Rack rail socket forge piece production device for coal mine conveying equipment and method of rack rail socket forge piece production device

By combining the support and heating components, efficient and stable forging of the gear rail socket forgings is achieved, solving the problems of low efficiency and high maintenance costs in the existing technology.

CN118875189AInactive Publication Date: 2024-11-01WUXI XINYOU FORGING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411047839.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing gear rail socket forging production equipment suffers from low processing efficiency, uneven temperature due to heat loss, and high maintenance costs.

Method used

It adopts a combined structure of support components, half mold components and heating components. The blank is heated synchronously by heating coils and ceramic heating rings. After the mold is closed, it is forged. Multiple mold cavities are used for simultaneous forming, and the mold cavities can be repaired individually when worn.

Benefits of technology

It improves forging efficiency and stability, maintains consistent billet temperature, and reduces maintenance costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118875189A_ABST
    Figure CN118875189A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of coal mine equipment production, and particularly discloses a rack rail socket forge piece production device for coal mine conveying equipment, the whole device is composed of a supporting assembly, a middle half die assembly, a side half die assembly, a side driving assembly, an upper punching die assembly, an upper driving assembly and an upper heating assembly; in the invention, a plurality of blanks are synchronously forged and molded, so that the hot die forging efficiency is improved; a heating rod I and a heating rod II are synchronously heated through a heating coil I and a heating coil II, so that a closed mold cavity formed by a middle half mold cavity and a side half mold cavity is heated, a blank in the closed mold cavity is heated, a heating state is maintained in the blank forging and pressing process, and the blank forging and pressing stability is improved; the whole lower die cavity adopts the two half die structures of the middle half die assembly and the side half die assembly, when the middle half die cavity and the side half die cavity are abraded or damaged, a single die cavity can be trimmed, and the maintenance cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of coal mine equipment production, in particular to a production device and method for a rack rail socket forging for coal mine conveying equipment. Background Art

[0002] The rack sockets used in grinding and conveying equipment are generally processed and formed by hot die forging. The hot die forging equipment used in the production of rack socket forgings in the prior art has the advantages of forging one-piece forming, fast forming speed and good forming quality, so it can meet general use requirements, but it still has the following disadvantages in actual use:

[0003] 1. The production device for rack socket forgings in the prior art generally adopts single die forging, and its processing efficiency needs to be further improved;

[0004] 2. In the prior art, the production device for rack socket forgings generally needs to preheat the production blank separately during the forging process, and then place the heated blank into the die cavity of the hot die forging equipment for forging. During the heating process, heat will be lost, and during the forging process, a large amount of heat exchange will occur after the forging contacts the die cavity, resulting in the inability to keep the internal and external temperatures of the blank consistent, so that the internal and external structural strength of the forging cannot be maintained uniformly. Therefore, its hot pressing stability needs to be further improved.

[0005] 3. In the prior art production device for rack socket forgings, the forging die cavity is generally formed in one piece. When the die cavity is worn, it needs to be repaired as a whole, which increases the cost of maintenance. Summary of the invention

[0006] The object of the present invention is to provide a production device and method for rack rail socket forgings for coal mine conveying equipment to solve the problems raised in the above-mentioned background technology.

[0007] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a production device for rack socket forgings for coal mine conveying equipment, comprising a support assembly, wherein the support assembly comprises side support plates which are symmetrically arranged on the left and right, and an upper support plate is fixedly provided at the upper end of the side support plate, an intermediate half-die assembly is fixedly provided in the middle of the side support plate and at the lower end of the upper support plate, side half-die assemblies are symmetrically provided on the left and right sides of the intermediate half-die assembly, a side driving assembly fixedly connected to the side half-die assembly is fixedly installed on the outer side of the side support plate, an upper punch die assembly is provided at the lower end of the upper support plate, and an upper heating assembly is sleeved on the outer side of the upper punch die assembly, and an upper driving assembly fixedly connected to the upper end of the upper punch die assembly is fixedly provided at the upper end of the upper support plate.

[0008] Preferably, the middle half-mold assembly includes a middle half-mold support seat, and side recovery grooves of a groove structure are symmetrically provided on the left and right sides of the middle half-mold support seat, a discharge port is provided at the front end of the side recovery groove, and a middle half-mold cavity of the groove structure is symmetrically provided on the left and right sides of the middle half-mold support seat.

