Method and device for adjusting sulfur content in blast furnace molten iron, electronic equipment and storage medium
By calculating the predicted value of the sulfur content of molten iron and adjusting the fuel ratio, the problem of inaccurate prediction of the sulfur content in blast furnace molten iron is solved, and the stability and compliance rate of molten iron quality are improved.
Patent Information
- Application Number
- CN202410952351.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-01
AI Technical Summary
The prior art cannot achieve accurate prediction of the sulfur content in blast furnace molten iron, resulting in poor molten iron quality stability.
By obtaining the first sulfur content influence factor of the blast furnace raw material in the previous smelting cycle and the second sulfur content influence factor of the blast furnace raw material in the current smelting cycle, the predicted value of the sulfur content of the molten iron is calculated, and the sulfur content of the molten iron is adjusted according to the preset target molten iron sulfur content Fuel ratio to achieve accurate adjustment of the sulfur content of molten iron.
The advance prediction and adjustment of the sulfur content in blast furnace molten iron has been achieved, the stability of the molten iron quality has been improved, the problem that the existing technology cannot achieve accurate prediction, and the compliance rate of the sulfur content of molten iron has been improved.
Smart Images

Figure CN118879959A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of blast furnace smelting, and in particular to a method, a device, an electronic device and a storage medium for adjusting the sulfur content in molten iron of a blast furnace. Background Art
[0002] Desulfurization is a very important process technology in blast furnace smelting. In the blast furnace smelting process, most of the sulfur comes from coke, and the sulfur content of coke is directly related to the sulfur content of molten iron. According to experience, 70-80% of the sulfur in molten iron comes from the sulfur in coke, and 20-30% comes from ore.
[0003] The sulfur contained in the ore mainly exists in the gangue of the ore. The ore starts an indirect reduction reaction at a temperature of more than 600°C inside the blast furnace. The iron in the ore is reduced, the gangue generates slag, and the organic sulfur in the ore decomposes. Part of the generated sulfur is discharged with the blast furnace gas, and part circulates inside the blast furnace column. The slag generated by the gangue enters the furnace area after three stages: primary slag, middle slag, and intermediate slag. The desulfurization of molten iron is basically completed in these three stages.
[0004] Coke contains sulfur. Since coke burns in large quantities in the tuyere area of the blast furnace, the sulfur decomposed by the coke combustion directly enters the hearth and mixes with the slag in the hearth area. Part of the coke comes into contact with molten iron in the hearth area, and the sulfur directly enters the molten iron.
[0005] The existing technology for regulating the sulfur content in molten iron in blast furnaces cannot achieve accurate prediction of the sulfur content in the molten iron, which is not conducive to pre-adjustment by operators, resulting in poor stability of the molten iron quality. Summary of the invention
[0006] The present invention provides a method, device, electronic device and storage medium for adjusting the sulfur content in molten iron of a blast furnace, so as to solve the problem that the prior art cannot accurately predict the sulfur content in molten iron, which is not conducive to pre-adjustment by operators and leads to poor stability of molten iron quality.
[0007] According to one aspect of the present invention, there is provided a method for adjusting the sulfur content in molten iron of a blast furnace, comprising:
[0008] Obtaining the first sulfur content influencing factor of the blast furnace raw material in the previous smelting cycle and the second sulfur content influencing factor of the blast furnace raw material in the current smelting cycle;
[0009] performing correlation processing on the first sulfur content influencing factors to determine correlation coefficients between the first sulfur content influencing factors;
[0010] Calculating a predicted value of sulfur content in molten iron according to the second sulfur content influencing factor, the correlation coefficient and a preset correction coefficient;
[0011] Based on the preset target sulfur content of the molten iron and the predicted value of the sulfur content of the molten iron, the preset target fuel ratio is adjusted so that the preset target sulfur content of the molten iron is equal to the predicted value of the sulfur content of the molten iron.
[0012] Optionally, the first sulfur content influencing factor includes the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle; the correlation coefficient includes a first correlation coefficient;
[0013] Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors includes:
[0014] According to the sulfur content of the molten iron and the temperature of the molten iron in the previous smelting cycle, the first correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0015]
[0016] Wherein, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of the molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of the molten iron in the previous smelting cycle and the temperature of the molten iron in the previous smelting cycle.
[0017] Optionally, the first sulfur content influencing factor also includes the basicity of the charge in the previous smelting cycle; the correlation coefficient also includes a second correlation coefficient;
[0018] Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors further includes:
[0019] According to the sulfur content of the molten iron and the basicity of the charge in the previous smelting cycle, the second correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0020]
[0021] Wherein, r(S1, R1) is the second correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, R1 is the basicity of the charge in the previous smelting cycle, cov(S1, R1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the basicity of the charge in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the basicity of the charge in the previous smelting cycle.
