Municipal road crack repair detection method and system
By comprehensively analyzing the pavement image, settlement and vehicle data of municipal roads, and evaluating the cracking degree and strain index of cracks, the problem that traditional visual monitoring methods cannot accurately evaluate crack depth and predict crack expansion is solved, and road maintenance efficiency and safety are improved. Extend the service life of the road.
Patent Information
- Application Number
- CN202411337310.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-25
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-09-25
AI Technical Summary
Traditional visual monitoring methods cannot accurately evaluate the three-dimensional structural characteristics and internal microscopic damage of municipal road cracks, it is difficult to predict the expansion trend of cracks and its long-term impact on road structure, and it is impossible to comprehensively analyze the complex factors affecting the development of cracks.
A municipal road crack repair detection method is adopted to calculate the crack degree, expansion status and strain index of the cracks, and comprehensively evaluate the severity of the cracks and the repair needs by obtaining pavement images, settlement data, ambient temperature data and vehicle data.
It achieves a more accurate prediction of the tendency of crack deterioration, improves the efficiency and effectiveness of road maintenance work, ensures road safety and stability, and extends the service life of the road.
Smart Images

Figure CN118864456B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of image data processing, and in particular to a municipal road crack repair detection method and system. Background Art
[0002] Municipal roads are part of urban public utility projects and an indispensable part of urban operations. Due to the service life of roads, they are often damaged by the external environment, so they need to be inspected and repaired in real time. In the current road maintenance practice, the assessment and repair of cracks in municipal roads is a key step to ensure road safety and extend service life.
[0003] Traditional visual monitoring methods rely on manual or preliminary image recognition technology to inspect the road surface. This method can only capture the surface characteristics of cracks, such as length, width and morphology, and cannot accurately evaluate the three-dimensional structural characteristics of cracks, accurately measure the depth of cracks or identify the microscopic damage inside them. These limitations lead to maintenance decisions often based on incomplete information, which may overlook cracks that are not conspicuous but may deteriorate rapidly. It is difficult to predict the expansion trend of cracks and the long-term impact on the structural integrity of the road. In addition, the development of road cracks is affected by many factors, such as temperature changes, moisture penetration, vehicle loads and the properties of the base material. It is difficult for traditional visual inspections to conduct a comprehensive analysis of these complex factors, and thus it is impossible to effectively predict the expansion of cracks and the impact on road performance. Summary of the invention
[0004] The invention provides a municipal road crack repair detection method and system to solve the existing problems.
[0005] A municipal road crack repair detection method and system of the present invention adopts the following technical solutions:
[0006] An embodiment of the present invention provides a municipal road crack repair detection method, the method comprising the following steps:
[0007] Acquire a number of road surface images within a preset acquisition time period; the road surface images include a number of cracks and corresponding crack edges; acquire settlement data of any road surface, ambient temperature data within a preset time period, and vehicle data passing through any road surface;
[0008] According to the length of the crack and the grayscale expression of the pixel point corresponding to the crack, the cracking degree of any crack is obtained; according to the length growth rate of the crack and the directional characteristics of the crack edge, the expansion of any crack is determined;
[0009] The settlement data is processed to obtain the settlement rate of the road surface. The strain index of any road surface is obtained by combining the ambient temperature data, the vehicle data on the road surface, and the settlement rate of the road surface. The comprehensive expansion of any crack is obtained by combining the expansion of the crack and the strain index of the road surface to which the crack belongs.
[0010] The comprehensive expansion of cracks and the cracking degree of cracks are combined to obtain the comprehensive performance degree of any crack;
[0011] The severity of all cracks is judged according to the comprehensive performance of the cracks, and corresponding repairs are carried out.
[0012] Furthermore, the cracking degree of any crack is obtained according to the length of the crack and the grayscale expression of the pixel point corresponding to the crack, including the specific method of:
[0013]
[0014] in, Indicates the degree of cracking of any crack, represents the length of the crack, represents the length of the road surface to which the crack belongs, represents the grayscale mean of all pixels on the crack, Represents the normalization function.
