Semiconductor device and method for manufacturing semiconductor device
By adopting a conductor stacked structure and optimizing insulator materials in semiconductor devices, the challenges of miniaturization and high integration in the existing technology are solved, and semiconductor device designs with efficient storage capacity and low power consumption are achieved.
Patent Information
- Application Number
- CN202380027107.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-25
- Filing Date
- 2023-03-13
- Publication Date
- 2024-10-29
AI Technical Summary
Existing semiconductor devices have challenges in achieving miniaturization or high integration, increasing operating speed, uniformity of electrical characteristics, reliability, and low power consumption. In particular, there is room for improvement in storage capacity and productivity.
Semiconductor device design including transistors, capacitors and specific insulators is adopted, in which the conductor stacked structure is used to improve integration and productivity, and by optimizing the combination of insulator and conductor materials, the impurity concentration and oxygen vacancies are reduced, and the frequency characteristics and frequency characteristics of the transistor are improved. On-state current.
Miniaturized or highly integrated semiconductor devices are realized, which improves the working speed and uniformity of electrical characteristics, reduces power consumption, and improves storage capacity and productivity.
Smart Images

Figure CN118872402A_ABST
Abstract
Description
Technical Field
[0001] One embodiment of the present invention relates to a semiconductor device, a storage device, and an electronic device. Another embodiment of the present invention relates to a method for manufacturing a semiconductor device.
[0002] Note that one embodiment of the present invention is not limited to the above-mentioned technical field. As an example of the technical field of one embodiment of the present invention, a semiconductor device, a display device, a light-emitting device, a power storage device, a storage device, an electronic device, a lighting device, an input device (such as a touch sensor), an input-output device (such as a touch panel), and a driving method or a manufacturing method of the above-mentioned device can be cited.
[0003] In this specification, etc., semiconductor devices refer to all devices that can work by utilizing semiconductor characteristics. In addition to semiconductor elements such as transistors, semiconductor circuits, computing devices, and storage devices are also a form of semiconductor devices. Display devices (liquid crystal display devices, light-emitting display devices, etc.), projection devices, lighting devices, electro-optical devices, power storage devices, storage devices, semiconductor circuits, camera devices, electronic devices, etc. sometimes include semiconductor devices. Background Art
[0004] In recent years, semiconductor devices such as LSI (Large Scale Integration), CPU (Central Processing Unit), GPU (Graphic Processing Unit), and memory (storage device) have been developed. These semiconductor devices are used in various electronic devices such as computers and portable information terminals. In addition, various storage methods of memory are developed according to the purpose, such as temporary storage during the execution of calculation processing and long-term storage of data. As typical storage methods of memory, for example, DRAM (Dynamic Random Access Memory), SRAM (Static Random Access Memory) and flash memory can be cited.
[0005] In addition, as the amount of data used increases, semiconductor devices having larger storage capacity are required. Patent Document 1 and Non-Patent Document 1 disclose memory cells formed by stacking transistors.
[0006] [Prior technical literature]
[0007] [Patent Document]
[0008] [Patent Document 1] International Patent Application Publication No. 2021 / 053473
[0009] [Non-patent literature]
[0010] [Non-patent document 1] M. Oota et al., “3D-Stacked CAAC-In-Ga-Zn Oxide FETs with Gate Length of 72nm”, IEDM Tech. Dig., 2019, pp. 50-53 Summary of the invention
[0011] Technical problem to be solved by the invention
[0012] One of the purposes of one embodiment of the present invention is to provide a semiconductor device that can achieve miniaturization or high integration. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with a high operating speed. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with good electrical characteristics. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with small unevenness in the electrical characteristics of transistors. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with high reliability. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with a large on-state current. One of the purposes of one embodiment of the present invention is to provide a semiconductor device with low power consumption. One of the purposes of one embodiment of the present invention is to provide a novel semiconductor device. One of the purposes of one embodiment of the present invention is to provide a method for manufacturing a semiconductor device with high productivity. One of the purposes of one embodiment of the present invention is to provide a method for manufacturing a novel semiconductor device.
[0013] One of the purposes of one embodiment of the present invention is to provide a storage device with a large storage capacity. One of the purposes of one embodiment of the present invention is to provide a storage device with a small footprint. One of the purposes of one embodiment of the present invention is to provide a storage device with high reliability. One of the purposes of one embodiment of the present invention is to provide a storage device with low power consumption. One of the purposes of one embodiment of the present invention is to provide a novel storage device. One of the purposes of one embodiment of the present invention is to provide a method for manufacturing a storage device with high productivity. One of the purposes of one embodiment of the present invention is to provide a method for manufacturing a novel storage device.
[0014] Note that the description of these objectives does not prevent the existence of other objectives. One embodiment of the present invention does not need to achieve all of the above objectives. Objectives other than the above objectives can be extracted from the description of the specification, drawings, and claims.
[0015] Solutions to technical problems
[0016] One embodiment of the present invention is a semiconductor device, comprising: a first memory cell; a second memory cell on the first memory cell; a first conductor; and a second conductor on the first conductor, wherein the first memory cell and the second memory cell both comprise a transistor, a capacitor, and a first insulator on the transistor, the transistor comprises a metal oxide, a third conductor on the metal oxide, a fourth conductor and a second insulator, a fifth conductor on the second insulator, a third insulator under the metal oxide, and a sixth conductor under the third insulator, the capacitor comprises a seventh conductor, a fourth insulator on the seventh conductor, and an eighth conductor on the fourth insulator, and the seventh conductor, the fourth insulator, and the eighth conductor are connected to each other. A portion is located on the first insulator, the fourth conductor is in contact with the seventh conductor through an opening set in the first insulator, the first conductor includes a portion in contact with the third conductor included in the first storage unit, the top surface of the first conductor includes a portion in contact with the bottom surface of the second conductor, the second conductor includes a portion in contact with the third conductor included in the second storage unit, the sixth conductor included in the second storage unit contains the same material as the eighth conductor included in the first storage unit, and, in a cross-section of the transistor, one side end portion of the third conductor is roughly aligned with one side end portion of the metal oxide, and one side end portion of the fourth conductor is roughly aligned with another side end portion of the metal oxide.
[0017] In the above semiconductor device, it is preferable that the first conductor is in contact with a part of a top surface and one side end portion of a third conductor included in the first memory cell.
[0018] In the above semiconductor device, preferably, a side end portion of the third insulator is substantially aligned with a side end portion of the metal oxide.
[0019] In the above semiconductor device, preferably, the third conductor and the fourth conductor both include a first layer and a second layer on the first layer, the first layer includes a metal nitride, and the conductivity of the second layer is higher than that of the first layer. In the above semiconductor device, preferably, the first layer includes tantalum nitride, and the second layer includes tungsten.
[0020] In the above semiconductor device, it is preferred that the device further comprises: a fifth insulator in contact with the top surface of the third conductor; and a sixth insulator in contact with the top surface of the fourth conductor, wherein the side end of the sixth insulator is substantially aligned with the side end of the fourth conductor.
[0021] In the above-mentioned semiconductor device, it is preferred that it also includes: a seventh insulator covering the third conductor, the fourth conductor, the metal oxide and the third insulator, wherein the seventh insulator includes a first opening overlapping with the area sandwiched between the third conductor and the fourth conductor, and also includes a second opening overlapping with the opening of the first insulator, the second insulator and at least a portion of the fifth conductor are arranged in the first opening of the seventh insulator, and the seventh conductor, the fourth insulator and at least a portion of the eighth conductor are arranged in the second opening of the seventh insulator.
[0022] In the above semiconductor device, preferably, an eighth insulator is included on the first insulator, a top surface of the eighth insulator is in contact with a portion of the fourth insulator, and the eighth insulator includes an opening overlapping with an opening of the first insulator. In the above semiconductor device, preferably, a thickness of the eighth insulator is greater than or equal to 50 nm and less than or equal to 250 nm. In the above semiconductor device, preferably, the first insulator contains aluminum oxide.
[0023] In the above-mentioned semiconductor device, it is preferred that it also includes: a ninth insulator contacting the bottom surface of the sixth conductor, wherein the ninth insulator included in the second storage unit is in contact with the top surface of the eighth insulator included in the first storage unit, and the ninth insulator included in the second storage unit contains the same material as the fourth insulator included in the first storage unit.
[0024] In the above semiconductor device, preferably, the side end portion of the seventh conductor is covered with a fourth insulator. In the above semiconductor device, preferably, the fourth insulator includes one or both of zirconium oxide and aluminum oxide.
[0025] In the above semiconductor device, preferably, the sixth conductor overlaps with the fifth conductor via a metal oxide.
[0026] In the above semiconductor device, preferably, it further comprises: a tenth insulator in contact with a side surface of the first conductor, wherein at least a portion of the third conductor is exposed from the tenth insulator and in contact with the first conductor. In the above semiconductor device, preferably, the tenth insulator comprises one or both of aluminum oxide and silicon nitride.
[0027] Another embodiment of the present invention is a method for manufacturing a semiconductor device, comprising the following steps: depositing a first insulator, a second insulator, a metal oxide, a second conductor, and a third insulator in sequence on a first conductor; forming an island-shaped second insulator, an island-shaped metal oxide, an island-shaped second conductor, and an island-shaped third insulator by processing the second insulator, the metal oxide, the second conductor, and the third insulator; depositing a fourth insulator in a manner covering the first insulator, the island-shaped second insulator, the island-shaped metal oxide, the island-shaped second conductor, and the island-shaped third insulator; forming a first opening in the fourth insulator, dividing the island-shaped third insulator in a manner overlapping with the first opening to form a fifth insulator and a sixth insulator, and forming the island-shaped second conductor in a manner overlapping with the first opening; A third conductor and a fourth conductor are formed by dividing the body; a seventh insulator and a fifth conductor on the seventh insulator are formed in the first opening; an eighth insulator is deposited on the fourth insulator and the fifth conductor; a second opening reaching the third conductor is formed in the eighth insulator, the fourth insulator and the fifth insulator; a sixth conductor is formed in the second opening; a ninth insulator and a seventh conductor are deposited so as to cover the sixth conductor; and a tenth insulator, an eleventh insulator, an eighth conductor on the tenth insulator and a ninth conductor on the eleventh insulator are formed by processing the ninth insulator and the seventh conductor, the eighth conductor overlaps with the tenth insulator and the sixth conductor, and the ninth conductor overlaps with the metal oxide and the fifth conductor.
[0028] In the above-mentioned method for manufacturing a semiconductor device, preferably, before forming the second opening, a third opening is formed by passing through the eighth insulator, the fourth insulator, the sixth insulator and the first insulator, a tenth conductor is formed in the third opening, and the tenth conductor contacts a portion of the fourth conductor.
[0029] In the above-mentioned method for manufacturing a semiconductor device, it is preferred that before processing the second insulator, the metal oxide, the second conductor and the third insulator, a metal film is deposited on the third insulator, and an organic coating film is deposited on the metal film, and the second insulator, the metal oxide, the second conductor and the third insulator are processed using a capacitively coupled plasma etching device.
[0030] In the above-mentioned method for manufacturing a semiconductor device, preferably, when processing the second conductor, the power of the lower electrode of the processing chamber of the capacitively coupled plasma etching device is 10 W or less. In the above-mentioned method for manufacturing a semiconductor device, preferably, when processing the second conductor, before the organic coating film disappears, an island-shaped second conductor is formed.
[0031] In the above method for manufacturing a semiconductor device, it is preferred that the first conductor overlaps with the metal oxide and the fifth conductor.
[0032] In the above method for manufacturing a semiconductor device, preferably, the first insulator includes hafnium oxide.
[0033] In the above method for manufacturing a semiconductor device, preferably, the second insulator includes silicon oxide.
[0034] In the above method for manufacturing a semiconductor device, preferably, the metal oxide contains indium, gallium, and zinc.
[0035] In the above method for manufacturing a semiconductor device, preferably, the second electric conductor has a stacked-layer structure of a layer containing tantalum nitride and a layer containing tungsten on the layer containing tantalum nitride.
[0036] In the above method for manufacturing a semiconductor device, preferably, the eighth insulator has a thickness of 50 nm to 250 nm.
[0037] In the above method for manufacturing a semiconductor device, preferably, the tenth insulator includes the same material as the eleventh insulator, and the eighth conductor includes the same material as the ninth conductor.
[0038] Effects of the Invention
[0039] According to one embodiment of the present invention, a semiconductor device capable of miniaturization or high integration can be provided. According to one embodiment of the present invention, a semiconductor device with a high operating speed can be provided. According to one embodiment of the present invention, a semiconductor device with good electrical characteristics can be provided. According to one embodiment of the present invention, a semiconductor device with small unevenness in the electrical characteristics of transistors can be provided. According to one embodiment of the present invention, a semiconductor device with high reliability can be provided. According to one embodiment of the present invention, a semiconductor device with large on-state current can be provided. According to one embodiment of the present invention, a semiconductor device with low power consumption can be provided. According to one embodiment of the present invention, a novel semiconductor device can be provided. According to one embodiment of the present invention, a method for manufacturing a semiconductor device with high productivity can be provided. According to one embodiment of the present invention, a method for manufacturing a novel semiconductor device can be provided.
[0040] According to one embodiment of the present invention, a storage device with large storage capacity can be provided. According to one embodiment of the present invention, a storage device with small occupied area can be provided. According to one embodiment of the present invention, a storage device with high reliability can be provided. According to one embodiment of the present invention, a storage device with low power consumption can be provided. According to one embodiment of the present invention, a novel storage device can be provided. According to one embodiment of the present invention, a method for manufacturing a storage device with high productivity can be provided. According to one embodiment of the present invention, a method for manufacturing a novel storage device can be provided.
[0041] Note that the description of these effects does not prevent the existence of other effects. One embodiment of the present invention does not necessarily have all of the above effects. Effects other than the above effects can be extracted from the description of the specification, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] Figure 1 is a cross-sectional view showing an example of a semiconductor device.
[0043] Figure 2A and Figure 2B is a cross-sectional view showing an example of a semiconductor device.
[0044] Figure 3A and Figure 3B is a cross-sectional view showing an example of a semiconductor device.
[0045] Figure 4A and Figure 4B is a cross-sectional view showing an example of a semiconductor device.
[0046] Figure 5 is a cross-sectional view showing an example of a semiconductor device.
[0047] Fig. 6A and Figure 6B is a plan view showing an example of a semiconductor device.
[0048] 7A to 7C A diagram showing an example of a method for manufacturing a semiconductor device.
[0049] FIG. 8A to FIG. 8F A diagram showing an example of a method for manufacturing a semiconductor device.
[0050] 9A to 9C A diagram showing an example of a method for manufacturing a semiconductor device.
[0051] FIG. 10A to FIG. 10C A diagram showing an example of a method for manufacturing a semiconductor device.
[0052] FIG. 11A to FIG. 11C A diagram showing an example of a method for manufacturing a semiconductor device.
[0053] FIG. 12A to FIG. 12C A diagram showing an example of a method for manufacturing a semiconductor device.
[0054] Fig.13A and Fig. 13B A diagram showing an example of a method for manufacturing a semiconductor device.
[0055] Fig.14 A diagram showing an example of a method for manufacturing a semiconductor device.
[0056] Fig.15 is a block diagram showing an example of a storage device.
[0057] Fig.16A and Fig. 16B 1 is a schematic diagram and a circuit diagram showing an example of a storage device.
[0058] Fig.17A and Fig. 17B is a schematic diagram showing an example of a storage device.
[0059] Fig.18 is a circuit diagram showing an example of a storage device.
[0060] Fig.19 is a timing chart showing an operation example of the storage device.
[0061] Fig. 20A and Fig. 20B is a circuit diagram showing an example of a storage device.
[0062] Fig.21A and Fig.21B is a circuit diagram showing an example of a storage device.
[0063] Fig.22A and Fig. 22B is a diagram showing an example of a semiconductor device.
[0064] Fig.23A and Fig. 23B It is a diagram showing an example of an electronic component.
[0065] FIG. 24A to FIG. 24J is a diagram showing an example of an electronic device.
[0066] FIG. 25A to FIG. 25E is a diagram showing an example of an electronic device.
[0067] FIG. 26A to FIG. 26C is a diagram showing an example of an electronic device.
[0068] Fig. 27 is a diagram showing an example of space equipment.
[0069] Fig.28A and Fig.28B is a diagram according to this embodiment.
[0070] Fig.29A and Fig.29B is a cross-sectional SEM image according to this example.
[0071] Fig. 30A and Fig. 30B is a cross-sectional SEM image according to this example. DETAILED DESCRIPTION
[0072] The embodiments are described in detail with reference to the accompanying drawings. However, a person skilled in the art can easily understand that the present invention is not limited to the following description and can be transformed into various forms without departing from the purpose and scope of the present invention. Therefore, the present invention should not be interpreted as being limited to the contents described in the embodiments shown below.
[0073] In addition, in the invention structure described below, the same reference numerals are used in common between different drawings to represent the same parts or parts with the same function, and their repeated descriptions are omitted. In addition, when representing parts with the same function, the same hatching is sometimes used without adding a reference numeral.
[0074] In addition, for ease of understanding, the position, size, and range of each component shown in the drawings may not represent its actual position, size, and range. Therefore, the disclosed invention is not necessarily limited to the position, size, and range disclosed in the drawings.
[0075] Note that in this specification, etc., ordinal numbers such as "first" and "second" are added for convenience, but they do not limit the number of structural elements or the order of structural elements (for example, the order of processes or the order of stacking). In addition, the ordinal numbers added to structural elements in one part of this specification may not be consistent with the ordinal numbers added to the structural elements in other parts of this specification or in the claims.
[0076] In addition, depending on the situation or condition, "film" and "layer" may be interchanged. For example, "conductive layer" may be replaced with "conductive film". Also, for example, "insulating film" may be replaced with "insulating layer". Also, depending on the situation or condition, "conductive body" may be replaced with "conductive layer" or "conductive film". Also, depending on the situation or condition, "insulator" may be replaced with "insulating layer" or "insulating film".
[0077] The opening includes, for example, a groove, a slit, etc. A region where the opening is formed is sometimes referred to as an opening portion.
[0078] In addition, the drawings used in this embodiment mode show the case where the side wall of the insulator in the opening of the insulator is substantially perpendicular to the substrate surface or the formed surface, but the side wall may be tapered.
[0079] Note that in this specification, etc., a tapered shape refers to a shape in which at least a portion of the side surface of a constituent element is inclined relative to a substrate surface or a formed surface. For example, it is preferable to include a region where the angle formed by the inclined side surface and the substrate surface or the formed surface (hereinafter sometimes referred to as a taper angle) is less than 90°. Here, the side surface and the substrate surface of the structure do not necessarily have to be completely flat, and may be a nearly planar shape with a slight curvature or a nearly planar shape with fine concave-convex shapes.
[0080] (Implementation Method 1)
[0081] In this embodiment, refer to Figures 1 to 14 A semiconductor device according to one embodiment of the present invention will be described.
[0082] One embodiment of the present invention is a semiconductor device, comprising: a first memory cell; a second memory cell on the first memory cell; a first conductor; and a second conductor on the first conductor, wherein the first memory cell and the second memory cell both comprise a transistor, a capacitor, and a first insulator on the transistor, the transistor comprises a metal oxide, a third conductor on the metal oxide, a fourth conductor and a second insulator, a fifth conductor on the second insulator, a third insulator under the metal oxide, and a sixth conductor under the third insulator, the capacitor comprises a seventh conductor, a fourth insulator on the seventh conductor, and an eighth conductor on the fourth insulator, and the seventh conductor, the fourth insulator, and the eighth conductor are connected to each other. A portion is located on the first insulator, the fourth conductor is in contact with the seventh conductor through an opening set in the first insulator, the first conductor includes a portion in contact with the third conductor included in the first storage unit, the top surface of the first conductor includes a portion in contact with the bottom surface of the second conductor, the second conductor includes a portion in contact with the third conductor included in the second storage unit, the sixth conductor included in the second storage unit contains the same material as the eighth conductor included in the first storage unit, and, in a cross-section of the transistor, one side end portion of the third conductor is roughly aligned with one side end portion of the metal oxide, and one side end portion of the fourth conductor is roughly aligned with another side end portion of the metal oxide.
[0083] A semiconductor device according to one embodiment of the present invention includes a transistor (OS transistor) containing a metal oxide in a channel formation region. Since the off-state current of the OS transistor is small, the storage content can be maintained for a long time by using it in a storage device. In other words, since a refresh operation is not required or the frequency of the refresh operation is extremely low, the power consumption of the storage device can be substantially reduced. In addition, the frequency characteristics of the OS transistor are high, so the storage device can be read and written at a high speed.
[0084] In addition, the first conductor and the second conductor included in the semiconductor device of one embodiment of the present invention can be used as a part of the write and read bit lines (also simply referred to as bit lines) in the storage device. That is, in the storage device using one embodiment of the present invention, a structure in which the third conductor is in direct contact with the bit line can be adopted. By adopting this structure, there is no need to set up an electrode for connection between the third conductor and the bit line, and the integration of the storage unit can be improved.
[0085] In addition, in a semiconductor device according to one embodiment of the present invention, a plurality of memory cells are stacked, and a stacked structure of a plurality of conductors is applied to a bit line. The first conductor has a portion in contact with the third conductor in the first memory cell, and the second conductor has a portion in contact with the third conductor in the second memory cell. Thus, the top surface of the first conductor has a portion in contact with the bottom surface of the second conductor. In this way, by having a stacked structure of a plurality of conductors as a conductor used as a bit line, the manufacturing yield of the semiconductor device according to one embodiment of the present invention can be improved compared to a case where a single conductor is used for the bit line.
[0086] In a method for manufacturing a semiconductor device according to one embodiment of the present invention, the sixth conductor included in the second memory cell and the eighth conductor included in the first memory cell can be formed in the same layer using the same process. In this case, the sixth conductor included in the second memory cell includes the same material as the eighth conductor included in the first memory cell. By adopting such a structure, the method for manufacturing a semiconductor device according to one embodiment of the present invention can improve productivity compared to a case where the sixth conductor included in the second memory cell and the eighth conductor included in the first memory cell are not formed using the same process.
[0087] In a method for manufacturing a semiconductor device according to one embodiment of the present invention, an island-shaped metal oxide and a conductor on the island-shaped metal oxide (a conductor that becomes a third conductor and a fourth conductor in a subsequent process) can be processed into an island shape in the same process. After this process, one side end of the third conductor is roughly aligned with one side end of the metal oxide, and one side end of the fourth conductor is roughly aligned with the other side end of the metal oxide. By adopting this structure, the method for manufacturing a semiconductor device according to one embodiment of the present invention can improve productivity compared to a case where the island-shaped metal oxide and the conductor on the island-shaped metal oxide are formed in different processes.
[0088] <Cross-sectional Structure Example 1 of Semiconductor Device>
[0089] Reference Figure 1 An example of a cross-sectional structure of a semiconductor device according to one embodiment of the present invention is described through FIG. 4 .
[0090] Note that Figure 1In FIG. 4 , the X direction is parallel to the channel length direction of the transistor, the Y direction is perpendicular to the X direction, and the Z direction is perpendicular to the X direction and the Y direction.
[0091] Figure 1 The semiconductor device shown includes an insulator 210, a conductor 209 embedded in the insulator 210, an insulator 212 on the insulator 210, an insulator 214 on the insulator 212, m (m is an integer greater than or equal to 1) layers (first layer 11_1 to m-th layer 11_m) on the insulator 214, m conductors 240 (conductors 240_1 to 240_m) extending in the Z direction through the m layers and electrically connected to the conductor 209, an insulator 286 on the m-th layer 11_m, and an insulator 287 on the insulator 286. In addition, the structural elements included in the semiconductor device of this embodiment may have either a single-layer structure or a stacked-layer structure.
[0092] The conductor 240 preferably includes a conductor 240a and a conductor 240b. Figure 1 As shown, for example, the conductor 240_1 includes the conductor 240a1 and the conductor 240b1, and the conductor 240_m includes the conductor 240am and the conductor 240bm. Hereinafter, the conductors 240a1 to 240am are sometimes collectively referred to as the conductor 240a. In addition, the conductors 240b1 to 240bm are sometimes collectively referred to as the conductor 240b.
[0093] The conductor 209 is used as a part of a circuit element, such as a switch, a transistor, a capacitor, an inductor, a resistor, or a diode, a wiring, an electrode, or a terminal.
[0094] Figure 1 , the first layer 11_1 at the bottom, the second layer 11_2 on the first layer 11_1, the third layer 11_3 on the second layer 11_2, and the mth layer 11_m at the top are shown. Figure 1 2 shows the conductor 240_1 at the bottom, the conductor 240_2 on the conductor 240_1 , the conductor 240_3 on the conductor 240_2 , and the conductor 240_m at the top, among the m conductors 240 .
[0095] In this embodiment, an example having m layers and m conductors 240 is shown, but the present invention is not limited thereto. For example, the number of conductors 240 may be more than 2 and less than m. Thus, compared with a case where there is only one conductor 240 (including one conductor 240a and one conductor 240b), the yield of the semiconductor device can be improved.
[0096] The semiconductor device of this embodiment can be used as a memory cell (or memory array) of a memory device. Each of the m layers is equivalent to the memory array 20[i] of the memory device described in Embodiment 2. A plurality of memory cells are provided in each of the m layers. The conductor 209 is electrically connected to a driving circuit for driving the memory cell provided below the conductor 209. By increasing the number of stacked layers of the memory array (increasing the value of m), the storage capacity of the memory device can be increased without increasing the occupied area of the memory cell. Therefore, the occupied area per bit is reduced, and a memory device with a small size and a large storage capacity can be realized.
[0097] Since the second layer and above of the m layers have the same structure, the second layer 11_2 is mainly described in this embodiment. In addition, the first layer 11_1 and the second layer 11_2 are mainly described, and the first layer 11_1 and the second layer 11_2 are omitted.
[0098] The first layer 11_1 includes transistors 202a and 202b and capacitors 101a and 101b.
[0099] The second layer 11_2 includes transistors 201a and 201b and capacitors 101a and 101b. Each of the third layer 11_3 to the m-th layer 11_m also includes transistors 201a and 201b and capacitors 101a and 101b.
[0100] like Figure 1 As shown in FIG. 1 , the right side structure and the left side structure of the first layer 11_1 and the second layer 11_2 are symmetrical with the conductor 240 as the boundary. Figure 1 In the embodiment, the transistor 201a is symmetrical with the transistor 201b, the transistor 202a is symmetrical with the transistor 202b, and the capacitor 101a is symmetrical with the capacitor 101b. In this embodiment, the left side structure (transistors 201a, 202a and capacitor 101a) of the first layer 11_1 and the second layer 11_2 is mainly described as an example.
[0101] The transistor 202a in the first layer 11_1 is provided on the insulator 214. A conductor 205 (conductor 205a and conductor 205b) is provided as a gate electrode on the lower side of the transistor 202a. One electrode (lower electrode) of the capacitor 101a is physically and electrically connected to one of the source and the drain of the transistor 202a.
[0102] One electrode (lower electrode) of the capacitor 101a included in the second layer 11_2 is physically and electrically connected to one of the source and drain of the transistor 201a included in the second layer 11_2. A conductor 261 (conductor 261a and conductor 261b) is provided as a gate electrode on the lower side of the transistor 201a. The conductor 261 included in the transistor 201a in the second layer 11_2 is formed in the same layer as the other electrode (upper electrode) of the capacitor 101a included in the first layer 11_1. The conductor 261 of the transistor 201a included in the second layer 11_2 and the other electrode of the capacitor 101a included in the first layer 11_1 can be formed in the same process.
[0103] Similarly, the upper electrode of the capacitor 101 a included in the second layer 11_2 is formed in the same layer as the conductor 261 of the transistor 201 a included in the third layer 11_3 .
[0104] Thus, in the first layer 11_1, the upper electrode of the capacitor is not formed in the same layer as the conductor 205, and in the layers above the second layer 11_2, the conductor 261 is formed in the same layer as the upper electrode of the capacitor 101a in the next layer. The first layer 11_1 and the layers above the second layer 11_2 are different from each other in this respect.
[0105] In addition, the other of the source and the drain of the transistor 202 a in the first layer 11_1 is connected to the conductor 240_1 , and the other of the source and the drain of the transistor 201 a in the second layer 11_2 is connected to the conductor 240_2 .
[0106] Here, after stacking m memory cells, in the case of a stacked structure in which an opening for setting the conductor 240 is provided in an insulator, the opening needs to be made deep, so that sometimes the difficulty of processing becomes high or sometimes the manufacturing yield is reduced. Specifically, sometimes it is difficult to maintain the width of the opening (also referred to as the opening diameter. Figure 1 For example, the width of the upper side (m-th layer side) of the opening tends to be wider, and the width of the lower side (first layer side) of the opening tends to be narrower.
[0107] Here, in the manufacturing method of the semiconductor device of the present embodiment, after forming the transistors 202a and 202b included in the first layer 11_1, an opening for setting the conductor 240_1 is set in the laminated structure of the insulator, and the conductor 240_1 is embedded in the opening. Furthermore, after forming the conductor 240_1, the capacitors 101a and 101b are formed. Then, the transistors 201a and 201b included in the second layer 11_2 are formed, and the opening for setting the conductor 240_2 is set in the laminated structure of the insulator, and the conductor 240_2 is embedded in the opening. Furthermore, after forming the conductor 240_2, the capacitors 101a and 101b are formed. By repeating this process, m layers can be electrically connected to m conductors. By using multiple conductors, the depth of one opening can be shallower, which is easier to process, so the manufacturing yield can be improved.
[0108] Figure 2A Show Figure 1 The enlarged view of the structure of the second layer 11_2 and the left half of its vicinity (the structure shown on the conductor 240_2 and its left side). Figure 2B Show Figure 2A In addition, Figure 3A An enlarged cross-sectional view of the transistor 201a in the channel length direction is shown. Figure 3B FIG. 2 is an enlarged cross-sectional view of the transistor 201a in the channel width direction. Figure 4A and Figure 4B Show Figure 1 An enlarged view of a region where the conductor 240_2 is in contact with the other of the source and the drain of the transistor 201a and its vicinity in the structure shown. Figure 4A is an enlarged cross-sectional view of the transistor 201a in the channel length direction. Figure 4B This is an enlarged cross-sectional view of the transistor 201 a in the channel width direction.
[0109] like Figure 2A As shown, the second layer 11_2 includes a transistor 201a and a capacitor 101a.
[0110] Transistor 201a includes a conductor 261 (conductor 261a and conductor 261b) arranged in a manner embedded in an insulator 284, an insulator 222 on conductor 261, an insulator 224 on insulator 222, an oxide 230 (oxide 230a and oxide 230b) on insulator 224, a conductor 242a (conductor 242a1 and conductor 242a2) and a conductor 242b (conductor 242b1 and conductor 242b2) on oxide 230, an insulator 271a on conductor 242a, an insulator 271b on conductor 242b, an insulator 250 on oxide 230, and a conductor 260 (conductor 260a and conductor 260b) on insulator 250.
[0111] An insulator 275 is provided on the insulators 271a and 271b, and an insulator 280 is provided on the insulator 275. The insulator 250 and the conductor 260 are embedded in openings provided in the insulators 280 and 275. An insulator 282 is provided on the insulator 280 and the conductor 260. Furthermore, an insulator 283 is provided on the insulator 282, and an insulator 285 is provided on the insulator 283. Furthermore, an insulator 284 is provided on the insulator 285.
