Submerged-arc welding flux flow self-adaptive control method based on arc sensing
Through the flux flow adaptive control method combined with arc sensing and scanning line laser system, the problem of difficult flux flow in submerged arc welding is solved, and the welding quality and cost improvement is achieved.
Patent Information
- Application Number
- CN202411230100.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During submerged arc welding, it is difficult to achieve adaptive control of the flux flow, resulting in unstable weld quality and waste of cost.
Adaptive control system for flow of submerged arc welding flux based on arc sensing is adopted, the theoretical thickness of the flux is calculated through the arc signal acquisition system, and the actual thickness of the flux is detected in real time in combination with the scanning line laser system, and the flux is adjusted by flux thickness status identification and adaptive control methods. flow.
It realizes precise control of flux flow during welding, improves welding quality and efficiency, reduces costs, and overcomes the problem of difficult flux flow to adapt.
Smart Images

Figure CN118905394A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of submerged arc welding flux flow adaptive control, and is a submerged arc welding flux flow adaptive control method based on arc sensing. Background Art
[0002] Submerged arc welding is a welding method in which an arc burns under a flux layer. It has inherent advantages such as stable welding quality, high welding productivity, no arc light and little smoke, and is widely used in the production of important steel structures such as pressure vessels, pipe segment manufacturing, box beams and columns. In the submerged arc welding process, the flux flow rate has a crucial impact on the quality of the weld. Insufficient flux coverage will cause the arc to be exposed and air to be drawn in, resulting in pores. Excessive flux coverage will cause flux waste. Appropriate flux flow is conducive to maintaining arc stability and forming beautiful welds, while saving costs. However, there is currently no method that can achieve adaptive control of flux flow in submerged arc welding. In response to this problem, the present invention discloses a method for adaptive control of flux flow in submerged arc welding based on arc sensing. Summary of the invention
[0003] The invention discloses a submerged arc welding flux flow adaptive control method based on arc sensing, which is used to control the flux flow, improve welding quality and efficiency, and reduce costs during the submerged arc welding process. The invention is characterized in that: the submerged arc welding flux flow adaptive control method based on arc sensing is composed of a submerged arc welding flux flow adaptive control system based on arc sensing; the submerged arc welding flux flow adaptive control system based on arc sensing is composed of a welding wire reel, a wire feeding mechanism, a submerged arc welding gun, a clamping device, an arc signal acquisition system, a submerged arc welding flux flow adaptive controller, and a scanning line laser system; the welding The wire reel is used to store and protect the welding wire; the wire feeding mechanism is used to transfer the welding wire for welding; the submerged arc welding torch is used to transmit welding current and transfer the welding wire for welding; the clamping device is used to fix the submerged arc welding flux flow adaptive controller on the welding torch; the arc signal acquisition system is used to collect arc voltage signals during welding; the submerged arc welding flux flow adaptive controller is used to identify the current flux thickness state, add flux in real time and adaptively control the flux flow in the flux funnel during welding; the scanning line laser system is used to obtain the height of the flux surface at the weld groove. The schematic diagram of the submerged arc welding flux flow adaptive control system based on arc sensing is shown in the figure. Figure 1 shown.
[0004] The arc sensing-based submerged arc welding flux flow adaptive control method is characterized in that: the theoretical thickness of the flux required in the welding process is calculated using the arc sensing-based submerged arc welding flux theoretical thickness calculation method; the arc sensing-based submerged arc welding flux theoretical thickness calculation method is achieved by detecting the welding voltage U, the corresponding arc length L = f(U), where f is a function model between the arc length and the arc voltage, and a relationship variable m is set, then the required theoretical thickness of the flux h = L+m.
[0005] The arc sensing-based submerged arc welding flux flow adaptive control method is characterized in that: the actual thickness of the flux is detected in real time by using a scanning line laser-based submerged arc welding flux actual thickness real-time detection method; the scanning line laser-based submerged arc welding flux actual thickness real-time detection method is to use two front and rear scanning lasers to scan the surface shape of the weld groove before and after welding during the welding process, and obtain the groove center point height h l With h s , then the actual thickness of the flux h r =h s -h l .
