White light-emitting material for electroluminescence, application of white light-emitting material, white light-emitting transistor with planar light source configuration and application of white light-emitting transistor

By using phosphorescent materials and guest-doped host materials in OLET, efficient energy transfer and white light emission are achieved, solving the problem of poor white light performance of OLET, reaching 13.9% external quantum efficiency and low driving voltage, promoting its advancement in display technology applications in.

CN118853142APending Publication Date: 2024-10-29INST OF CHEM CHINESE ACAD OF SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410523350.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-28
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

Existing organic light-emitting transistors (OLETs) have great challenges in emitting white light performance. Low external quantum efficiency and limited tunable color emission limit their application in display technology.

Method used

White luminescent materials containing phosphorescent materials and guest-doped host materials are used. By adding phosphorescent and fluorescent guests in the active layer, efficient energy transfer is achieved, and by precisely regulating the energy transfer between the host and the guest, high external quantum efficiency and Controllable white light emission.

Benefits of technology

It achieves an external quantum efficiency of up to 13.9%, small efficiency roll-off and high loop stability, as well as a driving voltage below 5V, supporting full-color display and lighting applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118853142A_ABST
    Figure CN118853142A_ABST
Patent Text Reader

Abstract

The invention relates to the field of organic light-emitting transistors for emitting white light, and discloses a white light-emitting material for electroluminescence, application of the white light-emitting material, a white light-emitting transistor with an area light source plane structure and application of the white light-emitting transistor. The materials include: a phosphorescent material and a guest-doped host material. According to the efficient and stable area emission type OLET based on unique lateral integrated device configuration provided by the invention, effective energy transfer of phosphorescent and fluorescent objects is added in the active layer of the device, so that controllable emission color even white light emission becomes possible. High external quantum efficiency (EQE) of 13.9%, smaller efficiency roll-off and higher loop stability, and high Ion / Ioff ratio of 105 and effective gate adjustability of ultra-low driving voltage lower than 5V are achieved. The 4 * 6 white light emitting OLET array is used for full-color display, which shows that the 4 * 6 white light emitting OLET array has huge application potential in the aspect of advanced display technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of organic light-emitting transistors emitting white light, and in particular to a white light-emitting material for electroluminescence and its application, and a white light-emitting transistor with a planar configuration of a surface light source and its application. Background Art

[0002] Organic light-emitting transistors (OLETs) are an emerging integrated optoelectronic device that has the dual functions of electrical switching of organic field-effect transistors (OFETs) and light emission of organic light-emitting diodes (OLEDs). The unique integrated device structure of OLETs gives them great technological application potential in the fields of next-generation smart displays, integrated optoelectronics, and optical communications. However, compared with other optoelectronic devices, the development of OLETs is still seriously lagging, mainly due to the limited high-performance active materials and immature device manufacturing processes.

[0003] As a possible smallest integrated optoelectronic device, OLET requires its active materials to integrate high carrier mobility and strong solid-state emission properties in one molecule to achieve charge transport and light emission functions. The development of such materials remains challenging due to the conflict between high mobility and strong emission in terms of molecular structure and packaging. On the other hand, from the perspective of improving the efficiency of OLET devices, it remains unclear how to balance charge injection and transport and effectively improve light coupling output.

[0004] In recent years, a series of advanced progress has been made in the design of constituent materials and the optimization of device manufacturing technology. For example, through molecular design innovation, some new organic semiconductor molecules that combine high carrier mobility and strong emissivity have been developed. In addition, the strategies of molecular doping and co-crystal engineering have also been applied to develop high-mobility emissive organic semiconductor systems. High-performance vertical OLETs with low voltage and low power characteristics have been achieved through single-walled carbon nanotube network source electrodes for red, green and blue light emission.

[0005] However, despite these impressive advances in the field of OLETs, their overall performance remains relatively poor, with most external quantum efficiency (EQE) values ​​below 1%, and the development of tunable color emission and even white OLETs is very limited.

[0006] Therefore, it remains challenging to fabricate high-performance stable OLET devices with tunable color emission or even white emission, which is urgently needed to promote the application of OLET in display technology. Summary of the invention

[0007] The purpose of the present invention is to overcome the problem of poor performance of OLET in emitting white light in the prior art, and to provide a white light-emitting material and application for electroluminescence, as well as a white light-emitting transistor and application in a planar configuration of a surface light source.

[0008] In order to achieve the above-mentioned object, the first aspect of the present invention provides a white light-emitting material for electroluminescence, wherein the material comprises: a phosphorescent material and a guest-doped host material, wherein the guest in the guest-doped host material is 5,6,11,12-tetraphenylnaphthacene, 2-(4-diphenylamino)phenyl-10,10-dioxo-9-hydrogen-thioxanthen-9-one (TXO-TPA), bis(2-(3,5-dimethylphenyl)quinoline-C2,N')(acetylacetonate)iridium(III) (Ir(dmpq)2(acac)), bis[(4-n-hexylphenyl)isoquinoline](acetylacetonate)iridium(I II), bis[5-hexyl-2-(1-isoquinolyl)phenyl](2,4-pentanedione)iridium (Hex-Ir(Piq)2acac), bis(2-(2'-benzothienyl)pyridine-N,C3')(acetylacetonate)iridium (Ir(btp)2(acac)), 7,1-bis(4-(diphenylamino)phenyl)-2,3-dicyanopyrazinophenanthrene (TPA-DCPP), n-hexylphenyl)quinoline](acetylacetonate)iridium(III) (Hex-Ir(Phq)2acac), 4-(dicyanomethyl)-2-methyl-6-[2-(2,3,6,7-tetrahydro- 1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran (DCM2), (E)-2-(2-tert-butyl-6-(2-(2,6,6-trimethyl-2,4,5,6-tetrahydro-1H-pyrrolo[3,2,1-IJ]]quinolin-8-yl)vinyl)-4H-pyran-4-ylidene)malononitrile (DCQTB), tri(2,2',6,6'-tetramethyl-3,5-heptanedione)iridium (Ir(DMP)3), bis(4-(4-tert-butyl-phenyl)-thiophene[3,2-C]pyridine-C2,N)iridium(III) acetylacetonate (PO-01 -TB), acetylacetonate di(4-phenyl-thiophene[3,2-C]pyridine-C2,N)iridium(III) (PO-01), 2-(9-phenyl-9H-carbazole-3-yl)-1,1-dioxide-9H-thioxanthen-9-one (TXO-PHCZ), (OC-6-33)-bis[2-(2-quinolyl)phenyl](2,2,6,6-tetramethyl-3,5-heptanedione)iridium, bis(2-phenylquinoline)(2,2,6,6-tetramethylheptane-3,5-dioate)iridium(III) (PQ2lr(dpm)) and rubrene;The host material in the guest-doped host material is selected from 1,3-bis(N-carbazolyl)benzene, 8-hydroxyquinoline aluminum, 4,4'-bis(9-carbazole)biphenyl, 4,4'-bis(2,2-tolylvinyl)biphenyl, 3-tert-butyl-9,10-di(2-naphthalene)anthracene, 2,2":7",2""-tert-9,9'-spirobis[9H-fluorene], 9,10-di(2-naphthyl)anthracene, 4,4'-bis(2,2-distyryl)-1,1'-biphenyl, 2-tert-butyl-9,10-di(2-naphthyl)anthracene, 2-(9,9-spirobifluorene-2-yl)-9,9-spirobifluorene and 2,7-bis[9,9-di(4-methylphenyl)-fluoro-2-yl]- ... at least one of bis(4,6-difluorophenylpyridine-N,C2) pyridine formyl iridium, perylene, bis[4-(9,9-dimethyl-9,10-dihydroacridine) phenyl] sulfone, bis(3,4,5-trifluoro-2-(2-pyridyl)phenyl-(2-carboxylpyridyl)iridium(III), 4,4'-bis(9-ethyl-3-carbazole vinyl)-1,1'-biphenyl, 4,4'-bis[4-(di-p-tolylamino)phenylphenyl]biphenyl, bis(2-hydroxyphenylpyridine)beryllium, 10-(4-(4,6-diphenyl-1,3,5-triazol-2-yl)phenyl)-9,9-dimethyl-9,10-dihydroacridine, 1,1'-(4,4'-( 4-phenyl-4H-1,2,4-triazole-3,5-diyl)bis(4,1-phenylene))bis(1H-phenoxazine), 3,3'-(1,4-phenyldi-2,1-vinyl)bis(9-ethyl-9H-carbazole), 9,9'-(5-(4,6-diphenyl-1,3,5-triazine-2-yl)-1,3-phenylene)bis(9H-carbazole), 1,1'-bis(3,5-bis(trifluoromethyl)phenyl)-9,9'-bianthracene, 9'-[4-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-9,3':6',9"-TER-9H-carbazole, 9,9',9",9"'-(((6-phenyl-1,3,5-triazine-2,4- At least one of N5,N5,N9,N9-tetraphenylspiro[benzo[C]fluorene-7,9'-fluorene]-5,9-diamine, bis[4-(3,6-di-tert-butyl-9-carbazyl)phenyl]sulfone, bis[4-tert-butyl-2',6'-difluoro-2,3'-bipyridyl](acetylacetonate)iridium(III), 9-[2,3-bis(9H-carbazol-9-yl)-5-(diphenyl-1,3,5-triazine-2-yl)phenyl]-9Hcarbazole, 2,3,4,6-tetra(9H-carbazol-9-yl)-5-fluorobenzonitrile, and (E)-N,N-diphenyl-4-(4-(pyrene-1-yl)phenyl)aniline. ;

