal wire, comprises: Based on the chemical vapor deposition process, a second dielectric layer is deposited on the first dielectric layer, and the second dielectric layer is used to block metal diffusion; After photoresist is coated on the second dielectric layer, exposure and development are performed, and through holes connected to the metal wires are formed by etching in the second dielectric layer.

[0006] In some embodiments, the vias are filled with a metal compound, including: Based on a physical vapor deposition process, the through hole is filled and a metal deposition layer is formed on the second dielectric layer; The metal deposition layer is ground to remove the metal compound on the surface of the second dielectric layer and to retain the metal compound filled in the through hole.

[0007] In some embodiments, grinding the metal deposition layer to remove the metal compound on the surface of the second dielectric layer and retain the metal compound filled in the through hole includes: Based on the chemical mechanical polishing process, the metal deposition layer is polished to planarize the second dielectric layer; According to the preset processing accuracy, the thickness of chemical etching and mechanical grinding is controlled to remove the metal compounds on the surface of the second dielectric layer.

[0008] In some embodiments, the vias are arranged in pairs in the second dielectric layer in areas above corresponding metal wires.

[0009] In some embodiments, a CrSi thin film resistor having a preset length is formed by depositing the second dielectric layer, including: Depositing a CrSi film on the second dielectric layer and performing a high temperature annealing process; A partial area of ​​the CrSi film is removed to form a CrSi thin film resistor with a preset length on the second dielectric layer.

[0010] In some embodiments, removing a portion of the CrSi film to form a CrSi thin film resistor having a preset length on the second dielectric layer includes: Coating a photoresist on the CrSi film, and exposing and developing the photoresist according to a preset mask; Etching the CrSi film to remove the peripheral area of ​​the CrSi film; The remaining CrSi film covers the area where the metal wire is located to form a CrSi film resistor.

[0011] In some embodiments, when two metal wires are disposed in the first dielectric layer, before coating a photoresist on the CrSi film and exposing and developing the photoresist according to a preset mask, the method further includes: A mask pattern matching the distance between the two metal wires is selected so that the length of the CrSi thin film resistor matches the distance between the two metal wires.

[0012] In some embodiments, the first dielectric layer, the second dielectric layer, and the third dielectric layer are all insulating layers formed by depositing insulating materials.

[0013] In a second aspect, the present application further provides a CrSi thin film resistor, which is prepared according to the CrSi thin film resistor preparation method described in the first aspect.

[0014] The CrSi thin film resistor of the present application is etched by a dry etching process, which can well control the morphology of the thin film resistor. Compared with the existing CrSi thin film resistor structure, the CrSi thin film resistor of the present application is simpler in structure and has a simpler process flow. The etching process is relatively simple, which can shorten the research and development cycle and save a certain amount of processing raw material costs. It has great advantages in being applied to mass production of large-size wafers. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 A schematic diagram of the steps of a method for preparing a CrSi thin film resistor provided in one embodiment of the present application.

[0016] Figure 2 A schematic diagram of the steps of preparing a CrSi thin film resistor on a second dielectric layer provided in one embodiment of the present application.

[0017] Figure 3 A schematic structural cross-sectional diagram of a process for preparing a CrSi thin film resistor provided in one embodiment of the present application. DETAILED DESCRIPTION

[0018] The embodiments of the present application are further described in detail below in conjunction with the accompanying drawings and examples. It is to be understood that the specific embodiments described herein are only used to explain the embodiments of the present application, rather than to limit the embodiments of the present application. It should also be noted that, for ease of description, only the parts related to the embodiments of the present application rather than all structures are shown in the accompanying drawings, and those skilled in the art should be able to think of it after reading the specification of this application that as long as the technical features do not contradict each other, any combination of the technical features can constitute an optional implementation method.

