Groove type MOSFET device and preparation method thereof, electronic equipment and preparation method thereof

By employing an equally spaced trench design and appropriate gate oxide thickness in trench MOSFET devices, the problems of high on-resistance and complex manufacturing processes have been solved, resulting in low-cost and high-efficiency power devices.

CN118919559AInactive Publication Date: 2024-11-08深圳市创飞芯源半导体有限公司
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410937962.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-12-19
Filing Date
2024-07-12
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing trench MOSFET devices suffer from high on-resistance and complex fabrication processes, which limit their application in high-efficiency, low-cost devices.

Method used

By employing a design with multiple first and second trenches arranged at equal intervals, combined with appropriate gate oxide thickness and body conductivity type, the manufacturing process is simplified and the epitaxial resistance is reduced.

Benefits of technology

This achieves low on-resistance and high breakdown voltage, simplifies the manufacturing process, reduces costs, and promotes the commercialization of high-performance power devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919559A_ABST
    Figure CN118919559A_ABST
Patent Text Reader

Abstract

The invention provides a trench type MOSFET device and a preparation method thereof, and an electronic device and a preparation method thereof, and the trench type MOSFET device comprises a substrate with a first conductive type; the epitaxial layer grows on the substrate and is provided with the first conduction type; the plurality of first grooves are formed in the epitaxial layer, the plurality of first grooves are arranged at equal intervals, and the widths of the plurality of first grooves are the same; and the gate oxide layer is formed in the plurality of first trenches, so that the epitaxial region resistance of the trench type MOSFET can be reduced, the breakdown voltage can be improved, the production process can be simplified, and the cost can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application claims priority to the Chinese invention patent application with application number 202311746879.X filed on December 19, 2023, entitled “Trench MOSFET device and preparation method, electronic device and preparation method”. Technical Field

[0002] The present application relates to the field of semiconductor technology, and in particular to a trench MOSFET device and a preparation method, an electronic device and a preparation method. Background Art

[0003] With the growing demand for high-efficiency and high-power density solutions in industries such as automotive electronics, switching power supplies, and industrial control, semiconductor devices, especially power MOSFETs (Metal-Oxide-Semiconductor Field-Effect Transistor), have become indispensable key components. In the pursuit of excellent performance, improving power conversion efficiency and power density has become the core goal of designing high-efficiency power switching devices. Among them, the on-resistance of power MOSFET, as a key indicator to measure device performance, directly affects the power loss of the device in the working state. Specifically, the on-resistance of MOSFET mainly includes: channel resistance, epitaxial region resistance, and substrate resistance. Under the premise of ensuring the same breakdown voltage, reducing the characteristic on-resistance can not only reduce the chip area, but also effectively reduce the parasitic capacitance of the device, thereby reducing the energy loss during the switching process.

[0004] In recent years, trench-gate power devices have attracted widespread attention due to their significant performance advantages - lower on-resistance and higher switching speed. The trench gate and super junction structure enable the device to achieve fast switching response while maintaining low on-resistance, effectively reducing switching losses and improving overall system efficiency. However, the manufacturing cost of such devices is relatively high, and the complexity of the production process increases the difficulty of yield control, limiting its application in a wider range of fields.

[0005] In response to the above challenges, SGTMOSFET (Shielded Gate Trench MOSFET), as an advanced power semiconductor device, has demonstrated superior performance to traditional trench MOSFETs with its lower on-resistance. However, its complex process places higher demands on equipment accuracy and technical level, thereby pushing up production costs. In view of this, it is an urgent technical problem to provide a trench MOSFET with low epitaxial region resistance, simplify the production process, reduce costs, promote the commercialization of high-performance power devices, and meet the market's urgent demand for high-efficiency, low-cost devices. Summary of the invention

[0006] The present application provides a trench MOSFET device, a preparation method, an electronic device and an electronic device preparation method, which solves the problem in the prior art that a trench MOSFET with low on-resistance and simple preparation process cannot be provided.