[0009] The second aspect of the present invention provides a use of the material according to the first aspect of the present invention in an electroluminescent device.

[0010] A third aspect of the present invention provides a white light emitting transistor with a planar configuration of a surface light source, wherein the light emitting unit included in the transistor contains the material of the first aspect of the present invention.

[0011] The fourth aspect of the present invention provides an application of the surface light source planar configuration white light emitting transistor of the third aspect of the present invention in a white light emitting OLET array, full-color display and lighting.

[0012] Through the above technical scheme, the present invention provides a highly efficient and stable area emission type OLET based on a unique lateral integrated device configuration, which incorporates efficient energy transfer of phosphorescent and fluorescent guests in the active layer, making adjustable emission color and even white light emission possible. By precisely adjusting the energy transfer between the host and the guest in the active layer, a high external quantum efficiency (EQE) of up to 13.9% is achieved, which is the highest value reported so far in this field. In addition, a small efficiency roll-off and high loop stability are achieved, as well as a 10 5 Level High I on / I off ratio (current on-off ratio) and effective gate tunability with ultra-low driving voltage below 5 V. A 4 × 6 white-light-emitting OLET array for full-color display was demonstrated, indicating its great application potential in advanced display technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1-1 and Figure 1-2 Schematic diagram of the structure of a light-emitting transistor device that emits a surface light source.

[0014] Figure 2 Schematic diagram of the structure of the light-emitting transistor device (a) and optical photograph (b, scale 0.2 mm) of the surface light source prepared in Example 1.

[0015] Figure 3 The relationship curves of source-drain current-brightness-gate voltage (a), brightness and gate voltage (b), and external quantum efficiency (EQE) and brightness (c) of the device in Example 1 are shown.

[0016] Figure 4 These are luminescent photos of the device in Example 1 at gate voltages of -5 V (a), -6 V (b), and -20 V (c). DETAILED DESCRIPTION

[0017] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0018] The first aspect of the present invention provides a white light-emitting material for electroluminescence, wherein the material comprises: a phosphorescent material and a guest-doped host material, wherein the guest in the guest-doped host material is 5,6,11,12-tetraphenyltetracene, 2-(4-diphenylamino)phenyl-10,10-dioxo-9-hydro-thioxanthen-9-one (TXO-TPA), bis(2-(3,5-dimethylphenyl)quinoline-C2,N')(acetylacetonate)iridium(III) (Ir(dmpq)2(acac)), bis[(4-n-hexylphenyl)isoquinoline](acetylacetonate)iridium(III), di[5 -hexyl-2-(1-isoquinolyl)phenyl](2,4-pentanedione)iridium (Hex-Ir(Piq)2acac), bis(2-(2'-benzothienyl)pyridine-N,C3')(acetylacetonate)iridium (Ir(btp)2(acac)), 7,1-bis(4-(diphenylamino)phenyl)-2,3-dicyanopyrazinophenanthrene (TPA-DCPP), n-hexylphenyl)quinoline](acetylacetonate)iridium(III) (Hex-Ir(Phq)2acac), 4-(dicyanomethyl)-2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5 H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran (DCM2), (E)-2-(2-tert-butyl-6-(2-(2,6,6-trimethyl-2,4,5,6-tetrahydro-1H-pyrrolo[3,2,1-IJ]]quinolin-8-yl)vinyl)-4H-pyran-4-ylidene)malononitrile (DCQTB), tris(2,2',6,6'-tetramethyl-3,5-heptanedione)iridium (Ir(DMP)3), bis(4-(4-tert-butyl-phenyl)-thiophene[3,2-C]pyridine-C2,N)iridium(III) acetylacetonate (PO-01-T B), at least one of bis(4-phenyl-thiophene[3,2-C]pyridine-C2,N)iridium(III) acetylacetonate (PO-01), 2-(9-phenyl-9H-carbazole-3-yl)-1,1-dioxide-9H-thioxanthen-9-one (TXO-PHCZ), (OC-6-33)-bis[2-(2-quinolyl)phenyl](2,2,6,6-tetramethyl-3,5-heptanedione)iridium, bis(2-phenylquinoline)(2,2,6,6-tetramethylheptane-3,5-dioate)iridium(III) (PQ2lr(dpm)) and rubrene;

[0019] The host material in the guest-doped host material is at least one selected from 1,3-bis(N-carbazolyl)benzene, 8-hydroxyquinoline aluminum, 4,4'-bis(9-carbazole)biphenyl, 4,4'-bis(2,2-tolylvinyl)biphenyl, 3-tert-butyl-9,10-di(2-naphthalene)anthracene, 2,2":7",2""-tert-9,9'-spirobis[9H-fluorene], 9,10-di(2-naphthyl)anthracene, 4,4'-bis(2,2-distyryl)-1,1'-biphenyl, 2-tert-butyl-9,10-di(2-naphthyl)anthracene, 2-(9,9-spirobifluorene-2-yl)-9,9-spirobifluorene and 2,7-bis[9,9-di(4-methylphenyl)-fluoro-2-yl]-9,9-di(4-methylphenyl)fluorene;

[0020] The phosphorescent material is selected from bis(4,6-difluorophenylpyridine-N,C2) pyridine carboxylate iridium, perylene, bis[4-(9,9-dimethyl-9,10-dihydroacridine)phenyl]sulfone, bis(3,4,5-trifluoro-2-(2-pyridyl)phenyl-(2-carboxylpyridyl)iridium(III), 4,4'-bis(9-ethyl-3-carbazole vinyl)-1,1'-biphenyl, 4,4'-bis[4-(di-p-tolylamino)phenylphenyl]biphenyl, bis(2-hydroxyphenylpyridine)beryllium, 10-(4-(4 ,6-diphenyl-1,3,5-triazol-2-yl)phenyl)-9,9-dimethyl-9,10-dihydroacridine, 1,1'-(4,4'-(4-phenyl-4H-1,2,4-triazol-3,5-diyl)bis(4,1-phenylene))bis(1H-phenoxazine), 3,3'-(1,4-phenyldi-2,1-vinyl)bis(9-ethyl-9H-carbazole), 9,9'-(5-(4,6-diphenyl-1,3,5-triazine-2-yl)-1,3-phenylene)bis(9H-carbazole ), 1,1'-bis(3,5-bis(trifluoromethyl)phenyl)-9,9'-bianthracene, 9'-[4-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-9,3':6',9"-TER-9H-carbazole, 9,9',9",9"'-(((6-phenyl-1,3,5-triazine-2,4-diyl)bis(benzene-5,3,1-triyl))tetrakis(9H-carbazole), N5,N5,N9,N9-tetraphenylspiro[benzo[C]fluorene-7,9'-fluorene]-5,9-dicarbazole At least one of amine, bis[4-(3,6-di-tert-butyl-9-carbazol-1-yl)phenyl]sulfone, bis[4-tert-butyl-2',6'-difluoro-2,3'-bipyridyl](acetylacetonate)iridium(III), 9-[2,3-bis(9H-carbazol-9-yl)-5-(diphenyl-1,3,5-triazine-2-yl)phenyl]-9Hcarbazole, 2,3,4,6-tetrakis(9H-carbazol-9-yl)-5-fluorobenzonitrile, and (E)-N,N-diphenyl-4-(4-(pyrene-1-yl)phenyl)aniline.