[0022] Optionally, the first sulfur content influencing factor also includes the furnace activity offset in the previous smelting cycle; the correlation coefficient also includes a third correlation coefficient;
[0023] Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors further includes:
[0024] According to the sulfur content of the molten iron and the hearth activity offset in the previous smelting cycle, the third correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0025]
[0026] Wherein, r(S1, y1) is the third correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, y1 is the hearth activity offset in the previous smelting cycle, cov(S1, y1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the hearth activity offset in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the activity offset of the hearth in the previous smelting cycle.
[0027] Optionally, the second sulfur content influencing factor includes molten iron temperature in the current smelting cycle, charge basicity in the current smelting cycle, and furnace activity offset in the current smelting cycle;
[0028] The calculating the predicted value of the sulfur content in the molten iron according to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient comprises:
[0029] According to the molten iron temperature in the current smelting cycle, the charge basicity in the current smelting cycle, the furnace activity offset in the current smelting cycle, the correlation coefficient and the preset correction coefficient, the following formula is used to calculate the predicted value of the molten iron sulfur content:
[0030] ((rR0+rT0+ry0) / 3)×β, where r is the correlation coefficient, R0 is the basicity of the charge in the current smelting cycle; T0 is the molten iron temperature in the current smelting cycle, y0 is the furnace activity offset in the current smelting cycle, and β is the preset correction coefficient.
[0031] Optionally, adjusting the preset target fuel ratio based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content includes:
[0032] When the preset target molten iron sulfur content is less than the molten iron sulfur content prediction value, reducing the preset target fuel ratio;
[0033] When the preset target molten iron sulfur content is greater than the predicted value of the molten iron sulfur content, the preset target fuel ratio is increased.
[0034] According to another aspect of the present invention, there is provided a device for adjusting the sulfur content in molten iron of a blast furnace, comprising:
[0035] An acquisition module, the acquisition module is used to acquire a first sulfur content influencing factor of a blast furnace raw material in a previous smelting cycle, and a second sulfur content influencing factor of a blast furnace raw material in a current smelting cycle;
[0036] A correlation coefficient determination module, wherein the correlation coefficient determination module is used to perform correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors;
[0037] A molten iron sulfur content prediction value calculation module, the molten iron sulfur content prediction value calculation module is used to calculate the molten iron sulfur content prediction value according to the second sulfur content influencing factor, the correlation coefficient and a preset correction coefficient;
[0038] The regulating module is used to adjust the preset target fuel ratio based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content, so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content.
[0039] Optionally, the correlation coefficient calculation module includes a first correlation coefficient calculation submodule, and the first correlation coefficient submodule is used to calculate the first correlation coefficient between the first sulfur content influencing factors according to the molten iron sulfur content and the molten iron temperature in the previous smelting cycle using the following formula:
[0040]
[0041] Wherein, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of the molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of the molten iron in the previous smelting cycle and the temperature of the molten iron in the previous smelting cycle.
[0042] According to another aspect of the present invention, an electronic device is provided, the electronic device comprising:
[0043] at least one processor; and
[0044] a memory communicatively connected to the at least one processor; wherein,
[0045] The memory stores a computer program executable by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can execute the method for adjusting the sulfur content in molten iron in a blast furnace as described in any embodiment of the present invention.
[0046] According to another aspect of the present invention, a computer-readable storage medium is provided, wherein the computer-readable storage medium stores computer instructions, and the computer instructions are used to enable a processor to implement the method for adjusting the sulfur content in molten iron in a blast furnace as described in any embodiment of the present invention when executed.
[0047] The embodiment of the present invention provides a method, device, electronic device and storage medium for adjusting the sulfur content in molten iron of a blast furnace. The method includes: obtaining the first sulfur content influencing factor of the blast furnace raw material in the previous smelting cycle, and the second sulfur content influencing factor of the blast furnace raw material in the current smelting cycle; performing correlation processing on the first sulfur content influencing factor to determine the correlation coefficient between the first sulfur content influencing factors; calculating the molten iron sulfur content prediction value according to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient; based on the preset target molten iron sulfur content and the molten iron sulfur content prediction value, adjusting the preset target fuel ratio so that the preset target molten iron sulfur content is equal to the molten iron sulfur content prediction value. The technical solution provided by the embodiment of the present invention determines the correlation coefficient between the first sulfur content influencing factor by performing correlation processing on the first sulfur content influencing factor, and the correlation coefficient represents the correlation between the molten iron sulfur content and the first sulfur content influencing factor. That is, the correlation between the molten iron sulfur content and the molten iron temperature of the blast furnace, the basicity of the blast furnace charge, and the deviation of the furnace activity index. According to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient, the predicted value of the sulfur content in the molten iron is calculated, and the fuel ratio of the raw materials to be smelted is adjusted according to the predicted value of the sulfur content in the molten iron. Compared with the prior art, the sulfur content in the molten iron is first detected in real time, and the operator then adjusts the real-time detected sulfur content in the molten iron according to the quantitatively calculated theoretical sulfur content in the molten iron, which has a lag. The technical solution provided in the embodiment of the present application realizes the advanced predictive adjustment of the sulfur content in the blast furnace molten iron, effectively improves the stability of the molten iron quality, and solves the problem that the prior art cannot achieve accurate prediction of the sulfur content in the molten iron, which is not conducive to the operator's advance adjustment, resulting in poor stability of the molten iron quality.