[0007] In order to achieve the above-mentioned object, in a first aspect, an embodiment of the present application provides a trench MOSFET device, comprising: a substrate having a first conductivity type;

[0008] an epitaxial layer, the epitaxial layer being grown on the substrate and having the first conductivity type;

[0009] A plurality of first trenches are formed in the epitaxial layer, wherein the plurality of first trenches are arranged at equal intervals and have the same width.

[0010] Optionally, the gate oxide layer has a thickness of 60nm-120nm.

[0011] Optionally, the width of the first groove is 0.3-0.4 μm.

[0012] Optionally, the epitaxial layer has a thickness of 4 μm.

[0013] Optionally, the gate conductor material is polysilicon, which is formed by a vapor deposition process.

[0014] Optionally, the trench MOSFET device further includes a plurality of second trenches formed in the epitaxial layer, wherein the plurality of second trenches are located in a terminal region of the MOSFET device and are used as terminals of the MOSFET device.

[0015] Optionally, the plurality of second grooves are arranged at equal intervals and have the same groove width.

[0016] Optionally, the spacing between the plurality of second grooves is less than or equal to the spacing between the plurality of first grooves.

[0017] Optionally, the spacing between the plurality of second grooves is 50%-100% of the spacing between the plurality of first grooves.

[0018] In a second aspect, an embodiment of the present application provides a method for preparing a trench MOSFET device, wherein the method is used to prepare a trench MOSFET device as described in any one of the first aspects, and the method for preparing the trench MOSFET comprises:

[0019] growing an epitaxial layer on a semiconductor substrate;

[0020] Etching a groove in the epitaxial layer;

[0021] growing a gate oxide layer of a preset thickness on the trench;

[0022] Depositing POLY in the groove and etching it so that the POLY fills the groove;

[0023] Perform body injection and diffusion of preset concentration into the gate oxide layer;

[0024] The source injection and diffusion, isolation layer deposition, contact etching and injection, and metal deposition and etching are completed in sequence to complete the preparation of the trench MOSFET structure.

[0025] In a third aspect, an embodiment of the present application provides an electronic device, comprising the trench MOSFET device as described in any one of the first aspects.

[0026] In a fourth aspect, an embodiment of the present application provides a method for preparing an electronic device, wherein the method for preparing an electronic device includes the method for preparing a trench MOSFET as described in any one of the second aspects.

[0027] A trench MOSFET device provided in an embodiment of the present application includes: a substrate having a first conductivity type; an epitaxial layer, the epitaxial layer grown on the substrate and having the first conductivity type; a plurality of first trenches formed in the epitaxial layer, the plurality of first trenches being arranged at equal intervals and having the same width; and a gate oxide layer formed in the plurality of first trenches, thereby solving the problem in the prior art that a trench MOSFET with low on-resistance and simple preparation process cannot be provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 A schematic diagram of trench etching in an embodiment of the present invention is shown;

[0029] Figure 2 A schematic diagram showing the growth of a gate oxide layer in an embodiment of the present invention is shown;

[0030] Figure 3 A schematic diagram showing Poly deposition and etching in an embodiment of the present invention is shown;

[0031] Figure 4 A schematic diagram showing Body injection and diffusion in an embodiment of the present invention is shown;

[0032] Figure 5 A schematic diagram showing source injection and diffusion in an embodiment of the present invention is shown;

[0033] Figure 6 A schematic diagram of depositing an isolation layer in an embodiment of the present invention is shown;

[0034] Figure 7 A schematic diagram of contact etching and implantation in an embodiment of the present invention is shown;

[0035] Figure 8 A schematic diagram of metal deposition and etching in an embodiment of the present invention is shown;

[0036] Fig. 9 A schematic diagram showing a structure in which a plurality of second grooves are used as terminals in an embodiment of the present invention is shown;

[0037] Fig.10 A schematic diagram showing a MOSFET device structure using a body ring as a terminal in an embodiment of the present invention is shown;

[0038] Figure 11A-11C A schematic diagram of a MOSFET device structure simulation in an embodiment of the present invention is shown;

[0039] Figure 12A-12C A schematic diagram of a MOSFET device structure simulation in the prior art is shown. DETAILED DESCRIPTION

[0040] In the following description, specific details such as specific system structures and technologies are provided for the purpose of illustration rather than limitation, so as to provide a thorough understanding of the embodiments of the present application. However, it should be clear to those skilled in the art that the present application can also be implemented in other embodiments without these specific details. In other cases, detailed descriptions of the well-known specific structures of SGT-MOSFET devices and the working principles of SGT-MOSFET are omitted to avoid unnecessary details that hinder the description of the present application.

