Manufacturing method of ferroelectric memory and ferroelectric memory structure
By forming deep-hole capacitors on semiconductor substrates and combining photolithography and etching processes, the problem of insufficient integration of 3D ferroelectric memory has been solved, achieving improved storage density and process compatibility, and reducing manufacturing costs.
Patent Information
- Application Number
- CN202411085676.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-01
AI Technical Summary
Existing 3D ferroelectric memories have insufficient integration, which limits the improvement of storage density, and they also have poor compatibility with traditional processes.
Deep-hole capacitors are formed on semiconductor substrates by depositing electrode materials and high-dielectric-constant ferroelectric oxide layers, combined with photolithography and etching processes to form the capacitor structure, which is then connected to metal interconnects and board lines to improve storage density.
Without altering the existing standard FAB process, the integration and storage density of ferroelectric memory have been improved, while manufacturing costs have been reduced.
Smart Images

Figure CN118890903A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of memory technology, and in particular to a manufacturing method of a ferroelectric memory and a ferroelectric memory structure. Background Art
[0002] Ferroelectric memory is a non-volatile memory with a special process. When an electric field is applied to the ferroelectric transistor, the central atom stops at the first low energy state along the electric field, and when the electric field is reversed and applied to the same ferroelectric transistor, the central atom moves in the crystal along the direction of the electric field and stops at the second low energy state. A large number of central atoms move and couple in the crystal unit cell to form ferroelectric domains, which form polarized charges under the action of the electric field. The polarized charge formed by the reversal of the ferroelectric domain under the electric field is higher, and the polarized charge formed by the non-reversal of the ferroelectric domain under the electric field is lower. This binary stable state of ferroelectric materials allows ferroelectrics to be used as memory. When the electric field is removed, the central atom remains in a low energy state, and the state of the memory is preserved and will not disappear.
[0003] The ferroelectric domain can be reversed under an electric field to form a high polarized charge, or there is no inversion to form a low polarized charge to determine whether the storage unit is in the "1" or "0" state. The reversal of the ferroelectric domain does not require a high electric field, and only a normal operating voltage can change the state of the storage unit to "1" or "0". There is no need for a charge pump to generate high voltage data erasure, so there is no erase delay phenomenon. This feature makes the ferroelectric memory write fast and has an unlimited write life, and it is not easy to be written out. In addition, compared with existing non-volatile memory technology, ferroelectric memory has a higher write speed and a longer read and write life.
[0004] Figure 1 A circuit schematic diagram of an exemplary ferroelectric memory cell is shown. A ferroelectric memory cell is a storage element of a ferroelectric memory device and can include various designs and configurations. Figure 1 As shown in FIG. 1 , the ferroelectric memory cell is a "1T-1C" cell, which includes a capacitor and a transistor. The transistor is an NMOS transistor. The source S of the transistor is electrically connected to the bit line BL, the gate of the transistor is electrically connected to the word line WL, the drain D of the transistor is electrically connected to the lower electrode of the capacitor, and the upper electrode of the capacitor is connected to the plate line PL. There are two common structures of ferroelectric memory devices, namely Figure 2 and 3 As shown, Figure 2 The figure shows the COB (Capacitor Over BL) structure where the capacitor is located above the bit line. Figure 3 The figure shows the CUB (Capacitor Under BL) structure where the capacitor is located under the bit line. In comparison, the CUB structure can basically be implemented using a standard FAB process, has better process compatibility, and is more compact.
[0005] In addition, in order to ensure that a strong signal can be obtained when the polarization of the ferroelectric capacitor of the ferroelectric memory cell changes, the area of the ferroelectric capacitor needs to be large enough. The ferroelectric capacitor of the planar 2D ferroelectric memory occupies a large area, which limits the integration of the 2D ferroelectric memory cell. Although some products are beginning to adopt three-dimensional (3D) ferroelectric memory structures, as the integration of products increases, the storage density requirements for ferroelectric memory cells are also getting higher and higher. Summary of the invention
[0006] In view of some or all of the problems in the prior art, the present invention provides a method for manufacturing a ferroelectric memory in a first aspect, which can further improve the integration of ferroelectric memory cells on the basis of the existing 3D deep trench capacitor. The manufacturing method comprises: Providing a semiconductor substrate, the semiconductor substrate comprising a ferroelectric memory cell region, the ferroelectric memory cell region having a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region; forming a first interconnect structure, the first interconnect structure comprising conductive pillars and a first dielectric layer between the conductive pillars, wherein the conductive pillars comprise first capacitor conductive pillars and first bit line conductive pillars; forming a second dielectric layer and a first sacrificial layer in sequence on the surface of the first dielectric layer; Forming a deep hole in the second dielectric layer and the first sacrificial layer by photolithography and etching processes, wherein the bottom of the deep hole exposes the end surface of the first capacitor conductive column; Depositing electrode material on the deep hole and the surface of the first sacrificial layer to form a first electrode layer; Removing part of the electrode material, leaving only the first electrode layer at the bottom and side of the deep hole; removing the first sacrificial layer; forming a high-K ferroelectric oxide layer and a second electrode layer in sequence on the surfaces of the first electrode layer and the second dielectric layer to form a capacitor structure; forming a filling layer, wherein a surface of the filling layer is not lower than a surface of the second electrode layer; Removing part of the second electrode layer and the high dielectric constant ferroelectric oxide layer on the top surface by photolithography and etching processes, so that each capacitor is separated from each other; Metal interconnects and plate and bit lines are formed.
