Display device and method of manufacturing same

By using multifunctional resin protection components in the display device and combining with a simplified manufacturing process, the problems of single function and complex process in the prior art are solved, and efficient and low-cost display device protection is achieved.

CN118900607APending Publication Date: 2024-11-05SAMSUNG DISPLAY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410364532.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-04
Filing Date
2024-03-28
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The protective components of existing display devices are difficult to have the functions of heat dissipation, electromagnetic wave shielding, light blocking and shock absorption at the same time, and the manufacturing process is complex, resulting in high costs and high defect risks.

Method used

The open-cell frame is formed by the first resin, and the second resin fills the frame and cures to form a protective member with an adhesive, filler, light barrier material and foaming agent. After the frame is removed, the mother substrate is cut and applied directly to the Display the lower surface of the panel to simplify the process and improve yield.

Benefits of technology

The multifunctional protection of the display device is realized, reducing manufacturing costs and defect risks, while improving process simplification and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900607A_ABST
    Figure CN118900607A_ABST
Patent Text Reader

Abstract

The invention relates to a display device and a method of manufacturing the same. The method includes: forming a frame including an opening by applying a first resin to a surface of a mother substrate and curing the first resin; forming a protective member by applying a second resin to the opening of the frame and curing the second resin; and cutting the mother substrate along a region between the protective members after removing the frame, wherein the second resin includes a material different from a material of the first resin.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2023-0058507 filed in the Korean Intellectual Property Office on May 4, 2023, the disclosure of which is incorporated herein in its entirety by reference. Technical Field

[0003] Aspects of some embodiments of the present disclosure relate to a display device and a method of manufacturing the display device. Background Art

[0004] With the development of multimedia, display devices become more and more important. Display devices include liquid crystal displays (LCDs) and organic light emitting displays (OLEDs).

[0005] The display device may include a protection member having functions such as heat dissipation and buffering on a lower surface of the display panel to protect itself from heat generated from a light emitting element or a driving chip driving the light emitting element and external impact.

[0006] Such a protective member may include a plurality of different functional layers that perform their respective functions (such as heat dissipation and buffering), but may also include a single functional layer that can perform all of the above functions.

[0007] The above information disclosed in this Background section is only for enhancement of understanding of the background technology, and therefore, the information discussed in this Background section does not necessarily constitute prior art. Summary of the invention

[0008] Aspects of some embodiments of the present disclosure include a display device including a protection member having a heat dissipation function, an electromagnetic wave shielding function, a light blocking function, and a shock absorbing function.

[0009] Aspects of some embodiments of the present disclosure may also include a method of manufacturing a display device having a relatively improved yield of a protection member forming process.

[0010] However, aspects of the embodiments of the present disclosure are not limited to those specifically described herein. The above and other aspects of the embodiments of the present disclosure will become more apparent to those skilled in the art to which the present disclosure belongs by referring to the detailed description of the present disclosure given below.

[0011] According to some embodiments of the present disclosure, in a method for manufacturing a display device, the method includes: forming a frame including an opening by applying a first resin to a surface of a mother substrate and curing the first resin, forming a protective member by applying a second resin to the opening of the frame and curing the second resin, and cutting the mother substrate along an area between the protective members after removing the frame, wherein the second resin includes a material different from that of the first resin.

[0012] According to some embodiments, in the forming of the protection member, the protection member is surrounded by the frame and is located in the opening.

[0013] According to some embodiments, in the forming of the protection member, a thickness of the second resin before being cured in the opening is less than or equal to a thickness of the frame.

[0014] According to some embodiments, the thickness of the second resin after curing in the open hole is 40% to 60% of the thickness of the second resin before curing.

[0015] According to some embodiments, each protection member has a thickness of 100 μm to 300 μm.

[0016] According to some embodiments, the second resin includes at least one of a binder, a first filler, a second filler, a light blocking material, and a foaming agent.

[0017] According to some embodiments, the first filler includes at least one of a carbon-based material and a ceramic-based material, and the second filler includes at least one of a carbon-based material and a metal-based material.

[0018] According to some embodiments, the light blocking material includes at least one of carbon black, a black pigment, and a black dye.

[0019] According to some embodiments, the binder includes at least one of an acrylic resin, a urethane resin, a silicone resin, and a rubber resin.

[0020] According to some embodiments, the elongation of the frame is 200% or more.

[0021] According to some embodiments, in the forming of the frame, the first resin is cured by at least one of thermal curing, natural curing, and ultraviolet curing.

[0022] According to some embodiments, the second resin has a viscosity of 10,000 cPs to 50,000 cPs.

[0023] According to some embodiments, in the removal of the frame, the protection member includes a removal mark formed on a side surface thereof due to the removal of the frame.

[0024] According to some embodiments, in the cutting of the mother substrate, the dummy is located between the protection members, and the mother substrate is cut along a region between the dummy and each of the protection members.

[0025] According to some embodiments, in the forming of the protection member, the second resin is applied into the openings by a screen printing method using a doctor blade.

[0026] According to some embodiments, the method further includes forming a display layer on another surface of the mother substrate opposite to the surface.

[0027] According to some embodiments of the present disclosure, a display device includes: a substrate; a display layer located on a first surface of the substrate; and a protective member located on a second surface of the substrate opposite to the first surface and including a resin, wherein the protective member includes a removal mark on a side surface thereof, and the removal mark is formed by removing a frame surrounding the protective member.

[0028] According to some embodiments, the protective member has a thickness of 100 μm to 300 μm.

[0029] According to some embodiments, the resin includes at least one of a binder, a first filler, a second filler, a light blocking material, and a foaming agent.

[0030] According to some embodiments, the first filler includes at least one of a carbon-based material and a ceramic-based material, and the second filler includes at least one of a carbon-based material and a metal-based material.

[0031] According to some embodiments, the light blocking material includes at least one of carbon black, a black pigment, and a black dye.

[0032] According to some embodiments, the binder includes at least one of an acrylic resin, a urethane resin, a silicone resin, and a rubber resin.

[0033] According to some embodiments, the elongation of the frame is 200% or more.

[0034] A display device according to some embodiments of the present disclosure may include a protection member having a heat dissipation function, an electromagnetic wave shielding function, a light blocking function, and a shock absorbing function.

[0035] The method of manufacturing a display device according to some embodiments of the present disclosure may relatively improve the yield of a protective member forming process.

[0036] However, the features of the embodiments according to the present disclosure are not limited to those specifically stated herein. The above and other features of the embodiments according to the present disclosure will become more apparent to those skilled in the art to which the present disclosure belongs by referring to the claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] These and / or other features will become more apparent and more easily understood through the following description of the embodiments in conjunction with the accompanying drawings, in which:

[0038] Figure 1 is a schematic perspective view of a display device according to some embodiments;

[0039] Figure 2 is a schematic cross-sectional view of a display device according to some embodiments;

[0040] Figure 3 is a schematic plan view of a display device according to some embodiments;

[0041] Figure 4 is an equivalent circuit diagram of a pixel according to some embodiments;

[0042] Figure 5 is a schematic cross-sectional view of a portion of a display panel according to some embodiments;

[0043] Figure 6 is a schematic cross-sectional view of a portion of a display device according to some embodiments;

[0044] Figure 7 schematically illustrates a state of a protective member before curing according to some embodiments;

[0045] Figure 8 schematically illustrates a state of a protective member after curing according to some embodiments;

[0046] Fig. 9 A flowchart for explaining a method of manufacturing a display device according to some embodiments;

[0047] Fig.10 To illustrate the Fig. 9 A perspective view of operation S100;

[0048] Fig.11 To illustrate the Fig. 9 A perspective view of operation S200;

[0049] Fig.12 According to some embodiments, Fig.11 A cross-sectional view taken along line X1-X1';

[0050] Fig.13 To illustrate the Fig. 9 A perspective view of operation S300;

[0051] Fig.14 According to some embodiments, Fig.13 A cross-sectional view taken along line X2-X2';

[0052] Fig.15 To illustrate the Fig. 9 A perspective view of operation S300;

[0053] Fig.16 According to some embodiments, Fig.15 A cross-sectional view taken along line X3-X3';

[0054] Fig.17 To illustrate the Fig. 9 A perspective view of operation S400;

[0055] Fig.18 According to some embodiments, Fig.17 A cross-sectional view taken along line X4-X4';

[0056] Fig.19 To illustrate the Fig.17 A perspective view of operation S400;

[0057] Fig. 20 A flowchart for explaining a method of manufacturing a display device according to some embodiments;

[0058] Fig.21 To illustrate the Fig. 20 A perspective view of operation S300_2;

[0059] Fig. 22 According to some embodiments, Fig.21 A cross-sectional view taken along line X5-X5';

[0060] Fig.23 To illustrate the Fig. 20 A perspective view of operation S400_2;

[0061] Fig.24 To illustrate the Fig. 20 A perspective view of operation S400_2; and

[0062] Fig.25 According to some embodiments, Fig.24 A cross-sectional view taken along line X6-X6'. DETAILED DESCRIPTION

[0063] Now the aspects of some embodiments of the present invention will be more fully described below with reference to the attached drawings, in which aspects of some embodiments of the present invention are shown. However, the invention can be implemented in different forms and should not be interpreted as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided so that the disclosure will be more thorough and more complete, and the scope of the embodiments according to the present invention will be more fully communicated to those skilled in the art.