[0015] Furthermore, the method of determining the expansion of any crack according to the crack length growth rate and the directional characteristics of the crack edge includes the following specific methods:
[0016] Get the length growth rate of the crack;
[0017] According to the directional characteristics of the crack edge, a directional angle interval-directional angle interval frequency histogram of the crack is obtained;
[0018] The expansion of any crack is obtained as follows:
[0019]
[0020] in, represents the expansion of any crack, represents the length growth rate of the crack, represents the maximum direction angle interval frequency on the direction angle interval-direction angle interval frequency histogram of the crack, It represents the mean value of all the directional angle interval frequencies on the directional angle interval-directional angle interval frequency histogram of the crack.
[0021] Furthermore, the specific method for obtaining the length growth rate of the crack is:
[0022] by As the origin, a coordinate system is established with the sampling time as the X-axis and the crack length as the Y-axis, and a time-length scatter plot of any crack is drawn; a straight line is fitted to the scattered points in the time-length scatter plot of the crack, and the slope of the fitted straight line is recorded as the length growth rate of the crack.
[0023] Furthermore, the specific method for obtaining the direction angle interval-direction angle interval frequency histogram of the crack according to the direction characteristics of the crack edge is:
[0024] Taking the horizontal right direction as the standard direction, obtaining the direction angle of any pixel point on the edge of any crack, taking the preset angle as the direction angle interval size, obtaining the number of pixel points in any direction angle interval; dividing the number of pixel points in any direction angle interval by the number of all pixel points to obtain the frequency of the direction angle interval, and drawing the direction angle interval-direction angle interval frequency histogram of the crack;
[0025] The directional angle interval-directional angle interval frequency histogram of any crack is used to describe the directional characteristics of the crack edge.
[0026] Furthermore, the settlement data is processed to obtain the settlement rate of the road surface, and the strain index of any road surface is obtained by combining the ambient temperature data, the vehicle data of the road surface, and the settlement rate of the road surface, including the specific method of:
[0027] The settlement rate of any road surface is obtained by using small baseline subset technique on the settlement data;
[0028] The strain index of any road surface is obtained as follows:
[0029]
[0030] in, represents the strain index of any road surface, Indicates the average value of the ambient temperature during the acquisition period. is the total number of heavy vehicles passing through the road during the collection period, is the total number of vehicles passing the road during the collection period, is the settlement rate of the road surface.
[0031] Furthermore, the comprehensive crack expansion and the strain index of the road surface to which the crack belongs are combined to obtain the comprehensive expansion of any crack, including the following specific methods:
[0032] The comprehensive expansion of any crack is in direct proportion to the expansion of the crack and the strain index of the road surface to which the crack belongs.
[0033] Furthermore, the comprehensive expansion of the cracks and the cracking degree of the cracks are combined to obtain the comprehensive performance degree of any crack, including the following specific methods:
[0034]
[0035] in, Indicates the comprehensive performance of any crack. Indicates the degree of cracking of the crack, represents the comprehensive expansion of the cracks, Represents the normalization function.
[0036] Furthermore, the comprehensive performance of all cracks on any road surface is comprehensively evaluated to determine the crack conditions of the road surface and to perform corresponding repairs, including the following specific methods:
[0037] Adding the comprehensive performance levels of all cracks on any road surface to obtain the comprehensive performance of cracks on the road surface;
[0038] When the comprehensive performance of road cracks is less than or equal to the preset first parameter, the road surface is recorded as a non-dangerous state; when the comprehensive performance of road cracks is greater than the preset first parameter and less than the preset second parameter, the road surface is recorded as a relatively dangerous state and road repair is arranged; when the comprehensive performance of road cracks is greater than or equal to the preset second parameter, the road surface is recorded as a high-dangerous state, and vehicles passing through the road surface need to be stopped and repairs must be carried out immediately.