[0019] The terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects, and are not used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable when appropriate, so that the embodiments of the present application can be implemented in an order other than those illustrated or described here, and the objects distinguished by "first", "second", etc. are generally a class, and the number of objects is not limited. For example, the first object can be one or more. In addition, "and / or" in the specification and claims represents at least one of the connected objects, and the character " / " generally represents that the objects associated before and after are in an "or" relationship. In the description of the present application, "multiple" means two or more, and "several" means one or more.

[0020] CrSi thin film resistors are commonly used high-resistance thin film materials with high resistivity, good stability and small temperature coefficient. They can usually play a role in protecting circuits, adjusting signals and oscillations. In related technologies, thin film resistors are usually prepared in small-sized wafers such as 8-inch wafers, but in large-sized wafers such as 12-inch wafers, the preparation process of thin film resistors is relatively more complicated and requires more processing steps.

[0021] In this regard, the present application provides a method for preparing a CrSi thin film resistor, such as Figure 1 As shown, Figure 1 The schematic diagram of the steps of the CrSi thin film resistor preparation method provided in an embodiment of the present application is to deposit a dielectric layer on a substrate and prepare a thin film resistor, and to etch using a dry etching process, which can well control the morphology of the thin film resistor. Compared with the existing CrSi thin film resistor preparation structure, the structure is simpler and the process flow is more concise. The specific steps include step S110-step S160: Step S110 , providing a substrate, and depositing a first dielectric layer on the substrate.

[0022] For a wafer, the wafer is used as a substrate, and then a first dielectric layer is deposited thereon. The first dielectric layer is an insulating layer. For example, a layer of insulating material is deposited on the substrate by chemical vapor deposition to serve as the first dielectric layer.

[0023] Step S120: embedding metal wires on the first dielectric layer.

[0024] It is conceivable that the metal wire is exposed on the surface of the first dielectric layer. During the preparation process, a photoresist can be coated on the first dielectric layer, and the photoresist is exposed and developed, and then the first dielectric layer is etched to form a groove capable of accommodating the metal wire, and then the metal wire is embedded in the groove. Optionally, in some embodiments, the metal wire can be formed by depositing metal in the groove. It should be conceivable that when multiple metal wires are embedded, the number of etched grooves is consistent with the number of metal wires to be formed.

[0025] Step S130 , depositing a second dielectric layer on the first dielectric layer, and etching the second dielectric layer to form through holes connected to the metal wires.

[0026] After the metal wire is embedded, a second dielectric layer is deposited on the first dielectric layer, and the second dielectric layer is also an insulating layer. It can be imagined that the second dielectric layer covers the location of the metal wire. Correspondingly, a through hole is etched on the second dielectric layer corresponding to the location of the metal wire, and the through hole is connected to the metal wire, that is, the through hole serves as a connecting hole to facilitate filling of metal compounds to achieve connection between the upper and lower surfaces of the second dielectric layer. Optionally, in one embodiment, the through holes are arranged in pairs in the second dielectric layer corresponding to the area above the metal wire, so that the CrSi thin film resistor on the second dielectric layer can be connected to the metal wire through the through holes arranged in pairs.

[0027] For example, in one embodiment, the deposition of the second dielectric layer on the first dielectric layer may be performed based on a chemical vapor deposition process, and the preparation of the through hole may be performed based on a photolithography process, and the specific steps include step S131-step S132: Step S131 : Based on a chemical vapor deposition process, a second dielectric layer is deposited on the first dielectric layer to form a second dielectric layer, where the second dielectric layer is used to block metal diffusion.

[0028] Step S132: After coating the photoresist on the second dielectric layer, performing exposure and development, and etching the second dielectric layer to form a through hole connected to the metal wire.

[0029] It can be understood that the second dielectric layer is formed on the first dielectric layer by chemical vapor deposition, and the second dielectric layer covers the metal wire, that is, an insulating material is deposited on the metal wire to cover the metal wire, and the second dielectric layer can be used to block metal diffusion. Accordingly, in the area of ​​the second dielectric layer covering the metal wire, corresponding through holes need to be prepared to connect the metal wire.

