Experimental system and method for melting and solidification characteristics of lead-bismuth alloy
By designing a multi-module lead-bismuth alloy melting and solidification characteristic experimental system, efficient heating and cooling is achieved using inert gas, electrical heating, thermal oil and air modules, the existing system cannot generate high temperature gradients and lack of regulation capabilities, and achieves the problem of efficient heating and cooling. Efficient study on the melting and solidification characteristics of lead-bismuth alloys was carried out.
Patent Information
- Application Number
- CN202410982419.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-11-08
AI Technical Summary
The existing experimental system for melting and solidification characteristics of lead-bismuth alloys cannot generate a higher temperature gradient, and lacks stable feedback function and regulation capabilities, making it difficult to meet the demand for the safety of reactors in the study of the melting and solidification characteristics of lead-bismuth alloys under different temperature gradients.
A lead-bismuth alloy melting and solidification characteristics experimental system including injection module, experimental module, thermal oil module, air module, heating module and signal processor is designed, using an inert gas bottle, an electric heating rod, a thermal oil pump, an air compressor and Various sensors can achieve efficient heating and cooling through valve control, and can adjust system parameters at an efficiency of 15°C/min.
A high-efficiency lead-bismuth alloy melting and solidification stress experiment was achieved, and the system parameters were adjusted easily and quickly, and the stress characteristics of lead-bismuth alloys on fuel elements can be studied under different heating and cooling methods.
Smart Images

Figure CN118919106A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a lead-bismuth fast reactor thermal hydraulic verification experimental system and method, and in particular to a lead-bismuth alloy melting and solidification characteristic experimental system and method. Background Art
[0002] The lead-cooled fast reactor is one of the six types of fourth-generation reactors. Lead-bismuth alloy has many advantages as a coolant for the reactor. For example, lead-bismuth alloy has a high boiling point, which prevents boiling from occurring in the reactor and makes it difficult for heat transfer to deteriorate, effectively improving the operating range and safety limits of the reactor. Lead-bismuth alloy has stable chemical properties and will not undergo violent chemical reactions with water or air, greatly simplifying the handling of coolant leakage accidents and improving the economy and safety of the reactor. Lead-bismuth alloy has a large neutron elastic scattering cross-section and a short neutron mean free path, so the neutron leakage rate is low and the reflection effect is good, making it easier to design into a small modular reactor. However, as a liquid metal, lead-bismuth alloy is in solid state at room temperature. Therefore, for some special mobile small reactors, if lead-bismuth alloy is always placed in a primary circuit, the reactor will experience a phase change process during start-up, shutdown and accident conditions. During this process, lead-bismuth alloy will produce stress on the internal components of the reactor, especially thinner pipes such as fuel elements and steam generator heat transfer tubes. Therefore, studying the melting and solidification characteristics of lead-bismuth alloy under different temperature gradients is crucial to the safety of lead-bismuth fast reactors.
[0003] The existing lead-bismuth alloy melting and solidification characteristics experimental system is mainly used to study the influence of lead-bismuth alloy on the stress of components when melting or solidifying under different temperature gradients. The experimental system does not have complete measurement means and equipment to generate high temperature gradients, and it is difficult to meet the requirements of having stable feedback function and adjustment ability. Summary of the invention
[0004] The purpose of the present invention is to solve the technical problems that the existing lead-bismuth alloy melting and solidification characteristics experimental system does not have complete measurement means and cannot produce a high temperature gradient, and it is difficult to meet the requirements of stable feedback function and adjustment ability, and to provide a lead-bismuth alloy melting and solidification characteristics experimental system and method.
[0005] In order to achieve the above object, the present invention adopts the following technical solution:
[0006] A lead-bismuth alloy melting and solidification characteristics experimental system, which is special in that it includes an injection module, an experimental module, a heat transfer oil module, an air module, a heating module, a collection board and a signal processor;
[0007] The injection module includes an inert gas bottle and a lead-bismuth alloy storage tank connected to the inert gas bottle; a first pressure sensor is arranged on the outlet pipeline of the inert gas bottle; a second pressure sensor and a first temperature sensor are arranged on the lead-bismuth alloy storage tank; a third valve is arranged on the pipeline between the inert gas bottle and the lead-bismuth alloy storage tank;
[0008] The experimental module includes an experimental tank, a third pressure sensor, a second temperature sensor, a plurality of electric heating rods and a liquid level sensor arranged on the experimental tank; the experimental tank is a sandwich structure, and the sandwich is used to introduce compressed air or heat transfer oil; the inlet of the experimental tank is connected to the outlet of the lead-bismuth alloy storage tank, and a first valve is arranged on the pipeline between the inlet of the experimental tank and the outlet of the lead-bismuth alloy storage tank; a fifth pressure sensor and a fourth temperature sensor are arranged at the inlet of the sandwich of the experimental tank, the inlet of the sandwich of the experimental tank is respectively connected to the outlet of the heat transfer oil module and the outlet of the air module, and a fifth valve is arranged between the inlet of the sandwich of the experimental tank and the outlet of the air module, and a sixth valve is arranged between the inlet of the sandwich of the experimental tank and the outlet of the heat transfer oil module; the outlet of the sandwich of the experimental tank is connected to the inlet of the heat transfer oil module, the outlet of the sandwich of the experimental tank is provided with a sixth pressure sensor and a fifth temperature sensor, and a seventh valve is arranged on the pipeline between the outlet of the sandwich of the experimental tank and the inlet of the heat transfer oil module; an eighth valve for exhaust is arranged on the pipeline between the seventh valve and the outlet of the sandwich of the experimental tank;
[0009] The electric heating rod is provided with a strain gauge, which is used to obtain the stress characteristics of the wall surface of the electric heating rod when the lead-bismuth alloy melts and solidifies;
[0010] The heating module is arranged outside the lead-bismuth alloy storage tank, the experimental tank and all pipelines;
[0011] All pressure sensors, temperature sensors, strain gauges, heating modules and liquid level sensors are connected to the signal processor through acquisition boards.