[0006] The submerged arc welding flux flow adaptive control method based on arc sensing is characterized in that: the flux flow is controlled by using the submerged arc welding flux flow control method; the submerged arc welding flux flow control method includes a flux thickness state recognition method and a flux flow adaptive control method; the flux thickness state recognition method is to calculate the deviation value ΔH=hh between the theoretical thickness and the actual thickness r And compared with the deviation threshold a, if -a≤ΔH≤a, it is considered that there is no deviation; if ΔH>a, it is considered that the theoretical thickness exceeds the actual thickness, and the flux flow should be reduced; if ΔH<-a, it is considered that the actual thickness exceeds the theoretical thickness, and the flux flow should be increased; the flux flow adaptive control method is to realize the flux flow adaptive control by calculating the change deviation of the difference between the actual flux thickness and the theoretical flux thickness in real time, and judging the current flux thickness state. Schematic diagram of submerged arc welding weld flux thickness is shown in Figure 3 The flux thickness status identification process is as shown in Figure 4 The flux flow adaptive control method process is as follows Figure 5 shown.
[0007] Advantageous Effects of the Invention
[0008] The present invention relates to a submerged arc welding flux flow adaptive control method based on arc sensing. A submerged arc welding flux theoretical thickness calculation method based on arc sensing is used to calculate the theoretical thickness of the flux required in the welding process; a submerged arc welding flux actual thickness real-time detection method based on scanning line laser is used to detect the actual thickness of the flux in real time; and a submerged arc welding flux flow control method is used to control the flux flow. The present invention overcomes the difficulty of realizing adaptive control of the submerged arc welding flux flow. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 This is the schematic diagram of the submerged arc welding flux flow adaptive control system based on arc sensing.
[0010] Figure 2 The flowchart of the adaptive control method of flux flow in submerged arc welding based on arc sensing.
[0011] Figure 3 Schematic diagram of flux thickness of submerged arc welding weld.
[0012] Figure 4 This is a flow chart of the flux thickness status identification method.
[0013] Figure 5 This is a flow chart of the flux flow adaptive control method.
[0014] In the figure: q0, q1, q2 are calculated by equation (1). k is the kth calculation cycle. H(k) is calculated by equation (2).
[0015] Hc(k) is calculated by equation (3). p , K i and K d is the PID control parameter.
[0016]
[0017] In the formula, K p is the proportionality coefficient, T I is the integration time constant, T D is the differential time constant.
[0018] H(k)=ΔH(k)-a (2)
[0019] Where ΔH(k) is the flux thickness deviation obtained in the kth calculation cycle, and a is the preset flux thickness deviation threshold.
[0020] Hc(k)=H(k)-H(k-1)(3) Specific implementation methods
[0022] In order to better express the technical solution and beneficial effects of the entire invention, the present invention is further described in detail below with reference to the accompanying drawings and implementation examples. The implementation methods of the present invention are not limited thereto.
[0023] Step 1: Calculation of theoretical flux thickness
[0024] In the submerged arc welding process based on arc sensing, the theoretical thickness of the flux is the basic data of the submerged arc welding flux flow adaptive system. To solve this problem, the present invention discloses a method for calculating the theoretical thickness of the flux. Figure 1 As shown, before calculating the theoretical thickness of the flux, Figure 1 The arc signal acquisition system in the system will receive the arc signal for a period of time in advance, and obtain the maximum voltage value U in the arc signal after filtering. max and minimum voltage value U min , and thus calculate the voltage value U=(U max +U min ) / 2. When calculating the theoretical thickness of the flux, the functional relationship between the arc length and the voltage is used to obtain the corresponding arc length L=f(U), where f is the functional model between the arc length and the arc voltage. Thus, the theoretical thickness of the flux is obtained as h=L+m.
[0025] Step 2: Obtaining the actual thickness of the flux
[0026] In the arc sensing-based submerged arc welding process, the actual thickness of the flux can be used to reflect whether the current flux thickness meets expectations. To address this problem, the present invention discloses a method for obtaining the actual thickness of the flux, which can obtain the actual thickness of the flux based on the difference in the center height of the groove before and after welding during the welding process. Figure 1 As shown in the figure, during the welding process, the scanning line laser system in the front of the welding direction scans the surface shape of the weld groove without flux and obtains the height h of the center point of the groove l ; The scanning line laser system behind the welding direction scans the surface shape of the weld groove after adding flux to obtain the height h of the center point of the groove s ; then the actual thickness of the flux h r =h s -h l .