[0021] In a preferred embodiment of the present invention, preferably, the phosphorescent material is selected from bis[2-(4,6-difluorophenyl)pyridine-C2,N])iridium(III), and the host material is selected from 1,3-bis(N-carbazolyl)benzene.

[0022] In a preferred embodiment of the present invention, preferably, the molar ratio of the phosphorescent material: the guest: the host material is 5-30: 0.1-3: 67-94.9, preferably 15-25: 0.5-1: 75-85, and most preferably 20: 0.8: 79.2. This can more effectively solve the technical problems of the present invention, obtain high external quantum efficiency and other effects, and provide good white light emission effects.

[0023] The second aspect of the present invention provides a use of the material according to the first aspect of the present invention in an electroluminescent device.

[0024] A third aspect of the present invention provides a white light emitting transistor with a planar configuration of a surface light source, wherein the light emitting unit included in the transistor contains the material of the first aspect of the present invention.

[0025] In a preferred embodiment of the present invention, preferably, the transistor has a lateral integration structure and a bottom light emitting device structure.

[0026] In the present invention, the lateral integration structure refers to that the source electrode and the drain electrode are not arranged on the same plane (such as Figure 1-1 and 1-2 As shown); the bottom light-emitting device structure refers to the device emitting light toward the substrate.

[0027] In a preferred embodiment of the present invention, preferably, the transistor further includes a source electrode, a drain electrode, and a charge buffer layer disposed under the drain electrode.

[0028] In a preferred embodiment of the present invention, preferably, the source electrode and the drain electrode are arranged in a non-planar manner. In a preferred embodiment of the present invention, preferably, the transistor further comprises a semiconductor charge transport layer disposed below the source electrode and the charge buffer layer.

[0029] In a preferred embodiment of the present invention, preferably, the source electrode and the drain electrode are arranged on different sides of the semiconductor charge transport layer.

[0030] In a preferred embodiment of the present invention, preferably, the light emitting unit is arranged on the charge buffer layer.

[0031] In a preferred embodiment of the present invention, preferably, the transistor further comprises an electron transport layer disposed on the light-emitting unit.

[0032] In a preferred embodiment of the present invention, preferably, the transistor further comprises a dielectric layer disposed under the semiconductor charge transfer layer and a gate electrode and a substrate disposed under the dielectric layer.

[0033] In the present invention, the relative positions of the source electrode, drain electrode, light emitting unit, charge buffer layer, semiconductor charge transport layer, dielectric layer, gate electrode and substrate included in the transistor are as follows: Figure 1-1 Or as shown in 1-2.

[0034] In a preferred embodiment of the present invention, preferably, the EQE peak value of the transistor is up to 13.9%, preferably 5-13.9%, more preferably 10-13.9%, the roll-off efficiency is not more than 25% at 500 nits brightness, and the current switching ratio is (0.1-5)×105 , preferably (0.4-3.5)×10 5 , the driving voltage is not greater than 5V.

[0035] According to an embodiment of the present invention, the surface light source planar configuration white light emitting transistor further includes a semiconductor charge transport layer.

[0036] Preferably, the semiconductor charge transport layer is disposed below the source electrode. In one embodiment of the present invention, the charge buffer layer is disposed above the semiconductor charge transport layer.

[0037] According to an embodiment of the present invention, the transistor further comprises a light emitting unit, and preferably the light emitting unit is arranged under the drain electrode.

[0038] In one embodiment of the present invention, the charge buffer layer is disposed below the light emitting unit. In another embodiment of the present invention, the charge buffer layer is disposed below the source electrode and the light emitting unit.

[0039] According to an embodiment of the present invention, the charge buffer layer may be disposed between the drain electrode (or source electrode) and the semiconductor charge transport layer, or between the semiconductor charge transport layer and the light emitting unit.

[0040] According to an embodiment of the present invention, the light-emitting surface (including the light-emitting unit) of the transistor is U-shaped, and the source electrode is arranged on the U-shaped opening side.

[0041] According to one embodiment of the present invention, the planar shape of the drain electrode, the light emitting unit and the charge buffer layer is U-shaped, and the source electrode is arranged on the side of the U-shaped opening.

[0042] According to another embodiment of the present invention, the planar shape of the drain electrode and the light-emitting unit is U-shaped, the source electrode is arranged on the U-shaped opening side, and the charge buffer layer is preferably arranged under the source electrode.

[0043] Preferably, the transistor comprises:

[0044] substrate;

[0045] A dielectric layer disposed on the surface of the substrate;

[0046] a semiconductor charge transport layer disposed on the dielectric layer;

[0047] A source electrode and a charge buffer layer are arranged on the semiconductor charge transport layer, preferably the source electrode and the charge buffer layer are arranged on different sides of the semiconductor charge transport layer;

[0048] A light emitting unit, an electron transport layer and a drain electrode are sequentially arranged on the charge buffer layer.

[0049] Preferably, the surface light source planar configuration light emitting transistor comprises:

[0050] substrate;

[0051] A dielectric layer disposed on the surface of the substrate;

[0052] a semiconductor charge transport layer disposed on the dielectric layer;

[0053] A charge buffer layer disposed on the semiconductor charge transport layer;

[0054] A source electrode and a light-emitting unit are sequentially arranged on the charge buffer layer, preferably the source electrode and the light-emitting unit are on different sides of the charge buffer layer;

[0055] An electron transport layer and a drain electrode are sequentially arranged on the light emitting unit.

[0056] It should be noted that when an element such as a layer, film, crystal, region or substrate is referred to as being disposed "on" or "under" another element or "between two elements", it can be placed directly on / under the other element, or one or more intervening layers may also be present.

[0057] According to an embodiment of the present invention, the source electrode and the drain electrode are arranged in a non-planar manner, that is, there is a height difference between the two. For example, the source electrode and the charge buffer layer are both located above the semiconductor charge transport layer, and there may or may not be a gap between the two, the thickness may be the same or different, the charge buffer layer may cover the source electrode, or the two are independent of each other, the drain electrode is arranged on the charge buffer layer (the drain electrode may completely cover or partially cover the charge buffer layer), and a conductive channel is formed between the drain electrode and the source electrode; optionally, a light-emitting unit is arranged between the drain electrode and the charge buffer layer, and the light-emitting unit may completely cover or partially cover the charge buffer layer and / or the source electrode. For example, the source electrode and the light-emitting power source are both arranged on the charge buffer layer, the drain electrode is arranged on the light-emitting unit, and a conductive channel is formed between the drain electrode and the source electrode, and the thickness of the source electrode and the light-emitting unit may be the same or different, there may or may not be a gap between the light-emitting unit and the source electrode, the light-emitting unit may cover the source electrode, or the two are independent of each other. The light-emitting part is the entire effective area of ​​the source electrode or the drain electrode, and the gate voltage can adjust the light-emitting brightness.

[0058] According to an embodiment of the present invention, the charge buffer layer and the source electrode can be arranged on different sides of the semiconductor charge transport layer. The inventor first proposed the introduction of the charge buffer layer and its position. For the thickness and area of ​​the charge buffer layer and other layers, those skilled in the art can adjust them according to actual needs.

[0059] According to an embodiment of the present invention, the substrate is preferably a modified glass with a gate electrode. The gate electrodes can be rigid or flexible transparent electrodes or opaque electrodes, independently selected from any one or more of the following substances, including but not limited to: metals, such as magnesium, calcium, sodium, potassium, titanium, indium, yttrium, lithium, gadolinium, aluminum, silver, tin, nickel, gold, molybdenum, iron and lead; alloys of the aforementioned metals; multilayer materials, such as LiF-Al, LiO2-Al or LiF-Al-Ag; and metal oxides, such as ITO, IZO, MoO x etc.; heavily doped silicon. Those skilled in the art will appreciate that the specific metal type selected can be adjusted according to the energy band of the semiconductor material. Preferred examples include indium tin oxide modified glass, heavily doped silicon, and indium gallium zinc oxide modified glass.