[0112] The oxide 230 includes a region serving as a channel formation region of the transistor 201 a .
[0113] The conductor 242a includes a region functioning as one of a source electrode and a drain electrode of the transistor 201a. The conductor 242b includes a region functioning as the other of a source electrode and a drain electrode of the transistor 201a.
[0114] like Figure 2A As shown, in the cross section of the transistor 201a, it is preferred that one side end of the conductor 242a is roughly aligned with one side end of the oxide 230, and one side end of the conductor 242b is roughly aligned with the other side end of the oxide 230. Furthermore, the side end of the insulator 224 is preferably roughly aligned with the side end of the oxide 230. In one embodiment of the present invention, the insulator 224, the oxide 230, and the conductors that become the conductors 242a and the conductors 242b in the subsequent process can be processed into an island shape at one time. Thus, a semiconductor device according to one embodiment of the present invention can be manufactured with high productivity. When processed as above, the side ends of the insulator 224, the oxide 230, the conductor 242a, and the conductor 242b are roughly aligned as above.
[0115] The insulator 271a and the insulator 271b are films that protect the conductors 242a and 242b during the above-mentioned island-shaped processing. For example, the insulator 271a and the insulator 271b are used as an etching stop layer when removing the hard mask during the processing of the conductors 242a and 242b. Figure 2A As shown, in the cross section of transistor 201a, it is preferred that the side end of insulator 271a on the insulator 250 side is roughly aligned with the side end of conductor 242a on the insulator 250 side, and both sides of the side end of insulator 271b are roughly aligned with the side end of conductor 242b.
[0116] In the case where the side ends are aligned or roughly aligned in the cross section and the top surface shapes are aligned or roughly aligned, it can be said that at least a portion of the edges of the stacked layers overlap when viewed from above. For example, this includes a case where the lower portion of the side end of the upper layer contacts the upper portion of the side end of the lower layer. In addition, for example, this includes a case where the upper layer and the lower layer are processed by the same or a portion of the same mask pattern. However, there are cases where the edges do not overlap accurately, and sometimes a portion of the upper layer is located on the inner side of the lower layer or a portion of the upper layer is located on the outer side of the lower layer. In this case, it can also be said that "the side ends are roughly aligned" or "the top surface shapes are roughly aligned."
[0117] The conductor 260 includes a region that functions as a first gate electrode (upper gate electrode) of the transistor 201a. The insulator 250 includes a region that functions as a first gate insulator of the transistor 201a. The conductor 261 includes a region that functions as a second gate electrode (lower gate electrode) of the transistor 201a. The insulator 224 and the insulator 222 both include a region that functions as a second gate insulator of the transistor 201a.
[0118] The capacitor 101 a includes a conductor 153 on the conductor 242 b , an insulator 154 on the conductor 153 , and a conductor 160 (a conductor 160 a and a conductor 160 b ) on the insulator 154 .
[0119] At least a portion of each of the conductor 153, the insulator 154, and the conductor 160 is disposed inside the opening provided in the insulator 271b, the insulator 275, the insulator 280, the insulator 282, the insulator 283, and the insulator 285. An end portion of each of the conductor 153, the insulator 154, and the conductor 160 is located at least on the insulator 282, preferably on the insulator 285. The insulator 154 is provided so as to cover the end portion of the conductor 153. Thus, the conductor 153 and the conductor 160 can be electrically insulated.
[0120] The deeper the depth of the openings provided in the insulators 271b, 275, 280, 282, 283, and 285 (that is, the thickness of one or more of the insulators 271b, 275, 280, 282, 283, and 285 is made thicker), the greater the electrostatic capacitance of the capacitor 101a can be. By increasing the electrostatic capacitance of the capacitor 101a per unit area, miniaturization or high integration of the semiconductor device can be achieved.
[0121] The conductor 153 includes a region that serves as one electrode (lower electrode) of the capacitor 101a. The insulator 154 includes a region that serves as a dielectric of the capacitor 101a. The conductor 160 includes a region that serves as the other electrode (upper electrode) of the capacitor 101a. The capacitor 101a forms a MIM (Metal-Insulator-Metal) capacitor.
[0122] Here, the conductor 160 used as the upper electrode of the capacitor 101a of the lower layer (for example, the first layer 11_1) and the conductor 261 used as the second gate electrode of the transistor 201a of the upper layer (for example, the second layer 11_2) are formed in the same layer. In other words, the conductor 160 of the capacitor 101a of the lower layer and the conductor 261 of the transistor 201a of the upper layer are formed in a manner of being embedded in an opening formed in the same insulator 284. The conductor 160 of the capacitor 101a of the lower layer and the conductor 261 of the transistor 201a of the upper layer are formed by processing a conductive film, and have the above-mentioned structure. At this time, the conductor 160 of the capacitor 101a of the lower layer contains the same material as the conductor 261 of the transistor 201a of the upper layer.
[0123] It is preferable to provide the insulator 263 in contact with the bottom surface of the conductor 261. In the above process, the insulator 263 is formed simultaneously with the insulator 154 used as the dielectric film of the capacitor 101a in the lower layer when the conductor 160 of the capacitor 101a in the lower layer and the conductor 261 of the transistor 201a in the upper layer are formed. That is, the insulator 154 of the capacitor 101a in the lower layer (for example, the first layer 11_1) and the insulator 263 of the transistor 201a in the upper layer (for example, the second layer 11_2) are formed in the same layer. In other words, the insulator 154 of the capacitor 101a in the lower layer and the insulator 263 of the transistor 201a in the upper layer are formed in a manner embedded in an opening formed in the same insulator 284. Here, the insulator 154 of the capacitor 101a in the lower layer includes the same material as the insulator 263 of the transistor 201a in the upper layer.
[0124] As described above, by simultaneously forming the conductor 160 and the insulator 154 of the lower capacitor 101a and the conductor 261 and the insulator 263 of the upper transistor 201a, the manufacturing process of the semiconductor device according to this embodiment can be shortened, thereby improving the productivity of the semiconductor device.
[0125] Figure 2A The upper electrode (conductor 160) of the capacitor 101a of the lower layer (for example, the first layer 11_1) and the second gate electrode (conductor 261) of the transistor 201a of the upper layer (for example, the second layer 11_2) are respectively provided, but the present invention is not limited to this. Figure 2B As shown, the conductor 160 may also serve as an upper electrode of the capacitor 101a of the lower layer (eg, the first layer 11_1) and a second gate electrode of the transistor 201a of the upper layer (eg, the second layer 11_2).
[0126] The conductor 242 b provided on the oxide 230 so as to overlap with the oxide 230 is used as a wiring electrically connected to the conductor 153 of the capacitor 101 a .
[0127] The conductor 242a provided on the oxide 230 so as to overlap with the oxide 230 is used as a wiring electrically connected to the conductor 240. For example, Figure 2A In the figure, the top surface and side ends of the conductor 242a are electrically connected to the conductor 240_2 extending in the Z direction.
[0128] Since the conductor 240_2 directly contacts at least one of the top surface and the side end of the conductor 242a, it is not necessary to separately provide an electrode for connection, so the occupied area of the memory array can be reduced. In addition, the integration of the memory cell is improved, and the storage capacity can be increased. In addition, the conductor 240_2 is preferably in contact with a part of the top surface and the side end of the conductor 242a. By the conductor 240_2 contacting multiple surfaces of the conductor 242a, the contact resistance between the conductor 240_2 and the conductor 242a can be reduced.
[0129] like Figure 4A As shown, the conductor 240a2 includes a region having a width W1 and a region having a width W2. The width W1 corresponds to the distance of the opening between the conductor 242a included in the transistor 201a and the conductor 242a included in the transistor 201b. The width W2 corresponds to the uppermost diameter of the opening provided in the insulator 285, for example, the distance between the interface of the insulator 285 and the conductor 240a2 on the transistor 201a side and the interface of the insulator 285 and the conductor 240a2 on the transistor 201b side.
[0130] like Figure 4AAs shown in FIG. 1 , the width W2 is preferably larger than the width W1. In this structure, the conductor 240_2 is in contact with at least a portion of the top surface and a portion of the side end of the conductor 242a. Therefore, the area of the region where the conductor 240_2 is in contact with the conductor 242a can be increased. Note that in this specification, the term " Figure 4A The contact between the conductor 240_2 and the conductor 242a shown in FIG. 1 is referred to as a top-side contact.
[0131] In a state where the conductor 242a of the transistor 201a and the conductor 242b of the transistor 201b are formed into island shapes, an opening from the insulator 285 to the insulator 284 can be formed. Figure 4B As shown, sometimes the opening does not overlap with the conductor 242a in the cross section of the opening in the YZ plane.
[0132] In addition, it is preferable to set the conductor 240 (for example, Figure 4A and Figure 4B The insulator 241 corresponding to the side contact of the conductor 240_2). Figure 4A and Figure 4B As shown, the insulator 241 is preferably provided between the conductor 240_2 and the insulator 284, the insulator 222, the insulator 224, the oxide 230, the insulator 271a, the insulator 275, the insulator 280, the insulator 282, the insulator 283, and the insulator 285. Here, at least a portion of the conductor 242a is exposed from the insulator 241 and is in contact with the conductor 240_2. By adopting such a structure, the insulator 241 can prevent impurities such as hydrogen and oxygen in the conductor 240_2 from diffusing into the oxide 230. As a result, the electrical characteristics and reliability of the transistor 201a can be improved.
[0133] Next, a transistor included in the semiconductor device of this embodiment will be described in detail.
[0134] Note that the following description mainly uses the components of the transistor 201a as an example, but the invention can also be applied to the components of the transistor 202a.
[0135] The oxide 230 preferably includes an oxide 230a on the insulator 224 and an oxide 230b on the oxide 230a. When the oxide 230a is included under the oxide 230b, diffusion of impurities from a structure formed under the oxide 230a to the oxide 230b can be suppressed.
[0136] In this embodiment, an example is shown in which the oxide 230 has a two-layer structure of the oxide 230 a and the oxide 230 b , but the present invention is not limited thereto. For example, the oxide 230 may have a single-layer structure of the oxide 230 b or a stacked-layer structure of three or more layers.
[0137] like Figure 3A As shown, oxide 230b includes region 230bc in transistor 201a, region 230ba and region 230bb provided in a manner sandwiching region 230bc. Here, region 230bc is used as a channel formation region. In addition, region 230ba is used as one of a source region and a drain region, and region 230bb is used as the other of the source region and the drain region. At least a portion of region 230bc overlaps with conductor 260. Region 230ba overlaps with conductor 242a, and region 230bb overlaps with conductor 242b.
[0138] Compared with the regions 230ba and 230bb, the region 230bc has fewer oxygen vacancies and a lower impurity concentration, so the region 230bc is a high resistance region with a low carrier concentration. Therefore, the region 230bc can be said to be an i-type (intrinsic) or substantially i-type region.
[0139] In addition, regions 230ba and 230bb have many oxygen vacancies or high concentrations of impurities such as hydrogen, nitrogen, and metal elements, and are therefore low-resistance regions with high carrier concentrations. That is, regions 230ba and 230bb are n-type regions (low-resistance regions) with high carrier concentrations compared to region 230bc.
[0140] In addition, the carrier concentration of the region 230bc is preferably 1×10 18 cm -3 Below, less than 1×10 17 cm -3 , less than 1×10 16 cm -3 , less than 1×10 15 cm -3 , less than 1×10 14 cm -3 , less than 1×10 13 cm -3 , less than 1×10 12 cm -3 , less than 1×10 11 cm -3 or less than 1×10 10 cm -3 In addition, there is no particular limitation on the lower limit of the carrier concentration in the region 230bc. For example, it can be set to 1×10 -9 cm -3 .
[0141] In the case where the purpose is to reduce the carrier concentration of the oxide 230b, the impurity concentration in the oxide 230b is reduced to reduce the defect state density. In this specification, etc., a state in which the impurity concentration is low and the defect state density is low is referred to as "high-purity intrinsic" or "substantially high-purity intrinsic". In addition, an oxide semiconductor (or metal oxide) with a low carrier concentration is sometimes referred to as a "high-purity intrinsic oxide semiconductor" or "substantially high-purity intrinsic oxide semiconductor (or metal oxide)".
[0142] In order to stabilize the electrical characteristics of the transistor 201a, it is effective to reduce the impurity concentration in the oxide 230b. In order to reduce the impurity concentration in the oxide 230b, it is preferable to also reduce the impurity concentration in the nearby film. Impurities include hydrogen, nitrogen, alkali metals, alkaline earth metals, iron, nickel, silicon, etc. Note that the impurities in the oxide 230b refer to, for example, impurities other than the main component constituting the oxide 230b. For example, an element with a concentration of less than 0.1 atomic % can be said to be an impurity.
[0143] Note that the region 230bc, the region 230ba, and the region 230bb may be formed in the oxide 230b and the oxide 230a, respectively.
[0144] In the oxide 230, it is sometimes difficult to clearly detect the boundaries between the regions. The concentrations of the metal elements and impurity elements such as hydrogen and nitrogen detected in each region do not need to change in stages for each region, but may change gradually in each region. That is, the concentrations of the metal elements and impurity elements such as hydrogen and nitrogen may be lower as they are closer to the region 230bc.
[0145] A metal oxide used as a semiconductor (hereinafter, sometimes referred to as an oxide semiconductor) is preferably used for the oxide 230 (the oxide 230 a and the oxide 230 b ).
[0146] The band gap of the metal oxide used as a semiconductor is preferably 2 eV or more, and more preferably 2.5 eV or more. By using a metal oxide with a wide band gap, the off-state current of the transistor can be reduced.
[0147] As the oxide 230, for example, metal oxides such as indium oxide, gallium oxide, and zinc oxide are preferably used. In addition, as the oxide 230, for example, a metal oxide containing two or three selected from indium, element M, and zinc is preferably used. Here, element M is one or more selected from gallium, aluminum, silicon, boron, yttrium, tin, copper, vanadium, beryllium, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, and magnesium. In particular, element M is preferably one or more selected from aluminum, gallium, yttrium, and tin. Note that a metal oxide containing indium, element M, and zinc is sometimes referred to as In-M-Zn oxide.
[0148] The oxide 230 preferably has a stacked structure of a plurality of oxide layers having different chemical compositions. For example, the atomic number ratio of the element M in the metal oxide used for the oxide 230a relative to the metal element of the main component is preferably greater than the atomic number ratio of the element M in the metal oxide used for the oxide 230b relative to the metal element of the main component. In addition, the atomic number ratio of In to the element M in the metal oxide used for the oxide 230a is preferably greater than the atomic number ratio of In to the element M in the metal oxide used for the oxide 230b. By adopting this structure, it is possible to suppress the diffusion of impurities and oxygen from the structure formed below the oxide 230a to the oxide 230b.
[0149] Preferably, the atomic ratio of In to the element M in the metal oxide used for the oxide 230b is greater than the atomic ratio of In to the element M in the metal oxide used for the oxide 230a. With this structure, the transistor 201a can obtain high on-state current and high frequency characteristics.
[0150] In addition, since oxide 230a and oxide 230b contain a common element as a main component in addition to oxygen, the defect state density at the interface between oxide 230a and oxide 230b can be reduced, thereby reducing the influence of interface scattering on carrier conduction, and transistor 201a can obtain high on-state current and high frequency characteristics.
[0151] Specifically, as the oxide 230a, a metal oxide having a composition of In:M:Zn=1:3:4 [atomic ratio] or a composition close thereto, In:M:Zn=1:3:2 [atomic ratio] or a composition close thereto, or In:M:Zn=1:1:0.5 [atomic ratio] or a composition close thereto can be used. In addition, as the oxide 230b, a metal oxide having a composition of In:M:Zn=1:1:1 [atomic ratio] or a composition close thereto, In:M:Zn=1:1:1.2 [atomic ratio] or a composition close thereto, In:M:Zn=1:1:2 [atomic ratio] or a composition close thereto, or In:M:Zn=4:2:3 [atomic ratio] or a composition close thereto can be used. Note that the nearby composition includes a range of ±30% of the desired atomic ratio. In addition, gallium is preferably used as the element M. In addition, when a single layer of the oxide 230b is provided as the oxide 230, the metal oxide that can be used for the oxide 230a can also be applied as the oxide 230b. In addition, the composition of the metal oxide that can be used for the oxide 230a and the oxide 230b is not limited thereto. For example, the composition of the metal oxide that can be used for the oxide 230a can also be applied to the oxide 230b. Similarly, the composition of the metal oxide that can be used for the oxide 230b can also be applied to the oxide 230a.
[0152] Furthermore, when the metal oxide is deposited by sputtering, the above-mentioned atomic number ratio is not limited to the atomic number ratio of the deposited metal oxide, but may also be the atomic number ratio of the sputtering target used for the deposition of the metal oxide.
[0153] The oxide 230 b preferably has crystallinity. In particular, CAAC-OS (c-axis aligned crystalline oxide semiconductor) is preferably used as the oxide 230 b.
[0154] CAAC-OS has a dense structure with high crystallinity and is a metal oxide with few impurities and defects (e.g., oxygen vacancies). In particular, by heat treating the metal oxide at a temperature at which the metal oxide is not polycrystallized (e.g., above 400°C and below 600°C) after forming the metal oxide, the CAAC-OS can have a dense structure with higher crystallinity. In this way, by further increasing the density of CAAC-OS, the diffusion of impurities or oxygen in the CAAC-OS can be further reduced.
[0155] In addition, it is not easy to observe clear grain boundaries in CAAC-OS, so it is not easy to cause a decrease in electron mobility due to grain boundaries. Therefore, the physical properties of the metal oxide containing CAAC-OS are stable. Therefore, the metal oxide with CAAC-OS has heat resistance and high reliability.
[0156] In addition, by using a crystalline oxide such as CAAC-OS as the oxide 230 b, oxygen extraction from the source electrode or the drain electrode can be suppressed. Therefore, even when heat treatment is performed, oxygen extraction from the oxide 230 b can be reduced, so that the transistor 201 a is also stable to high temperatures (so-called thermal budget) in the manufacturing process.
[0157] In a transistor using an oxide semiconductor, if impurities and oxygen vacancies exist in the region where the oxide semiconductor forms a channel, the electrical characteristics are easily changed, and reliability is sometimes reduced. In addition, hydrogen near the oxygen vacancy forms a defect in which hydrogen enters the oxygen vacancy (hereinafter sometimes referred to as V O H) and may generate electrons that become carriers. Therefore, when oxygen vacancies are included in the region 230bc of the oxide semiconductor that forms the channel, the transistor will have a normally-on characteristic (a characteristic in which a channel exists and current flows in the transistor even when no voltage is applied to the gate electrode). Therefore, in the region 230bc of the oxide semiconductor, it is preferable to minimize impurities, oxygen vacancies, and V O H. In other words, it is preferable that the carrier concentration of the region 230 bc in the oxide semiconductor is reduced and the region 230 bc is converted to i-type (intrinsic) or substantially converted to i-type.
[0158] In contrast, by providing an insulator containing oxygen that is released by heating (hereinafter sometimes referred to as excess oxygen) near the oxide semiconductor and performing heat treatment, oxygen can be supplied from the insulator to the oxide semiconductor to reduce oxygen vacancies and V O H. Note that when too much oxygen is supplied to region 230ba or region 230bb, the on-state current of transistor 201a may decrease or the field effect mobility may decrease. Furthermore, when the amount of oxygen supplied to region 230ba or region 230bb is uneven within the substrate surface, the characteristics of the semiconductor device including the transistor become uneven. In addition, when the oxygen supplied from the insulator to the oxide semiconductor diffuses to the conductor such as the gate electrode, source electrode, and drain electrode, the conductor is sometimes oxidized, which leads to a loss of conductivity, thereby having a negative impact on the electrical characteristics and reliability of the transistor.
[0159] Therefore, in the oxide semiconductor, it is preferred that the carrier concentration of the region 230bc is reduced and the region 230bc is i-type or substantially i-type, while it is preferred that the carrier concentration of the regions 230ba and 230bb is high and the region 230bb is n-type. In other words, it is preferred to reduce the oxygen vacancies and V O H. In addition, it is preferable that the region 230ba and the region 230bb are not supplied with excessive oxygen and the V of the region 230ba and the region 230bb are not excessively reduced. O H content. In addition, it is preferable to have a structure that suppresses a decrease in the conductivity of the conductor 260, the conductor 242a, the conductor 242b, and the like. For example, it is preferable to have a structure that suppresses oxidation of the conductor 260, the conductor 242a, the conductor 242b, and the like. Note that hydrogen in the oxide semiconductor may form V O H, so in order to reduce V O H amount, it is necessary to reduce the hydrogen concentration.
[0160] Here, the semiconductor device in this embodiment has the following structure: the hydrogen concentration in the region 230bc is reduced; the oxidation of the conductors 242a, 242b, and 260 is suppressed; and the reduction of the hydrogen concentration in the regions 230ba and 230bb is suppressed.
[0161] The insulator 250 in contact with the region 230bc of the oxide 230b preferably has a function of capturing and fixing hydrogen. Thus, the hydrogen concentration in the region 230bc of the oxide 230b can be reduced. Therefore, the V O H and region 230bc is i-typed or substantially i-typed.
[0162] Here, if Figure 3AAs shown, the insulator 250 preferably has a stacked structure of an insulator 250a in contact with the oxide 230, an insulator 250b on the insulator 250a, and an insulator 250c on the insulator 250b. In this case, the insulator 250a preferably has a function of capturing and fixing hydrogen.
[0163] As an insulator having the function of capturing and fixing hydrogen, a metal oxide having an amorphous structure can be cited. As the insulator 250a, for example, a metal oxide such as magnesium oxide or an oxide containing one or both of aluminum and hafnium is preferably used. The above-mentioned metal oxide having an amorphous structure sometimes has the following property: the oxygen atom has a dangling bond and hydrogen is captured or fixed by the dangling bond. That is, it can be said that the metal oxide having an amorphous structure has a high ability to capture or fix hydrogen.
[0164] In addition, the insulator 250a preferably uses a high dielectric constant (high-k) material. As an example of a high-k material, there is an oxide containing one or both of aluminum and hafnium. When a high-k material is used as the insulator 250a, the gate potential applied when the transistor is operating can be reduced while maintaining the physical thickness of the gate insulator. In addition, the equivalent oxide thickness (EOT) of the insulator used as the gate insulator can be reduced.
[0165] Therefore, as the insulator 250a, it is preferred to use an oxide containing one or both of aluminum and hafnium, more preferably to use an oxide having an amorphous structure and containing one or both of aluminum and hafnium, and further preferably to use hafnium oxide having an amorphous structure. In this embodiment, hafnium oxide is used as the insulator 250a. In this case, the insulator 250a is an insulator containing at least oxygen and hafnium. In addition, the hafnium oxide has an amorphous structure. In this case, the insulator 250a has an amorphous structure.
[0166] Next, the insulator 250b is preferably an insulator having a thermally stable structure such as silicon oxide or silicon oxynitride. In addition, the insulator 250b may also have a stacked structure. In this case, the insulator 250b may have a stacked structure in which an insulator that can be used for the insulator 250a is provided on the silicon oxide or silicon oxynitride. For example, the insulator 250 may also have a stacked structure including silicon oxide or silicon oxynitride and hafnium oxide on the silicon oxide or silicon oxynitride.
[0167] Note that in this specification, etc., "oxynitride" refers to a material containing more oxygen than nitrogen in its composition, and "nitride oxide" refers to a material containing more nitrogen than oxygen in its composition. For example, "silicon oxynitride" refers to a material containing more oxygen than nitrogen in its composition, and "silicon nitride oxide" refers to a material containing more nitrogen than oxygen in its composition.
[0168] In order to suppress oxidation of the conductors 242a, 242b, and 260, an oxygen blocking insulator is preferably provided near each of the conductors 242a, 242b, and 260. In the semiconductor device described in this embodiment, the insulators are, for example, the insulators 250a, 250c, and 275.
[0169] In addition, in this specification, etc., a blocking insulator refers to an insulator having a barrier property. In this specification, etc., the barrier property refers to a function of suppressing the diffusion of the corresponding substance (it can also be said that the permeability is low). Alternatively, it refers to a function of capturing and fixing the corresponding substance (also called doping).
[0170] Examples of oxygen blocking insulators include oxides containing one or both of aluminum and hafnium, magnesium oxide, gallium oxide, indium gallium zinc oxide, silicon nitride, and silicon oxynitride. In addition, examples of oxides containing one or both of aluminum and hafnium include aluminum oxide, hafnium oxide, an oxide containing aluminum and hafnium (hafnium aluminate), and an oxide containing hafnium and silicon (hafnium silicate). For example, the insulators 250a, 250c, and 275 preferably use a single layer or a stack of the above-mentioned oxygen blocking insulators.
[0171] The insulator 250a preferably has an oxygen barrier property. The insulator 250a is preferably at least less likely to allow oxygen to penetrate than the insulator 280. The insulator 250a has a region in contact with the side surface of the conductor 242a and the side surface of the conductor 242b. When the insulator 250a has an oxygen barrier property, it is possible to suppress the side surfaces of the conductor 242a and the conductor 242b from being oxidized and forming an oxide film on the side surfaces. Therefore, it is possible to suppress a decrease in the on-state current of the transistor 201a or a decrease in the field effect mobility.
[0172] The insulator 250a is provided in contact with the top surface and side surfaces of the oxide 230b, the side surfaces of the oxide 230a, the side surfaces of the insulator 224, and the top surface of the insulator 222. When the insulator 250a has oxygen barrier properties, it is possible to suppress the release of oxygen from the region 230bc of the oxide 230b during heat treatment, etc. Therefore, the formation of oxygen vacancies in the oxides 230a and 230b can be reduced.
[0173] On the other hand, even if the insulator 280 contains excessive oxygen, excessive supply of the oxygen to the oxide 230a and the oxide 230b can be suppressed. Therefore, excessive oxidation of the regions 230ba and 230bb to reduce the on-state current of the transistor 201a or the field effect mobility can be suppressed.
[0174] Since an oxide containing one or both of aluminum and hafnium has an oxygen barrier property, it can be suitably used as the insulator 250 a .
[0175] The insulator 250c preferably has oxygen barrier properties. The insulator 250c is provided between the region 230bc of the oxide 230 and the conductor 260 and between the insulator 280 and the conductor 260. By adopting this structure, it is possible to suppress the diffusion of oxygen in the region 230bc of the oxide 230 into the conductor 260 and the formation of oxygen vacancies in the region 230bc of the oxide 230. In addition, it is possible to suppress the diffusion of oxygen in the oxide 230 and oxygen in the insulator 280 into the conductor 260 and the oxidation of the conductor 260. The insulator 250c is preferably at least less likely to allow oxygen to penetrate than the insulator 280. For example, silicon nitride is preferably used as the insulator 250c. In this case, the insulator 250c is an insulator containing at least nitrogen and silicon.
[0176] In addition, the insulator 250c preferably has a hydrogen barrier property, so that impurities such as hydrogen contained in the conductor 260 can be prevented from diffusing into the oxide 230b.
[0177] Insulator 275 preferably has oxygen barrier properties. Insulator 275 is provided between insulator 280 and conductor 242a and between insulator 280 and conductor 242b. By adopting this structure, it is possible to suppress the diffusion of oxygen contained in insulator 280 into conductor 242a and conductor 242b. Therefore, it is possible to suppress the oxidation of conductor 242a and conductor 242b caused by oxygen contained in insulator 280, thereby increasing resistivity and reducing on-state current. Insulator 275 is preferably at least less likely to allow oxygen to penetrate than insulator 280. For example, silicon nitride is preferably used as insulator 275. At this time, insulator 275 is an insulator containing at least nitrogen and silicon.
[0178] In order to suppress a decrease in the hydrogen concentration in the region 230ba and the region 230bb in the oxide 230, a hydrogen barrier insulator is preferably provided near the region 230ba and the region 230bb. In the semiconductor device described in this embodiment, the hydrogen barrier insulator is, for example, the insulator 275.
[0179] Examples of the hydrogen barrier insulator include oxides such as aluminum oxide, hafnium oxide, and tantalum oxide, and nitrides such as silicon nitride. For example, the insulator 275 preferably has a single-layer structure or a stacked-layer structure of the above hydrogen barrier insulators.
[0180] The insulator 275 preferably has a hydrogen barrier property. When the insulator 275 has a hydrogen barrier property, the insulator 250 can be prevented from capturing and fixing hydrogen in the regions 230ba and 230bb. Therefore, the regions 230ba and 230bb can be converted to n-type.
[0181] By adopting the above structure, region 230bc can be i-type or substantially i-type and region 230ba or region 230bb can be n-type, and a semiconductor device with good electrical characteristics can be provided. By adopting the above structure, even if the semiconductor device is miniaturized or highly integrated, it can have good electrical characteristics. In addition, by miniaturizing transistor 201a, high-frequency characteristics can be improved. Specifically, the cutoff frequency can be increased.
[0182] Insulators 250a to 250c are used as part of the first gate insulator. Insulators 250a to 250c are provided together with conductor 260 in an opening formed in insulator 280 or the like. In order to realize miniaturization of transistor 201a, the thickness of insulators 250a to 250c is preferably thin. The thickness of insulators 250a to 250c is preferably 0.1 nm or more and 10 nm or less, more preferably 0.1 nm or more and 5.0 nm or less, further preferably 0.5 nm or more and 5.0 nm or less, further preferably 1.0 nm or more and less than 5.0 nm, and further preferably 1.0 nm or more and 3.0 nm or less. In addition, at least a portion of insulators 250a to 250c may include an area of the above-mentioned thickness.
[0183] In order to reduce the thickness of the insulator 250a to the insulator 250c as described above, it is preferable to use the atomic layer deposition (ALD) method for deposition. The ALD method includes the thermal ALD method that uses only thermal energy to react the precursor and the reactant, and the PEALD (Plasma Enhanced ALD) method that uses the reactant excited by plasma. In the PEALD method, deposition can be performed at a lower temperature by using plasma, so it is sometimes preferred.
[0184] The ALD method can deposit atoms in layers, and thus has the advantages of being able to deposit extremely thin films, being able to deposit structures with high aspect ratios, being able to deposit with fewer defects such as pinholes, being able to deposit with excellent coverage, and being able to deposit at low temperatures. Therefore, the insulator 250 can be deposited with a small thickness and high coverage on the side surfaces of the openings formed in the insulator 280 and the like and on the side ends of the conductors 242a and 242b and the like.
[0185] The precursor used in the ALD method sometimes contains carbon, etc. Therefore, the film formed by the ALD method sometimes contains more impurities such as carbon than the film formed by other deposition methods. In addition, the quantitative analysis of impurities can be performed by secondary ion mass spectrometry (SIMS: Secondary Ion Mass Spectrometry), X-ray photoelectron spectroscopy (XPS: X-ray Photoelectron Spectroscopy) or Auger electron spectroscopy (AES: Auger Electron Spectroscopy).
[0186] Note that, in the above description, the insulator 250 has a three-layer structure of the insulators 250a to 250c, but the present invention is not limited thereto. The insulator 250 may have a structure including at least one of the insulators 250a to 250c. By forming the insulator 250 with one or two layers of the insulators 250a to 250c, the manufacturing process of the semiconductor device can be simplified, thereby improving productivity.
