Preparation method of semiconductor device, semiconductor device and memory chip

By forming an etching barrier layer on the side of the dielectric layer facing away from the semiconductor substrate and thinning it using a wet etching process, the process poor problem caused by the difference in the memory cell area and the peripheral circuit section during the preparation of capacitor components in DRAM is solved, and the semiconductor device is improved Preparation yield and performance.

CN118900561APending Publication Date: 2024-11-05CHENGDU HIGH-TECH JIN SCI&TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410991195.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

During the manufacturing of dynamic random access memory (DRAM), when the capacitive components that accumulate charge are prepared, the segment difference between the memory cell region and the peripheral circuit region is large, resulting in poor planarization process of dielectric layer and affecting the preparation yield of semiconductor devices .

Method used

By forming an etching barrier layer on the side of the dielectric layer facing away from the semiconductor substrate and removing the portion in contact with the first surface to expose the first part of the dielectric layer, the first part is thinned by using a wet etching process to avoid the second part Cause damage and reduce the need for chemical mechanical polishing.

Benefits of technology

It improves the production yield of semiconductor devices, reduces the damage probability of dielectric layers and capacitive components, simplifies the process flow, and reduces the preparation cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900561A_ABST
    Figure CN118900561A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a semiconductor device, the semiconductor device and a memory chip, the semiconductor device comprises a first region and a second region, and the preparation method of the semiconductor device comprises the following steps: forming a capacitor element located in the first region on one side of a semiconductor substrate; a dielectric layer is formed on the side, away from the semiconductor substrate, of the capacitor element, the dielectric layer comprises a first part located in the first region and a second part located in the second region, the first part comprises a first surface located on the side, away from the semiconductor substrate, of the capacitor element, and the second part comprises a second surface located on the side, away from the semiconductor substrate, of the capacitor element; the first surface is located on one side of the second surface deviating from the semiconductor substrate; forming an etching barrier layer on one side, deviating from the semiconductor substrate, of the dielectric layer, and patterning the etching barrier layer to expose the first part; and carrying out thinning treatment on the first part so as to enable the surface of one side, deviating from the semiconductor substrate, of the first part to be flush with the second surface. According to the preparation method of the semiconductor device provided by the invention, the preparation yield of the semiconductor device can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of semiconductor technology, and in particular, relates to a method for preparing a semiconductor device, a semiconductor device and a memory chip. Background Art

[0002] In the process of manufacturing dynamic random access memory (DRAM), when preparing capacitor elements for accumulating charge, the step difference between the storage unit area (cell area) and the peripheral circuit area (including the core area and the peri area) will be large. Flattening is achieved by preparing a dielectric layer above the capacitor element. However, the preparation of the dielectric layer is prone to process defects, resulting in a low preparation yield. Summary of the invention

[0003] The purpose of this application is to at least solve the problem of low yield rate of semiconductor device manufacturing. This purpose is achieved through the following technical solutions:

[0004] A first aspect of the present application provides a method for preparing a semiconductor device, wherein the semiconductor device comprises a first region and a second region, and the preparation method comprises:

[0005] providing a semiconductor substrate;

[0006] forming a capacitor element located in the first region on one side of the semiconductor substrate;

[0007] A dielectric layer is formed on a side of the capacitor away from the semiconductor substrate, the dielectric layer includes a first portion located in the first region and a second portion located in the second region, the first portion includes a first surface located on a side away from the semiconductor substrate, the second portion includes a second surface located on a side away from the semiconductor substrate, and the first surface is located on a side of the second surface away from the semiconductor substrate;

[0008] forming an etch stop layer on a side of the dielectric layer facing away from the semiconductor substrate, and patterning the etch stop layer to expose the first portion;

[0009] Performing a thinning process on the first portion so that a surface of the first portion facing away from the semiconductor substrate is flush with the second surface;

[0010] The etch stop layer is removed.