[0060] According to an embodiment of the present invention, the material in the semiconductor charge transport layer has good electrical properties, and preferably the mobility of the semiconductor charge transport layer is not less than 0.1 cm 2 V -1 s -1 For example, the semiconductor charge transport layer comprises an organic semiconductor material and / or an inorganic semiconductor material, for example, the organic semiconductor material is selected from a small molecule material and / or a polymer material.

[0061] Preferably, the organic semiconductor material is selected from one or more of the following substances, including but not limited to: 2,7-dioctyl[1]benzothieno[3,2-b]benzothiophene (C8-BTBT), 2,6-diphenylanthracene (DPA), 2,6-dinaphthylanthracene (dNaAnt), 2,6-di(p-hexylbenzene)anthracene (C6-DPA), 2,6-di(p-octylhexylbenzene)anthracene (C8-DPA), 2,6-di(p-decylbenzene)anthracene (C 10 -DPA), poly(3-hexylthiophene) (P3HT), 9,9-di-n-octylfluorene-benzothiadiazole copolymer (F8BT), poly[2,5-(2-octyldodecyl)-3,6-diketopyrrolopyrrole-alt-5,5-(2,5-di(thiophen-2-yl)thieno[3,2-b]thiophene)] (DPP-DTT), and C8-BTBT is also preferred.

[0062] Preferably, the inorganic semiconductor material is selected from one or more of the following substances including but not limited to: carbon nanotubes (CNTs), zinc tin oxide (ZTO), gallium nitride (GaN), silicon carbide (SiC), zinc selenide (ZnSe).

[0063] According to an embodiment of the present invention, the charge buffer layer (CTB layer) is used to uniformly distribute charges in a horizontal electric field. The material has suitable electrical properties, for example, selected from one or more of low-mobility organic materials, metal materials, pnp junctions, etc.; preferably, the low mobility refers to 2-5 orders of magnitude smaller than the mobility of the semiconductor charge transport layer. For example, the charge buffer layer is a layer formed by one or more of the low-mobility organic materials 4,4'-cyclohexylbis[N,N-bis(4-methylphenyl)aniline] (TAPC), N,N'-diphenyl-N,N'-(1-naphthyl)-1,1'-biphenyl-4,4'-diamine (NPB) and polyvinylcarbazole (PVK), and is preferably a layer formed by TAPC. For another example, the work function of the metal material matches the highest occupied molecular orbital (HOMO) energy level of the light-emitting unit, and the work function of the metal material can be defined as 4.5eV-6eV; preferably, the charge buffer layer is a layer formed by one or more of Au, such as Au, Ni, Pt, etc. in the metal material, for example, an ultra-thin layer, and the layer thickness can be 0.5-10nm, such as 1nm, 2nm, 3nm. For another example, the charge buffer layer is a layer formed by one or more of C60-pentacene-C60, C70-tetracene-C70, C60-tetracene-C70, etc. in the pnp junction.

[0064] According to an embodiment of the present invention, when the material in the charge buffer layer is an organic material with low mobility or a pnp junction, the thickness of the charge buffer layer is 20-80 nm, such as 30 nm, 40 nm, or 50 nm.

[0065] According to the embodiment of the present invention, the luminescent material contained in the luminescent unit, especially the one emitting white light, is as described above and will not be described in detail.

[0066] In a preferred embodiment of the present invention, phosphorescent blue emitters and fluorescent yellow emitters are doped in the active layer to achieve efficient energy transfer and fully collect singleton and triplet excitons generated after electron-hole recombination in the host material to achieve high EQE and adjustable color emission of the OLET.

[0067] In order to obtain tunable color emission OLETs, the energy transfer between the host (host material, such as mCP) and the guest (such as FIrpic / Rubrene) is regulated by precisely controlling the doping concentration of the guest molecules in the host system. A low driving voltage of less than 5 V is shown, which is crucial for achieving low power consumption. A luminescence energy of more than 10 cm is also obtained when constructing the device. 2 The high carrier mobility of 1.17V / Vs indicates excellent field-effect performance and fast switching characteristics.

[0068] Furthermore, the spectrum of light emitted by the light-emitting unit is between 390nm and 780nm.

[0069] In the present invention, the term "doping" refers to a material of any layer having physical properties different from the material occupying the maximum weight percentage of the corresponding layer, added to the material occupying the maximum weight percentage in an amount corresponding to a weight percentage not exceeding 30%. The host material and the dopant material of any layer are distinguishable from each other.

[0070] In a preferred embodiment of the present invention, the transistor further comprises an electron transport layer disposed on the light-emitting unit. The material of the electron transport layer may be selected from 3,3'-[5'-[3-(3-pyridyl)phenyl][1,1':3',1"-terphenyl]-3,3"-diyl]bipyridine (TmPyPB), 1,3-bis(3,5-bipyridin-3-ylphenyl)benzene (B3pypb), 2,9-dimethyl-4,7-diphenyl-1,10-phenanthroline (BCP), 4,7-diphenyl-1,10-phenanthroline (Bphen), 2-phenyl-9,10-di(2-naphthyl)-anthracene (PADN), 3-(biphenyl-4-yl)-5-(4-tert-butylphenyl)-4-phenyl-4H-1,2,4-triazole (TA Z), 8-hydroxyquinoline-lithium (Liq), 4,6-bis(3,5-di(3-pyridyl)phenyl)-2-methylpyrimidine (B3PYMPM), 2-(4-biphenyl)-5-phenyloxadiazole (PBD), 1,3-bis(3,5-bipyridyl-3-phenyl)benzene (BmPyPhB), tris[2,4,6-trimethyl-3-(3-pyridyl)phenyl]borane (3TPYMB), 2,4,6-tris(3'-(pyridin-3-yl)biphenyl-3-yl)-1,3,5-triazine (TmPPPyTz), 1,3,5-tris(1-phenyl-1H-benzimidazol-2-yl)benzene (TPBi), 1,3, 5-Tris(6-(3-(pyridin-3-yl)phenyl)pyridin-2-yl)benzene (Tm3PyP26PyB), diphenylbis[4-(pyridin-3-yl)phenyl]silane (DPPS), 1,3-bis[2-(2,2'-bipyridin-6-yl)-1,3,4-oxadiazol-5-yl]benzene (BPY-OXD), N,N'-diphenyl-N,N'-(1-naphthyl)-1,1'-biphenyl-4,4'-diamine (NPB), N,N'-diphenyl-N,N'-bis(3-methylphenyl)-1,1'-biphenyl-4,4'-diamine (TPD), N,N'-(9h-fluorene-9,9-diyl)bis(4, 1-phenyl)bis(N-phenylnaphthalene-1-amine) (NPBAPF), N,N',N",N"'-tetra-1-naphthyl-N,N',N",N"'-tetraphenyl-9,9'-spirobis[9H-fluorene]-2,2',7,7'-tetramine (Spiro-2NPB), 3,5,6-trichloropyridin-2-ol (TCP), dichlorotriazinylaminofluorescein (DTAF), 4,4'-cyclohexylbis[N,N-di(4-methylphenyl)aniline] (TAPC), 2,6-diphenylanthracene (DPA), 2,6-dinaphthylanthracene (dNaAnt), 1,4-bis(10-phenylanthracen-9-yl)benzene (BD1), 4,4'-Bis[4-(diphenylamino)phenyl]biphenyl (BDAVBi), perylene (Perylene), bis(dimethyl-dihydroacridine)phenylsulfone (DMAC-DPS), bis[2-(5-cyano-4,6-difluorophenyl)pyridine-C2,N)]picolinyliridium (FCNirPic), iridium(III)bis[(2,3,4-difluorophenyl)-pyridine-N,C2']picolinate (Ir(tfpd)2pic), bis[2,4-dimethyl-6-(4-methyl-2-quinolyl-κN)phenyl-κC](2,2,6 ,6-tetramethyl-3,5-heptanedione-κO3 (Ir(mphmq)2tmd), 4,4'-bis[4-(di-p-tolylamino)phenylvinyl]biphenyl (DPAVBi), 9,9'-(5-(4,6-diphenyl-1,3,5-triazine-2-yl)-1,3-phenyl)bis(9H-carbazole) (DCzTrz), 5,5-dibromo-4,4-tetradecanoyl-2,2-bithiophene (fac-Ir(dpbic)3), tris(2-phenylpyridine)iridium (Ir(ppy)3), tris[2-(p-tolyl)pyridine]iridium (III )(Ir(mppy)3), bis(2-phenylpyridine-C2,N)iridium(III) acetylacetonate (Ir(ppy)2(acac)), bis(2-(naphthalene-2-yl)pyridine)(acetylacetonate)iridium(III) (Ir(npy)2acac), tris[2-(3-methyl-2-pyridyl)phenyl]iridium (Ir(3mppy)3), bis(2-(3,5-dimethylphenyl)quinoline-C2,N')(acetylacetonate)iridium(III) (Ir(dmpq)2acac), bis(2-(2'-benzothienyl)-pyridine-N, At least one of iridium (C3') (acetylacetonate) (Ir(btp)2(acac)), 4-(dicyanomethylene)-2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran (DCM2), rubrene (Rubrene), tris(2-(3,5-dimethylphenyl)quinoline-C2,N')iridium (III) (Ir(dmpq)3), and 2,8-di-tert-butyl-5,11-bis(4-tert-butylphenyl)-6,12-diphenyl tetracene (TBRb). ,