[0012] Furthermore, the thermal oil module includes a high-temperature oil pump, a high-temperature thermal oil tank, a blast-type radiator and a heater;
[0013] The inlet of the high-temperature oil pump is connected to the outlet of the high-temperature thermal oil tank, the outlet of the high-temperature oil pump is connected to the inlet of the heater, and a first flow meter is provided on the pipeline between the outlet of the high-temperature oil pump and the inlet of the heater; the outlet of the heater is connected to the interlayer inlet of the experimental tank through a sixth valve;
[0014] The inlet of the blast type radiator is connected to the outlet of the interlayer of the experimental tank through the seventh valve, and the outlet of the blast type radiator is connected to the inlet of the high temperature thermal oil tank;
[0015] The high temperature oil pump, heater, interlayer of the experimental tank, blast radiator and high temperature heat transfer oil tank form a heat transfer oil circuit;
[0016] The blast radiator is used to cool the thermal oil;
[0017] The heater is used to increase the temperature of the thermal oil.
[0018] Further, the air module includes an air compressor and a gas storage tank;
[0019] The inlet of the air compressor is connected to the external atmosphere, and the outlet is connected to the inlet of the gas storage tank; the air compressor is used to fill the gas storage tank with compressed air;
[0020] A fourth pressure sensor and a third temperature sensor are provided on the gas storage tank; the outlet of the gas storage tank is connected to the interlayer inlet of the experimental tank through a fifth valve, and a second flow meter is provided on the pipeline between the fifth valve and the outlet of the gas storage tank.
[0021] Furthermore, the invention also includes a heat preservation unit;
[0022] The heat preservation unit includes a heat preservation layer wrapped around the heating module;
[0023] The test tank is provided with a check valve, which is used to discharge the excess gas in the test tank;
[0024] The outlet of the inert gas bottle is connected to the gas inlet of the experimental tank, and a fourth valve is provided on the pipeline between the inert gas bottle and the gas inlet of the experimental tank, which is used to fill the experimental tank with inert gas to protect the lead-bismuth alloy in the experimental tank;
[0025] A heating rod is provided in the high-temperature thermal oil tank;
[0026] A second valve is provided on the lead-bismuth alloy storage tank, and the second valve is used to discharge excess gas in the lead-bismuth alloy storage tank.
[0027] Furthermore, the inert gas bottle is a high-purity argon gas bottle;
[0028] The heating module adopts electric heating wire.
[0029] The experimental method for studying the melting and solidification characteristics of lead-bismuth alloy is characterized in that it includes a melting characteristic experiment of lead-bismuth alloy and a solidification characteristic experiment of lead-bismuth alloy;
[0030] The lead-bismuth alloy melting characteristics experiment is A experiment or B experiment:
[0031] A experiment includes the following steps:
[0032] A1] Use the heating module to preheat the lead-bismuth alloy storage tank, experimental tank and all pipelines;
[0033] A2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank changes from solid to liquid, the first valve and the third valve are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank is added into the experimental tank using an inert gas bottle, the first valve and the third valve are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank;
[0034] A3] When the temperature of the lead-bismuth alloy in the test tank drops below 50°C, turn on the multiple electric heating rods in the test tank to continue heating the lead-bismuth alloy until the lead-bismuth alloy is completely melted;
[0035] A4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod, obtain the stress characteristics of the wall of the electric heating rod when the lead-bismuth alloy is melted, complete the lead-bismuth alloy melting characteristic experiment, and turn off the electric heating rod;
[0036] Experiment B includes the following steps:
[0037] B1] Use the heating module to preheat the lead-bismuth alloy storage tank, experimental tank and all pipelines;
[0038] B2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank changes from solid to liquid, the first valve and the third valve are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank is added into the experimental tank using an inert gas bottle, the first valve and the third valve are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank;
[0039] B3] When the temperature of the lead-bismuth alloy in the experimental tank drops below 50°C, the sixth valve and the seventh valve are opened, the heat transfer oil module is turned on, and the lead-bismuth alloy in the experimental tank is continuously heated, and the temperature of the heat transfer oil in the heat transfer oil module is maintained to be greater than or equal to 200°C until the lead-bismuth alloy in the experimental tank is completely melted;
[0040] B4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod, obtain the stress characteristics of the wall of the electric heating rod when the lead-bismuth alloy melts, complete the lead-bismuth alloy melting characteristic experiment, and close the sixth valve, the seventh valve and the heat transfer oil module;
[0041] The solidification characteristics experiment of lead-bismuth alloy is C experiment or D experiment:
[0042] The C experiment includes the following steps:
[0043] C1] Use the heating module to preheat the lead-bismuth alloy storage tank, experimental tank and all pipelines;
[0044] C2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank changes from solid to liquid, open the first valve and the third valve, use the inert gas bottle to add the lead-bismuth alloy in the lead-bismuth alloy storage tank into the experimental tank, and close the first valve and the third valve;
[0045] C3] Open the fifth valve and the eighth valve, turn on the air module, and continue to cool the lead-bismuth alloy in the experimental tank until the lead-bismuth alloy is completely solidified;
[0046] C4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod to study the stress characteristics of the wall of the electric heating rod during the solidification of the lead-bismuth alloy, complete the lead-bismuth alloy solidification characteristics experiment, and close the fifth valve, the eighth valve and the air module;
[0047] The D experiment includes the following steps:
[0048] D1] Use the heating module to preheat the lead-bismuth alloy storage tank, experimental tank and all pipelines;
[0049] D2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank changes from solid to liquid, open the first valve and the third valve, use the inert gas bottle to add the lead-bismuth alloy in the lead-bismuth alloy storage tank into the experimental tank, and close the first valve and the third valve;
[0050] D3] Open the sixth valve and the seventh valve, turn on the heat transfer oil module, continue to cool the lead-bismuth alloy in the experimental tank, and keep the temperature of the heat transfer oil in the heat transfer oil module less than or equal to 100°C until the lead-bismuth alloy is completely solidified;
[0051] D4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod to study the stress characteristics of the wall of the electric heating rod during the solidification of lead-bismuth alloy, complete the lead-bismuth alloy solidification characteristics experiment, and close the sixth valve, the seventh valve and the heat transfer oil module.