[0039] An embodiment of the present invention provides a municipal road crack repair detection system, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements any one of the steps of the municipal road crack repair detection method when executing the computer program.
[0040] The beneficial effect of the technical solution of the present invention is that by comprehensively considering various external factors that affect the development of cracks, the actual condition of the cracks and their potential expansion risks can be more comprehensively reflected. By considering the influence of various external factors and introducing correction factors, the deterioration trend of the cracks can be more accurately predicted, providing a scientific basis for the timing and scope of repair work. This method not only improves the efficiency and effectiveness of road maintenance work, but also helps to reasonably allocate maintenance resources, ensure the safety and stability of the road, and thus extend the service life of the road. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0042] Figure 1 The present invention is a flowchart of the steps of a municipal road crack repair detection method.
[0043] Figure 2 It is a schematic diagram of straight line fitting of a crack time-length scatter plot of a municipal road crack repair detection method of the present invention.
[0044] Figure 3 It is a crack direction angle interval-direction angle interval frequency histogram of a municipal road crack repair detection method of the present invention. DETAILED DESCRIPTION
[0045] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the following is a detailed description of a municipal road crack repair detection method and system proposed by the present invention, its specific implementation method, structure, features and effects, in conjunction with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.
[0046] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0047] The specific scheme of a municipal road crack repair detection method and system provided by the present invention is described in detail below with reference to the accompanying drawings.
[0048] See also Figure 1 , which shows a flow chart of the steps of a municipal road crack repair detection method provided by an embodiment of the present invention, the method comprising the following steps:
[0049] Step S001: Collect data related to municipal road cracks.
[0050] Specifically, in order to implement a municipal road crack repair detection method proposed in this embodiment, it is first necessary to collect municipal road crack related data, and the specific process is as follows:
[0051] Preset the collection time period and collection frequency, and obtain several road surface images within several road surface collection time periods; use the Canny algorithm to perform edge detection on any road surface image, and obtain several cracks and corresponding crack edges of the road surface image; obtain the length data of any crack; obtain the settlement data of any road surface; obtain the vehicle data passing through any road surface within the preset time period, and the vehicle data includes the vehicle type and the number of vehicles corresponding to each type; obtain the ambient temperature data within the collection time period.
[0052] It should be noted that, based on experience, the preset collection time period is set to 30 days, and the preset collection frequency is set to 1 day, which can be adjusted according to actual conditions and are not specifically limited in this embodiment.
[0053] It should be noted that the Canny algorithm is an existing algorithm for edge detection, and thus it is not described in detail in this embodiment.
[0054] It should be noted that the road surface image is collected by a drone, the crack length data is collected by a strain sensor, the road surface settlement data comes from the surface settlement monitoring technology that monitors the elevation changes of the road surface, the vehicle data is obtained through an intelligent traffic management system, and the ambient temperature data is obtained through a thermometer.
[0055] So far, the relevant data of municipal road cracks are obtained through the above method.
[0056] Step S002: Obtain the degree of any crack according to the length of the crack and the grayscale expression of the pixel point corresponding to the crack; determine the expansion of any crack according to the growth rate of the length of the crack and the directional characteristics of the crack edge.
[0057] Step 2.1, obtaining the cracking degree of any crack according to the length of the crack and the grayscale expression of the pixel point corresponding to the crack.
[0058] It should be noted that when evaluating the extent of cracks, a preliminary determination of the severity of the cracks is a crucial step.
[0059] When determining the extent of pavement cracks mainly from the number of cracks on the pavement surface and the pavement performance, multiple factors need to be considered. First, the length and width of the cracks are key indicators of the severity of the cracks. Long and wide cracks usually mean more serious structural damage and may require emergency repairs. Secondly, the pavement size and the range of crack distribution are also important factors in assessing the extent of cracking. Large-area pavement cracks may affect the stability and safety of vehicle driving, so special attention needs to be paid.
[0060] It should be noted that the grayscale value of the pixels in the road crack area is usually smaller, because the cracks usually reflect less light than the surrounding road surface, resulting in a smaller grayscale value.