[0071] According to the embodiment of the present invention, the semiconductor charge transport layer, charge buffer layer, light-emitting unit and electron transport layer can be obtained by processing methods known in the art that are conducive to charge transport and visible light emission, and the processing methods include but are not limited to vacuum evaporation coating method (vacuum thermal evaporation), physical vapor transport method (physical vapor transport), solution shearing method (solution shearing), solution epitaxial growth method (solution epitaxy), spin coating method (spin coating), inkjet printing method (inkjet printing). Those skilled in the art can understand that the specific method used can be specifically selected according to the physical properties (such as solubility, melting and boiling points, etc.) of the semiconductor material actually used.

[0072] For example, the preparation method including the semiconductor charge transport layer, the charge buffer layer, the light-emitting unit and the electron transport layer can be selected from any one of the following methods:

[0073] Method 1: In a vapor deposition chamber, a thin film of the small molecule material is deposited on the dielectric layer and the electrode by vacuum evaporation coating to obtain an active layer;

[0074] Method 2: Spin coating a solution of active layer material on the dielectric layer and the electrode by spin coating to obtain an active layer;

[0075] Method 3: preparing and growing a single crystal film of the small molecule material by a solution epitaxial growth method: dissolving the small molecule material in a solvent that is immiscible with water, slowly dripping the obtained mixed uniform solution onto a water surface, spreading the mixed solution on the water surface, and waiting for the solvent therein to evaporate to obtain the single crystal film; inserting a supporting substrate with a dielectric layer into water to transfer the single crystal film to the surface of the dielectric layer to obtain an active layer;

[0076] Method 4: Prepare a single crystal film of the small molecule material by a solution shearing method: dissolve the small molecule material in an organic solvent, drop the resulting uniformly mixed solution onto a supporting substrate with a dielectric layer, and then slowly shear and stretch the dropped solution to form an active layer.

[0077] Charges are injected from the electrode at one end of the semiconductor charge transfer layer (taking the source electrode as an example), and are transferred to the other end in the extremely thin conductive channel formed under the external gate voltage. After the action of the charge buffer layer, a relatively uniform current injection is formed under the other electrode (taking the drain electrode as an example), and the charges are recombined with the electrons injected by the drain electrode to form a uniform surface light source.

[0078] According to an embodiment of the present invention, the thickness of the semiconductor charge transport layer, charge buffer layer, light-emitting unit and electron transport layer are all in the nanometer to submicron level, for example, the thickness of each layer can independently be 5-500nm, for example, 10-100nm.

[0079] According to an embodiment of the present invention, the number of the light-emitting components (referring to the charge buffer layer, the light-emitting unit and the electron transport layer) is at least one, for example, two, three or more. When the number of the light-emitting components is two, three or more, the charge buffer layer, the light-emitting unit and the electron transport layer are optionally the same or different. Each light-emitting component is connected by a charge generation layer (CGL).

[0080] According to an embodiment of the present invention, the source electrode, drain electrode, and gate electrode of the planar configuration white light-emitting transistor of the surface light source can be transparent electrodes or opaque electrodes, and are independently selected from any one or more of the following substances, including but not limited to: metals, such as magnesium, calcium, sodium, potassium, titanium, indium, yttrium, lithium, gadolinium, aluminum, silver, tin, nickel, gold, molybdenum, iron, and lead; alloys of the aforementioned metals; multilayer materials, such as LiF / Al, LiO2 / Al, or LiF / Al / Ag; and metal oxides, such as ITO, IZO, MoO x etc.; heavily doped silicon. Those skilled in the art will appreciate that the specific type of metal selected can be adjusted according to the energy band of the semiconductor material.

[0081] According to an embodiment of the present invention, the source electrode, drain electrode and gate electrode are prepared by methods known in the art, such as vacuum thermal evaporation, inkjet printing, electron beam deposition, etc.

[0082] According to an embodiment of the present invention, there is no particular restriction on the type of the dielectric layer, which may be an inorganic material dielectric layer and / or an organic material dielectric layer. Exemplarily, the dielectric layer is an inorganic material dielectric layer, such as a dielectric layer formed by an inorganic oxide (Al2O3, SiO2); and / or, the dielectric layer is an organic material dielectric layer, such as a dielectric layer formed by polymethyl methacrylate (PMMA), and cross-linked poly (vinyl alcohol) (C-PVA) modified with a high-k perfluoro (1-butenyl vinyl ether) polymer (CYTOP) is used as a dielectric layer, which can reduce the driving voltage.

[0083] According to an embodiment of the present invention, the dielectric layer can be prepared by a method known in the art, for example, at least one of a thermal growth method, a physical vapor deposition method, a spin coating method, etc. can be selected.

[0084] According to the embodiment of the present invention, there is no particular limitation on the thickness of the dielectric layer. For example, the thickness of the dielectric layer is 10-800 nm. Those skilled in the art can adjust the thickness of the dielectric layer according to actual needs.

[0085] According to an embodiment of the present invention, the surface light source planar configuration white light emitting transistor adopts a bottom-emitting device structure.

[0086] According to the embodiment of the present invention, the planar configuration white light emitting transistor of the surface light source can emit planar light matching the color of the light emitting unit under an external voltage.

[0087] The present invention also provides a method for preparing the planar light-emitting transistor emitting from the above-mentioned surface light source, comprising the following steps: providing a charge buffer layer under the drain electrode or the source electrode; the drain electrode, the source electrode and the charge buffer layer all have the meanings as shown above.

[0088] According to an embodiment of the present invention, the preparation method comprises the following steps: providing a charge buffer layer between the drain electrode (or source electrode) and the semiconductor charge transport layer, or providing a charge buffer layer between the semiconductor charge transport layer and the light emitting unit;

[0089] The drain electrode, source electrode, semiconductor charge transport layer, light emitting unit and charge buffer layer all have the meanings as indicated above.

[0090] Preferably, the structure including the semiconductor charge transport layer, the charge buffer layer, the light-emitting unit and the electron transport layer is recorded as an active layer, and the active layer is prepared by the above scheme.

[0091] The transistor device of the present invention has good compatibility with low temperature process technology, such as solution processing technology (inkjet printing, electrofluidic printing, roll-to-roll, etc.).

