Fatigue simulation method and system based on crack growth rate
Through the fatigue simulation method based on crack propagation rate, the problem of discreteness of the aging structure life evaluation and prediction results of traditional methods is solved, and the precise fatigue cycle times and life of structural parts is evaluated, and the limitations of traditional methods are overcome. Improves the accuracy of fatigue performance evaluation.
Patent Information
- Application Number
- CN202411100554.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-08
AI Technical Summary
The traditional fatigue simulation prediction method cannot accurately evaluate the remaining life of aging structures with defects, and the prediction results are highly discrete, and the impacts of loading order and material properties cannot be taken into account, which limits its application potential, especially in the problem of metal fatigue failure. In this case, the concealment and randomness of the crack propagation stage make life expectancy difficult.
Fatigue simulation method based on crack propagation rate, by detecting the fracture toughness and initial crack length of the material, establishing a stress strength simulation model, and using finite element simulation software to perform crack propagation simulation, combining stress strength factor and crack propagation rate formula, calculate crack length changes , and determine whether the threshold value is exceeded to determine the number of failure cycles of the structural part.
It realizes accurate prediction of the number of fatigue cycles of structural parts, provides a more refined crack propagation rate simulation, can accurately evaluate the remaining life of structural parts, overcomes the limitations of traditional methods, and improves the accuracy of fatigue performance evaluation.
Smart Images

Figure CN118917152A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of fatigue simulation, and in particular to a fatigue simulation method and system based on crack growth rate. Background Art
[0002] Traditional fatigue simulation prediction methods are mainly based on inputting SN or EN curves. The introduction and development of such methods have played a positive role in improving traditional structural types and reducing accident rates. However, their inherent theoretical defects have greatly limited their further application potential, such as: they are not suitable for the remaining life assessment of aging structures with existing defects; the prediction results are relatively discrete; the effects of loading sequence and material properties cannot be taken into account; it is precisely because of the many limitations of the SN curve method that the application of fracture mechanics in engineering fatigue assessment has become more and more urgent. The metal fatigue failure problem is a key performance indicator of automotive parts, which is generally divided into three stages: fatigue crack initiation, fatigue crack propagation and final failure. Since many parts (such as the front axle of commercial vehicles) do not have high requirements for the surface quality of parts, there are some tiny cracks in the parts themselves. The main stage that determines the fatigue life of such parts is the fatigue crack propagation stage. Fracture toughness is an important parameter for evaluating the crack propagation rate, which determines the speed of the crack propagation rate and is mainly obtained through V-mouth impact test. Crack propagation is easily affected by loads and material microstructures due to its concealment and randomness, which makes it impossible to accurately describe it quantitatively, which also affects life prediction and is one of the core issues restricting material service reliability. Therefore, it is necessary to reasonably evaluate the fatigue performance of the structure based on the method of fracture mechanics and accurately predict the fatigue residual life of the structural node through the method of crack propagation. Summary of the invention
[0003] In order to solve the above technical problem or at least partially solve the above technical problem, the present invention provides a fatigue simulation method and system based on crack growth rate.
[0004] In a first aspect, the present invention provides a fatigue simulation method based on crack growth rate, comprising: detecting the fracture toughness and initial crack length of the material used for the structural part, and determining the crack threshold according to the crack length when the fracture toughness preset material fails;
[0005] Establish a stress intensity simulation model for structural parts, configure the corresponding stress ratio and load for the structural parts according to the fatigue cycle requirements, and configure the elastic modulus, Poisson's ratio, yield strength, and tensile strength parameters of the materials used for the structural parts to perform stress intensity simulation calculations to determine the stress intensity factor and stress intensity factor range;
[0006] Based on the ODB file of the stress intensity simulation calculation results and the preset crack growth rate formula, the crack growth simulation under fatigue cycle is carried out in the finite element simulation software. During the crack growth simulation, the initial crack length and fracture toughness parameters of the material are provided, and the crack growth rate after each fatigue cycle is calculated and output using the crack growth rate formula. The crack growth rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle.
[0007] Determine whether there is a crack length exceeding the crack threshold in the structural part. If there is a crack length exceeding the crack threshold, it is determined that the structural part has failed and the final number of fatigue cycles is obtained. If it does not exceed the threshold, increase the number of fatigue cycles and continue the simulation.