[0009] Preferably, an intermediate half-mold heating groove is opened on the inner side of the intermediate half-mold cavity and at the upper end of the intermediate half-mold support seat, and an intermediate half-mold heating seat with a groove body structure is embedded in the intermediate half-mold heating groove, and a fixed support plate I is provided at the bottom of the intermediate half-mold heating seat, and a heating rod I is evenly and vertically fixedly connected to the upper end of the fixed support plate I, and a heating coil I is wound around the outer side of the heating rod I, a cover plate I is buckled at the upper port of the intermediate half-mold heating seat, and an external plug I is inserted into the groove body of the intermediate half-mold heating seat at the front end of the intermediate half-mold support seat, and the external plug I is electrically connected to the heating coil I.

[0010] Preferably, the side half-mold assembly includes side half-mold seats symmetrically arranged on the left and right sides of the middle half-mold support seat, and a side half-mold cavity with a groove structure is opened on the inner side of the side half-mold seat, the side half-mold cavity and the middle half-mold cavity are symmetrically arranged, and a side half-mold heating groove with a groove structure is opened on the inner side of the side half-mold cavity and at the upper end of the side half-mold seat, the side half-mold heating groove is embedded with a side half-mold heating seat, and a fixed support plate II is provided at the bottom of the groove of the side half-mold heating seat, the upper end of the fixed support plate II is vertically fixedly connected with uniformly arranged heating rods II, the outer side of the heating rods II is wound with a heating coil II, a cover plate II is buckled at the upper port of the side half-mold heating seat, and an external plug II is inserted into the groove body of the side half-mold heating seat at the front end of the side half-mold seat, and the external plug II is electrically connected to the heating coil II.

[0011] Preferably, the side drive assembly includes a side drive cylinder I fixedly installed on the outside of the side support plate, and a connecting plate I is fixedly connected to the inner side of the side support plate and at the end of the piston rod of the side drive cylinder I, and the connecting plate I is fixedly connected to the outer side surface of the side half-mold base.

[0012] Preferably, the upper punch die assembly comprises an upper punch die support seat provided at the lower end of the upper support plate, and evenly distributed die heads are vertically fixedly connected to the lower end surface of the upper punch die support seat.

[0013] Preferably, the upper driving assembly includes an upper driving cylinder II fixedly mounted on the upper end of an upper support plate, and a connecting plate II is fixedly connected to the lower end of the upper support plate and to the end of the piston rod of the upper driving cylinder II, and the connecting plate II is fixedly connected to the upper end surface of the upper punch support seat.

[0014] Preferably, an upper heating seat fixing plate is symmetrically fixed to the lower end of the upper support plate and on the inner side surface of the side support plate, the upper heating assembly is fixedly installed on the lower end of the upper heating seat fixing plate, the lower end of the upper heating seat fixing plate and the lower end of the upper heating assembly are provided with an upper sealing plate horizontally connected to the inner wall of the side support plate, and a die opening corresponding to the position of the die head is opened on the wall of the upper sealing plate, spring door plates are symmetrically hinged on both sides of the lower end of the die opening, and side sealing plates are symmetrically buckled on the front and rear ends of the side support plate and the upper support plate.

[0015] Preferably, the upper heating assembly includes an upper heating seat annularly sleeved on the outside of the die head, and heating seat side mounting plates fixedly connected to the upper heating seat fixing plate are symmetrically provided on the left and right sides of the upper end of the upper heating seat, and a ceramic heating ring is fixedly embedded in the middle of the upper heating seat.

[0016] Preferably, the present invention also relates to a method for producing a rack rail socket forging for coal mine conveying equipment, the method specifically comprising the following steps:

[0017] Step 1: Preparation: prepare the blank of the workpiece to be forged and place it next to the processing equipment, and electrically connect the external plug I, external plug II, and ceramic heating ring to the external power supply respectively, and place the recovery container at the discharge port, thus completing the preparation action;

[0018] Step 2: The lower mold is closed, and the side driving cylinder 1 is controlled to extend, so that its piston rod and the side driving cylinder 1 push the side half mold seat inward, so that the side half mold seat and the middle half mold support seat are oppositely fitted, so that the side half mold cavity and the middle half mold cavity are buckled to form a complete lower mold cavity, and the lower mold closing action is completed;