[0092] In the present invention, a preferred surface light source planar configuration white light emitting transistor has a laterally integrated OLET device configuration, and has unique advantages such as stable area emission, excellent gate adjustment capability and large aperture ratio. Indium tin oxide (ITO) modified glass is used as a substrate, and due to the high transparency of ITO modified glass, the transmittance of the electroluminescence of the OLET device is effectively optimized to more than 84%. In this case, the light emission efficiency is significantly improved compared with the previous top emission OLET. In addition, phosphorescent blue emitters and fluorescent yellow emitters are doped in the light-emitting unit to achieve efficient energy transfer and fully collect singleton and triplet excitons generated after electron-hole recombination in the host material to achieve high EQE and adjustable color emission of the OLET. In addition, cross-linked poly (vinyl alcohol) (C-PVA) modified with high-k perfluoro (1-butenyl vinyl ether) polymer (CYTOP) is used as a dielectric layer to reduce the driving voltage. 2,7-Dioctyl[1]benzothiophene[3,2-b][1]benzothiophene (C8-BTBT) was selected as the semiconductor charge transport layer, and 1,1-bis[(di-4-toluidine)phenyl]cyclohexane (TAPC) was used as the CTB layer to uniformly distribute the charges in the horizontal electric field. In the light-emitting unit, the phosphorescent material bis[2-(4,6-difluorophenyl)pyridine-C2,N](picolinato)iridium(III) (FIrpic) and the yellow fluorescent material rubrene were doped as guests into the host material 1,3-bis(N-carbazolyl)benzene (mCP). The electron transport layer of tris(2,4,6-trimethyl-3-(pyridin-3-yl)phenyl)borane (3TPYMB) was deposited on the top of the light-emitting unit. Finally, a 2nmLiF / 110nmAl composite top electrode was deposited to complete the device. The energy level diagram of the fabricated tunable color emission and white OLET shows good contact of the source and drain electrodes. During device operation, holes are injected from the source electrode and then transferred to the host mCP, which is blocked by the higher energy barrier formed by 3TPYMB. Then, the holes recombine with the electrons injected from the drain to generate 25% singleton excitons and 75% triplet excitons in the mCP. Subsequently, the singleton excitons are transferred to FIrpic and Rubrene respectively via Forster resonance energy transfer (FRET). The singleton excitons in FIrpic are rapidly converted into triplets through efficient intrasystem crossing (ISC), thanks to the improved spin-orbit coupling of Ir atoms. Finally, the triplet excitons decay to the ground state, emitting phosphorescence. At the same time, the singleton excitons in Rubrene decay back to the ground state, producing yellow emission.

[0093] In order to obtain tunable color emission OLETs, the energy transfer between the mCP host and the FIrpic / Rubrene guest can be adjusted by precisely controlling the doping concentration of the guest molecules in the host system. For example, three evaporated films with different doping concentrations were prepared, including mCP:10% FIrpic:3% Rubrene, mCP:20% FIrpic:3% Rubrene, and mCP:30% FIrpic:3% Rubrene, and were used to construct the corresponding OLETs devices A, device B, and device C, respectively. All devices were fabricated under the same conditions. The electroluminescence (EL) performance of these devices was evaluated and compared, and the typical light and electrical transfer and output curves showed good gate adjustment capabilities. The I of device A, device B, and device C were on / I off The ratios are 1.1×10 5 , 2.0×10 5 and 3.4×10 5 In addition to the excellent gate regulation performance, all OLETs exhibited low driving voltages below 5 V, which is crucial for achieving low power consumption, due to the introduction of high-k dielectric layers of CYTOP and C-PVA. These OLETs also achieved a gate drive voltage of more than 10 cm 2 / Vs high carrier mobility, indicating that they have excellent field effect performance and fast switching characteristics. In addition, the test pictures also show that the color of electroluminescence changes from yellow to white with the adjustment of doping concentration. Uniform white area emission was successfully obtained throughout the frequency sweep process, which is mainly due to the redistributed uniform current density under the drain. The EL intensity of this white area emission also increases with the increase of gate voltage.

[0094] The EL spectrum of the above device contains blue emission from 450nm to 520nm from FIrpic and yellow emission from 520nm to 700nm from Rubrene, which proves that Dexter and The resonance energy is efficiently transferred from mCP to FIrpic and Rubrene, respectively. In addition, the EL spectra of device A, device B and device C and their corresponding CIE coordinates can clearly show that the EL emission is effectively adjusted from CIE coordinates (0.45, 0.50) to (0.48, 0.50), demonstrating the different energy transfer efficiencies in different doping concentration systems. However, the EL spectra of device A, device B and device C contain more yellow fluorescence emission from ruby. Therefore, in order to obtain the white emission of this OLET, the doping concentration of ruby ​​is further optimized on the basis of device B, reducing it from 3% to 0.8%, while keeping the FIrcip concentration unchanged. It is very obvious that the blue emission of FIrcip from the OLET (device D) of mCP:20% FIrpic:0.8% Rubrene is significantly increased, which leads to more white emission, and the corresponding CIE coordinates are (0.36, 0.48). In addition, device D also presents typical optical and electrical transfer and output curves, showing good gate adjustment ability, I on / I off Ratio up to 4.6×10 4 , the driving voltage is as low as ~5V.

[0095] In addition to the excellent gate regulation and low drive voltage of these devices, the electro-optical conversion efficiency is also optimized by changing the doping ratio and precisely adjusting the energy transfer efficiency between the host and the guest in the emission active layer. In device A, a peak EQE of 2.6% and a corresponding current efficiency of 7.7 cd / A are obtained, with a maximum luminescence of 567 cd / cm 2 It is very exciting that the EQE peaks of devices B and C were successfully improved to 12% and 13.9%, respectively, which are the highest values ​​in this field so far. Devices B and C also achieved corresponding current efficiencies of 38.7cd / A and 344.8cd / A, and the maximum luminous output exceeded 1300cd / cm 2 For white light emitting device D, a peak EQE of 11.1% was achieved, with a maximum current efficiency of 33.8 cd / A and a maximum luminous output of 1617 cd / cm 2 It provides an ideal device unit for realizing new full-color display technology. In addition, white OLET has a brightness of 500cd / cm 2 The OLET device provided by the present invention has a small efficiency roll-off of 28%, which is mainly attributed to the suppression of exciton-charge annihilation brought about by the high exciton utilization efficiency. Compared with the existing OLET devices, the high EQE and brightness as well as the excellent stability of the OLET provided by the present invention are outstanding.

[0096] Furthermore, using these high-efficiency white OLET units, a 4×6 white OLET array can be realized. The device structure and the schematic diagram of the pixel unit circuit of the white OLET array designed according to the present invention show that this white CBT-OLET array exhibits stable, uniform and bright regional luminescence, providing an ideal platform for realizing full-color display based on OLET.

[0097] In addition, full-color electroluminescent displays have gained considerable attention in recent decades, mainly due to its ease of use and convenience for displaying information, brand missions, and advertisements of products and services. Based on the white OLET array of the present invention, two different full-color display modes can be further obtained. First, a customized rectangular RGB mask is covered on the white OLET array. A uniform and bright RGB full-color display and its corresponding RGB emission spectrum are demonstrated. Similarly, a unique full-display mask with ICCAS capital letters is used for full-color display based on white OLET. Overall, the successful fabrication of stable and uniform white OLET and the realization of full-color display indicate the great potential application prospects of OLET in the new generation of displays and other related fields.

[0098] In summary, the present invention provides a high-performance area-emitting OLET based on a unique uniform horizontal charge distribution device configuration. By precisely adjusting the energy transfer between the mCP host and the FIrpic / Rubrene guest in the active layer, a white-light emitting OLET with a peak EQE of 13.9% was successfully achieved. In addition, due to the prevention of exciton-charge annihilation and the introduction of a high-k dielectric layer, a high-energy luminescent efficiency of 500 cd / cm 2 A small efficiency roll-off of 28% was obtained with a current switching ratio of up to 10 5 , the driving voltage is lower than 5 V, indicating its stable and effective gate tunability as well as low power consumption. Finally, white emission OLET array and full-color display are proposed. This work provides an effective method for constructing high-performance white OLET, showing great significance for promoting the application of OLET in future display technology.

[0099] The preparation of the OLET device of the present invention can be carried out in the following specific implementation manner:

[0100] Photophysical characterization: Steady-state absorption spectra of FIrpic and Rubrene diluted solutions were recorded on a Jasco V-570 spectrometer and an Analytik Jena Specord 210 spectrophotometer, respectively. Photoluminescence spectra of FIrpic and Rubrene diluted solutions were recorded on a Jasco FP-6600 spectrofluorimeter.

[0101] Fabrication of OLET devices: All OLET devices are fabricated on transparent ITO-modified glass substrates. The thickness of ITO is between 1200-1600 angstroms and the resistance is 9-15Ω / sq.

[0102] First, the ITO-modified glass substrate was cleaned with n-hexane, chloroform, and isopropanol in an ultrasonic bath for 10 min, then dried with nitrogen and treated with oxygen plasma (40 W) for 5 min. Subsequently, the ITO-modified glass was transferred to a glove box to complete the following fabrication and characterization processes.

[0103] C-PVA (concentration of 4200 rpm × 45 s, baked at 100 °C for 90 min) / CYTOP (concentration or brand of 5000 rpm × 60 s, baked at 100 °C for 30 min) was spin-coated on a clean ITO-modified glass substrate as a dielectric layer.

