Electronic component with heat dissipation part and manufacturing method thereof
By forming a porous metal layer on the bonding surface between the electronic components and the heat dissipation portion and using paste solder, the thermal stress absorption and cracking problems caused by the small porosity of the solder in the prior art are solved, and the heat dissipation performance and durability are improved.
Patent Information
- Application Number
- CN202380026715.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-13
- Filing Date
- 2023-04-28
- Publication Date
- 2024-11-01
AI Technical Summary
When existing electronic components with heat dissipation parts reduce the porosity of the solder to improve heat dissipation performance, thermal stress is prone to difficult to absorb, resulting in the possibility of cracks entering the joint part and affecting durability.
By forming a porous metal layer with uniform air pores on the bonding surface between the electronic component and the heat dissipation portion, air pores in the jointing member are added, so that even in the case of cracking, the crack expansion is suppressed, and the printing process is carried out. Paste-like solder is applied to the bonding surface to improve the pore distribution of the bonding portion.
The improvement of heat dissipation performance and durability are achieved, ensuring the stability and heat dissipation efficiency of the joint components under thermal stress.
Smart Images

Figure CN118891719A_ABST
Abstract
Description
[0001] Cross-references of related applications
[0002] This application is based on Japanese Patent Application No. 2022-79355 filed on May 13, 2022, and the contents thereof are cited herein. Technical Field
[0003] The invention relates to an electronic component with a heat dissipation portion and a manufacturing method thereof. Background Art
[0004] In the past, electronic components with heat dissipation parts have been developed in which electronic components and heat dissipation parts for dissipating heat from the electronic components are integrated. For example, Patent Document 1 discloses the following technology: in an electronic component with a heat dissipation part, when the heat dissipation part and the electronic component are joined by soldering, the porosity of the solder is set to be 10% or less. As a result, the thermal resistance of the joint can be reduced, and thus the heat dissipation performance can be improved.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2003-282770
[0008] However, as in the technique described in Patent Document 1, if the solder porosity of the joint is reduced, it becomes difficult to absorb the stress when thermal stress acts on the joint, and thus cracks may easily enter the joint. Summary of the invention
[0009] The present invention has been made in view of the above-mentioned points, and an object of the present invention is to provide an electronic component with a heat dissipation portion and a method for manufacturing the electronic component, which can achieve both improved heat dissipation performance and improved durability.
[0010] In order to achieve the above object, an electronic component with a heat dissipation portion according to one embodiment of the present invention includes:
[0011] Electronic components that generate heat during operation;
[0012] a heat dissipation portion that dissipates heat generated by the electronic components to an ambient fluid; and
[0013] a bonding component that bonds the electronic component to the heat dissipation portion,
[0014] The joint area between the electronic components and the heat sink is 100mm 2 above,
[0015] The bonding component forms a porous metal layer with pores evenly distributed throughout.
[0016] Thus, since the bonding component forms a porous metal layer, the temperature distribution can be reduced in the entire surface of the bonding component. In addition, even if cracks occur in the bonding component, they can be absorbed by the pores, so the cracks can be suppressed from expanding. As a result, it is possible to achieve both improved heat dissipation performance and improved durability.
[0017] In addition, in a method for manufacturing an electronic component with a heat dissipation portion according to one embodiment of the present invention, the electronic component with a heat dissipation portion is formed by joining a heat dissipation portion to an electronic component that generates heat during operation, and the heat dissipation portion dissipates heat generated by the electronic component to an ambient fluid, and is characterized in that:
[0018] The joint area between the electronic components and the heat sink is 100mm 2 above,
[0019] The printing step includes applying a solder paste to at least one of a bonding surface of the electronic component and a bonding surface of the heat dissipation portion through a mesh. The solder paste is a bonding member for bonding the electronic component to the heat dissipation portion.
[0020] As a result, the pores in the bonding component can be increased, so the temperature distribution can be reduced in the entire surface of the bonding component. In addition, even if cracks occur in the bonding component, they can be absorbed by the pores, so the cracks can be suppressed from expanding. As a result, it is possible to achieve both improved heat dissipation performance and improved durability. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is an explanatory diagram showing the overall structure of a semiconductor device in one embodiment.
[0022] Figure 2 It is an explanatory diagram showing the surface of a joining member in one embodiment.