[0048] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0050] Figure 1 A flow chart of a method for adjusting sulfur content in molten iron in a blast furnace provided by an embodiment of the present invention;
[0051] Figure 2 A schematic diagram of the structure of a device for adjusting the sulfur content in molten iron in a blast furnace provided by an embodiment of the present invention;
[0052] Figure 3 A schematic diagram of the structure of an electronic device that can be used to implement the embodiment of the present invention is shown. DETAILED DESCRIPTION
[0053] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0054] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0055] Figure 1 The present invention provides a flowchart of a method for adjusting the sulfur content in molten iron of a blast furnace. This embodiment can be applied to the control of the sulfur content in molten iron of a blast furnace. The method can be performed by an adjusting device for adjusting the sulfur content in molten iron of a blast furnace. The adjusting device can be implemented in the form of hardware and / or software. The adjusting device can be configured in any electronic device with a communication function. Figure 1 , the method comprising:
[0056] S110. Obtain a first sulfur content influencing factor of blast furnace raw materials in a previous smelting cycle, and a second sulfur content influencing factor of blast furnace raw materials in a current smelting cycle.
[0057] Among them, the first sulfur content influencing factor and the second sulfur content influencing factor are key factors affecting the sulfur content in molten iron, including the basicity Rn of the blast furnace charge, the temperature Tn of the blast furnace molten iron, the activity index Kn of the blast furnace hearth, etc. The smelting cycle is the time from the time when the blast furnace charge is put into the blast furnace from the top of the blast furnace to the time when the charge becomes slag iron and enters the blast furnace hearth. The smelting cycle is generally 6-8 hours. The previous smelting cycle is the situation where the molten iron generated by smelting inside the blast furnace is discharged; the current smelting cycle is the situation where smelting is being carried out inside the blast furnace. It should be noted that the blast furnace smelting cycle can be any time as the starting point. For example: the smelting cycle of a blast furnace is 8 hours, the previous smelting cycle can be from 8 o'clock to 16 o'clock, and the next smelting cycle can be from 16 o'clock to 24 o'clock. When there are N cycles of blast furnace smelting, two adjacent smelting cycles can take any time as the starting point. For example, 8 o'clock to 16 o'clock is the previous smelting cycle, and 9 o'clock to 17 o'clock can also be the current smelting cycle. The basicity Rn of the blast furnace charge is the ratio of the basic oxide to the acidic oxide. The basic oxide content includes the calcium oxide CaO content plus the magnesium oxide MgO content. When multiple ores are used, the sum of the basic oxide contents in all the ores is the total basic oxide content of the raw materials entering the furnace, which is represented by the symbol An; the acidic oxide content includes the silicon dioxide SiO2 content plus the aluminum oxide Al2O3 content. The acidic oxide content includes the total acidic oxide content in the ore, coke, and coal-injected coal powder, which is represented by the symbol Bn. The expression of the basicity Rn of the blast furnace charge is Rn=An / Bn.
[0058] Specifically, the first sulfur content influencing factor of the blast furnace raw material in the previous smelting cycle and the second sulfur content influencing factor of the blast furnace raw material in the current smelting cycle are obtained by real-time detection of the laser spectrum. Exemplarily, the blast furnace charge basicity R1, blast furnace molten iron temperature T1 and blast furnace hearth activity index K1 in the previous smelting cycle and the blast furnace charge basicity R0, blast furnace molten iron temperature T0 and blast furnace hearth activity index K0 in the current smelting cycle are obtained by real-time detection of the laser spectrum.
[0059] S120: performing correlation processing on the first sulfur content influencing factors to determine correlation coefficients between the first sulfur content influencing factors.
[0060] Specifically, according to the blast furnace hearth activity index in the first sulfur content influencing factor, the hearth activity index offset is determined, and the blast furnace molten iron temperature, blast furnace charge basicity, and hearth activity index deviation in the previous smelting cycle are subjected to correlation processing to determine the correlation coefficient between the first sulfur content influencing factors. Among them, the correlation coefficient represents the correlation between the molten iron sulfur content and the first sulfur content influencing factor. That is, the correlation between the molten iron sulfur content and the blast furnace molten iron temperature, blast furnace charge basicity, and hearth activity index deviation. The hearth activity index offset is the ratio of the hearth activity index k in the current smelting cycle to the hearth activity index k0 in the historical smelting cycle, represented by y, representing the degree of hearth activity index offset. K increases compared to K0 and y < 1, indicating that the hearth activity has deteriorated, K decreases compared to K0 and y > 1, indicating that the hearth activity has improved, and K0 is a positive number greater than 0 during normal production. The hearth activity index within the historical smelting cycle refers to the hearth activity index during the historical long-term stable state, which can represent the overall activity level of the blast furnace hearth.
