Preparation method of double-layer car roof fairing
By adopting a double-layer structure on the car roof diffuser, using a weight-reducing layer of PDCPD and SMC materials and a protective layer of epoxy resin, combined with transverse reinforcement ribs, the problems of large weight and poor protection of the existing diffuser are solved. It achieves high strength, acid and alkali resistance and convenient repair effects.
Patent Information
- Application Number
- CN202410934447.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-01
AI Technical Summary
The existing automobile roof shroud material has low toughness and high density, resulting in large weight and poor external protection. It is difficult to repair the traditional single-layer shroud locally and has high cost.
A double-layer structure is adopted, a weight-reducing layer is designed using PDCPD material and SMC material, and a protective layer is prepared through epoxy resin material, combined with transverse reinforcement ribs to form a high-strength, acid and alkali resistance diversion cover, which is convenient for local repair.
Weight reduction and wave transmittance are achieved, the strength and toughness of the shroud are improved, the maintenance costs are reduced, and good protection and repair convenience are provided through the use of epoxy resin materials.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of automobile parts, and in particular to a method for preparing a double-layer roof air deflector. Background Art
[0002] The deflector has the function of reducing wind resistance, guiding the airflow to smoothly transition from the cab along the top of the cargo box, improving the fluid performance indicators at the front end of the cargo box, reducing or avoiding air vortices between the cab and the cargo box, thereby improving fuel economy.
[0003] In order to realize products such as "lightweight, electrification, intelligence, networking, and sharing", most of the top cover air shrouds on the market are made of SMC materials. SMC materials have low toughness, high density, and require internal support, which makes the entire system heavy. In addition, traditional single-layer air shrouds often need to be replaced on a large scale when the outside is damaged, and cannot be repaired locally, which is costly and has poor external protection.
[0004] Based on the above technical problems, technicians in this field urgently need to develop a method for preparing a double-layer roof fairing that can effectively reduce weight, enhance wave transmittance, has high strength, good toughness, and has a protective layer and is easy to repair. Summary of the invention
[0005] The purpose of the present invention is to provide a method for preparing a double-layer roof fairing which can effectively reduce weight, enhance wave transmittance, has high strength, good toughness, has a protective layer, and is easy to repair.
[0006] In order to achieve the above object, the present invention provides the following technical solutions:
[0007] A method for preparing a double-layer roof air deflector of the present invention comprises the following steps:
[0008] Step 1: Material preparation: prepare some PDCPD materials and SMC materials, some acid-resistant and alkali-resistant coatings, a fairing mold, a grinding tool, a car primer, a car topcoat, and epoxy resin glue, wherein the preparation of the epoxy resin glue includes 70-90 parts of epoxy resin, 10-20 parts of polyetheramine curing agent, and 4 parts of ultraviolet absorber, and vacuum packaging is adopted for 3-5 hours, and heating and mixing are performed to make epoxy resin glue;
[0009] Step 2: Weight reduction layer molding: PDCPD material and SMC material are mixed in proportion and fully stirred through a stirring device, and the stirred mixed material is injected into the air deflector mold to initially form a weight reduction layer blank. The mixed demoulding of PDCPD material and SMC material is convenient and can effectively reduce weight;
[0010] Step 3: Grinding: Use a grinding tool to grind the outer surface of the weight loss layer blank once, spray a layer of conventional polyurea coating on the weight loss layer blank, then grind it again, and spray acid and alkali resistant coating to form a weight loss layer;
[0011] Step 4: Protective layer molding: Inject the prepared epoxy resin glue into the air deflector mold to form a protective layer blank. The size of the protective layer blank is designed according to the weight loss layer to ensure that it can be completely covered on the outside of the weight loss layer to form a double-layer air deflector structure. Since the epoxy resin material has a certain elasticity, it will not affect the coating effect and can be completely fitted with the weight loss layer;
[0012] Step 5: Punching: After the double-layer air deflector structure is formed, holes are punched according to the roof air deflector structure for connection with the vehicle body;
[0013] Step 6: Spray primer: Spray primer on the polished double-layer air deflector;
[0014] Step 7: Spraying topcoat: spraying topcoat on the double-layer air deflector after spraying primer to obtain a finished double-layer air deflector.
