O-shaped ring electro-deposition manufacturing device and method

By designing an O-ring electrodeposition manufacturing device, using voltage-steady power supply and rotary lifting actions to prepare metal O-rings under normal temperature and pressure, the problems of high cost and high energy consumption in the prior art are solved, and the problem of O-ring preparation in the prior art is realized. High efficiency and low energy consumption manufacturing effect.

CN118910681APending Publication Date: 2024-11-08CHANGZHOU UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410954484.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The method of preparing O-rings in the prior art is costly, has a large energy consumption and a complex process, making it difficult to efficiently manufacture high-quality O-rings under normal temperature and pressure.

Method used

An O-ring electrodeposition manufacturing device is designed, including a base module, a rotary module, a micro-feed module and a nozzle module. The conduction of the nozzle assembly and the copper round rod electrode is driven by a voltage-regulating power supply, and copper ions are deposited by current, combined with Rotating and lifting actions enable the preparation of metal O-rings at normal temperature and pressure.

Benefits of technology

It realizes the manufacture of metal O-rings at room temperature and pressure at high efficiency, low energy consumption and low cost, ensuring the thickness uniformity and dimensional accuracy of the prepared O-rings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118910681A_ABST
    Figure CN118910681A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of additive manufacturing, and particularly relates to an O-shaped ring electro-deposition manufacturing device and method.The O-shaped ring electro-deposition manufacturing device comprises a base module, a rotating module, a micro-feeding module and a spray head module; the micro-feeding module comprises a stabilized voltage supply, a current sensor and a micro-feeding assembly; the rotating module comprises a driving assembly, a copper round rod electrode and a conductive assembly; the nozzle module comprises a nozzle assembly and an electroplate liquid assembly, the stabilized voltage supply supplies power to the nozzle assembly and the conductive assembly, the electroplate liquid assembly sprays electroplate liquid, the electroplate liquid assembly enables the copper round bar electrode to be conductive, copper ions are deposited under the action of current, and the motion shaft moves in the Z direction so as to drive the nozzle assembly to do lifting motion. The driving assembly drives the copper round bar electrode to rotate, and the O-shaped ring with the uniform thickness is prepared on the copper round bar electrode at the normal temperature and the normal pressure through the two actions of lifting and rotating.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of additive manufacturing, and in particular relates to an O-ring electrodeposition manufacturing device and method. Background Art

[0002] O-rings are often used in the sealing field in industry. They have the ability to withstand high temperature and high pressure environments and can be used to prevent liquid and gas leakage. Powder metallurgy is a common method for preparing O-rings. The process of preparing O-rings by powder metallurgy includes raw material mixing, pressing, sintering, processing, and surface treatment. Pressing requires corresponding molds, and the sintering process consumes a lot of energy.

[0003] Therefore, in the existing technology, other methods such as laser additive manufacturing and electron beam additive manufacturing are chosen to prepare O-rings, but these processing technologies are generally costly, have harsh preparation environment requirements, and complex processes, so how to efficiently manufacture high-quality O-rings is a challenge. Summary of the invention

[0004] In view of this, in order to solve the problems existing in the prior art, the purpose of the present invention is to provide an O-ring electrodeposition manufacturing device and method, which can prepare metal O-rings at room temperature and pressure, and has the effects of simplicity, high efficiency, low energy consumption, safety, environmental protection and low cost.

[0005] In order to achieve the above object, the technical solution adopted by the present invention is:

[0006] An O-ring electrodeposition manufacturing device, comprising: a base module, a rotating module, a micro-feeding module and a nozzle module, wherein the rotating module, the micro-feeding module and the nozzle module are all arranged on the base module;

[0007] The micro-feed module includes a voltage-stabilized power supply, a current sensor and a micro-feed component, wherein the voltage-stabilized power supply is connected to the current sensor, and the micro-feed component has a motion axis moving along the Z direction;

[0008] The rotating module comprises a driving component, a copper round rod electrode and a conductive component, the two ends of the copper round rod electrode are respectively connected to the driving component and the conductive component, the conductive component is connected to the voltage-stabilized power supply, the driving component is used to drive the copper round rod electrode to rotate, the conductive component is used to conduct electricity to the copper round rod electrode, the driving component is connected to the micro-feeding component, and the driving component is connected to the current sensor;

[0009] The nozzle module includes a nozzle assembly and a plating liquid assembly. The nozzle assembly is installed on the moving shaft. The lower end of the nozzle assembly is located above the copper round rod electrode. One end of the plating liquid assembly is connected to the nozzle assembly through a pipeline. The upper end of the nozzle assembly is connected to the voltage-stabilized power supply.

[0010] The specific technical effect is: the nozzle assembly and the conductive assembly are powered by a voltage-stabilized power supply, the electroplating liquid assembly is used to spray the electroplating liquid toward the copper round rod electrode, and the conductive assembly is combined to make the copper round rod electrode conductive, and copper ions are deposited under the action of the current, so that a metal O-ring can be prepared at room temperature and pressure; the moving axis moves along the Z direction to drive the nozzle assembly to perform a lifting movement, and the driving assembly drives the copper round rod electrode to rotate. Through the two actions of lifting and rotating, an O-ring with uniform thickness can be prepared on the copper round rod electrode.

[0011] Furthermore, the micro-feed assembly includes: a stepper motor and two end clamps, one end of the two end clamps is connected to the base module, the other end of the two end clamps is connected to one end of the stepper motor, the motion shaft is arranged on the other end of the stepper motor, and the drive assembly is connected to the stepper motor.