[0061] For example, the blast furnace molten iron temperature T1 in the last smelting cycle, the blast furnace charge basicity R1, the furnace hearth activity index K0 in the historical long-term stable state, and the furnace hearth activity index deviation y1 are shown in the following Table 1:
[0062] Table 1
[0063]
[0064] S130. Calculate a predicted value of sulfur content in the molten iron according to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient.
[0065] Among them, the preset correction coefficient β is the ratio of the total sulfur content Q1 of the charge in the previous smelting cycle to the total sulfur content Q0 in the current smelting cycle, which is recorded as β=Q0 / Q1. The total sulfur content Q1 of the charge in the previous smelting cycle and the total sulfur content Q0 in the current smelting cycle can be obtained by detection. The purpose of setting the preset correction coefficient is to improve the accuracy of the calculation of the predicted value of the sulfur content in the molten iron. Since part of the sulfur element in the blast furnace charge will be taken away with the coal gas, and the other part will be enriched inside the blast furnace, the sulfur content deviation of these two parts is large and cannot be accurately detected in real time. Therefore, it is necessary to set the correction coefficient β. The purpose of calculating the predicted value of the sulfur content in the molten iron is to adjust the second sulfur content influencing factor according to the predicted value of the sulfur content in the molten iron, and to adjust the ratio of the raw materials to be smelted, so as to realize the advance prediction and adjustment of the sulfur content in the molten iron in the blast furnace.
[0066] S140. Based on a preset target molten iron sulfur content and a predicted value of the molten iron sulfur content, adjust the preset target fuel ratio so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content.
[0067] Among them, the preset target molten iron sulfur content and the preset target fuel ratio can be pre-set according to production requirements.
[0068] Specifically, the preset target sulfur content in the molten iron is compared with the predicted sulfur content in the molten iron, and according to the comparison result, the preset target fuel ratio is adjusted, that is, the ratio of the raw materials entering the furnace is adjusted, so that the preset target sulfur content in the molten iron is equal to the predicted sulfur content in the molten iron.
[0069] The technical solution provided by the embodiment of the present invention performs correlation processing on the first sulfur content influencing factor to determine the correlation coefficient between the first sulfur content influencing factors, and the correlation coefficient represents the correlation between the sulfur content of molten iron and the first sulfur content influencing factor. That is, the correlation between the sulfur content of molten iron and the temperature of molten iron in the blast furnace, the basicity of the blast furnace charge, and the deviation of the furnace activity index. According to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient, the molten iron sulfur content prediction value is calculated, and the fuel ratio of the raw materials to be smelted is adjusted according to the molten iron sulfur content prediction value. Compared with the prior art, the sulfur content in the molten iron is first detected in real time, and the operator adjusts the sulfur content in the molten iron detected in real time according to the quantitatively calculated theoretical sulfur content in the molten iron, which has hysteresis, and the technical solution provided by the embodiment of the present application realizes the advance prediction and adjustment of the sulfur content in the molten iron in the blast furnace, effectively improves the stability of the molten iron quality, and solves the problem that the prior art cannot realize the accurate prediction of the sulfur content in the molten iron, which is not conducive to the pre-adjustment of the operator, resulting in poor stability of the molten iron quality.
[0070] Optionally, the first sulfur content influencing factor includes the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle; the correlation coefficient includes the first correlation coefficient;
[0071] The first sulfur content influencing factors are subjected to correlation processing to determine the correlation coefficients between the first sulfur content influencing factors, including:
[0072] According to the sulfur content of molten iron and the temperature of molten iron in the previous smelting cycle, the first correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0073]
[0074] In the formula, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the temperature of molten iron in the previous smelting cycle.
[0075] The first correlation coefficient represents the correlation between the sulfur content of molten iron in the previous smelting cycle and the temperature of molten iron in the previous smelting cycle. The first correlation coefficient is calculated using covariance and variance because in blast furnace production, the data are random, covariance can better represent the linear level of random data, and variance can better represent the stability of data. Molten iron temperature is negatively correlated with molten iron sulfur content.
[0076] Optionally, the first sulfur content influencing factor also includes the basicity of the charge in the previous smelting cycle; the correlation coefficient also includes a second correlation coefficient;
[0077] Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors also includes:
[0078] According to the sulfur content of molten iron and the basicity of the charge in the previous smelting cycle, the second correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0079]
[0080] In the formula, r(S1, R1) is the second correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, R1 is the basicity of the charge in the previous smelting cycle, cov(S1, R1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the basicity of the charge in the previous smelting cycle, It is the variance of the sulfur content in molten iron and the basicity of charge in the previous smelting cycle.