[0052] Furthermore, the step B3] is specifically as follows:
[0053] When the temperature of the lead-bismuth alloy in the experimental tank drops below 50°C, open the sixth valve, the seventh valve and the high-temperature oil pump, and use the high-temperature oil pump to circulate the heat transfer oil in the heat transfer oil loop formed by the high-temperature oil pump, the heater, the interlayer of the experimental tank, the blower radiator and the high-temperature heat transfer oil tank. At the same time, turn on the heater to continuously heat the heat transfer oil, keeping the heat transfer oil temperature greater than or equal to 200°C until the lead-bismuth alloy in the experimental tank is completely melted.
[0054] Furthermore, the step C3] is specifically as follows:
[0055] Open the fifth valve and the eighth valve, use the air compressor to compress the external atmosphere and store it in the gas storage tank. At the same time, the compressed air passes through the interlayer of the fifth valve and the experimental tank for heat exchange, continuously cooling the lead-bismuth alloy in the experimental tank until it is completely solidified. Finally, the compressed air is discharged through the eighth valve.
[0056] Furthermore, the step D3] is specifically as follows:
[0057] Open the sixth valve, the seventh valve and the high-temperature oil pump, and use the high-temperature oil pump to circulate the heat transfer oil in the heat transfer oil loop formed by the high-temperature oil pump, the heater, the interlayer of the experimental tank, the blast radiator and the high-temperature heat transfer oil tank. At the same time, open the blast radiator to continuously cool the heat transfer oil, and keep the heat transfer oil temperature less than or equal to 100°C until the lead-bismuth alloy is completely solidified.
[0058] Furthermore, after the lead-bismuth alloy melting property experiment or the lead-bismuth alloy solidification property experiment is completed, it also includes:
[0059] Open the first valve to return the lead-bismuth alloy from the experimental tank to the lead-bismuth alloy storage tank, and fill the lead-bismuth alloy storage tank with argon gas for protection until the pressure in the lead-bismuth alloy storage tank drops to 0.3 MPa. Then, close all valves, turn off the signal processor, cut off the power supply, and the experiment ends.
[0060] Beneficial effects of the present invention:
[0061] 1. The present invention provides a lead-bismuth alloy melting and solidification characteristic experimental system, which can carry out lead-bismuth alloy melting and solidification stress experiments under high-efficiency heating and cooling conditions, with an efficiency of up to 15°C / min, and can achieve simple and quick adjustment of system parameters.
[0062] 2. The present invention provides an experimental method for studying the melting and solidification characteristics of lead-bismuth alloy, which can be used to carry out melting experiments of lead-bismuth alloy heated by electric heating rods, melting experiments of lead-bismuth alloy heated by heat transfer oil, solidification experiments of lead-bismuth alloy cooled by heat transfer oil, and solidification experiments of lead-bismuth alloy cooled by air. It can be used to study the stress characteristics of fuel elements (i.e., electric heating rods are used instead of lead-bismuth alloys) under different heating and cooling methods in lead-bismuth fast reactors due to the melting and solidification characteristics of lead-bismuth alloys. BRIEF DESCRIPTION OF THE DRAWINGS
[0063] Figure 1 It is a schematic diagram of an embodiment of a lead-bismuth alloy melting and solidification characteristics experimental system of the present invention.