[0012] The specific technical effect is: the stepper motor 1 is fixed by clamps at both ends, and only the moving axis of the stepper motor 1 moves along the Z direction to drive the nozzle assembly to perform a lifting movement, which can ensure the stability of the nozzle assembly during the lifting process, and then ensure the dimensional accuracy of the prepared O-ring.

[0013] Furthermore, the driving assembly comprises:

[0014] A single chip microcomputer, the single chip microcomputer is arranged on the base module, the single chip microcomputer is connected to the micro-feeding component and the current sensor;

[0015] A motor driver, the motor driver is arranged on the base module, and the motor driver is connected to the single chip microcomputer;

[0016] A motor bracket, wherein the motor bracket is arranged on the base module;

[0017] A second stepper motor, wherein the second stepper motor is arranged on the motor bracket, and the motor driver is used to control the second stepper motor;

[0018] A coupling, one end of which is connected to the rotating shaft of the second stepper motor, and the other end of which is connected to the copper round rod electrode.

[0019] The specific technical effect is: the motor driver is controlled by the single-chip microcomputer, and then the speed of the stepper motor two is controlled, so as to ensure the uniform density of the prepared O-ring, and the current signal of the voltage-stabilized power supply is monitored by the current sensor, and the monitored current signal is converted into a voltage signal through ADC to the single-chip microcomputer. When the single-chip microcomputer receives the output voltage signal of the current sensor, the moving axis of the stepper motor one can be pulled to a specified height in the Z-axis direction.

[0020] Furthermore, the conductive component includes: a conductive slip ring and a slip ring bracket, the two ends of the conductive slip ring are respectively connected to the copper round rod electrode and the slip ring bracket, the conductive slip ring is connected to the voltage-stabilized power supply, and the slip ring bracket is arranged on the base module.

[0021] The specific technical effect is: the conductive slip ring enables the copper round rod electrode to conduct electricity, allowing copper ions to be deposited under the action of electric current.

[0022] Furthermore, the nozzle assembly comprises:

[0023] A spray head, one side of which is connected to the moving shaft, and a spray channel is provided in the spray head;

[0024] A nozzle, the nozzle is arranged at the lower end of the nozzle and directly faces the spray channel, the nozzle is communicated with the spray channel, and the nozzle is arranged above the copper round rod electrode;

[0025] A platinum electrode, the platinum electrode is arranged in the spray channel, the lower end of the platinum electrode extends out of the lower end of the nozzle, there is a distance H1 between the lower end of the platinum electrode and the lower end of the nozzle, and the upper end of the platinum electrode is connected to the voltage-stabilized power supply;

[0026] A knob is installed on the other side of the nozzle, a plating liquid channel is provided in the knob, the plating liquid channel is connected with the spray channel, and one end of the plating liquid assembly is connected with the plating liquid channel through a pipeline.

[0027] The specific technical effect is: the plating solution channel is connected with the spray channel, the plating solution can flow to the copper round rod electrode through the platinum electrode, the platinum electrode is connected to the voltage-stabilized power supply, the conductive slip ring enables the copper round rod electrode to conduct electricity, and the copper ions are deposited on the copper round rod electrode using the electrodeposition technology.

[0028] Furthermore, the electroplating liquid assembly includes: a plating liquid circulation tank and a peristaltic pump, the plating liquid circulation tank and the peristaltic pump are both arranged on the base module, the plating liquid circulation tank is arranged below the copper round rod electrode, the plating liquid circulation tank is connected to the peristaltic pump through a pipeline, and the peristaltic pump is connected to the plating liquid channel through a pipeline.

[0029] The specific technical effect is: the peristaltic pump allows the electroplating solution to flow from the plating solution circulation tank into the plating solution channel at a certain flow rate, and the plating solution circulation tank is arranged below the copper round rod electrode to receive excess electroplating solution, so that the electroplating solution can be recycled.

[0030] Furthermore, a wax-plated film area is provided on the copper round rod electrode, and a conductive film and two insulating films are sleeved on the wax-plated film area. The two insulating films are respectively against the two ends of the conductive film, and the lower end of the nozzle assembly is arranged above the conductive film.

[0031] The specific technical effect is: a conductive film is attached to the copper round rod electrode to isolate the O-ring from the copper round rod electrode, and it is also convenient to remove the prepared O-ring from the copper round rod electrode, and insulating films are set at both ends of the insulating film so that copper ions are only deposited in the area on the conductive film.

[0032] Furthermore, the thickness of the conductive film is smaller than the thickness of the insulating film.

[0033] The specific technical effect is: because the thickness of the conductive film is less than that of the insulating film, the insulating film can play a limiting role, so that the copper ions are only deposited in the area on the conductive film.

[0034] Further, the base module includes a substrate, a first group of bases, a second group of bases, a third group of bases and a fourth group of bases, the first group of bases is arranged on the substrate, the two ends of the second group of bases are respectively connected to the first group of bases and the fourth group of bases, the third group of bases is arranged on the second group of bases and has a distance with the first group of bases, the voltage-stabilized power supply, the plating liquid assembly and at least a part of the driving assembly are arranged on the substrate, at least a part of the driving assembly is arranged on the third group of bases, the conductive assembly is arranged on the third group of bases, and the micro-feed assembly is arranged on the fourth group of bases.