[0081] The second correlation coefficient can represent the correlation between the sulfur content of molten iron in the last smelting cycle and the basicity of the charge in the last smelting cycle. The basicity of the charge is negatively correlated with the sulfur content of molten iron.
[0082] Optionally, the first sulfur content influencing factor also includes the furnace activity offset in the previous smelting cycle; the correlation coefficient also includes a third correlation coefficient;
[0083] Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors also includes:
[0084] According to the sulfur content of molten iron and the deviation of the hearth activity in the previous smelting cycle, the third correlation coefficient between the first sulfur content influencing factors is calculated using the following formula:
[0085]
[0086] In the formula, r(S1, y1) is the third correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, y1 is the offset of the hearth activity in the previous smelting cycle, cov(S1, y1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the offset of the hearth activity in the previous smelting cycle, It is the variance of the sulfur content of molten iron and the activity offset of the hearth in the previous smelting cycle.
[0087] The third correlation coefficient can represent the correlation between the sulfur content of molten iron in the last smelting cycle and the deviation of the activity index of the hearth in the last smelting cycle. The deviation of the activity index of the hearth is negatively correlated with the sulfur content of molten iron.
[0088] Optionally, the second sulfur content influencing factor includes molten iron temperature in the current smelting cycle, charge basicity in the current smelting cycle, and furnace activity offset in the current smelting cycle;
[0089] According to the second sulfur content influencing factor, correlation coefficient and preset correction coefficient, the predicted value of sulfur content in molten iron is calculated including:
[0090] According to the molten iron temperature in the current smelting cycle, the basicity of the charge in the current smelting cycle, the offset of the furnace activity in the current smelting cycle, the correlation coefficient and the preset correction coefficient, the following formula is used to calculate the predicted value of the sulfur content in the molten iron:
[0091] ((rR0+rT0+ry0) / 3)×β, where r is the correlation coefficient, R0 is the basicity of the charge in the current smelting cycle; T0 is the molten iron temperature in the current smelting cycle, y0 is the activity offset of the furnace in the current smelting cycle, and β is the preset correction coefficient.
[0092] Optionally, based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content, adjusting the preset target fuel ratio so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content includes:
[0093] When the preset target molten iron sulfur content is less than the predicted value of the molten iron sulfur content, the preset target fuel ratio is reduced; when the preset target molten iron sulfur content is greater than the predicted value of the molten iron sulfur content, the preset target fuel ratio is increased.
[0094] Specifically, during the normal production of the blast furnace, the temperature of the molten iron in the blast furnace directly affects the sulfur content in the molten iron. If the temperature of the molten iron in the blast furnace increases, the sulfur content in the molten iron will decrease. Conversely, if the temperature of the molten iron in the blast furnace decreases, the sulfur content in the molten iron will increase. Therefore, the predicted value of the molten iron sulfur content is compared with the preset target molten iron sulfur content. When the preset target molten iron sulfur content is less than the predicted value of the molten iron sulfur content, it means that the molten iron temperature in the blast furnace is relatively high. The operator can further balance the molten iron temperature in the blast furnace by lowering the preset target fuel ratio, because the fuel ratio is the ratio of coke plus pulverized coal to molten iron output, that is, it is necessary to reduce the amount of coke and pulverized coal, and increase the amount of ore, until the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content, so as to avoid large fluctuations in the molten iron sulfur content. When the preset target sulfur content of molten iron is greater than the predicted sulfur content of molten iron, it indicates that the temperature of molten iron in the blast furnace is low. The operator can further balance the temperature of molten iron in the blast furnace by increasing the preset target fuel ratio, because the fuel ratio is the ratio of coke plus pulverized coal injection to molten iron output, that is, it is necessary to increase the amount of coke and pulverized coal injection and reduce the amount of ore until the preset target sulfur content of molten iron is equal to the predicted sulfur content of molten iron, so as to avoid large fluctuations in the sulfur content of molten iron. It should be noted that the charge fuel ratio in the current smelting cycle is reduced by 1kg / t compared with the charge fuel ratio of the previous smelting cycle, and the molten iron temperature in the current smelting cycle is adjusted by reducing the charge fuel ratio by 3-5℃ compared with the charge fuel ratio of the previous smelting cycle.