[0064] It will also be understood that when a layer is referred to as being “on” another layer or substrate, it can be directly on the other layer or substrate, or intervening layers may also be present. Throughout the specification, the same reference numerals refer to the same components.

[0065] Hereinafter, aspects of some embodiments of the present disclosure will be described in more detail with reference to the accompanying drawings.

[0066] Figure 1 is a schematic perspective view of a display device 1 according to some embodiments.

[0067] refer to Figure 1 , the display device 1 can be applied to portable electronic devices (such as mobile phones, smart phones, tablet personal computers (PCs), mobile communication terminals, electronic notebooks, electronic books, portable multimedia players (PMPs), navigation devices, and ultra-mobile PCs (UMPCs)), as well as various products (such as televisions, notebook computers, displays, billboards, and Internet of Things (IoT) devices). In addition, the display device 1 can be applied to wearable devices (such as smart watches, watch phones, glasses-type displays, and head-mounted displays (HMDs)). In addition, the display device 1 can be applied to a dashboard of a vehicle, a center information display (CID) located on a center instrument panel or dashboard of the vehicle, an interior mirror display that replaces a side mirror of the vehicle, or a display located on the back of a front seat as entertainment for rear seat passengers of the vehicle. Although an embodiment in which the display device 1 is a smart phone is illustrated in the accompanying drawings as an example, the present disclosure is not limited thereto.

[0068] The display device 1 may include a display area DA and a non-display area NDA located outside the display area DA (e.g., located at the periphery of the display area DA or located outside the occupied space of the display area DA). The display area DA may display an image through the pixels PX located in the display area DA. Figure 1A single pixel PX is explained, but as will be understood by those skilled in the art, the display area DA may include any appropriate number of pixels PX depending on the design and size of the display device 1. The non-display area NDA may be an area that is located outside the display area DA and does not display an image. The non-display area NDA may completely surround the display area DA. A driver for providing an electrical signal or power to the display area DA may be located in the non-display area NDA. A pad (which is an area to which an electronic device or a printed circuit board can be electrically connected) may be located in the non-display area NDA.

[0069] exist Figure 1 , a case where the display area DA is a polygon (e.g., a rectangle) whose length along the second direction DR2 is less than the length along the first direction DR1 is explained as an example. However, in another example, the display area DA may be a polygon (e.g., a quadrilateral) whose length along the first direction DR1 is less than or equal to the length along the second direction DR2.

[0070] In the drawings, the first direction DR1 and the second direction DR2 are horizontal directions that intersect each other. For example, the first direction DR1 and the second direction DR2 may be orthogonal to each other. In addition, the third direction DR3 may be a vertical direction that intersects (e.g., is orthogonal to) the first direction DR1 and the second direction DR2. In this specification, the direction indicated by the arrows of each of the first direction DR1 to the third direction DR3 may be referred to as one side, and the opposite direction may be referred to as the other side.

[0071] Although the case where the display area DA has a substantially rectangular shape is explained as an example, the present disclosure is not limited thereto. In another example, the display area DA may have various shapes such as an N-gon (where N is a natural number of 3 or more), a circle, and an ellipse, and according to some embodiments, the corners or vertices of the N-gon may be rounded.

[0072] Although each corner of the display area DA is explained as including a vertex where straight lines intersect, the present disclosure is not limited thereto. In another example, the display area DA may be a polygon with rounded corners.

[0073] Figure 2 is a schematic cross-sectional view of a display device 1 according to some embodiments.

[0074] refer to Figure 2 , the display device 1 may include a display panel 10 and a cover window 50 .

[0075] The display panel 10 may be a light-emitting display panel including a light-emitting element as a display element. For example, the display panel 10 may be an organic light-emitting display panel using an organic light-emitting diode including an organic light-emitting layer, a micro light-emitting diode display panel using a micro light-emitting diode, a quantum dot light-emitting display panel using a quantum dot light-emitting diode including a quantum dot light-emitting layer, or an inorganic light-emitting display panel using an inorganic light-emitting element including an inorganic semiconductor.

[0076] The display panel 10 may be a rigid display panel that is hard and not easily bent, or a flexible display panel that is flexible and can be relatively easily bent, folded, or rolled without damaging the display panel 10. For example, the display panel 10 may be a foldable display panel that can be folded or unfolded, a curved display panel whose display surface is curved, a curved display panel whose area other than the display surface is curved, a rollable display panel that can be rolled or unfolded, or a stretchable display panel that can be stretched.

[0077] The display panel 10 may include a substrate 100 , a display layer 200 , a touch screen layer TSL, an optical function layer OFL, and a protective member 300 .

[0078] The substrate 100 may be made of an insulating material such as glass, quartz, or polymer resin.

[0079] According to some embodiments, the substrate 100 may be a rigid substrate. For example, the substrate 100 may include at least one of glass and quartz.

[0080] According to some embodiments, the substrate 100 may be a flexible substrate that can be bent, folded, or rolled. For example, the substrate 100 may include a polymer resin (such as polyethersulfone, polyacrylate, polyetherimide, polyethylene naphthalate, polyethylene terephthalate, polyphenylene sulfide, polyarylate, polyimide, polycarbonate, or cellulose acetate propionate).

[0081] According to some embodiments, the substrate 100 may have a multi-layer structure including a layer including the above polymer resin and an inorganic layer. For example, the substrate 100 may include two layers including the above polymer resin and an inorganic isolation layer interposed between the two layers.

[0082] The display layer 200 may be located on the substrate 100. The display layer 200 may be a layer including pixels and configured to display an image. The display layer 200 may include a circuit layer including a thin film transistor, a display element layer in which a display element is located, and a sealing member for sealing the display element layer.

[0083] The display layer 200 may be divided into a display area DA and a non-display area NDA. The display area DA may be an area in which pixels are arranged to display an image. The non-display area NDA may be an area located outside the display area DA (e.g., located at the periphery of the display area DA or located outside the occupied space of the display area DA) and where no image is displayed. The non-display area NDA may surround the display area DA. The non-display area NDA may be an area extending from the outside of the display area DA to the edge of the display panel 10. In the display area DA, not only pixels may be arranged, but also pixel circuits for driving pixels, scan lines connected to the pixel circuits, data lines, power lines, and the like may be arranged. In the non-display area NDA, a scan driver for transmitting a scan signal to a scan line and a fan-out line connecting the data line and the display driver, and the like may be arranged.

[0084] According to design, various functional layers may be located on the display layer 200. According to some embodiments, a touch screen layer TSL may be located on the display layer 200. The touch screen layer TSL may include a touch electrode, and may be a layer for detecting a user's touch.

[0085] According to some embodiments, the touch screen layer TSL may be directly formed on the encapsulation member ENCM (see FIG. Figure 6 For example, the display panel 10 may have an embedded touch structure, in which the touch screen layer TSL is directly located on the packaging member ENCM (see FIG. Figure 6 )superior.

[0086] According to some embodiments, the touch screen layer TSL may be formed separately and then bonded to the encapsulation member ENCM (see FIG. 1 ) of the display layer 200 through an adhesive layer (such as an optically transparent adhesive layer). Figure 6 ).

[0087] The optical function layer OFL may be located on the touch screen layer TSL. The optical function layer OFL may include an anti-reflection layer. The anti-reflection layer may reduce reflectivity of light (external light) incident from the outside to the display device 1.

[0088] In some embodiments, the anti-reflection layer may be provided as a polarizing film. The polarizing film may include a linear polarizer and a phase retardation film such as a quarter wavelength (λ / 4) plate. The phase retardation film may be located on the touch screen layer TSL, and the linear polarizer may be located on the phase retardation film.

