Steel bar truss and surface treatment process

By introducing reinforcing components and reinforcing components into the steel truss, using collars, connecting plates and other components to support the upper and lower chord steel bars, and fixing the reinforcement plates with bolts, the problem of the lack of support structure at the welds is solved and the structural strength is improved. Stability and protection effect of welding joints.

CN118855166AInactive Publication Date: 2024-10-29鸿志远科技股份有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410985847.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing steel truss lacks a support structure and a protective structure at the welding points, resulting in poor support and prone to rust or breakage.

Method used

Reinforcement components A and B are used to support the upper and lower chord steel bars through components such as collars, connecting plates, bottom plates, support plates, and inner plates. Bolts and fixing nuts are used to fix the reinforcement plates to ensure welding. stability and protection.

Benefits of technology

It improves the overall stability of the steel truss and the protection effect of the welding joints, prevents rust and breakage, and enhances the support capacity of the structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118855166A_ABST
    Figure CN118855166A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of steel bar trusses, discloses a steel bar truss and a surface treatment process, and solves the problem that the interior of the steel bar truss is not provided with other supporting structures and a protection structure for a welding position, the steel bar truss comprises an upper chord steel bar, a lower chord steel bar and a web member steel bar, and a reinforcing component A is arranged on the outer side of the upper chord steel bar; a reinforcing component B is arranged between the lower chord steel bars, the lantern rings slide to the lower chord steel bars, the height of the inner plate is adjusted through cooperation of the positioning grooves and the positioning protruding blocks till the connecting plate B is attached to the bottom layer of the upper chord steel bar, the positioning protruding blocks pop up and are clamped into the positioning grooves, and the inner plate is fixed; and then the two sets of reinforcing plates are used for clamping and protecting the welding position of the upper chord steel bar and the web member steel bar, bolts are matched with fixing nuts to fix the reinforcing plates through a threaded groove A and a threaded groove B, the structural stability is improved, and the purposes of further supporting the steel bar truss and protecting the welding position are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steel bar trusses, in particular to a steel bar truss and a surface treatment process. Background Art

[0002] A steel truss is a building structural element consisting of an upper chord, a lower chord and web bars, connected by nodes to form a stable triangular structure, used to enhance the bearing capacity and stability of a building. Usually the surface is treated with anti-corrosion treatment, such as painting or galvanizing, to extend its service life.

[0003] The existing Chinese patent with publication number CN206256587U discloses a steel truss, including a bottom form, a lower chord, an upper chord, a web bar, vertical steel bars and a support horizontal steel bar. The bottom form is replaced by a galvanized steel plate instead of a construction template floor, and the lower chord, the upper chord, the web bar, the vertical steel bars and the support horizontal steel bars are directly laid on the bottom form, and the bottom form is buckled in sequence, and the steel bars are arranged evenly, so that the spacing between the upper and lower layers of steel bars and the thickness of the concrete protective layer can be fully guaranteed, and then the support vertical bars are spot welded to the upper flange of the beam, the studs are welded, the steel bars are tied, and then a small amount of steel bar installation engineering is performed, and concrete can be poured to form a steel truss concrete cast-in-place slab. However, during use, the patent only supports the structure by welding the lower chord, the upper chord and the web bar steel bars to the floor deck, and the structure does not have other supporting structures and protective structures for the welding points. When the welding points are rusted or broken, there is no other structure to support them, resulting in a poor supporting effect.

[0004] In view of the above problems, a steel bar truss and a surface treatment process are proposed to solve the above problems. Summary of the invention

[0005] The purpose of the present invention is to provide a steel bar truss and a surface treatment process. The device is used to work, thereby solving the problem in the background technology that the steel bar truss has no other supporting structure inside and no protective structure for the welding point.

[0006] To achieve the above object, the present invention provides the following technical solutions: a steel bar truss, comprising an upper chord steel bar, a lower chord steel bar is arranged below the upper chord steel bar, two groups of the lower chord steel bars are arranged symmetrically, a web steel bar is welded between the upper chord steel bar and the lower chord steel bar, a reinforcement component A for reinforcing and protecting the welding position is arranged outside the upper chord steel bar, and a reinforcement component B for improving structural stability is arranged between the two groups of the lower chord steel bars;

[0007] The reinforcement component B includes a ring sleeved on the outside of the lower chord steel bar, and a connecting plate A is fixedly connected to the outside of the ring. There are two groups of rings in total, and the two groups of rings are symmetrically arranged on the outside of the lower chord steel bar. A base plate is arranged between the two groups of connecting plates A. The two groups of connecting plates A are slidably connected to both sides of the base plate, and a support plate is fixedly connected to the upper surface of the base plate. The inner plate is slidably connected to the upper surface of the support plate. The connecting plate B is fixedly connected to the upper surface of the inner plate. The upper surface of the connecting plate B is fitted with the bottom of the upper chord steel bar. A positioning groove is provided on one side of the support plate, and a positioning protrusion is movably connected to one side of the inner plate. The positioning protrusion can be compressed inside the inner plate, and the positioning protrusion and the positioning groove are arranged correspondingly.

