Crystal ingot facet area detection method for improving contrast ratio through lateral pressure stress
By applying lateral compressive stress and excitation light irradiation at a specific wavelength, combined with fluorescence signal analysis, the problem of low contrast in the detection area of the small faceted area of the silicon carbide ingot is solved, achieving a more accurate detection effect, and is suitable for the detection of a variety of materials.
Patent Information
- Application Number
- CN202411153297.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-08
AI Technical Summary
The prior art is difficult to accurately detect the small-faceted areas of silicon carbide ingots, mainly due to the small fluorescence brightness difference between the small-faceted areas and the non-faceted areas, resulting in low contrast, which affects the accuracy of detection.
通过施加侧向压应力,结合特定波长的激发光照射和荧光信号的分析,提高小面区域与非小面区域的荧光对比度,利用荧光的中心波长和强度区分两种区域。
It significantly improves the accuracy and reliability of small-faceted area detection, and is suitable for silicon carbide ingots and other materials with similar optical and mechanical properties, enhancing the accuracy and flexibility of detection.
Smart Images

Figure CN118914154A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of wafer processing technology, and in particular to a method for detecting a small facet area of a crystal ingot by improving contrast through lateral compressive stress. Background Art
[0002] The facet region of a silicon carbide ingot refers to a region inside or on the surface of a crystal with specific crystal plane orientation and structural characteristics. Usually, facet regions are formed during crystal growth due to local lattice defects, impurity accumulation, or other changes in growth regulation. The crystal structure of these regions is significantly different from the surrounding non-facet regions, and exhibits different physical and chemical properties.
[0003] During the growth of silicon carbide ingots, the inhomogeneity of conditions such as temperature, pressure, and airflow leads to changes in the crystal growth rate and direction, forming different crystal plane orientations; local temperature gradients also lead to the accumulation of stress inside the crystal, resulting in small face areas. In addition, lattice defects such as dislocations, twins, and grain boundaries can also lead to uneven crystal structures during crystal growth, and these defective areas often form small face areas.
[0004] The crystal orientation of the facet area is different from that of the non-facet area, and the non-facet area has a more uniform crystal orientation. Due to the difference in crystal orientation and structure, the facet area also differs from the non-facet area in terms of mechanical strength, hardness, elastic modulus, etc. In optics, due to the difference in refractive index and transmittance between the facet area and the non-facet area, in laser cracking, the depth of concentration of the femtosecond laser used in the ingot is different, and the light intensity will also be different, which causes the depth of the crack area to be different, and the length of the crack will also be different. By identifying the facet area, the processing parameters can be optimized to produce highly uniform cracks and improve the utilization rate of the ingot.
[0005] Patent CN111162017A (Small face area detection method and detection device, wafer production method and laser processing device) discloses the use of fluorescence brightness to detect small face areas. However, it can be seen from the relevant results that the difference in fluorescence brightness between the small face area and the non-small face area is small, resulting in a low contrast between the small face area and the non-small face area, which is not conducive to accurate detection of the small face area. Summary of the invention
[0006] In order to solve the above problems, the present invention provides a method for detecting a small facet area of a crystal ingot with improved contrast by lateral compressive stress, comprising the following steps: Step 1, applying lateral compressive stress to the ingot; Step 2, irradiating various areas of the surface of the ingot with excitation light, and collecting fluorescence from each area; Step 3: Determine the facet area based on the central wavelength and intensity of the fluorescence.
[0007] The core concept of the present invention is to utilize the introduction of lateral compressive stress, irradiate with excitation light and detect fluorescence signals to improve the contrast between the small facet area and the non-small facet area of the silicon carbide ingot, thereby achieving more accurate detection of the small facet area. Specifically, by applying lateral compressive stress to the silicon carbide ingot, the stress distribution inside the crystal changes: the small facet area and the non-small facet area have different responses to stress due to differences in crystal structure and defects. Excitation light of a specific wavelength is used to illuminate the surface of the ingot, and each area reflects fluorescence under the action of the excitation light. The intensity and central wavelength of the fluorescence signal are affected by the internal structure and stress state of the crystal. The fluorescence response of different areas is different. By collecting and analyzing the fluorescence signals of each area, especially the central wavelength and intensity, the small facet area and the non-small facet area can be distinguished.