[0007] Furthermore, the manufacturing method further comprises: forming an etch stop layer on the surface of the first dielectric layer, and forming a hard mask layer on the surface of the first sacrificial layer, and the forming of the deep hole comprises: patterning the hard mask layer by photolithography and etching processes; Using the patterned hard mask layer as a mask for etching, deep holes are formed in the second dielectric layer and the first sacrificial layer to expose the end surface of the first capacitor conductive column; The hard mask layer is removed.
[0008] Furthermore, the second dielectric layer and the first sacrificial layer are made of different materials.
[0009] Furthermore, the second dielectric layer and the first sacrificial layer are made of the same material, and the manufacturing method further comprises: A barrier layer is formed between the second dielectric layer and the first sacrificial layer.
[0010] Further, removing part of the electrode material includes: forming a second sacrificial layer on a surface of the first electrode layer; Removing the electrode material covering the surface of the first sacrificial layer by an etching process; The second sacrificial layer is removed by a wet removal process.
[0011] Furthermore, the first sacrificial layer is removed while the second sacrificial layer is removed by the same process.
[0012] Furthermore, the filling layer is made of a dielectric material, and the formation of the filling layer includes: forming an etching stop layer on a surface of the second electrode layer; A dielectric material is deposited on the surface of the etch stop layer to form a filling layer.
[0013] Furthermore, the forming of the filling layer includes: A conductive material is deposited on the surface of the second electrode layer to form a filling layer.
[0014] Furthermore, the forming of the filling layer further comprises: TiN is deposited on the surface of the conductive material.
[0015] Furthermore, the manufacturing method further comprises: Part of the second electrode layer and the high dielectric constant (high K) ferroelectric oxide layer on the top surface are removed by photolithography and etching processes, so that each capacitor is separated from each other.
[0016] Furthermore, the manufacturing method further comprises: The surface of the filling layer is flattened by a grinding process.
[0017] Further, forming metal interconnects and plate lines and bit lines includes: Drilling holes on the filling layer to form conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar and a second bit line conductive pillar, one end of the second capacitor conductive pillar is electrically connected to the second electrode layer, and one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the filling layer, wherein a portion electrically connected to the second capacitor conductive column forms a plate line, and a portion electrically connected to the second bit line conductive column forms a bit line.
[0018] Further, forming metal interconnects and plate lines and bit lines includes: forming a second bit line conductive pillar on one side of the capacitor, wherein one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the filling layer, wherein a portion contacting the filling layer forms a plate line, and a portion electrically connected to the second bit line conductive pillar forms a bit line.
[0019] Further, forming metal interconnects and plate lines and bit lines includes: Forming a third dielectric layer on the surface of the filling layer, drilling holes in the third dielectric layer, and forming conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar and a second bit line conductive pillar, one end of the second capacitor conductive pillar is electrically connected to the filling layer, and one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the third dielectric layer, wherein a portion electrically connected to the second capacitor conductive pillar forms a plate line, and a portion electrically connected to the second bit line conductive pillar forms a bit line.
[0020] Based on the manufacturing method as described above, the second aspect of the present invention provides a ferroelectric memory structure, comprising: A semiconductor substrate, wherein the semiconductor substrate comprises a ferroelectric memory cell region, wherein the ferroelectric memory cell region comprises a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region; A first interconnect structure is disposed above the semiconductor substrate, wherein the first interconnect structure comprises a first capacitor conductive column, a first bit line conductive column and a first dielectric layer between the conductive columns; A second dielectric layer stacked on the first dielectric layer; A capacitor, comprising a first electrode layer, a high dielectric constant ferroelectric oxide layer and a second electrode layer, wherein the bottom and part of the side wall of the first electrode layer are deposited on the inner surface of the deep hole of the second dielectric layer and are electrically connected to the first capacitor conductive column, the high dielectric constant ferroelectric oxide layer is deposited on the inner surface of the first electrode layer, the outer surface not covered by the second dielectric layer and the surface of the second dielectric layer, and the second electrode layer is deposited on the surface of the high dielectric constant ferroelectric oxide layer; A plate line and a bit line, wherein the plate line is connected to the second electrode layer through a metal interconnection, and the bit line is connected to the first bit line conductive pillar through a second bit line conductive pillar.