[0008] Furthermore, a compression groove is opened on the inner wall of the bottom plate, and a partition is fixedly connected to the inner wall of the bottom plate. The partition evenly divides the compression groove. Springs are fixedly connected on both sides of the partition. The other ends of the two groups of springs are fixedly connected to one side of the connecting plate A.

[0009] Furthermore, the reinforcement component A includes a top plate arranged on the outside of the upper chord steel bars, the top plate is arranged corresponding to the welding point between the upper chord steel bars and the web steel bars, reinforcement grooves are opened on both sides of the top plate, and reinforcement plates are slidably connected inside the two groups of reinforcement grooves, a threaded groove A is opened on one side of the reinforcement plate, a bolt is threadedly connected to one side of the reinforcement plate, one end of the bolt is fitted with one side of one group of the reinforcement plates, and the other end of the bolt is threadedly connected with a fixing nut, and the fixing nut is fitted with one side of the other group of the reinforcement plates.

[0010] Furthermore, a thread groove B is provided on one side of the connecting plate B, the thread groove B is arranged corresponding to the thread groove A, and the bolt penetrates and connects to the inside of the thread groove B.

[0011] Another technical solution proposed by the present invention is to provide a surface treatment process for a steel bar truss, comprising the following steps:

[0012] S1: placing the upper chord steel bars, lower chord steel bars and web steel bars in the fixed structure of the surface treatment device in turn, using the fixed structure for stable clamping, and then cooperating with the rust removal structure in the treatment device to remove rust from the surfaces of the upper chord steel bars, lower chord steel bars and web steel bars;

[0013] S2: The upper chord steel bars, lower chord steel bars and web steel bars after rust removal are transported to the inside of the surface treatment device through the fixed structure. After adjusting to a suitable position, the spray paint structure inside the treatment device is turned on, and the upper chord steel bars, lower chord steel bars and web steel bars are driven to rotate in coordination with the fixed structure to complete the uniform spray paint operation;

[0014] S3: The upper chord steel bars, lower chord steel bars and web bar steel bars after painting are placed statically inside the surface treatment device, and the drying structure is turned on. After the upper chord steel bars, lower chord steel bars and web bar steel bars are completely dried, they are transported out of the treatment device through the fixed structure to complete the surface treatment process.

[0015] Further, in S1, the surface treatment device includes a processing plate, the upper surface of the processing plate is fixedly connected to a processing frame, the processing frame is provided with a clamping mechanism for fixing the steel bar and driving the steel bar to move, and the processing frame is also provided with a rust removal component for rust removal;

[0016] The clamping mechanism includes a motor B fixedly connected to one side of the processing frame, and the output end of the motor B is fixedly connected to a double-threaded rod, one end of the double-threaded rod penetrates the processing frame and is rotatably connected to the inner wall of the processing frame, and a movable block is threadedly connected to the outer side of the double-threaded rod. There are two groups of movable blocks, and the two groups of movable blocks are symmetrically arranged. A pressure plate is fixedly connected to the inner wall of the processing frame, and the bottom surface of the pressure plate is in contact with the upper surface of the movable block. A track plate is fixedly connected to one side of the movable block, and a movable groove is opened on the upper surface of the track plate. A motor B is arranged inside the movable block, and a screw rod is fixedly connected to the output end of the motor B, one end of the screw rod penetrates the movable block and the track plate and is rotatably connected to the inner wall of the movable groove, and a clamping plate is slidably connected inside the movable groove, and the clamping plate is threadedly connected to the screw rod.

[0017] Furthermore, a rotating assembly for fixing and driving the steel bars to rotate is provided inside the clamping plate, and the rotating assembly includes a motor A fixedly connected to one side of the clamping plate, a rotating shaft B is fixedly connected to the output end of the motor A, and a clamping tube is fixedly connected to one end of the rotating shaft B. Both the rotating shaft B and the clamping tube are rotatably connected to the inside of the clamping plate, and a clamping hole is provided on one side of the clamping tube.

[0018] Furthermore, the rust removal component includes a motor A fixedly connected to one side of the processing frame, the output end of the motor A is fixedly connected to the rotating shaft A, the outer side of the rotating shaft A is fixedly connected to a rust removal steel brush, the bottom end of the rust removal steel brush is in contact with the upper surface of the clamping tube, a waste chip groove is provided on the upper surface of the processing plate, and a collection box is fixedly connected to the bottom surface of the processing plate, the waste chip groove passes through the processing plate and is arranged corresponding to the opening of the collection box.