[0064] Description of reference numerals:
[0065] 1- inert gas bottle, 2- lead-bismuth alloy storage tank, 3- experimental tank, 4- electric heating rod, 5- gas storage tank, 6- air compressor, 7- high temperature oil pump, 8- high temperature thermal oil tank, 9- blast radiator, 10- heater, 11- check valve, 12- liquid level sensor, 101- first flow meter, 102- second flow meter, 201- first pressure sensor, 202- second pressure sensor, 203- third pressure sensor, 204- fourth pressure sensor, 205- fourth pressure sensor, 206- fifth pressure sensor, 207- fifth pressure sensor, 208- fifth pressure sensor, 209- sixth pressure sensor, 210- sixth pressure sensor, 211- eighth pressure sensor, 212- eighth pressure sensor, 213- eighth pressure sensor, 214- eighth pressure sensor, 215- eighth pressure sensor, 216- eighth pressure sensor, 217- eighth pressure sensor, 218- eighth pressure sensor, 219- eighth pressure sensor, 220- eighth pressure sensor, 221- eighth pressure sensor, 222- eighth pressure sensor, 223- eighth pressure sensor, 224- eighth pressure sensor, 225- eighth pressure sensor, 226- eighth pressure sensor, 227- eighth pressure sensor, 228- eighth pressure sensor, 229- eighth pressure sensor, 230- eighth pressure sensor, 231- eighth pressure sensor, 232- eighth pressure sensor, 233- eighth pressure sensor, 234- eighth pressure sensor, 235- eighth pressure sensor, 236- eighth pressure sensor, 237- eighth pressure sensor, 238- eighth pressure sensor, 239- eighth pressure sensor, 240- eighth pressure sensor, 241- eighth pressure sensor, 242- eighth pressure sensor, 243- eighth pressure sensor, 244- eighth pressure sensor, 245 5-fifth pressure sensor, 206-sixth pressure sensor, 301-first temperature sensor, 302-second temperature sensor, 303-third temperature sensor, 304-fourth temperature sensor, 305-fifth temperature sensor, 306-sixth temperature sensor, 401-first valve, 402-second valve, 403-third valve, 404-fourth valve, 405-fifth valve, 406-sixth valve, 407-seventh valve, 408-eighth valve. DETAILED DESCRIPTION
[0066] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings and embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0067] like Figure 1 As shown, a lead-bismuth alloy melting and solidification characteristics experimental system comprises an injection module, an experimental module, a heat transfer oil module, an air module, a heating module, a heat preservation unit, a collection board and a signal processor; the injection module comprises an inert gas bottle 1 and a lead-bismuth alloy storage tank 2 connected to the inert gas bottle 1; the experimental module comprises an experimental tank 3, a third pressure sensor 203, a second temperature sensor 302, a plurality of electric heating rods 4 and a liquid level sensor 12 arranged on the experimental tank 3; the heat transfer oil module comprises a high-temperature oil pump 7, a high-temperature heat transfer oil tank 8, a blast type radiator 9 and a heater 10; the air module comprises an air compressor 6 and a gas storage tank 5; the heat transfer oil module is used to provide different temperature The heat transfer oil of a certain degree is used to heat or cool the lead-bismuth alloy in the experimental tank 3; the air module is used to cool the lead-bismuth alloy in the experimental tank 3; high-temperature resistant strain gauges are installed in the axial and circumferential directions of the electric heating rod 4, and the strain gauges are used to obtain the stress characteristics of the wall of the electric heating rod 4 when the lead-bismuth alloy melts and solidifies; the liquid level sensor 12 is used to measure the liquid level of the lead-bismuth alloy in the experimental tank 3, the third pressure sensor 203 is used to measure the pressure of the lead-bismuth alloy in the experimental tank 3, and the second temperature sensor 302 is used to measure the temperature of the lead-bismuth alloy in the experimental tank 3; in this embodiment, the inert gas bottle adopts the inert gas bottle 1; the inert gas bottle 1 adopts a high-purity argon gas bottle, and the heating module adopts an electric heating wire.
[0068] A first pressure sensor 201 is provided on the outlet pipeline of the high-purity argon gas cylinder, and the first pressure sensor 201 is used to measure the pressure of the argon gas pipeline on the high-purity argon gas cylinder; a second pressure sensor 202, a first temperature sensor 301 and a second valve 402 are provided on the lead-bismuth alloy storage tank 2; the second valve 402 is used to discharge excess gas in the lead-bismuth alloy storage tank 2; a third valve 403 is provided on the pipeline between the high-purity argon gas cylinder and the lead-bismuth alloy storage tank 2, and the third valve 403 is used to adjust the flow rate of argon gas; the lead-bismuth alloy storage tank 2 is used to store lead-bismuth alloy; the high-purity argon gas cylinder is used to store inert gas to protect the lead-bismuth alloy and to press the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 into the experimental tank 3.
[0069] The experimental tank 3 is filled with lead-bismuth alloy, and a check valve 11 is arranged on it, which is used to discharge excess gas in the experimental tank 3; the outlet of the high-purity argon gas cylinder is connected to the gas inlet of the experimental tank 3, and a fourth valve 404 is arranged on the pipeline between the high-purity argon gas cylinder and the gas inlet of the experimental tank 3. The high-purity argon gas cylinder provides argon gas to the lead-bismuth alloy storage tank 2 and the experimental tank 3 through the third valve 403 and the fourth valve 404, respectively, which is used to fill the experimental tank 3 with argon gas to protect the lead-bismuth alloy in the experimental tank 3. The inlet of the experimental tank 3 is connected to the outlet of the lead-bismuth alloy storage tank 2, and a first valve 401 is arranged on the pipeline between the inlet of the experimental tank 3 and the outlet of the lead-bismuth alloy storage tank 2.
[0070] The experimental tank 3 is a sandwich structure, and the sandwich is used to pass compressed air or thermal oil. A fifth pressure sensor 205 and a fourth temperature sensor 304 are arranged at the inlet of the sandwich of the experimental tank 3, and the inlet of the sandwich of the experimental tank 3 is respectively connected to the outlet of the thermal oil module and the outlet of the air module, and a fifth valve 405 is arranged between the inlet of the sandwich of the experimental tank 3 and the outlet of the air module, and a sixth valve 406 is arranged between the inlet of the sandwich of the experimental tank 3 and the outlet of the thermal oil module; the outlet of the sandwich of the experimental tank 3 is connected to the inlet of the thermal oil module, and a sixth pressure sensor 206 and a fifth temperature sensor 305 are arranged at the outlet of the sandwich of the experimental tank 3, and a seventh valve 407 is arranged on the pipeline between the outlet of the sandwich of the experimental tank 3 and the inlet of the thermal oil module; an eighth valve 408 for exhaust is arranged on the pipeline between the seventh valve 407 and the outlet of the sandwich of the experimental tank 3, and the eighth valve 408 is used to discharge the compressed air in the sandwich of the experimental tank 3.