[0061] Therefore, the extent of the cracks can be determined by the length of the cracks relative to the road surface and the color of the cracks.
[0062] As an embodiment, the degree of cracking of any crack is obtained as follows:
[0063]
[0064] in, Indicates the degree of cracking of any crack, represents the length of the crack, represents the length of the road surface to which the crack belongs, represents the grayscale mean of all pixels on the crack, Represents the normalization function.
[0065] Step 2.2, determine the expansion of any crack based on the length growth rate of the crack and the directional characteristics of the crack edge.
[0066] It should be noted that some cracks may be caused by temperature changes or vehicle loads, while other cracks may be caused by aging pavement materials or unstable foundations. By carefully observing the morphological characteristics of the cracks, its cause and development trend can be more accurately determined.
[0067] It should be noted that by deeply analyzing historical data, we can understand the speed of crack expansion and possible driving factors, and thus predict the trend of future crack expansion. This analysis involves recording and studying the changes in the length, width and depth of the cracks over time to identify the expansion rate and direction.
[0068] First, the length growth rate of the crack is obtained.
[0069] Specifically, As the origin, a coordinate system is established with the sampling time as the X-axis and the crack length as the Y-axis, and a time-length scatter plot of any crack is drawn; a straight line is fitted to the scattered points in the time-length scatter plot of the crack, and the slope of the fitted straight line is recorded as the length growth rate of the crack.
[0070] The straight line fitting diagram of the time-length scatter plot of any crack is shown in the figure below: Figure 2 shown.
[0071] It should be noted that the method used for the straight line fitting is the least square method, which is an existing straight line fitting method, so it is not described in detail in this embodiment.
[0072] Secondly, obtain the crack direction angle interval-direction angle interval frequency histogram.
[0073] Specifically, taking the horizontal right direction as the standard direction, obtaining the direction angle of any pixel point on the edge of any crack, taking the preset angle as the direction angle interval size, obtaining the number of pixel points in any direction angle interval; dividing the number of pixel points in any direction angle interval by the number of all pixel points to obtain the frequency of the direction angle interval, and drawing the direction angle interval-direction angle interval frequency histogram of the crack;
[0074] The directional angle interval-directional angle interval frequency histogram of any crack is used to describe the directional characteristics of the crack edge.
[0075] The frequency histogram of the direction angle interval-direction angle interval of any crack is as follows: Figure 3 shown.
[0076] It should be noted that the preset angle is set to 30 degrees based on experience and can be adjusted according to actual conditions, and this embodiment does not specifically limit it.
[0077] Finally, the expansion of any crack is determined based on the crack length growth rate and the directional characteristics of the crack edge.
[0078] It should be noted that the expansion characteristics of cracks are mainly reflected in the changes in the cracks. During the sampling period, the faster the length of the crack changes, the more significant the expansion of the crack. In addition, the cracks open in a single direction with obvious direction characteristics, indicating that there is a certain external force and the direction of destruction is consistent, so the expansion of the cracks is more significant.
[0079] As an example, the expansion of any crack The way to obtain is:
[0080]
[0081] in, represents the length growth rate of any crack, represents the maximum direction angle interval frequency on the direction angle interval-direction angle interval frequency histogram of the crack, It represents the mean value of all the directional angle interval frequencies on the directional angle interval-directional angle interval frequency histogram of the crack.
[0082] It should be noted that It represents the difference between the maximum directional angle interval frequency of any crack opening directional angle and the average frequency of all directional angle intervals. The larger the value, the more obvious the direction trend of the crack, and therefore the more obvious the expansion of the crack.
[0083] So far, the cracking degree and expansion of any crack are obtained through the above method.
[0084] Step S003: Process the settlement data to obtain the settlement rate of the road surface, and combine the ambient temperature data, the vehicle data of the road surface, and the settlement rate of the road surface to obtain the strain index of any road surface; comprehensively consider the expansion of the cracks and the strain index of the road surface to which the cracks belong to obtain the comprehensive expansion of any cracks.