[0089] The cover window 50 may be located on the optical function layer OFL. The cover window 50 may be attached to the optical function layer OFL by a transparent adhesive member such as an optically transparent adhesive film.

[0090] The cover window 50 may be located on the display panel 10 to cover the upper surface of the display panel 10. Therefore, the cover window 50 may play a role in protecting the upper surface of the display panel 10.

[0091] According to some embodiments, the cover window 50 may be a flexible window. The cover window 50 may protect the display panel 10 while being easily bent in response to an external force without cracks, etc. The cover window 50 may include glass, sapphire, or plastic. For example, the cover window 50 may be ultra-thin glass (UTG) or colorless polyimide (CPI). According to some embodiments, the cover window 50 may have a structure in which a flexible polymer layer is located on the surface of a glass substrate or may consist of only a polymer layer.

[0092] The protective member 300 may be located below the substrate 100. The protective member 300 may play a role in protecting the display panel 10. For example, the protective member 300 may protect the display panel 10 from the impact transmitted from below the display panel 10, and may prevent the components located on the protective member 300 from being deformed. In addition, the protective member 300 may include a material with excellent thermal conductivity to perform a heat dissipation function. The protective member 300 may also include a conductive material to absorb electromagnetic waves and prevent electrical interference. In addition, the protective member 300 may include a light blocking material to block light from outside the display device 1 and reduce the reflectivity of light transmitted from above. Accordingly, the protective member 300 can relatively improve the reliability of the display panel 10.

[0093] Figure 3 According to some embodiments of the display device 1 (see Figure 1 ) is a schematic plan view of the . Figure 4 is an equivalent circuit diagram of a pixel PX according to some embodiments.

[0094] refer to Figure 3 and Figure 4 The display panel 10 may include a display area DA and a non-display area NDA surrounding at least a portion of the display area DA. The display panel 10 may include a plurality of pixels PX located in the display area DA. Each pixel PX may include a pixel circuit PC and a light emitting element DPE connected to the pixel circuit PC.

[0095] The pixel circuit PC may include a first transistor T1, a second transistor T2 and a storage capacitor Cst. Each pixel PX may emit, for example, red light, green light or blue light, or red light, green light, blue light or white light through a light emitting element DPE. The first transistor T1 and the second transistor T2 may be implemented as thin film transistors.

[0096] The first transistor T1 is a driving transistor and is connected to the driving voltage line PL and the storage capacitor Cst. The first transistor T1 can control the driving current flowing from the driving voltage line PL to the light emitting element DPE according to the value of the voltage stored in the storage capacitor Cst. The light emitting element DPE can emit light with brightness (e.g., set or predetermined brightness) in response to the driving current. The counter electrode (e.g., cathode) of the light emitting element DPE can receive the second power supply voltage ELVSS.

[0097] The second transistor T2 is a switching transistor and is connected to the scan line SL and the data line DL. The second transistor T2 may transfer a data voltage received from the data line DL to the first transistor T1 according to a switching voltage received from the scan line SL. The storage capacitor Cst may be connected to the second transistor T2 and the driving voltage line PL, and may store a voltage corresponding to a difference between a voltage received from the second transistor T2 and a first power supply voltage ELVDD supplied to the driving voltage line PL.

[0098] Despite Figure 4 The pixel circuit PC includes two transistors and one storage capacitor, but the embodiments of the present disclosure are not limited thereto. That is, the number of thin film transistors and the number of capacitors included in the pixel circuit PC may be variously changed according to the design of the pixel circuit PC. For example, in addition to the two thin film transistors above, the pixel circuit PC may further include four, five or more thin film transistors. In addition, in addition to the storage capacitor Cst above, one or more capacitors may be further included.

[0099] In addition, although the case in which the first transistor T1 and the second transistor T2 are PMOS transistors is explained in the drawings as an example, all or some of the transistors may be NMOS transistors.

[0100] In the non-display area NDA, a first scan driver 1100 and a second scan driver 1200 for supplying scan signals to the pixels PX, a data driver 1300 for supplying data signals to the pixels PX, and a main power line for supplying a first power supply voltage and a second power supply voltage may be provided. The first scan driver 1100 and the second scan driver 1200 may be located in the non-display area NDA and may be located at both sides of the display area DA with the display area DA interposed therebetween, but the present disclosure is not limited thereto.

[0101] exist Figure 3 In the embodiment, the data driver 1300 is disposed adjacent to the lower side of the substrate 100. However, according to some embodiments, the data driver 1300 may be located on a flexible printed circuit board (FPCB) electrically connected to a pad located at one side of the display panel 10.

[0102] Figure 5 is a schematic cross-sectional view of a portion of a display panel according to some embodiments.

[0103] refer to Figure 5 , the pixel circuit PC may be located on the substrate 100 , and the light emitting element DPE electrically connected to the pixel circuit PC may be located on the pixel circuit PC.

[0104] The substrate 100 may include at least one of glass, quartz, and polymer resin. The substrate 100 may have a single-layer or multi-layer structure.

[0105] The buffer layer 201 may be located on the substrate 100. The buffer layer 201 may reduce or block the penetration of foreign matter, moisture or external air from below the substrate 100 and improve the smoothness of the upper surface of the substrate 100. The buffer layer 201 may include an inorganic material (such as an oxide or a nitride), an organic material, or an organic / inorganic composite material, and may have a single-layer or multi-layer structure of an inorganic material and an organic material. An isolation layer (not shown) may be further included between the substrate 100 and the buffer layer 201 to block the penetration of external air.

[0106] The pixel circuit PC may be located on the buffer layer 201. The pixel circuit PC may include a thin film transistor TFT and a storage capacitor Cst. The thin film transistor TFT may include a semiconductor layer Act, a gate electrode GE, a source electrode SE, and a drain electrode DE. The current embodiment shows a top gate structure in which the gate electrode GE is located on the semiconductor layer Act with the gate insulating layer 203 interposed therebetween. However, in some embodiments, the thin film transistor TFT may have a bottom gate structure.

[0107] The semiconductor layer Act may be located on the buffer layer 201. The semiconductor layer Act may include a channel region and a source region and a drain region located on both sides of the channel region and doped with impurities. Here, the impurities may include N-type impurities or P-type impurities. The semiconductor layer Act may include amorphous silicon or polycrystalline silicon. As a specific example, the semiconductor layer Act may include an oxide of at least one material selected from indium (In), gallium (Ga), tin (Sn), zirconium (Zr), vanadium (V), hafnium (Hf), cadmium (Cd), germanium (Ge), chromium (Cr), titanium (Ti), aluminum (Al), cesium (Cs), cerium (Ce) and zinc (Zn). In addition, the semiconductor layer Act may include a Zn oxide material (such as Zn oxide, In-Zn oxide or Ga-In-Zn oxide). In addition, the semiconductor layer Act may include IGZO (In-Ga-Zn-O), ITZO (In-Sn-Zn-O), or IGTZO (In-Ga-Sn-Zn-O) semiconductor containing a metal such as indium (In), gallium (Ga), or tin (Sn) in ZnO.

[0108] The gate electrode GE may be located on the semiconductor layer Act to overlap at least a portion of the semiconductor layer Act. For example, the gate electrode GE may overlap the channel region of the semiconductor layer Act. The gate electrode GE may include various conductive materials including molybdenum (Mo), aluminum (Al), copper (Cu) and / or titanium (Ti), and may have various layer structures. For example, the gate electrode GE may include a Mo layer and an Al layer, or may have a multilayer structure of Mo / Al / Mo. In addition, in some embodiments, the gate electrode GE may have a multilayer structure including an ITO layer covering a metal material.

[0109] The gate insulating layer 203 between the semiconductor layer Act and the gate electrode GE may include an inorganic insulating material such as silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, titanium oxide, tantalum oxide, or hafnium oxide. The gate insulating layer 203 may be a single layer or multiple layers including the above materials.

[0110] The source electrode SE and the drain electrode DE may also include various conductive materials including molybdenum (Mo), aluminum (Al), copper (Cu) and / or titanium (Ti), and may have various layer structures. For example, the source electrode SE and the drain electrode DE may include a Ti layer and an Al layer, or may have a multilayer structure of Ti / Al / Ti. The source electrode SE and the drain electrode DE may be connected to the source region and the drain region of the semiconductor layer Act through a contact hole. In addition, in some embodiments, the source electrode SE and the drain electrode DE may have a multilayer structure including an ITO layer covering a metal material.