[0023] Figure 3 This is a characteristic diagram showing the relationship between the distance between pores in the porous metal layer and the durability index.
[0024] Figure 4 This is a characteristic diagram showing the relationship between the thickness dimension and the porosity in the porous metal layer.
[0025] Figure 5 It is an explanatory diagram showing a bonding surface of a heat dissipation portion in one embodiment. DETAILED DESCRIPTION
[0026] Hereinafter, an embodiment of the present invention will be described using the accompanying drawings. Figure 1As shown, in this embodiment, as an electronic component with a heat sink, a semiconductor device 1 integrally provided with a heat sink 2 is used. The semiconductor device 1 of this embodiment includes a substrate 10, a semiconductor element 20, and a cover 30. The semiconductor device 1 of this embodiment corresponds to an electronic component.
[0027] When the semiconductor device 1 is mounted on the main board 3 as an external component, the substrate 10 functions as an interposer of the semiconductor element 20. The substrate 10 is mounted on the upper surface of the main board 3 via the solder balls 60. More specifically, the substrate 10 is mounted on the upper surface of the main board 3 via the solder balls 60 in a state where the lower surface of the substrate 10 faces the upper surface of the main board 3. As the substrate 10, for example, a ceramic substrate, a printed circuit board, a glass epoxy substrate, etc. can be used.
[0028] The semiconductor element 20 is mounted on the upper surface of the substrate 10 via bump electrodes (not shown). More specifically, the semiconductor element 20 is mounted on the upper surface of the substrate 10 via bump electrodes with the surface (ie, lower surface) of the semiconductor element 20 facing the upper surface of the substrate 10.
[0029] The semiconductor element 20 is flip-chip bonded to the upper surface of the substrate 10. The semiconductor element 20 can be an IC chip formed by a general semiconductor process. In addition, bump electrodes are provided on the surface of the semiconductor element 20 and are made of solder, gold, Cu, or the like.
[0030] The cover 30 is a sealing member that seals the semiconductor element 20. The cover 30 is fixed to the upper surface of the substrate 10 via a sealing member (not shown). In addition, the back surface (i.e., the upper surface) of the semiconductor element 20 and the cover 30 are bonded by an adhesive member 50. The sealing member and the adhesive member 50 can use a material having a higher melting temperature than the bump electrode.
[0031] The heat dissipation unit 2 is a heat dissipation component that dissipates heat generated by the semiconductor device 1 to air as an ambient fluid. The heat dissipation unit 2 is made of a material with excellent thermal conductivity. In this embodiment, the heat dissipation unit 2 is made of a metal such as aluminum alloy or copper. The heat dissipation unit 2 includes a plate portion 21 and a heat sink portion 22.
[0032] The plate portion 21 is formed in a plate shape. The plate portion 21 is configured to contact the upper surface of the cover 30 of the semiconductor device 1 (i.e., the surface opposite to the surface to which the semiconductor element 20 is bonded). The heat sink portion 22 is a heat transfer component that expands the heat transfer area with the air and promotes heat exchange between the air and the semiconductor device 1. A plurality of heat sink portions 22 are provided in a manner protruding upward from the upper surface of the plate portion 21 (i.e., the surface opposite to the surface in contact with the cover 30).
[0033] The semiconductor device 1 and the heat dissipation part 2 are bonded by a bonding member 4. In the present embodiment, the bonding member 4 is made of solder. That is, the semiconductor device 1 and the heat dissipation part 2 are soldered. At least one of the bonding surface of the semiconductor device 1 bonded to the bonding member 4 and the bonding surface of the heat dissipation part 2 bonded to the bonding member 4 is nickel plated.
[0034] The bonding area between the semiconductor device 1 and the heat dissipation unit 2 is 100 mm 2 In this embodiment, the junction between the semiconductor device 1 and the heat dissipation unit 2 is 30 mm in angle, and the junction area between the semiconductor device 1 and the heat dissipation unit 2 is 900 mm 2 .
[0035] like Figure 2 As shown, the bonding member 4 forms a porous metal layer 40 with pores 41 uniformly distributed throughout. Figure 2 This is the surface viewed from the upper side (that is, the heat dissipation portion 2 side) of the bonding member 4 of the present embodiment.