[0015] In the above technical solution, the present invention provides a method for preparing a double-layer roof air deflector, which has the following beneficial effects:
[0016] The invention discloses a method for preparing a double-layer roof air deflector, which can be used to prepare a double-layer structure air deflector. The weight reduction layer of the commercial vehicle roof air deflector is designed by using PDCPD material and SMC material to achieve weight reduction, enhance wave transmittance, and have high strength and good toughness. The protective layer is prepared by using epoxy resin material, which has better acid and alkali resistance, and external damage can be locally repaired by using epoxy resin material, which has good protection and saves cost during maintenance. The overall stability is improved by arranging transverse reinforcing ribs inside the air deflector, and no other supporting components are required. DETAILED DESCRIPTION
[0017] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention will be further described in detail below.
[0018] A method for preparing a double-layer roof air deflector of the present invention comprises the following steps:
[0019] Step 1: Material preparation: prepare some PDCPD materials and SMC materials, some acid-resistant and alkali-resistant coatings, a fairing mold, a grinding tool, a car primer, a car topcoat, and epoxy resin glue, wherein the preparation of the epoxy resin glue includes 70-90 parts of epoxy resin, 10-20 parts of polyetheramine curing agent, and 4 parts of ultraviolet absorber, and vacuum packaging is adopted for 3-5 hours, and heating and mixing are performed to make epoxy resin glue;
[0020] Step 2: Weight reduction layer molding: PDCPD material and SMC material are mixed in proportion and fully stirred through a stirring device, and the stirred mixed material is injected into the air deflector mold to initially form a weight reduction layer blank. The mixed demoulding of PDCPD material and SMC material is convenient and can effectively reduce weight;
[0021] Step 3: Grinding: Use a grinding tool to grind the outer surface of the weight loss layer blank once, spray a layer of conventional polyurea coating on the weight loss layer blank, then grind it again, and spray acid and alkali resistant coating to form a weight loss layer;
[0022] Step 4: Protective layer molding: Inject the prepared epoxy resin glue into the air deflector mold to form a protective layer blank. The size of the protective layer blank is designed according to the weight loss layer to ensure that it can be completely covered on the outside of the weight loss layer to form a double-layer air deflector structure. Since the epoxy resin material has a certain elasticity, it will not affect the coating effect and can be completely fitted with the weight loss layer;
[0023] Step 5: Punching: After the double-layer air deflector structure is formed, holes are punched according to the roof air deflector structure for connection with the vehicle body;
[0024] Step 6: Spray primer: Spray primer on the polished double-layer air deflector;
[0025] Step 7: Spraying topcoat: spraying topcoat on the double-layer air deflector after spraying primer to obtain a finished double-layer air deflector.
[0026] As a further introduction to this embodiment, in step five, the thickness of the primer is 80 to 120 μm, preferably 120 μm.
[0027] As a further introduction to this embodiment, after the primer is sprayed in step 5, the weight-reducing layer blank with the primer is left to stand for 5 to 12 hours, or air-dried by a fan.
[0028] As a further introduction to this embodiment, after the polishing work is completed in step three, a reinforcing rib is transversely arranged in the weight-reducing layer. The shape of the reinforcing rib is determined according to the internal space of the weight-reducing layer blank, and the reinforcing rib is made of PDCPD material.
[0029] As a further introduction to this embodiment, the volume content required to be filled when the PDCPD material and the SMC material are molded is calculated according to the material molding shrinkage ratio of 0.9%, and then the shrinkage is reduced through secondary filling. The secondary filling is entirely made of PDCPD material to reduce the degree of shrinkage of the product.
[0030] As a preferred technical solution of this embodiment, in the step 2, the content ratio of the PDCPD material and the SMC material is 6:4.