[0021] Furthermore, the interior of the capacitor is filled with a dielectric material, and the plate line is connected to the second electrode plate through a second capacitor conductive column formed in the dielectric material.
[0022] Furthermore, the interior of the capacitor is filled with a conductive material, the plate line is formed on the surface of the conductive material, and is electrically connected to the second electrode plate through the conductive material.
[0023] Furthermore, the ferroelectric memory structure further includes a conductive metal layer, which is electrically connected to the plate line through a conductive column.
[0024] The present invention provides a method for manufacturing a ferroelectric memory and a ferroelectric memory structure. After a sacrificial layer of a certain thickness is set on the surface of the dielectric layer, a deep hole required for manufacturing a capacitor is formed, so that a ferroelectric material and a second electrode layer can also be deposited on a part of the outer surface of the first electrode layer, and then the deep hole volume with the same aspect ratio has a larger area than the traditional deep hole capacitor, which effectively improves the storage density of the ferroelectric memory. At the same time, the manufacturing method is compatible with the standard FAB process, which is easy to integrate and reduces the manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] To further illustrate the above and other advantages and features of various embodiments of the present invention, a more specific description of various embodiments of the present invention will be presented with reference to the accompanying drawings. It will be understood that these drawings only depict typical embodiments of the present invention and are therefore not to be considered as limiting the scope thereof. In the accompanying drawings, for clarity, identical or corresponding parts will be represented by identical or similar reference numerals.
[0026] Figure 1 A circuit schematic diagram showing an exemplary ferroelectric memory cell; Figure 2 A COB ferroelectric memory structure with capacitors located above the bit lines is shown; Figure 3 A CUB ferroelectric memory structure is shown with the capacitor located below the bit line; Figure 4A schematic flow chart showing a method for manufacturing a ferroelectric memory according to an embodiment of the present invention; Figures 5 to 10 A schematic diagram showing a partial process of a method for manufacturing a ferroelectric memory according to an embodiment of the present invention; Fig.11 and 12 A semiconductor substrate with a flat structure and a semiconductor substrate with a vertical structure according to an embodiment of the present invention are respectively shown; Fig.13 A schematic diagram showing a depression formed beside a conductive pillar during deep hole etching according to an embodiment of the present invention; Figures 14 to 16 A schematic diagram showing a process of etching a portion of the first electrode layer according to an embodiment of the present invention; Figures 17 to 22 Schematic diagrams of capacitor structures with different filling layers according to different embodiments of the present invention are respectively shown; Figures 23 to 26 Schematic diagrams showing plate lines and bit lines of ferroelectric memory devices according to different embodiments of the present invention; Figures 27 to 29 A schematic diagram showing a process of forming a plate line and a bit line of a ferroelectric memory according to an embodiment of the present invention. DETAILED DESCRIPTION
[0027] In the following description, the present invention is described with reference to various embodiments. However, those skilled in the art will recognize that various embodiments can be implemented without one or more specific details or with other replacement and / or additional methods, materials or components. In other cases, well-known structures, materials or operations are not shown or described in detail to avoid blurring the inventive point of the present invention. Similarly, for the purpose of explanation, specific quantities, materials and configurations are set forth to provide a comprehensive understanding of embodiments of the present invention. However, the present invention is not limited to these specific details. In addition, it should be understood that the various embodiments shown in the drawings are illustrative representations and are not necessarily drawn in correct proportions.
[0028] In this specification, reference to "one embodiment" or "the embodiment" means that a particular feature, structure, or characteristic described in conjunction with the embodiment is included in at least one embodiment of the present invention. The phrase "in one embodiment" appearing in various places in this specification does not necessarily all refer to the same embodiment.
[0029] In general, terms can be understood, at least in part, based on the context in which they are used. For example, the term "one or more" as used herein can be used to describe any feature, structure, or characteristic in the singular, or to describe a combination of features, structures, or characteristics in the plural, based at least in part on the context. Similarly, terms such as "a," "an," or "the" can also be understood, at least in part, based on the context, to express singular usage or to express plural usage.
[0030] It can be easily understood that the meaning of “on,” “over,” and “above” in the present invention should be interpreted in the broadest manner, so that “on” not only means being directly on something, but also includes being on something with intervening features or layers between the two, and “on,” or “above” not only means being on or over something, but also includes being on or over something (i.e., directly on something) without intervening features or layers between the two.
[0031] In addition, spatially relative terms, such as "below", "beneath", "lower", "above", "upper", etc., may be used herein for convenience to describe the relationship of one element or feature relative to another element or feature as shown in the drawings. Spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings. The device may be otherwise oriented (rotated 90° or at other orientations) and the spatially relative descriptors used herein should be interpreted accordingly.