[0104] The preparation of the insulating layer was carried out according to the previously reported method. -6 A 50nm C8-BTBT layer was deposited on glass / ITO / C-PVA / CYTOP in a vacuum chamber at 100 mbar. 2nm MoO on top contact x / 40nm Au electrode was evaporated onto C8-BTBT. Then a 50nm TAPC charge buffer layer, a 35nm mCP:x%Firpic:y%Rubrene (where x is 10-30, y is 0.8-30, for example x=10, y=3; x=20, y=30; x=30, y=3; x=20, y=0.8) light emitting unit and a 40nm electron transport layer were evaporated in sequence. Finally, a 2nm LiF / 110nm Al drain electrode was deposited, which was non-planar with the source electrode, completing the fabrication of the OLET.

[0105] Characterization of OLET devices: Electrical characteristics were performed by a semiconductor FS-PRO (Platform Design Automation, Inc.) in a glove box. Photomultiplier tubes (H10721) were calibrated with a standardized integrating sphere (Spectrum TEQ-EL, Ocean Optical, Inc.) to obtain optical data of OLET. Photos of single OLET and arrays were obtained by a digital CCD and a camera, respectively. Spectra were obtained by a spectrometer (EQPro, Ocean Optical).

[0106] The fourth aspect of the present invention provides an application of the surface light source planar configuration white light emitting transistor of the third aspect of the present invention in a white light emitting OLET array, full-color display and lighting.

[0107] The planar light-emitting transistor emitted by the above-mentioned surface light source may be a transistor containing one light-emitting component, or may be a series-connected transistor containing at least two light-emitting components.

[0108] Beneficial effects of the present invention:

[0109] Most of the traditional planar light-emitting transistors have linear or strip-shaped light emission and cannot present a good surface light source. In order to overcome the shortcomings of traditional light-emitting transistors, the present invention proposes a light-emitting transistor with a charge buffer layer. The inventors found that by inserting a charge buffer layer under the source electrode or the drain electrode, between the drain electrode (or source electrode) and the semiconductor charge transfer layer, or between the charge transfer layer and the light-emitting unit, the current density can be redistributed in the transistor, and the prepared planar light-emitting transistor can achieve a stable surface light source emission consistent with the shape of the drain electrode, providing uniform RGB area emission. The shape of the drain electrode can be circular, square, diamond, fork, etc. At the same time, it has good gate tunability (on / off ratio up to (0.1-5)×10 5 ), high loop stability and arbitrary tunability, and a high aperture ratio that can be adjusted according to actual needs, such as from no less than 10% of the existing technology to more than 94%. Due to the flexibility of organic semiconductors, they can be integrated with wearable devices, which is more advantageous for expanding the functions and application scenarios of wearable surface light source devices.

[0110] 1. The surface light source emitting planar light emitting transistor device of the present invention can realize the surface light source emission that is not affected by the gate voltage, which is conducive to the application of the device in the display field.

[0111] 2. The surface light source emitting planar light-emitting transistor device described in the present invention can realize the construction of a high aperture ratio electroluminescent device, can have good compatibility with flexible wearable devices, and plays an important role in promoting the development of light-emitting transistor devices.

[0112] 3. The present invention develops a light-emitting transistor device based on an organic semiconductor surface light source, which can maximize the use of the advantages of the organic semiconductor material system, such as richness, light weight, low price, and easy processing, and provides an effective solution for the large-area controllable and arrayed preparation of light-emitting transistor devices.

[0113] "Aperture ratio" refers to the percentage of the area of ​​the light-emitting surface to the sum of the areas of the light-emitting surface and the opening surface. By adjusting the area ratio of the light-emitting surface, transistors with a series of aperture ratios (for example, an aperture ratio of 10%, 15%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, 82%, 85%, 88%, 90%, 94%) can be obtained.

[0114] The technical solution provided by the present invention obtains high-performance tunable color emission OLETs based on a unique lateral integrated device structure, which can adjust the uniform charge distribution in the horizontal electric field to achieve uniform and stable regional emission. By adding phosphorescent blue emission and fluorescent yellow emission guests to the light-emitting unit and introducing a transparent substrate, efficient energy transfer, high exciton utilization and high light outcoupling efficiency enable high EQE and tunable color emission. By precisely adjusting the energy transfer between the host and the guest in the light-emitting unit, a high-quality white light emitting OLET is finally achieved, with the International Commission on Illumination (CIE) of (0.36, 0.48), a peak EQE of 13.9%, and a current efficiency of 44.8 cd / A, which are the highest values ​​reported in this field so far. In addition, due to the high exciton utilization efficiency, exciton-charge annihilation is effectively prevented in this white light OLET, resulting in a small efficiency roll-off and high loop stability, with an effective gate adjustability of 10 5 High I on / I off ratio and an ultra-low driving voltage below 5 V. Finally, a white-emitting OLET array for full-color display is proposed, which provides an effective method for constructing high-performance white OLETs and shows great significance for promoting the application of OLETs in future display technologies.

[0115] Unless otherwise specified, the experimental methods used in the following examples are all conventional methods; the reagents, materials, etc. used in the following examples, unless otherwise specified, can be obtained from commercial channels.

[0116] Example 1

[0117] Planar light-emitting field effect transistor device based on 1,3-bis(N-carbazolyl)benzene:bis(4,6-difluorophenylpyridine-N,C2)pyridinecarboxylate iridium:Rubrene white light-emitting unit with surface light source

[0118] 1) Glass / Indium Tin Oxide (ITO) sheet cleaning and dielectric layer preparation:

[0119] Before use, the glass sheet with the ITO layer was ultrasonically treated with deionized water, acetone, and isopropanol for about 10 minutes each, and then quickly dried with nitrogen. The surface energy level was modified in an O2 plasma cleaning machine for 5 minutes and the residual organic solvent on the surface was removed.

[0120] PVA powder (average M w ≈205000 g mol -1 ) was dissolved in deionized water (58 mg mL -1), and the solution was stirred at 800 rpm for 6 hours. Afterwards, glutaraldehyde (GA, 50 wt%) was added to the solution (1:80 volume ratio). The prepared PVA solution was spin coated on a glass / ITO substrate (4200 rpm×45 s) to obtain a 350 nm thick film. The film was then thermally annealed at 100°C in air for 90 minutes. Subsequently, a perfluororesin CYTOP (CTL-809M, M type) layer (about 10 nm) was spin coated on the PVA layer and annealed at 100°C for 30 minutes.

[0121] 2) Preparation of organic charge transport layer C8-BTBT

[0122] The patterned metal mask was fixed to the substrate, and 50 nm of C8-BTBT was thermally evaporated on the glass / ITO / dielectric layer by a vacuum coating machine.

[0123] 3) Preparation of source electrode

[0124] Replace the mask and fix it to the substrate, and use the vacuum coating machine to thermally evaporate 2nm MoO on the glass / ITO / dielectric layer / C8-BTBT. x and 40nm Au.

[0125] 4) Preparation of charge buffer layer and light-emitting unit:

[0126] Replace the mask and fix it to the substrate, and use the vacuum coating machine to coat the glass / ITO / dielectric layer / C8-BTBT / MoO x A 40nm TAPC charge buffer layer and a light-emitting unit 30nm 2% Rubrene:1,3-bis(N-carbazolyl)benzene / bis(4,6-difluorophenylpyridine-N,C2)picolinyliridium / 40nm TmPyPB were deposited on Au.

[0127] The molar ratio of Rubrene, 1,3-bis(N-carbazolyl)benzene and bis(4,6-difluorophenylpyridine-N,C2)picolinyliridium is 20:0.8:79.2.

[0128] 5) Preparation of drain electrode:

[0129] Replace the mask and fix it to the substrate, and use the vacuum coating machine to coat the glass / ITO / dielectric layer / C8-BTBT / MoO x 2nm LiF / 120nmAl were deposited on / Au / TAPC / 2%Rubrene:1,3-bis(N-carbazolyl)benzene / bis(4,6-difluorophenylpyridine-N,C2)picolinyliridium / 40nm 3TPYMB in sequence as the drain electrode. The device was prepared. The schematic diagram and optical photo of the device are shown in Figure 1. Figure 2 (a) and Figure 2 (b) as shown.

