Thick Q355B hot rolled steel coil and production method thereof
By adjusting chemical composition and controlled rolling and cooling technology, the manganese content in the thick-spec Q355B hot-rolled steel coil is reduced, and titanium alloy is used to replace part of manganese. Combined with controlled rolling and cooling technology and laminar flow cooling technology, the increase in manganese costs is solved. The problem has achieved cost savings and performance maintenance, with significant economic benefits and environmental value.
Patent Information
- Application Number
- CN202410958016.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-11-01
AI Technical Summary
The production costs of existing thick-specification Q355B low alloy high-strength hot-rolled steel coils have increased due to the increase in ferromanganese costs. It is necessary to explore ways to reduce manganese content to reduce production costs while maintaining material performance.
By adjusting the chemical composition, the titanium alloy is controlled by controlling carbon (C) by 0.15-0.20%, manganese (Mn) by 0.60-0.75%, titanium (Ti) by 0.038-0.05%, and controlled rolling and cooling technology, including rough rolling and final rolling, is adopted. and finish rolling final rolling temperature control, as well as laminar flow cooling technology, ensures refinement and rapid cooling of austenite grains.
It effectively reduces the use of manganese, reduces production costs, and maintains the excellent mechanical properties of steel, complies with national standards, and has significant economic benefits and environmental value.
Abstract
Description
Technical Field
[0001] The invention belongs to the field of steel, and relates to a thick specification Q355B hot-rolled steel coil and a production method thereof. Background Art
[0002] Low alloy high strength structural steel Q355B hot rolled steel coil is widely used in many key industrial fields due to its excellent mechanical properties and cost-effectiveness, such as bridge construction, automobile manufacturing, shipbuilding, construction engineering, pressure vessels and special equipment. This type of steel can provide high strength and toughness while maintaining good weldability and formability through reasonable alloying and heat treatment processes, meeting the strict requirements of modern engineering projects.
[0003] At present, the production of thick-gauge Q355B low-alloy high-strength hot-rolled steel coils (thickness range 3.0-20mm) on the market generally relies on carbon and manganese as the main strengthening elements, and adopts a high-carbon and high-manganese chemical composition design strategy, that is, the carbon (C) content is controlled at 0.15% to 0.20%, and the manganese (Mn) content is set between 1.20% and 1.60%. This design aims to improve the hardness and tensile strength of the material through the synergistic effect of carbon and manganese. However, in recent years, with the continuous increase in the cost of ferromanganese, the production cost of such steel has increased significantly, which has posed a considerable economic burden on the entire steel industry and its downstream users.
[0004] Faced with this challenge, the industry urgently needs to explore and develop new alloy strengthening methods, combined with advanced controlled rolling and controlled cooling processes, to reduce the use of manganese, reduce production costs, and ensure that the comprehensive performance of the material is not compromised. This is not only conducive to the improvement of economic benefits of steel companies, but also an important measure to respond to the global trend of energy conservation and emission reduction and promote sustainable development. Therefore, research and innovation on new methods to reduce manganese content while maintaining or even improving steel performance is of great significance for saving social resources and promoting industrial upgrading. Summary of the invention
[0005] In view of this, the purpose of the present invention is to provide a thick-gauge Q355B hot-rolled steel coil and a production method thereof, by reducing the Mn content in the steel, adding an appropriate amount of Ti alloy, and through a controlled rolling and controlled cooling process, to ensure that the performance of the thick-gauge Q355B low-alloy high-strength hot-rolled steel coil is qualified, effectively reduce production costs, and save social resources.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solution: a thick specification Q355B hot-rolled steel coil, the chemical composition of which is controlled as follows: carbon (C) 0.15-0.20%, manganese (Mn) 0.60-0.75%, titanium (Ti) 0.038-0.05%, and inevitable impurities and the remainder of iron (Fe).
[0007] Optionally, the thickness specification of the steel coil is 3.0-20mm.
[0008] A production method for a thick-gauge Q355B hot-rolled steel coil is applicable to a thick-gauge Q355B hot-rolled steel coil as described above, and comprises the following steps: the target temperature of the final rough rolling is controlled at 1020-1080°C, the target temperature of the final fine rolling is controlled at 810-900°C, and the final rolling temperature fluctuation range is controlled within ±20°C, and the refinement of austenite grains is achieved through precise temperature control, thereby improving the strength and toughness of the steel.
[0009] Optionally, laminar cooling technology is used after rolling to quickly cool the rolled piece to the phase change region, the coiling temperature is controlled at 550-630°C, and the temperature fluctuation range is controlled within ±20°C.