[0036] Here, the distance between adjacent pores 41 in the porous metal layer 40 is defined as the inter-pore distance Lp. Figure 3 The relationship between the pore distance Lp in the porous metal layer 40 and the durability is shown. Figure 3 The durability index on the vertical axis is an indicator of the durability against damage to the bonding component 4 and the substrate 10 due to long-term use. The larger the value of the durability index, the higher the durability. In addition, the "damage to the bonding component 4 and the substrate 10 due to long-term use" here is caused by thermal distortion, thermal degradation, pressure fluctuation, swelling, etc.
[0037] according to Figure 3 It is known that when the pore distance Lp is greater than 1 mm, the durability decreases sharply. Therefore, the porous metal layer 40 is formed so that the pore distance Lp is less than 1 mm at any position. That is, the porous metal layer 40 is formed so that the pore distance Lp is less than 1 mm at any position in the porous metal layer 40. In other words, when viewed from a direction perpendicular to the bonding surface between the semiconductor device 1 and the heat dissipation unit 2, the porous metal layer 40 has a pore distance Lp of 1 mm per unit area. 2 At least one air hole 41 is formed inside. This can improve durability.
[0038] Here, the length of the porous metal layer 40 in the arrangement direction of the semiconductor device 1 and the heat dissipation portion 2 is defined as the thickness dimension Wp. 2) is defined as the porosity Rv. In the present embodiment, the arrangement direction of the semiconductor device 1 and the heat dissipation portion 2 in the porous metal layer 40 is parallel to the direction perpendicular to the bonding surface in the porous metal layer 40 .
[0039] According to the research findings of the inventors of this application, Figure 4 As shown in the shaded portion, in the semiconductor device 1 of this embodiment, as long as the thickness dimension Wp and the porosity Rv of the porous metal layer 40 satisfy the relationship Rv≤-6.23Wp+1, the heat dissipation performance can be improved. At this time, in the porous metal layer 40, the temperature difference dT is 1°C, the heat transfer coefficient λ is 64.2W / (m·K), and the heat flow rate q is 400kW / m 2 Therefore, in the present embodiment, the thickness dimension Wp and the porosity Rv of the porous metal layer 40 are set to satisfy the relationship of Rv≤-6.23Wp+1.
[0040] like Figure 5 As shown, a groove portion 23 is formed on the bonding surface of the plate portion 21 of the heat dissipation portion 2 that is bonded to the bonding member 4. The end of the groove portion 23 is open to the outside of the heat dissipation portion 2. That is, the inside of the groove portion 23 is connected to the outside of the heat dissipation portion 2 (that is, the air as the ambient fluid). In this embodiment, two straight groove portions 23 are formed in a cross-shaped manner on the bonding surface of the plate portion 21 that is bonded to the semiconductor device 1.
[0041] Next, a method for manufacturing the semiconductor device 1 integrally provided with the heat dissipation portion 2 in the present embodiment will be described. First, a step of preparing the semiconductor device 1 and the heat dissipation portion 2 is performed.
[0042] Next, a printing process is performed. In the printing process, a paste solder is applied to at least one of the bonding surface of the semiconductor device 1 and the bonding surface of the heat dissipation portion 2 through a mesh. The paste solder contains a flux that improves the bonding properties of the solder. In this embodiment, the content of the flux in the solder is about 50%.
[0043] Next, a joining step is performed to solder the joining portion between the semiconductor device 1 and the heat dissipation portion 2. In the present embodiment, the joining portion between the semiconductor device 1 and the heat dissipation portion 2 is soldered by reflow soldering.
[0044] Specifically, first, after placing the heat dissipation portion 2 at a predetermined position on the bonding surface of the substrate 10, the substrate 10 is placed in a heating furnace. Then, after a preheating process at about 180°C, the temperature is raised to about 220°C to melt the solder. Thereafter, the heat dissipation portion 2 is soldered and bonded to the bonding surface of the substrate 10 by cooling until the solder solidifies.
[0045] As described above, the heat dissipation portion 2 is soldered and bonded to the semiconductor device 1. In addition, a finishing process and the like are performed. In this way, the semiconductor device 1 in which the heat dissipation portion 2 is integrally provided is completed.