[0030] Then, a photoresist is coated on the second dielectric layer, and then exposed and developed to form an area corresponding to the through hole on the photoresist, and then the second dielectric layer in the area is etched to form a through hole in the second dielectric layer. It can be imagined that the position of the through hole corresponds to the metal wire, that is, the area where the through hole is located in the second dielectric layer is located is above the metal wire. In this regard, the through hole can connect the metal wire, thereby realizing the connection between the upper and lower surfaces of the second dielectric layer.

[0031] Step S140: filling the through hole with a metal compound.

[0032] After the through hole is etched, the through hole is filled with a metal compound to achieve connection between the upper and lower surfaces of the second dielectric layer. In one implementation, the through hole can be filled by depositing a metal compound on the second dielectric layer to form a metal deposition layer to achieve filling of the through hole. The specific steps include step S141-step S142: Step S141 : filling the through hole and depositing a metal deposition layer on the second dielectric layer based on a physical vapor deposition process.

[0033] Step S142 : grinding the metal deposition layer to remove the metal compound on the surface of the second dielectric layer and retaining the metal compound filled in the through hole.

[0034] It can be understood that based on the physical vapor deposition process, the metal compound is deposited on the second dielectric layer by physical vapor deposition. For this, the metal compound can fill the through hole and form a metal deposition layer on the second dielectric layer. Then, the metal deposition layer is mechanically ground to remove the metal compound on the surface of the second dielectric layer. It is worth noting that the mechanical grinding process can be completed by an existing grinder. The grinding method of the grinder refers to the relevant technology and will not be described in detail. In addition, since the through hole runs through the second dielectric layer, the metal compound deposited in the second dielectric layer will fill the through hole, and then only the metal compound on the surface of the second dielectric layer is removed during grinding, and the metal compound filled in the through hole is retained.

[0035] It is conceivable that during the preparation process, the thickness of the metal deposition layer can be controlled by controlling the duration of physical vapor deposition. Since the metal deposition layer needs to be ground and removed in the end, the thickness of the metal deposition layer can be thinner to reduce the grinding time.

[0036] Step S150 , depositing a CrSi thin film resistor having a preset length on the second dielectric layer.

[0037] After removing the metal compound on the surface of the second dielectric layer, a CrSi film is deposited on the second dielectric layer to serve as a CrSi thin film resistor. It is conceivable that the CrSi thin film resistor can cover the location of the through hole. To this end, the CrSi thin film resistor can be connected to the metal wire through the metal compound filled in the through hole, and the second dielectric layer is an insulating layer for separating the metal wire and the CrSi thin film resistor. After depositing a CrSi thin film on the second dielectric layer, the CrSi thin film can be etched to form a CrSi thin film resistor with a preset length.

[0038] Step S160 , depositing a third dielectric layer on the CrSi thin film resistor to wrap the CrSi thin film resistor with the third dielectric layer.

[0039] In addition, after forming the CrSi thin film resistor, it is necessary to deposit an insulating layer on the CrSi thin film resistor to form a third dielectric layer on the CrSi thin film resistor, and the CrSi thin film resistor is wrapped by the third dielectric layer to protect the CrSi thin film resistor. It can be imagined that the third dielectric layer is also on the second dielectric layer, and is deposited on the second dielectric layer by chemical vapor deposition. Since there is a CrSi thin film resistor on the second dielectric layer, the third dielectric layer is on the CrSi thin film resistor in the area corresponding to the CrSi thin film resistor on the second dielectric layer, thereby wrapping the CrSi thin film resistor.

[0040] From the above scheme, it can be seen that the CrSi thin film resistor of the present application scheme can well control the morphology of the thin film resistor by etching with a dry etching process, and the CrSi thin film resistor of the present application scheme is simpler in structure. For mass production of large-size wafers, the preparation process of the CrSi thin film resistor of the present application scheme is simple, and the morphology of the thin film resistor can be effectively controlled, so that it has a great advantage and helps to improve production efficiency.