[0008] Traditional fluorescence detection is difficult to distinguish faceted areas from non-faceted areas with high contrast. The present invention increases the difference in fluorescence signals between these areas by applying lateral compressive stress, significantly improving the contrast of detection. The present invention combines the central wavelength and intensity of fluorescence data to provide a more reliable judgment standard. Even if a single parameter is not sufficient to distinguish, comprehensive analysis of the two parameters can improve accuracy and reliability.
[0009] Furthermore, in step 1, a hydraulic system is used to apply lateral compressive stress to the ingot. Applying a hydraulic system to apply lateral compressive stress to the ingot has the advantages of high control accuracy, uniform pressure, and flexible adjustment. The hydraulic system can accurately control the applied pressure through a hydraulic pump and a control valve, and by adjusting the flow and pressure of the hydraulic oil, it is easy to apply a constant and controllable lateral compressive stress to the ingot. Since the hydraulic oil transmits the pressure, the stress on each part of the ingot is uniform, ensuring the detection accuracy and the structural integrity of the ingot.
[0010] Furthermore, the hydraulic system includes an annular hydraulic chamber, the outer wall of the annular hydraulic chamber is a rigid material, the inner wall of the annular hydraulic chamber is an elastic material, the annular hydraulic chamber encloses a cylindrical space, and the ingot is placed in the cylindrical space. In this way, the rigid outer wall ensures the structural stability of the annular hydraulic chamber during the pressure application process, avoiding deformation and pressure loss, while the elastic inner wall can evenly transfer the hydraulic pressure to the surface of the ingot to ensure that the applied lateral stress is evenly distributed. Such a structural component can accurately control the applied pressure, and can also effectively avoid local stress concentration and reduce the risk of damage to the ingot. In addition, the design of the annular hydraulic chamber simplifies the adaptation to ingots of different sizes and shapes, and improves the flexibility and versatility of the system.
[0011] Furthermore, a support portion is provided at the bottom of the annular space, and the support portion is porous silicon. Porous silicon has high compressibility and good mechanical properties, and can effectively buffer the impact force on the ingot when lateral compressive stress is applied, reducing stress concentration at the bottom of the ingot and potential damage risks. In addition, the porous structure of porous silicon helps to absorb and disperse pressure, further evenly distribute stress, and maintain the stability and integrity of the ingot. The ingot is adsorbed on the sample table, and porous silicon ensures that the position of the ingot is fixed and does not move during the entire detection process, which helps to improve detection accuracy and repeatability.
[0012] Furthermore, the lateral compressive stress is greater than 0.1 GPa and less than 1.0 GPa. Pressures below 0.1 GPa cannot significantly change the stress distribution in the ingot, making it difficult to improve the fluorescence contrast between the facet area and the non-facet area; pressures above 1.0 GPa are likely to cause irreversible plastic deformation or rupture of the ingot, damaging the ingot structure.
[0013] Furthermore, in step 2, the excitation light is ultraviolet light. Ultraviolet light has a high photon energy and can effectively excite electrons in the silicon carbide ingot, thereby generating a significant fluorescence signal. Silicon carbide is a wide bandgap semiconductor material, and the wavelength of ultraviolet light can well match the bandgap of silicon nitride material, thereby stimulating a strong fluorescence signal.
[0014] Furthermore, the excitation light is irradiated obliquely on the surface of the ingot. If the excitation light is irradiated vertically, it will cause strong surface reflection light, which will interfere with the collection of fluorescence signals; oblique irradiation can reduce the interference of surface reflection and ensure that the collected fluorescence signals are purer and more accurate.
[0015] Furthermore, the wavelength of the excitation light is 370 nanometers. Ultraviolet light of 370 nanometers has sufficient energy to excite electron transitions in the silicon carbide ingot and generate significant fluorescence signals.
[0016] Furthermore, in step 3, the central wavelength of the fluorescence in the facet region is blue-shifted relative to the central wavelength of the fluorescence in the non-facet region. When lateral compressive stress is applied to the ingot, the stresses on the facet region and the non-facet region are different: the facet region is subjected to greater stress, which affects the electronic energy level structure of the crystal, causing the lattice constant to change, making the electronic band gap larger, increasing the energy level spacing, and when the excited electrons transition from the conduction band to the valence band, the energy of the emitted fluorescent photons increases and the wavelength becomes shorter, that is, a blue shift occurs. In addition, the facet region has a smaller grain size and a stronger quantum confinement effect, which makes the electronic energy level spacing larger, resulting in a blue shift in the fluorescence wavelength.
