Method for reworking product comprising MCT layer

Through the gradual removal and grinding method, the problems of film defects and rupture in the MCT layer product are solved, and the semiconductor product is reworked, ensuring the quality and flatness of the product, and re-forming the MCT layer structure that meets the standards is re-formed.

CN118899302APending Publication Date: 2024-11-05SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410949025.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

In semiconductor processes, products containing MCT layers may have film defects or thickness that are not up to standard, and may easily break or scratch during handling, resulting in the inability to determine the specific damaged film layer. Rework is required to obtain products with quality standards.

Method used

A product rework method including an MCT layer is provided by gradually removing the anti-reflective layer, titanium nitride layer, nitride layer and upper plate, etching the metal layer to expose the lower plate, and removing the lower plate by grinding until the contact is exposed For the pore and interlayer dielectric layer, determine whether the flatness meets the standard. If the standard is met, the film layer will be formed again, otherwise the product will be discarded. An optional method includes multiple grinding to expose the contact holes and the interlayer dielectric layer and re-forming the film layer on the surface of the interlayer dielectric layer.

Benefits of technology

The scratched or cracked film layer is effectively removed, and the MCT layer product that meets the quality standards is re-formed, ensuring the thickness and flatness of the product and avoiding product abandonment caused by damage to the film layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118899302A_ABST
    Figure CN118899302A_ABST
Patent Text Reader

Abstract

The invention provides a reworking method of a product comprising an MCT layer, comprising: providing a product comprising a defective MCT layer, the MCT layer comprising an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers having a defect, wherein the plurality of film layers comprise a lower-stage plate positioned on the surface of the interlayer dielectric layer, a metal layer positioned on the surface of the lower-stage plate, an upper polar plate positioned on the surface of the metal layer, a first nitriding layer and a second nitriding layer which are respectively positioned on part of the surface of the upper polar plate, and a titanium nitride layer positioned on the surface of the first nitriding layer; the anti-reflection layer is simultaneously positioned on the surfaces of the titanium nitride layer and the second nitride layer; grinding to remove the anti-reflection layer; sequentially grinding the titanium nitride layer, the first nitride layer, the second nitride layer and the upper electrode plate to expose the surface of the metal layer; etching the metal layer to expose the surface of the lower-level plate; and grinding the lower plate to expose the contact hole and the surface of the interlayer dielectric layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of semiconductor technology, and in particular to a reworking method for a product comprising an MCT layer. Background Art

[0002] In semiconductor process integration, MCT (Metal-Capacitor) products such as metal / dielectric / metal capacitors are often used to manufacture capacitors, such as Figure 1 As shown, a silicon nitride SiN dielectric layer and a titanium nitride TiN metal layer are sequentially deposited on the aluminum Al metal layer, the titanium nitride TiN metal layer serves as an upper electrode, and the aluminum Al metal layer serves as a lower electrode. By etching the upper electrode and the lower electrode respectively, a metal / dielectric / metal capacitor is obtained.

[0003] Please refer to Figure 1 The product containing MCT layer in the prior art includes: an interlayer dielectric layer 110, a contact hole 120 located in the interlayer dielectric layer 110, a metal capacitor lower plate 130 located on the surface of the interlayer dielectric layer 110, a metal layer 140 located on the surface of the lower plate 130, a metal capacitor upper plate 150 located on the surface of the metal layer 140, a first nitride layer 160 and a second nitride layer 170 respectively located on the surface of part of the upper plate 150, the first nitride layer 160 and the second nitride layer 170 completely covering the surface of all the upper plate 150, a titanium nitride layer 180 located on the surface of the first nitride layer 160, and an anti-reflection layer 190 located on the surfaces of the titanium nitride layer 180 and the second nitride layer 170 at the same time. Among them, the lower plate 130 is a combination of TI and TIN, the upper plate is a combination of TI and TiN, the materials of the first nitride layer 160 and the second nitride layer 170 are silicon nitride, the material of the metal layer 140 is aluminum, and the material of the contact hole is tungsten metal. The thickness of the anti-reflective layer 190 is approximately 200 angstroms, the thickness of the titanium nitride layer 180 is approximately 1000 angstroms, the thickness of the first nitride layer 160 is approximately 560 angstroms, the thickness of the second nitride layer 170 is approximately 160 angstroms, the thickness of the upper plate 150 is approximately 590 angstroms, of which the thickness of TI is 90 angstroms and the thickness of TiN is 500 angstroms, the thickness of the metal layer 140 is 4400 angstroms, and the thickness of the lower plate 130 is 550 angstroms, of which the thickness of TI is 300 angstroms and the thickness of TiN is 250 angstroms.

