Swinging welding wire indirect electric arc narrow gap welding device and method

By using swinging wire device in thick-wall structure welding, the welding wire periodically swings to both sides of the bevel during welding, solving the problem that the arc is difficult to heat the side walls in narrow gap welding, improving welding efficiency and quality, and reducing the Unfusion defect.

CN118926657APending Publication Date: 2024-11-12HARBIN INST OF TECH AT WEIHAI
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310517662.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In thick-wall structure welding, arcs are easily generated between the electrode and the bevel side wall during narrow gap welding, resulting in low welding efficiency, high residual stress and serious non-fusion defects, and conventional indirect arc welding devices are difficult to achieve under extremely narrow gaps. Effectively heat the bevel side walls.

Method used

The swinging wire device is used to make the welding wire swing periodically to both sides of the bevel during welding. Indirect arcs are generated between the end of the welding wire and the electrodes. The end of the welding wire swings to both sides of the bevel through the rotating module to improve arcing The heating effect of the side walls avoids the defect of the side walls without fusion.

Benefits of technology

It improves welding efficiency and welding quality, reduces unfusion defects, and enhances welding stability and filling efficiency for thick-wall structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926657A_ABST
    Figure CN118926657A_ABST
Patent Text Reader

Abstract

The invention discloses a swinging welding wire indirect electric arc ultra-narrow gap welding device and method. The device comprises a welding gun part, a wire feeding part, a rotating module and an insulating fixing plate. The insulating fixing plate is clamped on the walking mechanism, and the welding gun part, the wire feeding part and the rotating module are fixed on the insulating fixing plate and are insulated from one another. And the welding wire is connected with the positive electrode of the power supply through the wire feeding pipe, the conductive clamping block and the conductive rod. In the welding process, the end of the welding wire is driven by the rotating module to periodically swing to the two sides of the groove in a reciprocating mode. On one hand, arc starting of the side wall can be avoided through the characteristic that the workpiece is not powered on, the groove gap width is reduced, and the welding efficiency is improved. And on the other hand, the periodic swing of the welding wire can remarkably enhance the heating effect of the electric arc on the side wall of the groove, molten pool metal is promoted to spread towards the two sides of the groove, the defect that the side wall is not fused easily in the narrow gap welding process is overcome, and the joint quality is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of welding, and more particularly to a swing welding wire indirect arc ultra-narrow gap welding device and method. Background Art

[0002] In the field of thick-walled structure welding, narrow gap welding technology uses a groove with a very small angle for fill welding. Because of its small groove size, less welding materials are required to be filled, it has many advantages such as high welding efficiency, good joint performance and low residual stress, and has become one of the most competitive thick-walled structure welding technologies. The improvement in welding efficiency is mainly attributed to the reduction in groove gap width. However, when the groove gap width is reduced to less than 10 mm, the welding arc is very likely to be generated between the electrode and the groove side wall, and welding cannot be performed. Therefore, reducing the groove gap width and further improving production efficiency have become important development directions of narrow gap welding technology.

[0003] Unlike conventional welding methods, the workpiece is not connected to electricity during indirect arc welding, and the arc is generated between the electrodes. Therefore, using indirect arc for narrow gap welding can avoid the arc being generated between the electrode and the side wall of the groove. In addition, the energy of the arc is mainly used to heat the electrode material, and the melting efficiency of the welding material is significantly improved. In order to improve the filling efficiency of the welding material, Dalian University of Technology has developed and studied a three-wire gas shielded indirect arc welding method, device, surfacing method and narrow gap welding method (Chinese patent application number 201510145041.4). The above invention mainly focuses on improving the melting efficiency of the welding material, and still welds in a narrow gap groove with a gap width of more than 10 mm. And because the groove gap width is large, the arc energy is difficult to effectively heat the side wall of the groove, resulting in serious residual unfused defects after welding. In addition, using three consumable welding wires as electrodes, the stability of the welding process is poor and the welding quality is difficult to control. Harbin Institute of Technology has developed and studied a device and method for ultra-narrow gap welding of thick-walled structures based on indirect arc (Chinese patent application number 2023104846437). A non-consumable tungsten electrode and a molten welding wire are used as two electrodes for welding in a groove with a gap width of ≤6 mm. The high temperature zone of the arc can directly heat the side wall of the groove. However, during the welding process, large thick-walled structures conduct heat very quickly, and side wall unfused defects may still occur after welding. Summary of the invention