[0011] In the preparation method of the semiconductor device provided by the present application, an etching barrier layer is formed on the surface of the side of the dielectric layer away from the semiconductor substrate, and the part of the etching barrier layer in contact with the first surface is removed to expose the first part of the dielectric layer and shield the second part of the dielectric layer, so that in the subsequent thinning process of the first part, the wet etching process can be used to thin the first part, and the etching barrier layer can block the wet etching solution to avoid damage to the second part. That is, in the preparation method provided by the present application, the preparation of the etching barrier layer provides the possibility of subsequent thinning of the first part by a wet etching process. The yield of the thinning process of the first part by the wet etching process is better, so that the flattening process of the dielectric layer only needs to perform a wet etching step, and no subsequent chemical mechanical polishing process is required, thereby reducing the probability of damage to the first part and the capacitor element, so as to improve the preparation yield of the semiconductor device. In a feasible embodiment, the etching barrier layer is formed by a chemical vapor deposition process.

[0012] The second aspect of the present application further provides a semiconductor device, which is prepared by the method for preparing a semiconductor device provided by the first aspect of the present application, wherein the semiconductor device comprises a first region and a second region, and the semiconductor device comprises:

[0013] Semiconductor substrates;

[0014] A capacitor element, located on one side of the semiconductor substrate and located in the first region;

[0015] The dielectric layer includes a first portion located in the first area and a second portion located in the second area, wherein the first portion is located on a side of the capacitor away from the semiconductor substrate, and a surface of the first portion away from the semiconductor substrate is flush with a surface of the second portion away from the semiconductor substrate.

[0016] The third aspect of the present application also provides a memory chip, comprising the semiconductor device provided in the second aspect of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present application. Moreover, the same reference numerals are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0018] Figure 1 is a flow chart of a method for preparing a semiconductor device provided in an embodiment of the present application;

[0019] Figures 2 to 6 It is a schematic diagram of a preparation process of a semiconductor device provided in an embodiment of the present application.

[0020] The reference numerals are as follows:

[0021] 1. semiconductor device; A1. first area; A2. second area; 11. semiconductor substrate; 12. capacitor element; 120. second electrode; 13. dielectric layer; 131. first portion; 1311. first surface; 132. second portion; 1321. second surface; 14. etching stop layer; 15. isolation layer. DETAILED DESCRIPTION

[0022] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0023] It should be understood that the terms used herein are only for the purpose of describing specific example embodiments and are not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms "one", "an" and "said" as used herein may also be meant to include plural forms. The terms "include", "comprise", "contain", and "have" are inclusive, and therefore specify the existence of stated features, steps, operations, elements and / or parts, but do not exclude the existence or addition of one or more other features, steps, operations, elements, parts, and / or combinations thereof. The method steps, processes, and operations described herein are not interpreted as necessarily requiring them to be performed in the specific order described or illustrated, unless the execution order is clearly indicated. It should also be understood that additional or alternative steps may be used.

[0024] Although the terms first, second, third, etc. can be used in the text to describe multiple elements, components, regions, layers and / or sections, these elements, components, regions, layers and / or sections should not be limited by these terms. These terms can only be used to distinguish an element, component, region, layer or section from another region, layer or section. Unless the context clearly indicates, terms such as "first", "second" and other numerical terms do not imply order or sequence when used in the text. Therefore, the first element, component, region, layer or section discussed below can be referred to as the second element, component, region, layer or section without departing from the teaching of the example embodiments.

[0025] For ease of description, spatial relative terms may be used herein to describe the relationship of one element or feature relative to another element or feature as shown in the figure, such as "inside", "outside", "inner side", "outer side", "below", "below", "above", "above", etc. Such spatial relative terms are intended to include different orientations of the device in use or operation in addition to the orientation depicted in the figure. For example, if the device in the figure is turned over, then the elements described as "below other elements or features" or "below other elements or features" will subsequently be oriented as "above other elements or features" or "above other elements or features". Therefore, the example term "below..." can include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or in other directions) and the spatial relative descriptors used in the text are interpreted accordingly.