[0004] However, in the preparation process of products containing MCT layers, one or more of the film layers may be defective or the thickness may not meet the standard. For example, in case 1, the thickness of the first nitride layer 160 and the second nitride layer 170 may not meet the standard. In case 2 and case 3, the falling of the product during transportation caused fragments, resulting in scratches or cracks on one or more of the multiple film layers, and it is impossible to know the specific film layer that was damaged. Therefore, the product containing the MCT layer needs to be reworked. Summary of the invention

[0005] The object of the present invention is to provide a reworking method for a product containing an MCT layer, which can be used to rework the product containing the MCT layer, remove the scratched or broken film layer, and obtain a product containing the MCT layer that meets the quality standards.

[0006] In order to achieve the above object, the present invention provides a reworking method for a product containing an MCT layer, comprising:

[0007] A product containing an MCT layer having defects is provided, wherein the product containing the MCT layer comprises an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers having defects, wherein the plurality of film layers comprises a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer;

[0008] removing and grinding the anti-reflection layer in sequence;

[0009] Grinding the titanium nitride layer, the first nitride layer, the second nitride layer and the upper electrode plate in sequence to expose the surface of the metal layer;

[0010] Etching the metal layer to expose the surface of the lower board;

[0011] The lower plate is ground to expose the contact hole and the surface of the interlayer dielectric layer.

[0012] Optionally, in the reworking method of the product comprising the MCT layer, the defect includes that the thickness of the film layer does not meet the standard or the quality of the film layer does not meet the standard.

[0013] Optionally, in the reworking method of the product including the MCT layer, after grinding the surface of the lower board to expose the contact hole and the interlayer dielectric layer, the method further comprises:

[0014] It is determined whether the surface flatness of the contact hole after the film layer is removed meets the standard. If so, multiple film layers are re-formed on the surface of the interlayer dielectric layer. If not, the product containing the MCT layer is discarded.

[0015] Optionally, in the reworking method of the product comprising the MCT layer, the method of re-forming a plurality of film layers on the surface of the interlayer dielectric layer comprises:

[0016] A lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer are sequentially formed on the surface of the interlayer dielectric layer.

[0017] The present invention also provides a reworking method for a product containing an MCT layer, comprising:

[0018] A product containing an MCT layer having defects is provided, wherein the product containing the MCT layer comprises an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers having defects, wherein the plurality of film layers comprises a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer;

[0019] Starting from the surface of the anti-reflection layer, multiple grinding methods are used to grind the multiple film layers in sequence to expose the contact holes and the interlayer dielectric layer, and the time for each grinding is the same. After each grinding, the grinding machine is corrected so that the grinding parameters can meet the standards.

[0020] Optionally, in the reworking method of the product comprising the MCT layer, the defect includes that the thickness of the film layer does not meet the standard or the quality of the film layer does not meet the standard.

[0021] Optionally, in the reworking method of the product including the MCT layer, starting from the surface of the anti-reflection layer, a plurality of the film layers are sequentially ground by a multiple grinding method to expose the contact hole and the interlayer dielectric layer, and further comprising:

[0022] It is determined whether the surface flatness of the contact hole after the film layer is removed meets the standard. If so, multiple film layers are re-formed on the surface of the interlayer dielectric layer. If not, the product containing the MCT layer is discarded.

[0023] Optionally, in the reworking method of the product comprising the MCT layer, the method of re-forming a plurality of film layers on the surface of the interlayer dielectric layer comprises:

[0024] A lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer are sequentially formed on the surface of the interlayer dielectric layer.

[0025] Optionally, in the reworking method of the product containing the MCT layer, starting from the surface of the anti-reflection layer, a tungsten chemical mechanical polishing device is used to perform 3 to 5 polishing steps to sequentially polish the multiple film layers to expose the contact holes and the interlayer dielectric layer.

[0026] Optionally, in the reworking method of the product containing the MCT layer, the grinding time for each time is 40s to 100s.

[0027] In the reworking method of the product containing the MCT layer provided by the present invention, the scratched or broken film layer is removed, and the product containing the MCT layer is reworked.