[0041] The terms used in the following embodiments are only for the purpose of describing specific embodiments and are not intended to be limiting of the present application. As used in the specification and appended claims of the present application, the singular expressions "a", "said", "above", and "the" are intended to also include expressions such as "one or more", unless the context clearly indicates otherwise.

[0042] In recent years, trench-gate power devices have become a research hotspot in the field of power electronics due to their excellent performance - low on-resistance and high-speed switching characteristics. These structures allow devices to achieve fast switching while maintaining low resistance, greatly reducing switching losses and improving system efficiency. However, high manufacturing costs and complex production processes limit their widespread application, especially in cost-sensitive market areas.

[0043] To meet this challenge, SGTMOSFET (Shielded Gate Trench MOSFET) came into being. It stands out with its lower on-resistance and outperforms traditional trench MOSFET. However, its advanced process requirements also bring higher production costs. Therefore, there is an urgent need for a new device structure that aims to reduce the resistance of the epitaxial region of trench MOSFET and simplify the production process to achieve effective cost control, promote large-scale commercialization of high-performance power devices, and meet the market's strong demand for efficient and economical power devices.

[0044] Therefore, a trench MOSFET device provided in an embodiment of the present application includes: a substrate having a first conductivity type; an epitaxial layer, the epitaxial layer grown on the substrate and having the first conductivity type; a plurality of first trenches formed in the epitaxial layer, the plurality of first trenches being arranged at equal intervals and having the same width; and a gate oxide layer formed in the plurality of first trenches, thereby solving the problem in the prior art that a trench MOSFET with low on-resistance and simple preparation process cannot be provided.

[0045] Figures 1 to 8 The figure shows a process flow of manufacturing a trench MSOFET device in an embodiment of the present invention.

[0046] like Figure 1 As shown, a trench-type MSOFET device according to an embodiment of the present invention includes: a substrate having a first conductivity type; an epitaxial layer grown on the substrate, the epitaxial layer also having the first conductivity type; a plurality of trenches formed in the epitaxial layer, the plurality of trenches being arranged at equal intervals and having the same width; and a body region arranged between the plurality of trenches, the body region having a second conductivity type.

[0047] It should be noted that the body region further includes a first conductor region and a second conductor region, and the first conductor region and the second conductor region have different conductivity types. According to the types of the first conductor region and the second conductor region, a P-channel MOS transistor or an N-channel MOS transistor can be formed.

[0048] In this embodiment, the width of adjacent grooves is preferably 0.3um-0.4um, and the spacing (also called mesa) of the grooves is preferably 0.5um-0.8um. ​​It should be noted that the groove spacing described in this application is relatively small, because a larger groove spacing will lead to a decrease in the breakdown voltage BV, that is, the size of the groove spacing is inversely proportional to the breakdown voltage BV, but too small a groove spacing will lead to high costs and complex processes.

[0049] In one embodiment, the depth of the groove is 1.2-2.4 μm.

[0050] like Figure 2 As shown, in one embodiment, a gate oxide layer is formed in the plurality of trenches. The gate oxide layer also covers the surface of the spacer layer between the trenches. The thickness of the gate oxide layer is 60nm-120nm.

[0051] It should be noted that the gate oxide layer is a very thin silicon oxide film, which separates the gate and channel charges by forming an insulating layer on the gate surface. This oxide layer can effectively isolate the gate and the channel to prevent charge leakage and current leakage, thereby improving the insulation performance and switching speed of the MOSFET. In the prior art, the thickness of the gate oxide layer is usually between tens of nanometers and hundreds of nanometers. In this embodiment, the thickness of the gate oxide layer is increased, so that the trench MOSFET structure in this embodiment has a higher breakdown voltage.