[0032] It should be noted that the embodiments of the present invention describe the process steps in a specific order, but this is only for the purpose of illustrating the specific embodiment, rather than limiting the order of the steps. On the contrary, in different embodiments of the present invention, the order of the steps can be adjusted according to the adjustment of the process.
[0033] The term "substrate" as used herein refers to the material to which subsequent material layers are added. The substrate itself may be patterned. The material added to the substrate may be patterned, or may remain unpatterned. In addition, the substrate may include a variety of semiconductor materials, such as silicon, germanium, gallium arsenide, indium phosphide, etc. Alternatively, the substrate may also be made of electrically non-conductive materials, such as glass, plastic, or sapphire wafers.
[0034] The term "layer" as used herein refers to a material portion including a certain area with thickness. A layer may extend over the entirety of a structure below or above, or may have an extension less than that of a structure below or above. In addition, a layer may be an area of a homogeneous or heterogeneous continuous structure, the thickness of which is less than the thickness of the continuous structure. For example, a layer may be located between any pair of horizontal planes, or at the top or bottom surface of the continuous structure. A layer may extend horizontally, vertically, and / or along a tapered surface. A substrate may be a layer, may include one or more layers therein, and / or may have one or more layers thereon, and / or one or more layers below it. A layer may include multiple layers. For example, an interconnect layer may include one or more conductors and contact layers (wherein contacts, interconnects and / or through-holes are formed) and one or more dielectric layers.
[0035] Figure 4 A schematic flow chart showing a method for manufacturing a ferroelectric memory according to an embodiment of the present invention is shown. Figures 5 to 10 A schematic diagram of a part of the process of a method for manufacturing a ferroelectric memory according to an embodiment of the present invention is shown. As shown in the figure, a method for manufacturing a ferroelectric memory includes: First, in step 301, a semiconductor substrate is provided. The semiconductor substrate 401 may have completed the manufacturing process of the functional area. For example, the substrate 401 includes a circuit area and a ferroelectric memory cell area. The circuit area and the ferroelectric memory cell area have formed the source area, drain area, gate area, isolation area between devices, and electrodes and interconnecting metal lines above each functional area. The circuit area can be used to control the ferroelectric memory cell area. Fig.11 and 12 As shown, the semiconductor substrate may adopt a flat structure or a vertical structure; Next, in step 302, a first interconnect structure is formed. The first interconnect structure is formed on the surface of the semiconductor substrate, such as Figure 5As shown, in one embodiment of the present invention, forming a first interconnect structure includes: forming a first dielectric layer 421 on the surface of the semiconductor substrate, forming a through hole in the first dielectric layer 421 by through hole photolithography and etching, and the through hole exposes the external electrodes of each functional area on the semiconductor substrate; depositing an adhesive layer and a conductive material such as a tungsten metal layer in sequence to fill the through hole; and finally performing a chemical mechanical polishing process to remove the excess first dielectric layer, adhesive layer and conductive material layer, forming a plurality of conductive pillars 422 extending from the electrode on the surface of the semiconductor substrate to the top surface of the first dielectric layer 421. As shown in the figure, titanium nitride can be formed as an adhesive layer between the conductive pillar and the electrode on the surface of the semiconductor substrate and between the conductive pillar and the first dielectric layer (not shown in the figure). In one embodiment of the present invention, the conductive pillar includes a circuit conductive pillar, a first capacitor conductive pillar, a first bit line conductive pillar, etc. The circuit conductive column is connected to the surface electrode of the circuit area, the first capacitor conductive column is used to electrically connect the doped area (source or drain) of the transistor in the ferroelectric memory cell area with the capacitor, and the first bit line conductive column is used to electrically connect another doped area (drain or source) of the transistor in the ferroelectric memory cell area with the bit line.
[0036] In one embodiment of the present invention, the first dielectric layer can be inorganic materials such as silicon oxide, silicon oxynitride, borosilicate glass, phosphorus silicate glass (PSG), borophosphosilicate glass (BPSG), fluorinated glass silicate glass (FSG), low dielectric constant (low-K) dielectric, etc.; it can also be organic materials such as polyimide, photosensitive epoxy resin, solder mask ink, green paint, dry film, photosensitive build-up layer material, bisbenzocyclobutene resin (BCB) or phenylbenzobisoxazole resin (PBO). The first dielectric layer can be made by chemical vapor deposition, rolling, spin coating, spraying, printing, non-spin coating, hot pressing, vacuum lamination, immersion, pressure bonding, etc. The first dielectric layer can be a single material layer or a composite material layer formed by stacking multiple layers of materials.
[0037] Those skilled in the art should understand that the method for forming the first interconnect structure is not limited to the above specific example. In addition, other processes may be performed before or after the first interconnect structure is formed, for example, forming one or more other conductive interconnect structures.