[0017] Furthermore, in step 3, the intensity of the fluorescence in the facet region is less than that in the non-facet region. When lateral compressive stress is applied to the facet region, it is subjected to greater stress concentration than the non-facet region. This high stress concentration leads to aggravated lattice distortion, increased lattice defects and broken bonds, and thus significantly increased non-radiative recombination centers and reduced fluorescence intensity.
[0018] Beneficial effects of the present invention: (1) The present invention significantly improves the contrast between the small face area and the non-small face area by introducing lateral compressive stress and combining it with the analysis of the fluorescence center wavelength and intensity, thereby improving the accuracy of small face area detection.
[0019] (2) The method of the present invention is not only applicable to silicon carbide ingots, but can also be applied to other materials with similar optical and mechanical properties. By adjusting the excitation light wavelength and stress magnitude, it can be widely used in the detection and analysis of different materials.
[0020] Based on the above effects, the present invention has good application prospects in the field of wafer processing technology. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 Schematic diagram of a method for detecting a small facet area of an ingot using lateral compressive stress to enhance contrast.
[0022] Figure 2 is a schematic diagram of the annular hydraulic chamber.
[0023] In the figure: 1. annular hydraulic chamber; 2. supporting part; 3. ingot. DETAILED DESCRIPTION
[0024] In order to make the objectives, technical solutions and advantages of the present application more clearly understood, the present application is further described in detail below with reference to the accompanying drawings and examples.
[0025] The present invention provides a method for detecting a small facet area of a crystal ingot with improved contrast by lateral compressive stress, such as Figure 1 As shown, it includes 3 steps. To clearly illustrate the present invention, taking the small face area detection on the surface of silicon carbide ingot as an example, the 3 steps are respectively described as follows: Step 1: Apply lateral compressive stress to the ingot.
[0026] In this step, the ingot 3 is placed in the cylindrical space of the annular hydraulic chamber 1, as shown in FIG. Figure 2As shown, the depth of the annular hydraulic chamber 1 is greater than the height of the ingot 3, so as to facilitate the application of stress near the surface of the ingot 3. The outer wall of the annular hydraulic chamber 1 is made of rigid material, such as high-strength steel or titanium alloy. Rigid materials can withstand the huge pressure of high-pressure liquid to ensure that the annular hydraulic chamber 1 will not deform during operation. The outer wall of the annular hydraulic chamber 1 is a thick-walled structure to enhance its strength and durability. The thickness of the outer wall is calculated and designed according to the required maximum pressure to ensure its stability and reliability when lateral compressive stress is applied. The inner wall of the annular hydraulic chamber 1 is made of elastic material, such as silicone rubber or polyurethane. These materials have good elasticity and wear resistance, and can deform when pressure is applied, thereby uniformly transmitting the pressure to the ingot 3. The inner wall of the annular hydraulic chamber 1 is designed as a thin-walled structure so that it can be fully deformed and close to the surface of the ingot under pressure to ensure uniform pressure distribution. The annular hydraulic chamber 1 encloses a cylindrical space, and a support portion 2 is provided at the bottom of the annular space, and the support portion 2 is porous silicon. Porous silicon has high mechanical strength and good air permeability, and can reduce the overall weight and enhance the heat dissipation performance while providing support. In addition, the elastic modulus of porous silicon is low, which can buffer the pressure within a certain range and provide stable support. When used, the annular hydraulic chamber 1 is placed on the ceramic suction cup, and a negative pressure device is provided on the lower side of the ceramic suction cup. The negative pressure device inhales air, and the porous silicon can be ventilated, so that the entire device, especially the crystal ingot, is in an adsorbed state, which enhances the stability of the device. The hydraulic system consists of a hydraulic pump, a control valve, a hydraulic pipeline and an annular hydraulic chamber 1. The hydraulic pump provides power, adjusts the pressure through the control valve, and the hydraulic pipeline transmits the pressure to the annular hydraulic chamber 1. The liquid pressure acts on the inner wall of the annular hydraulic chamber 1, causing it to deform inward, thereby uniformly applying the lateral compressive stress to the surface of the crystal ingot. The control valve is used to adjust the pressure of the hydraulic system to ensure that the lateral compressive stress is greater than 0.1GPa and less than 1.0GPa, effectively changing the fluorescence characteristics of the crystal ingot 3 and improving the contrast between the small face area and the non-small face area. In addition, a pressure sensor is installed in the hydraulic system to monitor the pressure value in the annular hydraulic chamber 1 in real time. The data of the sensor is fed back to the control system to achieve accurate regulation and control of the pressure to avoid damage to the ingot caused by excessive or insufficient pressure.