[0111] The storage capacitor Cst may include a lower electrode CE1 and an upper electrode CE2 overlapping each other with the first interlayer insulating layer 205 interposed therebetween. The storage capacitor Cst may overlap with the thin film transistor TFT. The lower electrode CE1 and the upper electrode CE2 overlap each other (with the first interlayer insulating layer 205 interposed therebetween) and form a capacitor. In this case, the first interlayer insulating layer 205 serves as a dielectric layer of the storage capacitor Cst. Figure 5 , the gate electrode GE of the thin film transistor TFT is illustrated as the lower electrode CE1 of the storage capacitor Cst. According to some embodiments, the storage capacitor Cst may not overlap with the thin film transistor TFT. The storage capacitor Cst may be covered with the second interlayer insulating layer 207.

[0112] Each of the first interlayer insulating layer 205 and the second interlayer insulating layer 207 may include an inorganic insulating material such as silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, titanium oxide, tantalum oxide, or hafnium oxide. Each of the first interlayer insulating layer 205 and the second interlayer insulating layer 207 may be a single layer or multiple layers including the above materials.

[0113] The insulating layers 203 , 205 , 207 , etc. including the inorganic insulating material described above may be formed by, but not limited to, chemical vapor deposition (CVD) or atomic layer deposition (ALD).

[0114] The pixel circuit PC including the thin film transistor TFT and the storage capacitor Cst may be covered with an organic insulating layer 209. For example, the organic insulating layer 209 may cover the source electrode SE and the drain electrode DE. The organic insulating layer 209 may be located on the substrate 100 above the display area DA and the non-display area NDA outside the display area DA. The organic insulating layer 209 is a planarized insulating layer and may include a substantially flat upper surface. The organic insulating layer 209 may include an organic insulating material, such as a general polymer (such as polymethyl methacrylate (PMMA) or polystyrene (PS)), a polymer derivative having a phenolic group, an acrylic polymer, an imide polymer, an aryl ether polymer, an amide polymer, a fluorine polymer, a paraxylene polymer, a vinyl alcohol polymer, or a blend thereof. According to some embodiments, the organic insulating layer 209 may include polyimide.

[0115] The pixel electrode 221 may be formed on the organic insulating layer 209. The pixel electrode 221 may include a conductive oxide such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium oxide (In 2 O 3 ), indium gallium oxide (IGO), or aluminum zinc oxide (AZO). According to some embodiments, the pixel electrode 221 may include a reflective layer including silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), or a compound thereof. According to some embodiments, the pixel electrode 221 may further include a reflective layer including ITO, IZO, ZnO, or In 2 O 3 A layer made and located above / below the reflective layer.

[0116] The bank layer 215 may be formed on the pixel electrode 221. The bank layer 215 may include an opening exposing the upper surface of the pixel electrode 221 and may cover the edge of the pixel electrode 221. The bank layer 215 may include an organic insulating material. Alternatively, the bank layer 215 may include an inorganic insulating material (such as silicon nitride, silicon oxynitride, or silicon oxide). Alternatively, the bank layer 215 may include an organic insulating material and an inorganic insulating material.

[0117] The intermediate layer 222 may include a light emitting layer 222b. For example, the light emitting layer 222b may include an organic material. The light emitting layer 222b may include a polymer or a low molecular weight organic material that emits light having a color (e.g., a set or predetermined color). The intermediate layer 222 may include a first functional layer 222a located below the light emitting layer 222b and / or a second functional layer 222c located on the light emitting layer 222b.

[0118] The first functional layer 222a may be a single layer or a multilayer. For example, when the first functional layer 222a is made of a polymer material, it may be a hole transport layer (HTL) having a single layer structure, and may be made of poly-(3,4-ethylene-dioxythiophene) (PEDOT) or polyaniline (PANI). When the first functional layer 222a is made of a low molecular weight material, it may include a hole injection layer (HIL) and / or HTL.

[0119] The second functional layer 222c may be optional. For example, when the first functional layer 222a and the light emitting layer 222b are made of a polymer material, the second functional layer 222c may be formed. The second functional layer 222c may be a single layer or a multilayer. The second functional layer 222c may include an electron transport layer (ETL) and / or an electron injection layer (EIL).

[0120] The light emitting layer 222b of the intermediate layer 222 may be individually located in each pixel in the display area DA. The light emitting layer 222b may overlap with the opening of the bank layer 215 and / or the pixel electrode 221. Each of the first and second functional layers 222a and 222c of the intermediate layer 222 may be formed as a single body.

[0121] The counter electrode 223 may be made of a conductive material having a low work function. For example, the counter electrode 223 may include a (semi) transparent layer containing silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), lithium (Li), calcium (Ca) or an alloy thereof. Alternatively, the counter electrode 223 may further include, for example, ITO, IZO, ZnO or In on the (semi) transparent layer including the above materials. 2 O 3 The counter electrode 223 may be a single body and may be formed to cover the plurality of pixel electrodes 221 in the display area DA. The intermediate layer 222 and the counter electrode 223 may be formed by thermal evaporation.

[0122] The spacer 217 may be located on the bank layer 215. The spacer 217 may prevent damage to a light emitting diode or the like by ensuring a space (eg, a set or predetermined space) on a display element.

[0123] The spacer 217 may include an organic insulating material such as polyimide. Alternatively, the spacer 217 may include an inorganic insulating material such as silicon nitride or silicon oxide, or may include an organic insulating material and an inorganic insulating material. In addition, the spacer 217 may include a material different from that of the dam layer 215. Alternatively, the spacer 217 may include the same material as that of the dam layer 215. In this case, the dam layer 215 and the spacer 217 may be formed together in a mask process using a half-tone mask or the like.

[0124] The capping layer 230 may be located on the counter electrode 223. The capping layer 230 may include an inorganic material (eg, LiF) and / or an organic material. In some embodiments, the capping layer 230 may be omitted.

[0125] Figure 6 is a schematic cross-sectional view of a portion of a display device 1 according to some embodiments. Figure 7 The state of the protection member 300 before curing according to some embodiments is schematically illustrated. Figure 8 The state of the protection member 300 after curing according to some embodiments is schematically illustrated.

[0126] refer to Figures 6 to 8 , the cover window 50 may be located on the display panel 10. The cover window 50 may be located on the display panel 10 to completely cover the display panel 10.

[0127] The display panel 10 may include a substrate 100 , a display layer 200 on an upper surface of the substrate 100 , a functional layer (eg, a touch screen layer TSL and an optical functional layer OFL) on an upper surface of the display layer 200 , and a protection member 300 under the substrate 100 .

[0128] The insulating layer IL may be located between the substrate 100 and the display layer 200 and within the display layer 200. For example, as described above with reference to Figure 5 As described above, the display layer 200 may include a buffer layer 201 , a gate insulating layer 203 , a first interlayer insulating layer 205 , a second interlayer insulating layer 207 , and an organic insulating layer 209 as the insulating layer IL.

[0129] According to some embodiments, the display layer 200 of the display panel 10 may further include an encapsulation member ENCM. The encapsulation member ENCM may be an encapsulation layer for protecting the light emitting element DPE of the display layer 200 from moisture or oxygen from the outside. The encapsulation layer may include at least one organic encapsulation layer and at least one inorganic encapsulation layer. For example, the encapsulation layer may include a first inorganic encapsulation layer, an organic encapsulation layer, and a second inorganic encapsulation layer.

[0130] When the light emitting element DPE is an organic light emitting diode, the first inorganic encapsulation layer may cover the counter electrode 223 (see Figure 5) and may include silicon oxide, silicon nitride and / or silicon oxynitride. For example, the capping layer 230 (see Figure 5 ) may also be between the first inorganic encapsulation layer and the counter electrode 223 (see Figure 5 ). Because the first inorganic encapsulation layer is formed along the structure below it, its upper surface may not be flat or planar. Therefore, an organic encapsulation layer may be formed to cover the first inorganic encapsulation layer so that the upper surface of the first inorganic encapsulation layer may be flat or planar. The organic encapsulation layer may include one or more materials selected from the following: polyethylene terephthalate, polyethylene naphthalate, polycarbonate, polyimide, polyethylene sulfonate, polyoxymethylene, polyarylate and hexamethyldisiloxane. The second inorganic encapsulation layer may cover the organic encapsulation layer and may include silicon oxide, silicon nitride and / or silicon oxynitride, etc.