[0031] As a preferred technical solution of this embodiment, in step three, the acid and alkali resistant paint used is KN22 acid and alkali resistant paint, KN17 wear-resistant acid and alkali resistant paint or KN1000 high temperature acid and alkali resistant paint.
[0032] As a preferred technical solution of this embodiment, the thickness of the protective layer is 3 to 4.5 mm.
[0033] In the above technical solution, the present invention provides a method for preparing a double-layer roof air deflector, which has the following beneficial effects:
[0034] The invention discloses a method for preparing a double-layer roof air deflector, which can be used to prepare a double-layer structure air deflector. The weight reduction layer of the commercial vehicle roof air deflector is designed by using PDCPD material and SMC material to achieve weight reduction, enhance wave transmittance, and have high strength and good toughness. The protective layer is prepared by using epoxy resin material, which has better acid and alkali resistance, and external damage can be locally repaired by using epoxy resin material, which has good protection and saves cost during maintenance. The overall stability is improved by arranging transverse reinforcing ribs inside the air deflector, and no other supporting components are required.
[0035] The above description is only by way of illustration of certain exemplary embodiments of the present invention. It is undoubted that, for those skilled in the art, the described embodiments can be modified in various ways without departing from the spirit and scope of the present invention. Therefore, the above description is illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.
Claims
1. A method for preparing a double-layer roof deflector, characterized in that: The preparation method comprises the following steps: Step 1: Material preparation: prepare some PDCPD materials and SMC materials, some acid-resistant and alkali-resistant coatings, a fairing mold, a grinding tool, a car primer, a car topcoat, and epoxy resin glue, wherein the preparation of the epoxy resin glue includes 70-90 parts of epoxy resin, 10-20 parts of polyetheramine curing agent, and 4 parts of ultraviolet absorber, and vacuum packaging is adopted for 3-5 hours, and heating and mixing are performed to make epoxy resin glue; Step 2: Weight reduction layer molding: PDCPD material and SMC material are mixed in proportion and fully stirred through a stirring device, and the stirred mixed material is injected into the air guide cover mold to initially form a weight reduction layer blank; Step 3: Grinding: Use a grinding tool to grind the outer surface of the weight loss layer blank once, spray a layer of conventional polyurea coating on the weight loss layer blank, then grind it again, and spray acid and alkali resistant coating to form a weight loss layer; Step 4: Protective layer molding: Inject the prepared epoxy resin glue into the air deflector mold to form a protective layer blank. The size of the protective layer blank is designed according to the weight reduction layer to ensure that it can be completely covered on the outside of the weight reduction layer to form a double-layer air deflector structure; Step 5: Punching: After the double-layer air deflector structure is formed, holes are punched according to the roof air deflector structure for connection with the vehicle body; Step 6: Spray primer: Spray primer on the polished double-layer air deflector; Step 7: Spraying topcoat: spraying topcoat on the double-layer air deflector after spraying primer to obtain a finished double-layer air deflector.
2. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: In the step five, the thickness of the primer is 80-120 μm, preferably 120 μm.
3. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: After the primer spraying in step 5 is completed, the weight-reducing layer blank with the primer is left to stand for 5 to 12 hours, or air-dried by a fan.
4. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: After the polishing work is completed in step three, a reinforcing rib is transversely arranged in the weight-reducing layer. The shape of the reinforcing rib is determined according to the internal space of the weight-reducing layer blank, and the reinforcing rib is made of PDCPD material.
5. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: According to the material molding shrinkage ratio of 0.9%, the volume content required to be filled during molding of PDCPD material and SMC material is calculated, and then the shrinkage is reduced through secondary filling. PDCPD material is used for the secondary filling to reduce the degree of shrinkage of the product.
6. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: In the step 2, the content ratio of the PDCPD material and the SMC material is 6:
4.
7. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: In step three, the acid and alkali resistant paint used is KN22 acid and alkali resistant paint, KN17 wear-resistant acid and alkali resistant paint or KN1000 high temperature acid and alkali resistant paint.
8. The method for preparing a double-layer roof deflector according to claim 1, characterized in that: The thickness of the protective layer is 3 to 4.5 mm.