[0019] Step 3, heating, start the external power supply, respectively power on the heating coil I and the heating coil II through the external plug I and the external plug II, and simultaneously power on the ceramic heating ring, so that the heating rods I, II and the ceramic heating ring are heated synchronously, the heating rod I heats the mold cavity of the middle half mold cavity, the heating rod II heats the mold cavity of the side half mold cavity, and the ceramic heating ring heats the punch die head, and the heating action is started;

[0020] Step 4: Unloading: After the middle half-mold cavity, the side half-mold cavity and the die head are heated, the blank to be forged is placed in the closed cavity formed by the middle half-mold cavity and the side half-mold cavity, and the unloading action is completed;

[0021] Step 5: mold closing. After the blank in the closed mold cavity of the middle mold cavity and the side mold cavity is heated to the forging temperature, the upper drive cylinder II is started to extend, so that the piston rod of the upper drive cylinder II drives the connecting plate II and the upper punch die support seat to move downward synchronously, so that the punch head is introduced into the upper end of the closed mold cavity formed by the middle mold cavity and the side mold cavity, and at the same time, the lower end surface of the upper punch die support seat is fitted with the upper end surfaces of the middle mold support seat and the side mold seat, so that the mold closing action is completed;

[0022] Step six, collecting the material. After a certain period of time of mold closing, start the upper driving cylinder II to retract, so that the connecting plate II drives the upper punch support seat to move upward, so that the punch head is separated from the closed mold cavity formed by the middle half mold cavity and the side half mold cavity, and then start the side driving cylinder I to retract, so that the connecting plate I drives the side half mold seat to move outward, so that the side half mold cavity is separated from the middle half mold cavity, and then the workpiece forged in the closed mold cavity falls downward into the side recovery groove, and is finally led out from the discharge port to the recovery container, thus completing the mold opening and material collecting action.

[0023] Compared with the prior art, the invention has the following advantages:

[0024] 1. In the present invention, the side half-mold cavity and the middle half-mold cavity are combined to form a plurality of mold cavity structures. When working, the plurality of die heads at the lower end of the upper punch support seat and the plurality of mold cavities are synchronously closed and forged correspondingly, so that the plurality of blanks are synchronously forged and formed, thereby improving the efficiency of hot die forging;

[0025] 2. In the present invention, the blank to be forged is put into the closed mold cavity formed by the side half mold cavity and the middle half mold cavity, the external power supply is started, and the heating coil I and the heating coil II are used to heat the heating rod I and the heating rod II synchronously through the external plug I and the external plug II, and the ceramic heating ring is started to heat the closed mold cavity formed by the middle half mold cavity and the side half mold cavity, and then the blank in the closed mold cavity is heated. At the same time, the ceramic heating ring heats the die head, and after the blank is quickly heated to the corresponding forging temperature, the upper punch die assembly is closed at the upper end of the middle half mold assembly and the side half mold assembly to complete the forging of the blank. During the entire forging process, the blank maintains a heated state, and its own temperature is maintained in a relatively constant range, thereby improving the stability of the forging of the blank, maintaining a relatively consistent structural strength inside and outside the forging, and improving the stability of the overall performance of the forging;

[0026] 3. In the present invention, the entire lower mold cavity adopts a two-half mold structure of a middle half mold assembly and a side half mold assembly. When the mold cavities of the middle half mold cavity and the side half mold cavity are worn or damaged, a single mold cavity can be repaired to reduce maintenance costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is an axial side view of the overall structure of the present invention;

[0028] Figure 2 It is the front view of the overall structure of the present invention;

[0029] Figure 3 for Figure 2 Axial view of the cross-section structure at AA in the middle;

[0030] Figure 4 for Figure 3 The enlarged schematic diagram of the local structure at E in the middle;

[0031] Figure 5 for Figure 2 Axial view of the cross-section structure at the middle CC;

[0032] Figure 6 for Figure 5 A magnified schematic diagram of the local structure at F in the middle;

[0033] Figure 7 for Figure 2 Axial view of the cross-section structure at the middle BB;

[0034] Figure 8 for Figure 7 A magnified schematic diagram of the local structure at G in the middle;

[0035] Fig. 9 It is a left view of the overall structure of the present invention;

[0036] Fig.10 for Fig. 9 Axial view of the cross-section structure at the middle DD;

[0037] Fig.11 for Fig.10 A magnified schematic diagram of the local structure at H in the middle;

[0038] Fig.12 for Fig.10 A magnified schematic diagram of the local structure at point I in the middle.