[0130] 6) Performance testing and characterization of light-emitting field effect transistors:

[0131] In the nitrogen atmosphere of the glove box, a probe was used to apply voltage to the source, drain and gate electrodes respectively. The gate electrode was ITO, the source electrode was grounded, the voltage between the source and drain electrodes was -15V, and the voltage between the gate electrode and the source electrode varied from 0V to -15V in steps of -1V. In a dark environment, a photomultiplier tube at 0.5V was used to test the photocurrent of the device. The relationship curve of current-photocurrent-voltage was tested and the relationship between external quantum efficiency (EQE) and brightness was calculated. The maximum brightness of the device was 1170 nits, and the maximum EQE was as high as 13.9%. Figure 3 (a)- Figure 3 (c) is shown. The device luminescence photos were collected using a mobile phone camera. The device luminescence photos at gate voltages of -5V, -6V, and -20V are shown in Figure 2. Figure 4 (a) Figure 4 (b) and Figure 4 (c) shows uniform white light emission and good gate voltage controllability (on / off ratio up to 5×10 5 ), which is of great significance for the use of light-emitting transistors in the field of lighting.

[0132] Comparative Example

[0133] The highest external quantum efficiency of white light OLET reported so far is 2.4%, published in Journal of Materials Chemistry C. 2022, 10(26): 9786-93.

[0134] By comparing the effects of the above embodiments and the comparative examples, it can be seen that the embodiments using the technical solution of the present invention have the beneficial effect of high external quantum efficiency.

[0135] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A white luminescent material for electroluminescence, characterized in that: The materials include: phosphorescent materials and guest-doped host materials; The guest in the guest-doped host material is 5,6,11,12-tetraphenyl tetracene, 2-(4-diphenylamino)phenyl-10,10-dioxo-9-hydrogen-thioxanthen-9-one, bis(2-(3,5-dimethylphenyl)quinoline-C2,N')(acetylacetonate)iridium(III), bis[(4-n-hexylphenyl)isoquinoline](acetylacetonate)iridium(III), bis[5-hexyl-2-(1-isoquinolyl)phenyl](2,4-pentyl)phenyl] diketone)iridium, bis(2-(2'-benzothienyl)pyridine-N,C3')(acetylacetonate)iridium, 7,1-bis(4-(diphenylamino)phenyl)-2,3-dicyanopyrazinophenanthrene, n-hexylphenyl)quinoline](acetylacetonate)iridium(III), 4-(dicyanomethylidene)-2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran, (E)-2-( 2-tert-butyl-6-(2-(2,6,6-trimethyl-2,4,5,6-tetrahydro-1H-pyrrolo[3,2,1-IJ]]quinolin-8-yl)vinyl)-4H-pyran-4-ylidene)malononitrile, tris(2,2',6,6'-tetramethyl-3,5-heptanedione)iridium, acetylacetonate di(4-(4-tert-butyl-phenyl)-thiophene[3,2-C]pyridine-C2,N)iridium(III), acetylacetonate di(4-phenyl) at least one of 2-(2-phenyl-9H-carbazol-3-yl)-1,1-dioxide-9H-thioxanthen-9-one, (OC-6-33)-bis[2-(2-quinolyl)phenyl](2,2,6,6-tetramethyl-3,5-heptanedione)iridium, bis(2-phenylquinoline)(2,2,6,6-tetramethylheptane-3,5-dioate)iridium(III), and rubrene; The host material in the guest-doped host material is at least one selected from 1,3-bis(N-carbazolyl)benzene, 8-hydroxyquinoline aluminum, 4,4'-bis(9-carbazole)biphenyl, 4,4'-bis(2,2-tolylvinyl)biphenyl, 3-tert-butyl-9,10-di(2-naphthalene)anthracene, 2,2":7",2""-tert-9,9'-spirobis[9H-fluorene], 9,10-di(2-naphthyl)anthracene, 4,4'-bis(2,2-distyryl)-1,1'-biphenyl, 2-tert-butyl-9,10-di(2-naphthyl)anthracene, 2-(9,9-spirobifluorene-2-yl)-9,9-spirobifluorene and 2,7-bis[9,9-di(4-methylphenyl)-fluoro-2-yl]-9,9-di(4-methylphenyl)fluorene; The phosphorescent material is selected from bis(4,6-difluorophenylpyridine-N,C2) pyridine carboxylate iridium, perylene, bis[4-(9,9-dimethyl-9,10-dihydroacridine)phenyl]sulfone, bis(3,4,5-trifluoro-2-(2-pyridyl)phenyl-(2-carboxylpyridyl)iridium(III), 4,4'-bis(9-ethyl-3-carbazole vinyl)-1,1'-biphenyl, 4,4'-bis[4-(di-p-tolylamino)phenylphenyl]biphenyl, bis(2-hydroxyphenylpyridine)beryllium, 10-(4-(4 ,6-diphenyl-1,3,5-triazol-2-yl)phenyl)-9,9-dimethyl-9,10-dihydroacridine, 1,1'-(4,4'-(4-phenyl-4H-1,2,4-triazol-3,5-diyl)bis(4,1-phenylene))bis(1H-phenoxazine), 3,3'-(1,4-phenyldi-2,1-vinyl)bis(9-ethyl-9H-carbazole), 9,9'-(5-(4,6-diphenyl-1,3,5-triazine-2-yl)-1,3-phenylene)bis(9H-carbazole ), 1,1'-bis(3,5-bis(trifluoromethyl)phenyl)-9,9'-bianthracene, 9'-[4-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-9,3':6',9"-TER-9H-carbazole, 9,9',9",9"'-(((6-phenyl-1,3,5-triazine-2,4-diyl)bis(benzene-5,3,1-triyl))tetrakis(9H-carbazole), N5,N5,N9,N9-tetraphenylspiro[benzo[C]fluorene-7,9'-fluorene]-5,9-dicarbazole At least one of amine, bis[4-(3,6-di-tert-butyl-9-carbazol-1-yl)phenyl]sulfone, bis[4-tert-butyl-2',6'-difluoro-2,3'-bipyridyl](acetylacetonate)iridium(III), 9-[2,3-bis(9H-carbazol-9-yl)-5-(diphenyl-1,3,5-triazine-2-yl)phenyl]-9Hcarbazole, 2,3,4,6-tetrakis(9H-carbazol-9-yl)-5-fluorobenzonitrile, and (E)-N,N-diphenyl-4-(4-(pyrene-1-yl)phenyl)aniline.

2. The material according to claim 1, characterized in that The phosphorescent material is selected from bis[2-(4,6-difluorophenyl)pyridine-C2,N])iridium(III), the host material is selected from 1,3-bis(N-carbazolyl)benzene, and the guest is selected from rubrene.

3. The material according to claim 1 or 2, characterized in that The molar ratio of the phosphorescent material: the guest: the host material is 5-30: 0.1-3: 67-94.9, preferably 15-25: 0.5-1:75-85。 4. Use of the material according to any one of claims 1 to 3 in an electroluminescent device.

5. A white light emitting transistor with a planar configuration of a surface light source, characterized in that: The light-emitting unit included in the transistor comprises the material according to any one of claims 1 to 3.

6. The transistor according to claim 5, characterized in that The transistor has a lateral integration structure and a bottom light emitting device structure; Preferably, the transistor further comprises a source electrode, a drain electrode, and a charge buffer layer disposed under the drain electrode; Preferably, the source electrode and the drain electrode are arranged in a non-planar manner.

7. The transistor according to claim 6, characterized in that The transistor further includes a semiconductor charge transport layer disposed below the source electrode and the charge buffer layer; Preferably, the source electrode and the drain electrode are arranged on different sides of the semiconductor charge transport layer; Preferably, the light emitting unit is arranged on the charge buffer layer; Preferably, the transistor further comprises an electron transport layer disposed on the light emitting unit; Preferably, the transistor further comprises a dielectric layer disposed under the semiconductor charge transfer layer and a substrate disposed under the dielectric layer.

8. The transistor according to claim 7, characterized in that The EQE peak value of the transistor is no more than 13.9%, the roll-off efficiency is no more than 25% at a brightness of 500 nits, and the current switching ratio is (0.1-5)×10 5 , the driving voltage is not greater than 5V.

9. An application of the planar light source white light emitting transistor according to any one of claims 5 to 8 in white light emitting OLET arrays, full-color displays and lighting.