[0026] The inventor has found through research that in the process of manufacturing dynamic random access memory (DRAM), when preparing the capacitor element for accumulating charge, the step difference between the storage cell area (cell area) and the peripheral circuit area (including the core area and the peri area) will be large, and this step difference is easy to cause subsequent process failures, so the flattening process is indispensable. In order to eliminate this step difference, a dielectric layer is generally used for flattening. In the process of flattening through the dielectric layer, the upper surface of the dielectric layer needs to be flattened, specifically including: removing at least part of the dielectric layer on the capacitor element through a dry etching process to reduce the step difference between the storage cell area (cell area) and the peripheral circuit area (including the core area and the peri area), and then flattening the upper surface of the dielectric layer through a chemical mechanical polishing (CMP) process. Due to the loading effect when dry etching the dielectric layer, it is very easy to have poor dry etching process. When the chemical mechanical polishing process is performed later, the dielectric layer that has already been poor is easy to break under the polishing pressure or rotation pressure, and even cause damage to the capacitor element. After the breakage, part of the dielectric layer will be torn off, causing subsequent engineering failures. That is, the planarization process in the relevant technology is prone to failure, affecting the production yield of semiconductor devices.

[0027] like Figure 1 As shown, according to an embodiment of the present application, a method for preparing a semiconductor device is proposed, wherein the semiconductor device 1 includes a first area A1 and a second area A2, wherein, in the semiconductor device 1, the first area A1 may be a storage unit area (cell area), and the second area A2 may be a peripheral circuit area (including a Core area and a Peri area). The preparation method includes:

[0028] S200 , providing a semiconductor substrate 11 .

[0029] Specifically, the semiconductor substrate 11 may include a substrate and other structures / devices formed on one side of the substrate, such as connection lines, transistors, etc.

[0030] S400 , forming the capacitor 12 located in the first area A1 on one side of the semiconductor substrate 11 .

[0031] The steps for preparing the capacitor element 12 are the same as the steps for preparing the capacitor element 12 in the semiconductor device 1 in the conventional technology. The steps may include: forming a first electrode on the semiconductor substrate 11, forming a capacitor dielectric layer on the side of the first electrode away from the semiconductor substrate 11, and forming a second electrode 120 on the side of the capacitor dielectric layer away from the first electrode. The second electrode 120 may wrap the capacitor dielectric layer.

[0032] Specifically, a bit line is formed in the portion of the semiconductor substrate 11 located in the first area A1, and the first electrode of the capacitor 12 can be electrically connected to the bit line. The capacitor 12 may include a stack structure or a cylindrical structure formed on the bit line. The capacitor 12 can be read or written through the bit line.

[0033] S600, such as Figure 2 As shown, a dielectric layer 13 is formed on the side of the capacitor element 12 facing away from the semiconductor substrate 11, and the dielectric layer 13 includes a first portion 131 located in the first area A1 and a second portion 132 located in the second area A2. The first portion 131 includes a first surface 1311 located on the side facing away from the semiconductor substrate 11, and the second portion 132 includes a second surface 1321 located on the side facing away from the semiconductor substrate 11. The first surface 1311 is located on the side of the second surface 1321 facing away from the semiconductor substrate 11.

[0034] Specifically, since a capacitor element 12 is formed on one side of a portion located in the first area A1 of the semiconductor substrate 11, and a capacitor element 12 or other structure is not formed on one side of a portion located in the second area A2, the first portion 131 of the dielectric layer 13 is in contact with the capacitor element 12, and a distance between the first surface 1311 and the semiconductor substrate 11 is relatively large; the second portion 132 of the dielectric layer 13 is in contact with the semiconductor substrate 11, and a distance between the second surface 1321 and the semiconductor substrate 11 is relatively small, and therefore a relatively large step difference is formed between the first portion 131 and the second portion 132.

[0035] S800, such as Figure 3 and Figure 4 As shown, an etch stop layer 14 is formed on the side of the dielectric layer 13 facing away from the semiconductor substrate 11 , and the etch stop layer 14 is patterned to expose the first portion 131 .