[0035] A method for preparing an O-ring using an O-ring electrodeposition manufacturing device as described in any one of the above, wherein the method comprises the following steps:

[0036] Step S1, preparing an electroplating solution using anhydrous copper sulfate, and placing the prepared electroplating solution in the plating solution circulation tank;

[0037] Step S2, cleaning the copper round rod electrode with an acetone solution, and then immersing the cleaned copper round rod electrode in a deionized water solution for ultrasonic cleaning;

[0038] Step S3, pasting a conductive film and two insulating films on the wax-coated film-pasting area of ​​the copper round rod electrode after ultrasonic cleaning in step S2, wherein the two insulating films are located at both ends of the conductive film;

[0039] Step S4, installing the copper round rod electrode obtained in step S3 between the driving component and the conductive component;

[0040] Step S5, moving the nozzle assembly above the copper round rod electrode, with the nozzle located above the conductive film, turning on the peristaltic pump, and allowing the electroplating solution prepared in step S1 to flow from the plating solution circulation tank into the plating solution channel through the peristaltic pump at a flow rate of 12 ml / min to 15 ml / min;

[0041] Step S6, turning on the drive assembly, the single chip microcomputer controls the motor driver, the motor driver controls the stepper motor 2 to rotate at a speed of 120 rpm to 180 rpm, thereby driving the copper round rod electrode to rotate;

[0042] Step S7, turning on the voltage regulator power supply, the voltage regulator power supply performs electrodeposition at a voltage of 3.8V, and at the same time turning on the stepper motor 1, the motion axis moves along the Z direction, thereby driving the nozzle assembly to be pulled along the Z direction, and the copper ion deposits are deposited on the conductive film around the copper round rod electrode, and the deposition height of the copper ion deposits is h, and the range of h is 400μm to 800μm;

[0043] Step S8, after step S7 is completed, remove the copper round rod electrode with copper ion deposits, and peel off the insulating film and the copper ion deposits from the copper round rod electrode in sequence;

[0044] Step S9, placing the copper ion deposit peeled off in step S8 in a tube furnace, and performing annealing treatment under nitrogen protection, with the annealing temperature being 200° C. and the holding time being 30 min;

[0045] Step S10, cooling the copper ion deposit after the annealing treatment in step S9, and the preparation of the O-ring is completed.

[0046] The beneficial effects of the present invention are:

[0047] (1) The nozzle assembly and the conductive assembly are powered by a voltage-stabilized power supply, and the electroplating liquid assembly is used to spray the electroplating liquid toward the copper round rod electrode, and the conductive assembly is used to make the copper round rod electrode conductive, and copper ions are deposited under the action of the current, so that a metal O-ring can be prepared at room temperature and pressure;

[0048] (2) The motion axis moves along the Z direction, thereby driving the nozzle assembly to perform a lifting motion, and the driving assembly drives the copper round rod electrode to rotate. Through the two actions of lifting and rotating, an O-ring with uniform thickness can be prepared on the copper round rod electrode.

[0049] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0051] Figure 1 It is a structural schematic diagram of an O-ring electrodeposition manufacturing device of the present invention;

[0052] Figure 2 yes Figure 1 A partial enlarged view of the middle A;

[0053] Figure 3 is a cross-sectional view of a nozzle assembly of the present invention;

[0054] Figure 4 is a circuit diagram of a current sensor of the present invention;

[0055] Figure 5 is an exploded view of the base module of the present invention.

[0056] In the figure:

[0057] 1. Voltage stabilized power supply; 2. Base; 3. Peristaltic pump; 4. Slip ring bracket; 5. Conductive slip ring; 6. Copper round rod electrode; 7. Plating solution circulation tank; 8. Coupling; 9. Stepper motor 2; 10. Motor bracket; 11. Motor driver; 12. Single chip microcomputer; 13. Current sensor; 14. Nozzle; 15. Platinum electrode; 16. Connecting screws; 17. Stepper motor 1; 18. Two-end clamps; 19. Knob; 20. Plating solution channel; 21. Nozzle; 22. Conductive film; 23. Insulating film; 24. The first group of bases; 25. The second group of bases; 26. The third group of bases; 27. The fourth group of bases; 261. Aluminum profile 1; 262. Aluminum profile 2; 271. Aluminum profile 3; 272. Aluminum profile 4; 273. Aluminum profile 5; 28. Spray channel. DETAILED DESCRIPTION

[0058] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0059] like Figures 1 to 5As shown, an O-ring electrodeposition manufacturing device includes: a base module, a rotating module, a micro-feeding module and a nozzle module, wherein the rotating module, the micro-feeding module and the nozzle module are all arranged on the base module;

[0060] The micro-feed module includes a voltage-stabilized power supply 1, a current sensor 13 and a micro-feed component, wherein the voltage-stabilized power supply 1 is connected to the current sensor 13, and the micro-feed component has a motion axis moving along the Z direction;

[0061] The rotating module includes a driving component, a copper round rod electrode 6 and a conductive component. The two ends of the copper round rod electrode 6 are respectively connected to the driving component and the conductive component. The conductive component is connected to a voltage-stabilized power supply 1. The driving component is used to drive the copper round rod electrode 6 to rotate. The conductive component is used to conduct electricity to the copper round rod electrode 6. The driving component is connected to a micro-feeding component, and the driving component is connected to a current sensor 13.

[0062] The nozzle module includes a nozzle assembly and a plating liquid assembly. The nozzle assembly is installed on the moving shaft. The lower end of the nozzle assembly is located above the copper round rod electrode 6. One end of the plating liquid assembly is connected to the nozzle assembly through a pipeline. The upper end of the nozzle assembly is connected to the voltage-stabilized power supply 1.