[0071] The inlet of the high-temperature oil pump 7 is connected to the outlet of the high-temperature thermal oil tank 8, and the outlet of the high-temperature oil pump 7 is connected to the inlet of the heater 10. A first flow meter 101 is provided on the pipeline between the outlet of the high-temperature oil pump 7 and the inlet of the heater 10. The first flow meter 101 adopts a venturi flow meter and is used to measure the flow rate of the thermal oil. The outlet of the heater 10 is connected to the inlet of the interlayer of the experimental tank 3 through the sixth valve 406. The inlet of the blast radiator 9 is connected to the outlet of the interlayer of the experimental tank 3 through the seventh valve 407, and the outlet of the blast radiator 9 is connected to the inlet of the high-temperature thermal oil tank 8. A heating rod is installed in the high-temperature thermal oil tank 8 to preheat the thermal oil. The high-temperature oil pump 7, the heater 10, the interlayer of the experimental tank 3, the blast radiator 9 and the high-temperature thermal oil tank 8 form a thermal oil circuit. The blast radiator 9 is used to cool the thermal oil. The heater 10 is used to further increase the temperature of the thermal oil. The sixth valve 406 and the seventh valve 407 are used to adjust the flow rate of the thermal oil.
[0072] The inlet of the air compressor 6 is connected to the outside atmosphere, and the outlet is connected to the inlet of the gas storage tank 5; the air compressor 6 is used to compress the air and store it in the gas storage tank 5; the gas storage tank 5 is provided with a fourth pressure sensor 204 and a third temperature sensor 303; the outlet of the gas storage tank 5 is connected to the interlayer inlet of the experimental tank 3 through the fifth valve 405, and a second flow meter 102 is provided on the pipeline between the fifth valve 405 and the outlet of the gas storage tank 5, and the second flow meter 102 is a thermal gas mass flow meter. After the compressed air passes through the fifth valve 405 and the interlayer of the experimental tank 3 for heat exchange, it is finally discharged outdoors through the eighth valve 408.
[0073] The electric heating wire is wound around the lead-bismuth alloy storage tank 2, the experimental tank 3 and the outside of all pipelines. The electric heating wire melts the lead-bismuth alloy by generating heat; the insulation layer is coated on the outside of the electric heating wire; all pressure sensors, temperature sensors, strain gauges, electric heating wires and liquid level sensors 12 are connected to the signal processor through the acquisition board respectively.
[0074] The present invention provides a lead-bismuth alloy melting and solidification characteristic experimental system, which can carry out a lead-bismuth alloy melting experiment heated by an electric heating rod 4, a lead-bismuth alloy melting experiment heated by heat-conducting oil, a lead-bismuth alloy solidification experiment cooled by heat-conducting oil, and a lead-bismuth alloy solidification experiment cooled by air. In the experimental system, all tanks, pipes, and valve surfaces in contact with the lead-bismuth alloy are wrapped with electric heating wires, which are used to preheat the experimental circuit at the beginning of the experiment and perform thermal compensation during the experiment, and the electric heating wires are coated with a thermal insulation layer.
[0075] An experimental method for studying the melting and solidification characteristics of a lead-bismuth alloy includes a lead-bismuth alloy melting characteristic experiment and a lead-bismuth alloy solidification characteristic experiment; the lead-bismuth alloy melting characteristic experiment is an A experiment, and in other embodiments, a B experiment may also be used:
[0076] With the thermal oil module and the air module closed, experiment A includes the following steps:
[0077] A1] Use the heating module to preheat the lead-bismuth alloy storage tank 2, the experimental tank 3 and all pipelines;
[0078] A2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 changes from solid to liquid, the first valve 401 and the third valve 403 are opened, and the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 is added into the experimental tank 3 using an inert gas bottle, and the first valve 401 and the third valve 403 are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank 3;
[0079] A3] When the temperature of the lead-bismuth alloy in the experimental tank 3 drops below 50° C., the multiple electric heating rods 4 in the experimental tank 3 are turned on to continue heating the lead-bismuth alloy until the lead-bismuth alloy is completely melted;
[0080] A4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod 4, obtain the stress characteristics of the wall of the electric heating rod 4 when the lead-bismuth alloy is melted, complete the lead-bismuth alloy melting characteristic experiment, and turn off the electric heating rod 4;
[0081] When the multiple electric heating rods 4 in the experimental tank 3 and the air module are closed, the B experiment includes the following steps:
[0082] B1] Use the heating module to preheat the lead-bismuth alloy storage tank 2, the experimental tank 3 and all pipelines;
[0083] B2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 changes from solid to liquid, the first valve 401 and the third valve 403 are opened, and the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 is added into the experimental tank 3 using an inert gas bottle, and the first valve 401 and the third valve 403 are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank 3;
[0084] B3] When the temperature of the lead-bismuth alloy in the experimental tank 3 drops below 50°C, the sixth valve 406, the seventh valve 407 and the high-temperature oil pump 7 are opened, and the high-temperature oil pump 7 is used to circulate the heat transfer oil in the heat transfer oil loop formed by the high-temperature oil pump 7, the heater 10, the interlayer of the experimental tank 3, the blast radiator 9 and the high-temperature heat transfer oil tank 8. At the same time, the heater 10 is turned on to continuously heat the heat transfer oil, and the temperature of the heat transfer oil is kept greater than or equal to 200°C until the lead-bismuth alloy in the experimental tank 3 is completely melted;
[0085] B4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod 4, obtain the stress characteristics of the wall of the electric heating rod 4 when the lead-bismuth alloy melts, complete the lead-bismuth alloy melting characteristic experiment, and close the sixth valve 406, the seventh valve 407, the high-temperature oil pump 7, the blast radiator 9, the heater 10 and the thermal oil module;
[0086] When the thermal oil module and the plurality of electric heating rods 4 are turned off, the C experiment includes the following steps:
[0087] C1] Use the heating module to preheat the lead-bismuth alloy storage tank 2, the experimental tank 3 and all pipelines;
[0088] C2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 changes from solid to liquid, open the first valve 401 and the third valve 403, use the inert gas bottle to add the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 into the experimental tank 3, and close the first valve 401 and the third valve 403;
[0089] C3] Open the fifth valve 405 and the eighth valve 408, use the air compressor 6 to compress the external atmosphere and store it in the gas storage tank 5, and at the same time, the compressed air passes through the fifth valve 405 and the interlayer of the experimental tank 3 for heat exchange, continuously cooling the lead-bismuth alloy in the experimental tank 3 until it is completely solidified, and finally the compressed air is discharged through the eighth valve 408.