[0008] Furthermore, the preset crack growth rate formula is as follows:
[0009]
[0010] Where a is the crack length, N is the number of fatigue cycles; Δk is the stress intensity factor range; v0 is the crack growth rate when the material fails under ideal conditions, σ b is the tensile strength of the material used for the structural part, E is the elastic modulus of the material used for the structural part, α is the strength sensitivity coefficient of the material used for the structural part, indicating that the critical fatigue crack growth rate is proportional to the tensile strength, R is the stress ratio of the structural part, k IC is the fracture toughness of the material used for the structural part, and m is a constant related to the material used for the structural part.
[0011] Furthermore, the crack threshold is determined based on the crack length at which the fracture toughness preset material fails, including:
[0012] Among them, a max is the maximum value of the crack threshold, the crack threshold does not exceed a max , σ is stress, Y(θ) is the geometric correction factor related to the crack direction and stress direction, θ is the angle between the crack direction and the stress direction, k IC Fracture toughness of materials used for structural parts.
[0013] Furthermore, before crack propagation, the ODB file based on the minimum strain energy density criterion and stress intensity simulation calculation results determines whether crack propagation will occur, including:
[0014] Calculate the strain energy density factor S(θ,v,E,k) per unit volume at the crack tip based on the crack type of the structural component. C), where θ is the angle between the crack direction and the stress direction, v is the Poisson's ratio of the material used for the structural component, E is the elastic modulus of the material used for the structural component, C is the crack type parameter, which has 7 values, representing any combination of type I, II and III cracks, and k C stress intensity factors related to crack type parameters;
[0015] Determine whether the minimum strain energy density factor reaches the critical value of the strain energy density factor. If so, it is determined that the crack will expand, and the crack expansion is controlled along the distribution position of the minimum strain energy density factor. The crack expansion speed is controlled according to the crack expansion rate formula.
[0016] Furthermore, during the simulation process, the crack propagation is controlled based on the crack propagation rate and crack propagation direction, the crack is updated based on the crack propagation situation on the basis of the structural component model, and the crack mesh is refined to generate a crack length distribution cloud map after each fatigue cycle process, and the relationship between the number of fatigue cycles and the change in crack length is generated.
[0017] Furthermore, the crack mesh unit at the crack tip is set as a singular unit, the crack surface is set as an embedded element, and the mesh is refined near the crack tip so that the stress at the crack node acquires singularity. The degree of network refinement near the tip is determined by gradually refining and verifying that the crack extension result corresponding to the degree of refinement converges.
[0018] Furthermore, before modeling, the crack distribution of the structural parts is statistically analyzed, and initial cracks are added to the model of the constructed structural parts according to the crack distribution.
[0019] Furthermore, under various working conditions of the structural parts, strain sensors are set to record the load and stress ratio of the structural parts in the fatigue cycle. During simulation, based on the Abaqus software, the stress ratio and load under various working conditions are input into the structural part model through the boundary condition module to simulate the fatigue cycle under the corresponding working conditions.
[0020] In a second aspect, the present invention provides a fatigue simulation device based on crack growth rate, characterized in that it comprises: at least one processing unit, the processing unit is connected to a storage unit via a bus unit, the storage unit stores a computer program, and the processing unit executes the computer program to implement the fatigue simulation method based on crack growth rate.
[0021] In a third aspect, the present invention provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program, wherein when the computer program is executed by a processor, the fatigue simulation method based on crack propagation rate is implemented.
[0022] The above technical solution provided by the embodiment of the present invention has the following advantages compared with the prior art:
[0023] This application detects the fracture toughness and initial crack length of the structural material, and presets the crack threshold; establishes a stress strength simulation model for the structural part, configures the corresponding stress ratio and load for the structural part according to the fatigue cycle requirements, and configures the parameters of the material used for the structural part to perform stress strength simulation calculations; based on the ODB file of the stress strength simulation calculation results and the preset crack growth rate formula, performs crack growth simulation calculations in the finite element simulation software and outputs the crack growth rate after each fatigue cycle. The crack growth rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle; determines whether the structural part has a crack length exceeding the crack threshold. If so, it is determined that the structural part has failed, and the final number of fatigue cycles is obtained. If not, the number of fatigue cycles is increased and the simulation continues. This application provides a more sophisticated crack growth rate formula in the finite element software than the Paris crack growth calculation method, which can simulate the crack growth rate more accurately. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0026] Figure 1 A flowchart of a fatigue simulation method based on crack growth rate provided in an embodiment of the present application;
[0027] Figure 2 A schematic diagram of a crack length distribution cloud map provided in an embodiment of the present application;
[0028] Figure 3 A schematic diagram of the variation of crack length with fatigue cycle number provided in the embodiment of the present application;
[0029] Figure 4 A schematic diagram of a fatigue simulation device based on crack growth rate provided in an embodiment of the present application. DETAILED DESCRIPTION
[0030] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0031] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.