[0131] The protective member 300 may be located under the substrate 100. The protective member 300 may include a binder 310, a first filler 320-1, a second filler 320-2, a light blocking material 330, and a foaming agent 340 or a foaming agent 340'. The protective member 300 may have a thickness of 100 to 300 μm after curing.

[0132] The first filler 320-1 may have heat dissipation properties. Accordingly, the first filler 320-1 may include a material having excellent thermal conductivity. The first filler 320-1 may include at least one of a carbon-based material and a ceramic-based material. For example, when the first filler 320-1 includes a carbon-based material, they may include at least one of graphite, carbon nanotubes (CNTs), and carbon fibers. When the first filler 320-1 includes a ceramic-based material, they may include boron nitride (BN), aluminum nitride (AlN), beryllium oxide (BeO), silicon carbide (SiC), and aluminum oxide (AlO). 2 O 3 , aluminum oxide).

[0133] The first filler 320-1 may be a plate-shaped filler or a linear filler. Here, the first filler 320-1 may have a particle size of 5 μm to 200 μm. Accordingly, some of the first fillers 320-1 may contact each other to form a heat dissipation path T. For example, when the first filler 320-1 is a plate-shaped filler, some of the first fillers 320-1 may contact each other on the surface to form a heat dissipation path T. When the first filler 320-1 is a linear filler, some of the first fillers 320-1 may contact each other in line to form a heat dissipation path T. When the first filler 320-1 is a plate-shaped filler or a linear filler, they contact each other on the surface or in line to increase the contact area between them. Therefore, the heat dissipation path T can be easily formed.

[0134] The first filler 320-1 may be included in an amount of 50 to 80 weight % based on the total weight of the protection member 300. Here, the first filler 320-1 may be made of a mixture of a carbon-based material and a ceramic-based material, and may occupy 50 to 80 weight % of the protection member 300. However, the present disclosure is not limited thereto, and the first filler 320-1 may also be made of only a carbon-based material or only a ceramic-based material.

[0135] Since the first filler 320 - 1 occupies greater than or equal to half of the total weight of the protection member 300 , 50 wt % to 80 wt %, the first fillers 320 - 1 located adjacent to each other may contact each other and easily form a heat dissipation path T. Accordingly, the protection member 300 including the first filler 320 - 1 may effectively dissipate heat generated from the display panel 10 .

[0136] The second filler 320-2 may have electromagnetic wave shielding properties. Accordingly, the second filler 320-2 may include a material having excellent electrical conductivity. The second filler 320-2 may include at least one of a carbon-based material and a metal-based material. For example, when the second filler 320-2 includes a carbon-based material, they may include at least one of carbon fiber and carbon nanotube (CNT). When the second filler 320-2 includes a metal-based material, they may include at least one of silver-copper (Ag-Cu) alloy powder, nickel-copper (Ni-Cu) alloy powder, silver (Ag) nanowire, and silver-nickel (Ag-Ni) alloy powder.

[0137] When the first filler 320-1 includes a carbon-based material, they may also block electromagnetic waves to a certain extent. However, the second filler 320-2 may be added to further increase the electromagnetic wave shielding rate. Here, the second filler 320-2 may be included in an amount of 1 wt % to 10 wt % based on the total weight of the protective member 300. According to some embodiments, the electromagnetic wave shielding rate of the protective member 300 including the first filler 320-1 and the second filler 320-2 may be 40 dB to 90 dB, preferably 60 dB to 80 dB.

[0138] Thus, the content of the first filler 320-1 and the second filler 320-2 in the protective member 300 may be 51 wt % to 90 wt % based on the total weight of the protective member 300. More preferably, the first filler 320-1 and the second filler 320-2 may occupy 85 wt % or less based on the total weight of the protective member 300. Since the first filler 320-1 and the second filler 320-2 are included at 85 wt % or less, the adhesive 310 for fixing the first filler 320-1 and the second filler 320-2 may be sufficiently included. Therefore, the adhesiveness of the protective member 300 may be improved. Accordingly, the protective member 300 may be applied and bonded to the substrate 100 without a separate adhesive layer.

[0139] The adhesive 310 may fix the first filler 320-1 and the second filler 320-2. The adhesive 310 may include at least one of an acrylic resin, a urethane resin, a silicone resin, and a rubber resin. For example, the adhesive 310 may be made of acrylate, urethane, urethane acrylate, silicone, rubber, or a combination thereof. However, the present disclosure is not limited thereto, and any material having sufficient adhesive strength to fix the first filler 320-1 and the second filler 320-2 may be used.

[0140] The adhesive 310 can not only fix the first filler 320-1 and the second filler 320-2, but also absorb the impact applied to the display device 1. That is, due to the modulus characteristics of the adhesive 310 itself, the protection member 300 can protect the display panel 10 from the impact transmitted from below the protection member 300. However, the impact resistance of the protection member 300 can be improved not only by the elasticity of the adhesive 310 itself, but also by the content of the filler and the content of the foaming agent 340 to be described in more detail later. According to some embodiments, based on when a 2.0g steel ball falls from a height of 10cm, the amount of impact received by the pressure-sensitive paper located below the protection member 300 may be 10MPa to 40MPa.

[0141] In addition, the protective member 300 may further include a solvent that can dissolve the binder 310. The solvent volatilizes during the thermal curing process of the protective member 300, but a portion of the solvent may remain in the protective member 300. The solvent included in the protective member 300 may have a boiling point of 100°C to 200°C. This is because, when the boiling point of the solvent is less than 100°C, the solvent may volatilize during the process of forming the protective member 300 performed before the thermal curing process. In addition, since the solvent must be compatible with the binder 310 including at least one of acrylic resin, urethane resin, silicone resin and rubber resin, the solvent may include at least one of alcohol, ester, ketone and glycol solvents. For example, the solvent may include an alcohol solvent such as isobutyl alcohol, butanol or 2-(2-ethoxyethoxy)ethanol. The solvent may include an ester solvent such as butyl acetate or isobutyl acetate. The solvent may include a ketone solvent such as methyl isobutyl ketone. The solvent may include a glycol-based solvent such as propylene glycol methyl ether (PGME) or ethylene glycol monopropyl ether (EGPE).

[0142] Next, the light blocking material 330 may block light incident from below the display panel 10 and may reduce the reflectivity of light transmitted from above. For example, the light blocking material 330 may include at least one of carbon black, black pigment, and black dye. When the first filler 320-1 and the second filler 320-2 include a carbon-based material, they may also block light to a certain extent. However, the light blocking material 330 may be further included to further reduce the transmittance of light incident from below the display panel 10. According to some embodiments, the light blocking material 330 may be included in an amount of 1 wt % to 5 wt % based on the total weight of the protective member 300.

[0143] Next, the foaming agent 340 or the foaming agent 340 ′ may be a material whose volume increases when the protection member 300 is cured by heat or ultraviolet light. Figure 7 Shown in Figure 8 Before the volume of the foaming agent 340 increases, that is, before the protective member 300 is cured, and Figure 8 Shown in Figure 7 After the volume of the foaming agent 340' is increased, that is, the state after the protective member 300 is cured. Each of the foaming agent 340 and the foaming agent 340' may have a structure including a core part and a skin surrounding the core part. When heat or ultraviolet light is provided, the foaming material included in the core part may be vaporized, thereby increasing the volume of the foaming agent 340'. In each foaming agent 340 after foaming, the volume of the core part may be increased, and the skin may be thinner than the skin in each foaming agent 340' before foaming.

[0144] According to some embodiments, the foaming agent 340 or the foaming agent 340' may be a thermally expandable microcapsule. That is, when the foaming agent 340' is heated, the outer skin may soften while the foaming material is vaporized. Therefore, the volume of the foaming agent 340' may expand. The foaming agent 340 or the foaming agent 340' may be a low-temperature foaming agent and may start foaming at a temperature of about 70°C. Because the foaming agent 340 or the foaming agent 340' may foam at a low temperature, the foaming process may be performed without damaging the light-emitting element DPE included in the display panel 10.

[0145] The foaming process of the foaming agent 340' may be performed together with the curing process of the protection member 300. However, the embodiment according to the present disclosure is not limited thereto, and the foaming process of the foaming agent 340' and the curing process of the protection member 300 may also be performed as separate processes.

[0146] The foaming agent 340' may be included in an amount of 1 wt % to 10 wt % based on the total weight of the protection member 300. By adjusting the content of the foaming agent 340', the protection member 300 may have elasticity (eg, set or predetermined elasticity) and impact resistance.