[0095] High sulfur content in molten iron will lead to increased consumption of subsequent desulfurization in blast furnaces, affect the quality of molten iron, and increase the cost of steelmaking shedding; low sulfur content in molten iron indicates that the shedding capacity inside the blast furnace is excessive, which is an effect obtained by consuming a lot of heat, and is also a manifestation of high consumption of blast furnaces. The adjustment method of the prior art has a compliance rate of sulfur content in molten iron in blast furnaces of about 90%. The technical solution provided in the embodiment of the present invention analyzes the correlation between the key factors affecting blast furnace shedding, determines the predicted value of sulfur content in molten iron based on the correlation coefficient, realizes accurate prediction of sulfur content in molten iron in blast furnaces, provides adjustment ideas for operators, further stabilizes the quality of molten iron in blast furnaces, and saves production costs. In addition, the technical solution provided in the embodiment of the present invention analyzes and calculates the correlation between the sulfur content of molten iron that has been smelted and the key factors affecting blast furnace shedding, and dynamically adjusts the ingredients corresponding to the smelting in progress and to be smelted, so as to achieve a compliance rate of sulfur content in molten iron in blast furnaces of more than 98%, which is greatly improved compared with the prior art. Moreover, as the blast furnace production time goes by, the calculation accuracy will be greatly improved, providing a scientific reference solution for the industry.
[0096] Figure 2 A schematic diagram of the structure of a device for adjusting the sulfur content in molten iron of a blast furnace provided by an embodiment of the present invention. Figure 2The regulating device includes an acquisition module 210, a correlation coefficient calculation module 220, a molten iron sulfur content prediction value calculation module 230 and a regulating module 230.
[0097] The acquisition module 210 is used to acquire the first sulfur content influencing factor of the blast furnace raw material in the previous smelting cycle, and the second sulfur content influencing factor of the blast furnace raw material in the current smelting cycle;
[0098] The correlation coefficient determination module 220 is used to perform correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors;
[0099] The molten iron sulfur content prediction value calculation module 230 is used to calculate the molten iron sulfur content prediction value according to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient;
[0100] The adjustment module 240 is used to adjust the preset target fuel ratio based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content, so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content.
[0101] Optionally, the correlation coefficient calculation module includes a first correlation coefficient calculation submodule, and the first correlation coefficient submodule is used to calculate the first correlation coefficient between the first sulfur content influencing factors according to the sulfur content of the molten iron and the molten iron temperature in the previous smelting cycle using the following first preset formula:
[0102]
[0103] In the formula, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the temperature of molten iron in the previous smelting cycle.
[0104] The device for adjusting the sulfur content in molten iron in a blast furnace provided in an embodiment of the present invention can execute the method for adjusting the sulfur content in molten iron in a blast furnace provided in any embodiment of the present invention, and has functional modules and beneficial effects corresponding to the execution method.
[0105] Figure 3A schematic diagram of the structure of an electronic device that can be used to implement an embodiment of the present invention is shown. The electronic device is intended to represent various forms of digital computers, such as laptop computers, desktop computers, workbenches, personal digital assistants, servers, blade servers, mainframe computers, and other suitable computers. The electronic device can also represent various forms of mobile devices, such as personal digital processing, cellular phones, smart phones, wearable devices (such as helmets, glasses, watches, etc.) and other similar computing devices. The components shown herein, their connections and relationships, and their functions are merely examples and are not intended to limit the implementation of the present invention described and / or required herein.
[0106] like Figure 3 As shown, the electronic device 10 includes at least one processor 11, and a memory connected to the at least one processor 11, such as a read-only memory (ROM) 12, a random access memory (RAM) 13, etc., wherein the memory stores a computer program that can be executed by at least one processor, and the processor 11 can perform various appropriate actions and processes according to the computer program stored in the read-only memory (ROM) 12 or the computer program loaded from the storage unit 18 to the random access memory (RAM) 13. In the RAM 13, various programs and data required for the operation of the electronic device 10 can also be stored. The processor 11, the ROM 12, and the RAM 13 are connected to each other through a bus 14. An input / output (I / O) interface 15 is also connected to the bus 14.
[0107] A number of components in the electronic device 10 are connected to the I / O interface 15, including: an input unit 16, such as a keyboard, a mouse, etc.; an output unit 17, such as various types of displays, speakers, etc.; a storage unit 18, such as a disk, an optical disk, etc.; and a communication unit 19, such as a network card, a modem, a wireless communication transceiver, etc. The communication unit 19 allows the electronic device 10 to exchange information / data with other devices through a computer network such as the Internet and / or various telecommunication networks.
[0108] The processor 11 may be a variety of general and / or special processing components with processing and computing capabilities. Some examples of the processor 11 include, but are not limited to, a central processing unit (CPU), a graphics processing unit (GPU), various dedicated artificial intelligence (AI) computing chips, various processors running machine learning model algorithms, a digital signal processor (DSP), and any appropriate processor, controller, microcontroller, etc. The processor 11 executes the various methods and processes described above, such as a method for adjusting the sulfur content in molten iron in a blast furnace.
[0109] In some embodiments, the method for adjusting the sulfur content in blast furnace molten iron can be implemented as a computer program, which is tangibly contained in a computer-readable storage medium, such as a storage unit 18. In some embodiments, part or all of the computer program can be loaded and / or installed on the electronic device 10 via the ROM 12 and / or the communication unit 19. When the computer program is loaded into the RAM 13 and executed by the processor 11, one or more steps of the method for adjusting the sulfur content in the blast furnace molten iron described above can be performed. Alternatively, in other embodiments, the processor 11 can be configured to execute the method for adjusting the sulfur content in the blast furnace molten iron by any other appropriate means (for example, by means of firmware).