[0063] It should be noted here that: the nozzle assembly and the conductive assembly are powered by a voltage-stabilized power supply 1, and the electroplating liquid assembly is used to spray the electroplating liquid toward the copper round rod electrode 6, and the conductive assembly is combined to make the copper round rod electrode 6 conductive, and copper ions are deposited under the action of the current, so that a metal O-ring can be prepared at room temperature and pressure; the moving axis moves along the Z direction to drive the nozzle assembly to perform a lifting movement, and the driving assembly drives the copper round rod electrode 6 to rotate. Through the two actions of lifting and rotating, an O-ring with uniform thickness can be prepared on the copper round rod electrode 6.

[0064] The copper round rod electrode 6 has a diameter of 3 mm to 5 mm and a length of 100 mm to 150 mm.

[0065] The base module includes a substrate 2, a first group of bases 24, a second group of bases 25, a third group of bases 26 and a fourth group of bases 27. The first group of bases 24 is arranged on the substrate 2, the two ends of the second group of bases 25 are respectively connected to the first group of bases 24 and the fourth group of bases 27, the third group of bases 26 is arranged on the second group of bases 25 and has a distance with the first group of bases 24, the voltage-stabilized power supply 1, the plating liquid assembly and at least a part of the driving assembly are arranged on the substrate 2, at least a part of the driving assembly is arranged on the third group of bases 26, the conductive assembly is arranged on the third group of bases 26, and the micro-feed assembly is arranged on the fourth group of bases 27.

[0066] It should be noted that: the first group of bases 24 includes four first aluminum profiles, which are connected end to end through corner brackets to form a rectangular frame, and the rectangular frame is horizontally placed on the base 2; the second group of bases 25 includes four second aluminum profiles, which are vertically installed on the four corners of the rectangular frame through corner brackets;

[0067] The third group of bases 26 includes an aluminum profile 1 261 and an aluminum profile 262 arranged in parallel. The aluminum profile 1 261 is horizontally mounted on two second aluminum profiles through an angle bracket, and the aluminum profile 2 262 is horizontally mounted on another two second aluminum profiles through an angle bracket. The distance between the aluminum profile 1 261 and the aluminum profile 2 262 and the first aluminum profile is 10 cm to 15 cm.

[0068] The fourth group of bases 27 includes aluminum profile three 271, aluminum profile four 272 and aluminum profile five 273. The two ends of aluminum profile five 273 are respectively connected to the middle parts of aluminum profile three 271 and aluminum profile four 272. The fourth group of bases 27 is arranged in an I-shaped structure. Aluminum profile three 271 is horizontally installed on the upper ends of two second aluminum profiles through an angle code. Aluminum profile three 271 is located above aluminum profile one 261. Aluminum profile four 272 is horizontally installed on the upper ends of the other two second aluminum profiles through an angle code. Aluminum profile four 272 is located above aluminum profile two 262.

[0069] The micro-feed assembly includes: a stepper motor 17 and two end clamps 18, one end of the two end clamps 18 is connected to the base module, the other end of the two end clamps 18 is connected to one end of the stepper motor 17, the motion axis is set on the other end of the stepper motor 17, and the drive assembly is connected to the stepper motor 17.

[0070] It should be noted here that one end of the two-end clamp 18 is connected to the middle of the aluminum profile 5 273 through a thread, and the other end of the two-end clamp 18 is connected to one end of the stepper motor 17 through a thread. The stepper motor 17 is fixed by the two-end clamp 18, and only the moving axis of the stepper motor 17 moves along the Z direction to drive the nozzle assembly to perform a lifting movement, which can ensure the stability of the nozzle assembly during the lifting process, and then ensure the dimensional accuracy of the prepared O-ring.

[0071] The stepper motor 17 can be selected as a five-phase stepper motor.

[0072] The drive components include:

[0073] A single chip microcomputer 12, which is disposed on the base module and is connected to the micro-feeding component and the current sensor 13;

[0074] A motor driver 11, which is disposed on the base module and connected to the single-chip microcomputer 12;

[0075] The motor bracket 10 is arranged on the base module;

[0076] A stepper motor 9, the stepper motor 9 is arranged on a motor bracket 10, and a motor driver 11 is used to control the stepper motor 9;

[0077] A coupling 8, one end of the coupling 8 is connected to the rotating shaft of the stepping motor 2 9, and the other end of the coupling 8 is connected to the copper round rod electrode 6.

[0078] It should be noted here that: the motor bracket 10 is connected to the aluminum profile 261 by threads, the stepper motor 29 is placed horizontally and connected to the motor bracket 10 by threads, the copper round rod electrode 6 is connected to the rotating shaft of the stepper motor 29 by a coupling 8, the single-chip microcomputer 12 controls the motor driver 11, and the motor driver 11 controls the stepper motor 29 to rotate, thereby driving the copper round rod electrode 6 to rotate, thereby ensuring the dimensional accuracy of the prepared O-ring;

[0079] The single-chip microcomputer 12 is electrically connected to the five-phase stepper motor, one end of the current sensor 13 is connected to the voltage-stabilized power supply 1, and the other end of the current sensor 13 is connected to the single-chip microcomputer 12, and the current signal of the voltage-stabilized power supply 1 is monitored by the current sensor 13, and the monitored current signal is converted into a voltage signal through ADC and converted to the single-chip microcomputer 12. When the single-chip microcomputer 12 receives the output voltage of the current sensor 13, it satisfies the inequality U out >0.5U cc +0.4I * , the moving axis of the stepper motor 17 can be pulled to a specified height in the Z-axis direction;

[0080] Wherein, Uout is the output voltage of the current sensor 13, Ucc is the supply voltage of the current sensor 13, and I* is the output current of the monitored regulated power supply 1;

[0081] Preferably, Ucc is 5V, 0.8A≤I*≤1A;

[0082] Preferably, the specified height that the moving axis of the stepping motor 17 pulls up each time is ho, where ho=2 μm.