[0004] In view of this, the main purpose of the present invention is to provide an indirect arc ultra-narrow gap welding device and method using a swinging welding wire. On the one hand, the problem of arc starting on the side wall is avoided by utilizing the fact that the workpiece is not connected to electricity during indirect arc welding, so that the indirect arc can fill the ultra-narrow gap groove with welding. On the other hand, the use of a swinging welding wire device allows the welding wire to periodically swing toward both sides of the groove during welding, which can effectively promote the arc to heat the side wall metal of the workpiece and suppress the side wall unfusion defect that is very easy to occur during the narrow gap welding of thick-walled structures.

[0005] In a first aspect of the present invention, a swing wire indirect arc ultra-narrow gap welding device is provided. The device comprises a welding gun part, a wire feeding part, a rotating module and an insulating fixing plate. The insulating fixing plate is clamped on a traveling mechanism, and the welding gun part, the wire feeding part and the rotating module are fixed on the insulating fixing plate and insulated from each other.

[0006] Preferably, the welding gun part comprises a welding gun, an electrode and a ceramic nozzle. The electrode is electrically connected to the negative electrode of the power supply through the welding gun. The ceramic nozzle is filled with inert gas such as pure argon and extends into the groove to protect the electrode, arc and molten pool metal.

[0007] Preferably, the welding wire is connected to the positive electrode of the power supply through a wire feeding tube-conductive clamping block-conductive rod, and is clamped on the insulating fixed plate through a rotating module.

[0008] Preferably, the rotating module comprises a reduction motor, a transmission part, a bearing with a seat and a housing. The reduction motor and the bearing with a seat are assembled inside the housing, and the housing is made of an insulating material with good rigidity to ensure insulation between the motor and the conductive rod. The rotating module is sealed inside the housing to avoid external interference and pollution.

[0009] Preferably, the seat bearing limits the conductive rod, the inner ring of the seat bearing is fixed to the conductive rod, and the conductive rod can only rotate around itself as the axis under the drive of the motor.

[0010] Preferably, the reduction motor drives the conductive rod to rotate back and forth periodically through the transmission part, so that the end of the welding wire swings back and forth periodically toward both sides of the groove during welding. The transmission mode includes but is not limited to gear transmission, chain transmission, belt transmission and worm transmission.

[0011] Preferably, the extreme positions where the end of the welding wire swings toward both sides of the groove should avoid contact with the side wall metal, so as to avoid a short circuit between the welding wire and the side wall metal of the groove.

[0012] Preferably, the swing speed, swing amplitude, swing frequency and the dwell time of the welding wire to both sides are adjusted by the motor speed, the amplitude of the unidirectional rotation of the motor in one cycle, the motor rotation reversing frequency and the motor rotation reversing dwell time.

[0013] Preferably, the rotating module is assembled on the insulating fixed plate through the housing and the adjusting plate. The height of the welding wire end is adjusted by the housing and the adjusting plate, and the distance between the welding wire end and the electrode end is adjusted by the adjusting plate and the insulating fixed plate.

[0014] Preferably, the indirect arc is generated between the electrode end and the welding wire end, and periodically swings back and forth toward both sides of the groove under the pulling action of the welding wire end, thereby improving the heating effect on the side wall of the groove.