[0187] In this embodiment, the semiconductor device preferably has a structure for suppressing the mixing of hydrogen into the transistors 201a, 202a, etc. in addition to the above structure. For example, it is preferable to provide an insulator having a function of suppressing the diffusion of hydrogen so as to cover one or both of the upper and lower parts of the transistors 201a, 202a, etc. In the semiconductor device described in this embodiment, the insulator is, for example, the insulator 212, the insulator 214, the insulator 282, the insulator 283, and the insulator 286.
[0188] One or more of the insulator 212, the insulator 214, the insulator 282, the insulator 283, the insulator 286, and the insulator 287 are preferably used as a blocking insulator for inhibiting the diffusion of impurities such as water and hydrogen from the substrate side or above the transistors 201a, 202a, etc. to the transistors 201a, 202a, etc. Therefore, one or more of the insulator 212, the insulator 214, the insulator 282, and the insulator 286 preferably include an insulating material having a function of inhibiting the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules (N2O, NO, NO2, etc.), and copper atoms (not allowing the above impurities to pass through). In addition, it is preferred to include an insulating material having a function of inhibiting the diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.) (not allowing the above oxygen to pass through).
[0189] Insulator 212, insulator 214, insulator 282, insulator 283, insulator 286, and insulator 287 preferably include an insulator having a function of inhibiting the diffusion of impurities such as water and hydrogen and oxygen, for example, aluminum oxide, magnesium oxide, hafnium oxide, gallium oxide, indium gallium zinc oxide, silicon nitride, or silicon oxynitride. For example, as insulator 212, insulator 283, and insulator 287, silicon nitride with higher hydrogen barrier properties is preferably used. In addition, for example, insulator 214, insulator 282, and insulator 286 preferably include aluminum oxide or magnesium oxide with high performance of capturing and fixing hydrogen. Thus, impurities such as water and hydrogen can be inhibited from diffusing from the substrate side to transistors 201a, 202a, etc. through insulator 212 and insulator 214. Alternatively, impurities such as water and hydrogen can be inhibited from diffusing from an interlayer insulating film or the like disposed outside insulator 283 or insulator 287 to transistors 201a, 202a, etc. Alternatively, oxygen contained in the insulator 224 or the like can be suppressed from diffusing to the substrate side. Alternatively, oxygen contained in the insulator 280 or the like can be suppressed from diffusing above the transistors 201a, 202a or the like through the insulator 282 or the like. In this way, it is preferable to adopt a structure in which the upper and lower parts of the transistors 201a, 202a or the like are surrounded by an insulator having a function of suppressing diffusion of impurities such as water and hydrogen and oxygen.
[0190] In the transistors 201a and 201b, the conductor 261 is arranged so as to overlap with the oxide 230 and the conductor 260. Here, the conductor 261 is preferably provided so as to be embedded in an opening formed in the insulator 284. Figure 3B As shown, the conductor 261 is preferably arranged to extend in the channel width direction ( Figure 3B By adopting this structure, the conductor 261 is used as a wiring and is used as a second gate electrode in a plurality of transistors arranged in the Y direction.
[0191] The conductor 261 may have a single-layer structure or a stacked-layer structure. Figure 1 In the embodiment, the conductor 261 includes a conductor 261a and a conductor 261b. The conductor 261a is provided in a manner of contacting the bottom surface and the side wall of the opening. The conductor 261b is provided in a manner of contacting the top surface of the conductor 261a and the side wall of the opening. Here, the height of the top surface of the conductor 261b is substantially the same as the height of the top surface of the insulator 284.
[0192] Here, the conductor 261a preferably includes a conductive material having a function of suppressing the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules (N2O, NO, NO2, etc.), copper atoms, etc. Alternatively, it is preferred to include a conductive material having a function of suppressing the diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.).
[0193] By using a conductive material having a function of reducing the diffusion of hydrogen as the conductor 261a, impurities such as hydrogen contained in the conductor 261b can be prevented from diffusing to the oxide 230 through the insulator 284 and the like. In addition, by using a conductive material having a function of suppressing the diffusion of oxygen as the conductor 261a, it is possible to suppress the conductor 261b from being oxidized and the conductivity from being reduced. As the conductive material having the function of suppressing the diffusion of oxygen, for example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, etc. can be cited. The conductor 261a can have a single-layer structure or a stacked-layer structure of the above-mentioned conductive material. For example, titanium nitride is preferably used for the conductor 261a.
[0194] In addition, the conductor 261b is preferably made of a conductive material containing tungsten, copper, or aluminum as a main component. For example, tungsten is preferably used for the conductor 261b.
[0195] The conductor 261 can be used as a second gate electrode. In this case, the threshold voltage (Vth) of the transistor 201a can be controlled by independently changing the potential applied to the conductor 261 without linking it with the potential applied to the conductor 260. In particular, by applying a negative potential to the conductor 261, the Vth of the transistor 201a can be increased and the off-state current can be reduced. Thus, compared with the case where the negative potential is not applied to the conductor 261, when the negative potential is applied to the conductor 261, the drain current when the potential applied to the conductor 260 is 0V can be reduced.
[0196] In addition, the resistivity of the conductor 261 is designed in consideration of the potential applied to the conductor 261, and the thickness of the conductor 261 is set according to the resistivity. In addition, the thickness of the insulator 284 is substantially the same as that of the conductor 261. Here, it is preferable to reduce the thickness of the conductor 261 and the insulator 284 within the range allowed by the design of the conductor 261. By reducing the thickness of the insulator 284, the absolute amount of impurities such as hydrogen contained in the insulator 284 can be reduced, so that the diffusion of the impurities into the oxide 230 can be suppressed.
[0197] As described above, since conductor 261 is formed in the same layer as conductor 160, conductors 261a and 261b have the same structure as conductors 160a and 160b, respectively. Insulator 263 having the same structure as insulator 154 is provided in contact with the bottom surface of conductor 261.
[0198] In the transistors 202a and 202b, the conductor 205 is arranged so as to overlap with the oxide 230 and the conductor 260. Here, the conductor 205 is preferably provided so as to be embedded in the opening formed in the insulator 216. In addition, a part of the conductor 205 may be embedded in the insulator 214. The conductor 205 includes a conductor 205a and a conductor 205b on the conductor 205a. The conductor 205 may have the same structure as the conductor 261, the conductor 205a may have the same structure as the conductor 261a, and the conductor 205b may have the same structure as the conductor 261b.
[0199] Note that since the upper electrode of the capacitor does not need to be provided in the same layer as the conductor 205, it is not necessary to provide an insulator similar to the insulator 154 in the conductor 205, unlike the conductor 261. Therefore, the bottom surface of the conductor 205 is in contact with the insulator 214. Alternatively, the conductor 205 may be formed by depositing a conductive film so as to fit into an opening provided in the insulator 216 and removing the upper portion of the conductive film. In this case, the conductor 205a is provided so as to be in contact with the bottom surface and side surface of the conductor 205b.
[0200] Insulator 222 and insulator 224 are used as a second gate insulator.
[0201] The insulator 222 preferably has a function of suppressing the diffusion of hydrogen (e.g., at least one of hydrogen atoms and hydrogen molecules). In addition, the insulator 222 preferably has a function of suppressing the diffusion of oxygen (e.g., at least one of oxygen atoms and oxygen molecules). For example, compared with the insulator 224, the insulator 222 preferably has a function of suppressing the diffusion of one or both of hydrogen and oxygen.
[0202] The insulator 222 preferably uses an insulator containing an oxide of one or both of aluminum and hafnium as an insulating material. As the insulator, aluminum oxide, hafnium oxide, an oxide containing aluminum and hafnium (hafnium aluminate), etc. are preferably used. Alternatively, an oxide containing hafnium and zirconium is preferably used, for example, hafnium zirconium oxide is used. When the insulator 222 is formed using such a material, the insulator 222 is used as a layer to suppress the release of oxygen from the oxide 230 to the substrate side and the diffusion of impurities such as hydrogen from the surrounding parts of the transistors 201a and 202a to the oxide 230. Therefore, by providing the insulator 222, it is possible to suppress the diffusion of impurities such as hydrogen to the inner side of the transistors 201a, 202a, etc., and to suppress the generation of oxygen vacancies in the oxide 230. In addition, the conductor 205 and the conductor 160 can be suppressed from reacting with the oxygen contained in the insulator 224 and the oxide 230.
[0203] Alternatively, for example, aluminum oxide, bismuth oxide, germanium oxide, niobium oxide, silicon oxide, titanium oxide, tungsten oxide, yttrium oxide, or zirconium oxide may be added to the above-mentioned insulator. Alternatively, the above-mentioned insulator may be nitrided. In addition, silicon oxide, silicon oxynitride, or silicon nitride may be stacked on the above-mentioned insulator for use as the insulator 222.
[0204] In addition, as an insulator 222, for example, a single-layer structure or a stacked-layer structure of an insulator containing a so-called high-k material such as aluminum oxide, hafnium oxide, tantalum oxide, zirconium oxide, hafnium zirconium oxide, etc. may also be used. When miniaturization and high integration of transistors are performed, problems such as leakage current sometimes occur due to the thin film of the second gate insulator. By using a high-k material as an insulator used as the second gate insulator, the gate potential when the transistor is operating can be reduced while maintaining the physical thickness. In addition, as an insulator 222, a material with a high dielectric constant such as lead zirconate titanate (PZT), strontium titanate (SrTiO3), (Ba, Sr)TiO3 (BST) can sometimes be used.
[0205] As the insulator 224 in contact with the oxide 230 , for example, silicon oxide, silicon oxynitride, or the like is preferably used.
[0206] In addition, the insulator 222 and the insulator 224 may each have a stacked structure of two or more layers. In this case, the stacked structure is not limited to a stacked structure made of the same material, and may be a stacked structure made of different materials.
[0207] As the conductor 242a, the conductor 242b, and the conductor 260, it is preferable to use a conductive material that is not easily oxidized or a conductive material having a function of inhibiting oxygen diffusion. As the conductive material, for example, a conductive material containing nitrogen and a conductive material containing oxygen can be cited. Thus, the conductivity of the conductor 242a, the conductor 242b, and the conductor 260 can be suppressed from decreasing. When a conductive material containing metal and nitrogen is used as the conductor 242a, the conductor 242b, and the conductor 260, the conductor 242a, the conductor 242b, and the conductor 260 are conductors containing at least metal and nitrogen.
[0208] The conductors 242a and 242b may have a single-layer structure or a multi-layer structure. In addition, the conductor 260 may have a single-layer structure or a multi-layer structure.
[0209] Figure 2AThe conductors 242a and 242b are shown as having a two-layer structure. The conductor 242a is a laminated film of the conductor 242a1 and the conductor 242a2 on the conductor 242a1, and the conductor 242b is a laminated film of the conductor 242b1 and the conductor 242b2 on the conductor 242b1. At this time, as the layer in contact with the oxide 230b (conductor 242a1 and conductor 242b1), it is preferable to use a conductive material that is not easily oxidized or a conductive material having a function of inhibiting oxygen diffusion. This can suppress the reduction in the conductivity of the conductors 242a and 242b. In addition, by using a material that easily absorbs (extracts) hydrogen as the layer in contact with the oxide 230b (conductor 242a1 and conductor 242b1), the hydrogen concentration of the oxide 230 can be reduced, so it is preferred.
[0210] As the conductors 242a1 and 242b1, metal nitrides are preferably used, for example, nitrides containing tantalum, nitrides containing titanium, nitrides containing molybdenum, nitrides containing tungsten, nitrides containing tantalum and aluminum, nitrides containing titanium and aluminum, etc. are preferably used. In one embodiment of the present invention, nitrides containing tantalum are particularly preferably used. In addition, for example, ruthenium oxide, ruthenium nitride, oxides containing strontium and ruthenium, oxides containing lanthanum and nickel, etc. can also be used. These materials are conductive materials that are not easily oxidized or materials that maintain conductivity even if they absorb oxygen, so they are preferred.
[0211] Note that hydrogen contained in the oxide 230b or the like may diffuse into the conductor 242a1 or the conductor 242b1. In particular, when a nitride containing tantalum is used as the conductor 242a1 or the conductor 242b1, hydrogen contained in the oxide 230b or the like may easily diffuse into the conductor 242a1 or the conductor 242b1, and the diffused hydrogen may bond with nitrogen contained in the conductor 242a1 or the conductor 242b1. In other words, hydrogen contained in the oxide 230b or the like may be absorbed by the conductor 242a1 or the conductor 242b1.
[0212] The electrical conductivity of the conductor 242a2 and the conductor 242b2 is preferably higher than that of the conductor 242a1 and the conductor 242b1. For example, the thickness of the conductor 242a2 and the conductor 242b2 is preferably greater than that of the conductor 242a1 and the conductor 242b1. As the conductor 242a2 and the conductor 242b2, a conductor that can be used for the conductor 261b described above can be used. By adopting the above structure, the contact resistance between the conductor 242a2 and the conductor 240 and the contact resistance between the conductor 242b2 and the conductor 153 can be reduced. As a result, the operating speed of the semiconductor device according to this embodiment can be improved.
[0213] For example, tantalum nitride or titanium nitride can be used as the conductor 242 a 1 and the conductor 242 b 1 , and tungsten can be used as the conductor 242 a 2 and the conductor 242 b 2 .
[0214] In addition, in order to suppress the decrease in the conductivity of the conductors 242a and 242b, a crystalline oxide such as CAAC-OS is preferably used as the oxide 230b. In particular, it is preferred to use a metal oxide containing indium, zinc, and one or more selected from gallium, aluminum, and tin. When CAAC-OS is used, it is possible to suppress the conductor 242a or the conductor 242b from extracting oxygen from the oxide 230b. In addition, it is possible to suppress the decrease in the conductivity of the conductors 242a and 242b.
[0215] Insulators 271a and 271b are inorganic insulators used as etching stop layers when processing conductors 242a and 242b. Insulator 271a is in contact with the top surface of conductor 242a and the bottom surface of insulator 275, and insulator 271b is in contact with the top surface of conductor 242b and the bottom surface of insulator 275. Insulators 271a and 271b can use one or more of the insulators that can be used for insulators 250a to 250c. For example, insulators 271a and 271b can have a stacked film of a silicon nitride film and a silicon oxide film on the silicon nitride film.
[0216] like Figure 3A and Figure 3B As shown, the conductor 260 is arranged in the opening formed in the insulators forming the insulators 280, the insulator 275, the insulators 271a and the insulator 271b, the conductors forming the conductors 242a and the conductors 242b, the oxide 230, and the insulator 224. In the opening, the conductor 260 is provided so as to cover the side surfaces of the insulator 224, the side surfaces of the oxide 230a, the side surfaces of the oxide 230b, and the top surface of the oxide 230b via the insulator 250. In addition, the top surface of the conductor 260 is arranged so as to be substantially equal in height to the uppermost portion of the insulator 250 and the top surface of the insulator 280.
[0217] In the opening portion provided in the insulator 280 etc. where the conductor 260 and the insulator 250 are arranged, the side wall of the opening portion may be substantially perpendicular to the top surface of the insulator 222, or may have a tapered shape. When the side wall has a tapered shape, the coverage of the insulator 250 etc. provided in the opening portion of the insulator 280 can be improved, thereby reducing defects such as voids.
[0218] The conductor 260 is used as a first gate electrode of the transistor 201a. Figure 3B As shown, the conductor 260 is preferably arranged to extend in the channel width direction ( Figure 3BBy adopting this structure, the conductor 261 is used as a wiring and is used as a first gate electrode in a plurality of transistors arranged in the Y direction.
[0219] In the case of adopting the above structure, if Figure 3B As shown, when the cross section of the channel width of the transistor 201a is viewed, a curved surface may be provided between the side surface of the oxide 230b and the top surface of the oxide 230b. That is, the end of the side surface and the end of the top surface may be curved (hereinafter also referred to as rounded).
[0220] The curvature radius of the curved surface is preferably greater than 0 nm and less than the film thickness of the oxide 230b in the region overlapping with the conductor 242 or less than half the length of the region without the curved surface. Specifically, the curvature radius of the curved surface is greater than 0 nm and less than 20 nm, preferably greater than 1 nm and less than 15 nm, and more preferably greater than 2 nm and less than 10 nm. By adopting the above shape, the coverage of the oxide 230b of the insulator 250 and the conductor 260 can be improved.
[0221] In this specification, etc., a transistor structure in which a channel forming region is surrounded by an electric field of at least a first gate electrode is referred to as a surrounded channel (S-channel) structure. In addition, the S-channel structure disclosed in this specification, etc. is different from a Fin-type structure and a planar structure. On the other hand, the S-channel structure disclosed in this specification, etc. can be regarded as a type of Fin-type structure. In addition, in this specification, etc., a Fin-type structure refers to a structure in which a gate electrode is configured in a manner that surrounds at least two or more surfaces of a channel (specifically, two surfaces, three surfaces, or four surfaces, etc.). By adopting a Fin-type structure and an S-channel structure, resistance to short channel effects can be improved, in other words, a transistor that is not prone to short channel effects can be realized.
[0222] By adopting the above-mentioned S-channel structure as transistor 201a, the channel formation region can be electrically surrounded. The S-channel structure is a structure that electrically surrounds the channel formation region, so it can also be said that the structure is substantially the same as the GAA (Gate All Around: full surround gate) structure or the LGAA (Lateral Gate All Around: lateral full surround gate) structure. By making the transistor 201a have an S-channel structure, a GAA structure, or a LGAA structure, the channel formation region formed at or near the interface between the oxide 230 and the gate insulator can be set in the entire bulk of the oxide 230. Therefore, the current density flowing through the transistor can be increased, so it can be expected that the on-state current of the transistor or the field effect mobility of the transistor can be improved.
[0223] Note that as Figure 3B The transistor 201a shown is a transistor of an S-channel structure, but the semiconductor device of one embodiment of the present invention is not limited thereto. For example, as a structure of a transistor that can be used in one embodiment of the present invention, any one or more selected from a planar structure, a Fin structure, and a GAA structure can also be used.
[0224] In FIG2 , the conductor 260 has a two-layer structure. Here, the conductor 260 preferably includes a conductor 260a and a conductor 260b disposed on the conductor 260a. For example, the conductor 260a is preferably disposed so as to surround the bottom surface and side surfaces of the conductor 260b. At this time, as the conductor 260a, it is preferable to use a conductive material that is not easily oxidized or a conductive material that has a function of inhibiting oxygen diffusion.
[0225] As the conductor 260a, it is preferred to use a conductive material having a function of suppressing the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules, copper atoms, etc. In addition, it is preferred to use a conductive material having a function of suppressing the diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.).
[0226] In addition, when the conductor 260a has a function of suppressing the diffusion of oxygen, it is possible to suppress the decrease in conductivity caused by oxidation of the conductor 260b by oxygen contained in the insulator 280. As a conductive material having a function of suppressing the diffusion of oxygen, for example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, etc. can be used.
[0227] In addition, the conductor 260b preferably uses a conductor with high conductivity. For example, the conductor 260b can use a conductive material with tungsten, copper or aluminum as a main component. In addition, the conductor 260b can have a laminated structure, for example, a laminated structure of titanium or titanium nitride and the above conductive materials.
[0228] In the transistor 201a, the conductor 260 is formed in a self-aligned manner to fill an opening formed in the insulator 280 or the like. By forming the conductor 260 in this manner, the conductor 260 can be reliably arranged in a region between the conductor 242a and the conductor 242b without alignment.
[0229] The insulator 216, the insulator 280, the insulator 285, and the insulator 284 preferably have a lower dielectric constant than the insulator 214. By using a material having a low dielectric constant for the interlayer film, parasitic capacitance generated between wirings can be reduced.
[0230] For example, insulator 216, insulator 280, insulator 285 and insulator 284 preferably include one or more of silicon oxide, silicon oxynitride, silicon oxide added with fluorine, silicon oxide added with carbon, silicon oxide added with carbon and nitrogen, and silicon oxide having pores.
[0231] In particular, silicon oxide and silicon oxynitride are preferred because they have thermal stability. In particular, silicon oxide, silicon oxynitride, silicon oxide having pores and the like are preferred because they easily form a region containing oxygen released by heating.
[0232] In addition, the top surfaces of insulator 216 , insulator 280 , insulator 285 , and insulator 284 may also be planarized.
[0233] The concentration of impurities such as water and hydrogen in the insulator 280 is preferably reduced. For example, an oxide containing silicon, such as silicon oxide or silicon oxynitride, is preferably used as the insulator 280 .
[0234] The conductor 153 and the conductor 160 included in the capacitor 101a can be formed using various conductors that can be used for the conductor 205, the conductor 242, or the conductor 260. It is preferable that both the conductor 153 and the conductor 160 are deposited using a deposition method with good coverage such as the ALD method or the CVD method. For example, titanium nitride or tantalum nitride deposited by the ALD method or the CVD method can be used as the conductor 153.
[0235] The bottom surface of the conductor 153 is in contact with the top surface of the conductor 242b2. Here, by using a conductive material with good conductivity as the conductor 242b2, the contact resistance between the conductor 153 and the conductor 242b can be reduced.
[0236] For example, titanium nitride deposited by ALD or CVD may be used as the conductor 160a, and tungsten deposited by CVD may be used as the conductor 160b. Here, when the adhesion of tungsten to the insulator 154 is sufficiently high, a single layer structure of tungsten deposited by CVD may be used as the conductor 160.
[0237] The insulator 154 in the capacitor 101a preferably uses a high-k material (a material with a relatively high dielectric constant). The insulator 154 is preferably deposited using a deposition method with good coverage such as ALD or CVD.
[0238] As insulators of high dielectric constant (high-k) materials, for example, oxides, oxynitrides, oxynitrides and nitrides containing one or more metal elements selected from aluminum, hafnium, zirconium and gallium can be cited. In addition, the above oxides, oxynitrides, nitride oxides or nitrides can also contain silicon. Insulators composed of the above materials can also be used in a stacked manner.
[0239] For example, examples of insulators of high dielectric constant (high-k) materials include aluminum oxide, hafnium oxide, zirconium oxide, oxides containing aluminum and hafnium, oxynitrides containing aluminum and hafnium, oxides containing silicon and hafnium, oxynitrides containing silicon and hafnium, oxides containing silicon and zirconium, oxynitrides containing silicon and zirconium, oxides containing hafnium and zirconium, and oxynitrides containing hafnium and zirconium. By using such high-k materials, the thickness of the insulator 154 can be increased to a degree that can suppress leakage current, and the electrostatic capacitance of the capacitor 101a can be sufficiently ensured.
[0240] In addition, it is preferred to use an insulator composed of the above-mentioned materials in a stacked manner, and it is preferred to use a stacked structure of a material having a high dielectric constant (high-k) material and a dielectric strength greater than that of the high dielectric constant (high-k) material. For example, as the insulator 154, an insulator stacked in the order of zirconium oxide, aluminum oxide, and zirconium oxide can be used. In addition, for example, an insulator stacked in the order of zirconium oxide, aluminum oxide, zirconium oxide, and aluminum oxide can be used. In addition, for example, an insulating film stacked in the order of hafnium zirconium oxide, aluminum oxide, hafnium zirconium oxide, and aluminum oxide can be used. By using an insulator having a relatively large dielectric strength such as aluminum oxide in a stacked manner, the dielectric strength is increased, and thus the electrostatic destruction of the capacitor 101a can be suppressed.
[0241] The deeper the depth of the openings provided in the insulator 271b, the insulator 275, the insulator 280, the insulator 282, the insulator 283, and the insulator 285 (that is, the thickness of one or more of the insulator 271b, the insulator 275, the insulator 280, the insulator 282, the insulator 283, and the insulator 285 is made thicker), the greater the electrostatic capacitance of the capacitor 101a can be. Here, since the insulator 271b, the insulator 275, the insulator 282, and the insulator 283 are used as blocking insulators, it is preferable to set the thickness according to the blocking property required for the semiconductor device. In addition, since the thickness of the conductor 260 used as the gate electrode is determined according to the thickness of the insulator 280, the thickness of the insulator 280 is preferably set according to the thickness of the conductor 260 required for the semiconductor device.
[0242] Therefore, by adjusting the thickness of the insulator 285, the electrostatic capacitance of the capacitor 101a is preferably set. For example, the thickness of the insulator 285 is set within a range of 50 nm to 250 nm, and the depth of the above-mentioned opening is about 150 nm to 350 nm. By forming the capacitor 101a within the above-mentioned range, the capacitor 101a has sufficient electrostatic capacitance, and in a semiconductor device having a layer of stacked multiple memory cells, the height of one layer can be prevented from being excessively increased. In each of the multiple memory cell layers, the electrostatic capacitance of the capacitors provided in each memory cell can be made different. When adopting this structure, for example, the thickness of the insulator 285 provided in the layer of each memory cell can be made different.
[0243] In the opening portion provided in the insulator 285 or the like where the capacitor 101a is arranged, the side wall of the opening portion may be substantially perpendicular to the top surface of the insulator 222 or may have a tapered shape. The tapered side wall can improve the coverage of the conductor 153 or the like provided in the opening portion of the insulator 285 or the like, thereby reducing defects such as voids.
[0244] The conductor 240 is provided in the opening formed in the insulator 284, the insulator 222, the insulator 275, the insulator 280, the insulator 282, the insulator 283, and the insulator 285. Note that in the opening forming the conductor 240_1, the insulator 212, the insulator 214, and the insulator 216 also have openings formed therein. In addition, the conductor 240 is in contact with the top surface and the side end of the conductor 242a and the top surface of the conductor 240 in the lower layer. In addition, the conductor 240_1 is in contact with the top surface of the conductor 209.
[0245] The conductor 240 is used as a plug or wiring for electrically connecting a circuit element such as a switch, a transistor, a capacitor, an inductor, a resistor, a diode, or the like, a wiring, an electrode, or a terminal to the transistors 201 a and 202 a .
[0246] For example, in the memory device described in Embodiment 2, the conductor 240 is used as a write and read bit line.
[0247] The conductor 240 preferably has a laminated structure of a conductor 240a and a conductor 240b. Figure 4A and Figure 4BAs shown, the conductor 240a2 may have a structure in which the conductor 240a2 is provided in contact with the inner wall of the opening and the conductor 240b2 is provided inside the opening. That is, compared with the conductor 240b2, the conductor 240a2 is arranged near the insulator 222, the insulator 275, the insulator 280, the insulator 282, the insulator 283, the insulator 285, and the insulator 284. In addition, the conductor 240a2 contacts the top surface and the side end of the conductor 242a.
[0248] As the conductor 240a, it is preferable to use a conductive material having a function of inhibiting the penetration of impurities such as water and hydrogen. The conductor 240a may have a single-layer structure or a stacked-layer structure using, for example, one or more of tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, and ruthenium oxide. Thus, impurities such as water and hydrogen can be inhibited from mixing into the oxide 230 through the conductor 240.
[0249] In addition, since the conductor 240 is also used as wiring, it is preferable to use a conductor with high conductivity. For example, a conductive material mainly composed of tungsten, copper, or aluminum can be used for the conductor 240b.
[0250] For example, it is preferable to use titanium nitride as the conductor 240a and to use tungsten as the conductor 240b. In this case, the conductor 240a is a conductor containing titanium and nitrogen, and the conductor 240b is a conductor containing tungsten.
[0251] Furthermore, the conductor 240 may have a single-layer structure or a stacked-layer structure of three or more layers.
[0252] like Figure 2A As shown, it is preferable to provide the insulator 241 in contact with the side surface of the conductor 240. Specifically, the insulator 241 is provided in contact with the inner wall of the opening of the insulator 284, the insulator 222, the insulator 275, the insulator 280, the insulator 282, the insulator 283, the insulator 285, the insulator 216, the insulator 214, and the insulator 212. In addition, the insulator 241 is also formed on the side surface of the insulator 224, the oxide 230, and the conductor 242a formed to protrude in the opening. Here, at least a portion of the conductor 242a is exposed from the insulator 241 and is in contact with the conductor 240. That is, the conductor 240 is provided in a manner embedded in the inside of the above-mentioned opening via the insulator 241.
[0253] like Figure 4AAs shown in FIG. 1 , the uppermost portion of the insulator 241 formed below the conductor 242a is preferably located below the top surface of the conductor 242a. By adopting this structure, the conductor 240 can be in contact with at least a portion of the side end portion of the conductor 242a. In addition, the insulator 241 formed below the conductor 242a preferably includes a region in contact with the side surface of the oxide 230. By adopting this structure, impurities such as water and hydrogen contained in the insulator 280 and the like can be suppressed from mixing into the oxide 230 through the conductor 240.
[0254] As the insulator 241, a blocking insulating film that can be used for the insulator 275 or the like can be used. For example, an insulator such as silicon nitride, aluminum oxide, or silicon oxynitride can be used for the insulator 241. By adopting this structure, it is possible to suppress impurities such as water and hydrogen contained in the insulator 280 or the like from being mixed into the oxide 230 through the conductor 240. In particular, silicon nitride is preferred because it has a high barrier property against hydrogen. In addition, it is possible to suppress the absorption of oxygen contained in the insulator 280 by the conductor 240.
[0255] Figure 2A The insulator 241 is shown as a single-layer structure, but the present invention is not limited thereto. The insulator 241 may also have a stacked structure of two or more layers.
[0256] For example, Figure 4A and Figure 4B The insulator 241 is shown to have a two-layer structure of an insulator 241 a and an insulator 241 b on the insulator 241 a .
[0257] like Figure 4A and Figure 4B As shown, when the insulator 241 has a two-layer stacked structure, the insulator 241a in contact with the inner wall of the opening of the insulator 280 and the insulator 241b inside it preferably uses an oxygen blocking insulating film and a hydrogen blocking insulating film in combination. For example, aluminum oxide deposited by the ALD method can be used as the insulator 241a, and silicon nitride deposited by the PEALD method can be used as the insulator 241b. By adopting this structure, oxidation of the conductor 240 can be suppressed, and mixing of hydrogen from the conductor 240 into the oxide 230 and the like can be reduced.
[0258] The sidewalls of the opening where the conductor 240 and the insulator 241 are arranged may be substantially perpendicular to the top surface of the insulator 222 or may be tapered. The tapered sidewalls improve coverage of the insulator 241 and the like provided in the opening.
[0259] <Cross-sectional Structure Example 2 of Semiconductor Device>
[0260] use Figure 5 An example of a cross-sectional structure of a semiconductor device according to one embodiment of the present invention will be described.
[0261] exist Figure 5 In the semiconductor device shown in the figure, a layer including transistors 202c to 202e and the like (equivalent to the functional layer 50 described in Embodiment 2) is provided on a layer including transistors 310 and the like (equivalent to the driving circuit 21 described in Embodiment 2), and a layer including transistors 202c to 202e and the like is provided thereon. Figure 1 The stacked structure shown is the same as the stacked structure (equivalent to the plurality of memory cells 10 included in the memory array 20 described in Embodiment 2). Figure 5 The structure above the insulator 210 is Figure 1 Again, detailed description is omitted.
[0262] Figure 5 The transistor 310 included in the driving circuit 21 described in Embodiment 2 is shown. The transistor 310 is provided on a substrate 311, and includes a conductor 316 used as a gate, an insulator 315 used as a gate insulator, a semiconductor region 313 including a part of the substrate 311, and a low resistance region 314a and a low resistance region 314b used as a source region or a drain region. The transistor 310 can be a p-channel transistor or an n-channel transistor. As the substrate 311, for example, a single crystal silicon substrate can be used.