[0038] Next, in step 303, a second dielectric layer and a first sacrificial layer are formed. Figure 6As shown, a second dielectric layer 431 and a first sacrificial layer 432 are sequentially formed on the surface of the first dielectric layer 421. The thickness of the first sacrificial layer 432 may be the same as or different from that of the second dielectric layer 431. The thickness ratio of the second dielectric layer 431 to the first sacrificial layer 432 may be, for example, 1:1, 1:3, 1:4, 4:1, 3:1, etc. The specific thickness ratio may be determined according to the required capacitor area. The material of the second dielectric layer may be the same as or different from that of the first dielectric layer. In order to facilitate the subsequent removal of the sacrificial layer, the material of the second dielectric layer may be the same as or different from that of the first sacrificial layer. If the material of the second dielectric layer is the same as that of the first sacrificial layer, a barrier layer may also be provided between the second dielectric layer and the first sacrificial layer, so that when the first sacrificial layer is subsequently removed, it may stay on the barrier layer to avoid damaging the second dielectric layer. To facilitate the subsequent deep hole etching process, in one embodiment of the present invention, an etching stop layer 433 may be formed on the surface of the first dielectric layer, and silicon nitride SiNx, silicon oxynitride or titanium nitride TiN, amorphous carbon C and other materials may be deposited on the surface of the first sacrificial layer to form a hard mask layer 434; Next, in step 304, a capacitor deep hole is formed. Figure 7 As shown, a deep hole 441 is formed in the second dielectric layer and the first sacrificial layer by photolithography and etching processes, and the bottom of the deep hole exposes the end face of the first capacitor conductive column. In one embodiment of the present invention, the formation of the deep hole includes first patterning the hard mask layer by photolithography and etching processes, and then etching with the patterned hard mask layer as a mask to form a deep hole in the second dielectric layer and the first sacrificial layer to expose the end face of the first capacitor conductive column, and finally removing the hard mask layer. In some embodiments of the present invention, when etching the deep hole, the etching stops when etching reaches the first capacitor conductive column, but the surrounding dielectric layer continues to etch downward, so that a depression is formed around the first capacitor conductive column, such as Fig.13 shown.
[0039] Next, in step 305, a first electrode layer is formed. Electrode material is deposited on the deep hole and the surface of the first sacrificial layer to form a first electrode layer 451. Figure 8As shown, the first electrode layer 451 is an electrode layer of the capacitor, which can be one or more of the following materials: titanium (Ti), titanium nitride (TiN), titanium silicon nitride (TiSiNx), titanium aluminum nitride (TiAlNx), titanium carbonitride (TiCNx), tantalum nitride (TaNx), tantalum silicon nitride (TaSiNx), tantalum aluminum nitride (TaAlNx), tungsten nitride (WNx), tungsten silicide (WSix), tungsten carbonitride (WCNx), ruthenium (Ru), ruthenium oxide (RuOx), iridium (Ir), tungsten (W), carbon (C), doped polysilicon, transparent conductive oxide (TCO) or iridium oxide (IrOx) or a combination of these materials. The first electrode layer 451 can be deposited by one or more processes of atomic layer deposition ALD, chemical vapor deposition CVD, plasma enhanced chemical vapor deposition PECVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD and similar deposition processes; Next, in step 306, part of the electrode material and the first sacrificial layer are removed. Part of the electrode material is removed, leaving only the first electrode layer at the bottom and side of the deep hole, and the first sacrificial layer is removed. Fig. 9 In one embodiment of the present invention, a second sacrificial layer 461 is first formed on the surface of the first electrode layer, as shown in FIG. Fig.14 As shown, the electrode material covering the top surface of the first sacrificial layer is then removed by an etching process, as shown in FIG. Fig.15 As shown, and finally the second sacrificial layer is removed by a wet removal process, such as Fig.16 In one embodiment of the present invention, since the first sacrificial layer and the second sacrificial layer can be made of the same material, the first sacrificial layer can be removed while the second sacrificial layer is removed.