[0090] C4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod 4 to study the stress characteristics of the wall of the electric heating rod 4 during the solidification of the lead-bismuth alloy, complete the lead-bismuth alloy solidification characteristic experiment, and close the fifth valve 405, the eighth valve 408, the air compressor 6 and the air module;
[0091] Close the multiple electric heating rods 4 and the air module in the experimental tank 3. Experiment D includes the following steps:
[0092] D1] Use the heating module to preheat the lead-bismuth alloy storage tank 2, the experimental tank 3 and all pipelines;
[0093] D2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 changes from solid to liquid, the first valve 401 and the third valve 403 are opened, and the lead-bismuth alloy in the lead-bismuth alloy storage tank 2 is added into the experimental tank 3 using an inert gas bottle, and the lead-bismuth alloy solidifies into a solid state in the experimental tank 3, and the first valve 401 and the third valve 403 are closed;
[0094] D3] Open the sixth valve 406, the seventh valve 407 and the high-temperature oil pump 7, and use the high-temperature oil pump 7 to circulate the heat transfer oil in the heat transfer oil loop formed by the high-temperature oil pump 7, the heater 10, the interlayer of the experimental tank 3, the blast radiator 9 and the high-temperature heat transfer oil tank 8. At the same time, open the blast radiator 9 to continuously cool the heat transfer oil, and keep the heat transfer oil temperature less than or equal to 100° C. until the lead-bismuth alloy is completely solidified;
[0095] D4] Use the signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod 4 to study the stress characteristics of the wall of the electric heating rod 4 during the solidification of the lead-bismuth alloy, complete the lead-bismuth alloy solidification characteristics experiment, and close the sixth valve 406, the seventh valve 407, the high-temperature oil pump 7 and the heat transfer oil module.
[0096] In the present embodiment, after the lead-bismuth alloy melting characteristics experiment or the lead-bismuth alloy solidification characteristics experiment is completed, the power supply is also cut off and the experiment is ended. Specifically, the first valve 401 is opened to return the lead-bismuth alloy from the experimental tank 3 to the lead-bismuth alloy storage tank 2, and argon gas is filled into the lead-bismuth alloy storage tank 2 for protection until the pressure in the lead-bismuth alloy storage tank 2 drops to 0.3 MPa, then all valves are closed, the signal processor is turned off, the power supply is cut off, and the experiment is ended.
[0097] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A lead-bismuth alloy melting and solidification characteristics experimental system, characterized by: It includes injection module, experimental module, thermal oil module, air module, heating module, acquisition board and signal processor; The injection module comprises an inert gas bottle (1) and a lead-bismuth alloy storage tank (2) connected to the inert gas bottle (1); a first pressure sensor (201) is arranged on the outlet pipeline of the inert gas bottle (1); a second pressure sensor (202) and a first temperature sensor (301) are arranged on the lead-bismuth alloy storage tank (2); and a third valve (403) is arranged on the pipeline between the inert gas bottle (1) and the lead-bismuth alloy storage tank (2); The experimental module comprises an experimental tank (3), a third pressure sensor (203) arranged on the experimental tank (3), a second temperature sensor (302), a plurality of electric heating rods (4) and a liquid level sensor (12); the experimental tank (3) is a sandwich structure, and the sandwich is used to pass compressed air or heat transfer oil; the inlet of the experimental tank (3) is connected to the outlet of the lead-bismuth alloy storage tank (2), and a first valve (401) is arranged on the pipeline between the inlet of the experimental tank (3) and the outlet of the lead-bismuth alloy storage tank (2); a fifth pressure sensor (205) and a fourth temperature sensor (304) are arranged at the inlet of the sandwich of the experimental tank (3), and the inlet of the sandwich of the experimental tank (3) is respectively connected to the outlet of the heat transfer oil module. The outlet of the test tank (3) and the outlet of the air module are connected, and a fifth valve (405) is provided between the interlayer inlet of the test tank (3) and the outlet of the air module, and a sixth valve (406) is provided between the interlayer inlet of the test tank (3) and the outlet of the thermal oil module; the interlayer outlet of the test tank (3) is connected to the inlet of the thermal oil module, a sixth pressure sensor (206) and a fifth temperature sensor (305) are provided at the interlayer outlet of the test tank (3), and a seventh valve (407) is provided on the pipeline between the interlayer outlet of the test tank (3) and the inlet of the thermal oil module; an eighth valve (408) for exhaust is provided on the pipeline between the seventh valve (407) and the interlayer outlet of the test tank (3); The electric heating rod (4) is provided with a strain gauge, which is used to obtain the stress characteristics of the wall surface of the electric heating rod (4) when the lead-bismuth alloy melts and solidifies; The heating module is arranged outside the lead-bismuth alloy storage tank (2), the experimental tank (3) and all pipelines; All pressure sensors, temperature sensors, strain gauges, heating modules and liquid level sensors (12) are connected to the signal processor via an acquisition board.