[0041] In one embodiment, after the metal deposition layer is deposited on the surface of the second dielectric layer, after the through hole is filled, it is necessary to retain the metal compound in the through hole and remove the metal compound on the surface of the second dielectric layer. In this regard, based on the chemical mechanical polishing process, the metal deposition layer is ground to flatten the second dielectric layer, such as by using a grinder to grind the metal deposition layer on the second dielectric layer, and according to the preset processing accuracy, the thickness of chemical etching and mechanical grinding is controlled to remove the metal compound on the surface of the second dielectric layer. It can be imagined that the thickness of chemical etching and mechanical grinding matches the thickness of the metal deposition layer on the surface of the second dielectric layer to completely remove the metal compound on the surface of the second dielectric layer, so as to better deposit the CrSi film.

[0042] Figure 2 A schematic diagram of steps for preparing a CrSi thin film resistor on a second dielectric layer provided in an embodiment of the present application. In one embodiment, after removing the metal deposit on the second dielectric layer, a CrSi thin film is deposited on the second dielectric layer to form a corresponding CrSi thin film resistor. The specific steps are as follows: Step S210: depositing a CrSi film on the second dielectric layer and performing a high temperature annealing process.

[0043] Step S220: removing a portion of the CrSi film to form a CrSi thin film resistor with a preset length on the second dielectric layer.

[0044] It is understandable that after the CrSi film is deposited on the second dielectric layer, it needs to be subjected to high temperature annealing. High temperature annealing is a heat treatment process in which the material is exposed to high temperature for a period of time and then slowly cooled. In this regard, the density of the CrSi film is better, so as to facilitate the preparation of CrSi thin film resistors. Then, part of the CrSi film is removed. It can be imagined that the CrSi film needs to cover the position of the through hole. For this, part of the area at both ends of the CrSi film can be removed so that a CrSi thin film resistor with a preset length can be formed on the second dielectric layer.

[0045] It should be noted that, in one embodiment, part of the CrSi film may be removed after being deposited to form a CrSi film with a preset length on the second dielectric layer, and finally a high-temperature annealing treatment is performed to form a CrSi thin film resistor with good density.

[0046] Optionally, in one embodiment, by coating a photoresist on the CrSi film, and then selecting a preset mask to expose and develop the photoresist, it is conceivable that the pattern of the mask is adapted to the CrSi film with a preset length to be formed, such as when the remaining CrSi film needs to cover the area where the metal wire is located, the pattern of the mask is adapted to cover the area where the metal wire is located, and then after exposure and development, the photoresist outside the area is removed, so as to facilitate etching of the CrSi film not covered by the photoresist (using this part as the peripheral area of ​​the CrSi film), and to achieve the removal of the peripheral area of ​​the CrSi film, thereby forming a CrSi thin film resistor with a preset length. In this regard, by high-temperature annealing and removing part of the CrSi film, the CrSi thin film resistor formed on the second dielectric layer has better compactness and can also meet the length requirements, thereby meeting the application requirements in the circuit.

[0047] In some embodiments, two metal wires are provided, and correspondingly, the length of the formed CrSi thin film resistor can cover the two metal wires, such as the length of the CrSi thin film resistor on the second dielectric layer is equal to the distance between the two metal wires, wherein the distance between the two metal wires is the maximum spacing between the two metal wires, that is, the distance between the outermost sides of the two metal wires. In this regard, the pattern of the selected mask is matched to the distance between the two metal wires, and then after exposure and development, a corresponding length of photoresist is reserved so that the length of the CrSi thin film resistor formed by etching matches the distance between the two metal wires.

[0048] Figure 3This is a schematic diagram of a cross-sectional structure of a process for preparing a CrSi thin film resistor according to an embodiment of the present application. In the figure, (a)-(h) represent the cross-section of the device structure during the preparation process, and arrows indicate the order in which each device structure is generated during the preparation process. Figure 3 The preparation process is described.