[0263] Here, in Figure 5 In the transistor 310 shown, the semiconductor region 313 (a part of the substrate 311) forming the channel has a convex shape. In addition, a conductor 316 is provided in a manner that covers the side and top surfaces of the semiconductor region 313 via an insulator 315. In addition, the conductor 316 can use a material that adjusts the work function. Because the convex portion of the semiconductor substrate is utilized, this transistor 310 is also called a FIN-type transistor. In addition, an insulator having a mask for forming a convex portion in a manner that contacts the upper surface of the convex portion may also be provided. In addition, although a portion of the semiconductor substrate is processed to form a convex portion is shown here, a SOI (Silicon on Insulator) substrate may also be processed to form a semiconductor film having a convex shape.
[0264] Notice, Figure 5 The structure of the transistor 310 shown is just an example and is not limited to the above structure, and an appropriate transistor can be used according to the circuit structure or driving method.
[0265] A wiring layer including an interlayer film, wiring, and plugs may be provided between the structures. In addition, the wiring layer may be provided in a plurality of layers according to the design. In addition, in this specification, wiring and a plug electrically connected to the wiring may also be one component. That is, a part of the conductor may be used as wiring, and a part of the conductor may be used as a plug.
[0266] For example, an insulator 320, an insulator 322, an insulator 324, and an insulator 326 are sequentially stacked as interlayer films on the transistor 310. In addition, a conductor 328 and the like are embedded in the insulator 320 and the insulator 322. In addition, a conductor 330 and the like are embedded in the insulator 324 and the insulator 326. In addition, the conductor 328 and the conductor 330 are used as contact plugs or wirings.
[0267] Furthermore, the insulator used as an interlayer film may also be used as a planarization film to cover the concavo-convex shape thereunder. For example, in order to improve the flatness of the top surface of the insulator 322, planarization may be achieved by a planarization process such as chemical mechanical polishing (CMP).
[0268] also, Figure 5 202c, 202d, and 202e in the functional layer 50 described in Embodiment 2 are shown. The transistors 202c, 202d, and 202e have the same structure as the transistors 202a and 202b in the memory cell 10. The transistors 202c, 202d, and 202e correspond to Fig. 20A The transistors 202c, 202d, and 202e are similar to the transistors 52, 53, and 55 in that their sources and drains are connected in series.
[0269] An insulator 208 is provided over the transistors 202c, 202d, and 202e, and a conductor 207 is provided in an opening formed in the insulator 208. The insulator 208 can be an insulator similar to the insulator 210, and the conductor 207 can be a conductor similar to the conductor 209.
[0270] The bottom surface of the conductor 207 is provided so as to be in contact with the top surface of the conductor 260 of the transistor 202d. In addition, the top surface of the conductor 207 is provided so as to be in contact with the bottom surface of the conductor 209. With such a structure, the conductor 240 corresponding to the wiring BL used as a bit line can be electrically connected to the gate of the transistor 202c corresponding to the transistor 52.
[0271] <Example of Top Surface Structure of Semiconductor Device>
[0272] use Fig. 6A and Figure 6B An example of the top surface structure of a semiconductor device according to one embodiment of the present invention will be described.
[0273] In addition, Fig. 6A and Figure 6BIn the figure, the X direction is parallel to the channel length direction of the transistor shown in the figure, the Y direction is parallel to the channel width direction of the transistor shown in the figure, and the Z direction is perpendicular to the X direction and the Y direction. Fig. 6A and Figure 6B For the sake of simplicity, some components such as insulators are omitted. Fig. 6A and Figure 6B The frame surrounded by the double-dashed line shown represents a memory cell including a transistor and a capacitor.
[0274] Fig. 6A and Figure 6B 1 shows the layout of each layer that can be used for the second layer 11_2 and above, and also shows transistors 201a, 201b and capacitors 101a, 101b, etc. For example, in Fig. 6A When the top surface layout of the second layer 11_2 is shown, Fig. 6A The conductor 160 included in the second layer 11_2 (that is, the upper electrodes of the capacitors 101a and 101b in the second layer 11_2) and the conductor 261 included in the third layer 11_3 (that is, the back gate electrodes of the transistors 201a and 201b in the third layer 11_3) are shown. Figure 6B The conductor 160 included in the first layer 11_1 (that is, the back gate electrodes of the transistors 201a and 201b in the second layer 11_2) and the conductor 261 included in the second layer 11_2 (that is, the back gate electrodes of the transistors 201a and 201b in the second layer 11_2) are shown.
[0275] like Fig. 6A and Figure 6B As shown, the conductor 160, the conductor 260, and the conductor 261 are extended in the Y direction. The conductor 160, the conductor 260, and the conductor 261 are commonly included in the memory cells adjacent to each other in the Y direction, and are respectively used as wiring.
[0276] exist Fig. 6A and Figure 6B In the embodiment, the conductor 240 and the conductor 153 have circular shapes in a plan view, but the present invention is not limited thereto. For example, the conductor 240 may have a substantially circular shape such as an ellipse, a polygonal shape such as a quadrangle, or a shape in which the corners of a polygon such as a quadrangle are curved in a plan view.
[0277] Fig. 6A and Figure 6B Although the structure in which the conductor 160 is independently provided in two adjacent memory cells without the conductor 240 is shown, the present invention is not limited thereto. For example, two adjacent memory cells without the conductor 240 may also include one conductor 160 in common.
[0278] <Materials Constituting Semiconductor Devices>
[0279] The constituent materials that can be used for the semiconductor device are described below. Note that each layer constituting the semiconductor device may have a single-layer structure or a stacked-layer structure.
[0280] <<Substrate>>
[0281] As a substrate for forming a transistor, for example, an insulator substrate, a semiconductor substrate or a conductor substrate can be used. As an insulator substrate, for example, a glass substrate, a quartz substrate, a sapphire substrate, a stabilized zirconia substrate (yttria stabilized zirconia substrate, etc.) and a resin substrate can be cited. In addition, as a semiconductor substrate, for example, a semiconductor substrate made of silicon or germanium, etc., and a compound semiconductor substrate composed of silicon carbide, silicon germanium, gallium arsenide, indium phosphide, zinc oxide or gallium oxide can be cited. In addition, a semiconductor substrate having an insulator region inside the above-mentioned semiconductor substrate can also be cited, such as an SOI (Silicon On Insulator) substrate. As a conductor substrate, a graphite substrate, a metal substrate, an alloy substrate, a conductive resin substrate can be cited. In addition, as a substrate, for example, a substrate containing a metal nitride, a substrate containing a metal oxide, etc. can be cited. In addition, an insulator substrate provided with a conductor or a semiconductor, a semiconductor substrate provided with a conductor or an insulator, a conductor substrate provided with a semiconductor or an insulator, etc. can also be cited. Alternatively, a substrate having one or more elements provided on these substrates can also be used. Examples of the element provided over the substrate include a capacitor, a resistor, a switching element, a light emitting element, and a memory element.
[0282] <<Insulator>>
[0283] Examples of the insulator include oxides, nitrides, oxynitrides, oxynitrides, metal oxides, metal oxynitrides, and metal oxynitrides having insulating properties.
[0284] For example, when miniaturization and high integration of transistors are being carried out, problems such as leakage current may occur due to the thin filming of the gate insulator. By using a high-k material as an insulator used as a gate insulator, it is possible to achieve low voltage when the transistor is operating while maintaining the physical thickness. On the other hand, by using a material with a low relative dielectric constant for an insulator used as an interlayer film, it is possible to reduce the parasitic capacitance generated between wirings. Therefore, it is preferable to select a material according to the function of the insulator.
[0285] Examples of insulators having a relatively high dielectric constant include gallium oxide, hafnium oxide, zirconium oxide, oxides containing aluminum and hafnium, oxynitrides containing aluminum and hafnium, oxides containing silicon and hafnium, oxynitrides containing silicon and hafnium, or nitrides containing silicon and hafnium.
[0286] Examples of insulators having a relatively low dielectric constant include silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide added with fluorine, silicon oxide added with carbon, silicon oxide added with carbon and nitrogen, silicon oxide having pores, and resins.
[0287] In addition, by surrounding a transistor using a metal oxide with an insulator having the function of inhibiting the permeation of impurities such as hydrogen and oxygen, the electrical characteristics of the transistor can be stabilized. As an insulator having the function of inhibiting the permeation of impurities such as hydrogen and oxygen, for example, a single layer or stack of an insulator containing one or more of boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium and tantalum can be used. Specifically, as an insulator having the function of inhibiting the permeation of impurities such as hydrogen and oxygen, for example, metal oxides such as aluminum oxide, magnesium oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide, and tantalum oxide, and metal nitrides such as aluminum nitride, silicon oxynitride, and silicon nitride can be cited.
[0288] In addition, the insulator used as the gate insulator is preferably an insulator having a region containing oxygen that is released by heating. For example, by using a structure in which silicon oxide or silicon oxynitride having a region containing oxygen that is released by heating is in contact with the oxide 230, the oxygen vacancies contained in the oxide 230 can be filled.
[0289] <<Conductor>>
[0290] As the conductor, it is preferred to use a metal element selected from aluminum, chromium, copper, silver, gold, platinum, tantalum, nickel, titanium, molybdenum, tungsten, hafnium, vanadium, niobium, manganese, magnesium, zirconium, beryllium, indium, ruthenium, iridium, strontium and lanthanum, an alloy with the above metal elements as a component, or an alloy combining the above metal elements. As the conductor, for example, tantalum nitride, titanium nitride, tungsten, a nitride containing titanium and aluminum, a nitride containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, an oxide containing strontium and ruthenium, an oxide containing lanthanum and nickel, etc. In addition, tantalum nitride, titanium nitride, a nitride containing titanium and aluminum, a nitride containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, an oxide containing strontium and ruthenium, and an oxide containing lanthanum and nickel are conductive materials that are not easily oxidized or materials that maintain conductivity even when absorbing oxygen, so they are preferred. Alternatively, a semiconductor having high conductivity, such as polycrystalline silicon containing an impurity element such as phosphorus, or silicide such as nickel silicide may be used.
[0291] In the case of using a conductor with a stacked structure, for example, a stacked structure combining a material containing the above-mentioned metal element and a conductive material containing oxygen, a stacked structure combining a material containing the above-mentioned metal element and a conductive material containing nitrogen, or a stacked structure combining a material containing the above-mentioned metal element, a conductive material containing oxygen, and a conductive material containing nitrogen may be used.
[0292] In addition, when an oxide is used in the channel formation region of the transistor, a laminated structure combining a material containing the above-mentioned metal element and a conductive material containing oxygen is preferably used as a conductor used as a gate electrode. In this case, the conductive material containing oxygen is preferably arranged on one side of the channel formation region. By arranging the conductive material containing oxygen on one side of the channel formation region, oxygen separated from the conductive material is easily supplied to the channel formation region.
[0293] In particular, as a conductor used as a gate electrode, it is preferred to use a conductive material containing a metal element contained in a metal oxide in which a channel is formed and oxygen. In addition, a conductive material containing the above-mentioned metal element and nitrogen can also be used. For example, a conductive material containing nitrogen such as titanium nitride and tantalum nitride can be used. In addition, one or more of indium tin oxide, indium oxide containing tungsten oxide, indium zinc oxide containing tungsten oxide, indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc oxide, and indium tin oxide added with silicon can also be used. In addition, indium gallium zinc oxide containing nitrogen can also be used. By using the above-mentioned materials, hydrogen contained in the metal oxide in which a channel is formed can sometimes be captured. Alternatively, hydrogen mixed from an external insulator can sometimes be captured.
[0294] <<Metal Oxides>>
[0295] A metal oxide used as a semiconductor (oxide semiconductor) is preferably used as the oxide 230. Next, a metal oxide that can be used for the oxide 230 according to one embodiment of the present invention will be described.
[0296] The metal oxide preferably contains at least indium or zinc. In particular, it preferably contains indium and zinc. In addition, it preferably contains aluminum, gallium, yttrium, tin, etc. In addition, it may also contain one or more selected from boron, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium, and cobalt.
[0297] Here, the case where the metal oxide is an In-M-Zn oxide containing indium, element M and zinc is considered. Note that element M is aluminum, gallium, yttrium or tin. Other elements that can be applied to element M include boron, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium, cobalt, etc. Note that as element M, multiple of the above elements can sometimes be combined. In particular, element M is preferably selected from one or more of gallium, aluminum, yttrium and tin.
[0298] In particular, as a semiconductor layer of a transistor, it is preferred to use an oxide containing indium (In), gallium (Ga) and zinc (Zn) (also recorded as In-Ga-Zn oxide, IGZO). Alternatively, as a semiconductor layer of a transistor, an oxide containing indium (In), aluminum (Al) and zinc (Zn) (also recorded as IAZO) may be used. Alternatively, as a semiconductor layer, an oxide containing indium (In), aluminum (Al), gallium (Ga) and zinc (Zn) (IAGZO or IGAZO) may be used. Alternatively, as a semiconductor layer, an oxide containing indium (In), gallium (Ga), zinc (Zn) and tin (Sn) (also recorded as In-Ga-Zn-Sn oxide, IGZTO) may be used.
[0299] In addition, in this specification and the like, a metal oxide containing nitrogen may be referred to as a metal oxide (metal oxide). In addition, a metal oxide containing nitrogen may also be referred to as a metal oxynitride (metal oxynitride).
[0300] Hereinafter, In—Ga—Zn oxide will be described as an example of the metal oxide.
[0301] Examples of the crystalline structure of an oxide semiconductor include amorphous (including completely amorphous), CAAC (c-axis-aligned crystalline), NC (nanocrystalline), CAC (cloud-aligned composite), single crystal, and polycrystalline.
[0302] In addition, when focusing on the structure of oxide semiconductors, the classification of oxide semiconductors is sometimes different from the above. For example, oxide semiconductors can be classified into single-crystal oxide semiconductors and non-single-crystal oxide semiconductors other than single-crystal oxide semiconductors. As non-single-crystal oxide semiconductors, for example, the above-mentioned CAAC-OS and nc-OS can be cited. In addition, non-single-crystal oxide semiconductors include polycrystalline oxide semiconductors, a-like OS (amorphous-like oxide semiconductor) and amorphous oxide semiconductors.
[0303] Here, the details of the above-mentioned CAAC-OS, nc-OS and a-like OS are explained.
[0304] [CAAC-OS]
[0305] CAAC-OS is an oxide semiconductor including a plurality of crystalline regions, wherein the c-axis of the plurality of crystalline regions is oriented in a specific direction. In addition, the specific direction refers to the thickness direction of the CAAC-OS film, the normal direction of the formed surface of the CAAC-OS film, or the normal direction of the surface of the CAAC-OS film. In addition, the crystalline region is a region having a periodic atomic arrangement. Note that when the atomic arrangement is regarded as a lattice arrangement, the crystalline region is also a region having a consistent lattice arrangement. Furthermore, CAAC-OS has a region where a plurality of crystalline regions are connected in the ab plane direction, and sometimes the region has distortion. In addition, distortion refers to a portion where the direction of the lattice arrangement changes between a region having a consistent lattice arrangement and other regions having a consistent lattice arrangement in a region where a plurality of crystalline regions are connected. In other words, CAAC-OS refers to an oxide semiconductor having a c-axis orientation and having no obvious orientation in the ab plane direction.
[0306] In addition, each of the above-mentioned multiple crystallization regions is composed of one or more tiny crystals (crystallizations with a maximum diameter less than 10 nm). In the case where a crystallization region is composed of one tiny crystal, the maximum diameter of the crystallization region is less than 10 nm. In addition, in the case where a crystallization region is composed of multiple tiny crystals, the maximum diameter of the crystallization region is sometimes about tens of nm.
[0307] CAAC-OS is an oxide semiconductor with high crystallinity and no clear grain boundaries can be confirmed. Therefore, it can be said that in CAAC-OS, a decrease in electron mobility due to grain boundaries is not likely to occur. In addition, the crystallinity of an oxide semiconductor is sometimes reduced due to the mixing of impurities or the generation of defects, so it can be said that CAAC-OS is an oxide semiconductor with few impurities and defects (oxygen vacancies, etc.). Therefore, the physical properties of the oxide semiconductor including CAAC-OS are stable. Therefore, the oxide semiconductor including CAAC-OS has high heat resistance and high reliability. In addition, CAAC-OS is also stable to high temperatures (so-called thermal budget) in the manufacturing process. Therefore, by using CAAC-OS in OS transistors, the degree of freedom of the manufacturing process can be expanded.
[0308] [nc-OS]
[0309] In nc-OS, the atomic arrangement in a tiny region (e.g., a region of more than 1 nm and less than 10 nm, especially a region of more than 1 nm and less than 3 nm) is periodic. In other words, nc-OS has tiny crystals. In addition, for example, the size of the tiny crystal is more than 1 nm and less than 10 nm, especially more than 1 nm and less than 3 nm, and the tiny crystal is called a nanocrystal. In addition, in nc-OS, no regularity of crystal orientation is observed between different nanocrystals. Therefore, no orientation is observed in the entire film. Therefore, sometimes nc-OS is no different from a-like OS or amorphous oxide semiconductor in certain analysis methods.
[0310] [a-like OS]
[0311] A-like OS is an oxide semiconductor having a structure between nc-OS and amorphous oxide semiconductor. A-like OS contains voids or low-density regions. In other words, the crystallinity of a-like OS is lower than that of nc-OS and CAAC-OS. In addition, the hydrogen concentration in the film of a-like OS is higher than that in the film of nc-OS and CAAC-OS.
[0312] Next, the details of the above-mentioned CAC-OS will be described. In addition, CAC-OS is related to the material composition.
[0313] [CAC-OS]
[0314] CAC-OS refers to, for example, a structure in which elements contained in a metal oxide are unevenly distributed, wherein the size of the material containing the unevenly distributed elements is greater than or equal to 0.5 nm and less than or equal to 10 nm, preferably greater than or equal to 1 nm and less than or equal to 3 nm, or a similar size. Note that in the following, a state in which one or more metal elements are unevenly distributed in a metal oxide and regions containing the metal elements are mixed is also referred to as a mosaic or patch shape, and the size of the region is greater than or equal to 0.5 nm and less than or equal to 10 nm, preferably greater than or equal to 1 nm and less than or equal to 3 nm, or a similar size.
[0315] Furthermore, CAC-OS refers to a composite metal oxide having a structure in which the material is divided into a first region and a second region to form a mosaic shape and the first region is distributed in the film (hereinafter also referred to as a cloud shape). That is, CAC-OS refers to a composite metal oxide having a structure in which the first region and the second region are mixed.
[0316] In addition, CAC-OS in In-Ga-Zn oxide refers to a structure in which a region (first region) in which a part of the main component is In and a region (second region) in which a part of the main component is Ga exist irregularly in a mosaic shape in a material composition containing In, Ga, Zn, and O. Therefore, it can be inferred that CAC-OS has a structure in which metal elements are unevenly distributed.
[0317] CAC-OS can be formed, for example, by sputtering without heating the substrate. When CAC-OS is formed by sputtering, as the deposition gas, any one or more selected from an inert gas (typically argon), an oxygen gas, and a nitrogen gas can be used. In addition, the lower the flow rate ratio of the oxygen gas in the total flow rate of the deposition gas during deposition, the better. For example, the flow rate ratio of the oxygen gas in the total flow rate of the deposition gas during deposition is made greater than 0% and less than 30%, preferably greater than 0% and less than 10%.
[0318] Here, the first region is a region having higher conductivity than the second region. That is, when carriers flow through the first region, the conductivity as a metal oxide is exhibited. Therefore, when the first region is distributed in the metal oxide in a cloud-like manner, a high field effect mobility (μ) can be achieved.
[0319] On the other hand, the second region is a region having higher insulation than the first region. That is, when the second region is distributed in the metal oxide, leakage current can be suppressed.
[0320] Thus, when CAC-OS is used for a transistor, the complementary effect of the conductivity of the first region and the insulation of the second region can give CAC-OS a switch function (a function of controlling on / off). In other words, a portion of the CAC-OS material has a conductive function and another portion has an insulating function, and the entire material has a semiconductor function. By separating the conductive function and the insulating function, each function can be maximized. Therefore, by using CAC-OS for a transistor, a large on-state current (I on ), high field effect mobility (μ) and good switching performance.
[0321] In addition, transistors using CAC-OS have high reliability. Therefore, CAC-OS is most suitable for various semiconductor devices such as display devices.
[0322] Oxide semiconductors have various structures and various characteristics. The oxide semiconductor of one embodiment of the present invention may include two or more of an amorphous oxide semiconductor, a polycrystalline oxide semiconductor, a-like OS, CAC-OS, nc-OS, and CAAC-OS.
[0323] <<Other semiconductor materials>>
[0324] A semiconductor material having a band gap (a semiconductor material that is not a zero-band gap semiconductor) may be used as a semiconductor layer of a transistor. For example, a semiconductor of a single element such as silicon or a compound semiconductor such as gallium arsenide may be used.
[0325] In addition, as the semiconductor layer of the transistor, for example, a transition metal chalcogenide used as a semiconductor is preferably used. As transition metal chalcogenides that can be used as the semiconductor layer of the transistor, specifically molybdenum sulfide (typically MoS2), molybdenum selenide (typically MoSe2), molybdenum telluride (typically MoTe2), tungsten sulfide (typically WS2), tungsten selenide (typically WSe2), tungsten telluride (typically WTe2), hafnium sulfide (typically HfS2), hafnium selenide (typically HfSe2), zirconium sulfide (typically ZrS2), zirconium selenide (typically ZrSe2), etc. can be cited. By using the above-mentioned transition metal chalcogenides for the semiconductor layer of the transistor, a semiconductor device with a large on-state current can be provided.
[0326] <Example of Method for Manufacturing Semiconductor Device>
[0327] Use Figure 7 to Fig.14 An example of a method for manufacturing a semiconductor device according to one embodiment of the present invention is described. Figure 1 The case of the semiconductor device shown in FIG. 1 is described as an example.
[0328] Hereinafter, insulating materials for forming insulators, conductive materials for forming conductors, or semiconductor materials for forming semiconductors may be appropriately deposited using sputtering, chemical vapor deposition (CVD), molecular beam epitaxy (MBE), pulsed laser deposition (PLD), ALD, or the like.
[0329] As the sputtering method, there can be cited an RF sputtering method using a high frequency power supply as a sputtering power supply, a DC sputtering method using a direct current power supply, and a pulsed DC sputtering method in which the voltage applied to the electrode is changed in a pulsed manner. The RF sputtering method is mainly used when depositing insulating films, and the DC sputtering method is mainly used when depositing metal conductive films. In addition, the pulsed DC sputtering method is mainly used when depositing compounds such as oxides, nitrides, and carbides using a reactive sputtering method.
[0330] Note that the CVD method can be divided into a plasma enhanced CVD (PECVD) method using plasma, a thermal CVD (TCVD: Thermal CVD) method using heat, and a photo CVD (Photo CVD) method using light, etc. Furthermore, it can be classified into a metal CVD (MCVD: Metal CVD) method and an organic metal CVD (MOCVD: Metal Organic CVD) method according to the source gas used.
[0331] By utilizing the plasma CVD method, a high-quality film can be obtained at a lower temperature. In addition, since plasma is not used in the thermal CVD method, the plasma damage caused to the object to be processed can be reduced. For example, the wiring, electrodes, components (transistors, capacitors, etc.) included in the semiconductor device sometimes generate charge accumulation due to receiving charges from the plasma. At this time, the wiring, electrodes, components, etc. included in the semiconductor device are sometimes damaged due to the accumulated charges. On the other hand, since the above-mentioned plasma damage does not occur in the case of the thermal CVD method without using plasma, the yield of the semiconductor device can be improved. In addition, in the thermal CVD method, plasma damage during deposition is not generated, so a film with fewer defects can be obtained.
[0332] As the ALD method, a thermal ALD method in which a precursor and a reactant are reacted using only thermal energy, a PEALD method using a reactant excited by plasma, or the like is used.
[0333] The CVD method and the ALD method are different from the sputtering method in which particles released from a target material or the like are deposited. Therefore, the CVD method and the ALD method are deposition methods that are not easily affected by the shape of the object to be processed and have good step coverage. In particular, the ALD method has good step coverage and thickness uniformity, so the ALD method is suitable for forming a film covering the surface of an opening with a high aspect ratio. However, the deposition rate of the ALD method is relatively slow, so it is sometimes preferred to use it in combination with other deposition methods such as the CVD method with a fast deposition rate.
[0334] In addition, when the CVD method is used, a film of any composition can be deposited by adjusting the flow ratio of the source gas. For example, when the CVD method is used, a film whose composition continuously changes can be deposited by changing the flow ratio of the source gas while depositing. When depositing while changing the flow ratio of the source gas, since the time required for conveying or adjusting the pressure is not required, the deposition time can be shortened compared to the case where deposition is performed using multiple deposition chambers. Therefore, the productivity of the semiconductor device can sometimes be improved.
[0335] When the ALD method is used, a film of any composition can be deposited by introducing different precursors at the same time. Alternatively, when introducing different precursors, a film of any composition can be deposited by controlling the number of cycles of each precursor.
[0336] First, a substrate (not shown) is prepared, and an insulator 210 and a conductor 209 are formed on the substrate. Next, an insulator 212 is deposited on the insulator 210 and the conductor 209, and an insulator 214 is deposited on the insulator 212. Fig. 7A ).
[0337] The insulator 212 and the insulator 214 are each preferably deposited using a sputtering method. By using a sputtering method that does not require the use of molecules containing hydrogen as a deposition gas, the hydrogen concentration in the insulator 212 or the insulator 214 can be reduced. Note that the deposition method of the insulator 212 and the insulator 214 is not limited to the sputtering method, and a CVD method, an MBE method, a PLD method, an ALD method, or the like may be used.
[0338] The insulator 212 and the insulator 214 are preferably deposited continuously without being exposed to the atmosphere. For example, a multi-chamber deposition apparatus is preferably used. Thus, the insulator 212 and the insulator 214 can be deposited while reducing hydrogen in the film, and the mixing of hydrogen into the film between each deposition step can be reduced.
[0339] In this embodiment, silicon nitride is deposited by pulsed DC sputtering using a silicon target as an insulator 212 in a nitrogen-containing gas atmosphere. By using a pulsed DC sputtering method, particles generated by arcing on the target surface can be suppressed, so the thickness can be made more uniform. In addition, by using a pulse voltage, the rise or fall during discharge can be made sharper than that of a high-frequency voltage. As a result, power can be supplied to the electrode more efficiently to improve the sputtering rate and film quality.
[0340] By using an insulator such as silicon nitride that does not easily allow impurities such as water and hydrogen to pass through, it is possible to suppress the diffusion of impurities such as water and hydrogen contained in the layer below the insulator 212. In addition, by using an insulator such as silicon nitride that does not easily allow copper to pass through as the insulator 212, even if a metal such as copper that easily diffuses is used as the conductor of the layer below the insulator 212 (not shown), it is possible to suppress the metal from diffusing upward through the insulator 212.
[0341] In this embodiment, aluminum oxide is deposited as the insulator 214 by a pulsed DC sputtering method using an aluminum target in an oxygen-containing gas atmosphere. By using a pulsed DC sputtering method, the thickness can be made more uniform, thereby improving the sputtering rate and film quality. Here, RF (Radio Frequency) power can also be applied to the substrate. The amount of oxygen injected into the lower layer of the insulator 214 can be controlled according to the magnitude of the RF power applied to the substrate. As the RF power, for example, 0 W / cm 2 Above and 1.86W / cm 2 Below. In other words, the amount of oxygen can be changed to an amount suitable for the characteristics of the transistor by using the RF power when forming the insulator 214. Therefore, an amount of oxygen suitable for improving the reliability of the transistor can be injected. In addition, the frequency of RF is preferably above 10 MHz. Typically, it is 13.56 MHz. The higher the frequency of RF, the less damage to the substrate can be caused.
[0342] As the insulator 214, it is preferable to use a metal oxide having an amorphous structure, such as aluminum oxide, which has a high ability to capture and fix hydrogen. Thus, hydrogen contained in the insulator 216 or the like can be captured or fixed to prevent the hydrogen from diffusing to the oxide 230. In particular, it is particularly preferable to use aluminum oxide having an amorphous structure or aluminum oxide having an amorphous structure as the insulator 214, because hydrogen can be captured or fixed more effectively in some cases. Thus, a transistor and a semiconductor device with good characteristics and high reliability can be manufactured.
[0343] Next, a conductive film that becomes the conductor 205a is deposited on the insulator 214. The conductive film that becomes the conductor 205a preferably includes a conductor that has a function of inhibiting the transmission of oxygen. For example, the conductive film preferably uses one or more of tantalum nitride, tungsten nitride, and titanium nitride. In addition, the conductive film can use a laminated film of a conductor that has a function of inhibiting the transmission of oxygen and tantalum, tungsten, titanium, molybdenum, aluminum, copper, or a molybdenum-tungsten alloy. The conductive film that becomes the conductor 205a can be deposited, for example, by sputtering, CVD, MBE, PLD, ALD, or the like.
[0344] Next, a conductive film that becomes the conductor 205b is deposited on the conductive film that becomes the conductor 205a. The conductive film that becomes the conductor 205b preferably contains, for example, one or more of tantalum, tungsten, titanium, molybdenum, aluminum, copper, and a molybdenum-tungsten alloy. The conductive film can be deposited, for example, by plating, sputtering, CVD, MBE, PLD, or ALD. In this embodiment, tungsten is deposited as the conductive film that becomes the conductor 205b.
[0345] Next, the conductive film to be the conductive body 205a and the conductive film to be the conductive body 205b are processed by photolithography to form the conductive body 205 ( Fig. 7AThe conductor 205 can be formed by dry etching or wet etching. Since dry etching is suitable for micro-fabrication, dry etching is preferably used.
[0346] Next, an insulating film to be the insulator 216 is deposited to cover the conductor 205. The insulating film to be the insulator 216 is preferably deposited by a sputtering method. By using a sputtering method that does not require the use of molecules containing hydrogen for a deposition gas, the hydrogen concentration in the insulator 216 can be reduced. Note that the deposition method of the insulator 216 is not limited to the sputtering method, and for example, a CVD method, an MBE method, a PLD method, or an ALD method may also be used.
[0347] In this embodiment, silicon oxide is deposited by pulse DC sputtering using a silicon target in an atmosphere containing oxygen as the insulator 216. By using the pulse DC sputtering method, the film thickness distribution can be made more uniform, thereby improving the sputtering rate and film quality.
[0348] Next, a CMP process is performed to remove a portion of the insulating film that will become the insulator 216, thereby exposing the conductor 205. As a result, the insulator 216 remains in contact with the side surface of the conductor 205 ( Fig. 7A ).
[0349] In the above description, the method of first forming the conductor 205 and then forming the insulator 216 is shown, but the present invention is not limited thereto. For example, the insulator 216 having an opening may be first manufactured and then the conductor 205 may be formed so as to fit into the opening.
[0350] Next, an insulator 222 is deposited on the insulator 216 and the conductor 205 ( Figure 7B ).