[0147] The foaming agent 340 or the foaming agent 340' may be dispersed in the protective member 300 and may have the same size. According to some embodiments, the particle size of the foaming agent 340' after foaming may be 10 μm to 100 μm. However, the embodiments according to the present disclosure are not limited thereto, and the foaming agent 340 or the foaming agent 340' may also have different sizes. In addition, although in Figure 7 and Figure 8 The middle foaming agent 340 or the foaming agent 340 ′ has a spherical shape, but the present disclosure is not limited thereto, and the foaming agent 340 or the foaming agent 340 ′ may also have an elliptical shape.

[0148] As the volume of the foaming agent 340' increases, the area in which the first filler 320-1 included in the protection member 300 can be dispersed can be reduced. That is, when the volume of the foaming agent 340' increases, the first fillers 320-1 can be located closer to each other, and some of the first fillers 320-1 can contact each other to form the heat dissipation path T. Finally, the protection member 300 including the foaming agent 340 or the foaming agent 340' can more easily form the heat dissipation path T of the first filler 320-1 having heat dissipation characteristics. Therefore, the protection member 300 can effectively dissipate the heat generated from the display panel 10. Accordingly, the thermal conductivity of the protection member 300 including the foaming agent 340 or the foaming agent 340' and the first filler 320-1 can be 10W / mK to 50W / mK.

[0149] The protective member 300 may be formed to have high viscosity. For example, the protective member 300 may have a viscosity of 10000 cPs to 50000 cPs. According to some embodiments, the viscosity of the protective member 300 may be 20000 cPs to 40000 cPs.

[0150] As described above, the protective member 300 can perform a variety of functions to protect the display panel 10. For example, the protective member 300 can protect the display panel 10 from the impact transmitted from the bottom of the display device 1, perform a heat dissipation function, and block electromagnetic waves and light. In conventional technology, a protective member that performs the above protective functions is formed by manufacturing a plurality of functional layers having impact resistance, heat dissipation, electromagnetic wave blocking and light blocking functions, forming a composite sheet by a lamination process, and then attaching the composite sheet to the display panel by a lamination process. Therefore, the unit cost of the alternative protective member may be relatively high due to the manufacture and lamination process of the functional layer, and the risk of defects may be relatively high. However, when the protective member 300 is directly applied to the lower surface of the substrate 100, it can perform a variety of functions to protect the display panel 10, while the cost can be relatively reduced due to the simplification of the structure and materials, and the risk of defects is greatly reduced due to the simplification of the process.

[0151] A method of manufacturing a display device according to some embodiments will now be described.

[0152] Fig. 9 A flowchart is provided to explain a method of manufacturing a display device according to some embodiments. Fig.10 To explain Fig. 9 FIG. 1 is a perspective view of operation S100 . Fig.11 To explain Fig. 9 FIG. 1 is a perspective view of operation S200 . Fig.12 For along Fig.11 A cross-sectional view taken along line X1-X1'. Fig.13 To explain Fig. 9 FIG. 1 is a perspective view of operation S300 . Fig.14 For along Fig.13 A cross-sectional view taken along line X2-X2'. Fig.15 To explain Fig. 9 FIG. 1 is a perspective view of operation S300 . Fig.16 For along Fig.15 A cross-sectional view taken along line X3-X3'. Fig.17 To explain Fig. 9 FIG. 1 is a perspective view of operation S400 . Fig.18 For along Fig.17 A cross-sectional view taken along line X4-X4'. Fig.19 To explain Fig.17 FIG. 1 is a perspective view of operation S400 .

[0153] refer to Figures 9 to 19 According to an embodiment, a method S1 of manufacturing a display device may include: forming a display layer on one surface of a mother substrate (operation S100), forming a frame including an opening by applying a first resin to the other surface of the mother substrate and curing the first resin (operation S200), forming a protective member by applying a second resin to the opening of the frame and curing the second resin (operation S300), and cutting the mother substrate after removing the frame (operation S400).

[0154] First, if Fig.10 As explained in the above, in forming the display layer on one surface of the mother substrate (operation S100), the display layer 200 may be formed on a surface (eg, upper surface US) of the mother substrate MSUB. Fig.10 As explained in FIG. 1 , to form the display layer 200 , the mother substrate MSUB may be placed such that a third direction DR3 in which the upper surface US faces is upward in the drawing, and an opposite direction in which the lower surface DS faces is downward in the drawing.

[0155] The mother substrate MSUB can be made of the same substrate 100 (see Figure 2) is made of the same material as the material of the mother substrate MSUB. For example, the mother substrate MSUB may include at least one of glass, quartz, and a polymer resin. Since the display layer 200 has been described above, some repeated descriptions thereof may be omitted. The horizontal length and vertical length of the mother substrate MSUB may be about several meters. For example, the mother substrate MSUB may have a horizontal length of about 2.5m and a vertical length of about 2m, but embodiments according to the present disclosure are not limited thereto.

[0156] The display layers 200 may be located on the upper surface US of the mother substrate MSUB at regular intervals along the first direction DR1 and the second direction DR2. For example, the display layers 200 may be arranged along a matrix direction to respectively form display units.

[0157] Next, if Fig.11 and Fig.12 As explained in the figure, in forming a frame including openings by applying a first resin to another surface of the mother substrate and curing the first resin (operation S200), in order to perform a process of applying a protective member 300 under the mother substrate MSUB, the mother substrate MSUB can be placed so that the upper surface US faces downward and the lower surface DS faces upward.

[0158] The mother substrate MSUB may include an applying area APA overlapping the display layer 200 in the third direction DR3 and a cutting area CA surrounding the applying area APA.

[0159] The application area APA may be an area where the second resin RSN2 to be described later is applied, and may be an area overlapping the display layer 200. For example, the application area APA may have an area substantially the same as that of the display layer 200, and may completely overlap the display layer 200. However, the embodiment according to the present disclosure is not limited thereto, and the application area APA may also generally overlap the display layer 200, but may have an area smaller than the display layer 200 or an area larger than the display layer 200. The application area APA may overlap the display unit.

[0160] The cutting area CA may surround the application area APA. The cutting area CA may not generally overlap with the display layer 200. However, the embodiment according to the present disclosure is not limited thereto, and the cutting area CA may also partially overlap with the display layer 200. The cutting area CA may be an area through which a cutting line of a cutting member passes in a cutting process to be described later. The cutting area CA may be located between the application areas APA or surround the application area APA.

[0161] The first resin RSN1 may be applied to the cutting area CA through the first application head HD1. The first resin RSN1 may be applied to the cutting area CA through the first application head HD1 using any one of a printing method, a coating method, and a dispensing method. According to some embodiments, the first application head HD1 may quickly and accurately apply the first resin RSN1 to the cutting area CA using a dispensing method, but embodiments according to the present disclosure are not limited thereto.

[0162] The first resin RSN1 may include at least one of an acrylic resin, a urethane resin, a silicone resin, and a rubber resin. For example, the binder 310 may be made of acrylate, urethane, urethane acrylate, silicone, rubber, or a combination thereof. According to some embodiments, the first resin RSN1 may include a binder 310 (see FIG. 1 ) with a second resin RSN2 to be described later. Figure 7 ) of the same material.

[0163] The thickness of the first resin RSN1 after curing may be greater than or equal to the thickness of the second resin RSN2 before curing. That is, the thickness of the frame FRM may be greater than or equal to the thickness of the second resin RSN2 before curing. For example, the thickness of the first resin RSN1 after curing may be 200 μm to 600 μm.

[0164] The first resin RSN1 may have substantially the same thickness before and after curing. For example, the thickness of the first resin RSN1 before and after curing may be about 200 μm to 600 μm. According to some embodiments, the thickness of the first resin RSN1 before and after curing may be about 400 μm. Unlike the second resin RSN2 to be described later, the first resin RSN1 may have substantially the same thickness before and after curing because it hardly includes a high-volatile solvent. However, embodiments according to the present disclosure are not limited thereto, and if the first resin RSN1 includes a high-volatile solvent, the first resin RSN1 may also have different thicknesses before and after curing.

[0165] The first resin RSN1 may be cured by a curing process to form the frame FRM. The first resin RSN1 may be cured by at least one of thermal curing, natural curing, and ultraviolet curing. According to some embodiments, the first resin RSN1 may be cured by at least one of thermal curing and natural curing. When the first resin RSN1 is cured by at least one of thermal curing and natural curing, the elongation of the frame FRM may be improved.