[0010] The beneficial effect of the present invention is that the present invention proposes an innovative alloying strategy, which achieves significant cost savings while ensuring that thick-gauge Q355B low-alloy high-strength hot-rolled steel coils (thickness 3.0-20 mm) maintain excellent mechanical properties by replacing part of manganese (Mn) with titanium (Ti). Specifically, the key chemical components of the present invention are controlled as follows: carbon (C) 0.15-0.20%, manganese (Mn) 0.60-0.75%, and titanium (Ti) 0.038-0.05%. This composition adjustment effectively reduces the amount of expensive ferromanganese added, thereby reducing the overall production cost and having a positive impact on resource conservation and environmental protection. In addition, the present invention also optimizes the controlled rolling and controlled cooling process parameters to ensure the high performance of the steel. The target temperature of the final rough rolling is controlled at 1020-1080°C, the target temperature of the final fine rolling is controlled at 810-900°C, and the thickness group spacing is controlled. The final rolling temperature fluctuation range is strictly controlled within ±20°C. This series of measures promotes the fine control of austenite grains and significantly improves the strength and toughness of the steel. The subsequent laminar cooling process, through rapid cooling to the phase change region, accurately controls the coiling temperature at 550-630°C. The thickness group spacing is also controlled to ensure that the temperature fluctuation does not exceed ±20°C, effectively avoiding the abnormal growth of austenite grains, so that the final product fully meets the requirements of national standards.
[0011] In summary, the present invention has not only achieved a breakthrough in reducing costs, but also achieved efficient utilization of resources on the basis of ensuring that material performance meets standards, demonstrating significant economic benefits and environmental value, and is of great significance for promoting the development of the low-alloy high-strength structural steel industry in a green and sustainable direction.
[0012] Other advantages, objectives and features of the present invention will be described in the following description to some extent, and to some extent, will be obvious to those skilled in the art based on the following examination and study, or can be taught from the practice of the present invention. The objectives and other advantages of the present invention can be realized and obtained through the following description. DETAILED DESCRIPTION
[0013] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0014] The invention discloses a thick specification Q355B hot-rolled steel coil, the chemical composition of which is controlled as follows: carbon (C) 0.15-0.20%, manganese (Mn) 0.60-0.75%, titanium (Ti) 0.038-0.05%, inevitable impurities and residual iron (Fe), and the thickness specification of the steel coil is 3.0-20mm.
[0015] A production method of a thick-gauge Q355B hot-rolled steel coil is applicable to a thick-gauge Q355B hot-rolled steel coil as described above, and comprises the following steps: the target temperature of the final rough rolling is controlled at 1020-1080°C, the target temperature of the final fine rolling is controlled at 810-900°C, and the final rolling temperature fluctuation range is controlled within ±20°C, and the refinement of austenite grains is achieved through precise temperature control, thereby improving the strength and toughness of the steel; after rolling, laminar cooling technology is adopted to rapidly cool the rolled piece to a phase change region, the coiling temperature is controlled at 550-630°C, and the temperature fluctuation range is controlled within ±20°C.
[0016] The thick-gauge Q355B hot-rolled steel coil produced by this process has excellent performance: ① All indicators meet the requirements of the national standard GB / T1591-2018; ② Stable performance and large reserve of mechanical properties; ③ Good welding performance, suitable for various welding methods; ④ The problem of crack defects that are prone to occur when the hot charging temperature of high manganese steel billet is higher than 600℃ is solved, and the hot charging temperature is increased.
[0017] Products produced using this process can reduce production costs by 45 yuan per ton of steel.
[0018] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution, which should be included in the scope of the claims of the present invention.
Claims
1. A thick Q355B hot-rolled steel coil, characterized in that: The chemical composition of the steel coil is controlled as follows: carbon (C) 0.15-0.20%, manganese (Mn) 0.60-0.75%, titanium (Ti) 0.038-0.05%, and inevitable impurities and the remainder of iron (Fe).
2. The thick Q355B hot-rolled steel coil according to claim 1, characterized in that: The thickness of the steel coil is 3.0-20mm.
3. A method for producing a thick Q355B hot-rolled steel coil, applicable to a thick Q355B hot-rolled steel coil as claimed in any one of claims 1 or 2, characterized in that: The following steps are involved: The target temperature of the final rough rolling is controlled at 1020-1080℃, the target temperature of the final finishing rolling is controlled at 810-900℃, and the final rolling temperature fluctuation range is controlled within ±20℃. The refinement of austenite grains is achieved through precise temperature control, thereby improving the strength and toughness of the steel.
4. The method for producing a thick Q355B hot-rolled steel coil according to claim 3, characterized in that: After rolling, laminar cooling technology is used to quickly cool the rolled piece to the phase change region. The coiling temperature is controlled at 550-630°C, and the temperature fluctuation range is controlled within ±20°C.