[0028] Further, a new film layer is re-formed to form a new product containing an MCT layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a schematic diagram of the structure of a product including an MCT layer;

[0030] Figure 2 is a flow chart of a reworking method for a product including an MCT layer according to Embodiment 1 of the present invention;

[0031] Figures 3 to 5 is a structural schematic diagram of a product containing an MCT layer during a reworking process of a product containing an MCT layer according to Embodiment 1 of the present invention;

[0032] Figure 6 is a flow chart of a reworking method for a product including an MCT layer according to a second embodiment of the present invention;

[0033] 110 - interlayer dielectric layer, 120 - contact hole, 130 - lower plate, 140 - metal layer, 150 - upper plate, 160 - first nitride layer, 170 - second nitride layer, 180 - titanium nitride layer, 190 - anti-reflection layer. DETAILED DESCRIPTION

[0034] The specific implementation of the present invention will be described in more detail below in conjunction with the schematic diagram. The advantages and features of the present invention will become clearer based on the following description. It should be noted that the drawings are all in a very simplified form and are not in exact proportions, and are only used to facilitate and clearly assist in explaining the purpose of the embodiments of the present invention.

[0035] Hereinafter, the terms "first", "second", etc. are used to distinguish between similar elements and are not necessarily used to describe a particular order or chronological sequence. It is to be understood that these terms used in this manner are interchangeable where appropriate. Similarly, if the method described herein includes a series of steps, the order of these steps presented herein is not necessarily the only order in which these steps can be performed, and some of the steps described may be omitted and / or some other steps not described herein may be added to the method.

[0036] Furthermore, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.

[0037] Embodiment 1

[0038] Please refer to Figure 2 The present invention provides a reworking method for a product containing an MCT layer, comprising:

[0039] S11: Provide a product including a defective MCT layer, wherein the MCT layer includes an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers has a defect, wherein the plurality of film layers include a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on the surface of a portion of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer;

[0040] S12: grinding and removing the anti-reflection layer;

[0041] S13: grinding the titanium nitride layer, the first nitride layer, the second nitride layer and the upper electrode plate in sequence to expose the surface of the metal layer;

[0042] S14: etching the metal layer to expose the surface of the lower board;

[0043] S15: Grind the lower-level board to expose the contact holes and the surface of the interlayer dielectric layer.

[0044] For details, please refer to Figure 1, firstly, a defective MCT layer is provided, including a film layer whose thickness does not meet the standard or a film layer whose quality does not meet the standard. The MCT layer includes: an interlayer dielectric layer 110, a contact hole 120 located in the interlayer dielectric layer 110, a metal capacitor lower plate 130 located on the surface of the interlayer dielectric layer 110, a metal layer 140 located on the surface of the lower plate 130, a metal capacitor upper plate 150 located on the surface of the metal layer 140, a first nitride layer 160 and a second nitride layer 170 located on the surface of a portion of the upper plate 150, the first nitride layer 160 and the second nitride layer 170 completely covering the surface of all the upper plates 150, a titanium nitride layer 180 located on the surface of the first nitride layer 160, and an anti-reflection layer 190 located on the surfaces of both the titanium nitride layer 180 and the second nitride layer 170. The lower plate 130 is a combination of TI and TIN, the upper plate is a combination of TI and TiN, the materials of the first nitride layer 160 and the second nitride layer 170 are silicon nitride, the material of the metal layer 140 is aluminum, and the material of the contact hole is tungsten metal. The thickness of the anti-reflection layer 190 is about 200 angstroms, the thickness of the titanium nitride layer 180 is about 1000 angstroms, the thickness of the first nitride layer 160 is about 560 angstroms, the thickness of the second nitride layer 170 is about 160 angstroms, the thickness of the upper plate 150 is about 590 angstroms, the thickness of TI is 90 angstroms, the thickness of TiN is 500 angstroms, the thickness of the metal layer 140 is 4400 angstroms, the thickness of the lower plate 130 is 550 angstroms, the thickness of TI is 300 angstroms, and the thickness of TiN is 250 angstroms. If one or more of the film layers among the lower plate 130, metal layer 140, upper plate 150, first nitride layer 160, second nitride layer 170, titanium nitride layer 180 and anti-reflection layer 190 do not meet the thickness standards or the quality standards, such as wear and tear, the product containing the MCT layer is considered to be defective and needs to be reworked.

[0045] Next, please refer to Figure 3 , remove the anti-reflection layer 190 by grinding; then, grind the titanium nitride layer 180, the first nitride layer 160, the second nitride layer 170 and the upper electrode 150 in sequence, so as to expose the surface of the metal layer 140. Figure 4 , etch the metal layer 140 to expose the surface of the lower board 130, and the etching method can be a dry etching method. Figure 5 , continue to grind the lower board 130 by grinding to expose the contact hole 120 and the interlayer dielectric layer 110. Next, determine whether the surface flatness of the contact hole after the film layer is removed meets the standard. If so, re-form multiple film layers on the surface of the interlayer dielectric layer. If not, discard the product containing the MCT layer. If so, re-form multiple film layers on the surface of the interlayer dielectric layer. If not, discard the product containing the MCT layer.