[0027] Step 3: Adaptive control of flux flow in submerged arc welding
[0028] During the submerged arc welding process, the flux flow rate has a crucial impact on the quality of the weld. Insufficient flux coverage will cause the arc to be exposed and air to be drawn in, resulting in pores. Excessive flux coverage will cause flux waste. Appropriate flux flow is conducive to maintaining arc stability and forming beautiful welds, while saving costs. However, there is currently no method that can achieve adaptive control of flux flow in submerged arc welding. To address this problem, the present invention discloses a method for adaptive control of flux flow in submerged arc welding based on arc sensing, including a flux thickness state recognition method and a flux flow adaptive control method. Before performing adaptive flux flow control, Figure 1 The flux flow adaptive controller in the system will calculate the deviation ΔH=hh between the actual flux thickness and the theoretical flux thickness in real time. r and the rate of change of deviation, and compare it with the preset deviation threshold a, so as to identify the current state of flux thickness. If -a≤ΔH≤a, it is considered that there is no deviation and it is the optimal flux thickness; if ΔH>a, it is considered that the theoretical thickness exceeds the actual thickness, and the flux flow adaptive controller will use the flux flow adaptive control method to reduce the flux flow until -a≤ΔH≤a; if ΔH<-a, it is considered that the actual thickness exceeds the theoretical thickness, and the flux flow adaptive controller will use the flux flow adaptive control method to increase the flux flow until -a≤ΔH≤a.
Claims
1. An arc sensing-based adaptive control method for flux flow in submerged arc welding is used to control flux flow during submerged arc welding, and is characterized by: The arc sensing-based submerged arc welding flux flow adaptive control method is composed of an arc sensing-based submerged arc welding flux flow adaptive control system; the arc sensing-based submerged arc welding flux flow adaptive control system is composed of a wire reel, a wire feeding mechanism, a submerged arc welding gun, a clamping device, an arc signal acquisition system, a submerged arc welding flux flow adaptive controller and a scanning line laser system; the clamping device is used to fix the submerged arc welding flux flow adaptive controller on the welding gun; the arc signal acquisition system is used to collect arc voltage signals during the welding process; the submerged arc welding flux flow adaptive controller is used to identify the current flux thickness state, add flux in real time and adaptively control the flux flow in the flux funnel during the welding process; the scanning line laser system is used to obtain the flux surface height of the weld groove.
2. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: The theoretical thickness of the flux required during the welding process is calculated using a submerged arc welding flux theoretical thickness calculation method based on arc sensing; the submerged arc welding flux theoretical thickness calculation method based on arc sensing is achieved by detecting the welding voltage U, and the corresponding arc length L=f(U), where f is a function model between the arc length and the arc voltage, and a relationship variable m is set, then the theoretical thickness of the flux required at this time is h=L+m.
3. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: The actual thickness of submerged arc welding flux is detected in real time using a real-time detection method for the actual thickness of the flux based on scanning line laser.
4. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: The real-time detection method of the actual thickness of the submerged arc welding flux based on the scanning line laser is that during the welding process, the scanning line laser system located in front of the welding direction scans the surface shape of the weld groove without flux and obtains the height h of the center point of the groove. l The scanning line laser system located behind the welding direction scans the surface shape of the weld groove after adding flux and obtains the height h of the center point of the groove s ;The actual thickness of the flux h r =h s -h l .
5. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: A submerged arc welding flux flow control method is used to control the flux flow; the submerged arc welding flux flow control method includes a flux thickness state recognition method and a flux flow adaptive control method.
6. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: The solder paste thickness state identification method is achieved by calculating the deviation ΔH between the actual solder paste thickness and the theoretical solder paste thickness in real time and comparing it with a preset deviation threshold a; the solder paste thickness states include three types, namely, theoretical thickness exceeds actual thickness, optimal solder paste thickness, and actual thickness exceeds theoretical thickness; the theoretical thickness exceeds actual thickness when the solder paste thickness deviation ΔH>a; the optimal solder paste thickness is when the solder paste thickness deviation is within the preset deviation threshold, that is, -a≤ΔH≤a; the actual thickness exceeds theoretical thickness when the solder paste thickness deviation ΔH<-a.
7. The arc sensing-based submerged arc welding flux flow adaptive control method according to claim 1, characterized in that: The flux flow adaptive control method realizes the flux flow adaptive control by calculating the variation deviation of the difference between the actual flux thickness and the theoretical flux thickness in real time and judging the current flux thickness state.
Citation Information
Patent Citations
Submerged-arc welding device for profile steel machining
CN116372329A
Submerged arc welding solder flux feeding device
CN208680743U
Submerged arc welding device based on welding robot
CN218891306U
Method of laser-arc welding of the formulated pipe stock joint
RU2660541C1