[0052] In one embodiment, FIG9 shows a schematic diagram of a structure in which a plurality of second grooves are used as terminals in an embodiment of the present invention. Fig. 9 As shown, multiple second trenches can evenly distribute the electric field at the edge, avoid device breakdown caused by excessive concentration of the electric field, reduce edge parasitic capacitance, control charge accumulation, and reduce leakage current. In traditional MOSFET device structures, body rings are usually used as terminals, see Fig.10 . Fig.10 The schematic diagram of the MOSFET device structure using the body ring as the terminal in the embodiment of the present invention is shown. The body ring refers to the P-type region formed at the edge or terminal area of ​​the MOSFET, usually surrounding the source region. It uses the natural properties of the body diode to control the electric field distribution at the edge. However, for high-voltage application scenarios, the body ring as a terminal structure cannot meet the requirements. Fig. 9 The trench ring shown as the terminal can meet the high-voltage scenario requirements. Fig. 9 As shown, the plurality of second grooves are also arranged at equal intervals, and the widths of the plurality of second grooves are the same. However, the spacing between the plurality of second grooves is less than or equal to the spacing between the plurality of first grooves. Preferably, the spacing between the plurality of second grooves is 50%-100% of the spacing between the plurality of first grooves.

[0053] It should also be noted that the width of the plurality of second grooves may be the same as or different from the width of the plurality of first grooves, and the embodiment of the present application does not impose any specific limitation on the width of the plurality of second grooves and the width of the plurality of first grooves.

[0054] It should also be noted that, although the trench MOSFET provided in the embodiment of the present application introduces a depth-enhanced trench feature in the design, this design element inevitably leads to an increase in the input capacitance of the device. Although this feature limits the applicability of the device in high-frequency switching applications to some extent, it provides unique advantages for low-frequency switching scenarios, such as load switching circuits. In these low-frequency applications, the larger input capacitance does not significantly affect the overall system performance, but can instead bring into play its potential benefits in electrostatic discharge (ESD) protection and electromagnetic interference (EMI) suppression.

[0055] In another aspect, the present invention provides a method for preparing a trench MOSFET device, comprising the following steps:

[0056] Figure 1 FIG. 2 shows a schematic diagram of trench etching in an embodiment of the present invention. Figure 1 As shown, an epitaxial layer is grown on a semiconductor substrate, and a trench 101 is etched in the epitaxial layer. It should be noted that in this embodiment, any adjacent trenches 101 have the same spacing, and each trench 101 has the same width, and the trenches have a relatively deep trench depth.

[0057] Figure 2 FIG. 4 shows a schematic diagram of growing a gate oxide layer in an embodiment of the present invention. Figure 2 As described above, a gate oxide layer 102 with a preset thickness is grown on the trench. It should be noted that, in this embodiment, the thickness of the gate oxide layer is preferably 60nm-120nm.

[0058] Figure 3 The schematic diagram of Poly deposition and etching in the embodiment of the present invention is shown. POLY103 is deposited and etched in the groove so that POLY103 fills the groove. Specifically, the main function of POLY103 deposition and etching is to make the polysilicon gate in the transistor. This step includes two parts: deposition and etching. Among them, POLY103 deposition is the process of depositing polysilicon on a silicon wafer. The polysilicon gate is usually used in a field effect transistor (FET) as a switch of the device. After the polysilicon is deposited, heat treatment is required to eliminate stress and form a polysilicon film; POLY103 etching is the process of removing excess polysilicon by dry or wet etching after the polysilicon gate deposition is completed. The purpose of etching is to isolate the polysilicon gate from the source and drain while maintaining the shape and size of the gate. This step is crucial to the performance and stability of the device; through the process of POLY103 deposition and etching, a polysilicon gate with good performance can be produced, thereby realizing the miniaturization and high efficiency of semiconductor devices.

[0059] Figure 4FIG. 4 shows a schematic diagram of Body injection and diffusion in an embodiment of the present invention. Figure 4 As shown, Body 104 is implanted and diffused into the gate oxide layer.