[0039] In the figure: 1, support assembly; 2, middle half mold assembly; 3, side half mold assembly; 4, side drive assembly; 5, upper punch assembly; 6, upper drive assembly; 7, upper heating assembly; 101, side support plate; 102, upper support plate; 103, upper heating seat fixing plate; 104, upper sealing plate; 105, side sealing plate; 106, punch opening; 107, spring door plate; 201, middle half mold support seat; 202, side recovery groove; 203, discharge port; 205, middle half mold cavity; 206, middle half mold heating groove; 207, middle half mold heating seat; 208, fixed support plate I; 209, heating rod I; 21 0. Heating coil I; 211. Cover plate I; 212. External plug I; 301. Side half mold base; 302. Side half mold cavity; 303. Side half mold heating groove; 304. Side half mold heating base; 305. Fixed support plate II; 306. Heating rod II; 307. Heating coil II; 308. Cover plate II; 309. External plug II; 401. Side drive cylinder I; 402. Connecting plate I; 501. Upper punch support base; 502. Punch head; 601. Upper drive cylinder II; 602. Connecting plate II; 701. Upper heating base; 702. Heating base side mounting plate; 703. Ceramic heating ring. DETAILED DESCRIPTION

[0040] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0041] See also Figures 1 to 12The present invention provides a technical solution: a production device for a rack socket forging for coal mine conveying equipment, the whole device is composed of a support assembly 1, an intermediate half-die assembly 2, a side half-die assembly 3, a side drive assembly 4, an upper punch assembly 5, an upper drive assembly 6 and an upper heating assembly 7, wherein the support assembly 1 includes a side support plate 101 which is symmetrically arranged on the left and right sides, and an upper support plate 102 is fixedly arranged on the upper end of the side support plate 101, the intermediate half-die assembly 2 is fixedly installed in the middle of the side support plate 101 and is located at the lower end of the upper support plate 102, the side half-die assembly 3 is symmetrically distributed on the left and right sides of the intermediate half-die assembly 2, the side drive assembly 4 is symmetrically installed on the outer sides of the left and right ends of the side support plate 101, and the side drive assembly 4 is fixedly connected to the outer sides of the side half-die assembly 3, and the upper punch assembly 3 is fixedly connected to the outer sides of the side half-die assembly 3. The mold assembly 5 is located at the lower end of the upper support plate 102 and at the upper end of the middle half mold assembly 2. The upper heating assembly 7 is located on the outside of the upper punch die assembly 5. The upper drive assembly 6 is fixedly installed on the upper end of the upper support plate 102, and the lower end of the upper drive assembly 6 is fixedly connected to the upper end of the upper punch die assembly 5. The side support plate 101 plays a fixed supporting role relative to the side drive assembly 4. The upper support plate 102 plays a fixed supporting role relative to the upper drive assembly 6. The side drive assembly 4 plays a lateral driving role relative to the side half mold assembly 3. The upper drive assembly 6 plays an upper end driving role relative to the upper punch die assembly 5. The upper heating assembly 7 plays a heating role relative to the upper punch die assembly 5. The middle half mold assembly 2 and the side half mold assembly 3 each have their own heating capabilities.

[0042] Furthermore, the middle half mold assembly 2 includes a middle half mold support seat 201, and side recovery grooves 202 of a groove structure are symmetrically provided on the left and right sides of the middle half mold support seat 201, and a discharge port 203 is provided at the front end of the side recovery groove 202, and a middle half mold cavity 205 of a groove structure is symmetrically provided on the left and right sides of the middle half mold support seat 201, and a middle half mold heating groove 206 is provided on the inner side of the middle half mold cavity 205 and at the upper end of the middle half mold support seat 201, and a middle half mold heating seat 207 with a groove structure is embedded in the middle half mold heating groove 206, and a fixed support plate 1208 is provided at the bottom of the middle half mold heating seat 207, and a heating rod 1209 is evenly and vertically fixedly connected to the upper end of the fixed support plate 1208, and a heating coil 1210 is wound around the outer side of the heating rod 1209, and the upper port of the middle half mold heating seat 207 A cover plate I211 is buckled, and an external plug I212 is inserted into the groove body of the middle half-mold heating seat 207 at the front end of the middle half-mold support seat 201, and the external plug I212 is electrically connected to the heating coil I210, wherein the external plug I212 is electrically connected to the external power supply. When working, the external power supply is started to supply power to the heating coil I210 in the middle half-mold heating seat 207 through the external plug I212, so that the heating coil I210 performs electric induction heating on the heating rod I209, and the heating of the heating rod I209 heats the middle half-mold cavity 205 on the side of the middle half-mold heating groove 206, so that the blank is heated synchronously in the middle half-mold cavity 205, and after the blank is forged, the middle half-mold assembly 2 is separated from the side half-mold assembly 3, so that the forged blank falls from the middle half-mold cavity 205 into the side recovery groove 202.