[0032] Example 1
[0033] See also Figure 1 As shown, an embodiment of the present invention provides a fatigue simulation method based on crack growth rate, comprising:
[0034] The fracture toughness and initial crack length of the materials used in the structural parts are tested, and the crack threshold is determined based on the crack length when the fracture toughness preset material fails.
[0035] In the specific implementation process, the crack threshold is determined according to the crack length when the fracture toughness preset material fails, including:
[0036] Among them, a max is the maximum value of the crack threshold, the crack threshold does not exceed a max , σ is stress, Y(θ) is the geometric correction factor related to the crack direction and stress direction, θ is the angle between the crack direction and the stress direction, k IC Fracture toughness of materials used for structural parts.
[0037] Configure crack thresholds into drawing requirements.
[0038] A stress intensity simulation model of structural parts is established in Abaqus software. The corresponding stress ratio and load are configured for the structural parts according to the fatigue cycle requirements. The elastic modulus, Poisson's ratio, yield strength and tensile strength parameters of the materials used for the structural parts are also configured to perform stress intensity simulation calculations to determine the stress intensity factor and stress intensity factor range.
[0039] The fatigue cycle of the structural parts is designed based on the working conditions of the structural parts. In the specific implementation process, under various working conditions of the structural parts, the load and stress ratio of the structural parts in the fatigue cycle are recorded by setting strain sensors. During the simulation, based on the Abaqus software, the stress ratio and load under various working conditions are input into the structural part model through the boundary condition module to simulate the fatigue cycle under the corresponding working conditions. If the working conditions of the structural parts show a periodic pattern, the fatigue cycle is designed according to the load and stress ratio in a cycle.
[0040] Before modeling in the finite element simulation software, the crack distribution of the structural parts is statistically analyzed, and initial cracks are added to the model of the constructed structural parts according to the crack distribution, and the length of the initial cracks is configured.
[0041] Before crack propagation, the ODB file based on the minimum strain energy density criterion and stress intensity simulation calculation results determines whether crack propagation will occur, including:
[0042] Calculate the strain energy density factor S(θ,v,E,k) per unit volume at the crack tip based on the crack type of the structural component. C ), where θ is the angle between the crack direction and the stress direction, v is the Poisson's ratio of the material used for the structural component, E is the elastic modulus of the material used for the structural component, C is the crack type parameter, which has 7 values, representing any combination of type I, II and III cracks, and k C stress intensity factors related to crack type parameters;
[0043] Determine whether the minimum strain energy density factor reaches the critical value of the strain energy density factor. If so, it is determined that the crack will expand, and the crack expansion is controlled along the distribution position of the minimum strain energy density factor. The crack expansion speed is controlled according to the crack expansion rate formula.
[0044] During the specific implementation process, the strain energy density factor is related to the type of cracks, including seven situations: single type cracks of type I, II and III, type III composite cracks, type IIII composite cracks, type IIII composite cracks and type IIIIII composite cracks.
[0045] The strain energy density factor of type III composite crack is taken as an example for explanation.
[0046] S=ω1(E,v,θ)(k I ) 2 +ω2(E,v,θ)k I k II +ω3(E,v,θ)(k II ) 2 ,in,
[0047] ω1(E,v,θ),ω2(E,v,θ),ω3(E,v,θ) are the angles between the crack direction and the stress direction, v is the Poisson's ratio of the material used for the structural component, E is the coefficient related to the elastic modulus of the material used for the structural component, and k I is the stress intensity factor of type I crack, k II is the stress intensity factor of type II crack.
[0048] After determining that the crack will expand, the crack expansion simulation of the structural component under fatigue cycle is carried out in the finite element simulation software based on the ODB file of the stress intensity simulation calculation results and the preset crack expansion rate formula. During the crack expansion simulation, the initial crack length and fracture toughness parameters of the material are provided, and the crack expansion rate after each fatigue cycle is calculated and output using the crack expansion rate formula. The crack expansion rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle.