[0060] It should be further explained that Body104 injection is the process of injecting impurity ions into the gate of a semiconductor transistor. This process is usually achieved by ion implantation or dry deposition. The main functions of Body104 injection include: adjusting the threshold voltage. By injecting different types of ions (such as boron, phosphorus, etc.), the charge state of the semiconductor surface can be changed, thereby controlling the threshold voltage of the device. The threshold voltage is a key parameter for the on and off states of the transistor. By adjusting the dose and energy of Body104 injection, the threshold voltage can be effectively regulated. At the same time, by optimizing the dose and energy of Body104 injection, the performance parameters of the transistor, such as switching speed and transconductance, can be improved. For example, appropriately increasing the dose of Body104 injection can enhance the driving capability of the transistor and increase the switching speed. Secondly, Body104 injection can reduce the hot carrier effect and secondary breakdown effect in the device, thereby improving the reliability of the device. The hot carrier effect may cause electrons to generate too much heat in the transistor, while the secondary breakdown effect may cause the transistor to fail under excessively high voltage. Through Body104 injection, the occurrence of these problems can be reduced.

[0061] The diffusion of Body 104 can form a PN junction: Through the diffusion process, a PN junction (the junction area between positive and negative semiconductors) can be formed on the semiconductor chip. The PN junction is a key structure for realizing voltage amplification and current control functions, such as in devices such as diodes and transistors; the diffusion of Body 104 can optimize device performance. Specifically, by controlling the concentration and depth of diffusion, the performance of the PN junction can be optimized, such as reducing series resistance, improving frequency response, etc. For example, in a transistor, a PN junction with a suitable concentration distribution can be formed through the diffusion process, thereby improving the performance of the device and at the same time, the reliability can be improved. Specifically, the diffusion process can reduce the impact of mechanical stress and thermal stress on the device, thereby improving the reliability of the device. In the semiconductor manufacturing process, mechanical stress and thermal stress may cause material defects and performance degradation. Through the diffusion process, these problems can be alleviated.

[0062] Figure 5 FIG. 4 shows a schematic diagram of source injection and diffusion in an embodiment of the present invention. Figure 5 As shown, source105 is injected to form a source, and a PN junction can be formed on the semiconductor chip through the source105 diffusion process.

[0063] Figure 6 FIG. 4 shows a schematic diagram of depositing an isolation layer in an embodiment of the present invention. Figure 6 As shown, the deposited isolation layer 106 mainly forms a thin film on the wafer, which can effectively protect the circuit elements from the influence of the external environment, such as mechanical damage, chemical corrosion, etc. At the same time, the deposited isolation layer 106 can also be used as a dielectric material to effectively isolate the circuit elements to avoid problems such as circuit short circuit and mutual interference. In the integrated circuit manufacturing process, the formation of the deposited isolation layer is usually carried out by physical vapor deposition (PVD) or chemical vapor deposition (CVD) and other methods; among them, the PVD method mainly deposits the material on the wafer surface through physical processes such as evaporation or sputtering under high vacuum; and the CVD method uses chemical reactions to form a thin film on the wafer surface.

[0064] Figure 7 FIG. 2 shows a schematic diagram of contact etching and implantation in an embodiment of the present invention. Figure 7 As shown, Contact107 etching is a key step in semiconductor manufacturing for forming contact holes. Contact holes are interfaces for connecting transistors and external circuits. During the Contact107 etching process, chemical or physical methods are used to remove materials on the surface of the semiconductor to form contact holes with specific shapes and sizes, where the position and size of the contact holes depend on the design of the mask and the process parameters; and the purpose of Contact injection is to form a high-concentration doped region at the bottom of the contact hole in order to establish good electrical contact between the transistor and the external circuit, where the type and dose of the injected impurities depend on the process design and the target device characteristics.

[0065] Figure 8 FIG. 2 shows a schematic diagram of metal deposition and etching in an embodiment of the present invention. Figure 8 As shown in Figure 1, Metal108 deposition is a key step in semiconductor manufacturing for forming metal lines. Metal lines are conductive materials used to connect transistors and external circuits. During the Metal108 deposition process, metal materials are deposited on the semiconductor surface using chemical or physical methods; while Metal108 etching is a key step in semiconductor manufacturing for forming metal connection points. Metal connection points are conductive contact points used to connect transistors and external circuits. During the Metal108 etching process, chemical or physical methods are used to remove part of the metal material on the semiconductor surface to form metal connection points with specific shapes and sizes.