[0083] The stepper motor 2 9 can be selected as a two-phase stepper motor. Preferably, the rotation speed of the two-phase stepper motor is 90 rpm to 180 rpm.

[0084] The conductive assembly includes: a conductive slip ring 5 and a slip ring bracket 4. The two ends of the conductive slip ring 5 are respectively connected to the copper round rod electrode 6 and the slip ring bracket 4. The conductive slip ring 5 is connected to the voltage-stabilized power supply 1. The slip ring bracket 4 is arranged on the base module.

[0085] It should be noted here that: the slip ring bracket 4 is connected to the aluminum profile 262 by threads, the conductive slip ring 5 is connected to the slip ring bracket 4 by threads, the conductive slip ring 5 is provided with an inner hole, the left end of the copper round rod electrode 6 is arranged in the inner hole, the copper round rod electrode 6 is arranged horizontally, the conductive slip ring 5 is connected to the voltage-stabilized power supply 1, the conductive slip ring 5 enables the copper round rod electrode 6 to conduct electricity, and copper ions are deposited under the action of the current.

[0086] The nozzle assembly includes:

[0087] A spray head 14, one side of which is connected to the moving shaft, and a spray channel 28 is provided in the spray head 14;

[0088] Nozzle 21, the nozzle 21 is arranged at the lower end of the nozzle 14 and directly faces the spray channel 28, the nozzle 21 is connected to the spray channel 28, and the nozzle 21 is arranged above the copper round rod electrode 6;

[0089] A platinum electrode 15, the platinum electrode 15 is disposed in the spray channel 28, the lower end of the platinum electrode 15 extends out of the lower end of the nozzle 21, there is a distance between the lower end of the platinum electrode 15 and the lower end of the nozzle 21, and the upper end of the platinum electrode 15 is connected to the voltage-stabilized power supply 1;

[0090] The knob 19 is installed on the other side of the nozzle 14. A plating liquid channel 20 is provided in the knob 19. The plating liquid channel 20 is connected with the spray channel 28. One end of the plating liquid assembly is connected with the plating liquid channel 20 through a pipeline.

[0091] It should be noted here that: the plating solution channel 20 is connected to the spray channel 28, the plating solution can flow to the copper round rod electrode 6 through the platinum electrode 15, the platinum electrode 15 is connected to the voltage-stabilized power supply 1, the conductive slip ring 5 enables the copper round rod electrode 6 to be conductive, and copper ions are deposited on the copper round rod electrode 6 using electrodeposition technology.

[0092] One side of the nozzle 14 is connected to the moving shaft of the stepper motor 17 through a connecting screw 16. The distance between the lower end of the platinum electrode 15 and the lower end of the nozzle 21 ranges from 100μm to 200μm, and the distance between the lower end of the platinum electrode 15 and the copper round rod electrode 6 ranges from 40μm to 50μm.

[0093] The current sensor 13 can be a CC6920 chip, see Figure 4 As shown, IP+ is connected to the positive electrode of the regulated power supply 1, IP- is connected to the negative electrode of the regulated power supply 1, GND is connected to the ground of the PCB board, VCC is connected to the power supply voltage on the PCB board, and ADC / MCU is connected to the pin of the microcontroller 12.

[0094] See also Figure 1As shown, the positive electrode of the voltage-stabilized power supply 1 is also connected to the upper end of the platinum electrode 15 for supplying power to the platinum electrode 15, serving as the negative electrode of the electrodeposition process. The negative electrode of the voltage-stabilized power supply 1 is also connected to the conductive slip ring 5 for making the copper round rod electrode 6 conductive, so that copper ions are deposited under the action of the current.

[0095] The electroplating liquid assembly includes: a plating liquid circulation tank 7 and a peristaltic pump 3, both of which are arranged on the base module, the plating liquid circulation tank 7 is arranged below the copper round rod electrode 6, the plating liquid circulation tank 7 is connected to the peristaltic pump 3 through a pipeline, and the peristaltic pump 3 is connected to the plating liquid channel 20 through a pipeline.

[0096] It should be noted here that the peristaltic pump 3 allows the electroplating solution to flow from the electroplating solution circulation tank 7 into the electroplating solution channel 20 at a certain flow rate, and the electroplating solution circulation tank 7 is arranged below the copper round rod electrode 6 to receive excess electroplating solution, so that the electroplating solution can be recycled.

[0097] The water inlet pipe of the peristaltic pump 3 is connected to the plating solution circulation tank 7 , and the water outlet pipe of the peristaltic pump 3 is communicated with the plating solution channel 20 .

[0098] Preferably, the flow rate of the peristaltic pump 3 is 12 ml / min to 15 ml / min.

[0099] The copper round rod electrode 6 is provided with a wax-coated film area, on which a conductive film 22 and two insulating films 23 are sleeved. The two insulating films 23 are respectively against the two ends of the conductive film 22 . The lower end of the nozzle assembly is located above the conductive film 22 .

[0100] It should be noted here that: a conductive film 22 is attached to the copper round rod electrode 6 to isolate the O-ring from the copper round rod electrode 6, and it is also convenient to remove the prepared O-ring from the copper round rod electrode 6, and an insulating film 23 is set at both ends of the insulating film 23, so that copper ions are only deposited in the area on the conductive film 22.