[0049] A first dielectric layer 102 is deposited on the substrate, and a photoresist is coated on the first dielectric layer 102, and the photoresist is exposed and developed, and then the first dielectric layer 102 is etched to form a groove capable of accommodating the metal wire 101, and then the metal wire 101 is embedded in the groove, wherein two metal wires 101 are provided. In addition, a second dielectric layer 103 is deposited on the first dielectric layer 102. That is, as shown in FIG. Figure 3 The device structure shown in (a).

[0050] Further, a photoresist is coated on the second dielectric layer 103 to form a photoresist layer 104, and then exposed and developed, thereby forming a corresponding channel in the photoresist layer 104, so as to facilitate etching the second dielectric layer 103 to form a corresponding through hole 201. The specific structure is as follows: Figure 3 After etching the through hole 201 in the second dielectric layer 103, the photoresist on the second dielectric layer 103 needs to be removed. The device structure after removing the photoresist is as shown in FIG. Figure 3 As shown in (c), the through hole 201 is used to connect the metal wire 101, and the through hole 201 is located on the second dielectric layer 103 corresponding to the metal wire 101. The through holes 201 are arranged in pairs, that is, two through holes are arranged at the second dielectric layer 103 corresponding to the position of each metal wire 101.

[0051] Then, the through hole 201 is filled with a metal compound 202. The device structure after filling is as follows: Figure 3 As shown in (d), a layer of metal compound can be deposited on the second dielectric layer 103 by physical vapor deposition to fill the through holes, and then the metal compound can be polished by CMP (Chemical Mechanical Polishing) until the metal compound on the surface of the second dielectric layer 103 is completely removed and the through holes filled with the metal compound are exposed.

[0052] After filling the through hole, a CrSi film 105 is deposited on the second dielectric layer 103. The specific structure is as follows Figure 3 Then, a photoresist is coated on the CrSi film 105 to form a photoresist layer 104, and the photoresist layer 104 is exposed and developed. Accordingly, the specific structure is as follows: Figure 3As shown in (f) in the figure. In this regard, the CrSi film 105 is etched to remove a portion of the CrSi film 105, thereby forming a CrSi thin film resistor with a preset length on the second dielectric layer 103. The specific structure is as follows: Figure 3 As shown in (g).

[0053] Finally, it is necessary to deposit a third dielectric layer 106 on the CrSi thin film resistor. For example, a layer of insulating material is deposited on the CrSi thin film resistor by physical vapor deposition to form the third dielectric layer 106. The third dielectric layer 106 wraps the CrSi thin film resistor to protect the CrSi thin film resistor. The specific structure is as follows: Figure 3 As shown in (h).

[0054] In this regard, the CrSi thin film resistor of this scheme is etched by a dry etching process, which can well control the morphology of the thin film resistor. Compared with the existing CrSi thin film resistor structure, the CrSi thin film resistor of this scheme is simpler in structure and the process flow is also simpler. The etching process is relatively simple, which can shorten the R&D cycle and save a certain amount of processing raw material costs. It has great advantages in mass production of large-size wafers.

[0055] The present application also provides a CrSi thin film resistor, which is prepared by the above-mentioned CrSi thin film resistor preparation method. The CrSi thin film resistor has a simple structure, and the morphology of the CrSi thin film resistor can meet application requirements. It has high resistivity, good stability, and a small temperature coefficient.

[0056] It should also be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, commodity or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, commodity or device. In the absence of more restrictions, the elements defined by the sentence "comprises a ..." do not exclude the existence of other identical elements in the process, method, commodity or device including the elements.

[0057] Note that the above are only preferred embodiments of the present application and the technical principles used. Those skilled in the art will understand that the present application is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present application. Therefore, although the present application is described in more detail through the above embodiments, the present application is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present application, and the scope of the present application is determined by the scope of the appended claims.

