Method for manufacturing wide extruded sheet for calendering
By manufacturing the extruded sheet in a bending form in the hot extrusion step and processing it in the planarization step, the problem of the need for large-scale equipment to manufacture wide extruded sheets in the prior art is solved, and manufacturing on a small or medium-sized extruder is realized Wide-width boards reduce costs and extend equipment life.
Patent Information
- Application Number
- CN202310921550.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-09
- Filing Date
- 2023-07-26
- Publication Date
- 2024-11-12
AI Technical Summary
The prior art requires the use of large extruders and super-large extrusion dies when manufacturing wide-width extrusion sheets, resulting in high equipment investment costs, shortened mold life and increased engineering costs.
Wide-width sheets are manufactured on small or medium extruders by making cross-sectionally bent corrugated extruded sheets in the hot extrusion step and flattening with upper and lower rollers in the planarization step.
The production of relatively wide extruded flat sheet materials on small or medium extruders is achieved, reducing the burden on extruders and molds, reducing investment costs, and extending the life of the molds.
Smart Images

Figure CN118926334A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a plate, in particular to a method for manufacturing a wide plate which can use a small or medium-sized extruder to manufacture a wide plate with a relatively wide width.
[0002] That is, the present invention relates to a method for manufacturing wide-width extruded plates, which, after manufacturing an extruded plate with a corrugated shape having a curved cross-section in a hot extrusion step, flattens the curved cross-section by upper and lower rollers, thereby overcoming the limitation of the extrusion width based on the capacity of the extruder and enabling the manufacture of wide-width plates with relatively small equipment. Background Art
[0003] Metal sheets are used as materials in many fields and are usually produced by rolling.
[0004] Metal rolled plates are produced by melting and mixing metals to cast slabs, hot rolling the cast slabs to make flat plates, and rolling the flat plates into coils for cold rolling. In addition, in order to roll the plates over a wide width, the width of the mold used for casting the slabs needs to be cast wide, so a wide casting mold is required, and not only the cold rolling rolls but also the hot rolling rolls need to be manufactured to a wide width.
[0005] Regarding such rolled sheet technology, various technologies are being developed to reduce the defect rate or simplify the manufacturing process, and Patent Documents 1 to 4 are provided as examples.
[0006] The hot rolling device in Patent Document 1 includes: working rolls for rolling introduced billets; a cooling mechanism for dividing the working rolls into a plurality of cooling zones along the length direction of the working rolls and spraying cooling water having a cold air temperature set according to the cooling zone into each cooling zone; and a control unit for setting the cooling temperature of each cooling zone using a database and outputting the set cooling temperature to the cooling mechanism, wherein the database stores the degree of thermal expansion of each cooling zone of the working roll and the degree of change of the thickness characteristics of the cooling zone with the cooling temperature.
[0007] The hot rolling device of titanium plate in Patent Document 2 includes: a heating section for heating the titanium plate; a rough rolling section for rough rolling the titanium plate; and a conveying section for conveying the titanium plate from the heating section to the rough rolling section. A sled cooling section is formed on the titanium plate supported by the sled of the heating section, and the conveying section includes a heating table for heating the sled cooling section of the titanium plate. The rough rolling section includes: a feed roller section, which is provided on the inlet and outlet sides to supply the titanium plate; a working roller section, which rolls the titanium plate supplied by the feed roller section; and a guide section, which is located between the feed roller section and the working roller section, and guides the titanium plate.
[0008] The metal sheet rolling device of Patent Document 3 includes at least a pair of upper and lower working rolls and a pair of upper and lower reinforcing rolls, and is provided with: a pair of working roll clamps for holding each working roll; a shell or a process stopper for holding the working roll clamp; and a load detection device, which is arranged in the working roll clamp opposite to the shell or the process stopper, and detects the load in the rolling direction acting on the working roll clamp on at least one side of the rolling direction entrance side and the rolling direction exit side. At least one load detection device is arranged in each working roll clamp, and the point of action of the rolling direction force of the working roll is included in the range specified by the load detection device, so that the rotational torque generated by the rolling direction force in the working roll clamp and the reverse force of the reaction force to the rotational torque are balanced.