2. The lead-bismuth alloy melting and solidification characteristics experimental system according to claim 1, characterized in that: The thermal oil module comprises a high-temperature oil pump (7), a high-temperature thermal oil tank (8), a blast-type radiator (9) and a heater (10); The inlet of the high-temperature oil pump (7) is connected to the outlet of the high-temperature thermal oil tank (8), the outlet of the high-temperature oil pump (7) is connected to the inlet of the heater (10), and a first flow meter (101) is provided on the pipeline between the outlet of the high-temperature oil pump (7) and the inlet of the heater (10); the outlet of the heater (10) is connected to the interlayer inlet of the experimental tank (3) through a sixth valve (406); The inlet of the blast type radiator (9) is connected to the outlet of the interlayer of the experimental tank (3) through the seventh valve (407), and the outlet of the blast type radiator (9) is connected to the inlet of the high temperature thermal oil tank (8); The high-temperature oil pump (7), the heater (10), the interlayer of the experimental tank (3), the blast-type radiator (9) and the high-temperature heat-conducting oil tank (8) form a heat-conducting oil circuit; The blast-type radiator (9) is used to cool the heat-conducting oil; The heater (10) is used to increase the temperature of the heat transfer oil.
3. The lead-bismuth alloy melting and solidification characteristics experimental system according to claim 2, characterized in that: The air module comprises an air compressor (6) and a gas storage tank (5); The inlet of the air compressor (6) is connected to the external atmosphere, and the outlet is connected to the inlet of the gas storage tank (5); the air compressor (6) is used to fill the gas storage tank (5) with compressed air; The gas storage tank (5) is provided with a fourth pressure sensor (204) and a third temperature sensor (303); the outlet of the gas storage tank (5) is connected to the interlayer inlet of the experimental tank (3) through a fifth valve (405), and a second flow meter (102) is provided on the pipeline between the fifth valve (405) and the outlet of the gas storage tank (5).
4. The lead-bismuth alloy melting and solidification characteristics experimental system according to claim 3, characterized in that: Also includes a thermal insulation unit; The heat preservation unit comprises a heat preservation layer coated outside the heating module; The experimental tank (3) is provided with a check valve (11), and the check valve (11) is used to discharge excess gas in the experimental tank (3); The outlet of the inert gas bottle (1) is connected to the gas inlet of the experimental tank (3), and a fourth valve (404) is provided on the pipeline between the inert gas bottle (1) and the gas inlet of the experimental tank (3) for filling the experimental tank (3) with inert gas to protect the lead-bismuth alloy in the experimental tank (3); The high-temperature heat-conducting oil tank (8) is provided with a heating rod; The lead-bismuth alloy storage tank (2) is provided with a second valve (402), and the second valve (402) is used to discharge excess gas in the lead-bismuth alloy storage tank (2).
5. The lead-bismuth alloy melting and solidification characteristics experimental system according to claim 4, characterized in that: The inert gas bottle (1) is a high-purity argon gas bottle; The heating module adopts electric heating wire.