[0110] Various implementations of the systems and techniques described above herein can be implemented in digital electronic circuit systems, integrated circuit systems, field programmable gate arrays (FPGAs), application specific integrated circuits (ASICs), application specific standard products (ASSPs), systems on chips (SOCs), load programmable logic devices (CPLDs), computer hardware, firmware, software, and / or combinations thereof. These various implementations can include: being implemented in one or more computer programs that can be executed and / or interpreted on a programmable system including at least one programmable processor, which can be a special purpose or general purpose programmable processor that can receive data and instructions from a storage system, at least one input device, and at least one output device, and transmit data and instructions to the storage system, the at least one input device, and the at least one output device.
[0111] Computer programs for implementing the methods of the present invention may be written in any combination of one or more programming languages. These computer programs may be provided to a processor of a general-purpose computer, a special-purpose computer, or other programmable data processing device, so that when the computer program is executed by the processor, the functions / operations specified in the flow chart and / or block diagram are implemented. The computer program may be executed entirely on the machine, partially on the machine, partially on the machine and partially on a remote machine as a stand-alone software package, or entirely on a remote machine or server.
[0112] In the context of the present invention, a computer-readable storage medium may be a tangible medium that may contain or store a computer program for use by or in combination with an instruction execution system, device or equipment. A computer-readable storage medium may include, but is not limited to, electronic, magnetic, optical, electromagnetic, infrared, or semiconductor systems, devices or equipment, or any suitable combination of the foregoing. Alternatively, a computer-readable storage medium may be a machine-readable signal medium. A more specific example of a machine-readable storage medium may include an electrical connection based on one or more lines, a portable computer disk, a hard disk, a random access memory (RAM), a read-only memory (ROM), an erasable programmable read-only memory (EPROM or flash memory), an optical fiber, a portable compact disk read-only memory (CD-ROM), an optical storage device, a magnetic storage device, or any suitable combination of the foregoing.
[0113] To provide interaction with a user, the systems and techniques described herein may be implemented on an electronic device having: a display device (e.g., a CRT (cathode ray tube) or LCD (liquid crystal display) monitor) for displaying information to the user; and a keyboard and a pointing device (e.g., a mouse or trackball) through which the user can provide input to the electronic device. Other types of devices may also be used to provide interaction with the user; for example, the feedback provided to the user may be any form of sensory feedback (e.g., visual feedback, auditory feedback, or tactile feedback); and input from the user may be received in any form (including acoustic input, voice input, or tactile input).
[0114] The systems and techniques described herein may be implemented in a computing system that includes backend components (e.g., as a data server), or a computing system that includes middleware components (e.g., an application server), or a computing system that includes frontend components (e.g., a user computer with a graphical user interface or a web browser through which a user can interact with implementations of the systems and techniques described herein), or a computing system that includes any combination of such backend components, middleware components, or frontend components. The components of the system may be interconnected by any form or medium of digital data communication (e.g., a communication network). Examples of communication networks include: a local area network (LAN), a wide area network (WAN), a blockchain network, and the Internet.
[0115] A computing system may include a client and a server. The client and the server are generally remote from each other and usually interact through a communication network. The client and server relationship is generated by computer programs running on the corresponding computers and having a client-server relationship with each other. The server may be a cloud server, also known as a cloud computing server or cloud host, which is a host product in the cloud computing service system to solve the defects of difficult management and weak business scalability in traditional physical hosts and VPS services.
[0116] It should be understood that the various forms of processes shown above can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.
[0117] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for adjusting the sulfur content in molten iron of a blast furnace, characterized in that: include: Obtaining the first sulfur content influencing factor of the blast furnace raw material in the previous smelting cycle and the second sulfur content influencing factor of the blast furnace raw material in the current smelting cycle; performing correlation processing on the first sulfur content influencing factors to determine correlation coefficients between the first sulfur content influencing factors; Calculating a predicted value of sulfur content in molten iron according to the second sulfur content influencing factor, the correlation coefficient and a preset correction coefficient; Based on the preset target sulfur content of the molten iron and the predicted value of the sulfur content of the molten iron, the preset target fuel ratio is adjusted so that the preset target sulfur content of the molten iron is equal to the predicted value of the sulfur content of the molten iron.
2. The adjustment method according to claim 1, characterized in that: The first sulfur content influencing factor includes the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle; the correlation coefficient includes the first correlation coefficient; Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors includes: According to the sulfur content of the molten iron and the temperature of the molten iron in the previous smelting cycle, the first correlation coefficient between the first sulfur content influencing factors is calculated using the following formula: Wherein, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of the molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of the molten iron in the previous smelting cycle and the temperature of the molten iron in the previous smelting cycle.