[0019] Furthermore, a paint spraying mechanism for spraying paint on the steel bars is arranged inside the processing frame, and the paint spraying mechanism comprises a cylinder fixedly connected to the upper surface of the processing frame, one end of the cylinder penetrates the upper surface of the processing frame and is fixedly connected to a movable plate, one side of the movable plate is fixedly connected to an electric push rod, an inner groove is provided on the bottom surface of the movable plate, a bottom limit plate is fixedly connected to the inner wall of the inner groove, a driving block is slidably connected inside the inner groove, one end of the electric push rod penetrates one side of the movable plate and is fixedly connected to one side of the driving block, a paint injection barrel is fixedly connected to the bottom surface of the driving block, a paint spraying pump is fixedly connected to the bottom surface of the paint injection barrel, an atomizing nozzle is fixedly installed on the bottom surface of the paint spraying pump, a paint injection pipe is fixedly connected to the outer side of the paint injection barrel, and the paint injection pipe is externally connected to the raw material barrel.

[0020] Furthermore, a dryer is fixedly connected to one side of the processing frame, and one side of the dryer is communicated with the interior of the processing frame.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] The present invention provides a steel truss and surface treatment process. By setting a reinforcing component A and a reinforcing component B, before completing welding, the collar is slid to the bottom of the welding point between the web reinforcement and the upper chord reinforcement. After welding, the inner plate is adjusted in height by using the positioning groove and the positioning protrusion until the connecting plate B fits with the bottom layer of the upper chord reinforcement. The positioning protrusion pops out and snaps into the inside of the positioning groove, thereby fixing the inner plate. The collar, the connecting plate A, the bottom plate, the support plate and the inner plate are used to further support the upper chord reinforcement and the lower chord reinforcement, thereby improving the stability of the device. The top plate is placed Above the upper chord steel bars, two groups of reinforcement plates are slidably connected to the inside of the reinforcement groove to clamp and protect the welding points between the upper chord steel bars and the web steel bars. The two groups of reinforcement plates are fixed by bolts and fixing nuts. When fixing the reinforcement plates, the thread groove A corresponds to the thread groove B, and the bolts also pass through the thread groove B to ensure that the top plate is in a horizontal state when fixed. At the same time, the bolts are connected to the fixing nuts below, so that the reinforcement components A and B cooperate with each other to improve the stability of the structure, thereby achieving the purpose of further supporting the steel truss and protecting the welding points. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the steel bar truss structure of the present invention;

[0024] Figure 2 This is a schematic structural diagram of the reinforcement component A of the present invention;

[0025] Figure 3 This is a structural schematic diagram of the reinforcement component B of the present invention;

[0026] Figure 4 It is a schematic plan view of the internal structure of the bottom plate of the present invention;

[0027] Figure 5 It is a schematic diagram of a steel bar surface treatment device of the present invention;

[0028] Figure 6 It is a schematic diagram of the structure of the clamping mechanism of the present invention;

[0029] Figure 7 It is a schematic diagram of the structure of the rotating assembly of the present invention;

[0030] Figure 8 It is a schematic diagram of the paint spraying mechanism structure of the present invention;

[0031] Fig. 9 It is a schematic diagram of the internal structure of the movable plate of the present invention;

[0032] Fig.10 It is a partial structural schematic diagram of the paint spraying mechanism of the present invention.

[0033] In the figure: 1, upper chord steel bar; 2, lower chord steel bar; 3, web bar steel bar; 4, reinforcement component A; 41, top plate; 42, reinforcement groove; 43, reinforcement plate; 44, thread groove A; 45, bolt; 46, fixing nut; 5, reinforcement component B; 51, collar; 52, connecting plate A; 53, bottom plate; 531, partition; 532, compression groove; 533, spring; 54, support plate; 541, positioning groove; 55, inner plate; 551, positioning protrusion; 56, connecting plate B; 561, thread groove B; 6, processing plate; 61, processing frame; 62, waste chip groove; 63, collection box; 64, pressure plate; 65. Dryer; 7. Rust removal assembly; 71. Motor A; 72. Rotating shaft A; 73. Rust removal steel brush; 8. Clamping mechanism; 81. Motor B; 82. Double threaded rod; 83. Movable block; 84. Track plate; 841. Movable groove; 85. Screw rod; 86. Clamping plate; 87. Rotating assembly; 871. Motor A; 872. Rotating shaft B; 873. Clamping tube; 9. Paint spraying mechanism; 91. Cylinder; 92. Movable plate; 921. Inner groove; 922. Bottom limit plate; 93. Electric push rod; 94. Driving block; 95. Paint injection cylinder; 96. Paint spraying pump; 97. Atomizing nozzle; 98. Paint injection tube. DETAILED DESCRIPTION

[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0035] Embodiment 1

[0036] To further understand the content of the present invention, Figure 1-Figure 4 As shown, the following preferred technical solutions are provided:.