[0009] The method for manufacturing a high-strength aluminum rolled plate of Patent Document 4 comprises: a) preparing a high-strength aluminum rolled plate composed of 5.1 to 5.9 weight percent copper (Cu), 0.6 to 0.9 weight percent magnesium (Mg), 0.25 to 0.6 weight percent manganese (Mn), 0.15 to 0.25 weight percent silver (Ag), 0.07 to 0.13 weight percent zirconium (Zr), 0.04 to 0.1 weight percent silicon (Si), 0.09 to 0.15 weight percent iron (Fe), more than 0 and less than 0.1 weight percent titanium (Ti), 0.02 to 0.05 weight percent vanadium (V) and the remaining weight of aluminum (Al) and inevitable The present invention relates to a step of melting an aluminum alloy material composed of impurities; b) a step of casting a molten aluminum alloy; c) a step of homogenizing the molten alloy; d) a step of reheating the aluminum alloy after homogenization; e) a step of hot rolling the reheated aluminum alloy; f) a step of solution treatment of the hot-rolled aluminum alloy; g) a step of cold rolling the solution-treated aluminum rolled sheet; h) a step of performing a first aging treatment on the aluminum rolled sheet after cold rolling; and i) a step of performing a second aging treatment on the aluminum rolled sheet after the first aging treatment. The h) step is implemented at 20°C to 40°C for 20 to 200 hours. The i) step includes: (i-1) a step of maintaining at 160°C to 200°C for 1 to 20 hours; and (i-2) a step of air cooling the sheet after the i-1) step.
[0010] As described above, various plate manufacturing technologies have been developed, which adjust the thickness of a slab by rolling it through the working rolls of a rolling mill.
[0011] The rolled plate manufactured by the plate rolling technology of this common rolling mill is stretched in the length direction during the rolling process, but its width direction is no different from the width of the initial slab. In order to carry out wide-width rolling, it is necessary to cast a wide-width slab for rolling, so not only the slab manufacturing equipment, but also the scale of the hot rolling mill and the cold rolling mill has the problem of increasing. This problem also exists in the extrusion process. Since it is necessary to cast an ultra-large slab and manufacture an ultra-large extrusion die of a large extruder that can perform wide-width extrusion for extrusion, there are clear technical constraints based on wide-width extrusion. In addition, in order to make the thickness of the hot extruded material more than 10 tons, additional hot rolling is required. As the scale of the extruder increases, the pressure added to the extruder and the extrusion die increases. In order to reduce this pressure, there is a problem that the thickness of the extruded material needs to be increased.
[0012] Therefore, increasing the size of the extruder for wide-width extrusion will increase the investment cost of the equipment exponentially, thereby increasing the burden on the extrusion manufacturer. The manufacturing cost of the super-large extrusion die used for wide-width extrusion is also very expensive. In addition, as the pressure applied to the extrusion die increases, there is a problem of shortening the life of the extrusion die and increasing engineering costs.
[0013] [Prior technical literature]
[0014] [Patent Literature]
[0015] (Patent Document 0001) Korean Registered Patent No. 10-1328216
[0016] (Patent Document 0002) Korean Registered Patent No. 10-1485642
[0017] (Patent Document 0003) Korean Registered Patent No. 10-1639145
[0018] (Patent Document 0004) Korean Registered Patent No. 10-2487222 Summary of the invention
[0019] Technical issues to be solved
[0020] The present invention is developed to solve the problems of the prior art as described above, and its purpose is to provide a method for manufacturing a wide-width extruded plate for calendering, which can use a small or medium-sized extruder to manufacture a wide-width extruded material with a relatively wide width.
[0021] That is, the object of the present invention is to provide a method for manufacturing wide-width plate materials, which method, after manufacturing a corrugated extruded plate material with a curved cross-section in a hot extrusion step, flattens the curved cross-section by upper and lower rollers, thereby enabling the wide-width plate materials to be manufactured using relatively small equipment.
[0022] Problem Solution
[0023] In order to solve the above-mentioned purpose, the wide-width plate manufacturing method based on the present invention includes: a slab preheating step, preheating a slab with a circular or elliptical cross-section; an extrusion step, using an extrusion die with a curved forming hole to extrude the preheated slab to extrude a plate with a curved cross-section in the width direction; and a flattening step, using a flattening roller to flatten the extruded plate.