6. A method for testing the melting and solidification characteristics of a lead-bismuth alloy, based on the lead-bismuth alloy melting and solidification characteristics testing system according to any one of claims 1 to 5, characterized in that: Including lead-bismuth alloy melting characteristics experiment and lead-bismuth alloy solidification characteristics experiment; The lead-bismuth alloy melting characteristic experiment is experiment A or experiment B: The A experiment includes the following steps: A1] Preheating the lead-bismuth alloy storage tank (2), the experimental tank (3) and all pipelines using a heating module; A2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) changes from a solid state to a liquid state, the first valve (401) and the third valve (403) are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) is added to the experimental tank (3) using the inert gas bottle (1), the first valve (401) and the third valve (403) are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank (3); A3] When the temperature of the lead-bismuth alloy in the experimental tank (3) drops below 50° C., the plurality of electric heating rods (4) in the experimental tank (3) are turned on to continue heating the lead-bismuth alloy until the lead-bismuth alloy is completely melted; A4] using a signal processor to collect information on flow, pressure, temperature and strain gauges on the electric heating rod (4), obtaining stress characteristics of the wall of the electric heating rod (4) when the lead-bismuth alloy is melted, completing the lead-bismuth alloy melting characteristic experiment, and turning off the electric heating rod (4); The B experiment includes the following steps: B1] Preheating the lead-bismuth alloy storage tank (2), the experimental tank (3) and all pipelines using a heating module; B2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) changes from a solid state to a liquid state, the first valve (401) and the third valve (403) are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) is added to the experimental tank (3) using the inert gas bottle (1), the first valve (401) and the third valve (403) are closed, and the lead-bismuth alloy solidifies into a solid state in the experimental tank (3); B3] When the temperature of the lead-bismuth alloy in the experimental tank (3) drops below 50° C., the sixth valve (406) and the seventh valve (407) are opened, and the heat transfer oil module is turned on to continue heating the lead-bismuth alloy in the experimental tank (3), and the temperature of the heat transfer oil in the heat transfer oil module is maintained at or above 200° C. until the lead-bismuth alloy in the experimental tank (3) is completely melted; B4] using a signal processor to collect information on flow, pressure, temperature and strain gauges on the electric heating rod (4), obtaining stress characteristics of the wall of the electric heating rod (4) when the lead-bismuth alloy is melted, completing the lead-bismuth alloy melting characteristic experiment, and closing the sixth valve (406), the seventh valve (407) and the heat transfer oil module; The lead-bismuth alloy solidification property experiment is a C experiment or a D experiment: The C experiment includes the following steps: C1] Preheating the lead-bismuth alloy storage tank (2), the experimental tank (3) and all pipelines using a heating module; C2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) changes from solid to liquid, the first valve (401) and the third valve (403) are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) is added to the experimental tank (3) using the inert gas bottle (1), and the first valve (401) and the third valve (403) are closed; C3] Open the fifth valve (405) and the eighth valve (408), turn on the air module, and continue to cool the lead-bismuth alloy in the experimental tank (3) until the lead-bismuth alloy is completely solidified; C4] using a signal processor to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod (4) to study the stress characteristics of the wall of the electric heating rod (4) during the solidification of the lead-bismuth alloy, completing the lead-bismuth alloy solidification characteristic experiment, and closing the fifth valve (405), the eighth valve (408) and the air module; The D experiment includes the following steps: D1] Preheating the lead-bismuth alloy storage tank (2), the experimental tank (3) and all pipelines using a heating module; D2] When the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) changes from solid to liquid, the first valve (401) and the third valve (403) are opened, the lead-bismuth alloy in the lead-bismuth alloy storage tank (2) is added to the experimental tank (3) using the inert gas bottle (1), and the first valve (401) and the third valve (403) are closed; D3] Open the sixth valve (406) and the seventh valve (407), turn on the heat transfer oil module, continue to cool the lead-bismuth alloy in the experimental tank (3), and keep the temperature of the heat transfer oil in the heat transfer oil module less than or equal to 100° C. until the lead-bismuth alloy is completely solidified; D4] The signal processor is used to collect information on flow, pressure, temperature and the strain gauge on the electric heating rod (4) to study the stress characteristics of the wall of the electric heating rod (4) during the solidification of the lead-bismuth alloy, complete the lead-bismuth alloy solidification characteristics experiment, and close and open the sixth valve (406), the seventh valve (407) and the heat transfer oil module.
7. An experimental method for studying the melting and solidification characteristics of lead-bismuth alloy according to claim 6, characterized in that: Step B3] is specifically: When the temperature of the lead-bismuth alloy in the experimental tank (3) drops below 50° C., the sixth valve (406), the seventh valve (407) and the high-temperature oil pump (7) are opened, and the high-temperature oil pump (7) is used to circulate the heat transfer oil in a heat transfer oil circuit formed by the high-temperature oil pump (7), the heater (10), the interlayer of the experimental tank (3), the blast-type radiator (9) and the high-temperature heat transfer oil tank (8). At the same time, the heater (10) is turned on to continuously heat the heat transfer oil, and the temperature of the heat transfer oil is maintained at or above 200° C. until the lead-bismuth alloy in the experimental tank (3) is completely melted.
8. An experimental method for studying the melting and solidification characteristics of lead-bismuth alloy according to claim 7, characterized in that: Step C3] is specifically: The fifth valve (405) and the eighth valve (408) are opened, and the external atmosphere is compressed by the air compressor (6) and stored in the gas storage tank (5). At the same time, the compressed air passes through the interlayer of the fifth valve (405) and the experimental tank (3) for heat exchange, and the lead-bismuth alloy in the experimental tank (3) is continuously cooled until it is completely solidified. Finally, the compressed air is discharged through the eighth valve (408).
9. An experimental method for studying the melting and solidification characteristics of lead-bismuth alloy according to claim 8, characterized in that: Step D3] is specifically: The sixth valve (406), the seventh valve (407) and the high-temperature oil pump (7) are opened, and the high-temperature oil pump (7) is used to circulate the heat transfer oil in a heat transfer oil circuit formed by the high-temperature oil pump (7), the heater (10), the interlayer of the experimental tank (3), the blast type radiator (9) and the high-temperature heat transfer oil tank (8). At the same time, the blast type radiator (9) is opened to continuously cool the heat transfer oil, and the temperature of the heat transfer oil is maintained at less than or equal to 100° C., until the lead-bismuth alloy is completely solidified.
10. An experimental method for studying the melting and solidification characteristics of lead-bismuth alloy according to claim 9, characterized in that: After the lead-bismuth alloy melting property experiment or the lead-bismuth alloy solidification property experiment is completed, it also includes: The first valve (401) is opened to allow the lead-bismuth alloy to flow back from the experimental tank (3) to the lead-bismuth alloy storage tank (2), and argon gas is filled into the lead-bismuth alloy storage tank (2) for protection until the pressure in the lead-bismuth alloy storage tank (2) drops to 0.3 MPa. All valves are closed, the signal processor is turned off, and the power supply is cut off, and the experiment ends.