[0066] In another aspect, the present invention provides an electronic device comprising the trench MOSFET device described above.

[0067] In another aspect, the present invention provides a method for preparing an electronic device, including the method for preparing the trench MOSFET described above.

[0068] In order to further prove that the MOSFET device provided in the embodiment of the present application can achieve a low on-resistance level similar to that of SGT MOSFET through a unique structural design, and that the MOSFET device structure provided in the embodiment of the present application can be realized using a manufacturing process similar to that of traditional Trench MOSFET, the embodiment of the present application also provides simulation results, see Figures 11A-11C . Figure 11A-11C A schematic diagram of a MOSFET device structure simulation in an embodiment of the present invention is shown.

[0069] Figure 11A-11C A schematic diagram of a MOSFET device structure simulation in an embodiment of the present invention is shown.

[0070] like Fig.11A As shown, in the MOSFET device structure provided in the embodiment of the present application, the grooves are arranged at equal intervals and the widths of the grooves are the same. It should be noted that, under the condition that the grooves are arranged at equal intervals and the widths of the grooves are the same, the width of the grooves and the spacing between the grooves can be set.

[0071] Fig. 11B For Fig.11A The resistance value in the MOSFET device simulation provided in the embodiment of the present application is shown. Specifically, the resistance value is approximately 3.84788E+00mohm.

[0072] Fig. 11C Schematic diagram of MOSFET device simulation results provided in the embodiment of the present application. Fig. 11C The simulation results show that the drain breakdown voltage is 2.8000E+01(volts).

[0073] Figure 12A-12C A schematic diagram of a MOSFET device structure simulation in the prior art is shown.

[0074] like Fig. 12A As shown, in the MOSFET device structure provided in the prior art, the trenches are arranged at non-equidistant intervals.

[0075] Fig. 12B For Fig. 12A The resistance value in the MOSFET device simulation provided in the prior art is shown, specifically, the resistance value is approximately 3.84141E+00mohm.

[0076] Fig. 12C for Fig. 12A FIG. 1 is a schematic diagram of simulation results of a MOSFET device provided in the prior art. Fig. 12C The simulation results show that the drain breakdown voltage is 1.5500E+01(volts).

[0077] The simulation results prove that: when the resistivity of the epitaxial layer is 0.1ohm.cm and the thickness of the epitaxial layer is 4μm, that is, when the resistance values ​​of the trench terminal structure using the prior art and the MOSFET structure using the embodiment of the present application are almost the same, the breakdown voltage of the trench terminal structure using the prior art is 1.5500E+01 (volts), while the breakdown voltage of the MOSFET structure using the embodiment of the present application is 2.8000E+01 (volts).

[0078] In addition, the resistivity of the epitaxial layer of the MOSFET structure provided in the embodiment of the present application can also be much lower than that of the MOSFET device of the prior art. For example, the resistivity of the epitaxial layer of the MOSFET structure provided in the embodiment of the present application is more than 70% lower than that of the MOSFET device of the prior art. For example, the resistivity of the epitaxial layer of the 30V trench MOSFET is about 0.3ohm.cm, while the resistivity of the MOSFET provided in the embodiment of the present application is about 0.1ohm.cm.

[0079] In summary, an embodiment of the present application proposes a trench MOSFET device, comprising: a substrate having a first conductivity type; an epitaxial layer, the epitaxial layer grown on the substrate and having the first conductivity type; a plurality of first trenches formed in the epitaxial layer, the plurality of first trenches being arranged at equal intervals and having the same width; a gate oxide layer formed in the plurality of first trenches, thereby reducing the resistance of the epitaxial region of the trench MOSFET and increasing the breakdown voltage, while simplifying the production process, reducing costs, promoting the commercialization process of high-performance power devices, and meeting the market's urgent demand for high-efficiency, low-cost devices.

[0080] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described or recorded in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.

[0081] Those of ordinary skill in the art will appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of this application.