[0024] Preferably, in the slab preheating step, the preheating temperature is 400°C to 550°C.
[0025] Preferably, the flattening step is performed before the sheet is coiled.
[0026] The cross section of the extruded sheet extruded in the extrusion step has a symmetrical shape that is repeated in a sinusoidal wave shape.
[0027] Preferably, the flattening step is performed before or after cooling the extruded sheet, and then the sheet is made into a coil.
[0028] Effects of the Invention
[0029] Based on the wide-width plate manufacturing method of the present invention, an extruded plate with a curved cross-section is extruded using a small or medium-sized extruder, and flattened in the flattening step, thereby having the effect of being able to manufacture relatively wide extruded flat plate materials compared to extruded plates extruded by existing extruders.
[0030] In addition, the present invention can manufacture the thickness of the extruded material within 10 tons by extruding with a small or medium-sized extruder, which does not impose a burden on the extruder, thereby having the effect of preventing the extruder and the extrusion die from shortening their service life. In addition, relatively wide hot-rolled plates can be manufactured using small or medium-sized extruders, thereby having the effect of reducing the investment cost of large extruders and large extrusion dies.
[0031] In addition, since the output roller attached to the existing extruder can be used without modification, the investment cost required for equipment modification can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 This is a manufacturing process diagram of an example of a wide-width plate manufacturing method according to the present invention.
[0033] Figure 2 This is a manufacturing process diagram of another example of the wide-width plate manufacturing method based on the present invention.
[0034] Figure 3This is a cross-sectional view of another example in which the curved extruded plate material extruded in the extrusion step and the flat extruded flat plate material after the flattening step are different from each other in the wide plate manufacturing method based on the present invention.
[0035] The reference numerals are described as follows:
[0036] 10: Curved plate
[0037] 10s: bending part
[0038] 20: Extruded flat material DETAILED DESCRIPTION
[0039] The present invention can be implemented with various changes. Here, specific embodiments are shown in the drawings and described in detail. However, this is not intended to limit the present invention to specific embodiments, and should be understood to include all changes, equivalents and substitutes belonging to the thought and technical scope of the present invention.
[0040] In describing the various drawings, similar reference numerals are used for similar components. When a detailed description of a related known technology may make the gist of the present invention unclear when describing the present invention, the detailed description is omitted.
[0041] The invention can manufacture wide-width extruded materials with a relatively wide width by using a small or medium-sized extruder.
[0042] The manufacturing method of wide-width extruded plate for calendering based on the present invention is characterized in that it includes: a plate preheating step, in which a plate with a circular or elliptical cross-section is preheated; an extrusion step, in which the preheated plate is extruded using an extrusion die with a curved forming hole, thereby extruding a plate with a curved cross-section in the width direction; and a flattening step, in which the extruded plate is flattened using a flattening roller.
[0043] As mentioned above, the existing method for manufacturing hot-rolled plates includes rolling with extruded materials or hot-rolling and then cold-rolling cast slabs. The width of the plates manufactured in this way hardly increases during hot rolling or cold rolling. Therefore, in order to manufacture a relatively wide plate, it is necessary to make the size (width) of the slab very large for casting, or use a large-capacity extruder for wide extrusion during extrusion, and it is necessary to manufacture an ultra-large extrusion die that can be extruded by a large extruder for extrusion. In addition, in order to increase the scale of the extruder to make the thickness of the hot extruded material more than 10 tons, additional hot rolling is required. That is, as the scale of the extruder increases, the pressure applied to the extruder and the extrusion die increases. In order to reduce this pressure, the thickness of the extruded material needs to be increased.
[0044] In addition, in order to extrude a wide width, the scale of the extruder becomes larger, and the investment cost of the equipment increases exponentially, thereby increasing the burden on the extrusion manufacturer. The manufacturing cost of the extrusion die used for wide width extrusion is also very expensive. Moreover, as the pressure applied to the extrusion die increases, the life of the extrusion die shortens, and the engineering cost does not decrease but increases.
[0045] However, as described above, the present invention extrude a plate having a curved cross section in the width direction in the extrusion step and flattens it in the flattening step, thereby enabling the extruded plate to be manufactured using a small or medium-sized extruder.