[0351] As the insulator 222, an insulator containing an oxide of one or both of aluminum and hafnium is preferably deposited. As the insulator containing an oxide of one or both of aluminum and hafnium, for example, aluminum oxide, hafnium oxide, an oxide containing aluminum and hafnium (hafnium aluminate), etc. are preferably used. Alternatively, hafnium zirconium oxide is preferably used. The insulator containing an oxide of one or both of aluminum and hafnium has a barrier property to oxygen, hydrogen, and water. When the insulator 222 has a barrier property to hydrogen and water, the hydrogen and water contained in the structure surrounding the transistor can be suppressed from diffusing into the inside of the transistor through the insulator 222, thereby suppressing the generation of oxygen vacancies in the oxide 230.
[0352] Alternatively, the insulator 222 may be a stacked film of an insulator including an oxide of one or both of aluminum and hafnium, and silicon oxide, silicon oxynitride, silicon nitride, or silicon nitride oxide.
[0353] The insulator 222 can be deposited by, for example, sputtering, CVD, MBE, PLD, ALD, etc. In this embodiment, hafnium oxide is deposited by ALD as the insulator 222. Alternatively, a stack of silicon nitride deposited by PEALD and hafnium oxide deposited by ALD can be used as the insulator 222.
[0354] Next, heat treatment is preferably performed. The temperature of the heat treatment is preferably above 250°C and below 650°C, more preferably above 300°C and below 500°C, and further preferably above 320°C and below 450°C. The heat treatment is performed in a nitrogen gas or inert gas atmosphere or in an atmosphere containing an oxidizing gas of more than 10ppm, more than 1% or more than 10%. For example, when heat treatment is performed in a mixed atmosphere of nitrogen gas and oxygen gas, the proportion of oxygen gas is preferably set to about 20%. The heat treatment can also be performed under reduced pressure. Alternatively, the heat treatment can also be performed in a nitrogen gas or inert gas atmosphere, and then heat treatment is performed in an atmosphere containing an oxidizing gas of more than 10ppm, more than 1% or more than 10% in order to fill the detached oxygen.
[0355] In addition, the gas used in the above heat treatment is preferably highly purified. For example, the amount of water contained in the gas used in the above heat treatment is preferably 1 ppb or less, more preferably 0.1 ppb or less, and further preferably 0.05 ppb or less. By using a highly purified gas for heat treatment, it is possible to prevent moisture and the like from being absorbed by the insulator 222 and the like as much as possible.
[0356] In this embodiment, as a heat treatment, a treatment is performed at a flow rate ratio of nitrogen gas to oxygen gas of 4:1 and a temperature of 400° C. for 1 hour after the insulator 222 is deposited. By performing this heat treatment, impurities such as water and hydrogen contained in the insulator 222 can be removed. In addition, when a hafnium-containing oxide is used as the insulator 222, a part of the insulator 222 may be crystallized by performing this heat treatment. In addition, the heat treatment may be performed at a timing such as after the insulator 224 is deposited.
[0357] Next, an insulating film 224f is deposited on the insulator 222 ( Figure 7B ).
[0358] The insulating film 224f can be deposited by, for example, sputtering, CVD, MBE, PLD, ALD, or the like. In this embodiment, silicon oxide is deposited by sputtering as the insulating film 224f. By using a sputtering method that does not require the use of molecules containing hydrogen as a deposition gas, the hydrogen concentration in the insulating film 224f can be reduced. The insulating film 224f is in contact with the oxide 230a in a subsequent process, so it is preferable that the hydrogen concentration is reduced in this way.
[0359] Next, an oxide film 230af and an oxide film 230bf are sequentially deposited on the insulating film 224f ( Figure 7B ). It is preferred that the oxide film 230af and the oxide film 230bf are continuously deposited without being exposed to the atmosphere. By depositing the oxide film without being exposed to the atmosphere, impurities or moisture from the atmosphere can be prevented from adhering to the oxide film 230af and the oxide film 230bf, so that the vicinity of the interface between the oxide film 230af and the oxide film 230bf can be kept clean.
[0360] The oxide film 230af and the oxide film 230bf can be deposited by sputtering, CVD, MBE, PLD, ALD, etc. In the present embodiment, sputtering is used as a method for depositing the oxide film 230af and the oxide film 230bf.
[0361] For example, when the oxide film 230af and the oxide film 230bf are deposited by sputtering, oxygen or a mixed gas of oxygen and a rare gas is used as the sputtering gas. By increasing the proportion of oxygen contained in the sputtering gas, the excess oxygen in the deposited oxide film can be increased. In addition, when the above-mentioned oxide film is deposited by sputtering, an In-M-Zn oxide target or the like can be used.
[0362] In particular, when the oxide film 230af is deposited, part of the oxygen contained in the sputtering gas may be supplied to the insulating film 224f. Therefore, the proportion of oxygen contained in the sputtering gas is preferably 70% or more, more preferably 80% or more, and further preferably 100%.
[0363] In the case of forming the oxide film 230bf by sputtering, an oxygen-excess oxide semiconductor can be formed by depositing a film under the condition that the proportion of oxygen contained in the sputtering gas is greater than 30% and less than 100%, preferably greater than 70% and less than 100%. A transistor using an oxygen-excess oxide semiconductor in a channel formation region can obtain relatively high reliability. Note that one embodiment of the present invention is not limited to this. In the case of forming the oxide film 230bf by sputtering, when deposition is performed when the proportion of oxygen contained in the sputtering gas is set to greater than 1% and less than 30%, preferably greater than 5% and less than 20%, an oxygen-deficient oxide semiconductor is formed. A transistor using an oxygen-deficient oxide semiconductor in a channel formation region can have a higher field effect mobility. In addition, by performing deposition while heating the substrate, the crystallinity of the oxide film can be improved.
[0364] In this embodiment, the oxide film 230af is deposited by sputtering using an oxide target of In:Ga:Zn=1:3:4 [atomic ratio] or an oxide target of In:Ga:Zn=1:3:2 [atomic ratio]. In addition, the oxide film 230bf is deposited by sputtering using an oxide target of In:Ga:Zn=4:2:4.1 [atomic ratio], an oxide target of In:Ga:Zn=1:1:1 [atomic ratio], an oxide target of In:Ga:Zn=1:1:1.2 [atomic ratio], or an oxide target of In:Ga:Zn=1:1:2 [atomic ratio]. Each oxide film can be formed by appropriately selecting deposition conditions and atomic ratios according to the characteristics required for the oxide 230a and the oxide 230b.
[0365] Note that the insulating film 224f, the oxide film 230af, and the oxide film 230bf are preferably deposited by sputtering without being exposed to the atmosphere. For example, a multi-chamber deposition apparatus may be used. Thus, the intrusion of hydrogen into the insulating film 224f, the oxide film 230af, and the oxide film 230bf between each deposition step can be reduced.
[0366] Next, heat treatment is preferably performed. The heat treatment may be performed within a temperature range where polycrystallization does not occur in the oxide film 230af and the oxide film 230bf. The heat treatment temperature is preferably 100°C or higher, 250°C or higher, or 350°C or higher and 650°C or lower, 600°C or lower, or 550°C or lower.
[0367] Note that as an atmosphere for the heat treatment, the same atmosphere as that applicable to the heat treatment performed after the deposition of the insulator 222 can be exemplified.
[0368] In addition, the gas used in the heat treatment is preferably highly purified, similarly to the heat treatment performed after depositing the insulator 222. By performing the heat treatment using highly purified gas, it is possible to prevent moisture and the like from being absorbed by the oxide films 230af and 230bf as much as possible.
[0369] In this embodiment, as a heat treatment, a treatment is performed for 1 hour under the conditions of a flow ratio of nitrogen gas to oxygen gas of 4:1 and a temperature of 400°C. Such a heat treatment containing oxygen gas can reduce impurities such as carbon, water, and hydrogen in the oxide film 230af and the oxide film 230bf. By reducing the impurities in the film in this way, the crystallinity of the oxide film 230bf is improved, and a denser structure with a higher density can be achieved. Therefore, the crystallized area in the oxide film 230af and the oxide film 230bf can be increased, and the in-plane unevenness of the crystallized area in the oxide film 230af and the oxide film 230bf can be reduced. Therefore, the in-plane unevenness of the electrical characteristics of the transistor can be reduced.
[0370] In addition, by performing the heat treatment, hydrogen in the insulator 216, the insulating film 224f, the oxide film 230af, and the oxide film 230bf is transferred to the insulator 222 and absorbed by the insulator 222. In other words, hydrogen in the insulator 216, the insulating film 224f, the oxide film 230af, and the oxide film 230bf diffuses into the insulator 222. Therefore, although the hydrogen concentration of the insulator 222 increases, the hydrogen concentrations in the insulator 216, the insulating film 224f, the oxide film 230af, and the oxide film 230bf all decrease.
[0371] In particular, the insulating film 224f (later insulator 224) is used as a second gate insulator of the transistor 202a, and the oxide film 230af and the oxide film 230bf (later oxide 230a and oxide 230b) are used as a channel formation region of the transistor 202a. The transistor 202a including the insulating film 224f, the oxide film 230af, and the oxide film 230bf in which the hydrogen concentration is reduced has excellent reliability and is therefore preferred.
[0372] Next, a conductive film 242_1f is deposited on the oxide film 230bf, and a conductive film 242_2f is deposited on the conductive film 242_1f ( Figure 7B ). After the oxide film 230bf is deposited, the conductive film 242_1f is deposited on and in contact with the oxide film 230bf without an etching process, so that the top surface of the oxide film 230bf can be protected by the conductive film 242_1f. As a result, since the diffusion of impurities into the oxide 230 constituting the transistor can be reduced, the electrical characteristics and reliability of the semiconductor device can be improved.
[0373] The conductive film 242_1f and the conductive film 242_2f are respectively deposited by, for example, a sputtering method, a CVD method, an MBE method, a PLD method, or an ALD method.
[0374] In this embodiment, tantalum nitride is deposited as the conductive film 242_1f by sputtering, and tungsten is deposited as the conductive film 242_2f. In addition, heat treatment may be performed before depositing the conductive film 242_1f. The heat treatment may also be performed under reduced pressure, and the conductive film 242_1f is continuously deposited without being exposed to the atmosphere. By performing this treatment, moisture and hydrogen attached to the surface of the oxide 230b can be removed, and the moisture concentration and hydrogen concentration in the oxide 230a and the oxide 230b can be reduced. The temperature of the heat treatment is preferably above 100°C and below 400°C. In this embodiment, the temperature of the heat treatment is set to 250°C.
[0375] Next, an insulating film 271f is deposited on the conductive film 242_2f ( Figure 7B). The insulating film 271f can be deposited by sputtering, CVD, MBE, PLD, ALD, or the like. The insulating film 271f preferably uses an insulating film having a function of suppressing the permeation of oxygen. For example, a stacked film of a silicon nitride film and a silicon oxide film on the silicon nitride film deposited by sputtering can be used as the insulating film 271f.
[0376] Next, the insulating film 224f, the oxide film 230af, the oxide film 230bf, the conductive film 242_1f, the conductive film 242_2f, and the insulating film 271f are processed into island shapes by photolithography to form the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 ( Figure 7C ).
[0377] Here, it is preferred that the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 are processed into an island shape at one time. At this time, the side end of the conductor 242_1 and the side end of the conductor 242_2 are preferably roughly aligned with the side end of the oxide 230a and the oxide 230b. Furthermore, the side end of the insulator 224 is preferably roughly aligned with the side end of the oxide 230. Furthermore, the side end of the insulator 271 is preferably roughly aligned with the side end of the conductor 242. By adopting such a structure, a semiconductor device according to one embodiment of the present invention can be manufactured with high productivity.
[0378] At least a portion of the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 are formed so as to overlap with the conductor 205. In addition, at least a portion of a region between the conductor 242_1 and the conductor 242_2 is formed so as to overlap with the conductor 209. In addition, the insulator 222 is exposed in a region that does not overlap with the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271.
[0379] like Figure 7C As shown, the side surfaces of the insulator 224, oxide 230a, oxide 230b, conductor 242_1, conductor 242_2, and insulator 271 may be substantially perpendicular to the top surface of the insulator 222. With such a structure, it is possible to realize a reduction in area and a high density when arranging a plurality of transistors.
[0380] In addition, without being limited to the above structure, the side surfaces of the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 may also have a tapered shape. The taper angle of the side surfaces of the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 may be, for example, 60° or more and less than 90°. In this way, by having the side surfaces have a tapered shape, the coverage of the insulator 275 and the like is improved in the subsequent process, and defects such as voids can be reduced.
[0381] like Figure 7C As shown, the conductor 242, the oxide 230, and the insulator 224 are preferably formed into two islands. Note that the present invention is not limited to this, and the conductor 242, the oxide 230, and the insulator 224 may be formed into a single island having an opening at a position overlapping with the conductor 209.
[0382] The above processing can be performed by dry etching or wet etching. Processing by dry etching is suitable for micro-processing. In addition, the processing of the insulating film 224f, the oxide film 230af, the oxide film 230bf, the conductive film 242_1f, the conductive film 242_2f, and the insulating film 271f can also be performed under different conditions.
[0383] Note that in photolithography, first, the resist is exposed through a mask. Then, a developer is used to remove or leave the exposed area to form a resist mask. Then, the conductor, semiconductor, insulator, etc. can be processed into a desired shape by etching through the resist mask. For example, a resist can be exposed to light such as KrF excimer laser, ArF excimer laser, EUV (Extreme Ultraviolet) light, etc. to form a resist mask. In addition, an immersion technique in which exposure is performed in a state where liquid (e.g., water) is filled between the substrate and the projection lens can also be used. In addition, an electron beam or ion beam can also be used instead of the above light. Note that when an electron beam or an ion beam is used, a mask is not required. In addition, the resist mask can be removed by performing a dry etching process such as ashing, performing a wet etching process, performing a wet etching process after a dry etching process, or performing a dry etching process after a wet etching process.
[0384] Furthermore, a hard mask made of an insulator or a conductor can also be used under the resist mask. When a hard mask is used, an insulating film or a conductive film that becomes a hard mask material can be formed on the oxide film 230bf and a resist mask can be formed thereon, and then the hard mask material can be etched to form a hard mask of a desired shape. The etching of the oxide film 230bf and the like can be performed after removing the resist mask or without removing the resist mask. In the case of the latter, the resist mask sometimes disappears during etching. The hard mask can be removed by etching after etching the oxide film 230bf and the like. On the other hand, when the hard mask material does not affect the subsequent process or can be used in the subsequent process, it is not necessarily necessary to remove the hard mask.
[0385] As an etching gas for dry etching treatment, a halogen-containing etching gas can be used. Specifically, an etching gas containing one or more of fluorine, chlorine and bromine can be used. For example, as an etching gas, one or a mixed gas of C4F6 gas, C5F6 gas, C4F8 gas, CF4 gas, SF6 gas, CHF3 gas, CH2F2 gas, Cl2 gas, BCl3 gas, SiCl4 gas or BBr3 gas can be used. In addition, oxygen gas, carbonic acid gas, nitrogen gas, helium gas, argon gas, hydrogen gas or hydrocarbon gas can be appropriately added to the above-mentioned etching gas. In addition, according to the object to be processed by dry etching treatment, a gas that does not contain halogen gas but contains hydrocarbon gas or hydrogen gas can be used as an etching gas. As hydrocarbons used for etching gas, methane (CH4), ethane (C2H6), propane (C3H8), butane (C4H 10 ), ethylene (C2H4), propylene (C3H6), acetylene (C2H2) and propyne (C3H4) One or more. The etching conditions can be appropriately set according to the etching object.
[0386] As a dry etching device, a capacitively coupled plasma (CCP: Capacitively Coupled Plasma) etching device including parallel plate electrodes can be used. The capacitively coupled plasma etching device including parallel plate electrodes can also adopt a structure in which a high-frequency voltage is applied to one of the parallel plate electrodes. Alternatively, a structure in which multiple different high-frequency voltages are applied to one of the parallel plate electrodes can be adopted. Alternatively, a structure in which a high-frequency voltage with the same frequency is applied to each of the parallel plate electrodes can be adopted. Alternatively, a structure in which a high-frequency voltage with different frequencies is applied to each of the parallel plate electrodes can be adopted. Alternatively, a dry etching device with a high-density plasma source can be used. For example, as a dry etching device with a high-density plasma source, an inductively coupled plasma (ICP: Inductively Coupled Plasma) etching device or the like can be used.
[0387] The following reference FIG. 8A to FIG. 8F A specific example of processing of the insulating film 224f, the oxide film 230af, the oxide film 230bf, the conductive film 242_1f, the conductive film 242_2f, and the insulating film 271f will be described.
[0388] First, a hard mask layer 276f is deposited on the insulating film 271f ( Fig. 8A ). The hard mask layer 276f can be deposited by sputtering, CVD, MBE, PLD, or ALD. The hard mask layer 276f is a film used as a hard mask for forming the conductor 242 and the oxide 230 in a later process. As the hard mask layer 276f, a metal material or an inorganic insulating material can be used. For example, tungsten deposited by sputtering is used as the hard mask layer 276f. In addition, the hard mask layer 276f can be continuously deposited without being exposed to the atmosphere after the insulating film 271f is deposited.
[0389] Next, an organic coating film 277f is deposited on the hard mask layer 276f, and an organic coating film 278f is also deposited ( Fig. 8A ). The organic coating film 277f and the organic coating film 278f may also have the function of improving the adhesion between the hard mask and the resist mask described later. The organic coating film 277f and the organic coating film 278f are deposited, for example, by spin coating. The organic coating film 277f and the organic coating film 278f may use a non-photosensitive organic resin. In this embodiment, a SOC (Spin On Carbon) film is deposited as the organic coating film 277f, and a SOG (Spin On Glass) film is deposited as the organic coating film 278f. Here, the organic coating film 277f and the organic coating film 278f contain an organic solvent such as alcohol when coated, but in subsequent processes or when the semiconductor device is completed, the organic matter contained is sometimes reduced or removed. Note that the organic coating film may be provided as needed, and the organic coating film may also have a single-layer structure. In the case where it is sufficient to use only the resist mask described later, the organic coating film may not be provided.
[0390] Next, a resist mask 279 ( Fig. 8A ). As the resist mask 279, a photosensitive organic resin also called a photoresist can be used. For example, a positive photoresist or a negative photoresist can be used. For example, the photoresist that becomes the resist mask 279 can be deposited to a uniform thickness by using a spin coating method or the like.
[0391] The following is based on FIG. 8B to FIG. 8F In the process, a dry etching device is used to Fig. 8AThe etching process of the laminated film shown in FIG. FIG. 8B to FIG. 8F The process is preferably carried out continuously without exposure to the atmosphere. For example, a multi-chamber etching apparatus is used to carry out the process without exposure to the atmosphere. As the above-mentioned dry etching apparatus, a CCP etching apparatus can be used that applies high-frequency voltages of different frequencies to parallel plate electrodes of the processing chamber. In this case, a structure can be provided in which a high-frequency voltage is applied to the upper electrode and a low-frequency voltage is applied to the lower electrode on which the substrate is provided.
[0392] First, the organic coating film 278f is processed into an island shape to form an organic coating film 278 using a resist mask 279, and the organic coating film 277f is processed into an island shape to form an organic coating film 277 ( Figure 8B ). For example, when the organic coating film 278f is formed of a SOG film, CHF3 and O2 can be used as etching gases. In addition, for example, when the organic coating film 277f is formed of a SOC film, H2 and N2 can be used as etching gases.
[0393] The resist mask 279 may disappear before forming the organic coating film 277. When the resist mask 279 remains after forming the organic coating film 277, the resist mask 279 may be removed.
[0394] Next, the organic coating film 277 is used as a mask, the hard mask layer 276f is processed into an island shape to form a hard mask layer 276, the insulating film 271f is processed into an island shape to form an insulator 271, and the conductive film 242_2f and the conductive film 242_1f are processed into an island shape to form a conductor 242_2 and a conductor 242_1 ( Figure 8C ). For example, when a tungsten film is used for the hard mask layer 276f, CF4 and Cl2 can be used as etching gases. In addition, for example, when a stacked film of silicon nitride and silicon oxide is used as the insulating film 271f, CHF3 and O2 can be used as etching gases. In addition, for example, when a stacked film of a tungsten film is used as the conductive film 242_2f and a tantalum nitride film is used as the conductive film 242_1f, CHF3, Cl2, and Ar can be used as etching gases.
[0395] Here, sometimes the hard mask layer 276 and the conductive film 242_2f use the same metal material (such as tungsten). When the organic coating film 277 used as a mask in the etching of the conductive film 242_2f and the conductive film 242_1f disappears, the hard mask layer 276 is exposed to the etching. As a result, there is a concern that the conductive film 242_2f and the conductive film 242_1f are excessively etched, and the width of the conductor 242 is narrower than the designed width.
[0396] In the etching process of the conductive film 242_2f and the conductive film 242_1f, it is preferable to perform etching under the condition that the etching rate of the conductive film 242_2f and the conductive film 242_1f is greater than the etching rate of the organic coating film 277. For example, in the etching process of the conductive film 242_2f and the conductive film 242_1f, it is preferable to reduce the power of the lower electrode of the substrate. For example, the power of the lower electrode of the substrate can be lower than the power of the lower electrode when etching the hard mask layer 276f, preferably less than 25W, and more preferably less than 10W. By performing etching under such conditions, processing can be performed according to the design even in a semiconductor device having a microstructure.
[0397] Next, the oxide film 230bf and the oxide film 230af are processed into island shapes using the hard mask layer 276 to form the oxide 230b and the oxide 230a ( Fig.8D ). For example, when an oxide containing one or more selected from In, Ga, and Zn is used as the oxide film 230bf and the oxide film 230af, CH4 and Ar can be used as etching gases. The oxide containing In, Ga, and Zn reacts with CH3 radicals to easily form a highly volatile metal complex. Therefore, even if the substrate temperature is low, a gas containing CH4 is used, and the oxide containing In, Ga, and Zn, which is a material that is difficult to etch, can be easily processed.
[0398] Note that when Fig.8D When the organic coating film 277 remains after the steps shown, the resist mask can be removed by performing dry etching such as ashing, performing wet etching, performing wet etching followed by dry etching, or performing dry etching followed by wet etching.
[0399] Next, the insulating film 224f is processed into an island shape using the hard mask layer 276 to form the insulator 224 ( Fig. 8E ). For example, when a silicon oxide film is used as the insulating film 224f, CHF3 and Ar can be used as etching gases.
[0400] Here, in the processing of the insulating film 224f, the insulator 222 is preferably not overetched. Therefore, it is preferable to perform etching under conditions where the etching selectivity relative to the insulator 222 is large. For example, when the insulating film 224f contains silicon oxide and is etched using a gas containing fluorine, the insulator 222 preferably contains hafnium oxide. By performing etching in this way, in the following process, the insulator 275 can be set in a manner that contacts the side surface of the insulator 224 and the top surface of the insulator 222. That is, the insulator 224 can be separated from the insulator 280 by the insulator 275. By having such a structure, it is possible to prevent excess impurities such as oxygen and hydrogen from being mixed into the oxide 230 from the insulator 280 through the insulator 224.
[0401] Finally, the hard mask layer 276 is removed ( Fig.8F ). For example, when a tungsten film is used as the hard mask layer 276, CF4, Cl2, and O2 can be used as etching gases. In addition, when the hard mask layer 276 does not affect the subsequent process or can be used in the subsequent process, it is not necessary to remove the hard mask layer 276.
[0402] In addition, in the removal process of the hard mask layer 276, the insulator 271 is used as a mask for forming the conductor 242_2, and the conductor 242_2 does not have a curved surface between the side surface and the top surface. As a result, the ends of the conductor 242a and the conductor 242b where the side surface and the top surface intersect become angled. When the ends where the side surface and the top surface of the conductor 242 intersect become angled, the cross-sectional area of the conductor 242 increases compared to the case where the ends have a curved surface. As a result, the resistance of the conductor 242 decreases, thereby increasing the on-state current of the transistor.
[0403] As described above, the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 can be processed into an island shape at one time. Thus, the number of steps can be reduced compared to the case where the insulator 224, the oxide 230a, the oxide 230b, the conductor 242_1, the conductor 242_2, and the insulator 271 are processed into island shapes separately. Therefore, a method for manufacturing a semiconductor device with high productivity can be provided.
[0404] Next, the insulator 275 is deposited to cover the insulator 224 , the oxide 230 a , the oxide 230 b , the conductor 242_1 , the conductor 242_2 , and the insulator 271 , and the insulator 280 is deposited on the insulator 275 .
[0405] Here, the insulator 275 is preferably in contact with the top surface of the insulator 222 .
[0406] Insulator 280 is preferably formed by forming an insulating film to be insulator 280 and then subjecting the insulating film to CMP treatment to form an insulator with a flat top surface. Alternatively, silicon nitride may be deposited on insulator 280 by, for example, sputtering and then subjected to CMP treatment until the silicon nitride reaches insulator 280.
[0407] The insulator 275 and the insulator 280 can each be deposited by, for example, sputtering, CVD, MBE, PLD, or ALD.
[0408] The insulator 275 preferably uses an insulator that has a function of inhibiting oxygen transmission. For example, silicon nitride is preferably deposited by the PEALD method as the insulator 275. In addition, aluminum oxide is preferably deposited by the sputtering method as the insulator 275, and silicon nitride is deposited thereon by the PEALD method. When the insulator 275 has such a laminated structure, the function of inhibiting the diffusion of impurities such as water and hydrogen and oxygen can be improved.
[0409] Thus, the oxide 230a, the oxide 230b, the conductors 242_1, and the conductors 242_2 can be covered by the insulator 275 having the function of suppressing oxygen diffusion. Thus, direct diffusion of oxygen from the insulator 280 and the like into the insulator 224, the oxide 230a, the oxide 230b, the conductors 242_1, and the conductors 242_2 in a subsequent step can be reduced.
[0410] For example, silicon oxide is preferably deposited by sputtering as the insulator 280. By depositing an insulating film to be the insulator 280 by sputtering in an oxygen-containing atmosphere, an insulator 280 containing excess oxygen can be formed. By using a sputtering method that does not require the use of molecules containing hydrogen as a deposition gas, the hydrogen concentration in the insulator 280 can be reduced. In addition, a heat treatment may also be performed before the insulating film is deposited. The heat treatment may also be performed under reduced pressure, and the insulating film may be continuously deposited without being exposed to the atmosphere. By performing such a treatment, moisture and hydrogen attached to the surface of the insulator 275, etc. may be removed, and the moisture concentration and hydrogen concentration in the oxide 230a, the oxide 230b, and the insulator 224 may be reduced. The heat treatment may adopt the conditions of the above-mentioned heat treatment.
[0411] Next, the conductor 242_1, the conductor 242_2, the insulator 271, the insulator 275, and the insulator 280 are processed by photolithography to form an opening reaching the oxide 230b ( Fig. 9A ). The opening reaching the oxide 230 b is provided in a region where the oxide 230 b and the conductor 205 overlap.
[0412] In addition, the above-mentioned processing can be performed by dry etching or wet etching. In addition, the processing of the conductor 242_1, the conductor 242_2, the insulator 271, the insulator 275, and the insulator 280 can also be performed under different conditions.
[0413] Through this processing, the conductor 242_1 is divided into island-shaped conductors 242a1 and 242b1. Similarly, the conductor 242_2 is divided into island-shaped conductors 242a2 and 242b2. Similarly, the insulator 271 is divided into island-shaped insulators 271a and 271b.
[0414] Through the above-mentioned etching process, the following may occur: impurities are attached to the side surface of the oxide 230a, the top surface and side surface of the oxide 230b, the side surface of the conductors 242a and 242b, the side surface of the insulators 271a and 271b, the side surface of the insulator 275, and the side surface of the insulator 280; or the impurities diffuse into them. A process of removing these impurities may be performed. In addition, a damaged area may be formed on the surface of the oxide 230b due to the above-mentioned dry etching. In addition, such a damaged area may also be removed. As examples of such impurities, there may be mentioned impurities caused by the following components: components contained in the insulator 280, the side surface of the insulators 271a and 271b, the insulator 275, and the conductors 242a and 242b; components contained in the components of the device used when forming the above-mentioned opening; components contained in the gas or liquid used for etching, etc. As examples of such impurities, there may be mentioned hafnium, aluminum, silicon, tantalum, fluorine, chlorine, etc.
[0415] In particular, impurities such as aluminum and silicon sometimes reduce the crystallinity of oxide 230b. Therefore, impurities such as aluminum and silicon are preferably removed from the surface of oxide 230b and its vicinity. In addition, it is preferred to reduce the impurity concentration. For example, the concentration of aluminum atoms on the surface of oxide 230b and its vicinity is preferably 5.0 atomic % or less, more preferably 2.0 atomic % or less, more preferably 1.5 atomic % or less, further preferably 1.0 atomic % or less, and particularly preferably less than 0.3 atomic %.
[0416] Due to impurities such as aluminum and silicon, the density of the crystal structure is reduced in the low crystallinity region of the oxide 230b, so a large amount of V O H makes the transistor easily normally-on. Therefore, it is preferable to reduce or remove the region with low crystallinity in the oxide 230b.
[0417] In contrast, the oxide 230b preferably has a layered CAAC structure. In particular, it is preferred that the lower end of the drain of the oxide 230b also has a CAAC structure. Here, in the transistor, the conductor 242a or the conductor 242b is used as a drain. In other words, the oxide 230b near the lower end of the conductor 242a or the conductor 242b preferably has a CAAC structure. In this way, by removing the low-crystallinity region of the oxide 230b at the drain end that has a significant impact on the drain withstand voltage and making it have a CAAC structure, the variation of the electrical characteristics of the transistor can be further suppressed. In addition, the reliability of the transistor can be further improved.
[0418] In order to remove impurities and the like attached to the surface of the oxide 230b in the above-mentioned etching process, a cleaning process is performed. As a cleaning method, there are wet cleaning using a cleaning solution or the like (which may also be referred to as a wet etching process), plasma treatment using plasma, cleaning using a heat treatment, etc., and the above-mentioned cleanings may be appropriately combined. Note that the above-mentioned groove may become deeper by performing this cleaning process.
[0419] As wet cleaning, an aqueous solution, pure water or carbonated water etc. formed by diluting one or more of ammonia, oxalic acid, phosphoric acid or hydrofluoric acid with carbonated water or pure water can be used. Alternatively, ultrasonic cleaning can be performed using the above aqueous solution, pure water or carbonated water. In addition, the above cleaning can also be appropriately combined.
[0420] Note that in this specification, etc., an aqueous solution of hydrofluoric acid diluted with pure water is sometimes referred to as dilute hydrofluoric acid, and an aqueous solution of ammonia diluted with pure water is sometimes referred to as dilute ammonia water. In addition, the concentration, temperature, etc. of the aqueous solution can be appropriately adjusted according to the impurities to be removed, the structure of the semiconductor device to be washed, etc. The ammonia concentration of the dilute ammonia water is preferably set to 0.01% or more and 5% or less, and more preferably set to 0.1% or more and 0.5% or less. In addition, the hydrogen fluoride concentration of the dilute hydrofluoric acid is preferably set to 0.01ppm or more and 100ppm or less, and more preferably set to 0.1ppm or more and 10ppm or less.
[0421] In addition, it is preferable to use a frequency of 200 kHz or higher, and more preferably a frequency of 900 kHz or higher for ultrasonic cleaning. By using such a frequency, damage to the oxide 230 b and the like can be reduced.
[0422] The above-mentioned washing treatment may be performed multiple times, and the washing liquid may be changed for each washing treatment. For example, the first washing treatment may be a treatment using dilute hydrofluoric acid or dilute ammonia water, and the second washing treatment may be a treatment using pure water or carbonated water.