[0046] Next, a lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer are formed in sequence on the surface of the interlayer dielectric layer.

[0047] Embodiment 2

[0048] Please refer to Figure 6 Embodiment 2 of the present invention provides a reworking method for a product containing an MCT layer, comprising:

[0049] S21: Provide a product containing a defective MCT, wherein the MCT layer includes an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers has a defect, wherein the plurality of film layers include a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on the surface of a portion of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer;

[0050] S22: Starting from the surface of the anti-reflection layer, multiple film layers are ground in sequence using a multiple grinding method to expose the contact holes and the interlayer dielectric layer, and the grinding time for each time is the same. After each grinding, the grinding machine is corrected so that the grinding parameters can meet the standards.

[0051] For details, please refer to Figure 1, firstly, the defects include the thickness of the film layer not meeting the standard or the quality of the film layer not meeting the standard. The MCT layer includes: an interlayer dielectric layer 110, a contact hole 120 located in the interlayer dielectric layer 110, a metal capacitor lower plate 130 located on the surface of the interlayer dielectric layer 110, a metal layer 140 located on the surface of the lower plate 130, a metal capacitor upper plate 150 located on the surface of the metal layer 140, a first nitride layer 160 and a second nitride layer 170 located on the surface of part of the upper plate 150, the first nitride layer 160 and the second nitride layer 170 completely covering the surface of all the upper plates 150, a titanium nitride layer 180 located on the surface of the first nitride layer 160, and an anti-reflection layer 190 located on the surfaces of the titanium nitride layer 180 and the second nitride layer 170 at the same time. The lower plate 130 is a combination of TI and TIN, the upper plate is a combination of TI and TiN, the materials of the first nitride layer 160 and the second nitride layer 170 are silicon nitride, the material of the metal layer 140 is aluminum, and the material of the contact hole is tungsten metal. The thickness of the anti-reflection layer 190 is about 200 angstroms, the thickness of the titanium nitride layer 180 is about 1000 angstroms, the thickness of the first nitride layer 160 is about 560 angstroms, the thickness of the second nitride layer 170 is about 160 angstroms, the thickness of the upper plate 150 is about 590 angstroms, the thickness of TI is 90 angstroms, the thickness of TiN is 500 angstroms, the thickness of the metal layer 140 is 4400 angstroms, the thickness of the lower plate 130 is 550 angstroms, the thickness of TI is 300 angstroms, and the thickness of TiN is 250 angstroms. If one or more of the film layers among the lower plate 130, metal layer 140, upper plate 150, first nitride layer 160, second nitride layer 170, titanium nitride layer 180 and anti-reflection layer 190 do not meet the thickness standards or the quality standards, such as wear and tear, the product containing the MCT layer is considered to be defective and needs to be reworked.

[0052] Next, starting from the surface of the anti-reflection layer, a plurality of film layers are sequentially ground by a multiple grinding method to expose the contact holes and the interlayer dielectric layer, and the time for each grinding is the same, wherein the grinding machine is corrected after each grinding so that the grinding parameters can meet the standards. Specifically, starting from the surface of the anti-reflection layer 190, a tungsten chemical mechanical grinding device is used to grind 3 to 5 times, and multiple film layers are sequentially ground to expose the contact holes and the interlayer dielectric layer. The time for each grinding is 40s to 100s. The entire grinding time is 200s to 300s, and the grinding time is appropriately adjusted according to the thickness of each film layer.

[0053] Next, it is determined whether the surface flatness of the contact hole after the film layer is removed meets the standard. If it meets the standard, multiple film layers are re-formed on the surface of the interlayer dielectric layer. If it does not meet the standard, the product containing the MCT layer is discarded. Because the grinding method is used throughout the second embodiment, the metal layer is also ground. Therefore, there may be some metal layer residues on the surface of the interlayer dielectric layer 110 or the contact hole 120. This will affect the contact hole 120. If the impact is too large, it may affect the photolithography of the subsequent film layer formed on the contact hole 120. Therefore, it is necessary to detect the quality of the contact hole 120 in the end. Generally, the height of different places on the tungsten metal surface of the contact hole 120 can be checked to check the flatness of the tungsten metal surface of the contact hole 120. If the flatness meets the standard, multiple film layers are re-formed on the surface of the interlayer dielectric layer. In theory, the flatness of the second embodiment is better than that of the first embodiment, but the flatness may meet the standard.