[0166] According to some embodiments, when thermal curing is used, the heat treatment process may be performed at a temperature of 25° C. to 100° C. or less for about one hour. According to some embodiments, the heat treatment process may be performed at a temperature of about 90° C. Since the heat treatment process is performed at a relatively low temperature, the display panel 10 including the display layer 200 may not be damaged.

[0167] The frame FRM may have a relatively high elongation. For example, the elongation of the frame FRM may be 200% or more. When the elongation of the frame FRM is 200% or more, the frame FRM may be easily removed without breakage or residue in a removal process of the frame FRM to be described in more detail later.

[0168] The frame FRM may be located on the cutting area CA. The frame FRM may surround the application area APA. The frame FRM may include an opening OP. The opening OP may overlap the application area APA. The opening OP may overlap the display layer 200. Each of the openings OP may provide a space for applying the second resin RSN2 to be described later.

[0169] The frame FRM may include ribs RIB between the openings OP. The width W1 of the ribs RIB may be about 1 mm to 5 mm.

[0170] Next, if Figures 13 to 16 As explained in the description, in forming a protective member by applying a second resin to an opening of a frame and curing the second resin (operation S300), the second resin RSN2 may be applied to an application area APA by a second application head HD2 and a scraper (or scraper) BLD. The second resin RSN2 may be applied to the application area APA by the second application head HD2 and the scraper BLD using any one of a printing method, a coating method, and a dispensing method. According to some embodiments, the second application head HD2 may discharge the second resin RSN2 in a paste form onto one side of the frame FRM by using a dispensing method. The scraper BLD may move while pushing the second resin RSN2 discharged in a paste form from one side of the frame FRM to the other side of the frame FRM by using a screen printing method. Accordingly, the second resin RSN2 may be applied to the application area APA.

[0171] The outlet of the second application head HD2 may have a diameter greater than that of the first application head HD1. The maximum diameter of particles of the second resin RSN2 discharged from the second application head HD2 may be greater than that of particles of the first resin RSN1 discharged from the first application head HD1.

[0172] As referenced above Figure 7 As described above, the second resin RSN2 may include a binder 310 (see Figure 7 ), the first filler 320-1 (see Figure 7), the second filler 320-2 (see Figure 7 ), light blocking material 330 (see Figure 7 )、Foaming agent 340'(see Figure 7 ) and solvent.

[0173] The thickness TH1 of the second resin RSN2 before being cured may be less than or equal to the thickness of the frame FRM. For example, the thickness TH1 of the second resin RSN2 before being cured may be 200 μm to 600 μm.

[0174] The thickness TH2 of the second resin RSN2 after curing may be less than the thickness TH1 of the first resin RSN1 before curing. For example, the thickness TH2 of the second resin RSN2 after curing may be about 40% to 60% of the thickness TH1 of the first resin RSN1 before curing. The thickness TH2 of the second resin RSN2 after curing may be 100 μm to 300 μm.

[0175] The second resin RSN2 may be cured by a curing process to form the protection member 300. The second resin RSN2 may be cured by at least one of thermal curing, natural curing, and ultraviolet curing. According to some embodiments, the second resin RSN2 may be cured by at least one of thermal curing and natural curing. When the second resin RSN2 is cured by at least one of thermal curing and natural curing, the strength and elasticity of the protection member 300 may be relatively increased.

[0176] According to some embodiments, when thermal curing is used, the heat treatment process may be performed at a temperature of 25° C. to 100° C. or less for about one hour. According to some embodiments, the heat treatment process may be performed at a temperature of about 90° C. Since the heat treatment process is performed at a relatively low temperature, the display panel 10 including the display layer 200 may not be damaged.

[0177] The protection member 300 may be located on the application area APA. The protection member 300 may be surrounded by the frame FRM located on the cutting area CA. The protection member 300 may be located inside the opening OP of the frame FRM.

[0178] The thickness TH2 of each protection member 300 , that is, the thickness TH2 of the second resin RSN2 after curing may be about 100 μm to 300 μm.

[0179] Next, if Fig.17 and Fig.18 As explained in , in cutting the mother substrate after removing the frame (operation S400), the frame FRM may be removed from the mother substrate MSUB. As described above, since the elongation of the frame FRM is high, the frame FRM may be easily removed without residue on the mother substrate MSUB.

[0180] The cutting member CTW may cut the mother substrate MSUB. The cutting member CTW may cut the mother substrate MSUB along a cutting line located in the cutting area CA where the frame FRM has been removed. The cutting member CTW may be a cutting wheel or a laser. The mother substrate MSUB cut by the cutting member CTW may form the substrate 100 of each display unit (see Figure 2 ), and the display layer 200 may be located on the substrate 100 of each display unit (see Figure 2 )superior.

[0181] In the method S1 of manufacturing a display device according to some embodiments, before applying the second resin RSN2, a frame FRM is formed using a first resin RSN1 different from the second resin RSN2. Therefore, the yield of the formation process of the protective member 300 can be improved. For example, when the second resin RSN2 is applied using a mask using a metal material as in the conventional technology, the width W1 of the rib RIB is significantly smaller than the total size of the mask. Therefore, a lifting phenomenon or a phenomenon in which the second resin RSN2 penetrates into the cutting area CA instead of the application area APA may occur. On the other hand, when the second resin RSN2 is applied using the frame FRM including the first resin RSN1, the second resin RSN2 can be prevented from penetrating into the cutting area CA due to the adhesive strength of the first resin RSN1 to the mother substrate MSUB. In addition, because the frame FRM has a high elongation, it can be removed relatively easily. In addition, because the second resin RSN2 does not penetrate into the cutting area CA and does not leave foreign matter, contamination of the cutting member can be prevented during the cutting process.

[0182] In some embodiments, the removal mark RMM may be formed on the side surface of the protective member 300 directly contacting the frame FRM. For example, due to the adhesive strength between the frame FRM and the protective member 300, the removal mark RMM may be formed on the side surface of the protective member 300 when the frame FRM is removed.

[0183] like Fig.19 As explained in the figure, according to some embodiments, the cutting process may be performed in a state where the mother substrate MSUB is placed so that the third direction DR3 in which the upper surface US of the mother substrate MSUB faces is upward in the drawing and the opposite direction in which the lower surface DS of the mother substrate MSUB faces is downward in the drawing. That is, the cutting process may be performed in a direction from the upper surface US where the display layer 200 is located to the lower surface DS where the protection member 300 is located.

[0184] In some embodiments, when the mother substrate MSUB includes two or more substrates, each substrate can be cut separately. For example, when the mother substrate MSUB includes two substrates, Fig.17As explained in FIG. 1 , the substrate located on the lower surface DS side of the mother substrate MSUB may be cut first, and then Fig.19 As explained in , the substrate located on the upper surface US side of the mother substrate MSUB can be cut. The opposite situation is also possible. That is, the substrate located on the upper surface US side of the mother substrate MSUB can be cut first, and then the substrate located on the lower surface DS side of the mother substrate MSUB can be cut.

[0185] A method of manufacturing a display device according to an embodiment will now be described. According to some embodiments, the same elements as those of the above-described embodiments will be indicated by the same reference numerals, and some repeated descriptions may be omitted or briefly given, and differences will be mainly described.

[0186] Fig. 20 A flowchart is provided to explain a method of manufacturing a display device according to some embodiments. Fig.21 To explain Fig. 20 A perspective view of operation S300_2. Fig. 22 For along Fig.21 A cross-sectional view taken along line X5-X5'. Fig.23 To explain Fig. 20 A perspective view of operation S400_2. Fig.24 To explain Fig. 20 A perspective view of operation S400_2. Fig.25 For along Fig.24 A cross-sectional view taken along line X6-X6'.

[0187] exist Fig.23 In the embodiment, the third direction DR3 that the upper surface US of the mother substrate MSUB faces is downward, and the opposite direction that the lower surface DS of the mother substrate MSUB faces is upward. Fig.24 In the embodiment, the third direction DR3 in which the upper surface US of the mother substrate MSUB faces is upward, and the opposite direction in which the lower surface DS of the mother substrate MSUB faces is downward.

[0188] refer to Figure 20 to Figure 24 The method S2 for manufacturing a display device according to the current embodiment is different from the method S2 for manufacturing a display device according to the above reference. Fig. 9 The method S1 of manufacturing a display device according to the embodiment of the present invention is different in that a dummy DUM is included.