[0040] Next, in step 307, a high dielectric constant (high K) ferroelectric oxide layer and a second electrode layer are formed. A high K ferroelectric oxide layer 471 and a second electrode layer 472 are sequentially formed on the surfaces of the first electrode layer and the second dielectric layer to form a capacitor structure, such as Fig.10The high K ferroelectric oxide layer 471 is a dielectric layer of the capacitor, which is deposited on the inner surface of the first electrode layer, the outer surface not covered by the second dielectric layer, and the surface of the second dielectric layer. The ferroelectric material includes oxygen and one or more ferroelectric metals, including zirconium (Zr), hafnium (Hf), titanium (Ti), aluminum (Al), nickel (Ni) and / or iron (Fe), etc., and the ferroelectric material can be doped with Group II elements (such as calcium (Ca), strontium (Sr) or barium (Ba)); Group III elements (such as scandium (Sc), yttrium (Y), aluminum (Al), gallium (Ga) and indium (In)); and lanthanide elements (i.e., lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu)) or a composite of these materials. In one embodiment of the present invention, the high K ferroelectric oxide layer may be composed of one or more of the above materials, which may include one or more layers of composite materials. The high K ferroelectric oxide layer may be deposited by one or more processes selected from atomic layer deposition ALD, chemical vapor deposition CVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD, and similar deposition processes. The second electrode layer 472 is another electrode layer of the capacitor, and may be, for example, one or more of the following materials: titanium (Ti), titanium nitride (TiN), titanium silicon nitride (TiSiNx), titanium aluminum nitride (TiAlNx), titanium carbonitride (TiCNx), tantalum nitride (TaNx), tantalum silicon nitride (TaSiNx), tantalum aluminum nitride (TaAlNx), tungsten nitride (WNx), tungsten silicide (WSix), tungsten carbonitride (WCNx), ruthenium (Ru), ruthenium oxide (RuOx), iridium (Ir), tungsten (W), carbon (C), doped polysilicon, transparent conductive oxide (TCO) or iridium oxide (IrOx) or a combination of these materials. The second electrode layer 472 may be deposited by one or more of atomic layer deposition ALD, chemical vapor deposition CVD, plasma enhanced chemical vapor deposition PECVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD, and similar deposition processes.
[0041] Next, in step 308, the capacitor is filled. A filling layer is formed, and the surface of the filling layer is not lower than the surface of the second electrode layer. In one embodiment of the present invention, after the filling is completed, a grinding process is further used to flatten the surface of the filling layer. In an embodiment of the present invention, the material of the filling layer can be, for example, tungsten metal W, titanium nitride TiN, carbon C, electrode material poly, copper Cu and other conductive materials, or oxide Ox and other dielectric materials. Depending on the material used, the filling process used is different. Figures 17 to 20 The schematic diagrams of capacitor structures with different filling layers are shown respectively. Fig.17 It is a conductive material, for example, tungsten metal or electrode material 4811 can be deposited by a CVD process to completely or partially fill the capacitor, wherein the surface of the material is higher than the surface of the second electrode layer. The recessed part of the capacitor (deep holes and recesses formed by removing the first sacrificial layer) can also be deposited by a carbon deposition process, and then filled and hardened by baking, UV curing and other processes. Fig.18 The conductive material may be first deposited with tungsten metal or electrode material 4811 by CVD process, carbon deposition, etc. to completely or partially fill the recessed portion of the capacitor (deep hole and the recess formed by removing the first sacrificial layer), wherein the surface of the material is substantially flush with the surface of the second electrode layer, and then titanium nitride 4812 is deposited on the surface of the conductive material by PVD process and polished. In one embodiment of the present invention, the polishing process may also be omitted, thereby obtaining the following Fig.21 Uneven fill layer surface shown. Fig.19 The conductive material is also directly deposited by a process such as PVD, so a hole 4813 may be formed inside, but the top of the conductive material remains continuous, so it does not affect the performance of the capacitor. Similarly, this structure can also be formed without grinding. Fig. 22 Uneven surface shown. Fig. 20 For example, before depositing the dielectric material 4814, an etching stop layer 482 may be formed on the surface of the second electrode layer. The etching stop layer may be made of conductive or non-conductive materials. Different etching ratios may be selected in the subsequent etching process according to the different materials used. Similarly, holes may also be formed in deep holes when depositing dielectric materials. When dielectric materials are used, during the grinding process, the filling layer may be ground to expose the top of the second electrode layer, or part of the dielectric material may be retained.
[0042] Next, in step 309, capacitor cutting is performed by removing a portion of the second electrode layer and the high K ferroelectric oxide layer on the top surface through photolithography and etching processes, so that each capacitor is separated from each other.
[0043] Finally, in step 310, plate lines and bit lines are formed. Depending on the material of the filling layer, the formation process of the plate lines and bit lines is different. Fig.23 and 24 As shown, the filling layer material is a conductive material, and the formation of the plate line and the bit line includes: forming a third dielectric layer 491 on the surface of the filling layer, drilling holes on the third dielectric layer, and forming conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar 492 and a second bit line conductive pillar 493, one end of the second capacitor conductive pillar is electrically connected to the filling layer, and the second bit line conductive pillar further penetrates the second dielectric layer and is electrically connected to the first bit line conductive pillar, and then a conductive metal layer is formed on the surface of the third dielectric layer, wherein the portion electrically connected to the second capacitor conductive pillar forms a plate line 494, and the portion electrically connected to the second bit line conductive pillar forms a bit line 495. When the filling layer is made of tungsten metal, the plate line and the bit line can also be directly formed on the surface of the tungsten metal. Specifically, as Fig.25 As shown, a second bit line conductive pillar 493 is formed on one side of the capacitor, one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar, and then a conductive metal layer is formed on the surface of the filling layer, wherein the portion in contact with the filling layer forms a plate line 494, and the portion electrically connected to the second bit line conductive pillar forms a bit line 495. When a dielectric material is used, such as Fig.26 As shown, forming metal interconnects and plate lines and bit lines includes drilling holes on the filling layer and forming conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar 492 and a second bit line conductive pillar 493, one end of the second capacitor conductive pillar is electrically connected to the second electrode layer, and one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar, and then a conductive metal layer is formed on the surface of the filling layer, wherein the portion electrically connected to the second capacitor conductive pillar forms a plate line 494, and the portion electrically connected to the second bit line conductive pillar forms a bit line 495.