[0085] It should be noted that the cracking degree and expansion of any crack obtained in step S002 are all crack information directly reflected by the image obtained by visual monitoring, and the effective information expressed is limited, and it cannot well reflect the crack depth and crack damage characteristics, which leads to certain limitations in the evaluation of the crack deterioration rate. Therefore, this embodiment also combines various external factors, quantifies parameters and integrates them, and then uses them as correction factors for the deterioration rate, so as to reflect the development of cracks with a more complete evaluation system standard and provide a basis for repair decisions.
[0086] It should be noted that the external factors are further corrected by considering the conditions of the road surface where the cracks are located. On the one hand, the frequent passage of vehicles will accelerate the development of cracks, especially heavy vehicles. On the other hand, the deterioration of cracks will accelerate the settlement and deformation of the road surface. At the same time, the influence of ambient temperature is considered. The lower the temperature, the more likely it is that the pavement material will shrink, causing more transverse cracks and intensifying the expansion.
[0087] Step 3.1, the settlement data is processed to obtain the settlement rate of the road surface, and the strain index of any road surface is obtained by combining the ambient temperature data, the vehicle data of the road surface, and the settlement rate of the road surface.
[0088] Firstly, the small baseline subset technique is used to obtain the settlement rate of any road surface.
[0089] It should be noted that the small baseline subset technology is an existing technology that uses small baseline set interferometry to accurately estimate surface deformation, so it will not be described in detail in this embodiment.
[0090] Secondly, the strain index of any road surface is obtained by combining the ambient temperature data, vehicle data on the road surface, and the settlement rate of the road surface.
[0091] It should be noted that lower ambient temperature will cause cracks to intensify, and therefore is inversely proportional to the strain index of the road surface; the greater the proportion of heavy vehicles, the greater the road load pressure, and therefore the greater the strain index of the road surface; at the same time, the greater the settlement rate of the road surface, the faster the road surface deformation, the more significant the trend of crack enlargement, and therefore the greater the strain index of the road surface.
[0092] As an embodiment, the strain index of any road surface is obtained as follows:
[0093]
[0094] in, represents the strain index of any road surface, Indicates the average value of the ambient temperature during the acquisition period. is the total number of heavy vehicles passing through the road during the collection period, is the total number of vehicles passing the road during the collection period, is the settlement rate of the road surface.
[0095] It should be noted that It is the proportion of heavy vehicles passing on the road, indicating the contribution of traffic load to road subsidence and road cracks.
[0096] Step 3.2, comprehensively consider the crack expansion and the strain index of the pavement to which the crack belongs, and obtain the comprehensive expansion of any crack.
[0097] It should be noted that the expansion of the crack is obtained from the characteristics of the crack itself, and the strain index of the road surface to which the crack belongs is obtained from the road environment factors, vehicle factors, and settlement factors. By integrating the various factors included in the strain index into the expansion of the crack itself, the comprehensive expansion of the crack is obtained.
[0098] As an embodiment, a method for obtaining the comprehensive extension of any crack is as follows:
[0099]
[0100] in, The comprehensive extension of any crack, represents the strain index of the pavement to which the crack belongs, is the expansion of the crack.
[0101] So far, the comprehensive extension of any crack is obtained through the above method.
[0102] Step S004: The comprehensive expansion of the cracks and the cracking degree of the cracks are integrated to obtain the comprehensive performance degree of any crack.
[0103] It should be noted that the comprehensive expansion of cracks reflects the speed of crack expansion under various factors, making the future changes of cracks predictable. By combining the comprehensive expansion of cracks with the degree of cracking of the cracks themselves, the overall performance of the cracks can be obtained.
[0104] The greater the degree of cracking, the more serious the crack itself is, and the greater the comprehensive manifestation of the crack; at the same time, the more significant the comprehensive expansion of the crack, the greater the degree of possible change of the crack, the greater the tendency of the crack to crack, and therefore the greater the comprehensive manifestation of the crack.
