By designing an intermediate frequency heating furnace for straightening and opening of tungsten strips, the problems of insufficient heating temperature, low efficiency and easy pollution of molybdenum wire heating muffle furnace are solved, and efficient and pollution-free tungsten strip heating is achieved, which extends the equipment life and meets the needs of the molybdenum wire heating. The processing requirements of high-strength tungsten alloy wires are obtained.

CN118896478APending Publication Date: 2024-11-05HENAN POLYTECHNIC UNIV +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411138331.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The existing molybdenum wire heating muffle furnaces are insufficient in the process of tungsten strip straightening and blanking, low in heating temperature, easy to contaminate and short equipment life, which cannot meet the processing needs of high-strength tungsten alloy wires.

Method used

An intermediate frequency heating furnace for straightening and opening of tungsten strips is designed, including a shell, tungsten furnace tube, heating unit, front insulation unit, rear insulation unit, side insulation unit and protective gas unit, and the tungsten furnace tube is used to carry out IGBT power supply. Heating, the temperature can reach above 1800 degrees Celsius, and pollution is prevented by protection from inert gas.

Benefits of technology

It improves heating temperature and efficiency, avoids tungsten strip pollution, extends the equipment life, and ensures the preparation and processing quality of high-strength and large-length tungsten alloy wires.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118896478A_ABST
    Figure CN118896478A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of photovoltaics, and provides an intermediate frequency heating furnace for tungsten bar straightening and cogging. In the heating furnace, a shell is of a cylindrical structure with one open end and one closed end, a tungsten furnace tube is coaxially sleeved with the shell, a rear heat preservation unit is arranged between the tungsten furnace tube and the closed end of the shell, and a side heat preservation unit is arranged between the tungsten furnace tube and the inner side wall of the shell; a heating unit is arranged in the side heat preservation unit and surrounds the outer side of the tungsten furnace tube so as to heat the tungsten furnace tube; a baffle is arranged at the opening end of the shell, a front heat preservation unit is arranged between the baffle and the tungsten furnace tube, a feeding port is formed in the baffle, the baffle is sealed through a furnace door unit installed at the opening end of the shell, and meanwhile inert gas is introduced into the tungsten furnace tube in the heating process; the problems that in the existing tungsten alloy rod straightening and cogging process, a muffle furnace adopting molybdenum wire heating is insufficient in heating temperature and low in heating efficiency, tungsten bars are prone to being polluted, and heating equipment is short in service life are effectively solved, and a guarantee is provided for preparation of high-strength and large-length tungsten alloy wires.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of photovoltaic technology, and in particular to a medium frequency heating furnace for straightening and blanking tungsten bars. Background Art

[0002] With the rapid development of the photovoltaic field, the demand for silicon wafers has risen sharply. Currently, carbon steel cutting wires are mostly used to cut silicon wafers. In order to meet the "dual carbon" requirements and improve the utilization rate of silicon wafers, higher requirements are placed on the thickness and utilization rate of silicon wafers: thinner silicon wafers are required, and more silicon wafers can be cut from a single silicon ingot, which in turn requires the cutting wire to have a thinner wire diameter and higher strength. However, due to the priority of carbon steel wire strength (when the wire diameter is 0.035 mm, the breaking force is 4.0N, and the cutting requirement is ≥5.0N), the wire diameter of the cutting wire is generally greater than or equal to 0.045 mm. The breaking force of a smaller wire diameter cannot meet the cutting requirements, which seriously restricts the cutting of thin silicon wafers. In addition, due to the thicker wire diameter, the utilization rate of silicon ingots cannot be further improved.

[0003] Tungsten alloy wire has the characteristics of high strength (wire diameter 0.035 mm, breaking force ≥ 5.0N), good plastic deformation ability (machinable to 0.020-0.030 mm), etc. It is an ideal material to replace carbon steel cutting wire. For tungsten alloy, the quality of the blank determines the wire breakage rate in subsequent processing. Therefore, straightening and blanking of tungsten alloy strips are the core links of tungsten alloy wire processing; in the straightening and blanking process, precise control of heating temperature is the key to straightening and blanking.