[0037] Combination Figure 1-Figure 3 A steel truss comprises an upper chord steel bar 1, a lower chord steel bar 2 is arranged below the upper chord steel bar 1, two groups of the lower chord steel bars 2 are arranged in total, the two groups of the lower chord steel bars 2 are symmetrically arranged, a web steel bar 3 is welded between the upper chord steel bar 1 and the lower chord steel bar 2, a reinforcing component A4 for reinforcing and protecting the welding point is arranged on the outer side of the upper chord steel bar 1, and a reinforcing component B5 for improving structural stability is arranged between the two groups of the lower chord steel bars 2;

[0038] The reinforcement component B5 includes a ring 51 sleeved on the outer side of the lower chord steel bar 2, and a connecting plate A52 is fixedly connected to the outer side of the ring 51. There are two groups of the rings 51, and the two groups of the rings 51 are symmetrically arranged on the outer side of the lower chord steel bar 2. A bottom plate 53 is arranged between the two groups of the connecting plates A52. The two groups of the connecting plates A52 are slidably connected to both sides of the bottom plate 53. A support plate 54 is fixedly connected to the upper surface of the bottom plate 53, and an inner plate 55 is slidably connected to the upper surface of the support plate 54. A connecting plate B56 is fixedly connected to the upper surface of the inner plate 55. The upper surface of the connecting plate B56 is fitted with the bottom of the upper chord steel bar 1. A positioning groove 541 is provided on one side of the support plate 54, and a positioning groove 541 is movably connected to one side of the inner plate 55. Bump 551, the positioning bump 551 can be compressed inside the inner plate 55, the positioning bump 551 is set corresponding to the positioning groove 541, before completing the welding, the ring 51 is slid to the bottom of the welding point between the web reinforcement 3 and the upper chord reinforcement 1, after the welding is completed, the inner plate 55 is height adjusted by using the positioning groove 541 in conjunction with the positioning bump 551, until the connecting plate B56 fits with the bottom layer of the upper chord reinforcement 1, and the positioning bump 551 is snapped into the inside of the positioning groove 541, thereby fixing the inner plate 55, so as to further support the upper chord reinforcement 1 and the lower chord reinforcement 2 by using the ring 51, the connecting plate A52, the bottom plate 53, the support plate 54 and the inner plate 55, thereby improving the stability of the device.

[0039] A compression groove 532 is opened on the inner wall of the bottom plate 53, and a partition 531 is fixedly connected to the inner wall of the bottom plate 53. The partition 531 evenly divides the compression groove 532. Springs 533 are fixedly connected on both sides of the partition 531. The other ends of the two groups of springs 533 are fixedly connected to one side of the connecting plate A52. The partition 531, the compression groove 532 and the spring 533 are arranged to facilitate distance adjustment when welding the lower chord steel bars 2. At the same time, the spring 533 plays a certain buffering and protective effect during use.

[0040] The reinforcement component A4 includes a top plate 41 arranged on the outside of the upper chord steel bar 1, the top plate 41 is arranged corresponding to the welding position of the upper chord steel bar 1 and the web steel bar 3, both sides of the top plate 41 are provided with reinforcement grooves 42, and the two groups of reinforcement grooves 42 are slidably connected with reinforcement plates 43, one side of the reinforcement plate 43 is provided with a threaded groove A44, one side of the reinforcement plate 43 is threadedly connected with a bolt 45, one end of the bolt 45 is in contact with one side of one group of the reinforcement plates 43, and the other end of the bolt 45 is threadedly connected with a fixing screw The nut 46 and the fixing nut 46 are fitted with one side of the other group of the reinforcing plates 43. Through the arrangement of the top plate 41, the reinforcing groove 42, the reinforcing plate 43, the threaded groove A44, the bolt 45 and the fixing nut 46, the two groups of the reinforcing plates 43 are slidably connected to the inside of the reinforcing groove 42 to clamp and protect the welding point between the upper chord steel bar 1 and the web steel bar 3. The two groups of the reinforcing plates 43 are fixed by the bolts 45 and the fixing nuts 46, and the top plate 41 protects the upper chord steel bar 1 from the upper end.

[0041] A thread groove B561 is provided on one side of the connecting plate B56, and the thread groove B561 is arranged corresponding to the thread groove A44, and the bolt 45 is connected through the thread groove B561. When fixing the reinforcing plate 43, the thread groove A44 is aligned with the thread groove B561 before fixing, so as to ensure that the top plate 41 is in a horizontal state when fixed, and the bolt 45 is connected with the fixing nut 46 below, and cooperates with the reinforcing component B5 to improve the stability of the structure.