[0101] The thickness of the conductive film 22 is smaller than the thickness of the insulating film 23 .

[0102] It should be noted here that: since the thickness of the conductive film 22 is smaller than the thickness of the insulating film 23 , the insulating film 23 can play a limiting role, so that the copper ions are only deposited in the area on the conductive film 22 .

[0103] Preferably, the width of the conductive film 22 is 0.3 mm to 0.5 mm, and the thickness of the conductive film 22 is 0.05 mm to 0.2 mm; the width of each insulating film 23 is 3 mm to 5 mm, and the thickness of the insulating film 23 is 1 mm to 3 mm.

[0104] It should be noted here that the diameter of the nozzle 21 matches the width of the conductive film 22, so the moving axis of the stepper motor 17 only drives the nozzle assembly to be pulled along the Z direction, and does not move in the horizontal direction. It can also deposit O-rings with a width of 0.3mm to 0.5mm. The advantage of this unidirectional movement is that by limiting the moving direction, the relative displacement between the deposits can be reduced, thereby increasing the stability of the O-ring.

[0105] A method for preparing an O-ring using any one of the above-mentioned O-ring electrodeposition manufacturing devices, wherein the method comprises the following steps:

[0106] Step S1, using anhydrous copper sulfate to prepare an electroplating solution, and placing the prepared electroplating solution in a plating solution circulation tank 7;

[0107] Step S2, using an acetone solution to clean the copper round rod electrode 6, and then immersing the cleaned copper round rod electrode 6 in a deionized water solution for ultrasonic cleaning;

[0108] Step S3, pasting a conductive film 22 and two insulating films 23 on the wax-coated film pasting area of ​​the copper round rod electrode 6 after ultrasonic cleaning in step S2, wherein the two insulating films 23 are located at both ends of the conductive film 22;

[0109] Step S4, installing the copper round rod electrode 6 obtained in step S3 between the driving component and the conductive component;

[0110] Step S5, move the nozzle assembly to above the copper round rod electrode 6, with the nozzle 21 located above the conductive film 22, start the peristaltic pump 3, and let the electroplating solution prepared in step S1 flow from the plating solution circulation tank 7 into the plating solution channel 20 through the peristaltic pump 3 at a flow rate of 12 ml / min to 15 ml / min;

[0111] Step S6, start the driving component, the single chip microcomputer 12 controls the motor driver 11, the motor driver 11 controls the stepper motor 2 9 to rotate at a speed of 120 rpm to 180 rpm, thereby driving the copper round rod electrode 6 to rotate;

[0112] Step S7, turn on the stabilized power supply 1, the stabilized power supply 1 performs electrodeposition at a voltage of 3.8V, and at the same time turn on the stepper motor 17, the moving axis moves along the Z direction, thereby driving the nozzle assembly to be pulled along the Z direction, and the copper ion deposit is deposited on the conductive film 22 around the copper round rod electrode 6, and the deposition height of the copper ion deposit is h, and the range of h is 400μm to 800μm;

[0113] Step S8, after step S7 is completed, the copper round rod electrode 6 with the copper ion deposit is removed, and the insulating film 23 and the copper ion deposit are peeled off from the copper round rod electrode 6 in sequence;

[0114] Step S9, placing the copper ion deposit peeled off in step S8 in a tube furnace, and performing annealing treatment under nitrogen protection, with the annealing temperature being 200° C. and the holding time being 30 min;

[0115] Step S10, cooling the copper ion deposit after the annealing treatment in step S9, and the preparation of the O-ring is completed.

[0116] The above are only preferred embodiments of the present invention, and are not intended to limit the implementation and protection scope of the present invention.

[0117] The present invention also has the following implementation modes based on the above:

[0118] Step S1, using anhydrous copper sulfate powder crystals with a concentration of 99.5% to prepare a plating solution with a concentration of 1 mol / L, then adding 0.6 mol / L concentrated sulfuric acid and 200 mg polyethylene glycol to the above plating solution, and placing the prepared plating solution in a plating solution circulation tank 7;

[0119] Step S2, selecting a copper round rod electrode 6 with a length of 100 mm and a diameter of 5 mm, cleaning the copper round rod electrode 6 with an acetone solution, and then immersing the cleaned copper round rod electrode 6 in a deionized water solution for ultrasonic cleaning;

[0120] Step S3, a layer of graphite film with a width of 0.4 mm and a thickness of 0.1 mm is pasted on the wax-coated film area of ​​the copper round rod electrode 6 after ultrasonic cleaning in step S2, and a layer of paraffin film with a width of 3 mm and a thickness of 1 mm is plated on both sides of the graphite film.

[0121] The specific operation method of coating the paraffin film is as follows: preheat the paraffin for a certain period of time to the melting point of the wax liquid 58, immerse the two ends of the copper round rod electrode 6 in the wax liquid, then quickly take it out and dry it, so that a wax layer is formed on the surface of the copper round rod electrode 6, and repeat the operation 3 to 5 times to obtain a paraffin film with a thickness of about 1 mm.

[0122] The prepared copper round rod electrode 6 is installed between the conductive slip ring 5 and the coupling 8;

[0123] Step S4: preparing and installing the platinum electrode 15,

[0124] A 0.3 mm platinum wire is placed in a glass capillary with an outer diameter of 3 mm and an inner diameter of 0.5 mm, and then epoxy resin glue is filled therein to seal it. The sealed platinum electrode 15 is arranged in the spray channel 28 along the Z direction, and the lower end of the platinum electrode 15 extends out of the nozzle 21. The distance between the lower end of the platinum electrode 15 and the lower end of the nozzle 21 is 100 μm, and the distance between the lower end of the platinum electrode 15 and the copper round rod electrode 6 is 45 μm.