[0004] At present, a molybdenum wire-heated muffle furnace is used to heat the tungsten bars during the straightening and blanking stages. However, the maximum temperature of the molybdenum wire-heated muffle furnace is 1700℃, and the cleanliness of the furnace tube is not high. These drawbacks seriously affect the quality of tungsten bar straightening and blanking heating, and bring serious problems to the subsequent processing of tungsten alloy wire. Further increasing the heating temperature and avoiding contamination during the tungsten bar heating process are issues that need to be urgently addressed in the straightening and blanking processes of high-strength tungsten wires. Summary of the invention

[0005] The purpose of the present application is to provide a medium frequency heating furnace for straightening and blanking tungsten bars, so as to solve or alleviate the problems existing in the above-mentioned prior art.

[0006] In order to achieve the above objectives, this application provides the following technical solutions:

[0007] The present application provides a medium-frequency heating furnace for straightening and blanking tungsten bars, comprising: a shell, a tungsten furnace tube, a furnace door unit, a heating unit, a front insulation unit, a rear insulation unit, a side insulation unit and a protective gas unit; the shell is a cylindrical structure with one end open and the other end closed, the tungsten furnace tube is coaxially sleeved in the shell, the rear insulation unit is arranged between the tungsten furnace tube and the closed end of the shell, and the side insulation unit is arranged between the outer side wall of the tungsten furnace tube and the inner side wall of the shell; the heating unit is located in the side insulation unit and surrounds the outer side of the tungsten furnace tube for heating the tungsten furnace tube; a baffle is arranged at the open end of the shell, the front insulation unit is arranged between the baffle and the tungsten furnace tube, and a feed hole is opened on the baffle; the furnace door unit is installed at the open end of the shell for sealing the feed hole; the protective gas unit is used to introduce inert gas into the tungsten furnace tube.

[0008] Preferably, the shell is composed of bakelite shell plates, and the baffle is made of heat-resistant steel; wherein the bakelite shell plates constituting the shell and the shell and the baffle are sealed with refractory mud or rubber.

[0009] Preferably, the bottom end of the side heat-insulating unit is pressed against the rear heat-insulating unit, and the top end is flush with the front heat-insulating unit and pressed against the baffle.

[0010] Preferably, a tungsten plate is also laid on the inner bottom surface of the tungsten furnace tube to place the tungsten bar to be processed; and / or, a tungsten block is also placed between the tungsten furnace tube and the rear insulation unit, and one end of the tungsten block is connected to the rear insulation unit, and the other end is located on the tungsten plate, and the end of the tungsten plate close to the rear insulation unit penetrates into the tungsten furnace tube by 100-150 mm.

[0011] Preferably, the protective gas unit introduces the inert gas into the tungsten furnace tube through an air intake pipe, and correspondingly, an exhaust hole is provided on one end of the tungsten plate close to the furnace door unit, and a supporting protrusion is provided on the bottom surface of the tungsten plate, and the supporting protrusion is located on the inner bottom surface of the tungsten furnace tube; wherein, the air intake pipe passes through the shell and the side insulation unit in sequence from the outside of the shell, and faces the air hole, so that the inert gas forms a protective gas screen in the tungsten furnace tube after passing through a row of the air holes.

[0012] Preferably, the rear insulation unit and the side insulation unit both comprise a high-temperature insulation layer, a medium-temperature insulation layer and a low-temperature insulation layer, and the high-temperature insulation layer, the medium-temperature insulation layer and the low-temperature insulation layer are arranged in sequence along the normal direction from the tungsten furnace tube to the shell; wherein, the insulation range of the high-temperature insulation layer is 1900-2300°C, the insulation range of the medium-temperature insulation layer is 1600-1900°C, and the insulation range of the low-temperature insulation layer is 1000-1600°C; the insulation range of the front insulation unit is 1900-2300°C.

[0013] Preferably, the heating coil of the heating unit is located in the low-temperature insulation layer of the side insulation unit, and the heating coil is buried in alumina refractory mud for coating.