Claims

1. A method for preparing a CrSi thin film resistor, characterized in that: include: Providing a substrate, and depositing a first dielectric layer on the substrate; embedding a metal wire on the first dielectric layer; Depositing a second dielectric layer on the first dielectric layer, and etching the second dielectric layer to form a through hole connected to the metal wire; filling the through-hole with a metal compound; Depositing a CrSi thin film resistor having a preset length on the second dielectric layer; A third dielectric layer is deposited on the CrSi thin film resistor to wrap the CrSi thin film resistor through the third dielectric layer.

2. The method for preparing a CrSi thin film resistor according to claim 1, characterized in that: The step of depositing a second dielectric layer on the first dielectric layer, and etching the second dielectric layer to form a through hole connected to the metal wire, comprises: Based on a chemical vapor deposition process, depositing the second dielectric layer on the first dielectric layer, the second dielectric layer is used to block metal diffusion; After photoresist is coated on the second dielectric layer, exposure and development are performed, and through holes connected to the metal wires are formed by etching the second dielectric layer.

3. The method for preparing a CrSi thin film resistor according to claim 1, characterized in that: The method of filling the through hole with a metal compound comprises: Based on a physical vapor deposition process, filling the through hole and depositing a metal deposition layer on the second dielectric layer; The metal deposition layer is ground to remove the metal compound on the surface of the second dielectric layer and to retain the metal compound filled in the through hole.

4. The method for preparing a CrSi thin film resistor according to claim 3, characterized in that: The step of grinding the metal deposition layer to remove the metal compound on the surface of the second dielectric layer and retaining the metal compound filled in the through hole comprises: Based on a chemical mechanical polishing process, grinding the metal deposition layer to planarize the second dielectric layer; According to the preset processing accuracy, the thickness of chemical etching and mechanical grinding is controlled to remove the metal compound on the surface of the second dielectric layer.

5. The method for preparing a CrSi thin film resistor according to claim 3 or 4, characterized in that: The through holes are arranged in pairs in the second dielectric layer in an area corresponding to above the metal wires.

6. The method for preparing a CrSi thin film resistor according to claim 1, characterized in that: The step of depositing a CrSi thin film resistor having a preset length on the second dielectric layer comprises: Depositing a CrSi film on the second dielectric layer and performing a high temperature annealing process; A partial area of ​​the CrSi film is removed to form a CrSi thin film resistor with a preset length on the second dielectric layer.

7. The method for preparing a CrSi thin film resistor according to claim 6, characterized in that: The removing of a part of the CrSi film to form a CrSi thin film resistor having a preset length on the second dielectric layer includes: Coating a photoresist on the CrSi film, and exposing and developing the photoresist according to a preset mask; Etching the CrSi film to remove the peripheral area of ​​the CrSi film; The remaining CrSi film covers the area where the metal wire is located to form a CrSi thin film resistor.

8. The method for preparing a CrSi thin film resistor according to claim 7, characterized in that: In the case where two metal wires are disposed in the first dielectric layer, before coating photoresist on the CrSi film and exposing and developing the photoresist according to a preset mask, the method further comprises: A mask pattern matching the distance between the two metal wires is selected so that the length of the CrSi thin film resistor matches the distance between the two metal wires.

9. The method for preparing a CrSi thin film resistor according to claim 1, characterized in that: The first dielectric layer, the second dielectric layer and the third dielectric layer are all insulating layers formed by depositing insulating materials.

10. A CrSi thin film resistor, characterized in that: The CrSi thin film resistor is prepared according to the method for preparing a CrSi thin film resistor according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Electronic component

    CN115244692A

  • Semiconductor device and forming method thereof

    CN117497513A

  • Semiconductor device and method of manufacturing the same

    CN118284970A

Cited By

  • CrSi thin-film resistor preparation method, resistance device preparation method and resistance device

    CN119768045A

  • CrSi thin film resistor preparation method, resistor device preparation method, and resistor device

    CN119768045B