3. The adjustment method according to claim 2, characterized in that: The first sulfur content influencing factor also includes the basicity of the charge in the previous smelting cycle; the correlation coefficient also includes a second correlation coefficient; Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors further includes: According to the sulfur content of the molten iron and the basicity of the charge in the previous smelting cycle, the second correlation coefficient between the first sulfur content influencing factors is calculated using the following formula: Wherein, r(S1, R1) is the second correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, R1 is the basicity of the charge in the previous smelting cycle, cov(S1, R1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the basicity of the charge in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the basicity of the charge in the previous smelting cycle.
4. The adjustment method according to claim 2, characterized in that: The first sulfur content influencing factor also includes the furnace activity offset in the previous smelting cycle; the correlation coefficient also includes a third correlation coefficient; Performing correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors further includes: According to the sulfur content of the molten iron and the hearth activity offset in the previous smelting cycle, the third correlation coefficient between the first sulfur content influencing factors is calculated using the following formula: Wherein, r(S1, y1) is the third correlation coefficient, S1 is the sulfur content of molten iron in the previous smelting cycle, y1 is the hearth activity offset in the previous smelting cycle, cov(S1, y1) is the covariance of the sulfur content of molten iron in the previous smelting cycle and the hearth activity offset in the previous smelting cycle, It is the variance of the sulfur content of molten iron in the previous smelting cycle and the activity offset of the hearth in the previous smelting cycle.
5. The adjustment method according to claim 1, characterized in that: The second sulfur content influencing factor includes the molten iron temperature in the current smelting cycle, the basicity of the charge in the current smelting cycle, and the activity offset of the furnace in the current smelting cycle; The calculating the predicted value of the sulfur content in the molten iron according to the second sulfur content influencing factor, the correlation coefficient and the preset correction coefficient comprises: According to the molten iron temperature in the current smelting cycle, the charge basicity in the current smelting cycle, the furnace activity offset in the current smelting cycle, the correlation coefficient and the preset correction coefficient, the following formula is used to calculate the predicted value of the molten iron sulfur content: ((rR0+rT0+ry0) / 3)×β, where r is the correlation coefficient, R0 is the basicity of the charge in the current smelting cycle; T0 is the molten iron temperature in the current smelting cycle, y0 is the furnace activity offset in the current smelting cycle, and β is the preset correction coefficient.
6. The adjustment method according to claim 1, characterized in that: The adjusting the preset target fuel ratio based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content comprises: When the preset target molten iron sulfur content is less than the molten iron sulfur content prediction value, reducing the preset target fuel ratio; When the preset target molten iron sulfur content is greater than the predicted value of the molten iron sulfur content, the preset target fuel ratio is increased.
7. A device for regulating the sulfur content in molten iron of a blast furnace, characterized in that: include: An acquisition module, the acquisition module is used to acquire a first sulfur content influencing factor of a blast furnace raw material in a previous smelting cycle, and a second sulfur content influencing factor of a blast furnace raw material in a current smelting cycle; A correlation coefficient determination module, wherein the correlation coefficient calculation module is used to perform correlation processing on the first sulfur content influencing factors to determine the correlation coefficients between the first sulfur content influencing factors; A molten iron sulfur content prediction value calculation module, the molten iron sulfur content prediction value calculation module is used to calculate the molten iron sulfur content prediction value according to the second sulfur content influencing factor, the correlation coefficient and a preset correction coefficient; The regulating module is used to adjust the preset target fuel ratio based on the preset target molten iron sulfur content and the predicted value of the molten iron sulfur content, so that the preset target molten iron sulfur content is equal to the predicted value of the molten iron sulfur content.
8. The adjusting device according to claim 7, characterized in that: The correlation coefficient determination module includes a first correlation coefficient calculation submodule, which is used to calculate the first correlation coefficient between the first sulfur content influencing factors according to the molten iron sulfur content and the molten iron temperature in the previous smelting cycle using the following formula: Wherein, r(S1, T1) is the first correlation coefficient, S1 is the sulfur content of the molten iron in the previous smelting cycle, T1 is the molten iron temperature in the previous smelting cycle, cov(S1, T1) is the covariance of the sulfur content of the molten iron in the previous smelting cycle and the molten iron temperature in the previous smelting cycle, It is the variance of the sulfur content of the molten iron in the previous smelting cycle and the temperature of the molten iron in the previous smelting cycle.
9. An electronic device, characterized in that: The electronic device comprises: at least one processor; and a memory communicatively connected to the at least one processor; wherein, The memory stores a computer program executable by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can execute the method for adjusting the sulfur content in blast furnace molten iron according to any one of claims 1-6.
10. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores computer instructions, and the computer instructions are used to enable a processor to implement the method for adjusting the sulfur content in molten iron in a blast furnace according to any one of claims 1 to 6 when executed.