[0036] Specifically, the thickness of the etch stop layer 14 is D, 100 nm≤D≤200 nm.

[0037] Specifically, the etching stop layer 14 is patterned, the portion of the etching stop layer 14 located on the first surface 1311 is removed, and the portion of the etching stop layer 14 located on the second surface 1321 and the portion located on the side surface of the first portion 131 facing the second portion 132 are retained. That is, the first portion 131 can be exposed and the second portion 132 can be shielded by the etching stop layer 14.

[0038] S1000, such as Figure 5 As shown, the first portion 131 is thinned so that a surface of the first portion 131 facing away from the semiconductor substrate 11 is flush with the second surface 1321 .

[0039] Specifically, the first portion 131 is thinned to eliminate the step difference between the first portion 131 and the second portion 132 , thereby improving the flatness of the surface of the dielectric layer 13 facing away from the semiconductor substrate 11 , thereby improving the yield of subsequent processes.

[0040] S1200, such as Figure 6 As shown, the etch stop layer 14 is removed.

[0041] Specifically, the etching stop layer 14 is removed to avoid interfering with subsequent processes.

[0042] In the preparation method of the semiconductor device provided by the present application, an etching stop layer 14 is formed on the surface of the side of the dielectric layer 13 away from the semiconductor substrate 11, and the part of the etching stop layer 14 in contact with the first surface 1311 is removed to expose the first part 131 of the dielectric layer 13 and block the second part 132 of the dielectric layer 13, so that in the subsequent thinning process of the first part 131, the first part 131 can be thinned by a wet etching process, and the etching stop layer 14 can block the wet etching solution to avoid damage to the second part 132. That is, in the preparation method provided by the present application, the preparation of the etching stop layer 14 provides the possibility of thinning the first part 131 by a wet etching process. The yield of thinning the first part 131 by a wet etching process is better, so that the planarization process of the dielectric layer 13 only needs to perform a wet etching step, and no subsequent chemical mechanical polishing process is required, thereby reducing the probability of damage to the first part 131 and the capacitor element 12, so as to improve the preparation yield of the semiconductor device 1.

[0043] In a feasible implementation, the etch stop layer 14 is formed by a chemical vapor deposition process.

[0044] In the above embodiment, the etching stop layer 14 is directly formed as a whole layer by chemical vapor deposition, and the preparation method is simple.

[0045] In a possible implementation, Figure 3 As shown, the step of patterning the etching stop layer 14 includes:

[0046] The portion of the etch stop layer 14 located in the first area A1 is removed by a chemical mechanical polishing process.

[0047] Since the portion of the etch stop layer 14 located on the side of the first portion 131 away from the semiconductor substrate 11 is located at a relatively high position and has a faster etching rate, and the portion of the etch stop layer 14 located on the side of the second portion 132 away from the semiconductor substrate 11 has a slower etching rate, the portion of the etch stop layer 14 located on the side of the first portion 131 away from the semiconductor substrate 11 can be removed by a chemical mechanical polishing process. In the above embodiment, the etch stop layer 14 is first formed as a whole layer and then patterned. During the patterning process, since only the portion of the etch stop layer 14 located on the side of the first portion 131 of the dielectric layer 13 away from the semiconductor substrate 11 needs to be removed, and since the height of the first portion 131 is relatively high, the portion of the etch stop layer 14 located in the first area A1 can be removed by a chemical mechanical polishing process. Since the first portion 131 needs to be thinned later, the precision requirement for chemical mechanical polishing is also relatively low. It is only necessary to completely remove the portion of the etch stop layer 14 located in the first area A1 to avoid affecting the subsequent thinning process, and there is no need to accurately control not to damage the first portion 131.

[0048] In the above embodiment, in the process of preparing the etch stop layer 14 as a whole layer and then patterning it, no mask plate is needed, thereby saving costs.

[0049] In a possible implementation, Figure 4 As shown, the thinning process of the first portion 131 includes:

[0050] The first portion 131 is thinned by a wet etching process.