[0043] Furthermore, the side half mold assembly 3 includes a side half mold base 301 symmetrically arranged on the left and right sides of the middle half mold support base 201, and a side half mold cavity 302 with a groove structure is opened on the inner side of the side half mold base 301, and the side half mold cavity 302 is symmetrically arranged with the middle half mold cavity 205, and a side half mold heating groove 303 with a groove structure is opened on the inner side of the side half mold cavity 302 and at the upper end of the side half mold base 301, and a side half mold heating base 304 is embedded in the side half mold heating groove 303, and a side half mold heating base 304 is embedded in the side half mold A fixed support plate II305 is provided at the bottom of the groove of the heating seat 304, and a uniformly arranged heating rod II306 is vertically fixedly connected to the upper end of the fixed support plate II305. A heating coil II307 is wound around the outer side of the heating rod II306. A cover plate II308 is buckled at the upper end of the side half mold heating seat 304. An external plug II309 is plugged into the groove body of the side half mold heating seat 304 at the front end of the side half mold seat 301. The external plug II309 is connected to the heating coil II3 07, wherein the external plug II309 is electrically connected to the external power supply, and the side half mold cavity 302 and the middle half mold cavity 205 form a complete lower mold cavity when the middle half mold assembly 2 and the side half mold assembly 3 are molded together. When working, the external power supply is started to supply power to the heating coil II307 in the side half mold heating seat 304 through the external plug II309, so that the heating coil II307 performs electric induction heating on the heating rod II306, and the heating rod II306 is heated by the heating rod II306. The heating heats the side half-mold cavity 302 on the side of the side half-mold heating groove 303, so that the blank is heated synchronously in the side half-mold cavity 302. After the blank is forged, the middle half-mold assembly 2 is separated from the side half-mold assembly 3, so that the forged blank falls from the side half-mold cavity 302 into the side recovery groove 202. The half-mold structure of the middle half-mold cavity 205 and the side half-mold cavity 302 allows a single mold cavity to be quickly repaired after wear, thereby reducing the difficulty and cost of maintenance.

[0044] Furthermore, the side drive assembly 4 includes a side drive cylinder I401 fixedly installed on the outside of the side support plate 101, and a connecting plate I402 is fixedly connected to the inner side of the side support plate 101 and at the end of the piston rod of the side drive cylinder I401. The connecting plate I402 is fixedly connected to the outer side surface of the side half-mold base 301. When working, the piston rod of the side drive cylinder I401 drives the connecting plate I402 and the side half-mold base 301 to move synchronously. When the lower mold cavity is closed, the piston rod of the side drive cylinder I401 drives the connecting plate I402 and the side half-mold base 301 to move synchronously toward the side of the middle half-mold cavity 205, so that the middle half-mold cavity 205 and the side half-mold cavity 302 are merged to form a complete lower mold cavity.

[0045] Furthermore, the upper punch die assembly 5 includes an upper punch die support seat 501 disposed at the lower end of the upper support plate 102, and evenly distributed die heads 502 are vertically fixedly connected to the lower end surface of the upper punch die support seat 501, wherein the upper punch die support seat 501 plays an upper end fixed support role relative to the die head 502.

[0046] Furthermore, the upper driving assembly 6 includes an upper driving cylinder II601 fixedly installed on the upper end of the upper support plate 102, and a connecting plate II602 is fixedly connected to the lower end of the upper support plate 102 and the end of the piston rod of the upper driving cylinder II601, and the connecting plate II602 is fixedly connected to the upper end surface of the upper punch support seat 501. When working, the piston rod of the upper driving cylinder II601 drives the connecting plate II602 and the upper punch support seat 501 to move synchronously. When the upper and lower mold cavities are closed, the piston rod of the upper driving cylinder II601 drives the connecting plate II602 and the upper punch support seat 501 to move downward, so that the die head 502 at the lower end of the upper punch support seat 501 is inserted into the lower mold cavity formed by the middle half mold cavity 205 and the side half mold cavity 302, and the blank therein is forged so that it is forged and formed in the lower mold cavity.