[0042] Specifically, by setting the reinforcing components A4 and B5, before completing welding, the ring 51 is slid to the bottom of the welding point between the web reinforcement 3 and the upper chord reinforcement 1. After welding, the inner plate 55 is adjusted in height by using the positioning groove 541 in cooperation with the positioning protrusion 551 until the connecting plate B56 fits with the bottom layer of the upper chord reinforcement 1, and the positioning protrusion 551 pops out and snaps into the inside of the positioning groove 541, thereby fixing the inner plate 55. The ring 51, the connecting plate A52, the bottom plate 53, the support plate 54 and the inner plate 55 are further supported between the upper chord reinforcement 1 and the lower chord reinforcement 2 to improve the stability of the device. The top plate 41 is placed on the upper chord reinforcement 1, two groups of reinforcing plates 43 are slidably connected to the inside of the reinforcing groove 42 to clamp and protect the welding place between the upper chord steel bar 1 and the web steel bar 3, and the two groups of reinforcing plates 43 are fixed by bolts 45 and fixing nuts 46. When the reinforcing plates 43 are fixed, the thread groove A44 corresponds to the thread groove B561, and the bolt 45 also passes through the thread groove B561 to ensure that the top plate 41 is in a horizontal state when fixed. At the same time, the bolt 45 is connected with the fixing nut 46 below, so that the reinforcing component A4 and the reinforcing component B5 cooperate with each other to improve the stability of the structure, and achieve the purpose of further supporting the steel truss and protecting the welding place.

[0043] Embodiment 2

[0044] In order to solve the technical problem of how to uniformly treat the surface of the steel truss, such as Figure 5-Figure 9 As shown, the following preferred technical solutions are provided:

[0045] Another technical solution proposed by the present invention is to provide a surface treatment process for a steel bar truss, comprising the following steps:

[0046] S1: placing the upper chord steel bar 1, the lower chord steel bar 2 and the web steel bar 3 in the fixed structure of the surface treatment device in turn, using the fixed structure for stable clamping, and then cooperating with the rust removal structure in the treatment device to remove rust from the surfaces of the upper chord steel bar 1, the lower chord steel bar 2 and the web steel bar 3;

[0047] S2: The upper chord steel bars 1, the lower chord steel bars 2 and the web steel bars 3 after rust removal are transported to the inside of the surface treatment device through the fixed structure, and after adjusting to a suitable position, the spray paint structure inside the treatment device is turned on, and the upper chord steel bars 1, the lower chord steel bars 2 and the web steel bars 3 are driven to rotate in coordination with the fixed structure to complete the operation of uniform spray paint;

[0048] S3: The upper chord steel bars 1, the lower chord steel bars 2 and the web steel bars 3 after painting are placed statically inside the surface treatment device, and the drying structure is turned on. After the upper chord steel bars 1, the lower chord steel bars 2 and the web steel bars 3 are completely dried, they are transported out of the treatment device through the fixed structure to complete the surface treatment process.

[0049] In S1, the surface treatment device includes a processing plate 6, the upper surface of the processing plate 6 is fixedly connected to a processing frame 61, the processing frame 61 is provided with a clamping mechanism 8 for fixing the steel bar and driving the steel bar to move, and the processing frame 61 is also provided with a rust removal component 7 for rust removal;

[0050] The clamping mechanism 8 includes a motor B81 fixedly connected to one side of the processing frame 61, and the output end of the motor B81 is fixedly connected to a double-threaded rod 82, one end of the double-threaded rod 82 penetrates the processing frame 61 and is rotatably connected to the inner wall of the processing frame 61, and the outer side of the double-threaded rod 82 is threadedly connected to a movable block 83, and the movable blocks 83 are provided in two groups, and the two groups of movable blocks 83 are symmetrically arranged, and a pressure plate 64 is fixedly connected to the inner wall of the processing frame 61, and the bottom surface of the pressure plate 64 is in contact with the upper surface of the movable block 83, and a track plate 84 is fixedly connected to one side of the movable block 83, and a movable groove 841 is provided on the upper surface of the track plate 84, and a motor B is arranged inside the movable block 83, and a screw rod 85 is fixedly connected to the output end of the motor B, and one end of the screw rod 85 penetrates the movable block 83 and the track plate 84 and is rotatably connected to the inner wall of the movable groove 841, and a clamping plate 86 is slidably connected inside the movable groove 841, and the clamping plate 86 is threadedly connected to the screw rod 85. When fixing the steel bars, turn on the motor B inside the movable block 83, and the motor B rotates to drive the clamping plate 86 to slide along the screw rod 85 and connect to the inside of the movable groove 841, and the clamping plate 86 is transported to one side of the processing frame 61 for loading. When the steel bars are set between the two groups of the clamping plates 86, turn on the motor B81, and two groups of threads with opposite thread directions are set on the outside of the double-threaded rod 82, and the two groups of threads are symmetrically arranged. The motor B81 drives the double-threaded rod 82 to rotate, and the double-threaded rod 82 is used to bring the two groups of movable blocks 83 closer to the middle, so that the clamping plate 86 is used to clamp the steel bars, providing stable conditions for subsequent painting and rust removal.