[0105] As an embodiment, a method for obtaining the comprehensive performance degree of any crack is as follows:
[0106]
[0107] in, Indicates the comprehensive performance of any crack. Indicates the degree of cracking of the crack, represents the comprehensive expansion of the cracks, Represents the normalization function.
[0108] So far, the comprehensive performance degree of any crack is obtained through the above method.
[0109] Step S005: Determine the severity of all cracks according to the comprehensive performance of the cracks and perform corresponding repairs.
[0110] Adding the comprehensive performance levels of all cracks on any road surface to obtain the comprehensive performance of cracks on the road surface;
[0111] It should be noted that the comprehensive performance of the road surface reflects the damage to the road surface and the degree of need for road repair. When the comprehensive performance of the road surface is small, the road surface is still within the range of safe use and only needs to be monitored; when the comprehensive performance of the road surface is large, the road surface has obvious damage that affects vehicle driving, and it is necessary to focus on monitoring and timely maintenance of the road surface according to the relevant arrangements of the repair personnel to avoid greater damage; when the comprehensive performance of the road surface is very large, the road surface can already cause a large impact on driving vehicles, and large vehicles passing through may cause accidents such as road collapse. At this time, the road passage should be closed and road maintenance should be placed at the highest priority of the repair personnel.
[0112] When the comprehensive performance of road cracks is less than or equal to the preset first parameter, the road surface is recorded as a non-dangerous state; when the comprehensive performance of road cracks is greater than the preset first parameter and less than the preset second parameter, the road surface is recorded as a relatively dangerous state and road repair is arranged; when the comprehensive performance of road cracks is greater than or equal to the preset second parameter, the road surface is recorded as a high-dangerous state, and vehicles passing through the road surface need to be stopped and repairs must be carried out immediately.
[0113] It should be noted that, based on experience, the preset first parameter is set to 0.3, and the preset second parameter is set to 0.7, which can be adjusted according to actual conditions and are not specifically limited in this embodiment.
[0114] Through the above steps, the repair and detection of municipal road cracks are completed.
[0115] An embodiment of the present invention provides a municipal road crack repair detection system, which includes a memory, a processor, and a computer program stored in the memory and executable on the processor. When the processor executes the computer program, it implements any one of the steps of the municipal road crack repair detection method.
[0116] This embodiment can more comprehensively reflect the actual condition of cracks and their potential expansion risks by comprehensively considering various external factors that affect the development of cracks. By considering the influence of various external factors and introducing correction factors, the deterioration trend of cracks can be more accurately predicted, providing a scientific basis for the timing and scope of repair work. This method not only improves the efficiency and effectiveness of road maintenance work, but also helps to reasonably allocate maintenance resources, ensure the safety and stability of roads, and thus extend the service life of roads.
[0117] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A municipal road crack repair detection method, characterized in that: The method comprises the following steps: Acquire a number of road surface images within a preset acquisition time period; the road surface images include a number of cracks and corresponding crack edges; acquire settlement data of any road surface, ambient temperature data within a preset time period, and vehicle data passing through any road surface; According to the length of the crack and the grayscale expression of the pixel point corresponding to the crack, the cracking degree of any crack is obtained; according to the length growth rate of the crack and the directional characteristics of the crack edge, the expansion of any crack is determined; The settlement data is processed to obtain the settlement rate of the road surface. The strain index of any road surface is obtained by combining the ambient temperature data, the vehicle data on the road surface, and the settlement rate of the road surface. The comprehensive expansion of any crack is obtained by combining the expansion of the crack and the strain index of the road surface to which the crack belongs. The comprehensive expansion of cracks and the cracking degree of cracks are combined to obtain the comprehensive performance degree of any crack; Determine the severity of all cracks according to their comprehensive performance and carry out corresponding repairs; The method of obtaining the cracking degree of any crack according to the length of the crack and the grayscale expression of the pixel point corresponding to the crack includes: in, Indicates the degree of cracking of any crack, represents the length of the crack, represents the length of the road surface to which