[0047] Furthermore, an upper heating seat fixing plate 103 is symmetrically fixed to the lower end of the upper support plate 102 and on the inner side surface of the side support plate 101, and the upper heating assembly 7 is fixedly installed at the lower end of the upper heating seat fixing plate 103. An upper sealing plate 104 horizontally connected to the inner wall of the side support plate 101 is provided at the lower end of the upper heating seat fixing plate 103 and at the lower end of the upper heating assembly 7, and a die opening 106 corresponding to the position of the die head 502 is opened on the wall of the upper sealing plate 104, and spring door plates 107 are symmetrically hinged on both sides of the lower end of the die opening 106, and side sealing plates 105 are symmetrically buckled at the front and rear ends of the side support plate 101 and the upper support plate 102, wherein the upper heating seat fixing plate 103 is provided with a plurality of sealing plates 105 ... The plate 103 plays a role of fixing the upper end relative to the upper heating component 7. The upper sealing plate 104, the side sealing plate 105 and the side support plate 101 and the upper support plate 102 form a relatively closed space, which seals the upper die assembly 5 and the upper heating component 7, so that when the upper heating component 7 heats the upper die assembly 5, heat loss is effectively avoided. During operation, after the upper heating component 7 heats the upper die assembly 5, the upper driving component 6 drives the upper die assembly 5 to move downward, so that the die head 502 is pushed downward from the middle of the spring door plate 107 at the lower end of the die opening 106, and then the die head 502 continues to be inserted downward into the lower die cavity formed by the middle half die cavity 205 and the side half die cavity 302, and the blank in the lower die cavity is hot forged.

[0048] Furthermore, the upper heating assembly 7 includes an upper heating seat 701 annularly sleeved on the outside of the die head 502, and heating seat side mounting plates 702 fixedly connected to the upper heating seat fixing plate 103 are symmetrically provided on the left and right sides of the upper end of the upper heating seat 701, and a ceramic heating coil 703 is fixedly embedded in the middle of the upper heating seat 701. Here, the ceramic heating coil 703 is electrically connected to an external power supply. When working, the external power supply energizes the ceramic heating coil 703, so that the ceramic heating coil 703 heats the die head 502.

[0049] Furthermore, the present invention also relates to a method for producing a rack rail socket forging for coal mine conveying equipment, the method specifically comprising the following steps:

[0050] Step 1: Preparation: prepare the blank of the workpiece to be forged and place it next to the processing equipment, and electrically connect the external plug I, external plug II, and ceramic heating ring to the external power supply respectively, and place the recovery container at the discharge port, thus completing the preparation action;

[0051] Step 2: The lower mold is closed, and the side driving cylinder 1 is controlled to extend, so that its piston rod and the side driving cylinder 1 push the side half mold seat inward, so that the side half mold seat and the middle half mold support seat are oppositely fitted, so that the side half mold cavity and the middle half mold cavity are buckled to form a complete lower mold cavity, and the lower mold closing action is completed;

[0052] Step 3, heating, start the external power supply, respectively power on the heating coil I and the heating coil II through the external plug I and the external plug II, and simultaneously power on the ceramic heating ring, so that the heating rods I, II and the ceramic heating ring are heated synchronously, the heating rod I heats the mold cavity of the middle half mold cavity, the heating rod II heats the mold cavity of the side half mold cavity, and the ceramic heating ring heats the punch die head, and the heating action is started;

[0053] Step 4: Unloading: After the middle half-mold cavity, the side half-mold cavity and the die head are heated, the blank to be forged is placed in the closed cavity formed by the middle half-mold cavity and the side half-mold cavity, and the unloading action is completed;

[0054] Step 5: mold closing. After the blank in the closed mold cavity of the middle mold cavity and the side mold cavity is heated to the forging temperature, the upper drive cylinder II is started to extend, so that the piston rod of the upper drive cylinder II drives the connecting plate II and the upper punch die support seat to move downward synchronously, so that the punch head is introduced into the upper end of the closed mold cavity formed by the middle mold cavity and the side mold cavity, and at the same time, the lower end surface of the upper punch die support seat is fitted with the upper end surfaces of the middle mold support seat and the side mold seat, so that the mold closing action is completed;

[0055] Step six, collecting the material. After a certain period of time of mold closing, start the upper driving cylinder II to retract, so that the connecting plate II drives the upper punch support seat to move upward, so that the punch head is separated from the closed mold cavity formed by the middle half mold cavity and the side half mold cavity, and then start the side driving cylinder I to retract, so that the connecting plate I drives the side half mold seat to move outward, so that the side half mold cavity is separated from the middle half mold cavity, and then the workpiece forged in the closed mold cavity falls downward into the side recovery groove, and is finally led out from the discharge port to the recovery container, thus completing the mold opening and material collecting action.