[0051] A rotating assembly 87 for fixing and driving the steel bars to rotate is provided inside the clamping plate 86, and the rotating assembly 87 includes a motor A871 fixedly connected to one side of the clamping plate 86, and the output end of the motor A871 is fixedly connected to a rotating shaft B872, and one end of the rotating shaft B872 is fixedly connected to a clamping tube 873, and the rotating shaft B872 and the clamping tube 873 are both rotatably connected to the inside of the clamping plate 86, and a clamping hole is provided on one side of the clamping tube 873. When fixing the steel bars, the two ends of the steel bars are respectively placed in the clamping holes provided on one side of the clamping tube 873, and the two groups of the clamping plates 86 are brought together by the motor B81 to complete the fixation of the steel bars. In addition, when the steel bars need to be rotated, the motor A871 is turned on, and the motor A871 drives the rotating shaft B872 and the clamping tube 873 to rotate to complete the rotation operation.

[0052] The rust removal component 7 includes a motor A71 fixedly connected to one side of the processing frame 61, and the output end of the motor A71 is fixedly connected to a rotating shaft A72, and a rust removal steel brush 73 is fixedly connected to the outer side of the rotating shaft A72, and the bottom end of the rust removal steel brush 73 is in contact with the upper surface of the clamping tube 873. A waste chip groove 62 is provided on the upper surface of the processing plate 6, and a collection box 63 is fixedly connected to the bottom surface of the processing plate 6. The waste chip groove 62 penetrates the processing plate 6 and is arranged corresponding to the opening of the collection box 63. When performing the rust removal operation, the motor A71 and the motor A871 are turned on at the same time, and the rust removal steel brush 73 and the steel bars rotate simultaneously to remove the rust on the surface of the steel bars to complete the rust removal operation. The waste chips fall into the collection box 63 through the waste chip groove 62 for subsequent collection.

[0053] A paint spraying mechanism 9 for spraying paint on steel bars is arranged inside the processing frame 61, and the paint spraying mechanism 9 includes a cylinder 91 fixedly connected to the upper surface of the processing frame 61, one end of the cylinder 91 penetrates the upper surface of the processing frame 61 and is fixedly connected to a movable plate 92, one side of the movable plate 92 is fixedly connected to an electric push rod 93, an inner groove 921 is provided on the bottom surface of the movable plate 92, a bottom limit plate 922 is fixedly connected to the inner wall of the inner groove 921, a driving block 94 is slidably connected inside the inner groove 921, one end of the electric push rod 93 penetrates one side of the movable plate 92 and is fixedly connected to one side of the driving block 94, and a paint injection cylinder 95 is fixedly connected to the bottom surface of the driving block 94. A paint pump 96 is fixedly connected to the bottom of the paint injection cylinder 95, and an atomizing nozzle 97 is fixedly installed on the bottom of the paint injection cylinder 95. A paint injection pipe 98 is fixedly connected to the outer side of the paint injection cylinder 95, and the paint injection pipe 98 is externally connected to the raw material barrel. When spraying paint, the motor B inside the movable block 83 is first used to drive the screw rod 85 to rotate, so as to adjust the horizontal position of the clamping plate 86. When the steel bar corresponds to the atomizing nozzle 97, the cylinder 91 is turned on to adjust the vertical height of the atomizing nozzle 97. After the adjustment is completed, the electric push rod 93 and the motor A871 are turned on at the same time. While adjusting the paint spraying position, the steel bar is rotated to achieve uniform paint spraying on the steel bar.

[0054] A drying machine 65 is fixedly connected to one side of the processing frame 61 , and one side of the drying machine 65 is communicated with the interior of the processing frame 61 . The drying operation of the steel bar spray paint is completed through the drying machine 65 .