[0014] Preferably, it also includes: an infrared temperature measuring device, which is installed in the temperature measuring hole and is used to monitor the temperature of the outer wall of the tungsten furnace tube in real time; wherein the temperature measuring hole starts from the outer wall of the shell and penetrates to the outer wall of the tungsten furnace tube.

[0015] Preferably, the furnace door unit comprises: a furnace door cover, a connecting rod and a driving connecting member; the furnace door cover and the driving connecting member are arranged side by side and in parallel, the two ends of the connecting rod are respectively rotatably connected to the furnace door cover and the driving connecting member, and one end of the furnace door cover is rotatably mounted on the shell; the driving connecting member is connected to the output end of the driving unit mounted on the shell, so as to move under the drive of the driving unit, driving the furnace door cover to rotate around the axis of its rotational connection with the shell, so as to open or close the feed hole.

[0016] Preferably, the heating unit uses an IGBT power supply to heat the tungsten furnace tube, and the heating temperature is greater than or equal to 1800 degrees Celsius.

[0017] Beneficial effects:

[0018] In the medium-frequency heating furnace for straightening and blanking of tungsten bars provided in the embodiment of the present application, the shell is a cylindrical structure with one end open and the other end closed, the tungsten furnace tube is coaxially sleeved in the shell, and a rear insulation unit is arranged between the closed end of the shell, and a side insulation unit is arranged between the inner wall of the shell; the heating unit is arranged in the side insulation unit and surrounds the outer side of the tungsten furnace tube to heat the tungsten furnace tube; a baffle is arranged at the open end of the shell, a front insulation unit is arranged between the baffle and the tungsten furnace tube, and a feed port is opened on the baffle, and is sealed by a furnace door unit installed at the open end of the shell, and at the same time, inert gas is introduced into the tungsten furnace tube during the heating process, which effectively solves the problems of insufficient heating temperature, low heating efficiency, easy contamination of tungsten bars, short life of heating equipment, etc. in the muffle furnace that uses molybdenum wire for heating in the current tungsten alloy rod straightening and blanking process, and provides guarantee for the preparation of high-strength and long-length tungsten alloy wires. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The drawings constituting part of the present application are used to provide a further understanding of the present application. The exemplary embodiments and descriptions of the present application are used to explain the present application and do not constitute an improper limitation on the present application. Among them:

[0020] Figure 1 A schematic diagram of the structure of a medium frequency heating furnace for straightening and blanking tungsten bars provided according to some embodiments of the present application;

[0021] Figure 2 for Figure 1 Partial view at point A in the middle.

[0022] Description of reference numerals:

[0023] 1. Shell; 2. Tungsten furnace tube; 3. Heating coil; 4. Front insulation unit; 5. Rear insulation unit; 6. Side insulation unit; 7. Protective gas unit; 8. Tungsten plate; 9. Tungsten block; 10. Furnace door cover; 11. Connecting rod; 12. Driving connector; 13. Infrared temperature measuring device; 14. Exhaust duct; 15. Bottom plate; 16. Exhaust hole. DETAILED DESCRIPTION

[0024] The present application will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments. Each example is provided by way of explanation of the present application and does not limit the present application. In fact, it will be clear to those skilled in the art that modifications and variations may be made in the present application without departing from the scope or spirit of the present application. For example, a feature shown or described as a part of an embodiment may be used in another embodiment to produce yet another embodiment. All other embodiments obtained by those of ordinary skill in the art based on the embodiments in the embodiments of the present invention should belong to the scope of protection of the embodiments of the present invention.