[0423] In this embodiment, the cleaning process is performed by wet cleaning using dilute ammonia water. This cleaning process can remove impurities attached to the surface of the oxide 230a, the oxide 230b, etc. or diffused into the inside thereof. In addition, the crystallinity of the oxide 230b can be improved.
[0424] Heat treatment may also be performed after the above-mentioned etching or the above-mentioned washing. The temperature of the heat treatment is preferably above 100°C, above 250°C, or above 350°C and below 650°C, below 600°C, below 550°C, or below 400°C. The heat treatment is performed in an atmosphere of nitrogen gas, an inert gas, or an oxidizing gas containing more than 10 ppm, more than 1%, or more than 10%. For example, the heat treatment is preferably performed in an oxygen atmosphere. Thus, oxygen is supplied to the oxide 230a and the oxide 230b, so that oxygen vacancies can be reduced. In addition, by performing the above-mentioned heat treatment, the crystallinity of the oxide 230b can be improved. Furthermore, the hydrogen remaining in the oxide 230a and the oxide 230b reacts with the supplied oxygen and the hydrogen can be removed (dehydrated) in the form of H2O. Thus, the hydrogen remaining in the oxide 230a and the oxide 230b can be inhibited from recombinating with oxygen vacancies to form V O H. The heat treatment may be performed under reduced pressure. Alternatively, the heat treatment may be performed in an oxygen atmosphere and then continuously in a nitrogen atmosphere without being exposed to the air.
[0425] When the conductor 242a and the conductor 242b are heated while in contact with the oxide 230b, the sheet resistance of the oxide 230b in the region overlapping with the conductor 242a and the oxide 230b in the region overlapping with the conductor 242b may be reduced. In addition, the carrier concentration may be increased. Therefore, the resistance of the oxide 230b in the region overlapping with the conductor 242a and the oxide 230b in the region overlapping with the conductor 242b may be reduced in a self-aligned manner.
[0426] Next, an insulating film and a conductive film are deposited and processed so as to embed the openings, and an insulator 250, a conductor 260a, and a conductor 260b are provided at a position overlapping with the conductor 205 ( Fig. 9B ).
[0427] First, an insulating film to be the insulator 250 is deposited. The insulating film can be deposited, for example, by sputtering, CVD, MBE, PLD, or ALD. The insulating film is preferably deposited by the ALD method. Similar to the above-mentioned insulator 250, the insulator 250 is preferably formed thin, and thickness non-uniformity needs to be suppressed to a minimum. In this regard, the ALD method is a deposition method that alternately introduces precursors and reactants (for example, oxidants, etc.), and since the thickness of the film can be adjusted by the number of times the cycle is repeated, the thickness can be precisely adjusted. In addition, as Fig. 9B As shown, the insulator 250 needs to be deposited on the bottom and side surfaces of the opening with high coverage. By using the ALD method, since each atomic layer can be deposited on the bottom and side surfaces of the opening, the insulator 250 can be formed in the opening with high coverage.
[0428] In addition, when the insulating film that becomes the insulator 250 is deposited by the ALD method, ozone (O3), oxygen (O2), water (H2O), etc. can be used as an oxidant. By using ozone (O3), oxygen (O2), etc. that do not contain hydrogen as an oxidant, hydrogen diffused into the oxide 230b can be reduced.
[0429] like Figure 3A and Figure 3B As shown, the insulator 250 may have a stacked structure. In this case, aluminum oxide may be deposited by thermal ALD as an insulating film to become the insulator 250a, silicon oxide may be deposited by PEALD as an insulating film to become the insulator 250b, and silicon nitride may be deposited by PEALD as an insulating film to become the insulator 250c. Furthermore, the insulator 250b may also have a stacked structure. In this case, silicon oxide may be deposited by PEALD as an insulating film to become the insulator 250b, and hafnium oxide may be deposited thereon by thermal ALD.
[0430] Next, microwave treatment is preferably performed in an oxygen-containing atmosphere. Here, microwave treatment refers to, for example, treatment using a device including a power supply that generates high-density plasma using microwaves. In addition, in this specification, microwaves refer to electromagnetic waves having a frequency of 300 MHz or more and 300 GHz or less. Note that when the insulator 250 has a laminated structure, the above-mentioned microwave treatment is not necessarily performed after all the insulating films that become the insulator 250 are deposited. For example, microwave treatment may be performed after the insulating film that becomes the insulator 250a and the insulating film that becomes the insulator 250b are deposited, and then the insulating film that becomes the insulator 250c is deposited.
[0431] Microwave treatment, for example, preferably uses a microwave processing device including a power supply that generates high-density plasma using microwaves. Here, the frequency of the microwave processing device is preferably set to be above 300 MHz and below 300 GHz, more preferably above 2.4 GHz and below 2.5 GHz, for example, it can be 2.45 GHz. By using high-density plasma, high-density oxygen free radicals can be generated. In addition, the power of the power supply that applies microwaves in the microwave processing device is preferably above 1000 W and below 10000 W, preferably above 2000 W and below 5000 W. In addition, the microwave processing device may also include a power supply that applies RF to one side of the substrate. In addition, by applying RF to one side of the substrate, the oxygen ions generated by the high-density plasma can be efficiently introduced into the oxide 230 b.
[0432] In addition, the microwave treatment is preferably carried out under reduced pressure, and the pressure is preferably 10Pa or more and 1000Pa or less, more preferably 300Pa or more and 700Pa or less. In addition, the treatment temperature is preferably 750°C or less, more preferably 500°C or less, for example, about 250°C. In addition, it is also possible to continuously perform heat treatment without being exposed to the atmosphere after the oxygen plasma treatment. The temperature of the heat treatment is, for example, preferably 100°C or more and 750°C or less, more preferably 300°C or more and 500°C or less.
[0433] In addition, for example, the above-mentioned microwave treatment can be performed using oxygen gas and argon gas. Here, the oxygen flow ratio (O2 / (O2+Ar)) is greater than 0% and less than 100%. Preferably, the oxygen flow ratio (O2 / (O2+Ar)) is greater than 0% and less than 50%. More preferably, the oxygen flow ratio (O2 / (O2+Ar)) is greater than 10% and less than 40%. Further preferably, the oxygen flow ratio (O2 / (O2+Ar)) is greater than 10% and less than 30%. In this way, by performing microwave treatment in an oxygen-containing atmosphere, the carrier concentration in the oxide 230b can be reduced. In addition, by preventing excessive oxygen from being introduced into the processing chamber during microwave treatment, the carrier concentration in the oxide 230b can be prevented from being excessively reduced.
[0434] By performing microwave treatment in an oxygen-containing atmosphere, microwaves or high frequencies such as RF can be used to convert oxygen gas into plasma and the oxygen plasma can be applied to the region between the conductors 242a and 242b of the oxide 230b. The V O H is separated into oxygen vacancies and hydrogen, and hydrogen is removed from the region. In other words, V contained in the channel formation region can be reduced. O H. Therefore, oxygen vacancies and V O H and thus reduce the carrier concentration. In addition, by supplying oxygen radicals generated in the above oxygen plasma to oxygen vacancies formed in the channel formation region, the oxygen vacancies in the channel formation region can be further reduced, thereby reducing the carrier concentration.
[0435] As oxygen injected into the channel formation region, there are various forms such as oxygen atoms, oxygen molecules, oxygen ions and oxygen free radicals (also called O free radicals, atoms, molecules or ions containing unpaired electrons). The oxygen injected into the channel formation region can be any one or more of the above forms, and oxygen free radicals are particularly preferred. In addition, since the film quality of the insulator 250 can be improved, the reliability of the transistor is improved.
[0436] On the other hand, the oxide 230b has a region overlapping with any one of the conductors 242a and 242b. This region can be used as a source region or a drain region. Here, the conductors 242a and 242b are preferably used as a shielding film to protect against microwaves, RF and other high frequencies or oxygen plasma when microwave treatment is performed in an oxygen-containing atmosphere. Therefore, the conductors 242a and 242b preferably have a function of shielding electromagnetic waves of 300 MHz or more and 300 GHz or less, for example, 2.4 GHz or more and 2.5 GHz or less.
[0437] The conductors 242a and 242b shield the microwaves, high frequencies such as RF, oxygen plasma, etc., and thus do not act on the region of the oxide 230b that overlaps with any of the conductors 242a and 242b. Thus, the microwave treatment does not cause V to occur in the source region and the drain region. O The decrease in H and the supply of excessive oxygen can prevent the decrease in carrier concentration.
[0438] In addition, an insulator 250 having oxygen barrier properties is provided in contact with the side surfaces of the conductors 242a and 242b. Therefore, it is possible to suppress the formation of oxide films on the side surfaces of the conductors 242a and 242b due to the microwave treatment.
[0439] Since the film quality of the insulator 250 can be improved, the reliability of the transistor is improved.
[0440] As described above, oxygen vacancies and V can be selectively removed in the channel formation region of the oxide semiconductor. O H makes the channel formation region become i-type or substantially i-type. In addition, it is possible to suppress the region used as the source region or the drain region from being supplied with excessive oxygen and maintain the conductivity (the state of the low resistance region) before the microwave treatment. Thus, it is possible to suppress the change of the electrical characteristics of the transistor and suppress the non-uniformity of the electrical characteristics of the transistor within the substrate surface.
[0441] In addition, during the microwave treatment, sometimes the microwave and the molecules in the oxide 230b directly transfer heat energy to the oxide 230b due to electromagnetic interaction. Sometimes the oxide 230b is heated by the heat energy. Sometimes this heat treatment is called microwave annealing. By performing the microwave treatment in an oxygen-containing atmosphere, sometimes an effect equivalent to oxygen annealing can be obtained. In addition, it is considered that: when the oxide 230b contains hydrogen, the above heat energy is transferred to the hydrogen in the oxide 230b and the activated hydrogen is released from the oxide 230b.
[0442] Alternatively, microwave treatment may be performed before the insulating film to be the insulator 250 is deposited, instead of performing microwave treatment after the insulating film is deposited.
[0443] In addition, heat treatment may be performed while maintaining a reduced pressure state after microwave treatment after the insulating film that becomes the insulator 250 is deposited. By performing such treatment, hydrogen in the insulating film, the oxide 230b, and the oxide 230a can be efficiently removed. In addition, a portion of the hydrogen is sometimes doped by the conductors 242a and 242b. In addition, the step of maintaining a reduced pressure state for heat treatment after microwave treatment may be repeated. By repeatedly performing heat treatment, hydrogen in the insulating film, the oxide 230b, and the oxide 230a can be further efficiently removed. Note that the heat treatment temperature is preferably above 300°C and below 500°C. The above-mentioned microwave treatment, i.e., microwave annealing, may also serve as the heat treatment. When the oxide 230b, etc. is sufficiently heated by microwave annealing, the heat treatment may not be performed.
[0444] Furthermore, the diffusion of hydrogen, water, impurities, etc. can be suppressed by changing the film quality of the insulating film that becomes the insulator 250 through microwave treatment. Thus, the diffusion of hydrogen, water, impurities, etc. through the insulator 250 to the oxide 230b, the oxide 230a, etc. due to a post-process such as deposition of the conductive film that becomes the conductor 260 or a post-process such as heat treatment can be suppressed.
[0445] Next, a conductive film to be the conductor 260a and a conductive film to be the conductor 260b are sequentially deposited. The conductive film to be the conductor 260a and the conductive film to be the conductor 260b can be deposited by sputtering, CVD, MBE, PLD, ALD, or the like. In this embodiment, titanium nitride is deposited as the conductive film to be the conductor 260a by the ALD method, and tungsten is deposited as the conductive film to be the conductor 260b by the CVD method.
[0446] Next, the conductive film to be the insulator 250, the conductive film to be the conductor 260a, and the conductive film to be the conductor 260b are polished by CMP processing until the insulator 280 is exposed. That is, the portions of the insulating film to be the insulator 250, the conductive film to be the conductor 260a, and the conductive film to be the conductor 260b exposed from the openings are removed. Thus, the insulator 250 and the conductor 260 (the conductor 260a and the conductor 260b) ( Fig. 9B ).
[0447] Thus, the insulator 250 is provided in contact with the inner wall and the side surface of the opening overlapping the oxide 230b. In addition, the conductor 260 is arranged so as to be embedded in the opening via the insulator 250. Thus, the transistors 202a and 202b are formed. As described above, the transistors 202a and 202b can be manufactured simultaneously in the same process.
[0448] Next, heat treatment may be performed under the same conditions as the above heat treatment. In this embodiment, the treatment is performed at a temperature of 400° C. for 1 hour in a nitrogen atmosphere. Through this heat treatment, the water concentration and hydrogen concentration in the insulator 280 can be reduced. In addition, after the above heat treatment, the deposition of the insulator 282 is continuously performed without being exposed to the atmosphere.
[0449] Next, an insulator 282 is formed on the insulator 250, the conductor 260, and the insulator 280. Fig. 9C ). The insulator 282 can be deposited by sputtering, CVD, MBE, PLD, ALD, or the like. The insulator 282 is preferably deposited by sputtering. By using a sputtering method that does not require the use of molecules containing hydrogen as a deposition gas, the hydrogen concentration in the insulator 282 can be reduced.
[0450] In this embodiment, aluminum oxide is deposited as the insulator 282 by pulsed DC sputtering using an aluminum target in an atmosphere containing oxygen. By using pulsed DC sputtering, the thickness can be made more uniform, thereby improving the sputtering rate and film quality. In addition, the RF power applied to the substrate is set to 1.86 W / cm 2 Below. Preferably 0W / cm 2 Above 0.62W / cm 2 Note that the RF power is 0W / cm 2 It means that RF power is not applied to the substrate. The amount of oxygen injected into the lower layer of the insulator 282 can be controlled according to the size of the RF power applied to the substrate. For example, the smaller the RF power, the less oxygen is injected into the lower layer of the insulator 282, and the oxygen amount is easily saturated even if the insulator 282 is thin. In addition, the greater the RF power, the more oxygen is injected into the lower layer of the insulator 282. By reducing the RF power, the amount of oxygen injected into the insulator 280 can be suppressed. Alternatively, an insulator 282 having a two-layer stacked structure can be deposited. At this time, for example, the RF power applied to the substrate is set to 0W / cm 2 To deposit the lower layer of the insulator 282, the RF power applied to the substrate was set to 0.62 W / cm 2 To deposit an upper layer of insulator 282.
[0451] In addition, the frequency of RF is preferably 10 MHz or higher, and is typically 13.56 MHz. The higher the frequency of RF, the less damage to the substrate can be caused.
[0452] In addition, by depositing the insulator 282 in an oxygen-containing atmosphere by a sputtering method, oxygen can be added to the insulator 280 while being deposited. Thus, excess oxygen can be contained in the insulator 280. In this case, the insulator 282 is preferably deposited while the substrate is heated.
[0453] Next, an insulator 283 is formed on the insulator 282 ( Fig. 9C ). The insulator 283 can be deposited, for example, by sputtering, CVD, MBE, PLD, or ALD. The insulator 283 is preferably deposited by sputtering. By using a sputtering method that does not require molecules containing hydrogen to be used for the deposition gas, the hydrogen concentration in the insulator 283 can be reduced. In this embodiment, silicon nitride is deposited by sputtering as the insulator 283.
[0454] Next, an insulator 285 is formed on the insulator 283 ( Fig. 9C ). The insulator 285 can be deposited, for example, by sputtering, CVD, MBE, PLD, or ALD. The insulator 285 is preferably deposited by sputtering. By using a sputtering method that does not require the use of molecules containing hydrogen for the deposition gas, the hydrogen concentration in the insulator 285 can be reduced. In this embodiment, silicon oxide is deposited by sputtering as the insulator 285.
[0455] Here, the electrostatic capacitance of the capacitor 101a is preferably set by adjusting the thickness of the insulator 285. For example, the thickness of the insulator 285 is set within a range of 50 nm to 250 nm, and the depth of the opening for forming the capacitor 101a is about 150 nm to 350 nm. By forming the capacitor 101a within the above range, the capacitor 101a has a sufficient electrostatic capacitance, and in a semiconductor device having a plurality of memory cell layers stacked, the height of one layer can be prevented from being excessively increased.
[0456] Next, the insulators 285, 283, 282, 280, 275, 271a, 222, 216, 214, and 212 are processed by photolithography to form an opening ( Fig. 10A ). When viewed from above, the opening is preferably formed so that a portion of the top surface of the conductor 242a is exposed. In addition, when viewed from above, the opening may be circular, substantially circular such as an ellipse, a polygon such as a quadrangle, or a quadrangle such as a polygon with an arc at the corner.
[0457] When forming the opening, dry etching or wet etching can be used. Dry etching is suitable for micro-processing, so dry etching is preferably used. The above-mentioned gases can be used as etching gas.
[0458] Here, aluminum oxide and hafnium oxide are sometimes difficult to etch compared to silicon oxide or silicon oxynitride. Aluminum oxide and hafnium oxide can each be referred to as a difficult-to-etch material.
[0459] When the above-mentioned hard-to-etch materials are used as the insulators 282, 222, etc., by forming openings in advance in the insulators, etching can be performed with high yield. Fig. 10A The processing steps shown can thus improve the productivity of semiconductor devices. Fig. 10A In the processing step, when an opening is formed in the insulator at one time, the number of masks can be reduced, so it is preferred.
[0460] Fig. 10A The example in which the widths of the openings provided in the insulators 285, 283, 282, 280, 275, and 271a are substantially uniform is shown, but the invention is not limited thereto. When the etching rates of one or more of the insulators 285, 283, 282, 280, 275, and 271a are different, the ends of the insulators 285, 283, 282, 280, 275, and 271a may be uneven in cross section even if the openings are formed at one time.
[0461] also, Fig. 10A An example is shown in which the ends of the conductor 242a and the ends of the insulators 212, 214, 216, and 222 are roughly aligned in the opening, but the invention is not limited thereto. Depending on etching conditions, one or more of the insulators 212, 214, 216, and 222 may have their side surfaces etched, and their ends may be located inside the ends of the conductor 242a (on the transistor side).
[0462] For example, it is preferable to form openings in the insulators 212, 214, 216, 222, 271a, 275, 280, 282, 283, and 285 by anisotropic etching. Dry etching is preferably used as anisotropic etching. Thus, for example, Figure 1 An opening of the shape shown.
[0463] Next, an insulating film 241A ( Fig. 10B ). As the insulating film 241A, it is preferable to use an insulating film having a function of suppressing the diffusion of at least one of oxygen and hydrogen. For example, it is preferable to deposit a silicon nitride film by the PEALD method. Silicon nitride has high barrier properties to oxygen and hydrogen, so it is preferred. Note that the insulating film 241A may also have a stacked structure. As the insulating film 241A, for example, an aluminum oxide film may be deposited by the ALD method and a silicon nitride film may be deposited thereon by the PEALD method. When the insulating film 241A is deposited by the ALD method, the aluminum oxide film can be deposited at a lower temperature than the silicon nitride film. Therefore, by depositing the aluminum oxide film before depositing the silicon nitride film, oxidation of the conductor 260, the conductor 242, etc. can be suppressed.
[0464] The insulating film 241A is anisotropically etched to form the insulator 241 ( Fig. 10C ). Here, at least a portion of the conductor 242a is exposed from the insulator 241. The anisotropic etching performed on the insulating film 241A can be performed by, for example, dry etching. By providing the insulator 241 on the sidewall portion of the above-mentioned opening, the penetration of oxygen from the outside can be suppressed, and oxidation of the conductor 240 to be formed next can be prevented. In addition, impurities such as water and hydrogen contained in the conductor 240, the insulator 280, etc. can be prevented from diffusing into the oxide 230.
[0465] Next, the conductive film 240a1f and the conductive film 240b1f are sequentially deposited ( Fig.11A ). Here, a portion of the conductive film 240a1f contacts the conductor 242a through the opening of the insulator 241. The conductive film 240a1f preferably has a function of inhibiting the penetration of impurities such as water and hydrogen. As the conductive film 240a1f, for example, tantalum nitride or titanium nitride can be used. In addition, as the conductive film 240b1f, for example, tungsten, molybdenum or copper can be used. These conductive films can be deposited by, for example, sputtering, CVD, MBE, PLD or ALD.
[0466] By performing CMP treatment, a portion of the conductive film 240a1f and a portion of the conductive film 240b1f are removed to expose the top surface of the insulator 285. As a result, these conductive films remain only in the opening, thereby forming the conductive body 240_1 (conductive body 240a1 and conductive body 240b1) whose top surface is flat ( Fig. 11B ). Note that sometimes a portion of the top surface of the insulator 285 is removed due to the CMP process.
[0467] In this way, the conductor 240 electrically connected to the conductor 209 and the conductor 242a can be manufactured.
[0468] The insulators 285, 283, 282, 280, 275, and 271b are processed by photolithography to form an opening ( Fig. 11C ).
[0469] The width of the opening provided in this process is preferably micro. For example, the width of the opening is preferably less than 200nm, less than 100nm, less than 60nm, less than 50nm, less than 40nm, less than 30nm, less than 20nm, or less than 10nm and more than 1nm or more than 5nm. Thus, in order to form a micro opening, it is preferred to use a photolithography method using short-wavelength light such as EUV light or an electron beam. In addition, when viewed from above, the above-mentioned opening can be a circular shape, a roughly circular shape such as an ellipse, a polygonal shape such as a quadrangle, or a polygonal shape such as a quadrangle with an arc at the corner.
[0470] Since the aspect ratio of the opening provided in this step is large, it is preferable to process a part of the insulator 285, a part of the insulator 283, a part of the insulator 282, a part of the insulator 280, a part of the insulator 275, and a part of the insulator 271b by anisotropic etching. In particular, processing by dry etching is suitable for micro-processing and is therefore preferred. In addition, the processing may be performed under different conditions.
[0471] Next, a conductive film 153A ( Fig. 12A ). The conductive film 153A is preferably formed in contact with the side and bottom surfaces of the opening. Therefore, the conductive film 153A is preferably deposited using a deposition method with good coverage such as an ALD method or a CVD method. For example, titanium nitride or tantalum nitride is preferably deposited using an ALD method or a CVD method.
[0472] Next, a resist mask is provided on the conductive film 153A, and the conductive film 153A is processed by photolithography to form the conductor 153 ( Fig. 12B ). Thus, a portion of the conductor 153 is formed inside the opening, and another portion is in contact with a portion of the top surface of the insulator 282.
[0473] Alternatively, the conductive film 153A may be processed by a CMP method. In this case, the conductive film 153A may be processed into a shape in which the uppermost portion of the conductive body 153 is substantially aligned with the top surface of the insulator 282 .
[0474] Next, an insulating film 154A ( Fig. 12C ). The insulating film 154A is preferably formed in contact with the conductor 153 provided inside the opening. Therefore, the insulating film 154A is preferably deposited using a deposition method having good coverage such as ALD or CVD. The insulating film 154A is preferably formed using the above-mentioned high-k material.
[0475] Next, a conductive film 160A to become the conductor 160a and a conductive film 160B to become the conductor 160b are sequentially deposited ( Fig. 12C ). The conductive film 160A is preferably formed in contact with the insulating film 154A provided inside the opening, and the conductive film 160B is preferably formed in an embedded manner in the opening. Therefore, the conductive film 160A and the conductive film 160B are preferably deposited by a deposition method with good coverage such as the ALD method or the CVD method. For example, it is preferable to deposit titanium nitride as the conductive film 160A using the ALD method or the CVD method, and to deposit tungsten as the conductive film 160B using the CVD method.
[0476] Note that in the case where the conductive film 160B is deposited by CVD, Fig. 12C As shown in FIG. 1 , the average surface roughness of the top surface of the conductive film 160B sometimes becomes larger. Fig.13A As shown, the conductive film 160B is preferably planarized using a CMP method.
[0477] Next, the insulating film 154A, the conductive film 160A, and the conductive film 160B are processed by photolithography to form the insulator 154, the conductor 160a, the conductor 160b, the insulator 263, the conductor 261a, and the conductor 261b ( Fig. 13B ). In this case, it is preferable to form the insulator 154, the conductor 160a and the conductor 160b in such a manner as to cover the side end of the conductor 153. By adopting such a structure, the conductor 160 and the conductor 153 can be separated by the insulator 154, and the short circuit between the conductor 160 and the conductor 153 can be suppressed.
[0478] As described above, since the lower layer conductor 160 (that is, Fig. 13B The upper electrodes of the capacitors 101a and 101b shown in the figure) and the upper conductor 261 (that is, Fig.14 In the back gate electrodes of the transistors 201a and 201b shown in the figure, the conductor 160 of the lower layer has the same material as the conductor 261 of the upper layer. In addition, since the insulator 154 of the lower layer and the insulator 263 of the upper layer are formed from the insulating film 154A, the insulator 154 of the lower layer has the same material as the insulator 263 of the upper layer.
[0479] As described above, by simultaneously forming the lower conductor 160 and the insulator 154 and the upper conductor 261 and the insulator 263 , the number of manufacturing steps of the semiconductor device according to this embodiment can be reduced, thereby improving the productivity of the semiconductor device.
[0480] In the above, an example of processing the insulating film 154A is shown, but the present invention is not limited to this. In addition, it is also possible to have a structure in which only the conductive film 160A and the conductive film 160B are processed without processing the insulating film 154A and leaving it. In this way, the processing steps of the insulator 154 can be reduced, so that the productivity can be improved.
[0481] In the above description, the upper electrode (conductor 160) of the capacitor 101a and the second gate electrode (conductor 261) of the transistor 201a are provided separately, but the present invention is not limited to this. Figure 2B As shown, only the insulator 154, the conductor 160a, and the conductor 160b can be formed from the insulating film 154A, the conductive film 160A, and the conductive film 160B. In this case, the conductor 160 has a structure that serves as both the upper electrode of the capacitor 101a and the second gate electrode of the transistor 201a.
[0482] Through the above steps, capacitors 101a and 101b can be formed.
[0483] Then, it is preferred to provide an insulator 284 embedded between the adjacent conductors 160 and 261 ( Fig. 13B ) In addition, it is preferable to planarize the insulator 284 by a CMP method.
[0484] Then, by repeatedly forming the above-mentioned insulator 222 ( Figure 7B ) to the manufacture of capacitors 101a and 101b ( Fig. 13B ) process, the layers above the second layer 11_2 can be manufactured. For example, Fig.14 FIG. 2 shows an example of a cross-sectional structure when the formation of the insulator 285 of the second layer 11_2 is completed. Fig.14 As shown, according to Fig. 13B The conductor 261 formed in the step is arranged to overlap with the first gate electrodes of the transistors 201a and 201b and is used as the second gate electrodes of the transistors 201a and 201b.
[0485] Through the above process, it is possible to produce Figure 1 The semiconductor device shown.
[0486] The semiconductor device of this embodiment includes an OS transistor. The off-state current of the OS transistor is small, so a semiconductor device or a storage device with low power consumption can be realized. In addition, since the frequency characteristics of the OS transistor are high, a semiconductor device or a storage device with a fast operating speed can be realized. In addition, by using an OS transistor, a semiconductor device with good electrical characteristics, a semiconductor device with small uneven electrical characteristics of the transistor, a semiconductor device with large on-state current, and a semiconductor device or a storage device with high reliability can be realized.
[0487] Furthermore, the conductor 240 in the semiconductor device of this embodiment has a stacked-layer structure of a plurality of conductors, and thus the manufacturing yield can be improved compared to the case of using a single conductor.
[0488] This embodiment mode can be appropriately combined with other embodiment modes. In addition, in this specification, when a plurality of configuration examples are shown in one embodiment mode, the configuration examples can be appropriately combined.
[0489] (Implementation Method 2)
[0490] In this embodiment, refer to Fig.15 A storage device according to one embodiment of the present invention is described below through FIG. 21 .
[0491] In this embodiment mode, a structural example of a memory device using the semiconductor device described in the above embodiment mode as a memory cell is described. In this embodiment mode, a structural example of a memory device is described in which a layer including a functional circuit having a function of amplifying and outputting a data potential held in the memory cell is provided between layers including stacked memory cells.
[0492] [Configuration Example of Storage Device]
[0493] Fig.15 This is a block diagram showing a storage device according to one embodiment of the present invention.
[0494] Fig.15 The memory device 300 shown includes a driving circuit 21 and a memory array 20. The memory array 20 includes a plurality of memory cells 10 and a functional layer 50 having a plurality of functional circuits 51.
[0495] Fig.15 The example in which the memory array 20 includes a plurality of memory cells 10 arranged in a matrix of m rows and n columns (m and n are integers greater than or equal to 2) is shown. Fig.15 An example is shown in which a functional circuit 51 is provided for each wiring BL serving as a bit line, and an example is also shown in which the functional layer 50 includes a plurality of functional circuits 51 provided corresponding to n wirings BL.
[0496] exist Fig.15 , the 1st row and 1st column storage cell 10 is represented as storage cell 10[1, 1], and the mth row and nth column storage cell 10 is represented as storage cell 10[m, n]. In addition, in the present embodiment, etc., sometimes "row i" is written to represent an arbitrary row. In addition, sometimes "column j" is written to represent an arbitrary column. Therefore, i is an integer greater than 1 and less than m, and j is an integer greater than 1 and less than n. In addition, in the present embodiment, etc., the i-th row and j-th column storage cell 10 is represented as storage cell 10[i, j]. Note that in the present embodiment, etc., when expressed as "i+α" (α is a positive integer or a negative integer), "i+α" is not less than 1 and not greater than m. Similarly, when expressed as "j+α", "j+α" is not less than 1 and not greater than n.
[0497] In addition, the memory array 20 includes m wirings WL extending in the row direction, m wirings PL extending in the row direction, and n wirings BL extending in the column direction. In the present embodiment, etc., the first (1st row) wiring WL is represented as wiring WL[1], and the mth (mth row) wiring WL is represented as wiring WL[m]. Similarly, the first (1st row) wiring PL is represented as wiring PL[1], and the mth (mth row) wiring PL is represented as wiring PL[m]. Similarly, the first (1st column) wiring BL is represented as wiring BL[1], and the nth (nth column) wiring BL is represented as wiring BL[n].
[0498] The plurality of memory cells 10 arranged in the i-th row are electrically connected to the i-th row wiring WL (wiring WL[i]) and the i-th row wiring PL (wiring PL[i]). The plurality of memory cells 10 arranged in the j-th column are electrically connected to the j-th column wiring BL (wiring BL[j]).
[0499] The memory array 20 may use DOSRAM (registered trademark) (Dynamic Oxide Semiconductor Random Access Memory). DOSRAM is a RAM including 1T (transistor) 1C (capacitor) type memory cells, and is a memory in which the access transistor is an OS transistor. In the off state, the current flowing between the source and the drain of the OS transistor, that is, the leakage current is extremely small. In DOSRAM, by turning off the access transistor (making it non-conductive), the charge according to the data held in the capacitor can be maintained for a long time. Therefore, compared with a DRAM composed of a transistor (Si transistor) containing silicon in the channel formation region, the refresh operation frequency of the DOSRAM can be lower. As a result, low power consumption can be achieved.