[0046] That is, in the method for manufacturing wide-width plates of the present invention, in the extrusion step, a small or medium-sized extruder with a maximum width of less than 450 mm is used to extrude a plate having a curved cross-section. Thereafter, the plate is flattened by a roller in the flattening step, so that the width can be enlarged to a maximum of 900 mm. Furthermore, when the extrusion step is carried out using an extruder that can extrude a width of 650 mm, the width of the final rolled plate can be manufactured to a maximum of 1300 mm. Therefore, a smaller extruder can be used to manufacture large plates.
[0047] Therefore, by performing extrusion in a small or medium-sized extruder, the thickness of the extruded material can be manufactured to be within 10 tons, and no burden is imposed on the extruder, so the life of the extruder and the extrusion die can be prevented from being shortened.
[0048] Furthermore, in the present invention, since a relatively wide rolled plate can be manufactured using a small extruder, and since a large extruder and a large extrusion die are not used, the investment cost therefor can be reduced, and the bent cross-section of the extruded material before bending and cooling can be manufactured into a flat cross-section and rolled into a coil, thereby reducing the load on the flattening roller.
[0049] The flattening step is a step of making the curved surface into a flat plate, which can be implemented before the plate coiling machine. The height of the roller can be adjusted using the principle of the balancer, thereby flattening the corrugated extruded plate.
[0050] Taking the flattening step as an example, the feed port is kept at a distance of about 60 mm or more to facilitate the input of the extruded material. The intervals between the rollers are narrowed by grading and finally have a distance of 8 to 10 mm. The minimum setting of the rollers is 2 or more levels, and the corrugated extruded sheet is flattened by passing through multiple levels of rollers in sequence.
[0051] In the slab preheating step, the preheating temperature is preferably 400-550° C., and the flattening step is performed before coiling the slab into a coil.
[0052] The cross section of the extruded sheet extruded in the extrusion step can be made as follows Figure 3The various forms of bends shown are preferably formed so that the angle of the vertical portion is less than 90 degrees and the overall shape is repeated symmetrically in a sinusoidal wave shape, so that platform operations can be easily implemented.
[0053] The planarization step is preferably as follows Figure 2 as shown before the cooling step of the extruded sheet, or as Figure 1 This is shown after a cooling step before production into coils.
[0054] The existing hot extrusion plate manufacturing method cannot obtain a cross-sectional width of more than 450mm in a 12-inch extruder, and cannot obtain a cross-sectional width of more than 600mm in a 17-inch extruder. However, as mentioned above, the wide-width plate manufacturing method of the present invention can produce extruded plates with a width of more than 10% to about twice the maximum width that can be extruded by the extruder by extruding a curved cross-section.
[0055] That is, by flattening an extruded sheet having a corrugated extruded cross-section (a cross-section in the width direction forming a waveform) in a flattening step, a final extruded sheet having a width that is up to twice the width of the corrugated extruded sheet and that is flat and wide for calendering can be produced.
Claims
1. A method for manufacturing a wide extruded sheet for calendering, A slab preheating step for preheating the slab having a circular or elliptical cross section; An extrusion step, using an extrusion die formed with a curved forming hole to extrude the preheated slab to extrude a plate having a curved cross section in the width direction; and In the flattening step, the extruded sheet is flattened using two or more levels of flattening rollers.
2. The method for producing a wide extruded sheet for calendering according to claim 1, It is characterized in that In the slab preheating step, the preheating temperature is 400°C to 550°C.
3. The method for manufacturing a wide extruded sheet for calendering according to claim 1, It is characterized in that The flattening step is performed before the coil is rolled into a coil.
4. The method for producing a wide extruded sheet for calendering according to claim 1, It is characterized in that The cross section of the extruded sheet extruded in the extrusion step has a symmetrical shape that is repeated in a sinusoidal wave shape.
5. The method for manufacturing a wide extruded sheet for calendering according to claim 1, It is characterized in that The flattening step is performed before or after the extruded sheet is cooled.
Citation Information
Patent Citations
Method for preparing metal plane plate
CN102179422A
Wide magnesium alloy ultra-thin plate continuous extrusion device and method
CN102229044A
Process and equipment for manufacturing wide-width magnesium alloy plate in coils
CN102489958A
Die for double width aluminium plate extruding and manufacturing method of double width aluminium plate