[0082] In the embodiments provided in the present application, it should be understood that the disclosed devices / equipment and methods can be implemented in other ways. For example, the device / equipment embodiments described above are merely schematic, for example, the division of the modules or units is only a logical function division, and there may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some interfaces, indirect coupling or communication connection of devices or units, which can be electrical, mechanical or other forms.

[0083] It should be understood that when used in the present specification and the appended claims, the term "comprising" indicates the presence of described features, wholes, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components and / or combinations thereof.

[0084] It should also be understood that the term “and / or” used in the specification and appended claims refers to any and all possible combinations of one or more of the associated listed items, and includes these combinations.

[0085] As used in the specification and appended claims of this application, the term "if" can be interpreted as "when" or "uponce" or "in response to determining" or "in response to detecting", depending on the context. Similarly, the phrase "if it is determined" or "if [described condition or event] is detected" can be interpreted as meaning "uponce it is determined" or "in response to determining" or "uponce [described condition or event] is detected" or "in response to detecting [described condition or event]", depending on the context.

[0086] In addition, in the description of the present application specification and the appended claims, the terms "first", "second", "third", etc. are only used to distinguish the descriptions and cannot be understood as indicating or implying relative importance.

[0087] References to "one embodiment" or "some embodiments" etc. described in the specification of this application mean that one or more embodiments of the present application include specific features, structures or characteristics described in conjunction with the embodiment. Therefore, the statements "in one embodiment", "in some embodiments", "in some other embodiments", "in some other embodiments", etc. that appear in different places in this specification do not necessarily refer to the same embodiment, but mean "one or more but not all embodiments", unless otherwise specifically emphasized in other ways. The terms "including", "comprising", "having" and their variations all mean "including but not limited to", unless otherwise specifically emphasized in other ways.

[0088] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A trench MOSFET device, characterized in that: include: a substrate having a first conductivity type; an epitaxial layer, the epitaxial layer being grown on the substrate and having the first conductivity type; A plurality of first trenches are formed in the epitaxial layer, wherein the plurality of first trenches are arranged at equal intervals and have the same width.

2. The trench MOSFET device according to claim 1, characterized in that: The width of the first groove is 0.3-0.4 μm, the spacing of the first groove is 0.5 μm-0.8 μm, and the depth of the first groove is 1.2-2.4 μm.

3. The trench MOSFET device according to claim 1, characterized in that: The epitaxial layer has a thickness of 4 μm.

4. The trench MOSFET device according to claim 1, characterized in that: The trench MOSFET device further includes a plurality of second trenches formed in the epitaxial layer, wherein the plurality of second trenches are located in a terminal region of the MOSFET device and are used as terminals of the MOSFET device.

5. The trench MOSFET device according to claim 4, characterized in that: The plurality of second grooves are arranged at equal intervals and have the same groove width.

6. The trench MOSFET device according to claim 5, characterized in that: A pitch between the plurality of second grooves is less than or equal to a pitch between the plurality of first grooves.

7. The trench MOSFET device according to claim 6, characterized in that: The spacing between the plurality of second grooves is 50%-100% of the spacing between the plurality of first grooves.

8. A method for preparing a trench MOSFET device, characterized in that: For preparing the trench MOSFET structure according to any one of claims 1 to 7, comprising: growing an epitaxial layer on a semiconductor substrate; Etching a groove in the epitaxial layer; growing a gate oxide layer of a preset thickness on the trench; Depositing POLY in the groove and etching it so that the POLY fills the groove; Perform body injection and diffusion of preset concentration into the gate oxide layer; The source injection and diffusion, isolation layer deposition, contact etching and injection, and metal deposition and etching are completed in sequence to complete the preparation of the trench MOSFET structure.

9. An electronic device comprising the trench MOSFET device according to any one of claims 1 to 7.

10. A method for preparing an electronic device, comprising the method for preparing a trench MOSFET according to any one of claim 8.

Citation Information

Patent Citations

  • Power semiconductor device and manufacturing technology

    CN104241383A

  • Power semiconductor device and manufacturing method thereof

    CN111933700A

  • Shield gate trench MOSFET structure capable of optimizing terminal electric field and manufacturing method thereof

    CN114464667A

  • Preparation method of semiconductor structure and semiconductor structure

    CN115083901A