[0025] The existing tungsten alloy rod blank is heated by a molybdenum wire heating muffle furnace, which has the following disadvantages: First, the maximum heating temperature of the molybdenum wire heating muffle furnace is 1700℃, which cannot meet the straightening and blanking temperature of high alloy content tungsten alloy rod blanks; second, the furnace tube of the molybdenum wire heating muffle furnace is a corundum furnace tube, which contains a lot of pollutants, causing secondary pollution to the heated tungsten rod, thereby increasing the wire breakage rate of the subsequent processing of the tungsten alloy wire; third, the heating and cooling rates are slow, and it takes 7-10 days to increase from room temperature to the process temperature (1650℃), and 5-8 days to cool down, which seriously affects the service life; fourth, the service life is short: due to the use of molybdenum wire heating and corundum furnace tubes, its service life is about 6-12 months. These problems seriously affect the performance of tungsten alloy billet straightening and blanking, and bring inconvenience to the subsequent processing and use of high-strength tungsten alloy wire.

[0026] Based on this, the present application proposes a medium frequency heating furnace for straightening and blanking tungsten bars, which is used to solve the current problems of insufficient heating temperature, low heating efficiency, easy contamination of tungsten bars, and short life of heating equipment during the straightening and blanking of tungsten alloy rods, and provide guarantees for the preparation and processing of high-strength and long-length tungsten alloy wires.

[0027] like Figure 1 , Figure 2 As shown, the medium frequency heating furnace for straightening and blanking tungsten bars comprises: a shell 1, a tungsten furnace tube 2, a furnace door unit, a heating unit, a front insulation unit 4, a rear insulation unit 5, a side insulation unit 6 and a protective gas unit 7. The shell 1 is a cylindrical structure with one end open and the other end closed. The tungsten furnace tube 2 is coaxially sleeved in the shell 1, and the rear insulation unit 5 is arranged between the end of the tungsten furnace tube 2 and the closed end of the shell 1, and the side insulation unit 6 is arranged between the outer wall of the tungsten furnace tube 2 and the inner wall of the shell 1; a baffle is arranged at the open end of the shell 1, and the front insulation unit 4 is arranged between the baffle and the end of the tungsten furnace tube 2. There is a feed hole coaxial with the tungsten furnace tube 2 on the baffle, and a furnace door unit is installed at the open end of the shell 1 to seal the feed hole during the heating process of the tungsten alloy rod.

[0028] A heating unit is provided in the side insulation unit 6, which surrounds the outer side of the tungsten furnace tube 2 to heat the tungsten furnace tube 2. During the heating process of the tungsten alloy rod, an inert gas is introduced into the tungsten furnace tube 2 by the protective gas unit 7 to protect the heating process of the tungsten alloy rod.

[0029] In the present application, the shell 1 is a cylindrical structure (square in cross section) with one end open and the other end closed, which is composed of bakelite shell plates. Refractory mud or rubber is used to seal between the bakelite shell plates that constitute the shell 1. A baffle is set at the open end of the shell 1. The baffle is made of heat-resistant steel, and refractory mud or rubber is also used to seal between the baffle and the bakelite shell plate to improve the airtightness of the heating furnace and enhance the heating and heat preservation effect.

[0030] The rear insulation unit 5 and the side insulation unit 6 both include a high-temperature insulation layer, a medium-temperature insulation layer and a low-temperature insulation layer, and the high-temperature insulation layer, the medium-temperature insulation layer and the low-temperature insulation layer are arranged in sequence along the normal direction from the tungsten furnace tube 2 to the shell 1; wherein the insulation range of the high-temperature insulation layer is 1900-2300°C, the insulation range of the medium-temperature insulation layer is 1600-1900°C, and the insulation range of the low-temperature insulation layer is 1000-1600°C. Specifically, the high-temperature insulation layer is made of high-temperature zirconia insulation bricks with a temperature resistance of 1900-2300°C, the medium-temperature insulation layer is made of zirconia insulation bricks with a temperature resistance of 1600-1900°C, and the low-temperature insulation layer is made of alumina insulation bricks with a temperature resistance of 1000-1600°C. In addition, the front insulation unit 4 is made of high-temperature zirconia insulation bricks with a temperature resistance of 1900-2300°C.