[0056] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A production device for rack rail socket forgings for coal mine conveying equipment, characterized in that: The invention comprises a support assembly (1), wherein the support assembly (1) comprises a side support plate (101) symmetrically arranged on the left and right, and an upper support plate (102) is fixedly arranged at the upper end of the side support plate (101), an intermediate half-mold assembly (2) is fixedly arranged in the middle of the side support plate (101) and at the lower end of the upper support plate (102), and side half-mold assemblies (3) are symmetrically arranged on the left and right sides of the intermediate half-mold assembly (2), a side driving assembly (4) fixedly connected to the side half-mold assembly (3) is fixedly installed on the outer side of the side support plate (101), an upper punch assembly (5) is arranged at the lower end of the upper support plate (102), and an upper heating assembly (7) is sleeved on the outer side of the upper punch assembly (5), and an upper driving assembly (6) fixedly connected to the upper end of the upper punch assembly (5) is fixedly arranged at the upper end of the upper support plate (102).

2. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 1, characterized in that: The middle half-mold assembly (2) comprises a middle half-mold support seat (201), and side recovery grooves (202) of a groove structure are symmetrically provided on the left and right sides of the middle half-mold support seat (201), a discharge port (203) is provided at the front end of the side recovery groove (202), and a middle half-mold cavity (205) of a groove structure is symmetrically provided on the left and right sides of the middle half-mold support seat (201).

3. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 2, characterized in that: An intermediate half-mold heating groove (206) is provided on the inner side of the intermediate half-mold cavity (205) and at the upper end of the intermediate half-mold support seat (201); an intermediate half-mold heating seat (207) with a groove structure is embedded in the intermediate half-mold heating groove (206); a fixed support plate I (208) is provided at the bottom of the intermediate half-mold heating seat (207); a heating rod I (209) is evenly and vertically fixedly connected to the upper end of the fixed support plate I (208); a heating coil I (210) is wound around the outer side of the heating rod I (209); a cover plate I (211) is buckled at the upper end of the intermediate half-mold heating seat (207); an external plug I (212) is plugged into the groove body of the intermediate half-mold heating seat (207) at the front end of the intermediate half-mold support seat (201); and the external plug I (212) is electrically connected to the heating coil I (210).

4. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 3 is characterized in that: The side half mold assembly (3) comprises a side half mold seat (301) symmetrically arranged on the left and right sides of the middle half mold support seat (201), and a side half mold cavity (302) with a groove structure is provided on the inner side of the side half mold seat (301), and the side half mold cavity (302) and the middle half mold cavity (205) are arranged symmetrically, and a side half mold heating groove (303) with a groove structure is provided on the inner side of the side half mold cavity (302) and at the upper end of the side half mold seat (301), and a side half mold heating seat (304) is embedded in the side half mold heating groove (303), and a side half mold heating seat (304) is provided on the side half mold heating seat (304). A fixed support plate II (305) is provided at the bottom of the groove, and the upper end of the fixed support plate II (305) is vertically fixedly connected to uniformly arranged heating rods II (306), and a heating coil II (307) is wound around the outer side of the heating rod II (306). A cover plate II (308) is buckled at the upper end of the side half-mold heating seat (304), and an external plug II (309) is plugged into the groove body of the side half-mold heating seat (304) at the front end of the side half-mold seat (301), and the external plug II (309) is electrically connected to the heating coil II (307).

5. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 4, characterized in that: The side drive assembly (4) comprises a side drive cylinder I (401) fixedly mounted on the outside of the side support plate (101), a connecting plate I (402) fixedly connected to the inner side of the side support plate (101) and at the end of the piston rod of the side drive cylinder I (401), and the connecting plate I (402) is fixedly connected to the outer side surface of the side half mold base (301).

6. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 5, characterized in that: The upper punch die assembly (5) comprises an upper punch die support seat (501) provided at the lower end of the upper support plate (102), and evenly arranged punch die heads (502) are vertically fixedly connected to the lower end surface of the upper punch die support seat (501).

7. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 6, characterized in that: The upper driving assembly (6) comprises an upper driving cylinder II (601) fixedly mounted on the upper end of an upper supporting plate (102); a connecting plate II (602) is fixedly connected to the lower end of the upper supporting plate (102) and to the end of the piston rod of the upper driving cylinder II (601); and the connecting plate II (602) is fixedly connected to the upper end surface of the upper punch support seat (501).

8. The production device for a rack rail socket forging for coal mine conveying equipment according to claim 7, characterized in that: An upper heating seat fixing plate (103) is symmetrically fixedly provided at the lower end of the upper support plate (102) and on the inner side surface of the side support plate (101); the upper heating assembly (7) is fixedly installed at the lower end of the upper heating seat fixing plate (103); an upper sealing plate (104) horizontally plugged into the inner wall of the side support plate (101) is provided at the lower end of the upper heating seat fixing plate (103) and at the lower end of the upper heating assembly (7); a die opening (106) corresponding to the position of the die head (502) is provided on the wall of the upper sealing plate (104); spring door plates (107) are symmetrically hinged on both sides of the lower end of the die opening (106); and side sealing plates (105) are symmetrically buckled at the front and rear ends of the side support plate (101) and the upper support plate (102).

9. A production device for a rack rail socket forging for coal mine conveying equipment according to claim 8, characterized in that: The upper heating assembly (7) comprises an upper heating seat (701) annularly sleeved on the outside of the die head (502), and heating seat side mounting plates (702) fixedly connected to the upper heating seat fixing plate (103) are symmetrically arranged on the left and right sides of the upper end of the upper heating seat (701), and a ceramic heating ring (703) is fixedly embedded in the middle of the upper heating seat (701).

10. According to the device for producing rack rail socket forgings for coal mine conveying equipment according to claims 1-9, the present invention also relates to a method for producing rack rail socket forgings for coal mine conveying equipment, characterized in that: The method specifically comprises the following steps: Step 1: Preparation: prepare the blank of the workpiece to be forged and place it next to the processing equipment, and electrically connect the external plug I, external plug II, and ceramic heating ring to the external power supply respectively, and place the recovery container at the discharge port, thus completing the preparation action; Step 2: The lower mold is closed, and the side driving cylinder 1 is controlled to extend, so that its piston rod and the side driving cylinder 1 push the side half mold seat inward, so that the side half mold seat and the middle half mold support seat are oppositely fitted, so that the side half mold cavity and the middle half mold cavity are buckled to form a complete lower mold cavity, and the lower mold closing action is completed; Step 3, heating, start the external power supply, respectively power on the heating coil I and the heating coil II through the external plug I and the external plug II, and simultaneously power on the ceramic heating ring, so that the heating rods I, II and the ceramic heating ring are heated synchronously, the heating rod I heats the mold cavity of the middle half mold cavity, the heating rod II heats the mold cavity of the side half mold cavity, and the ceramic heating ring heats the punch die head, and the heating action is started; Step 4: Unloading: After the middle half-mold cavity, the side half-mold cavity and the die head are heated, the blank to be forged is placed in the closed cavity formed by the middle half-mold cavity and the side half-mold cavity, and the unloading action is completed; Step 5: mold closing. After the blank in the closed mold cavity of the middle mold cavity and the side mold cavity is heated to the forging temperature, the upper drive cylinder II is started to extend, so that the piston rod of the upper drive cylinder II drives the connecting plate II and the upper punch die support seat to move downward synchronously, so that the punch head is introduced into the upper end of the closed mold cavity formed by the middle mold cavity and the side mold cavity, and at the same time, the lower end surface of the upper punch die support seat is fitted with the upper end surfaces of the middle mold support seat and the side mold seat, so that the mold closing action is completed; Step six, collecting the material. After a certain period of time of mold closing, start the upper driving cylinder II to retract, so that the connecting plate II drives the upper punch support seat to move upward, so that the punch head is separated from the closed mold cavity formed by the middle half mold cavity and the side half mold cavity, and then start the side driving cylinder I to retract, so that the connecting plate I drives the side half mold seat to move outward, so that the side half mold cavity is separated from the middle half mold cavity, and then the workpiece forged in the closed mold cavity falls downward into the side recovery groove, and is finally led out from the discharge port to the recovery container, thus completing the mold opening and material collecting action.