[0051] In the above embodiment, the first part 131 is thinned by a wet etching process. It is only necessary to control the dosage, concentration and reaction time of the etching solution to more accurately control the thinned thickness. The flatness after thinning by the wet etching process is high, and no chemical mechanical polishing is required, thereby reducing the adverse effects on the dielectric layer 13 and the capacitor element 12 caused by the force during chemical mechanical polishing. Compared with the dry etching process in the related art, this step can reduce the alignment accuracy requirements during the etching process, thereby improving the etching deviation problem caused by low alignment accuracy. The mask step can be omitted, reducing the preparation cost. The wet etching process can reduce the pressure on the first part 131 and the capacitor element 12, thereby reducing the probability of the first part 131 and the capacitor element 12 being broken due to excessive pressure, which helps to improve the preparation yield.

[0052] In a feasible implementation manner, the material of the etch stop layer 14 includes silicon nitride.

[0053] Specifically, silicon nitride is highly stable, and the material is easily available and low in cost. Other materials that do not react with the etching solution of the dielectric layer 13 may also be used.

[0054] In a possible implementation, Figure 5 As shown, the step of removing the etching stop layer 14 includes:

[0055] The etching stop layer 14 is removed by an etching solution.

[0056] In the above embodiment, the etching stop layer 14 is also removed by etching solution, thereby reducing the impact of the removal process of the etching stop layer 14 on the flatness of the second surface 1321, and the removal method is simple, without the need for a mask plate, etc., and the cost is low.

[0057] Specifically, when the etching stop layer 14 is made of silicon nitride, the etching solution may be a phosphoric acid solution.

[0058] Specifically, the etching stop layer 14 includes a portion located on the side of the first portion 131 and a portion located on the side of the second portion 132 away from the semiconductor substrate 11, wherein the portion located on the side of the first portion 131 can limit the wet etching solution to prevent it from diffusing during the thinning process of the first portion 131. The portion located on the side of the second portion 132 away from the semiconductor substrate 11 can protect the second portion 132 to prevent the second surface from contacting the wet etching solution.

[0059] When removing the etching stop layer 14 , the etching solution simultaneously removes the portion located on the peripheral side of the first portion 131 and the portion located on the side of the second portion 132 away from the semiconductor substrate 11 .

[0060] In a feasible implementation manner, the dielectric layer 13 includes an oxide insulating layer, and the oxide insulating layer is formed by a chemical vapor deposition process.

[0061] In the above embodiment, the material of the dielectric layer 13 may include an oxide insulating material and is formed by chemical vapor deposition, which has a simple preparation process and low cost. The dielectric layer 13 can flatten the underlying film layer on the one hand to improve the preparation yield of thick subsequent film layers, and can also play an insulating role to achieve insulation between the capacitor element 12 and the subsequent film layers.

[0062] In a possible implementation, Figures 2 to 6 As shown, before the step of forming the capacitor element 12 located in the first area A1 on one side of the semiconductor substrate 11, the step further includes:

[0063] An isolation layer 15 is formed on the semiconductor substrate 11 side.

[0064] In the above-mentioned embodiment, the material of the isolation layer 15 may include SiBN.

[0065] Specifically, the isolation layer 15 can achieve isolation and insulation between the structure / routing inside the semiconductor substrate 11 and the subsequent film layer (such as the capacitor element 12), and can provide support for the preparation of the subsequent film layer. At the same time, it can protect the semiconductor substrate 11 to prevent the etching process from affecting the structure / device inside the semiconductor substrate 11, thereby improving the preparation yield of the semiconductor device 1.

[0066] The present application also provides a semiconductor device 1, which is prepared by any one of the methods for preparing a semiconductor device 1 provided in the above embodiments. Figure 6 As shown, the semiconductor device 1 includes a first area A1 and a second area A2, and the semiconductor device 1 includes a semiconductor substrate 11, a capacitor 12 and a dielectric layer 13, the capacitor 12 is located on one side of the semiconductor substrate 11 and is located in the first area A1; the dielectric layer 13 includes a first portion 131 located in the first area A1 and a second portion 132 located in the second area A2, the first portion 131 is located on a side of the capacitor 12 away from the semiconductor substrate 11, and a surface of the first portion 131 on a side away from the semiconductor substrate 11 is flush with a surface of the second portion 132 on a side away from the semiconductor substrate 11.