[0055] Specifically, when fixing the steel bar, the motor B inside the movable block 83 is turned on, and the motor B rotates to drive the clamping plate 86 to slide along the screw rod 85 and connect to the inside of the movable groove 841, and the clamping plate 86 is transported to one side of the processing frame 61 for loading. When fixing the steel bar, the two ends of the steel bar are respectively connected to the clamping holes on one side of the clamping tube 873, and the motor B81 is turned on. Two groups of threads with opposite thread directions are arranged on the outer side of the double-threaded rod 82, and the two groups of threads are symmetrically arranged. The motor B81 drives the double-threaded rod 82 to rotate, and the double-threaded rod 82 is used to bring the two groups of movable blocks 83 closer to the middle, so that the clamping plate 86 is used to clamp the steel bar. When performing the rust removal operation, the motor A71 and the motor A871 are turned on at the same time, and the rust removal steel is The brush 73 and the steel bar rotate simultaneously to remove the rust on the surface of the steel bar, completing the rust removal operation. The waste chips fall into the collection box 63 through the waste chip groove 62 for subsequent collection. When spraying paint, the motor B inside the movable block 83 is first used to drive the screw rod 85 to rotate, so as to adjust the horizontal position of the clamping plate 86. When the steel bar corresponds to the atomizing nozzle 97, the cylinder 91 is turned on to adjust the vertical height of the atomizing nozzle 97. After the adjustment, the electric push rod 93 and the motor A871 are turned on. While adjusting the paint spraying position, the steel bar is rotated to achieve uniform paint spraying on the steel bar. The drying operation of the steel bar spray paint is completed through the dryer 65, and finally the purpose of uniformly spraying paint on the outer side of the steel bar truss after rust removal is achieved.

[0056] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0057] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A steel bar truss, comprising an upper chord steel bar (1), a lower chord steel bar (2) is arranged below the upper chord steel bar (1), two groups of the lower chord steel bars (2) are arranged in total, the two groups of the lower chord steel bars (2) are symmetrically arranged, a web bar (3) is welded between the upper chord steel bar (1) and the lower chord steel bar (2), characterized in that: A reinforcing component A (4) for reinforcing and protecting the welding point is arranged outside the upper chord steel bars (1), and a reinforcing component B (5) for improving structural stability is arranged between the two groups of lower chord steel bars (2); The reinforcing component B (5) comprises a sleeve (51) sleeved on the outer side of the lower chord steel bar (2), a connecting plate A (52) being fixedly connected to the outer side of the sleeve (51), two groups of the sleeve (51) being provided, the two groups of the sleeve (51) being symmetrically arranged on the outer side of the lower chord steel bar (2), a bottom plate (53) being arranged between the two groups of the connecting plates A (52), the two groups of the connecting plates A (52) being slidably connected to the two sides of the bottom plate (53), and a support plate (53) being fixedly connected to the upper surface of the bottom plate (53) 54), the upper surface of the support plate (54) is slidably connected to the inner plate (55), the upper surface of the inner plate (55) is fixedly connected to the connecting plate B (56), the upper surface of the connecting plate B (56) is in contact with the bottom of the upper chord steel bar (1), a positioning groove (541) is provided on one side of the support plate (54), a positioning protrusion (551) is movably connected to one side of the inner plate (55), the positioning protrusion (551) can be compressed inside the inner plate (55), and the positioning protrusion (551) and the positioning groove (541) are arranged correspondingly.

2. A steel bar truss according to claim 1, characterized in that: The inner wall of the bottom plate (53) is provided with a compression groove (532), and a partition (531) is fixedly connected to the inner wall of the bottom plate (53), and the partition (531) evenly divides the compression groove (532), and springs (533) are fixedly connected to both sides of the partition (531), and the other ends of the two groups of springs (533) are fixedly connected to one side of the connecting plate A (52).

3. A steel bar truss according to claim 1, characterized in that: The reinforcing component A (4) comprises a top plate (41) arranged outside the upper chord steel bar (1), the top plate (41) being arranged corresponding to the welding position of the upper chord steel bar (1) and the web steel bar (3), both sides of the top plate (41) are provided with reinforcing grooves (42), the insides of two groups of the reinforcing grooves (42) are both slidably connected with reinforcing plates (43), one side of the reinforcing plate (43) is provided with a threaded groove A (44), one side of the reinforcing plate (43) is threadedly connected with a bolt (45), one end of the bolt (45) is in contact with one side of one group of the reinforcing plates (43), the other end of the bolt (45) is threadedly connected with a fixing nut (46), and the fixing nut (46) is in contact with one side of the other group of the reinforcing plates (43).

4. A steel bar truss according to claim 3, characterized in that: A thread groove B (561) is provided on one side of the connecting plate B (56), the thread groove B (561) is arranged corresponding to the thread groove A (44), and the bolt (45) penetrates and is connected to the inside of the thread groove B (561).

5. A surface treatment process for a steel truss according to any one of claims 1 to 4, characterized in that: The following steps are involved: S1: placing the upper chord steel bars (1), the lower chord steel bars (2) and the web steel bars (3) in a fixed structure in a surface treatment device, using the fixed structure to stably clamp them, and then using the rust removal structure in the treatment device to remove rust from the surfaces of the upper chord steel bars (1), the lower chord steel bars (2) and the web steel bars (3); S2: The rust-removed upper chord steel bars (1), lower chord steel bars (2) and web steel bars (3) are transported to the inside of the surface treatment device through the fixed structure, and after being adjusted to a suitable position, the painting structure inside the treatment device is turned on, and the upper chord steel bars (1), lower chord steel bars (2) and web steel bars (3) are driven to rotate in coordination with the fixed structure, so as to complete the operation of uniform painting; S3: The upper chord steel bars (1), the lower chord steel bars (2) and the web steel bars (3) after being sprayed with paint are placed statically in the surface treatment device, and the drying structure is turned on. After the upper chord steel bars (1), the lower chord steel bars (2) and the web steel bars (3) are completely dried, they are transported out of the treatment device through the fixed structure, and the surface treatment process is completed.