[0031] The cross section of the tungsten furnace tube 2 is square, made of pure tungsten, and coaxially sleeved in the shell 1, and the front insulation block (front insulation unit 4) and the rear insulation block are arranged at both ends of the tungsten furnace tube 2, wherein the rear insulation block is a part of the high-temperature insulation layer of the rear insulation unit 5, and the front insulation block is stacked to be flush with the end of the side insulation unit 6 and against the baffle. The end of the side insulation unit 6 (lower end: close to the closed end of the shell 1) is stacked against the high-temperature heat-resistant layer of the rear insulation unit 5, and the other end (top end: close to the open end of the shell 1) is stacked against the front insulation unit 4.

[0032] A tungsten plate 8 is laid on the inner bottom surface of the tungsten furnace tube 2, and the rear end of the tungsten plate 8 (close to the closed end of the shell 1) is flush with the end surface of the tungsten furnace tube 2 and abuts against the rear insulation block; the front end of the tungsten plate 8 (close to the open end of the shell 1) passes through the feed hole and is flush with the outer side surface of the baffle, so as to effectively reduce the wear of the tungsten furnace tube 2 and the front insulation unit 4.

[0033] A tungsten block 9 is also placed between the tungsten furnace tube 2 and the rear insulation unit 5, wherein one end of the tungsten block 9 abuts against the high-temperature insulation layer of the rear insulation unit 5, and the other end is located on the tungsten plate 8, and the end of the tungsten plate 8 close to the rear insulation unit 5 penetrates into the tungsten furnace tube 2 by 100-150 mm. The height of the tungsten block 9 is higher than the height of the tungsten bar placed in the tungsten furnace tube 2, thereby effectively ensuring that the tungsten bar is located in the effective heating range in the tungsten furnace tube 2.

[0034] In the present application, the heating coil 3 is located in the side insulation unit 6. Specifically, the heating coil 3 surrounds the high-temperature insulation layer of the side insulation unit 6. That is to say, a coil insulation layer (alumina material) is also provided outside the high-temperature insulation layer of the side insulation unit 6. The heating coil 3 is located in the coil insulation layer, and the heating coil 3 and the coil insulation layer are filled with alumina refractory mud and fixed by bakelite columns. Among them, the heating coil 3 is wound by a copper tube, and the surface is insulated by porcelain baking, glass fiber, cloth dipped in insulating paint winding and special material knotting. After the coil is manufactured, it needs to undergo a high water pressure test to ensure that the heating coil 3 does not leak during operation. The lead-out end of the heating coil 3 is made of copper, which is connected to the heating coil 3 by welding, and is connected to the IGBT medium frequency power supply. The tungsten furnace tube is heated to a temperature of 21800 degrees Celsius or above (including 1800 degrees Celsius) by the IGBT medium frequency power supply.

[0035] During the heating process, the heating temperature is monitored in real time by the infrared temperature measuring device 13. Specifically, a temperature measuring hole is set from the outer wall of the shell 1 to the outer wall of the tungsten furnace tube 2, and the infrared temperature measuring device 13 is installed in the temperature measuring hole to monitor the temperature of the outer wall of the tungsten furnace tube 2 in real time, so as to timely adjust the IGBT medium frequency power supply.

[0036] During the heating process of the tungsten bar, the protective gas unit 7 introduces inert gas (hydrogen, nitrogen, etc.) into the tungsten furnace tube 2 through the air inlet pipe, and adjusts the air inlet flow rate through the regulating valve to protect the heating process of the tungsten bar. Among them, the air inlet pipe is composed of two sections, one section buried in the side insulation unit 6 is a tungsten tube, and the part leaking out of the side insulation unit 6 is a high-temperature stainless steel tube.

[0037] At the same time, an exhaust hole 16 (the number is not less than 5, and the aperture is 2-5 mm) is opened on one end of the tungsten plate 8 near the furnace door unit, and a supporting protrusion is set on the bottom surface of the tungsten plate 8, and the supporting protrusion is located on the inner bottom surface of the tungsten furnace tube 2; the air intake duct passes through the shell 1 and the side insulation unit 6 in sequence from the outside of the shell 1, and then the inert gas enters the tungsten furnace tube 2 through an exhaust hole 16 with respect to the air holes on the tungsten plate 8, and a protective gas screen is formed in the tungsten furnace tube 2 to prevent outside air from entering the inside of the square furnace tube.