[0067] In the above embodiment, since the semiconductor device 1 does not need to use a dry etching process to pattern the dielectric layer 13 during the preparation process, and does not need to perform chemical mechanical polishing, the pressure on the dielectric layer 13 and the capacitor 12 can be reduced, thereby improving the yield of the semiconductor device 1. By adding an etching stop layer 14 and patterning the dielectric layer 13 using a wet etching process, the process is simple, and there is no need to use a mask for patterning, thereby saving costs, and the damage to the semiconductor device 1 is small, so that the yield of the semiconductor device 1 is high.

[0068] The present application also provides a memory chip, comprising the semiconductor device 1 provided in the above-mentioned embodiment of the present application.

[0069] The preparation cost of this memory chip is low and the yield rate is high, and the overall performance is significantly improved.

[0070] The above are only preferred specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.

Claims

1. A method for preparing a semiconductor device, characterized in that: The semiconductor device comprises a first region and a second region, and the preparation method comprises: providing a semiconductor substrate; forming a capacitor element located in the first region on one side of the semiconductor substrate; A dielectric layer is formed on a side of the capacitor away from the semiconductor substrate, the dielectric layer includes a first portion located in the first region and a second portion located in the second region, the first portion includes a first surface located on a side away from the semiconductor substrate, the second portion includes a second surface located on a side away from the semiconductor substrate, and the first surface is located on a side of the second surface away from the semiconductor substrate; forming an etch stop layer on a side of the dielectric layer facing away from the semiconductor substrate, and patterning the etch stop layer to expose the first portion; Performing a thinning process on the first portion so that a surface of the first portion facing away from the semiconductor substrate is flush with the second surface; The etch stop layer is removed.

2. The method for preparing a semiconductor device according to claim 1, wherein: The etch stop layer is formed by a chemical vapor deposition process.

3. The method for preparing a semiconductor device according to claim 1, wherein: The step of patterning the etch stop layer comprises: The portion of the etch stop layer located in the first region is removed by a chemical mechanical polishing process.

4. The method for preparing a semiconductor device according to claim 1, wherein: The thinning process of the first portion comprises: The first portion is thinned by a wet etching process.

5. The method for preparing a semiconductor device according to claim 1, characterized in that: The material of the etching stop layer includes silicon nitride.

6. The method for preparing a semiconductor device according to claim 5, characterized in that: The step of removing the etching stop layer comprises: The etching stop layer is removed by etching solution.

7. The method for preparing a semiconductor device according to claim 6, characterized in that: The etching solution includes a phosphoric acid solution.

8. The method for preparing a semiconductor device according to claim 1, characterized in that: The dielectric layer includes an oxide insulating layer, and the oxide insulating layer is formed by a chemical vapor deposition process.

9. The method for preparing a semiconductor device according to claim 1, wherein: Before the step of forming a capacitor element located in the first region on one side of the semiconductor substrate, the step further includes: An isolation layer is formed on one side of the semiconductor substrate.

10. A semiconductor device, characterized in that: The semiconductor device is prepared by the method for preparing a semiconductor device according to any one of claims 1 to 9, wherein the semiconductor device comprises a first region and a second region, and the semiconductor device comprises: Semiconductor substrates; A capacitor element, located on one side of the semiconductor substrate and located in the first region; The dielectric layer includes a first portion located in the first area and a second portion located in the second area, wherein the first portion is located on a side of the capacitor away from the semiconductor substrate, and a surface of the first portion away from the semiconductor substrate is flush with a surface of the second portion away from the semiconductor substrate.

11. A memory chip, characterized in that: Comprising the semiconductor device as claimed in claim 10.