High-temperature anti-oxidation coating processing device for neodymium-iron-boron alloy
An anti-oxidation coating was formed on the surface of NdFeB alloy by vacuum evaporation deposition technology, which solved the problem of coating peeling off at high temperature and improved the anti-oxidation performance of NdFeB alloy.
Patent Information
- Application Number
- CN202410912114.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-11-01
AI Technical Summary
In existing technologies, neodymium iron boron alloy coatings are prone to oxidation and peeling at high temperatures, making it difficult to effectively protect their surface.
An anti-oxidation coating is formed on the surface of NdFeB alloy using vacuum evaporation deposition technology. The alumina is heated by a grid and heating wire in a vacuum box to evaporate and deposit on the surface of NdFeB alloy, forming a high-temperature anti-oxidation coating.
This achieves strong coating adhesion, prevents oxidation and peeling at high temperatures, and improves the oxidation resistance of NdFeB alloys.
Smart Images

Figure CN118880245A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of NdFeB alloys, and more particularly to a high-temperature oxidation-resistant coating processing device for NdFeB alloys. Background Art
[0002] NdFeB alloy is a rare earth permanent magnet alloy composed of neodymium, iron and boron elements, with very high magnetic properties and energy density. Due to its excellent magnetic properties, NdFeB alloy is widely used in motors, sensors, magnetic transmission, medical equipment and other fields. The characteristics of NdFeB alloy include: High magnetic properties: It has very high remanence and coercivity, and is one of the most excellent magnetic materials known so far. High energy density: It has high energy density and can provide a strong magnetic field in a small volume. In order to improve the high temperature and oxidation resistance of NdFeB alloy, the outside of NdFeB alloy needs to be processed. When the coating is directly brushed onto the NdFeB alloy, the coating is easy to fall off. Summary of the invention
[0003] In order to overcome the deficiencies of the prior art, the present invention provides a high-temperature anti-oxidation coating processing device for NdFeB alloy, which has the beneficial effect that the anti-oxidation coating can be deposited on the NdFeB alloy by vacuum evaporation, and the coating is not easy to fall off.
[0004] A high-temperature anti-oxidation coating processing device for NdFeB alloy comprises a vacuum box in which a plurality of grids are arranged.
[0005] A vacuum pipe is arranged on one side of the vacuum box, and a one-way valve is arranged on the vacuum pipe.
[0006] The upper side of the vacuum box is provided with a cover plate, the lower side of the cover plate is provided with a boss, the boss is inserted into the upper part of the vacuum box, and a fixing platform is fixed on one side of the vacuum box.
[0007] An inclined plate is arranged on the upper part of the cover plate.
[0008] The utility model also comprises a base, a stand frame is fixed on the base, and a vacuum box is fixed on the lower part of the stand frame. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.
[0010] Figure 1 A schematic diagram of the structure of a high-temperature oxidation-resistant coating processing device for NdFeB alloy Figure 1 ;
[0011] Figure 2 A schematic diagram of the structure of a high-temperature oxidation-resistant coating processing device for NdFeB alloy Figure 2 ;
[0012] Figure 3 A schematic diagram of the structure of a high-temperature oxidation-resistant coating processing device for NdFeB alloy Figure 3 ;
[0013] Figure 4 A schematic diagram of the structure of a high-temperature oxidation-resistant coating processing device for NdFeB alloy Figure 4 ;
[0014] Figure 5 Schematic diagram of the vacuum box structure Figure 1 ;
[0015] Figure 6 Schematic diagram of the vacuum box structure Figure 2 ;
[0016] Figure 7 The structure of the stand is shown in Figure 1. Figure 1 ;
[0017] Figure 8 The structure of the stand is shown in Figure 1. Figure 2 ;
[0018] Fig. 9 The structure of the pad is shown in Figure 1. Figure 1 ;
[0019] Fig.10 The structure of the pad is shown in Figure 1. Figure 2 ;
[0020] Fig.11 The structure of the cross Figure 1 ;
[0021] Fig.12 The structure of the cross Figure 2 .
[0022] In the figure: vacuum box 101; heating wire 102; boss 103; cover plate 104; inclined plate 105; exhaust pipe 106; grille 107; check valve 108; fixing platform 109;
[0023] Stand 201; hydraulic cylinder 202; translation frame 203; motor 204; grinding disc 205; base 206;
[0024] Cushion block 301; carriage 302; hydraulic cylinder 2 303; empty seat 304;
[0025] Cross 401; hydraulic cylinder three 402; hinged rod 403; hydraulic cylinder four 404; clamping bar 405; sliding fork 406; motor two 407; protruding piece 408; turntable 409. DETAILED DESCRIPTION
[0026] like Figure 5-6As shown, this example can achieve the effect of forming a high-temperature anti-oxidation coating and preventing the high-temperature anti-oxidation coating from falling off.