[0038] At the same time, an exhaust pipe 14 is also provided to exhaust the gas in the tungsten furnace tube 2. Specifically, the exhaust pipe 14 extends radially from the front insulation unit 4 to the middle temperature insulation layer of the side insulation unit 6, and then extends axially through the baffle. A valve is also provided on the exhaust pipe 14 to control the air flow of the exhaust pipe 14.

[0039] In the present application, after the tungsten bar is placed on the tungsten plate 8 in the tungsten furnace tube 2, the furnace door unit seals the feed hole. The furnace door unit includes: a furnace door cover 10, a connecting rod 11 and a driving connector 12. The furnace door cover 10 and the driving connector 12 are arranged in parallel. The two ends of the connecting rod 11 are rotatably connected to the furnace door cover 10 and the driving connector 12 respectively, and one end of the furnace door cover 10 is rotatably mounted on the shell 1; the driving connector 12 is connected to the output end of the driving unit installed on the shell 1, and moves under the drive of the driving unit, driving the furnace door cover 10 to rotate around the axis of its rotational connection with the shell 1, thereby opening or closing the feed hole.

[0040] In a specific example, a stopper is provided between the furnace door cover 10 and the front heat preservation unit 4, and the stopper is used to prevent the furnace door cover 10 from directly contacting the front heat preservation unit 4, so as to effectively protect the front heat preservation unit 4 and the furnace door cover 10. At the same time, the driving unit uses a cylinder and a foot switch to control the furnace door cover 10, wherein the cylinder is connected to the housing 1 by bolts through a bracket.

[0041] In the present application, each insulation brick is connected by a form fit; the tungsten plate 8 placed in the tungsten furnace tube 2 is a consumable and needs to be replaced regularly to achieve effective protection of the tungsten furnace tube 2 and the front insulation unit 4; the air intake pipe, the exhaust pipe 14, the coil lead-out end, etc. are all sealed by high-temperature refractory mud, high-temperature rubber, etc.; a bottom plate 15 is also provided under the shell 1, and the shell 1 is connected to the bottom plate 15 by bolts.

[0042] During the operation, first, close the furnace door cover 10, open the valve of the air inlet pipe, close the valve of the exhaust pipe 14, flush nitrogen into the tungsten furnace tube 2 for 5-10 minutes, and then turn off the nitrogen; at the same time, flush hydrogen into the tungsten furnace tube 2 for 5-10 minutes, open the valve of the exhaust pipe 14, and conduct a detonation test through the exhaust pipe 14; after the detonation test is qualified, turn on the IGBT medium frequency power supply, heat the tungsten furnace tube 2 through the heating coil 3, and ignite the gas at the exhaust pipe 14 to raise the tungsten furnace tube 2 to the process temperature.

[0043] Then, the furnace door cover 10 is opened by the foot switch, and the tungsten bars to be heated are placed in turn on the tungsten plate 8 in the square tungsten furnace tube 2. After the placement is completed, the furnace door cover 10 is closed to heat the tungsten bars. When the tungsten bars are heated to the set process time, the furnace door cover 10 is opened again, and the heated tungsten bars are taken out for straightening or blanking.

[0044] In this process, the tungsten bar (tungsten alloy rod blank) is heated by a tungsten heating element, with high heating efficiency, good temperature zone uniformity, and high heating temperature (heating temperature is greater than or equal to 1800 degrees Celsius), which increases the heating temperature and eliminates secondary pollution of the tungsten bar, providing a guarantee for the straightening and opening of the tungsten alloy billet.