[0049] During the specific implementation, the preset crack growth rate formula is as follows:
[0050]
[0051] Where a is the crack length, N is the number of fatigue cycles; Δk is the stress intensity factor range; v0 is the crack growth rate when the material fails under ideal conditions, σ b is the tensile strength of the material used for the structural part, E is the elastic modulus of the material used for the structural part, α is the strength sensitivity coefficient of the material used for the structural part, indicating that the critical fatigue crack growth rate is proportional to the tensile strength, R is the stress ratio of the structural part, k IC is the fracture toughness of the material used for the structural part, and m is a constant related to the material used for the structural part.
[0052] During the simulation, the crack propagation is controlled based on the crack propagation rate and crack propagation direction. The crack is updated based on the crack propagation situation on the basis of the structural component model, and the crack mesh is refined to generate a crack length distribution cloud map after each fatigue cycle process, and the relationship between the number of fatigue cycles and the change in crack length is generated. In the process of updating the crack and refining the crack network, the crack mesh unit at the crack tip is set as a singular unit, the crack surface is set as an embedded element, and the mesh is refined near the crack tip so that the stress at the crack node obtains singularity. The method for determining the degree of network refinement near the tip is to verify the convergence of the crack propagation results corresponding to the degree of refinement through step-by-step refinement.
[0053] Determine whether there is a crack in the structural component module and whether its length exceeds the crack threshold. If there is a crack whose length exceeds the crack threshold, it is determined that the structural component has failed and the final number of fatigue cycles is obtained. If it does not exceed, increase the number of fatigue cycles and continue the simulation.
[0054] The present application will be described using an example in which the structural member is a front axle of a commercial vehicle.
[0055] Step 1: The material used for the front axle of the commercial vehicle is 42CrMo, the yield strength of 42CrMo is 760Mpa, the tensile strength of 42CrMo is 1050Mpa, the elastic modulus of 42CrMo is 210Gpa, and the Poisson's ratio of 42CrMo is 0.3. After testing and calculation, the fracture toughness of 42CrMo is 3200Mpa·m 0.5 After nondestructive testing, the length of the initial cracks was less than 0.01mm. When the parts are in use, cracks larger than 0.02mm are not allowed, otherwise the front axle of the commercial vehicle is judged to be failed, that is, the crack threshold is set to 0.02mm.
[0056] When a commercial vehicle is fully loaded and braking or going downhill, the load or stress on the front axle of the commercial vehicle is more obvious than in other working conditions. Therefore, the fatigue cycle of the front axle of a commercial vehicle is designed according to the extreme working conditions of full-load extreme braking or full-load downhill.
[0057] Step 2: According to the working conditions of the commercial vehicle under extreme braking on flat ground when fully loaded, the load and stress ratio of the front axle are recorded by attaching strain gauges, and the fatigue cycle is designed. Based on the Abaqus software, the stress ratio and load are input into the stress strength simulation model of the front axle of the commercial vehicle through the boundary condition module, and the fully loaded extreme braking condition is simulated, the stress distribution of the front axle is calculated, and the stress ratio of each node is output.
[0058] Step 3: Based on the ODB file of the stress intensity simulation calculation results in step 2, use Python to write a secondary development post-processing plug-in to develop the crack extension formula into the finite element software. The crack extension formula is as follows:
[0059]
[0060] Where a is the crack length, Δk is the stress intensity factor range, v0 is the crack growth rate when the material fails under ideal conditions, σ b is the tensile strength, E is the elastic modulus, α is the strength sensitivity coefficient of the material, indicating that the critical fatigue crack growth rate is proportional to the tensile strength, R is the stress ratio, N is the number of fatigue cycles, k IC is the fracture toughness, and m is a constant related to the material.
[0061] Based on the crack situation of the front axle of a commercial vehicle in the finite element method, the initial crack length is input into the script as 0.01mm and the fracture toughness is 3200Mpa·m. 0.5, v0 is set to 1mm / cycle, m is set to 3, α is set to -760Mpa, and the stress ratio is set to correspond to the node in step 2. Run the script, continuously increase the number of fatigue cycles, and output the change in crack length after each fatigue cycle, and integrate to obtain the crack length of the crack.
[0062] Step 4: Based on the calculation results of step 3, determine whether the crack length exceeds the crack threshold of 0.02 mm. If not, return to step 3 and continue to increase the fatigue times. If it exceeds, it is determined to be a failure. Figure 2 Shown is the crack length distribution cloud diagram after failure.
[0063] Step 5: Output the fatigue cycle number, crack length and other results, such as Figure 3 Shown is the fatigue life curve of the maximum point in the crack length distribution cloud diagram. After 3.5 million cycles, the crack length at the maximum point reaches 0.02008mm, which indicates that the service life of the front axle is 3.5 million times.