[0027] Since the high temperature anti-oxidation coating processing device of NdFeB alloy includes a vacuum box 101, a plurality of grids 107 are arranged in the vacuum box 101. The plurality of grids 107 are used to place NdFeB alloy, and aluminum oxide is placed at the bottom of the vacuum box 101. The vacuum box 101 is evacuated, and a plurality of electric heating wires 102 heat the aluminum oxide, so that the aluminum oxide evaporates and deposits on the NdFeB alloy to form a high temperature anti-oxidation coating, thereby preventing the high temperature anti-oxidation coating from falling off.
[0028] like Figure 5-6 As shown, this example can achieve the effect of conveniently evacuating the vacuum box 101 into a vacuum.
[0029] Since a vacuum box 101 is provided with a vacuum pipe 106 on one side, a one-way valve 108 is provided on the vacuum pipe 106, and the one-way valve 108 allows air to be drawn through the vacuum pipe 106, so as to conveniently draw a vacuum into the vacuum box 101. The one-way valve 108 can be opened to allow air to enter the vacuum pipe 106, so that the pressure inside and outside the vacuum box 101 is balanced.
[0030] like Figure 5-6 As shown, this example can achieve the effect of sealing the upper side of the vacuum box 101 .
[0031] Since the upper side of the vacuum box 101 is provided with a cover plate 104, the lower side of the cover plate 104 is provided with a boss 103, the boss 103 is inserted into the upper part of the vacuum box 101, and a fixing platform 109 is welded on one side of the vacuum box 101, the cover plate 104 is covered on the vacuum box 101 through the boss 103, thereby sealing the upper side of the vacuum box 101. After the cover plate 104 is opened, the cover plate 104 can be temporarily placed on the fixing platform 109.
[0032] like Figure 5-6 As shown, this example can achieve the effect of making the debris that falls on the upper side of the cover plate 104 slide down automatically.
[0033] Since the upper portion of the cover plate 104 is provided with an inclined plate 105 , the inclined plate 105 allows the sundries falling on the upper side of the cover plate 104 to slide down automatically.
[0034] like Figure 5-8 As shown, this example can achieve the effect of supporting the vacuum box 101 .
[0035] Since the processing device further includes a base 206 , the base 206 is connected to the stand 201 by screws, and the vacuum box 101 is connected to the lower part of the stand 201 by screws, the vacuum box 101 can be supported by the base 206 and the stand 201 .
[0036] like Figure 7-8 As shown, this example can achieve the effect of grinding one side of a rectangular NdFeB alloy.
[0037] Since the upper part of the vertical frame 201 is connected to the translation frame 203 for sliding in the left and right directions, the translation frame 203 is driven to slide by the hydraulic cylinder 202, and the lower part of the translation frame 203 is connected to the motor 204 by screws. The output shaft of the motor 204 is connected to the grinding disk 205. The motor 204 can drive the grinding disk 205 to rotate, and one side of the rectangular NdFeB alloy is polished through the right side of the grinding disk 205. After the NdFeB alloy is polished, it is easy for the aluminum oxide to evaporate and deposit on the NdFeB alloy.
[0038] like Figure 11-12 As shown, this example can achieve the effect of conveniently grinding all surfaces of the rectangular NdFeB alloy.
[0039] Since a cross 401 is welded to the right part of the stand 201, the four ends of the cross 401 are slidably connected with clamps 405, and the ends of the clamps 405 are connected to motor 2 407 by screws. A turntable 409 is connected to the output shaft of motor 2 407. The rectangular NdFeB alloy can be clamped up and down by bringing the upper and lower turntables 409 closer to each other, and the rectangular NdFeB alloy can be clamped front and back by bringing the front and rear turntables 409 closer to each other, and then each turntable 409 can drive the corresponding turntable 409 to rotate. After the two turntables 409 clamp the NdFeB alloy, the NdFeB alloy can be driven to rotate with the turntable 409, and then different surfaces of the NdFeB alloy are polished toward the polishing disk 205, so that all surfaces of the rectangular NdFeB alloy can be polished conveniently.
[0040] like Figure 11-12 As shown, this example can achieve the effect of preventing the NdFeB alloy from shaking during grinding.
[0041] Since the back of the turntable 409 is welded with four protruding pieces 408 in a ring shape, a sliding fork 406 is slidably connected to the clamping strip 405, and the sliding fork 406 is inserted into one of the protruding pieces 408. The sliding fork 406 is driven to slide by the hydraulic cylinder 404. The driving sliding fork 406 to insert into one of the protruding pieces 408 can fix the corresponding turntable 409. When the NdFeB alloy needs to be polished, the positions of the two turntables 409 clamping the NdFeB alloy are fixed, and then the NdFeB alloy is stably fixed to prevent the NdFeB alloy from shaking during polishing.