[0046] As described above, in the semiconductor device 1 of the present embodiment, the bonding component 4 forms a porous metal layer 40 in which the pores 41 are evenly distributed throughout. Therefore, the bonding between the semiconductor device 1 and the heat dissipation portion 2 becomes a spot-shaped bonding. As a result, the temperature distribution can be reduced in the entire surface of the bonding portion. In addition, even if cracks occur in the bonding component 4, they can be partially absorbed by the pores 41, so that the expansion of the cracks can be suppressed. In addition, the distance between the spot-shaped bonding portions is small, so the thermal stress can be reduced. As a result, it is possible to achieve a balance between improved heat dissipation performance and improved durability.
[0047] In addition, in the semiconductor device 1 of the present embodiment, when viewed from a direction perpendicular to the bonding surface between the semiconductor device 1 and the heat dissipation unit 2, the porous metal layer 40 has a unit area (i.e., 1 mm 2 ) is formed with at least one air hole 41. Thus, as described above Figure 2 As shown, durability can be improved.
[0048] In the semiconductor device 1 of the present embodiment, the porous metal layer 40 is configured so that the thickness dimension Wp and the porosity Rv satisfy the relationship Rv≤-6.23Wp+1. Figure 4 As shown, the heat dissipation performance can be improved.
[0049] In the semiconductor device 1 of the present embodiment, a groove 23 is formed on the bonding surface of the heat dissipation portion 2 that is bonded to the bonding member 4. Thus, during the bonding process, the gas in the bonding member 4 is easily released to the outside through the groove 23, so that the pores 41 can be evenly distributed in the bonding member 4.
[0050] However, when a component that needs to dissipate heat (such as an electronic component) is joined to a heat dissipation portion and the joint area of the joint portion is 100 mm 2 In the case of the above large area, a sheet solder without flux is usually used as a bonding part. In addition, soldering is performed by heating in a reducing environment, so that almost no voids are generated in the bonding part. Therefore, when thermal stress acts on the bonding part, it is difficult to absorb the stress, so that cracks easily enter the bonding part.
[0051] In contrast, the method for manufacturing the semiconductor device 1 of the present embodiment includes a printing step of applying a paste solder through a mesh to at least one of the bonding surface of the semiconductor device 1 and the bonding surface of the heat dissipation portion 2. As a result, the pores 41 can be evenly distributed in the bonding member 4. As a result, even if cracks occur in the bonding member 4, they can be partially absorbed by the pores 41, thereby improving durability.
[0052] The present invention is not limited to the above-described embodiment, and various modifications may be made as described below without departing from the gist of the present invention.
[0053] (1) In the above-mentioned embodiment, an example is described in which air is used as the ambient fluid and the heat dissipation portion 2 is configured so that the heat generated by the semiconductor device 1 is dissipated to the air, but the present invention is not limited to this method. For example, a refrigerant liquid may be used as the ambient fluid, and the heat dissipation portion 2 may be configured so that it is immersed in the refrigerant liquid so that the heat generated by the semiconductor device 1 is dissipated to the refrigerant liquid. In this case, an insulating fluid may be used as the refrigerant liquid. Specifically, a fluorine-based inert liquid may be used as the refrigerant liquid. The fluorine-based inert liquid is a refrigerant liquid having excellent insulation, heat transfer characteristics, and stability.
[0054] (2) In the above-mentioned embodiment, an example is described in which two grooves 23 are formed in a straight line in a manner that crosses each other on the bonding surface of the plate portion 21 of the heat dissipation portion 2, but the present invention is not limited to this embodiment. For example, one groove 23 or three or more grooves 23 may be formed. In addition, as long as the end of the groove 23 is open to the outside of the heat dissipation portion 2, it can be formed at any position of the bonding surface of the heat dissipation portion 2 that is bonded to the semiconductor device 1.
[0055] (other)
[0056] The electronic component with a heat dissipation portion and the method for manufacturing the same disclosed in this specification have the following features.
[0057] (Item 1)
[0058] Electronic components with heat sinks have:
[0059] An electronic component (1) which generates heat during operation;
[0060] a heat dissipation portion (2) which dissipates heat generated by the electronic component to an ambient fluid; and
[0061] a bonding component (4) for bonding the electronic component to the heat dissipation portion,
[0062] The bonding area between the electronic component and the heat dissipation part is 100 mm 2 above,
[0063] The bonding member forms a porous metal layer (40), and the pores (41) are uniformly distributed throughout the porous metal layer.
[0064] (Item 2)
[0065] In the electronic component with a heat dissipation portion described in item 1,
[0066] When viewed from a direction perpendicular to the bonding surface between the electronic component and the heat dissipation portion, the porous metal layer has at least one pore formed per unit area.