[0015] In a second aspect of the present invention, taking thick plate welding as an example, a method for ultra-narrow gap welding using the above-mentioned oscillating wire indirect arc ultra-narrow gap welding device is provided, comprising the following steps:

[0016] Step 1: Preset a certain angle of reverse deformation on the thick plate with groove processed and fix it by spot welding, clean the welding area and the nearby metal surface, and fix the thick plate to be welded on the welding platform by a clamp;

[0017] Step 2: Adjust the electrode end and the welding wire end to the appropriate position according to actual needs and fix them;

[0018] Step 3: Turn on the travel mechanism, welding power supply, rotating module power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, welding wire swing amplitude, welding wire swing cycle, dwell time after the welding wire swings to both sides, and gas flow of each ceramic nozzle;

[0019] Step 4: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, and start the arc after the shielding gas is introduced in advance for a period of time. After the arc is generated, the walking mechanism drives the welding gun to move to the arc-extinguishing end. During the welding process, the rotating module drives the conductive rod to drive the welding wire to swing back and forth periodically on both sides of the groove. After the end of the welding wire reaches the arc-extinguishing end, the arc is extinguished. When the welding wire swings to the middle position of the groove, it stops swinging. After a period of delayed gas supply, the gas valve is closed and the welding gun is moved to other designated positions. Repeat the above welding process continuously, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] The above and other objects, features and advantages of the present invention will become more apparent through the following description of the embodiments of the present invention with reference to the accompanying drawings, in which:

[0021] Figure 1 It is a schematic structural diagram of the indirect arc ultra-narrow gap welding device of the oscillating welding wire of the present invention.

[0022] In the figure, 1 is a welding gun, 2 is a ceramic nozzle, 3 is an electrode, 4 is a welding wire, 5 is a wire feeding tube, 6 is a conductive clamp, 7 is a conductive rod, 8 is a rotating module, 9 is a reduction motor, 10 is a seat bearing, 11 is a transmission part, 12 is a rotating module housing, 13 is a positioning plate, 14 is an insulating fixing plate, 15 is a welding gun clamp, 16 is a base plate, and 17 is a groove.

[0023] Figure 2 It is a schematic diagram of the welding wire at the center of the groove and swinging to the left and right sides of the groove.

[0024] In the figure, 1 is the wire feeding tube, 2 is the welding wire, and 3 is the groove.

[0025] Figure 3 Schematic diagram of the movement trajectory of the welding wire end during welding.

[0026] In the figure, 1 is the wire feeding tube, 2 is the welding wire, 3 is the moving track of the end of the welding wire, and 4 is the groove.

[0027] These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention. DETAILED DESCRIPTION

[0028] The present invention is described below based on examples, but the present invention is not limited to these examples. In the detailed description of the present invention below, some specific details are described in detail. It is possible for those skilled in the art to fully understand the present invention without the description of these details. In order to avoid confusing the essence of the present invention, known methods, processes, flows, and elements are not described in detail.

[0029] In addition, persons of ordinary skill in the art will appreciate that the drawings provided herein are for illustration purposes only and are not necessarily drawn to scale.

[0030] Unless the context clearly requires otherwise, throughout the specification and claims, the words "include", "comprising" and similar words should be interpreted in an inclusive sense rather than an exclusive or exhaustive sense; that is, in the sense of "including but not limited to".

[0031] In the description of the present invention, it should be understood that the terms "first", "second", etc. are only used for description and cannot be understood as indicating or implying relative importance. In addition, in the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0032] Various embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. The described exemplary embodiments are intended to help understand the present invention and are not intended to limit the scope of the present invention in any way.

[0033] The present invention provides an oscillating wire indirect arc ultra-narrow gap welding device and method, which enables the end of the welding wire to periodically reciprocate toward both sides of the groove on the basis of indirect arc ultra-narrow gap welding, so as to improve the fusion state of the groove side wall. The structure and use method of the oscillating wire indirect arc ultra-narrow gap welding device of the present invention are introduced in combination with specific examples:

[0034] like Figure 1 As shown, the oscillating wire indirect arc ultra-narrow gap welding device provided by the present invention comprises a welding gun part, a wire feeding part, a rotating module 8 and an insulating fixing plate 14. The insulating fixing plate 14 is clamped on the walking mechanism, and the welding gun part, the wire feeding part and the rotating module 8 are clamped on the insulating fixing plate 14 and insulated from each other.