[0044] In one embodiment of the present invention, a conductive metal layer electrically connected to the plate line may be further formed above the plate line and the bit line to facilitate electrical connection with the circuit structure of the circuit area.
[0045] In one embodiment of the present invention, when a conductive material is used for filling, the filling layer can also be directly cut to form plate lines and bit lines. The process in this structure is slightly different, such as Figures 27 to 29 As shown: First, if Fig. 27 As shown, after forming the second dielectric layer and the first sacrificial layer, drilling and filling are performed in the second dielectric layer and the first sacrificial layer to form a second bit line conductive pillar 1001, so that it is electrically connected to the first bit line conductive pillar; Next, if Fig.28 As shown, a capacitor is formed and filled and polished with a conductive material such as tungsten metal. It should be noted that, in this embodiment, the top surface of the second bit line conductive column is also covered with the high K ferroelectric oxide layer, the second electrode layer, and the filling layer; Finally, if Fig.29 As shown, part of the second electrode layer, the high K ferroelectric oxide layer and the filling layer on the top surface are removed by photolithography and etching processes, so that each capacitor is separated from each other. The filling layer of the capacitor part can be regarded as a plate line, and the high K ferroelectric oxide layer, the second electrode layer and the filling layer on the top of the second bit line conductive column are collectively regarded as a bit line.
[0046] Based on the ferroelectric memory structure obtained by the manufacturing method as described above, the first electrode layer of the capacitor is deposited in the deep hole of the second dielectric layer, but higher than the deep hole, the first electrode layer is electrically connected to the first capacitor conductive column, the high K ferroelectric oxide layer is deposited on the inner surface of the first electrode layer, the outer surface not covered by the second dielectric layer, and the surface of the second dielectric layer, and the second electrode layer is deposited on the surface of the high K ferroelectric oxide layer, and then under the same aspect ratio of the deep hole volume, the capacitor has a larger area than the traditional deep hole capacitor, effectively improving the storage density of the ferroelectric memory. At the same time, the manufacturing method is compatible with the standard FAB process, which is easy to integrate and reduces the manufacturing cost.
[0047] Although various embodiments of the present invention are described above, it should be understood that they are presented as examples only and not as limitations. It is obvious to those skilled in the relevant art that various combinations, modifications and changes can be made thereto without departing from the spirit and scope of the present invention. Therefore, the breadth and scope of the present invention disclosed herein should not be limited by the exemplary embodiments disclosed above, but should only be defined according to the attached claims and their equivalents.
Claims
1. A method for manufacturing a ferroelectric memory, characterized in that: Including steps: Providing a semiconductor substrate, the semiconductor substrate comprising a ferroelectric memory cell region, the ferroelectric memory cell region having a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above various functional regions; forming a first interconnect structure, the first interconnect structure comprising conductive pillars and a first dielectric layer between the conductive pillars, wherein the conductive pillars comprise a first capacitor conductive pillar and a first bit line conductive pillar; forming a second dielectric layer and a first sacrificial layer in sequence on the surface of the first dielectric layer; forming a deep hole in the second dielectric layer and the first sacrificial layer by photolithography and etching processes, wherein the bottom of the deep hole exposes the end surface of the first capacitor conductive column; Depositing electrode material in the deep hole and on the surface of the first sacrificial layer to form a first electrode layer; removing part of the electrode material, leaving only the first electrode layer at the bottom and side of the deep hole; removing the first sacrificial layer to expose at least a portion of the outer surface of the first electrode layer; forming a high-K ferroelectric oxide layer and a second electrode layer in sequence on the surfaces of the first electrode layer and the second dielectric layer to form a capacitor structure; forming a filling layer, wherein a surface of the filling layer is not lower than a surface of the second electrode layer; Removing a portion of the second electrode layer and the high dielectric constant ferroelectric oxide layer on the top surface by photolithography and etching processes, so that each capacitor is separated from each other; Metal interconnects, plate lines, and bit lines are formed.
2. The manufacturing method according to claim 1, wherein The method further includes forming an etch stop layer on the surface of the first dielectric layer and forming a hard mask layer on the surface of the first sacrificial layer, and the forming of the deep hole includes: patterning the hard mask layer by photolithography and etching processes; Using the patterned hard mask layer as a mask, etching is performed to form deep holes in the second dielectric layer and the first sacrificial layer to expose end surfaces of the first capacitor conductive pillars; The hard mask layer is removed.