[0500] In addition, as described in Embodiment Mode 1 and the like, by stacking OS transistors, the memory cell 10 can be stacked. Fig.15 In the memory array 20 shown, a plurality of memory arrays 20[1] to 20[m] may be stacked. By arranging the memory arrays 20[1] to 20[m] included in the memory array 20 in a direction perpendicular to the substrate surface on which the drive circuit 21 is disposed, the memory density of the memory cell 10 may be increased. In addition, the memory array 20 may be manufactured repeatedly using the same manufacturing process in the vertical direction. The memory device 300 may reduce the manufacturing cost of the memory array 20.
[0501] Wiring BL is used as a bit line for writing and reading data. Wiring WL is used as a word line for controlling the opening or closing (conduction state or non-conduction state) of the access transistor used as a switch. Wiring PL is used as a constant potential line connected to the capacitor. In addition, wiring CL (not shown) can be separately provided as a wiring for transmitting the back gate potential to the back gate of the OS transistor of the access transistor. In addition, a structure in which wiring PL also serves as a transmission back gate potential can also be adopted.
[0502] The memory cells 10 included in the memory arrays 20[1] to 20[m] are connected to the functional circuit 51 through the wiring BL. The wiring BL can be arranged in a direction perpendicular to the surface of the substrate on which the driving circuit 21 is provided. By arranging the wiring BL extending from the memory cells 10 included in the memory arrays 20[1] to 20[m] in a direction perpendicular to the surface of the substrate, the length of the wiring between the memory array 20 and the functional circuit 51 can be shortened. Therefore, since the signal transmission distance between the two circuits connected to the bit line can be shortened and the resistance and parasitic capacitance of the bit line can be greatly reduced, the power consumption and signal delay can be reduced. In addition, the operation can be performed even if the capacitance of the capacitor included in the memory cell 10 is reduced.
[0503] The functional circuit 51 has a function of amplifying the data potential held in the memory cell 10 and outputting it to the sense amplifier 46 included in the drive circuit 21 through the wiring GBL (not shown) described later. By adopting this structure, a small potential difference of the wiring BL can be amplified when reading data. The wiring GBL can be arranged in a direction perpendicular to the surface of the substrate on which the drive circuit 21 is provided, similarly to the wiring BL. By arranging the wiring BL and the wiring GBL extending from the memory cell 10 included in the memory array 20[1] to 20[m] in a direction perpendicular to the substrate surface, the length of the wiring between the functional circuit 51 and the sense amplifier 46 can be shortened. Therefore, since the signal transmission distance between the two circuits connected to the wiring GBL can be shortened and the resistance and parasitic capacitance of the wiring GBL can be greatly reduced, power consumption and signal delay can be reduced.
[0504] Furthermore, the wiring BL is provided in such a manner as to be in contact with the semiconductor layer of the transistor included in the memory cell 10. Alternatively, the wiring BL is provided in such a manner as to be in contact with a region of the semiconductor layer of the transistor included in the memory cell 10 that is used as a source or a drain. Alternatively, the wiring BL is provided in such a manner as to be in contact with a conductor that is in contact with a region of the semiconductor layer of the transistor included in the memory cell 10 that is used as a source or a drain. That is, the wiring BL can be said to be a wiring that electrically connects one of the source and the drain of the transistor included in the memory cell 10 in each layer of the memory array 20 to the functional circuit 51 in the vertical direction.
[0505] The memory array 20 can be overlapped on the drive circuit 21. By overlapping the drive circuit 21 and the memory array 20, the signal transmission distance between the drive circuit 21 and the memory array 20 can be shortened. Therefore, the resistance and parasitic capacitance between the drive circuit 21 and the memory array 20 are reduced, and the power consumption and signal delay can be reduced. In addition, the memory device 300 can be miniaturized.
[0506] By forming the functional circuit 51 with OS transistors similarly to the transistors included in the memory cell 10 of the DOSRAM, the functional circuit 51 can be freely arranged on a circuit using Si transistors similarly to the memory arrays 20[1] to 20[m], thereby making it easy to integrate. By adopting a structure in which the functional circuit 51 amplifies the signal, the circuits such as the sense amplifier 46 of the subsequent circuit can be miniaturized, thereby miniaturizing the memory device 300.
[0507] The drive circuit 21 includes a PSW 22 (power switch), a PSW 23 and a peripheral circuit 31. The peripheral circuit 31 includes a peripheral circuit 41, a control circuit 32 (control circuit) and a voltage generation circuit 33.
[0508] In the storage device 300, each circuit, each signal and each voltage can be appropriately selected as needed. Alternatively, other circuits or other signals can be added. Signals BW, CE, GW, CLK, WAKE, ADDR, WDA, PON1 and PON2 are signals input from the outside, and signal RDA is a signal output to the outside. Signal CLK is a clock signal.
[0509] In addition, the signal BW, the signal CE and the signal GW are control signals. The signal CE is a chip enable signal, the signal GW is a global write enable signal, and the signal BW is a byte write enable signal. The signal ADDR is an address signal. The signal WDA is write data, and the signal RDA is read data. The signals PON1 and PON2 are power gating control signals. In addition, the signals PON1 and PON2 can also be generated in the control circuit 32.
[0510] The control circuit 32 is a logic circuit that has the function of controlling the overall operation of the storage device 300. For example, the control circuit performs a logic operation on the signal CE, the signal GW, and the signal BW to determine the operation mode (for example, writing operation, reading operation) of the storage device 300. Alternatively, the control circuit 32 generates a control signal for the peripheral circuit 41 to execute the above operation mode.
[0511] The voltage generating circuit 33 has a function of generating a negative voltage. The signal WAKE has a function of controlling the input of the signal CLK to the voltage generating circuit 33. For example, when the signal WAKE is applied with an H level signal, the signal CLK is input to the voltage generating circuit 33, and the voltage generating circuit 33 generates a negative voltage.
[0512] The peripheral circuit 41 is a circuit for writing and reading data to the memory cell 10. In addition, the peripheral circuit 41 is a circuit for outputting various signals for controlling the functional circuit 51. The peripheral circuit 41 includes a row decoder 42 (RowDecoder), a column decoder 44 (ColumnDecoder), a row driver 43 (Row Driver), a column driver 45 (ColumnDriver), an input circuit 47 (Input Cir.), an output circuit 48 (Output Cir.), and a sense amplifier 46 (SenseAmplifier).
[0513] The row decoder 42 and the column decoder 44 have the function of decoding the signal ADDR. The row decoder 42 is a circuit for specifying a row to be accessed, and the column decoder 44 is a circuit for specifying a column to be accessed. The row driver 43 has the function of selecting the wiring WL specified by the row decoder 42. The column driver 45 has the following functions: a function of writing data to the memory cell 10; a function of reading data from the memory cell 10; a function of holding the read data, etc.
[0514] The input circuit 47 has a function of holding the signal WDA. The data held in the input circuit 47 is output to the column driver 45. The output data of the input circuit 47 is the data (Din) written to the memory cell 10. The data (Dout) read from the memory cell 10 by the column driver 45 is output to the output circuit 48. The output circuit 48 has a function of holding Dout. In addition, the output circuit 48 has a function of outputting Dout to the outside of the memory device 300. The data output from the output circuit 48 is the signal RDA.
[0515] PSW22 has a function of controlling the supply of VDD to the peripheral circuit 31. PSW23 has a function of controlling the supply of VHM to the row driver 43. Here, the high power supply voltage of the memory device 300 is VDD, and the low power supply voltage is GND (ground potential). In addition, VHM is a high power supply voltage for making the word line high, which is higher than VDD. The on / off of PSW22 is controlled by the signal PON1, and the on / off of PSW23 is controlled by the signal PON2. Fig.15 In the embodiment, the number of power domains to which VDD is supplied in the peripheral circuit 31 is one, but it may be more than one. In this case, a power switch may be provided for each power domain.
[0516] The memory array 20 includes memory arrays 20[1] to 20[m] (m is an integer greater than or equal to 2) and a functional layer 50. A plurality of memory arrays 20 may be stacked on the drive circuit 21. By stacking a plurality of memory arrays 20, the memory density of the memory cell 10 may be increased. Fig.16A 1 is a perspective view of a storage device 300 in which a functional layer 50 and five-layer (m=5) memory arrays 20 [ 1 ] to 20 [ 5 ] are stacked on a drive circuit 21 .
[0517] exist Fig.16A In the example, the storage array 20 disposed in the first layer is referred to as the storage array 20[1], the storage array 20 disposed in the second layer is referred to as the storage array 20[2], and the storage array 20 disposed in the fifth layer is referred to as the storage array 20[5]. Fig.16A The wiring WL, wiring PL, and wiring CL extending in the X direction and the wiring BL extending in the Z direction (a direction perpendicular to the substrate surface on which the driver circuit is provided) are shown. Note that in order to make the drawings easier to understand, description of a part of the wiring WL and wiring PL included in each of the memory arrays 20 is omitted.
[0518] Fig. 16B Show instructions Fig.16A FIG. 1 is a schematic diagram of a structural example of a functional circuit 51 connected to the wiring BL and a memory cell 10 included in the memory array 20 [1] to 20 [5] connected to the wiring BL. Fig. 16B The wiring GBL provided between the functional circuit 51 and the driving circuit 21 is shown. In addition, a structure that electrically connects one wiring BL to a plurality of memory cells (memory cells 10) is also referred to as a "memory string." Note that in the drawings, the wiring GBL is sometimes shown with a thick line for improved visibility.
[0519] Fig. 16B An example of a circuit structure of a memory cell 10 connected to a wiring BL is shown. The memory cell 10 includes a transistor 11 and a capacitor 12. Regarding the transistor 11, the capacitor 12, and each wiring (wiring BL, wiring WL, etc.), for example, wiring BL[1] and wiring WL[1] are sometimes referred to as wiring BL and wiring WL, etc. For an example of a cross-sectional structure of a memory element 10 corresponding to this circuit structure, refer to Embodiment 1.
[0520] The transistor 11 corresponds to the transistor 201a or the transistor 201b described in Embodiment 1. The capacitor 12 corresponds to the capacitor 101a or the capacitor 101b described in Embodiment 1. The wiring BL corresponds to the conductor 240 described in Embodiment 1.
[0521] As described in Embodiment 1, in the semiconductor device of one embodiment of the present invention, the wiring BL (conductor 240) is in direct contact with at least one of the top surface, side surface, and bottom surface of the conductor 242a including the region used as one of the source electrode and the drain electrode of the transistor 11 (transistor 201a). As a result, it is not necessary to separately provide an electrode for connection, so that the occupied area of the memory array 20 can be reduced. In addition, the integration degree of the memory element 10 is increased, and the storage capacity of the memory device 300 can be increased.
[0522] In the memory cell 10, one of the source and the drain of the transistor 11 is connected to the wiring BL. The other of the source and the drain of the transistor 11 is connected to one electrode of the capacitor 12. The other electrode of the capacitor 12 is connected to the wiring PL. The gate of the transistor 11 is connected to the wiring WL. The back gate of the transistor 11 is connected to the wiring CL.
[0523] Wiring PL is a wiring for supplying a constant potential for maintaining the potential of capacitor 12. Wiring CL is a constant potential for controlling the threshold voltage of transistor 11. Wiring PL and wiring CL may also be at the same potential. In this case, by connecting the two wirings, the number of wirings connected to memory cell 10 can be reduced.
[0524] Fig. 16B The wiring GBL shown is provided so as to electrically connect the driving circuit 21 and the functional layer 50 . Fig.17A FIG. 3 is a schematic diagram of a memory device 300 with a functional circuit 51 and memory arrays 20 [ 1 ] to 20 [ m ] as a repeating unit 70 . Fig.17A One wiring GBL is shown in the figure, but the wiring GBL may be appropriately provided according to the number of functional circuits 51 in the functional layer 50 .
[0525] Furthermore, the wiring GBL is provided in such a manner as to be in contact with the semiconductor layer of the transistor included in the functional circuit 51. Alternatively, the wiring GBL is provided in such a manner as to be in contact with a region of the semiconductor layer of the transistor included in the functional circuit 51 that is used as a source or a drain. Alternatively, the wiring GBL is provided in such a manner as to be in contact with a conductor that is in contact with a region of the semiconductor layer of the transistor included in the functional circuit 51 that is used as a source or a drain. That is, the wiring GBL can be said to be a wiring that electrically connects one of the source and the drain of the transistor included in the functional circuit 51 of the functional layer 50 to the drive circuit 21 in the vertical direction.
[0526] Alternatively, a structure may be provided in which a repeating unit 70 including a functional circuit 51 and memory arrays 20[1] to 20[m] is stacked. Fig. 17BThe repeating units 70 [1] to 70 [p] (p is an integer greater than or equal to 2) may be included. The wiring GBL is connected to the functional layer 50 included in the repeating unit 70. The wiring GBL may be appropriately provided according to the number of the functional circuits 51.
[0527] In one embodiment of the present invention, while stacking OS transistors, wiring used as a bit line is arranged in a direction perpendicular to the substrate surface provided with the driver circuit 21. By arranging the wiring used as the bit line extending from the memory array 20 in the vertical direction of the substrate surface, the length of the wiring between the memory array 20 and the driver circuit 21 can be shortened. Therefore, the parasitic capacitance of the bit line can be greatly reduced.
[0528] In addition, one embodiment of the present invention includes a functional layer 50 in a layer provided with the memory array 20, and the functional layer 50 includes a functional circuit 51 having a function of amplifying the data potential held in the memory cell 10 and outputting it. By adopting this structure, a small potential difference of the wiring BL used as a bit line when reading data can be amplified to drive the sense amplifier 46 included in the drive circuit 21. Since the circuit such as the sense amplifier can be miniaturized, the memory device 300 can be miniaturized. In addition, the operation can be performed even if the capacitance of the capacitor 12 included in the memory cell 10 is reduced.
[0529] [Configuration Example of Memory Array 20 and Functional Circuit 51]
[0530] Reference Fig.18 illustrate Figure 15 to Figure 1 7 and the structural examples of the functional circuit 51 and the structural examples of the sense amplifier 46 included in the memory array 20 and the driver circuit 21. Fig.18 The driving circuit 21 is shown, and the driving circuit 21 is connected to the wiring GBL (wiring GBL_A, wiring GBL_B), and the wiring GBL is connected to the functional circuit 51 (functional circuit 51_A, functional circuit 51_B), and the functional circuit 51 is connected to the memory cell 10 (memory cell 10_A, memory cell 10_B) connected to the different wiring BL (wiring BL_A, wiring BL_B). Fig.18 The driving circuit 21 shown in the figure shows a precharge circuit 71_A, a precharge circuit 71_B, a switch circuit 72_A, a switch circuit 72_B, and a write / read circuit 73 in addition to the sense amplifier 46 .
[0531] Transistors 52_a, 52_b, 53_a, 53_b, 54_a, 54_b, 55_a, and 55_b are shown as the functional circuits 51_A and 51_B. Fig.18The transistors 52_a, 52_b, 53_a, 53_b, 54_a, 54_b, 55_a, and 55_b shown are OS transistors like the transistor 11 included in the memory cell 10. The functional layer 50 including the functional circuit 51 can be stacked like the memory arrays 20[1] to 20[m].
[0532] Wiring BL_A is connected to the gate of transistor 52_a, and BL_B is connected to the gate of 52_b. Wiring GBL_A is connected to one of the source and drain of transistors 53_a and 54_a. GBL_B is connected to one of the source and drain of transistors 53_b and 54_b. Like wiring BL_A and BL_B, wiring GBL_A and GBL_B are arranged in the vertical direction and connected to the transistors included in the driving circuit 21. Fig.18 As shown, the gates of the transistors 53_a, 53_b, 54_a, 54_b, 55_a, and 55_b are supplied with the selection signal MUX, the control signal WE, or the control signal RE.
[0533] constitute Fig.18 The transistors 81_1 to 81_6 and 82_1 to 82_4 of the sense amplifier 46, the precharge circuit 71_A and the precharge circuit 71_B shown are composed of Si transistors. The switches 83_A to 83_D constituting the switch circuit 72_A and the switch circuit 72_B can also be composed of Si transistors. One of the source and drain of the transistors 53_a, 53_b, 54_a, and 54_b is connected to the transistor or switch constituting the precharge circuit 71_A, the precharge circuit 71_B, the sense amplifier 46, and the switch circuit 72_A.
[0534] Precharge circuit 71_A includes n-channel transistors 81_1 to 81_3 and precharges wiring BL_A and wiring BL_B to an intermediate potential VPC corresponding to VDD / 2 between the high power supply potential (VDD) and the second power supply potential (VSS) according to a precharge signal supplied to precharge line PCL1.
[0535] The precharge circuit 71_B includes n-channel transistors 81_4 to 81_6 and precharges the wirings GBL_A and GBL_B to an intermediate potential VPC corresponding to a potential VDD / 2 between VDD and VSS in accordance with a precharge signal supplied to the precharge line PCL2.
[0536] The sense amplifier 46 includes p-channel transistors 82_1 and 82_2 and n-channel transistors 82_3 and 82_4 connected to the wiring VHH or the wiring VLL. The wiring VHH or the wiring VLL is a wiring having a function of supplying VDD or VSS. The transistors 82_1 to 82_4 are transistors constituting an inverter loop. The potential of the wiring BL_A and the wiring BL_B precharged by selecting the memory cells 10_A and 10_B changes, and the potential of the wiring GBL_A and the wiring GBL_B is set to VDD or VSS according to the change. The potential of the wiring GBL_A and the wiring GBL_B can be output to the outside through the switch 83_C and the switch 83_D and the write-read circuit 73. The wiring BL_A and the wiring BL_B and the wiring GBL_A and the wiring GBL_B are equivalent to a bit line pair. The write-read circuit 73 is controlled to write a data signal according to the signal EN_data.
[0537] The switch circuit 72_A is a circuit for controlling the conduction state between the sense amplifier 46 and the wiring GBL_A and the wiring GBL_B. The switch circuit 72_A can be switched on or off by controlling the switching signal CSEL1. In the case where the switches 83_A and 83_B are n-channel transistors, they are turned on when the switching signal CSEL1 is at a high level, and are turned off when the switching signal CSEL1 is at a low level. The switch circuit 72_B is a circuit for controlling the conduction state between the write read circuit 73 and the bit line pair connected to the sense amplifier 46. The switch circuit 72_B can be switched on or off by controlling the switching signal CSEL2. The switches 83_C and 83_D can be the same as the switches 83_A and 83_B.
[0538] like Fig.18 As shown, the memory device 300 may have a structure in which the memory cell 10, the functional circuit 51, and the sense amplifier 46 are connected by the wiring BL and the wiring GBL arranged in the shortest vertical direction. Although the functional layer 50 including the transistor constituting the functional circuit 51 increases, the load of the wiring BL is reduced, so that the writing time can be shortened and the data can be easily read.
[0539] In addition, if Fig.18 As shown, each transistor included in the functional circuit 51_A, 51_B is controlled by the control signal WE, RE and the selection signal MUX. Each transistor can output the potential of the wiring BL to the driving circuit 21 through the wiring GBL according to the control signal and the selection signal. The functional circuits 51_A, 51_B can be used as a sense amplifier composed of OS transistors. By adopting this structure, a small potential difference of the wiring BL can be amplified during reading, and the sense amplifier 46 using Si transistors can be driven.
[0540] [Operation Example of Memory Cell 20, Functional Circuit 51, and Sense Amplifier 46]
[0541] exist Fig.19 Instructions are shown in Fig.18 The circuit diagram shown is a timing diagram of the operation. Fig.19 In the timing diagram shown, period T11 corresponds to the period of writing operation, period T12 corresponds to the period of precharging operation of wiring BL, period T13 corresponds to the period of precharging operation of wiring GBL, period T14 corresponds to the period of charge sharing operation, period T15 corresponds to the period of read standby operation, and period T16 corresponds to the period of reading operation.
[0542] In period T11, the potential of the wiring WL connected to the gate of the transistor 11 included in the memory cell 10 to which the data signal is to be written is set to a high level. At this time, the control signal WE and the signal EN_data are set to a high level, and the data signal is written to the memory cell through the wiring GBL and the wiring BL.
[0543] In the period T12, in order to precharge the wiring BL, the precharge line PCL1 is set to a high level while the control signal WE is set to a high level. The wiring BL is precharged to the precharge potential. In the period T12, it is preferable to set the wiring VHH or the wiring VLL that supplies the power supply voltage to the sense amplifier 46 to VDD / 2 to suppress the power consumption caused by the through current.
[0544] In period T13, in order to precharge the wiring GBL, the precharge line PCL2 is set to a high level. The wiring GBL is precharged to the precharge potential. In period T13, by setting the potentials of the wiring VHH and the wiring VLL to VDD, the wiring GBL with a large load can be precharged in a short time.
[0545] In the period T14, the potential of the wiring WL is set to a high level in order to perform charge sharing to balance the charge held in the memory cell 10 and the charge precharged to the wiring BL. In the period T14, it is preferable that the potential of the wiring VHH or the wiring VLL for supplying the power supply voltage to the sense amplifier 46 is set to VDD / 2 to suppress power consumption due to the through current.
[0546] In the period T15, the control signal RE and the selection signal MUX are set to high level. According to the potential of the wiring BL, a current flows through the transistor 52, and according to the amount of the current, the potential of the wiring GBL changes. By setting the switching signal CSEL1 to low level, the change of the potential of the wiring GBL is prevented from being affected by the sense amplifier 46. The wiring VHH or the wiring VLL is the same as the wiring VHH or the wiring VLL in the period T14.
[0547] In the period T16 , by setting the switching signal CSEL1 to a high level, the change in the potential of the wiring GBL is amplified by the bit line pair connected to the sense amplifier 46 , and the data signal written in the memory cell is read.
[0548] [Configuration example of functional circuit]
[0549] Next, refer to Fig. 20A , Fig. 20B and Fig.21A , Fig.21B A specific structural example of a functional circuit 51 used as a sense amplifier and composed of OS transistors included in the functional layer 50 will be described.
[0550] Fig. 20A Shows the equivalent of Fig.18 The functional circuit 51A is the functional circuit 51_A or 51_B shown. Fig. 20A The functional circuit 51A shown includes transistors 52 to 55. The transistors 52 to 55 can be respectively formed of OS transistors and are n-channel transistors.
[0551] The transistor 52 is a source follower transistor that amplifies the wiring GBL to a potential corresponding to the wiring BL during the reading of the data signal from the memory cell 10. The transistor 53 is a transistor used as a switch, in which the selection signal MUX is input to the gate and the on / off between the source and the drain is controlled according to the selection signal MUX. The transistor 54 is a transistor used as a switch, in which the control signal WE is input to the gate and the on / off between the source and the drain is controlled according to the control signal WE. The transistor 55 is a transistor used as a switch, in which the control signal RE is input to the gate and the on / off between the source and the drain is controlled according to the control signal RE. In addition, as an example, the ground potential GND as a fixed potential is applied to the source side of the transistor 55.
[0552] also, Fig. 20A The structure of the functional circuit 51A shown can be used Fig. 20B and Fig.21A , Fig.21B Deformation example shown. Fig. 20B The functional circuit 51B has a structure in which one of the source and the drain of the transistor 54 is connected to one of the source and the drain of the transistor 52 and is not connected to the wiring GBL. Fig.21A In the structure of the functional circuit 51C, the driving circuit 21 has the function of the transistor 53, and thus the transistor 53 is omitted. Fig.21B The transistor 55 is omitted in the structure of the functional circuit 51D.
[0553] In a semiconductor device of one embodiment of the present invention, an OS transistor with a very small off-state current is used as a transistor provided in a memory array 20. The OS transistor can be stacked on a substrate provided with a driving circuit 21 including Si transistors. Therefore, the same manufacturing process can be repeatedly used in the vertical direction for manufacturing, thereby achieving a reduction in manufacturing cost. In addition, in one embodiment of the present invention, the transistors constituting the memory cell 10 can also be arranged in the vertical direction instead of in the planar direction to increase the memory density, thereby achieving miniaturization of the memory device.
[0554] In addition, one embodiment of the present invention includes a functional layer 50 including a functional circuit 51. In the functional circuit, the wiring BL is connected to the gate of the transistor 52, so that the transistor 52 is used as an amplifier. By adopting this structure, a small potential difference of the wiring BL can be amplified during reading, and the sense amplifier 46 using Si transistors can be driven. The circuit such as the sense amplifier 46 using Si transistors can be miniaturized, so that the memory device can be miniaturized. In addition, even if the capacitance of the capacitor 12 included in the memory cell 10 is reduced, it can work.
[0555] This embodiment mode can be combined with other embodiment modes as appropriate.
[0556] (Implementation method 3)
[0557] In this embodiment, an example of a chip on which a memory device according to one embodiment of the present invention is mounted is described with reference to FIG. 22 .
[0558] exist Fig.22A and Fig. 22B A plurality of circuits (systems) are mounted on the illustrated chip 1200. The technology of integrating a plurality of circuits (systems) on one chip is sometimes referred to as a system on chip (SoC).
[0559] like Fig.22A As shown, the chip 1200 includes a CPU 1211, a GPU 1212, one or more simulation operation units 1213, one or more storage controllers 1214, one or more interfaces 1215, one or more network circuits 1216, and the like.
[0560] Bumps (not shown) are provided on the chip 1200. Fig. 22B As shown in FIG. 1 , the first surface of the package substrate 1201 is connected to the first surface of the package substrate 1201 . In addition, a plurality of bumps 1202 are provided on the back side of the first surface of the package substrate 1201 , and the bumps 1202 are connected to the motherboard 1203 .
[0561] In addition, a storage device such as DRAM 1221 and flash memory 1222 may be provided on the motherboard 1203. For example, the DOSRAM described in the above embodiment may be used for DRAM 1221. Thus, the DRAM 1221 can have low power consumption, high speed, and large capacity.
[0562] The CPU 1211 preferably has a plurality of CPU cores. In addition, the GPU 1212 preferably has a plurality of GPU cores. In addition, the CPU 1211 and the GPU 1212 may each have a memory for temporarily storing data. Alternatively, a memory commonly used by the CPU 1211 and the GPU 1212 may be provided on the chip 1200. The above-mentioned DOSRAM may be used for the memory. In addition, the GPU 1212 is suitable for parallel calculation of a plurality of data, which may be used for image processing or product-sum operations. By providing an image processing circuit or product-sum operation circuit using an OS transistor as the GPU 1212, image processing or product-sum operations may be performed with low power consumption.
[0563] In addition, since CPU1211 and GPU1212 are provided on the same chip, the wiring between CPU1211 and GPU1212 can be shortened, and data can be transferred from CPU1211 to GPU1212, data can be transferred between memories possessed by CPU1211 and GPU1212, and calculation results can be transferred from GPU1212 to CPU1211 after calculations in GPU1212 are completed at high speed.
[0564] The analog operation unit 1213 includes one or both of an A / D (analog / digital) conversion circuit and a D / A (digital / analog) conversion circuit. In addition, the analog operation unit 1213 may also include the above-mentioned product-sum operation circuit.
[0565] The memory controller 1214 has a circuit used as a controller of the DRAM 1221 and a circuit used as an interface of the flash memory 1222 .
[0566] The interface 1215 has an interface circuit with external connection devices such as a display device, a speaker, a microphone, an image capture device, a controller, etc. The controller includes a mouse, a keyboard, a game console controller, etc. As the above-mentioned interface, USB (Universal Serial Bus), HDMI (High-Definition Multimedia Interface) (registered trademark), etc. can be used.
[0567] The network circuit 1216 includes a network circuit such as a LAN (Local Area Network) and may also include a network security circuit.
[0568] The above circuits (systems) can be formed on the chip 1200 through the same manufacturing process. Therefore, even if the number of circuits required for the chip 1200 increases, there is no need to increase the number of manufacturing processes, and the chip 1200 can be manufactured at a low cost.
[0569] The package substrate 1201 provided with the chip 1200 having the GPU 1212 and the motherboard 1203 provided with the DRAM 1221 and the flash memory 1222 may be referred to as a GPU module 1204 .
[0570] The GPU module 1204 can reduce its size due to having the chip 1200 using SoC technology. In addition, the GPU module 1204 is suitable for portable electronic devices such as smartphones, tablet terminals, laptop personal computers, and portable (portable) game consoles due to its high image processing capabilities. In addition, by utilizing the product-sum operation circuit using the GPU 1212, methods such as deep neural networks (DNN), convolutional neural networks (CNN), recurrent neural networks (RNN), autoencoders, deep Boltzmann machines (DBM), and deep belief networks (DBN) can be performed, thereby using the chip 1200 as an AI chip, or the GPU module 1204 can be used as an AI system module.
[0571] This embodiment mode can be combined with other embodiment modes as appropriate.
[0572] (Implementation 4)
[0573] This embodiment shows an example of an electronic component in which a storage device according to one embodiment of the present invention is mounted.
[0574] [Electronic components]
[0575] Fig.23A The electronic component 700 and a substrate (circuit board 704 ) on which the electronic component 700 is mounted are shown in a perspective view. Fig.23A The electronic component 700 shown includes the storage device 300 of one embodiment of the present invention in a mold 711. Fig.23A 700 is omitted to show the inside. The electronic component 700 includes a land 712 on the outside of the mold 711. The land 712 is electrically connected to the electrode pad 713, and the electrode pad 713 is electrically connected to the storage device 300 through the lead 714. The electronic component 700 is mounted on a printed circuit board 702, for example. By combining a plurality of electronic components and electrically connecting them on the printed circuit board 702, a circuit board 704 is completed.
[0576] As shown in the above embodiment, the memory device 300 includes a driving circuit 21 and a memory array 20 .
[0577] Fig. 23B The electronic component 730 is a perspective view. The electronic component 730 is an example of a SiP (System in Package) or an MCM (Multi Chip Module). In the electronic component 730, an interposer 731 is provided on a package substrate 732 (printed circuit board), and a semiconductor device 735 and a plurality of storage devices 300 are provided on the interposer 731.
[0578] The electronic component 730 shows an example in which the storage device 300 is used as a high bandwidth memory (HBM). In addition, the semiconductor device 735 can use an integrated circuit (semiconductor device) such as a CPU, a GPU, or an FPGA.
[0579] The package substrate 732 may be, for example, a ceramic substrate, a plastic substrate, or a glass epoxy substrate. The interposer 731 may be, for example, a silicon interposer or a resin interposer.
[0580] The plug board 731 has a plurality of wirings and has the function of electrically connecting a plurality of integrated circuits with different terminal spacings. The plurality of wirings are arranged in a single layer or in multiple layers. In addition, the plug board 731 has the function of electrically connecting the integrated circuit arranged on the plug board 731 to the electrode arranged on the package substrate 732. Therefore, the plug board is sometimes also referred to as a "rewiring substrate" or "intermediate substrate". In addition, a through electrode is sometimes arranged in the plug board 731, and the integrated circuit is electrically connected to the package substrate 732 through the through electrode. In addition, when a silicon plug board is used, TSV (Through Silicon Via: silicon through hole) can also be used as a through electrode.
[0581] A silicon interposer is preferably used as the interposer 731. Since a silicon interposer does not need to be provided with active elements, it can be manufactured at a lower cost than an integrated circuit. On the other hand, the wiring formation of the silicon interposer can be performed in a semiconductor process, so it is easy to form fine wiring that is difficult to form when using a resin interposer.
[0582] In HBM, many wirings need to be connected to achieve a wide memory bandwidth. For this reason, it is required that fine wirings can be formed at a high density on the interposer on which the HBM is mounted. Therefore, a silicon interposer is preferably used as the interposer on which the HBM is mounted.