6. A steel bar truss and surface treatment process according to claim 5, characterized in that: In S1, the surface treatment device comprises a processing plate (6), the upper surface of the processing plate (6) is fixedly connected to a processing frame (61), the processing frame (61) is provided with a clamping mechanism (8) for fixing the steel bar and driving the steel bar to move, and the processing frame (61) is also provided with a rust removal component (7) for rust removal; The clamping mechanism (8) comprises a motor B (81) fixedly connected to one side of the processing frame (61); a double-threaded rod (82) is fixedly connected to the output end of the motor B (81); one end of the double-threaded rod (82) penetrates the processing frame (61) and is rotatably connected to the inner wall of the processing frame (61); a movable block (83) is threadedly connected to the outer side of the double-threaded rod (82); two groups of movable blocks (83) are provided, and the two groups of movable blocks (83) are symmetrically arranged; a pressing plate (64) is fixedly connected to the inner wall of the processing frame (61); the bottom of the pressing plate (64) is The movable block (83) is fitted with a track plate (84) on one side thereof, and a movable groove (841) is provided on the upper surface of the track plate (84). A motor B is arranged inside the movable block (83), and a screw rod (85) is fixedly connected to the output end of the motor B. One end of the screw rod (85) passes through the movable block (83) and the track plate (84) and is rotatably connected to the inner wall of the movable groove (841). A clamping plate (86) is slidably connected inside the movable groove (841), and the clamping plate (86) is threadedly connected to the screw rod (85).

7. A steel bar truss and surface treatment process according to claim 6, characterized in that: A rotating assembly (87) for fixing and driving the steel bar to rotate is arranged inside the clamping plate (86), and the rotating assembly (87) includes a motor A (871) fixedly connected to one side of the clamping plate (86), and the output end of the motor A (871) is fixedly connected to a rotating shaft B (872), and one end of the rotating shaft B (872) is fixedly connected to a clamping tube (873), and the rotating shaft B (872) and the clamping tube (873) are both rotatably connected to the inside of the clamping plate (86), and a clamping hole is opened on one side of the clamping tube (873).

8. A steel bar truss and surface treatment process according to claim 7, characterized in that: The rust removal assembly (7) comprises a motor A (71) fixedly connected to one side of a processing frame (61); a rotating shaft A (72) is fixedly connected to the output end of the motor A (71); a rust removal steel brush (73) is fixedly connected to the outer side of the rotating shaft A (72); the bottom end of the rust removal steel brush (73) is in contact with the upper surface of the clamping tube (873); a waste chip groove (62) is provided on the upper surface of the processing plate (6); a collection box (63) is fixedly connected to the bottom surface of the processing plate (6); the waste chip groove (62) penetrates the processing plate (6) and is arranged corresponding to the opening of the collection box (63).

9. A steel bar truss and surface treatment process according to claim 8, characterized in that: The processing frame (61) is provided with a paint spraying mechanism (9) for spraying paint on the steel bars. The paint spraying mechanism (9) comprises a cylinder (91) fixedly connected to the upper surface of the processing frame (61). One end of the cylinder (91) passes through the upper surface of the processing frame (61) and is fixedly connected to a movable plate (92). One side of the movable plate (92) is fixedly connected to an electric push rod (93). The bottom surface of the movable plate (92) is provided with an inner groove (921). The inner wall of the inner groove (921) is fixedly connected to a bottom limit plate (922). ), a driving block (94) is slidably connected inside the inner groove (921), one end of the electric push rod (93) passes through one side of the movable plate (92) and is fixedly connected to one side of the driving block (94), a paint injection cylinder (95) is fixedly connected to the bottom surface of the driving block (94), a paint spraying pump (96) is fixedly connected to the bottom surface of the paint injection cylinder (95), an atomizing nozzle (97) is fixedly installed on the bottom surface of the paint spraying pump (96), a paint injection pipe (98) is fixedly connected to the outside of the paint injection cylinder (95), and the paint injection pipe (98) is externally connected to the raw material barrel.

10. A steel bar truss and surface treatment process according to claim 9, characterized in that: A drying machine (65) is fixedly connected to one side of the processing frame (61), and one side of the drying machine (65) is communicated with the interior of the processing frame (61).