[0035] The welding gun part includes a welding gun 1, an electrode 3 and a ceramic nozzle 2. The electrode 3 is electrically connected to the negative electrode of the power supply through the welding gun 1. The ceramic nozzle 2 is filled with an inert gas such as pure argon and extends into the groove to protect the electrode 3, the arc and the molten pool metal. Preferably, in order to avoid burning of the electrode 3 and ensure good arc stability, the electrode 3 is made of a high melting point material such as tungsten.

[0036] The welding wire 4 is connected to the positive pole of the power supply through the wire feeding tube 5-conductive clamping block 6-conductive rod 7, and is clamped on the insulating fixing plate 14 through the rotating module 8.

[0037] The rotating module 8 includes a reduction motor 9, a transmission part 11, a bearing seat 10 and a housing 12. The reduction motor 9 and the bearing seat 10 are assembled on the inner side of the housing 12. The housing 12 is made of an insulating material with good rigidity to ensure that the reduction motor 9 is insulated from the conductive rod 7. The rotating module 8 is sealed inside the housing 12 to avoid external interference and pollution. The bearing seat 10 limits the conductive rod 7. The inner ring of the bearing seat 10 is fixed to the conductive rod 7. The conductive rod 7 can only rotate around itself as the axis under the drive of the reduction motor 9. The reduction motor 9 drives the conductive rod 7 to rotate periodically reciprocatingly through the transmission part 11, so that the end of the welding wire 4 swings back and forth to both sides of the groove 17 during the welding process. The transmission method includes but is not limited to gear transmission, chain transmission, belt transmission and worm transmission.

[0038] Preferably, the extreme positions where the end of the welding wire 4 swings toward both sides of the groove 17 should avoid contact with the side wall metal, so as to avoid short circuit between the welding wire 4 and the side wall metal of the groove 17.

[0039] Preferably, the swing speed, swing amplitude, swing frequency and the dwell time of the end of the welding wire 4 to both sides are adjusted by the rotation speed of the reduction motor 9, the amplitude of unidirectional rotation within a cycle, the rotation reversing frequency and the rotation reversing dwell time.

[0040] Preferably, the rotating module 8 is assembled on the insulating fixing plate 14 through the housing 12 and the adjusting plate 13. The height of the end of the welding wire 4 is adjusted by the housing 12 and the adjusting plate 13, and the distance between the end of the welding wire 4 and the end of the electrode 3 is adjusted by the adjusting plate 13 and the insulating fixing plate 14.

[0041] Preferably, the indirect arc is generated between the end of the electrode 3 and the end of the welding wire 4, and the arc is periodically reciprocated to both sides of the groove 17 under the pulling action of the end of the welding wire 4, so as to improve the heating effect on the side wall of the groove. Figure 2 shown.

[0042] Taking thick plate welding as an example, the method for using the oscillating welding wire indirect arc ultra-narrow gap welding device provided by the present invention is as follows:

[0043] Step 1: Grind the welding area and nearby metal surfaces of the thick plate with grooves processed, and use volatile organic solvents such as acetone or ethanol to wipe off the oil and dust on the surface. Preset the plates with a certain angle of reverse deformation, splice them together, spot weld them on the back, and then fix them on the welding platform with a clamp;

[0044] Step 2: Adjust the electrode end and the welding wire end to the appropriate position according to actual needs and fix them, check and ensure that the electrode and welding wire are in good electrical conduction with the negative and positive electrodes of the welding power source respectively, ensure that there is no conduction between the electrode and the welding wire, and check the shape of the electrode and the smoothness of wire feeding;