[0054] The method for re-forming multiple film layers on the surface of an interlayer dielectric layer includes: sequentially forming a lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer.

[0055] In summary, in the reworking method for a product including an MCT layer provided in an embodiment of the present invention, the scratched or cracked film layer is removed, and the product including the MCT layer is reworked.

[0056] Further, a new film layer is re-formed to form a new product containing an MCT layer.

[0057] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any technician in the relevant technical field, without departing from the scope of the technical solution of the present invention, makes any form of equivalent replacement or modification to the technical solution and technical content disclosed in the present invention, which does not depart from the content of the technical solution of the present invention and still falls within the protection scope of the present invention.

Claims

1. A method for reworking a product comprising an MCT layer, characterized in that: include: Provided is a product comprising a defective MCT layer, wherein the MCT layer comprises an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers having a defect, wherein the plurality of film layers comprises a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer; Grinding and removing the anti-reflection layer; Grinding the titanium nitride layer, the first nitride layer, the second nitride layer and the upper electrode plate in sequence to expose the surface of the metal layer; Etching the metal layer to expose the surface of the lower board; The lower plate is ground to expose the contact hole and the surface of the interlayer dielectric layer.

2. The reworking method of a product comprising an MCT layer according to claim 1, characterized in that: The defects include that the thickness of the film layer does not meet the standards or the quality of the film layer does not meet the standards.

3. The reworking method of a product comprising an MCT layer according to claim 1, characterized in that: After grinding the surface of the lower board to expose the contact hole and the interlayer dielectric layer, the method further includes: It is determined whether the surface flatness of the contact hole after the film layer is removed meets the standard. If so, multiple film layers are re-formed on the surface of the interlayer dielectric layer. If not, the product containing the MCT layer is discarded.

4. The reworking method of a product comprising an MCT layer as claimed in claim 3, characterized in that: The method for re-forming a plurality of film layers on the surface of the interlayer dielectric layer comprises: A lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer are sequentially formed on the surface of the interlayer dielectric layer.

5. A method for reworking a product comprising an MCT layer, characterized in that: include: Provided is a product comprising an MCT layer having defects, wherein the MCT layer comprises an interlayer dielectric layer, a contact hole located in the interlayer dielectric layer, and a plurality of film layers located on the surface of the interlayer dielectric layer, at least one of the plurality of film layers having defects, wherein the plurality of film layers comprises a lower plate located on the surface of the interlayer dielectric layer, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer; Starting from the surface of the anti-reflection layer, multiple grinding methods are used to grind the multiple film layers in sequence to expose the contact holes and the interlayer dielectric layer, and the time for each grinding is the same. After each grinding, the grinding machine is corrected so that the grinding parameters can meet the standards.

6. The reworking method of a product comprising an MCT layer according to claim 5, characterized in that: The defects include that the thickness of the film layer does not meet the standards or the quality of the film layer does not meet the standards.

7. The reworking method of a product comprising an MCT layer according to claim 5, characterized in that: Starting from the surface of the anti-reflection layer, a plurality of the film layers are ground in sequence by a multiple grinding method to expose the contact hole and the interlayer dielectric layer, and further comprising: It is determined whether the surface flatness of the contact hole after the film layer is removed meets the standard. If so, multiple film layers are re-formed on the surface of the interlayer dielectric layer. If not, the product containing the MCT layer is discarded.

8. The method for reworking a product comprising an MCT layer according to claim 5, characterized in that: The method for re-forming a plurality of film layers on the surface of the interlayer dielectric layer comprises: A lower plate, a metal layer located on the surface of the lower plate, an upper plate located on the surface of the metal layer, a first nitride layer and a second nitride layer respectively located on a portion of the surface of the upper plate, a titanium nitride layer located on the surface of the first nitride layer, and an anti-reflection layer located on the surfaces of both the titanium nitride layer and the second nitride layer are sequentially formed on the surface of the interlayer dielectric layer.

9. The method for reworking a product comprising an MCT layer according to claim 5, characterized in that: Starting from the surface of the anti-reflection layer, a tungsten chemical mechanical polishing process equipment is used to perform 3 to 5 polishing processes to sequentially polish the plurality of film layers to expose the contact holes and the interlayer dielectric layer.

10. The method for reworking a product comprising an MCT layer according to claim 5, characterized in that: Each grinding time is 40s to 100s.