the crack belongs, represents the grayscale mean of all pixels on the crack, represents the normalization function; The specific method of determining the expansion of any crack according to the crack length growth rate and the direction characteristics of the crack edge is as follows: Get the length growth rate of the crack; According to the directional characteristics of the crack edge, a directional angle interval-directional angle interval frequency histogram of the crack is obtained; The expansion of any crack is obtained as follows: in, represents the expansion of any crack, represents the length growth rate of the crack, represents the maximum direction angle interval frequency on the direction angle interval-direction angle interval frequency histogram of the crack, represents the mean value of all directional angle interval frequencies on the directional angle interval-directional angle interval frequency histogram of the crack; The specific method for obtaining the length growth rate of the crack is: by As the origin, the sampling time is taken as the X-axis, and the crack length is taken as the Y-axis to establish a coordinate system, and draw a time-length scatter plot of any crack; perform straight line fitting on the scattered points in the time-length scatter plot of the crack, and record the slope of the fitted straight line as the length growth rate of the crack; The specific method for obtaining the directional angle interval-directional angle interval frequency histogram of the crack according to the directional characteristics of the crack edge is: Taking the horizontal right direction as the standard direction, obtaining the direction angle of any pixel point on the edge of any crack, taking the preset angle as the direction angle interval size, obtaining the number of pixel points in any direction angle interval; dividing the number of pixel points in any direction angle interval by the number of all pixel points to obtain the frequency of the direction angle interval, and drawing the direction angle interval-direction angle interval frequency histogram of the crack; The directional angle interval-directional angle interval frequency histogram of any crack is used to describe the directional characteristics of the crack edge.
2. A municipal road crack repair detection method according to claim 1, characterized in that: The settlement data is processed to obtain the settlement rate of the road surface, and the strain index of any road surface is obtained by combining the ambient temperature data, the vehicle data of the road surface, and the settlement rate of the road surface, including the specific method of: The settlement rate of any road surface is obtained by using small baseline subset technique on the settlement data; The strain index of any road surface is obtained as follows: in, represents the strain index of any road surface, Indicates the average value of the ambient temperature during the acquisition period. is the total number of heavy vehicles passing through the road during the collection period, is the total number of vehicles passing the road during the collection period, is the settlement rate of the road surface.
3. A municipal road crack repair detection method according to claim 1, characterized in that: The comprehensive crack expansion and the strain index of the road surface to which the crack belongs are combined to obtain the comprehensive expansion of any crack, including the following specific methods: The comprehensive expansion of any crack is in direct proportion to the expansion of the crack and the strain index of the road surface to which the crack belongs.
4. A municipal road crack repair detection method according to claim 1, characterized in that: The comprehensive expansion of cracks and the cracking degree of cracks are combined to obtain the comprehensive performance degree of any cracks, including the following specific methods: in, Indicates the comprehensive performance of any crack. Indicates the degree of cracking of the crack, represents the comprehensive expansion of the cracks, Represents the normalization function.
5. A municipal road crack repair detection method according to claim 1, characterized in that: The comprehensive performance degree of all cracks on any road surface is comprehensively evaluated to determine the crack conditions of the road surface and to perform corresponding repairs, including the following specific methods: Adding the comprehensive performance levels of all cracks on any road surface to obtain the comprehensive performance of cracks on the road surface; When the comprehensive performance of road cracks is less than or equal to the preset first parameter, the road surface is recorded as a non-dangerous state; when the comprehensive performance of road cracks is greater than the preset first parameter and less than the preset second parameter, the road surface is recorded as a relatively dangerous state and road repair is arranged; when the comprehensive performance of road cracks is greater than or equal to the preset second parameter, the road surface is recorded as a high-dangerous state, and vehicles passing through the road surface need to be stopped and repairs must be carried out immediately.
6. A municipal road crack repair detection system, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the computer program, the steps of a municipal road crack repair detection method as described in any one of claims 1 to 5 are implemented.