[0042] like Figure 11-12 As shown, this example can achieve the effect of exposing different surfaces of the rectangular NdFeB alloy for grinding.
[0043] Since the processing device also includes four hinged rods 403, the four hinged rods 403 are hinged to each other, and the four hinge points of the four hinged rods 403 are connected to four clamping strips 405, and a hydraulic cylinder three 402 is fixed to one of the clamping strips 405, and the movable end of the hydraulic cylinder three 402 is fixed to the cross 401. Since the four hinged rods 403 form a parallelogram mechanism, when the upper and lower clamping strips 405 are close to each other, the front and rear clamping strips 405 automatically move away from each other; when the upper and lower clamping strips 405 move away from each other, the front and rear clamping strips 405 automatically move closer to each other, thereby facilitating switching between the front and rear and upper and lower clamping modes, and facilitating exposing different surfaces of the rectangular NdFeB alloy for grinding.
[0044] like Figure 9-12 As shown, this example can achieve the effect of preventing the NdFeB alloy from moving to the right due to pressure when grinding the NdFeB alloy.
[0045] Since an empty seat 304 is welded in the middle of the cross 401, a slide 302 is slidably connected to the empty seat 304, a cushion block 301 is fixed to the end of the slide 302, and the slide 302 is driven to slide by the second hydraulic cylinder 303. When the grinding disc 205 grinds the left side of the rectangular NdFeB alloy, the second hydraulic cylinder 303 drives the slide 302 to move leftward on the empty seat 304, so that the cushion block 301 presses on the right side of the rectangular NdFeB alloy to prevent the NdFeB alloy from moving rightward under pressure when grinding the NdFeB alloy. When the NdFeB alloy needs to be pushed into the vacuum box 101, the cushion block 301 is driven to move leftward to push the NdFeB alloy into the vacuum box 101 at the lower side.
Claims
1. A high temperature anti-oxidation coating processing device for NdFeB alloy, comprising a vacuum box (101), characterized in that: A plurality of grids (107) are arranged in the vacuum box (101), and a plurality of electric heating wires (102) are evenly distributed at the bottom of the vacuum box (101).
2. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 1, characterized in that: A vacuum tube (106) is provided on one side of the vacuum box (101), and a one-way valve (108) is provided on the vacuum tube (106).
3. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 2, characterized in that: The upper side of the vacuum box (101) is provided with a cover plate (104), the lower side of the cover plate (104) is provided with a boss (103), the boss (103) is inserted into the upper part of the vacuum box (101), and a fixing platform (109) is fixed on one side of the vacuum box (101).
4. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 3, characterized in that: An inclined plate (105) is provided on the upper portion of the cover plate (104).
5. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 4, characterized in that: It also includes a base (206), a stand (201) is fixed on the base (206), and the vacuum box (101) is fixed at the lower part of the stand (201).
6. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 5, characterized in that: The upper part of the vertical frame (201) is connected to a translation frame (203) in a sliding manner in the left-right direction. The translation frame (203) is driven to slide by a hydraulic cylinder (202). A motor (204) is fixed to the lower part of the translation frame (203). A grinding disc (205) is fixed to the output shaft of the motor (204).
7. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 6, characterized in that: A cross (401) is fixed to the right part of the stand (201), and four ends of the cross (401) are slidably connected with clamping strips (405), and a second motor (407) is fixed to the end of the clamping strip (405), and a rotating disk (409) is fixed on the output shaft of the second motor (407).
8. The high temperature anti-oxidation coating processing device of NdFeB alloy according to claim 7, characterized in that: The back of the rotating disk (409) is fixed with four protruding pieces (408) in a ring shape, and a sliding fork (406) is slidably connected to the clamping strip (405). The sliding fork (406) is inserted into one of the protruding pieces (408), and the sliding fork (406) is driven to slide by a hydraulic cylinder (404).
9. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 8, characterized in that: It also includes four hinged rods (403), the four hinged rods (403) are hinged to each other, the four hinge points of the four hinged rods (403) are connected to four clamping strips (405), a hydraulic cylinder three (402) is fixed on one of the clamping strips (405), and the movable end of the hydraulic cylinder three (402) is fixed on the cross (401).
10. The high temperature oxidation resistant coating processing device of NdFeB alloy according to claim 9, characterized in that: An empty seat (304) is fixed in the middle of the cross (401), a slide (302) is slidably connected to the empty seat (304), a cushion block (301) is fixed at the end of the slide (302), and the slide (302) is driven to slide by a second hydraulic cylinder (303).