3. The manufacturing method according to claim 1, wherein: The second dielectric layer and the first sacrificial layer are made of different materials.
4. The manufacturing method according to claim 1, wherein: The second dielectric layer is made of the same material as the first sacrificial layer, and the manufacturing method further comprises the steps of: A barrier layer is formed between the second dielectric layer and the first sacrificial layer.
5. The manufacturing method according to claim 1, wherein: Removing part of the electrode material includes the following steps: forming a second sacrificial layer on a surface of the first electrode layer; removing the electrode material covering the surface of the first sacrificial layer by an etching process; The second sacrificial layer is removed by a wet removal process.
6. The manufacturing method according to claim 5, wherein: The first sacrificial layer is removed simultaneously with the removal of the second sacrificial layer using the same process.
7. The manufacturing method according to claim 1, wherein: The filling layer is made of dielectric material, and the formation of the filling layer includes the following steps: forming an etch stop layer on a surface of the second electrode layer; A dielectric material is deposited on the surface of the etch stop layer to form a filling layer.
8. The manufacturing method according to claim 1, wherein: The formation of the filling layer comprises the steps of: A conductive material is deposited on the surface of the second electrode layer to form a filling layer.
9. The manufacturing method according to claim 8, wherein: The formation of the filling layer further comprises the steps of: TiN is deposited on the surface of the conductive material.
10. The manufacturing method according to claim 1, wherein Also includes the steps: The surface of the filling layer is flattened by a grinding process.
11. The manufacturing method according to claim 1, wherein Also includes the steps: Part of the second electrode layer and the high-K ferroelectric oxide layer are removed through photolithography and etching processes, so that each capacitor is separated from each other.
12. The manufacturing method according to claim 7, wherein: The steps of forming metal interconnects and plate lines and bit lines include: Drilling holes in the filling layer to form conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar and a second bit line conductive pillar, one end of the second capacitor conductive pillar is electrically connected to the second electrode layer, and one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the filling layer, wherein a portion electrically connected to the second capacitor conductive pillar forms a plate line, and a portion electrically connected to the second bit line conductive pillar forms a bit line.
13. The manufacturing method according to claim 8, wherein: The steps of forming metal interconnects and plate lines and bit lines include: forming a second bit line conductive pillar on one side of the capacitor, wherein one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the filling layer, wherein a portion contacting the filling layer forms a plate line, and a portion electrically connected to the second bit line conductive pillar forms a bit line.
14. The manufacturing method according to claim 8, wherein: The steps of forming metal interconnects and plate lines and bit lines include: forming a third dielectric layer on a surface of the filling layer, drilling holes in the third dielectric layer, and forming conductive pillars, wherein the conductive pillars include a second capacitor conductive pillar and a second bit line conductive pillar, one end of the second capacitor conductive pillar is electrically connected to the filling layer, and one end of the second bit line conductive pillar is electrically connected to the first bit line conductive pillar; A conductive metal layer is formed on the surface of the third dielectric layer, wherein a portion electrically connected to the second capacitor conductive pillar forms a plate line, and a portion electrically connected to the second bit line conductive pillar forms a bit line.
15. A ferroelectric memory structure, characterized in that: include: A semiconductor substrate comprising a ferroelectric memory cell region having a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above various functional regions; A first interconnect structure is provided above the semiconductor substrate, the first interconnect structure comprising a first capacitor conductive pillar, a first bit line conductive pillar, and a first dielectric layer between the conductive pillars; a second dielectric layer stacked on the first dielectric layer; A capacitor comprising a first electrode layer, a high-K ferroelectric oxide layer, and a second electrode layer, wherein the first electrode layer is deposited in a deep hole of the second dielectric layer but higher than the deep hole, the first electrode layer is electrically connected to the first capacitor conductive column, the high-K ferroelectric oxide layer is deposited on the inner surface of the first electrode layer, the outer surface not covered by the second dielectric layer, and the surface of the second dielectric layer, and the second electrode layer is deposited on the surface of the high-K ferroelectric oxide layer; A plate line and a bit line, wherein the plate line is connected to the second electrode layer through a metal interconnection, and the bit line is connected to the first bit line conductive pillar through a second bit line conductive pillar.
16. The ferroelectric memory structure according to claim 15, wherein: The interior of the capacitor is filled with a dielectric material, and the plate line is connected to the second electrode plate through a second capacitor conductive column formed in the dielectric material.
17. The ferroelectric memory structure according to claim 15, wherein: The capacitor is filled with a conductive material. The plate line is formed on a surface of the conductive material and is electrically connected to the second electrode plate through the conductive material.
18. The ferroelectric memory structure according to claim 15, wherein: The invention also includes a conductive metal layer, which is electrically connected to the plate line through a conductive column.