[0045] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0046] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0047] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0048] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0049] In the present invention, the terms "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" mean that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0050] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. A medium frequency heating furnace for straightening and blanking tungsten bars, characterized in that: include: Shell, tungsten furnace tube, furnace door unit, heating unit, front insulation unit, rear insulation unit, side insulation unit and protective gas unit; The shell is a cylindrical structure with one end open and the other end closed. The tungsten furnace tube is coaxially sleeved in the shell. The rear insulation unit is arranged between the tungsten furnace tube and the closed end of the shell. The side insulation unit is arranged between the outer side wall of the tungsten furnace tube and the inner side wall of the shell. The heating unit is located in the side heat preservation unit and surrounds the outer side of the tungsten furnace tube, and is used to heat the tungsten furnace tube; The open end of the shell is provided with a baffle, the front heat preservation unit is arranged between the baffle and the tungsten furnace tube, and a feed hole is opened on the baffle; The furnace door unit is installed at the open end of the shell and is used to seal the feed hole; The protective gas unit is used to introduce inert gas into the tungsten furnace tube.

2. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 1 is characterized in that: The shell is composed of bakelite shell plates, and the baffle is made of heat-resistant steel; wherein the bakelite shell plates constituting the shell and the shell and the baffle are sealed with refractory mud or rubber.

3. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 1 is characterized in that: The bottom end of the side heat-insulating unit is pressed against the rear heat-insulating unit, and the top end is flush with the front heat-insulating unit and pressed against the baffle.

4. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 1 is characterized in that: The inner bottom surface of the tungsten furnace tube is also paved with a tungsten plate to place the tungsten bars to be processed; and / or, A tungsten block is placed between the tungsten furnace tube and the rear insulation unit, and one end of the tungsten block is connected to the rear insulation unit, and the other end is located on the tungsten plate, and the end of the tungsten plate close to the rear insulation unit penetrates into the tungsten furnace tube by 100-150 mm.

5. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 4, characterized in that: The protective gas unit introduces the inert gas into the tungsten furnace tube through an air inlet pipe. Correspondingly, an exhaust hole is provided on one end of the tungsten plate close to the furnace door unit, and a supporting protrusion is provided on the bottom surface of the tungsten plate, and the supporting protrusion is located on the inner bottom surface of the tungsten furnace tube; The air inlet pipe passes through the shell and the side insulation unit in sequence from the outside of the shell, and faces the air holes, so that the inert gas forms a protective gas screen in the tungsten furnace tube after passing through a row of the air holes.

6. According to claim 1, the medium frequency heating furnace for straightening and blanking tungsten bars is characterized in that: The rear insulation unit and the side insulation unit each comprise a high temperature insulation layer, a medium temperature insulation layer and a low temperature insulation layer, and the high temperature insulation layer, the medium temperature insulation layer and the low temperature insulation layer are sequentially arranged along the normal direction from the tungsten furnace tube to the shell; The insulation range of the high temperature insulation layer is 1900-2300°C, the insulation range of the medium temperature insulation layer is 1600-1900°C, and the insulation range of the low temperature insulation layer is 1000-1600°C. The front heat preservation unit has a heat preservation range of 1900-2300°C.

7. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 6, characterized in that: The heating coil of the heating unit is located in the low-temperature insulation layer of the side insulation unit, and the heating coil is buried in alumina refractory mud for coating.

8. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 1, characterized in that: Also includes: An infrared temperature measuring device is installed in the temperature measuring hole and is used to monitor the temperature of the outer wall of the tungsten furnace tube in real time; wherein the temperature measuring hole starts from the outer wall of the shell and penetrates to the outer wall of the tungsten furnace tube.

9. The medium frequency heating furnace for straightening and blanking tungsten bars according to claim 1, characterized in that: The furnace door unit comprises: a furnace door cover, a connecting rod and a driving connecting piece; The furnace door cover and the driving connecting member are arranged in parallel, the two ends of the connecting rod are rotatably connected to the furnace door cover and the driving connecting member respectively, and one end of the furnace door cover is rotatably mounted on the shell; The driving connector is connected to the output end of the driving unit installed on the shell, so as to move under the drive of the driving unit, driving the furnace door cover to rotate around the axis of its rotation connection with the shell to open or close the feed hole.

10. The medium frequency heating furnace for straightening and blanking tungsten bars according to any one of claims 1 to 9, characterized in that: The heating unit uses an IGBT power supply to heat the tungsten furnace tube, and the heating temperature is greater than or equal to 1800 degrees Celsius.