[0067] The unit area is 1 mm 2 ,
[0068] The length of the porous metal layer in the arrangement direction of the electronic component and the heat dissipation portion is defined as a thickness dimension (Wp).
[0069] When the area ratio of the pores contained in each unit area when the porous metal layer is viewed from a direction perpendicular to the bonding surface is defined as porosity (Rv),
[0070] The thickness dimension and the porosity satisfy the relationship of Rv≤-6.23Wp+1.
[0071] (Item 3)
[0072] In the electronic component with a heat dissipation portion described in item 1 or 2,
[0073] The bonding member is solder.
[0074] (Item 4)
[0075] In the electronic component with a heat dissipation portion described in any one of items 1 to 3,
[0076] At least one of a bonding surface of the electronic component bonded to the bonding member and a bonding surface of the heat dissipating portion bonded to the bonding member is plated with nickel.
[0077] (Item 5)
[0078] In the electronic component with a heat dissipation portion described in any one of items 1 to 4,
[0079] A groove portion (23) is formed on a joining surface of the heat dissipating portion that is joined to the joining member.
[0080] (Item 6)
[0081] A method for manufacturing an electronic component with a heat dissipation portion, wherein the electronic component with a heat dissipation portion is formed by joining a heat dissipation portion (2) to an electronic component (1) that generates heat during operation, wherein the heat dissipation portion dissipates heat generated by the electronic component to an ambient fluid.
[0082] The bonding area between the electronic component and the heat dissipation part is 100 mm 2 above,
[0083] The method comprises a printing step of applying a solder paste to at least one of a bonding surface of the electronic component and a bonding surface of the heat dissipation portion through a mesh, the solder paste being a bonding member for bonding the electronic component to the heat dissipation portion.
[0084] The present invention is described based on the embodiments, but it should be understood that the present invention is not limited to the embodiments and structures. The present invention also includes various modifications and variations within the scope of equality. In addition, various combinations and methods, and other combinations and methods including only one element, above or below them are also included in the scope and thought scope of the present invention.
Claims
1. An electronic component with a heat dissipation portion, characterized in that: have: An electronic component (1) which generates heat during operation; A heat dissipation unit (2) which dissipates heat generated by the electronic component to an ambient fluid; as well as a bonding component (4) for bonding the electronic component to the heat dissipation portion, The bonding area between the electronic component and the heat dissipation part is 100 mm 2 above, The bonding member forms a porous metal layer (40), and the pores (41) are evenly distributed throughout the porous metal layer.
2. The electronic component with a heat dissipation portion according to claim 1, characterized in that: When viewed from a direction perpendicular to the bonding surface between the electronic component and the heat dissipation portion, the porous metal layer has at least one pore formed per unit area. The unit area is 1 mm 2 , The length of the porous metal layer in the arrangement direction of the electronic component and the heat dissipation portion is defined as a thickness dimension (Wp). When the area ratio of the pores contained in each unit area when the porous metal layer is viewed from a direction perpendicular to the bonding surface is defined as porosity (Rv), The thickness dimension and the porosity satisfy the relationship of Rv≤-6.23Wp+1.
3. The electronic component with a heat dissipation portion according to claim 1 or 2, characterized in that: The bonding member is solder.
4. The electronic component with a heat dissipation portion according to any one of claims 1 to 3, characterized in that: At least one of a bonding surface of the electronic component bonded to the bonding member and a bonding surface of the heat dissipating portion bonded to the bonding member is plated with nickel.
5. The electronic component with a heat dissipation portion according to any one of claims 1 to 4, characterized in that: A groove portion (23) is formed on a joining surface of the heat dissipating portion that is joined to the joining member.
6. A method for manufacturing an electronic component with a heat dissipation portion, wherein the electronic component with a heat dissipation portion is formed by joining a heat dissipation portion (2) to an electronic component (1) that generates heat during operation, wherein the heat dissipation portion dissipates heat generated by the electronic component to an ambient fluid, wherein: The bonding area between the electronic component and the heat dissipation part is 100 mm 2 above, The method comprises a printing step of applying a solder paste to at least one of a bonding surface of the electronic component and a bonding surface of the heat dissipation portion through a mesh, the solder paste being a bonding member for bonding the electronic component to the heat dissipation portion.