[0064] Example 2
[0065] An embodiment of the present invention provides a fatigue simulation device based on crack growth rate, comprising: at least one processing unit, the processing unit is connected to a storage unit via a bus unit, the storage unit stores a computer program, and the processing unit executes the computer program to implement the fatigue simulation method based on crack growth rate, comprising:
[0066] Test the fracture toughness and initial crack length of the materials used in the structural parts, and determine the crack threshold based on the crack length when the fracture toughness preset material fails;
[0067] Establish a stress intensity simulation model for structural parts, configure the corresponding stress ratio and load for the structural parts according to the fatigue cycle requirements, and configure the elastic modulus, Poisson's ratio, yield strength, and tensile strength parameters of the materials used for the structural parts to perform stress intensity simulation calculations to determine the stress intensity factor and stress intensity factor range;
[0068] Based on the ODB file of the stress intensity simulation calculation results and the preset crack growth rate formula, the crack growth simulation under fatigue cycle is carried out in the finite element simulation software. During the crack growth simulation, the initial crack length and fracture toughness parameters of the material are provided, and the crack growth rate after each fatigue cycle is calculated and output using the crack growth rate formula. The crack growth rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle.
[0069] Determine whether there is a crack length exceeding the crack threshold in the structural part. If there is a crack length exceeding the crack threshold, it is determined that the structural part has failed and the final number of fatigue cycles is obtained. If it does not exceed the threshold, increase the number of fatigue cycles and continue the simulation.
[0070] Of course, the computer program stored in the storage unit of a fatigue simulation device based on crack growth rate provided in an embodiment of the present invention is not limited to the method operations described above, and can also execute related operations in a fatigue simulation method based on crack growth rate provided in any embodiment of the present invention.
[0071] Example 3
[0072] An embodiment of the present invention provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program, and when the computer program is executed by a host computer and a hardware-in-the-loop simulation test platform, the fatigue simulation method based on crack growth rate is implemented, including:
[0073] Test the fracture toughness and initial crack length of the materials used in the structural parts, and determine the crack threshold based on the crack length when the fracture toughness preset material fails;
[0074] Establish a stress intensity simulation model for structural parts, configure the corresponding stress ratio and load for the structural parts according to the fatigue cycle requirements, and configure the elastic modulus, Poisson's ratio, yield strength, and tensile strength parameters of the materials used for the structural parts to perform stress intensity simulation calculations to determine the stress intensity factor and stress intensity factor range;
[0075] Based on the ODB file of the stress intensity simulation calculation results and the preset crack growth rate formula, the crack growth simulation under fatigue cycle is carried out in the finite element simulation software. During the crack growth simulation, the initial crack length and fracture toughness parameters of the material are provided, and the crack growth rate after each fatigue cycle is calculated and output using the crack growth rate formula. The crack growth rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle.
[0076] Determine whether there is a crack length exceeding the crack threshold in the structural part. If there is a crack length exceeding the crack threshold, it is determined that the structural part has failed and the final number of fatigue cycles is obtained. If it does not exceed the threshold, increase the number of fatigue cycles and continue the simulation.
[0077] A computer-readable storage medium provided in an embodiment of the present invention stores a computer program which is not limited to the method operations described above, but can also execute related operations in a fatigue simulation method based on crack growth rate provided in any embodiment of the present invention.
[0078] In the embodiments provided by the present invention, it should be understood that the disclosed devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic. For example, the description division of the circuit is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling shown or discussed can be indirect coupling through some interfaces, devices or units, which can be electrical, mechanical or other forms.
[0079] The foregoing is merely a specific embodiment of the present invention, which enables those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features claimed herein.
Claims
1. A fatigue simulation method based on crack growth rate, It is characterized in that include: Test the fracture toughness and initial crack length of the materials used in the structural parts, and determine the crack threshold based on the crack length when the fracture toughness preset material fails; Establish a stress intensity simulation model for structural parts, configure the corresponding stress ratio and load for the structural parts according to the fatigue cycle requirements, and configure the elastic modulus, Poisson's ratio, yield strength, and tensile strength parameters of the materials used for the structural parts to perform stress intensity simulation calculations to determine the stress intensity factor and stress intensity factor range; Based on the ODB file of the stress intensity simulation calculation results and the preset crack growth rate formula, the crack growth simulation under fatigue cycle is carried out in the finite element simulation software. During the crack growth simulation, the initial crack length and fracture toughness parameters of the material are provided, and the crack growth rate after each fatigue cycle is calculated and output using the crack growth rate formula. The crack growth rate is integrated with the number of fatigue cycles to obtain the crack length after each fatigue cycle. Determine whether there is a crack length exceeding the crack threshold in the structural part. If there is a crack length exceeding the crack threshold, it is determined that the structural part has failed and the final number of fatigue cycles is obtained. If it does not exceed the threshold, increase the number of fatigue cycles and continue the simulation.