[0583] In addition, in SiP, MCM, etc. using a silicon interposer, the reliability degradation caused by the difference in expansion coefficient between the integrated circuit and the interposer is not likely to occur. In addition, since the surface flatness of the silicon interposer is high, poor connection between the integrated circuit disposed on the silicon interposer and the silicon interposer is not likely to occur. It is particularly preferred to use the silicon interposer for 2.5D packaging (2.5D mounting) in which a plurality of integrated circuits are arranged horizontally and disposed on the interposer.
[0584] In addition, a heat sink (heat sink plate) may be provided so as to overlap with the electronic component 730. When a heat sink is provided, it is preferable to make the height of the integrated circuit provided on the interposer 731 consistent. For example, in the electronic component 730 shown in this embodiment, it is preferable to make the height of the storage device 300 and the semiconductor device 735 consistent.
[0585] In order to mount the electronic component 730 on another substrate, an electrode 733 may be provided on the bottom of the package substrate 732 . Fig. 23B An example of forming the electrode 733 using solder balls is shown. By arranging solder balls in a matrix on the bottom of the package substrate 732, BGA (Ball Grid Array) mounting can be achieved. Alternatively, the electrode 733 can be formed using conductive needles. By arranging conductive needles in a matrix on the bottom of the package substrate 732, PGA (Pin Grid Array) mounting can be achieved.
[0586] The electronic component 730 can be mounted on other substrates by various mounting methods, not limited to BGA and PGA. As mounting methods, for example, SPGA (Staggered Pin Grid Array), LGA (Land Grid Array), QFP (Quad Flat Package), QFJ (Quad Flat J-leaded package) and QFN (Quad Flat Non-leaded package) can be cited.
[0587] This embodiment mode can be combined with other embodiment modes as appropriate.
[0588] (Implementation 5)
[0589] In this embodiment, an application example of a storage device which is one embodiment of the present invention will be described.
[0590] The storage device of one embodiment of the present invention can be applied to the storage device of various electronic devices (for example, information terminals, computers, smart phones, e-book reader terminals, digital still cameras, video cameras, video playback devices, navigation systems, and game consoles). In addition, it can be used for image sensors, IoT (Internet of Things), and medical equipment. Thus, power saving of electronic devices can be achieved. Note that here, computers include tablet computers, notebook computers, desktop computers, and large computers such as server systems.
[0591] An example of an electronic device including a storage device according to one embodiment of the present invention is described. Note that FIG. 24A to FIG. 24J , FIG. 25A to FIG. 25E The electronic component 700 or the electronic component 730 having the storage device described in the above embodiment is shown as being included in each electronic device.
[0592] [Mobile phone]
[0593] Fig.24A The information terminal 5500 shown is a mobile phone (smartphone) which is one of the information terminals. The information terminal 5500 includes a housing 5510 and a display portion 5511 . The display portion 5511 has a touch panel as an input interface, and the housing 5510 is provided with buttons.
[0594] By applying the storage device of one embodiment of the present invention to the information terminal 5500, it is possible to store documents temporarily generated when a program is executed (for example, a cache when a web browser is used).
[0595] [Wearable terminal]
[0596] Fig. 24B An information terminal 5900 as an example of a wearable terminal is shown. The information terminal 5900 includes a housing 5901, a display portion 5902, an operation switch 5903, an operation switch 5904, a strap 5905, and the like.
[0597] Similar to the above-mentioned information terminal 5500, by applying the storage device of one embodiment of the present invention to a wearable terminal, it is possible to store documents temporarily generated when a program is executed.
[0598] [Information Terminal]
[0599] Fig.24C 1 shows a desktop information terminal 5300. The desktop information terminal 5300 includes an information terminal body 5301, a display portion 5302, and a keyboard 5303.
[0600] Similar to the above-described information terminal 5500 , by applying the storage device of one embodiment of the present invention to the desktop information terminal 5300 , it is possible to store a document temporarily generated when a program is executed.
[0601] exist FIG. 24A to FIG. 24C As the electronic devices, a smartphone, a wearable terminal, and a desktop information terminal are described, but as other information terminals, for example, a PDA (Personal Digital Assistant), a notebook information terminal, and a workstation can be cited.
[0602] [Electrical products]
[0603] Fig.24D An electric refrigerator-freezer 5800 is shown as an example of an electric appliance. The electric refrigerator-freezer 5800 includes a housing 5801, a refrigerator door 5802, a freezer door 5803, etc. For example, the electric refrigerator-freezer 5800 is an electric refrigerator-freezer that supports IoT (Internet of Things).
[0604] The storage device of one embodiment of the present invention can be applied to the electric refrigerator-freezer 5800. By using the Internet or the like, the electric refrigerator-freezer 5800 can send information such as food stored in the electric refrigerator-freezer 5800 or the expiration date of the food to an information terminal or the like. The electric refrigerator-freezer 5800 can store a document temporarily generated when sending the information in the storage device of one embodiment of the present invention.
[0605] exist Fig.24D In the description, an electric refrigerator-freezer is described as an electrical appliance, but other electrical appliances include, for example, a vacuum cleaner, a microwave oven, an electric oven, an electric rice cooker, a water heater, an IH cooker, a water dispenser, a heating and cooling air conditioner including an air conditioner, a washing machine, a dryer, and audio-visual equipment.
[0606] [Game console]
[0607] Fig.24E A portable game machine 5200 as an example of a game machine is shown. The portable game machine 5200 includes a housing 5201, a display portion 5202, buttons 5203, and the like.
[0608] also, Fig.24F The following is a stationary game machine 7500 as an example of a game machine. The stationary game machine 7500 can be said to be a stationary game machine for home use. The stationary game machine 7500 includes a main body 7520 and a controller 7522. The main body 7520 can be connected to the controller 7522 wirelessly or by wire. Fig.24FAlthough not shown in the figure, the controller 7522 may include a display unit for displaying game images, a touch panel as an input interface other than buttons, a joystick, a rotating grip or a sliding grip, etc. In addition, the controller 7522 is not limited to Fig.24F The shape of the controller 7522 may be changed according to the type of game. For example, in shooting games such as FPS (First Person Shooter), a controller that imitates the shape of a gun may be used as a trigger button. In addition, for example, in music games, a controller that imitates the shape of a musical instrument or a musical device may be used. Furthermore, a fixed game console may be provided with one or more of a camera, a depth sensor, and a microphone, and may be operated by gestures or voice of the game player instead of using a controller.
[0609] In addition, the images of the above-mentioned game machine can be output by a display device such as a television device, a personal computer monitor, a game monitor, or a head-mounted display.
[0610] The storage device of one embodiment of the present invention can be used in the portable game machine 5200 or the stationary game machine 7500 to reduce power consumption. In addition, the heat generated by the circuit can be reduced by reducing power consumption, thereby reducing the impact of heat on the circuit itself, peripheral circuits and modules.
[0611] Furthermore, by using the storage device of one embodiment of the present invention in the portable game machine 5200 or the stationary game machine 7500, it is possible to store calculation files temporarily generated when a game is executed.
[0612] exist Fig.24E and Fig.24F In the embodiment, a portable game machine and a fixed game machine for home use are described as an example of a game machine. As other game machines, for example, arcade game machines arranged in recreational facilities (game centers, amusement parks, etc.) and pitching machines for batting practice arranged in sports facilities can be cited.
[0613] [Mobile body]
[0614] A storage device according to one embodiment of the present invention can be applied to a vehicle as a moving object and the vicinity of a driver's seat of the vehicle.
[0615] Figure 24G A car 5700 is shown as an example of a moving object.
[0616] A dashboard that can display a speedometer, a tachometer, a travel distance, a refueling amount, a gear state, an air-conditioning setting, etc. to provide various information is provided near the driver's seat of the automobile 5700. In addition, a storage device that represents the above information may also be provided near the driver's seat.
[0617] In particular, by displaying the image captured by the camera device (not shown) installed on the automobile 5700 on the above-mentioned display device, the field of vision blocked by pillars, etc., the blind spot of the driver's seat, etc. can be supplemented, thereby improving safety. In other words, by displaying the image captured by the camera device installed outside the automobile 5700, the blind spot can be supplemented to improve safety.
[0618] The storage device of one embodiment of the present invention can temporarily store data. For example, the storage device can be applied to the automatic driving system of the automobile 5700, the navigation system, the danger prediction system, etc. to temporarily store necessary data. In addition, the recording of the driving recorder installed in the automobile 5700 can also be stored.
[0619] In addition, although the above example describes a car as an example of a mobile body, the mobile body is not limited to the car. For example, a tram, a monorail, a ship, and a flying object (a helicopter, an unmanned aerial vehicle (UAV), an airplane, a rocket) can also be cited as a mobile body.
[0620] [camera]
[0621] A storage device according to one embodiment of the present invention can be applied to a camera.
[0622] Fig.24H A digital camera 6240 is shown as an example of an image pickup device. The digital camera 6240 includes a housing 6241, a display unit 6242, an operation switch 6243, a shutter button 6244, etc., and is equipped with a detachable lens 6246. Note that here, the digital camera 6240 adopts a structure in which the lens 6246 can be detached from the housing 6241, but the lens 6246 and the housing 6241 may be formed as one body. In addition, the digital camera 6240 may also have a flash device and a viewfinder, etc. that are separately installed.
[0623] The use of a storage device according to one embodiment of the present invention in a digital camera 6240 can reduce power consumption. In addition, the heat generated by the circuit can be reduced by reducing power consumption, thereby reducing the impact of heat on the circuit itself, peripheral circuits, and modules.
[0624] [Video Camera]
[0625] A storage device according to one embodiment of the present invention can be applied to a video camera.
[0626] Fig.24IA video camera 6300 as an example of a camera device is shown. The video camera 6300 includes a first housing 6301, a second housing 6302, a display unit 6303, an operation switch 6304, a lens 6305, a connection unit 6306, and the like. The operation switch 6304 and the lens 6305 are provided on the first housing 6301, and the display unit 6303 is provided on the second housing 6302. The first housing 6301 and the second housing 6302 are connected by the connection unit 6306, and the angle between the first housing 6301 and the second housing 6302 can be changed by the connection unit 6306. The image of the display unit 6303 can also be switched according to the angle between the first housing 6301 and the second housing 6302 in the connection unit 6306.
[0627] When recording an image captured by the video camera 6300, encoding is required according to a data recording method. With the storage device of one embodiment of the present invention, the video camera 6300 can store a file temporarily generated during encoding.
[0628] [ICD]
[0629] The storage device according to one embodiment of the present invention can be applied to an implantable cardioverter-defibrillator (ICD).
[0630] Fig.24J 1 is a schematic cross-sectional view showing an example of an ICD. An ICD main body 5400 includes at least a battery 5401, an electronic component 700, a regulator, a control circuit, an antenna 5404, a wire 5402 to the right atrium, and a wire 5403 to the right ventricle.
[0631] The ICD body 5400 is surgically placed in the body, and two metal wires pass through the subclavian vein 5405 and the superior vena cava 5406 of the human body, and the tip of one metal wire is placed in the right ventricle, and the tip of the other metal wire is placed in the right atrium.
[0632] ICD main body 5400 has the function of a pacemaker, and paces the heart when the heart rhythm is out of a predetermined range. In addition, when the heart rhythm does not improve even with pacing (rapid ventricular frequency or ventricular fibrillation, etc.), treatment using defibrillation is performed.
[0633] In order to perform pacing and defibrillation appropriately, the ICD main body 5400 needs to monitor the heart rhythm frequently. Therefore, the ICD main body 5400 includes a sensor for detecting the heart rhythm. In addition, the ICD main body 5400 can store the heart rhythm data measured by the sensor, the number of times and time of treatment using pacing, etc. in the electronic component 700.
[0634] In addition, since power is received by antenna 5404, the power is charged to battery 5401. In addition, safety can be improved by including a plurality of batteries in ICD main body 5400. Specifically, even if some batteries in ICD main body 5400 fail, other batteries can function and be used as auxiliary power sources.
[0635] In addition, in addition to the antenna 5404 capable of receiving power, an antenna capable of sending physiological signals may also be included. For example, a system for monitoring cardiac activity in which physiological signals such as pulse, respiratory rate, heart rhythm, and body temperature can be confirmed by an external monitoring device may be constructed.
[0636] [Expansion unit for PC]
[0637] A storage device according to one embodiment of the present invention can be applied to a computer such as a PC (Personal Computer) or an expansion device for an information terminal.
[0638] Fig.25A An example of such an expansion device is an expansion device 6100 that is portable and has a chip that can store data installed outside a PC. The expansion device 6100 is connected to the PC by, for example, a USB (Universal Serial Bus) or the like, and can use the chip to store data. Fig.25A A portable expansion device 6100 is shown, but the expansion device according to one embodiment of the present invention is not limited thereto. For example, a larger expansion device equipped with a cooling fan or the like may be used.
[0639] The expansion device 6100 includes a housing 6101, a cover 6102, a USB connector 6103, and a substrate 6104. The substrate 6104 is accommodated in the housing 6101. The substrate 6104 is provided with a circuit for driving a storage device or the like of one embodiment of the present invention. For example, the substrate 6104 is mounted with an electronic component 700 and a controller chip 6106. The USB connector 6103 is used as an interface for connecting to an external device.
[0640] [SD card]
[0641] A storage device according to one embodiment of the present invention can be applied to an SD card that can be mounted on electronic devices such as information terminals and digital cameras.
[0642] Fig.25B This is a schematic diagram of the appearance of an SD card. Fig.25C51 is a schematic diagram of the internal structure of an SD card. An SD card 5110 includes a housing 5111, a connector 5112, and a substrate 5113. The connector 5112 has the function of an interface connected to an external device. The substrate 5113 is accommodated in the housing 5111. The substrate 5113 is provided with a storage device and a circuit that drives the storage device. For example, the substrate 5113 is installed with an electronic component 700 and a controller chip 5115. In addition, the circuit structures of the electronic component 700 and the controller chip 5115 are not limited to the above description, and the circuit structure can be appropriately changed according to the situation. For example, the write circuit, row driver, read circuit, etc. possessed by the electronic component can also be installed on the controller chip 5115 instead of the electronic component 700.
[0643] The capacity of the SD card 5110 can be increased by also providing the electronic component 700 on the back side of the substrate 5113. In addition, a wireless chip having a wireless communication function can be provided on the substrate 5113. Thus, wireless communication between an external device and the SD card 5110 can be performed, and data of the electronic component 700 can be read and written.
[0644] [SSD]
[0645] A storage device according to one embodiment of the present invention can be applied to an SSD (Solid State Drive) that can be mounted on an electronic device such as an information terminal.
[0646] Fig.25D This is a schematic diagram of the appearance of SSD. Fig.25E 5150 is a schematic diagram of the internal structure of the SSD. The SSD5150 includes a housing 5151, a connector 5152, and a substrate 5153. The connector 5152 has the function of connecting to an interface of an external device. The substrate 5153 is accommodated in the housing 5151. The substrate 5153 is provided with a storage device and a circuit that drives the storage device. For example, the substrate 5153 is installed with an electronic component 700, a memory chip 5155, and a controller chip 5156. By also providing the electronic component 700 on the back side of the substrate 5153, the capacity of the SSD5150 can be increased. A working memory is installed in the memory chip 5155. For example, a DRAM chip can be used for the memory chip 5155. A processor, an ECC (Error Check and Correct) circuit, etc. are installed in the controller chip 5156. Note that the circuit structures of the electronic component 700, the memory chip 5155, and the controller chip 5155 are not limited to the above description, and the circuit structure can be appropriately changed according to the situation. For example, a memory used as a working memory can also be provided in the controller chip 5156.
[0647] [computer]
[0648] Fig.26A The computer 5600 shown is an example of a large-scale computer. In the computer 5600 , a plurality of rack-mounted computers 5620 are housed in a rack 5610 .
[0649] Computer 5620 may have, for example, Fig.26B The structure of the stereogram is shown. Fig.26B In the embodiment, the computer 5620 includes a motherboard 5630, and the motherboard 5630 includes a plurality of slots 5631 and a plurality of connection terminals. A personal computer card 5621 is inserted into the slot 5631. The personal computer card 5621 includes connection terminals 5623, 5624, and 5625, which are connected to the motherboard 5630.
[0650] Fig.26C The personal computer card 5621 shown is an example of a processing board including a CPU, a GPU, a storage device, etc. The personal computer card 5621 has a board 5622. In addition, the board 5622 includes a connection terminal 5623, a connection terminal 5624, a connection terminal 5625, a semiconductor device 5626, a semiconductor device 5627, a semiconductor device 5628, and a connection terminal 5629. Note that Fig.26C Semiconductor devices other than the semiconductor device 5626, the semiconductor device 5627, and the semiconductor device 5628 are shown. For description of these semiconductor devices, refer to the description of the semiconductor device 5626, the semiconductor device 5627, and the semiconductor device 5628 described below.
[0651] The connection terminal 5629 has a shape that can be inserted into the slot 5631 of the motherboard 5630, and is used as an interface for connecting the personal computer card 5621 and the motherboard 5630. Examples of the standard of the connection terminal 5629 include PCIe and the like.
[0652] The connection terminals 5623, 5624, and 5625 can be used as interfaces for supplying power to the personal computer card 5621 or inputting signals, for example. In addition, for example, they can be used as interfaces for outputting signals calculated by the personal computer card 5621, for example. As the specifications of the connection terminals 5623, 5624, and 5625, for example, USB (Universal Serial Bus), SATA (Serial ATA), and SCSI (Small Computer System Interface) can be cited. In addition, when video signals are output from the connection terminals 5623, 5624, and 5625, HDMI (registered trademark) and the like can be cited as the specifications.
[0653] The semiconductor device 5626 includes a terminal (not shown) for inputting and outputting a signal. By inserting the terminal into a socket (not shown) included in the board 5622 , the semiconductor device 5626 and the board 5622 can be electrically connected.
[0654] The semiconductor device 5627 includes a plurality of terminals, and the semiconductor device 5627 and the board 5622 can be electrically connected by soldering the terminals to wiring provided on the board 5622 by reflow soldering. As the semiconductor device 5627, for example, an FPGA (Field Programmable Gate Array), a GPU, a CPU, etc. can be cited. As the semiconductor device 5627, for example, an electronic component 730 can be used.
[0655] The semiconductor device 5628 includes a plurality of terminals, and the semiconductor device 5628 and the board 5622 can be electrically connected by soldering the terminals to wirings provided on the board 5622 by reflow soldering. As the semiconductor device 5628, for example, a memory device can be cited. As the semiconductor device 5628, for example, the electronic component 700 can be used.
[0656] The computer 5600 can be used as a parallel computer. By using the computer 5600 as a parallel computer, for example, large-scale calculations required for learning and inference of artificial intelligence can be performed.
[0657] By using a storage device of one embodiment of the present invention in the above-mentioned various electronic devices, miniaturization and low power consumption of the electronic devices can be achieved. In addition, the power consumption of the storage device of one embodiment of the present invention is low, thereby reducing the heating of the circuit. Thus, the negative impact of the heating on the circuit itself, the peripheral circuit and the module can be reduced. In addition, by using a storage device of one embodiment of the present invention, an electronic device that can work stably even in a high temperature environment can be realized. Thus, the reliability of the electronic device can be improved.
[0658] This embodiment mode can be combined with other embodiment modes as appropriate.
[0659] (Implementation 6)
[0660] In this embodiment, using Fig. 27 A specific example in which a semiconductor device according to one embodiment of the present invention is applied to space equipment will be described.
[0661] A semiconductor device of one embodiment of the present invention includes an OS transistor. The electrical characteristics of the OS transistor change little due to exposure to radiation. In other words, it has high resistance to radiation, so it can be appropriately used in an environment where radiation may be incident. For example, an OS transistor can be appropriately used when used in outer space. Specifically, an OS transistor can be used as a transistor constituting a semiconductor device provided in a space shuttle, an artificial satellite, or a space probe. Examples of radiation include X-rays and neutron radiation. In addition, outer space refers to, for example, a place above 100 km in altitude, but the outer space described in this specification may also include one or more of the thermosphere, mesosphere, and stratosphere.
[0662] exist Fig. 27 In FIG. 6 , an artificial satellite 6800 is shown as an example of a space device. The artificial satellite 6800 includes a main body 6801, a solar cell panel 6802, an antenna 6803, a secondary battery 6805, and a control device 6807. Fig. 27 An example of a planet 6804 in outer space is shown.
[0663] In addition, outer space is an environment where the radiation dose is more than 100 times that of the ground. Examples of radiation include: electromagnetic waves (electromagnetic radiation) represented by X-rays and gamma rays; and particle radiation represented by alpha rays, beta rays, neutron rays, proton rays, heavy ion rays, muon rays, etc.
[0664] When sunlight shines on the solar cell panel 6802, the power required for the artificial satellite 6800 to operate is generated. However, for example, when sunlight does not shine on the solar cell panel or when the amount of sunlight shining on the solar cell panel is small, the amount of power generated is reduced. Therefore, there is a possibility that the power required for the artificial satellite 6800 to operate may not be generated. In order to operate the artificial satellite 6800 even when the generated power is small, it is preferable to provide a secondary battery 6805 in the artificial satellite 6800. In addition, the solar cell panel is sometimes referred to as a solar cell module.
[0665] The artificial satellite 6800 can generate a signal. The signal is transmitted through the antenna 6803, and a receiver on the ground or other artificial satellites can receive the signal. By receiving the signal transmitted by the artificial satellite 6800, the position of the receiver receiving the signal can be measured. Thus, the artificial satellite 6800 can constitute a satellite positioning system.
[0666] In addition, the control device 6807 has a function of controlling the artificial satellite 6800. The control device 6807 is composed of, for example, any one or more selected from a CPU, a GPU, and a storage device. In addition, as the control device 6807, a semiconductor device including an OS transistor in one embodiment of the present invention is preferably used. Compared with Si transistors, the electrical characteristics of OS transistors change less due to exposure to radiation. In other words, OS transistors have high reliability and can be used appropriately even in an environment where radiation may be incident.
[0667] In addition, the artificial satellite 6800 may include a sensor. For example, by including a visible light sensor, the artificial satellite 6800 may have a function of detecting sunlight reflected from an object on the ground. Or, by including a thermal infrared sensor, the artificial satellite 6800 may have a function of detecting thermal infrared rays released from the ground. Thus, the artificial satellite 6800 may be used as an earth observation satellite, for example.
[0668] Note that although an artificial satellite is described as an example of space equipment in this embodiment, the present invention is not limited to this. For example, a semiconductor device according to one embodiment of the present invention can be suitably applied to space equipment such as a spacecraft, a space capsule, and a space probe.
[0669] Alternatively, for example, the OS transistor can be used as a transistor constituting a semiconductor device in a working robot provided in a nuclear power plant or a radioactive waste processing or disposal site. In particular, the OS transistor can be suitably used as a transistor constituting a semiconductor device provided in a remotely operated robot that is remotely operated during the removal of a reactor facility, the removal of nuclear fuel or fuel fragments, or field investigations in a space with a large amount of radioactive materials.
[0670] This embodiment mode can be combined with other embodiment modes as appropriate.
[0671] [Example]
[0672] In this embodiment, the manufacturing FIG. 8A to FIG. 8F The structure including the oxide 230 is shown with a cross-sectional SEM observation result.
[0673] In this embodiment, a sample is prepared on a silicon substrate in the following order: a base silicon oxide film, a hafnium oxide film (hereinafter referred to as an HfOx film), a silicon oxide film (hereinafter referred to as an SiOx film), an In-Ga-Zn oxide film (hereinafter referred to as an IGZO film), a stacked film of tantalum nitride and tungsten (hereinafter referred to as a TaNx\W film), a stacked film of silicon nitride and silicon oxide (hereinafter referred to as a SiNx\SiOx film), a tungsten film (hereinafter referred to as a W film), an SOC film, and an SOG film. A resist mask is set on the sample and a resist is formed. FIG. 8A to FIG. 8F The etching process is shown.
[0674] Here, the base silicon oxide film corresponds to FIG. 8A to FIG. 8F The insulator 216 shown. The HfOx film corresponds to the insulator 222. The SiOx film corresponds to the insulating film 224f and the insulator 224. The IGZO film corresponds to the stacked film of the oxide film 230af and the oxide film 230bf and the stacked film of the oxide 230a and the oxide 230b. The TaNx\W film corresponds to the stacked film of the conductive film 242_1f and the...
Claims
1. A semiconductor device comprising: a first storage unit; a second storage unit on the first storage unit; a first electrical conductor; as well as a second conductor on the first conductor, The first storage unit and the second storage unit both include a transistor, a capacitor, and a first insulator on the transistor. The transistor includes a metal oxide, a third conductor on the metal oxide, a fourth conductor and a second insulator, a fifth conductor on the second insulator, a third insulator under the metal oxide, and a sixth conductor under the third insulator. The capacitor includes a seventh conductor, a fourth insulator on the seventh conductor, and an eighth conductor on the fourth insulator, The seventh conductor, the fourth insulator, and a portion of the eighth conductor are located on the first insulator. The fourth conductor is in contact with the seventh conductor through the opening provided in the first insulator, The first conductor includes a portion in contact with the third conductor included in the first memory cell, The top surface of the first conductor includes a portion in contact with the bottom surface of the second conductor, The second conductor includes a portion in contact with the third conductor included in the second memory cell, The sixth conductor included in the second memory cell includes the same material as the eighth conductor included in the first memory cell, Furthermore, in a cross section of the transistor, one side end of the third conductor is substantially aligned with one side end of the metal oxide, and one side end of the fourth conductor is substantially aligned with another side end of the metal oxide.
2. The semiconductor device according to claim 1, The first conductor is in contact with a portion of the top surface and the one side end portion of the third conductor included in the first memory cell.
3. The semiconductor device according to claim 1, The side end of the third insulator is substantially aligned with the side end of the metal oxide.
4. The semiconductor device according to claim 1, wherein the third conductor and the fourth conductor both include a first layer and a second layer on the first layer, The first layer comprises a metal nitride, And the electrical conductivity of the second layer is higher than that of the first layer.
5. The semiconductor device according to claim 4, wherein the first layer comprises tantalum nitride, And the second layer includes tungsten.
6. The semiconductor device according to claim 1, further comprising: a fifth insulator in contact with a top surface of the third electrical conductor; as well as a sixth insulator in contact with the top surface of the fourth conductor, The side end portion of the sixth insulator is substantially aligned with the side end portion of the fourth conductor.
7. The semiconductor device according to any one of claims 1 to 6, further comprising: a seventh insulator covering the third conductor, the fourth conductor, the metal oxide and the third insulator, wherein the seventh insulator includes a first opening overlapping with a region sandwiched between the third electrical conductor and the fourth electrical conductor, and also includes a second opening overlapping with an opening of the first insulator, The second insulator and at least a portion of the fifth conductor are disposed in the first opening of the seventh insulator. Furthermore, the seventh conductor, the fourth insulator, and at least a portion of the eighth conductor are arranged in the second opening of the seventh insulator.
8. The semiconductor device according to claim 7, wherein an eighth insulator is included on the first insulator, The top surface of the eighth insulator contacts a portion of the fourth insulator, And the eighth insulator includes an opening overlapping with the opening of the first insulator.
9. The semiconductor device according to claim 8, The eighth insulator has a thickness of not less than 50 nm and not more than 250 nm.
10. The semiconductor device according to claim 8, further comprising: a ninth insulator in contact with the bottom surface of the sixth conductor, wherein the ninth insulator included in the second memory cell contacts the top surface of the eighth insulator included in the first memory cell, And the ninth insulator included in the second memory cell includes the same material as the fourth insulator included in the first memory cell.
11. The semiconductor device according to claim 7, The side end portion of the seventh conductor is covered by the fourth insulator.
12. The semiconductor device according to claim 7, The fourth insulator includes one or both of zirconium oxide and aluminum oxide.
13. The semiconductor device according to claim 7, The sixth conductor overlaps with the fifth conductor via the metal oxide.
14. The semiconductor device according to claim 7, further comprising: a tenth insulator in contact with a side surface of the first conductor, At least a portion of the third conductor is exposed from the tenth insulator and is in contact with the first conductor.
15. The semiconductor device according to claim 14, The tenth insulator includes one or both of aluminum oxide and silicon nitride.
16. The semiconductor device according to claim 7, The first insulator comprises aluminum oxide.
17. A method for manufacturing a semiconductor device, comprising the following steps: Depositing a first insulator, a second insulator, a metal oxide, a second conductor and a third insulator in sequence on the first conductor; Forming an island-shaped second insulator, an island-shaped metal oxide, an island-shaped second conductor and an island-shaped third insulator by processing the second insulator, the metal oxide, the second conductor and the third insulator; Depositing a fourth insulator in a manner of covering the first insulator, the island-shaped second insulator, the island-shaped metal oxide, the island-shaped second conductor, and the island-shaped third insulator; forming a first opening in the fourth insulator, dividing the island-shaped third insulator so as to overlap with the first opening to form a fifth insulator and a sixth insulator, and dividing the island-shaped second conductor so as to form a third conductor and a fourth conductor; forming a seventh insulator in the first opening and a fifth conductor on the seventh insulator; depositing an eighth insulator on the fourth insulator and the fifth conductor; forming a second opening reaching the third conductor in the eighth insulator, the fourth insulator, and the fifth insulator; forming a sixth conductor in the second opening; Depositing a ninth insulator and a seventh conductor in a manner of covering the sixth conductor; as well as The ninth insulator and the seventh conductor are processed to form a tenth insulator, an eleventh insulator, an eighth conductor on the tenth insulator, and a ninth conductor on the eleventh insulator. The eighth conductor overlaps with the tenth insulator and the sixth conductor, and the ninth conductor overlaps with the metal oxide and the fifth conductor.
18. The method for manufacturing a semiconductor device according to claim 17, Before forming the second opening, a third opening is formed by passing through the eighth insulator, the fourth insulator, the sixth insulator and the first insulator, forming a tenth conductor in the third opening, And the tenth electrical conductor is in contact with a portion of the fourth electrical conductor.
19. The method for manufacturing a semiconductor device according to claim 17, Before processing the second insulator, the metal oxide, the second conductor and the third insulator, a metal film is deposited on the third insulator, and an organic coating film is deposited on the metal film. The second insulator, the metal oxide, the second conductor and the third insulator are processed using a capacitively coupled plasma etching device.
20. The method for manufacturing a semiconductor device according to claim 19, The island-shaped second conductor is formed before the organic coating film disappears when the second conductor is processed.
21. The method for manufacturing a semiconductor device according to claim 19, When processing the second conductor, the power of the lower electrode of the processing chamber of the capacitively coupled plasma etching device is less than 10W.
22. The method for manufacturing a semiconductor device according to claim 17, The first conductor overlaps with the metal oxide and the fifth conductor.
23. The method for manufacturing a semiconductor device according to claim 17, The first insulator comprises hafnium oxide.
24. The method for manufacturing a semiconductor device according to claim 17, The second insulator comprises silicon oxide.
25. The method for manufacturing a semiconductor device according to claim 17, The metal oxide comprises indium, gallium and zinc.
26. The method for manufacturing a semiconductor device according to claim 17, The second electrical conductor has a stacked-layer structure of a layer containing tantalum nitride and a layer containing tungsten on the layer containing tantalum nitride.
27. The method for manufacturing a semiconductor device according to claim 17, The eighth insulator has a thickness of not less than 50 nm and not more than 250 nm.