[0125] Step S5, move the nozzle assembly to above the copper round rod electrode 6, the nozzle 21 is located above the conductive film 22, start the peristaltic pump 3, and let the electroplating solution prepared in step S1 flow from the plating solution circulation tank 7 into the plating solution channel 20 through the peristaltic pump 3 at a flow rate of 12 ml / min;

[0126] Step S6, start the driving component, the single chip microcomputer 12 controls the motor driver 11, the motor driver 11 controls the two-phase stepper motor to rotate at a speed of 135 rpm, and then drives the copper round rod electrode 6 to rotate;

[0127] Step S7, turn on the stabilized power supply 1, the stabilized power supply 1 performs electrodeposition at a voltage of 3.8V, and at the same time turn on the five-phase stepper motor, the moving axis of the five-phase stepper motor moves along the Z direction, and then drives the nozzle assembly to be pulled along the Z direction, and the copper ion deposits are deposited on the conductive film 22 around the copper round rod electrode 6.

[0128] Ucc is 5V, I* is 0.9A, therefore, when the output voltage of the current sensor 13 is greater than 2.86V, the five-phase stepper motor moves in the Z-axis direction, the height ho of each pull of the five-phase stepper motor is 2μm, and the number of pulls n of the five-phase stepper motor is 200 times, then the deposition height of the copper ion deposit h=n×ho, h is 400μm;

[0129] Step S8, after step S7 is completed, remove the copper round rod electrode 6 with copper ion deposits, peel off the insulating film 23 and the copper ion deposits from the copper round rod electrode 6 in turn, put the copper round rod electrode 6 with paraffin film at both ends into 55°C water, retreat until the copper round rod electrode 6 base can be seen, and then remove the O-ring with tweezers;

[0130] Step S9, placing the O-ring peeled off in step S8 in a tube furnace, and performing annealing treatment under nitrogen protection, the annealing temperature is 200° C., and the holding time is 30 minutes;

[0131] Step S10, cooling the copper ion deposit after the annealing treatment in step S9, and the preparation of the O-ring is completed, and an O-ring with an inner diameter of 5.1 mm and a thickness of 400 um is obtained.

[0132] The beneficial effects of the present invention are:

[0133] (1) The nozzle assembly and the conductive assembly are powered by a voltage-stabilized power supply 1, and the electroplating liquid assembly is used to spray the electroplating liquid toward the copper round rod electrode 6. The conductive assembly is then used to make the copper round rod electrode 6 conductive, and copper ions are deposited under the action of the current, so that a metal O-ring can be prepared at room temperature and pressure;

[0134] (2) The motion axis moves along the Z direction to drive the nozzle assembly to perform a lifting motion, and the driving assembly drives the copper round rod electrode 6 to rotate. Through the two actions of lifting and rotating, an O-ring with uniform thickness can be prepared on the copper round rod electrode 6.

[0135] The various devices selected in this application are all universal standard parts or parts known to those skilled in the art, and their structures and principles can be known to those skilled in the art through technical manuals or conventional experimental methods.

[0136] In the description of the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0137] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0138] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.

Claims

1. An O-ring electrodeposition manufacturing device, It is characterized in that include: A base module, a rotating module, a micro-feeding module and a nozzle (14) module, wherein the rotating module, the micro-feeding module and the nozzle (14) module are all arranged on the base module; The micro-feed module comprises a voltage-stabilized power supply (1), a current sensor (13) and a micro-feed component, wherein the voltage-stabilized power supply (1) is connected to the current sensor (13), and the micro-feed component has a motion axis that moves along the Z direction; The rotating module comprises a driving component, a copper round rod electrode (6) and a conductive component, the two ends of the copper round rod electrode (6) are respectively connected to the driving component and the conductive component, the conductive component is connected to the voltage-stabilized power supply (1), the driving component is used to drive the copper round rod electrode (6) to rotate, the conductive component is used to conduct electricity to the copper round rod electrode (6), the driving component is connected to the micro-feeding component, and the driving component is connected to the current sensor (13); The nozzle (14) module comprises a nozzle (14) component and an electroplating liquid component. The nozzle (14) component is mounted on the moving shaft. The lower end of the nozzle (14) component is located above the copper round rod electrode (6). One end of the electroplating liquid component is connected to the nozzle (14) component through a pipeline. The upper end of the nozzle (14) component is connected to the voltage-stabilized power supply (1).

2. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The micro-feed assembly comprises: a stepper motor (17) and two end clamps (18), one end of the two end clamps (18) is connected to a base module, the other end of the two end clamps (18) is connected to one end of the stepper motor (17), the motion shaft is arranged on the other end of the stepper motor (17), and the drive assembly is connected to the stepper motor (17).

3. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The drive assembly comprises: A single-chip microcomputer (12), the single-chip microcomputer (12) being arranged on the base module, the single-chip microcomputer (12) being connected to the micro-feeding component and the current sensor (13); A motor driver (11), the motor driver (11) being arranged on the base module, and the motor driver (11) being connected to the single chip computer (12); A motor bracket (10), wherein the motor bracket (10) is arranged on the base module; A second stepping motor (9), wherein the second stepping motor (9) is arranged on the motor bracket (10), and the motor driver (11) is used to control the second stepping motor (9); A coupling (8), one end of the coupling (8) is connected to the rotating shaft of the second stepping motor (9), and the other end of the coupling (8) is connected to the copper round rod electrode (6).

4. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The conductive component comprises: a conductive slip ring (5) and a slip ring bracket (4); two ends of the conductive slip ring (5) are respectively connected to the copper round rod electrode (6) and the slip ring bracket (4); the conductive slip ring (5) is connected to the voltage-stabilized power supply (1); and the slip ring bracket (4) is arranged on the base module.

5. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The nozzle (14) assembly comprises: A spray head (14), one side of the spray head (14) is connected to the moving shaft, and a spray channel (28) is provided in the spray head (14); A nozzle (21), the nozzle (21) being arranged at the lower end of the nozzle head (14) and facing the spray channel (28), the nozzle (21) being connected to the spray channel (28), and the nozzle (21) being arranged above the copper round rod electrode (6); a platinum electrode (15), the platinum electrode (15) being arranged in the spray channel (28), the lower end of the platinum electrode (15) extending out of the lower end of the nozzle (21), a distance H1 being provided between the lower end of the platinum electrode (15) and the lower end of the nozzle (21), and the upper end of the platinum electrode (15) being connected to the voltage-stabilized power supply (1); A knob (19) is installed on the other side of the nozzle (14), a plating liquid channel (20) is provided in the knob (19), the plating liquid channel (20) is connected with the spray channel (28), and one end of the plating liquid component is connected with the plating liquid channel (20) through a pipeline.

6. An O-ring electrodeposition manufacturing device as claimed in claim 5, It is characterized in that The electroplating liquid component comprises: a plating liquid circulation tank (7) and a peristaltic pump (3); the plating liquid circulation tank (7) and the peristaltic pump (3) are both arranged on the base module; the plating liquid circulation tank (7) is arranged below the copper round rod electrode (6); the plating liquid circulation tank (7) and the peristaltic pump (3) are connected via a pipeline; and the peristaltic pump (3) is connected to the plating liquid channel (20) via a pipeline.

7. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The copper round rod electrode (6) is provided with a wax-coated film area, and a conductive film (22) and two insulating films (23) are sleeved on the wax-coated film area. The two insulating films (23) are respectively abutted against two ends of the conductive film (22), and the lower end of the nozzle (14) assembly is arranged above the conductive film (22).

8. An O-ring electrodeposition manufacturing device as claimed in claim 7, It is characterized in that The thickness of the conductive film (22) is smaller than the thickness of the insulating film (23).

9. An O-ring electrodeposition manufacturing device as claimed in claim 1, It is characterized in that The base module comprises a substrate (2), a first group of bases (24), a second group of bases (25), a third group of bases (26) and a fourth group of bases (27); the first group of bases (24) is arranged on the substrate (2); two ends of the second group of bases (25) are respectively connected to the first group of bases (24) and the fourth group of bases (27); the third group of bases (26) is arranged on the second group of bases (25) and has a spacing with the first group of bases (24); the voltage-stabilized power supply (1), the electroplating liquid component and at least a part of the driving component are arranged on the substrate (2); at least a part of the driving component is arranged on the third group of bases (26); the conductive component is arranged on the third group of bases (26); and the micro-feeding component is arranged on the fourth group of bases (27).

10. A method for preparing an O-ring using the O-ring electrodeposition manufacturing device according to any one of claims 1 to 9, It is characterized in that The steps include: Step S1, preparing an electroplating solution using anhydrous copper sulfate, and placing the prepared electroplating solution in the plating solution circulation tank (7); Step S2, using an acetone solution to clean the copper round rod electrode (6), and then immersing the cleaned copper round rod electrode (6) in a deionized water solution for ultrasonic cleaning; Step S3, pasting a conductive film (22) and two insulating films (23) on the wax-coated film-pasting area of ​​the copper round rod electrode (6) after ultrasonic cleaning in step S2, wherein the two insulating films (23) are located at both ends of the conductive film (22); Step S4, installing the copper round rod electrode (6) obtained in step S3 between the driving component and the conductive component; Step S5, moving the nozzle (14) assembly to above the copper round rod electrode (6), with the nozzle (21) located above the conductive film (22), turning on the peristaltic pump (3), and allowing the electroplating solution prepared in step S1 to flow from the plating solution circulation tank (7) through the peristaltic pump (3) into the plating solution channel (20) at a flow rate of 12 ml / min to 15 ml / min; Step S6, start the driving component, the single chip microcomputer (12) controls the motor driver (11), the motor driver (11) controls the second stepping motor (9) to rotate at a speed of 120 rpm to 180 rpm, thereby driving the copper round rod electrode (6) to rotate; Step S7, turning on the voltage stabilizer (1), the voltage stabilizer (1) performs electrodeposition at a voltage of 3.8V, and at the same time turning on the stepper motor 1 (17), the moving axis moves along the Z direction, thereby driving the nozzle (14) assembly to be pulled along the Z direction, and the copper ion deposits are deposited on the conductive film (22) around the copper round rod electrode (6), and the deposition height of the copper ion deposits is h, and the range of h is 400μm to 800μm; Step S8, after step S7 is completed, remove the copper round rod electrode (6) with the copper ion deposit, and peel off the insulating film (23) and the copper ion deposit from the copper round rod electrode (6) in sequence; Step S9, placing the copper ion deposit peeled off in step S8 in a tube furnace, and performing annealing treatment under nitrogen protection, with the annealing temperature being 200° C. and the holding time being 30 min; Step S10, cooling the copper ion deposit after the annealing treatment in step S9, and the preparation of the O-ring is completed.