2. According to the fatigue simulation method based on crack growth rate of claim 1, It is characterized in that The preset crack growth rate formula is as follows: Where a is the crack length, N is the number of fatigue cycles; Δk is the stress intensity factor range; v 0 is the crack growth rate when the material fails under ideal conditions, σ b is the tensile strength of the material used for the structural part, E is the elastic modulus of the material used for the structural part, α is the strength sensitivity coefficient of the material used for the structural part, indicating that the critical fatigue crack growth rate is proportional to the tensile strength, R is the stress ratio of the structural part, k IC is the fracture toughness of the material used for the structural part, and m is a constant related to the material used for the structural part.
3. According to the fatigue simulation method based on crack growth rate of claim 1, It is characterized in that Determining the crack threshold based on the fracture toughness preset crack length at material failure includes: Among them, a max is the maximum value of the crack threshold, the crack threshold does not exceed a max , σ is stress, Y(θ) is the geometric correction factor related to the crack direction and stress direction, θ is the angle between the crack direction and the stress direction, k IC Fracture toughness of materials used for structural parts.
4. According to the fatigue simulation method based on crack growth rate of claim 1, It is characterized in that Before crack propagation, the ODB file based on the minimum strain energy density criterion and stress intensity simulation calculation results determines whether crack propagation will occur, including: Calculate the strain energy density factor S(θ,v,E,k) per unit volume at the crack tip based on the crack type of the structural component. C ), where θ is the angle between the crack direction and the stress direction, v is the Poisson's ratio of the material used for the structural component, E is the elastic modulus of the material used for the structural component, C is the crack type parameter, which has 7 values, representing any combination of type I, II and III cracks, and k C stress intensity factors related to crack type parameters; Determine whether the minimum strain energy density factor reaches the critical value of the strain energy density factor. If so, it is determined that the crack will expand, and the crack expansion is controlled along the distribution position of the minimum strain energy density factor. The crack expansion speed is controlled according to the crack expansion rate formula.
5. According to the fatigue simulation method based on crack growth rate of claim 4, It is characterized in that During the simulation process, the crack propagation is controlled based on the crack propagation rate and crack propagation direction. The crack is updated based on the crack propagation situation on the basis of the structural component model, and the crack mesh is refined to generate a crack length distribution cloud map after each fatigue cycle process, and generate the relationship between the number of fatigue cycles and the change in crack length.
6. According to the fatigue simulation method based on crack growth rate of claim 5, It is characterized in that The crack mesh unit at the crack tip is set as a singular unit, the crack surface is set as an embedded element, and the mesh is refined near the crack tip to make the stress at the crack node singular. The degree of network refinement near the tip is determined by gradually refining and verifying that the crack extension result corresponding to the degree of refinement converges.
7. The fatigue simulation method based on crack growth rate according to claim 1, It is characterized in that Before modeling the structural parts in the finite element simulation software, the crack distribution of the structural parts is statistically analyzed, and initial cracks are added to the model of the constructed structural parts according to the crack distribution.
8. The fatigue simulation method based on crack growth rate according to claim 1, It is characterized in that Under various working conditions of the structural parts, strain sensors are set to record the load and stress ratio of the structural parts in the fatigue cycle. During simulation, based on the Abaqus software, the stress ratio and load under various working conditions are input into the structural part model through the boundary condition module to simulate the fatigue cycle under the corresponding working conditions.
9. A fatigue simulation device based on crack growth rate, It is characterized in that include: At least one processing unit, the processing unit is connected to the storage unit via a bus unit, the storage unit stores a computer program, and the processing unit executes the computer program to implement the fatigue simulation method based on crack growth rate described in any one of claims 1-8.
10. A computer-readable storage medium storing a computer program, It is characterized in that When the computer program is executed by a processor, the fatigue simulation method based on crack growth rate as described in any one of claims 1 to 8 is implemented.