[0189] For example, according to the embodiment, the method S2 of manufacturing a display device may include: forming a display layer on one surface of a mother substrate (operation S100), forming a frame including openings and dummy openings by applying a first resin to the other surface of the mother substrate and curing the first resin (operation S200_2), forming a protective member and a dummy by applying a second resin to the openings and the dummy openings of the frame and curing the second resin (operation S300_2), and cutting the mother substrate from one surface to the other surface after removing the frame (operation S400).

[0190] First, if Fig.24 and Fig.25 As explained in the above, in forming the display layer on one surface of the mother substrate (operation S100), the display layer 200 may be formed on a surface (eg, upper surface US) of the mother substrate MSUB.

[0191] The display layers 200 may be located on the upper surface US of the mother substrate MSUB at regular intervals along the first direction DR1 and the second direction DR2. For example, the display layers 200 may be arranged along a matrix direction to form display units, respectively. Fig.25 As explained in , the display layers 200 may be spaced apart from each other with a dummy area DMA (an area in which a dummy object DUM to be described later is located) therebetween.

[0192] Next, if Fig.21 and Fig. 22 As explained in , in forming the frame including the openings and the dummy openings by applying the first resin to the other surface of the mother substrate and curing the first resin (operation S200_2), the mother substrate MSUB may further include a dummy area DMA.

[0193] Each of the dummy areas DMA is an area where the dummy object DUM is located, and may be an area overlapping with the dummy object DUM. The dummy area DMA may be surrounded by the cutting area CA. The dummy area DMA may include a first dummy area located between the application areas APA in the second direction DR2, a second dummy area located between the application areas APA in the first direction DR1, and a third dummy area located between the second dummy areas in the second direction DR2 and / or between the first dummy areas in the first direction DR1.

[0194] The first resin RSN1 may be applied onto the cutting area CA except the application area APA and the dummy area DMA.

[0195] The frame FRM formed by curing the first resin RSN1 may surround the application area APA and the dummy area DMA. The frame FRM may include an opening OP overlapping the application area APA and a dummy opening DOP overlapping the dummy area DMA. The dummy opening DOP may include a first dummy opening DOP1 overlapping the first dummy area, a second dummy opening DOP2 overlapping the second dummy area, and a third dummy opening DOP3 overlapping the third dummy area.

[0196] Next, in forming the protection member and the dummy by applying the second resin to the opening and the dummy opening of the frame and curing the second resin (operation S300_2), the protection member 300 and the dummy DUM may be formed by curing the second resin RSN2. The dummy DUM may be formed to have substantially the same thickness as the protection member 300 and to have the same material as the protection member 300 by the same process.

[0197] The dummy object DUM may be located on the dummy area DMA. The dummy object DUM may be surrounded by the frame FRM located on the cutting area CA. The dummy object DUM may be located in the dummy opening DOP of the frame FRM. The dummy object DUM may include a first dummy object DUM1 located in the first dummy opening DOP1, a second dummy object DUM2 located in the second dummy opening DOP2, and a third dummy object DUM3 located in the third dummy opening DOP3. Each of the first dummy objects DUM1 may be located between the protective members 300 in the second direction DR2, each of the second dummy objects DUM2 may be located between the protective members 300 in the first direction DR1, and each of the third dummy objects DUM3 may be located between the second dummy objects DUM2 in the second direction DR2 or between the first dummy objects DUM1 in the first direction DR1.

[0198] Next, if Figure 23 to Figure 25 As explained in , after removing the frame, the mother substrate is cut from one surface to another surface (operation S400), and the frame FRM can be removed from the mother substrate MSUB. As described above, since the elongation of the frame FRM is high, the frame FRM can be easily removed without residue on the mother substrate MSUB.

[0199] For example, the cutting member CTW may cut the mother substrate MSUB along the cutting area CA between the first dummy DUM1 and the protection member 300, between the second dummy DUM2 and the protection member 300, between the first dummy DUM1 and the third dummy DUM3, and between the second dummy DUM2 and the third dummy DUM3.

[0200] In some embodiments, Fig.24 and Fig.25 As explained in FIG. 1 , the cutting process may be performed from the upper surface US where the display layer 200 is located to the lower surface DS where the protection member 300 is located.

[0201] In the method S2 of manufacturing a display device according to some embodiments, since the dummy DUM is formed between the protective members 300, the mother substrate MSUB can be prevented from being partially bent due to the pressure of the cutting member CTW during the cutting process. Accordingly, internal fracture or chipping defects of the mother substrate MSUB can be prevented.

[0202] Summarizing the detailed description, those skilled in the art will appreciate that many variations and modifications may be made to the disclosed embodiments without departing substantially from the principles of the present invention. Therefore, the embodiments disclosed in the present invention are used in a general and descriptive sense only, and not for a limiting purpose.

Claims

1. A method for manufacturing a display device, the method comprising: include: forming a frame including openings by applying a first resin to a surface of a mother substrate and curing the first resin; forming a protective member by applying a second resin to the opening of the frame and curing the second resin; as well as cutting the mother substrate along the area between the protection members after removing the frame, The second resin includes a material different from a material of the first resin. 2 . The method of manufacturing a display device according to claim 1 , wherein in the forming of the protection member, the protection member is surrounded by the frame and is located in the opening. 3 . The method of manufacturing a display device according to claim 1 , wherein in the forming of the protection member, a thickness of the second resin before being cured in the opening is less than or equal to a thickness of the frame. 4 . The method of manufacturing a display device according to claim 3 , wherein a thickness of the second resin after being cured in the opening is in a range of 40% to 60% of the thickness of the second resin before being cured. 5 . The method of manufacturing a display device according to claim 1 , wherein a thickness of each protection member is in a range of 100 μm to 300 μm. 6 . The method of manufacturing a display device according to claim 1 , wherein the second resin comprises at least one of a binder, a first filler, a second filler, a light blocking material, and a foaming agent.

7. The method for manufacturing a display device according to claim 6, in: The first filler includes at least one of a carbon material and a ceramic material, and The second filler includes at least one of a carbon-based material and a metal-based material. 8 . The method of manufacturing a display device according to claim 6 , wherein the light blocking material comprises at least one of carbon black, a black pigment, and a black dye. 9 . The method of manufacturing a display device according to claim 6 , wherein the adhesive comprises at least one of acrylic resin, urethane resin, silicone resin, and rubber resin. 10 . The method of manufacturing a display device according to claim 1 , wherein an elongation rate of the frame is 200% or more. 11 . The method of manufacturing a display device according to claim 1 , wherein in the forming of the frame, the first resin is cured by at least one of thermal curing, natural curing, and ultraviolet curing. 12 . The method of manufacturing a display device according to claim 1 , wherein the second resin has a viscosity ranging from 10000 cPs to 50000 cPs. 13 . The method of manufacturing a display device according to claim 1 , wherein in the removing of the frame, the protection member includes a removal mark formed on a side surface thereof due to the removal of the frame.

14. The method for manufacturing a display device according to claim 1, in: In the cutting of the mother substrate, the dummy is located between the protection members, and The mother substrate is cut along a region between the dummy and each of the protection members. 15 . The method of manufacturing a display device according to claim 1 , wherein in the forming of the protection member, the second resin is applied into the opening by a screen printing method using a doctor blade. 16 . The method of manufacturing a display device according to claim 1 , further comprising forming a display layer on another surface of the mother substrate opposite to the surface.

17. A display device, include: substrate; A display layer, located on the first surface of the substrate; and a protective member located on a second surface of the substrate opposite to the first surface and including a resin, in: The protective member includes a removal mark on a side surface thereof, and The removal mark is formed by removing a frame surrounding the protective member. 18 . The display device according to claim 17 , wherein a thickness of the protection member is in a range of 100 μm to 300 μm. 19 . The display device according to claim 17 , wherein the resin comprises at least one of a binder, a first filler, a second filler, a light blocking material, and a foaming agent.

20. The display device according to claim 19, in: The first filler includes at least one of a carbon material and a ceramic material, and The second filler includes at least one of a carbon-based material and a metal-based material. 21 . The display device of claim 19 , wherein the light blocking material comprises at least one of carbon black, a black pigment, and a black dye. 22 . The display device of claim 19 , wherein the adhesive comprises at least one of an acrylic resin, a urethane resin, a silicone resin, and a rubber resin.

23. The display device of claim 17, wherein an elongation rate of the frame is 200% or more.