[0027] Step 2: Excitation light illuminates various areas on the surface of the ingot, and collects fluorescence from each area.
[0028] In this step, a high-power UV LED or xenon lamp is used as a light source to provide stable, high-energy UV light. The 370-nanometer UV light is guided to the surface of the ingot through the optical path system, and the incident angle is between 30 degrees and 60 degrees. Irradiation at an inclined angle can reduce the reflection interference of light on the surface of the ingot and increase the absorption efficiency of light, thereby improving the intensity and clarity of the fluorescence signal. In addition, oblique irradiation helps to excite and collect deeper fluorescence signals and improve the detection ability of the internal structure and facet area of the ingot. Using a highly sensitive photomultiplier tube (PMT) or charge-coupled device (CCD) as a fluorescence detector can accurately capture and measure weak fluorescence signals. Equipped with a spectrum analyzer to analyze the collected fluorescence signals, measure the central wavelength and intensity of the fluorescence, and provide a fluorescence spectrum. Move the ingot so that the excitation light irradiates different areas of the ingot to obtain fluorescence signals in different areas. In this step, preliminary data processing is also included, that is, filtering out background noise, enhancing the signal, and obtaining clear fluorescence data.
[0029] Step 3: Determine the facet area based on the central wavelength and intensity of the fluorescence.
[0030] In this step, wavelength information is extracted from the fluorescence data, and the software is used to detect the peak of the fluorescence signal and calculate the central wavelength; the fluorescence intensity data is extracted, the intensity of each area is compared, and the area with lower intensity is identified. The wavelength and intensity data are converted into image form, and different areas are represented by color coding; the wavelength map and the intensity map are superimposed, and the image contrast is enhanced by image processing software to clearly identify the small face area. Among them, the central wavelength of the fluorescence in the small face area is blue-shifted relative to the central wavelength of the fluorescence in the non-small face area, and the intensity of the fluorescence in the small face area is less than the intensity of the fluorescence in the non-small face area. After that, the small face area is marked on the image. In the future, the splitting laser parameters will be optimized in the small face area to improve the wafer processing accuracy and the utilization rate of the ingot.
[0031] In summary, the present invention provides a method for detecting small face areas by improving contrast through lateral compressive stress, comprising the following steps: applying lateral compressive stress to the ingot, irradiating the surface of the ingot with excitation light and collecting fluorescence from various areas, and determining the small face area by the central wavelength and intensity of the fluorescence. The excitation light is ultraviolet light with a wavelength of 370 nanometers, which obliquely irradiates the surface of the ingot to enhance the fluorescence contrast between the small face area and the non-small face area. A hydraulic system is used to apply lateral compressive stress of 0.1 GPa to 1.0 GPa, and a high-sensitivity photomultiplier tube or charge-coupled device is used to collect and analyze fluorescence signals, thereby achieving accurate detection of small face areas, which has good application prospects in the field of wafer processing technology.
[0032] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application shall be included in the scope of protection of the present application.
Claims
1. A method for detecting a small facet area of an ingot with improved contrast by lateral compressive stress, It is characterized in that The steps include: Step 1, applying lateral compressive stress to the ingot; Step 2, irradiating various areas of the surface of the ingot with excitation light, and collecting fluorescence from each area; Step 3: Determine the facet area based on the central wavelength and intensity of the fluorescence.
2. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 1, Features: In step 1, a hydraulic system is used to apply lateral compressive stress to the ingot.
3. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 2, Features: The hydraulic system comprises an annular hydraulic chamber, the outer wall of the annular hydraulic chamber is made of rigid material, the inner wall of the annular hydraulic chamber is made of elastic material, the annular hydraulic chamber encloses a cylindrical space, and the ingot is placed in the cylindrical space.
4. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 3, Features: A supporting part is provided at the bottom of the annular space, and the supporting part is porous silicon.
5. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 4, Features: The lateral compressive stress is greater than 0.1 GPa and less than 1.0 GPa.
6. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 1, Features: In step 2, the excitation light is ultraviolet light.
7. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 6, Features: The excitation light obliquely illuminates the surface of the ingot.
8. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to claim 7, Features: The wavelength of the excitation light is 370 nanometers.
9. The method for detecting a small facet area of an ingot with improved contrast due to lateral compressive stress according to any one of claims 1 to 8, Features: In step 3, the central wavelength of the facet region fluorescence is blue-shifted relative to the central wavelength of the non-facet region fluorescence.