[0045] Step 3: Turn on the travel mechanism, welding power supply, rotating module power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, welding wire swing amplitude, welding wire swing cycle, dwell time after the welding wire swings to both sides and gas flow of each ceramic nozzle;

[0046] Step 4: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, and start the arc after the shielding gas is introduced in advance for a period of time. After the arc is generated between the electrode and the welding wire, the walking mechanism drives the welding gun to move to the arc-extinguishing end. During the welding process, the rotating module drives the conductive rod to drive the welding wire to swing back and forth periodically on both sides of the groove. When the end of the welding wire swings to the side wall of the groove, the arc directly heats the metal on the side wall of the groove, and the molten droplets formed by the melting of the end of the welding wire can also directly transfer to both sides of the groove. After the end of the welding wire reaches the arc-extinguishing end, the arc is extinguished. When the welding wire swings to the middle position of the groove, it stops swinging, and the gas valve is closed after a period of delayed gas supply, and the welding gun is moved to other specified positions. The movement trajectory of the end of the welding wire is as follows: Figure 3 Repeat the above welding process continuously, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height.

[0047] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A device and method for ultra-narrow gap welding with an indirect arc using an oscillating welding wire, characterized in that: The method suppresses the side wall non-fusion defect that is easily generated in the indirect arc ultra-narrow gap welding process by periodically swinging the welding wire back and forth toward both sides of the groove.

2. A swing wire indirect arc ultra-narrow gap welding device, characterized in that: The invention comprises a welding gun part, a wire feeding part, a rotating module and an insulating fixing plate. The insulating fixing plate is clamped on the walking mechanism, and the welding gun part, the wire feeding part and the rotating module are fixed on the insulating fixing plate and insulated from each other.

3. The oscillating wire indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The welding wire is connected to the positive electrode of the power supply through a wire feeding tube, a conductive clamping block and a conductive rod, and is clamped on an insulating fixed plate through a rotating module.

4. The oscillating wire indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The rotating module includes a reduction motor, a transmission part, a bearing with a seat and a housing. The reduction motor and the bearing with a seat are assembled on the inner side of the housing, and the housing is made of an insulating material with good rigidity to ensure the insulation between the motor and the conductive rod. The bearing with a seat limits the conductive rod, and the conductive rod can only rotate around itself as the axis.

5. The oscillating wire indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The reduction motor drives the conductive rod to rotate periodically through the transmission part, so that the end of the welding wire swings back and forth toward both sides of the groove during welding. The transmission mode includes but is not limited to gear transmission, chain transmission, belt transmission and worm transmission.

6. The oscillating wire indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The rotating module is assembled on the insulating fixed plate through the shell and the adjusting plate. The height of the welding wire end and the distance between the welding wire end and the electrode end are adjusted by changing the positions of the three.

7. The oscillating wire indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The electrode is connected to the negative pole of the power supply through a welding gun. An indirect arc is generated between the end of the electrode and the end of the welding wire and heats the substrate and the welding wire.

8. A method for welding using the oscillating wire indirect arc ultra-narrow gap welding device according to any one of claims 2 to 7, characterized in that: The steps include: Step 1: Spot weld and fix the thick plate with grooves, clean the surface and clamp it on the welding platform. Adjust the electrode end and the welding wire end to the appropriate position according to actual needs and fix them; Step 2: Turn on the travel mechanism, welding power supply, rotating module power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, welding wire swing amplitude, welding wire swing cycle, dwell time after the welding wire swings to both sides, and gas flow of each ceramic nozzle; Step 3: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, and start the arc after the shielding gas is introduced in advance for a period of time. After the arc is generated, the walking mechanism drives the welding gun to move to the arc-extinguishing end. During the welding process, the rotating module drives the conductive rod to drive the welding wire to swing back and forth periodically on both sides of the groove. The arc is extinguished after the end of the welding wire reaches the arc-extinguishing end. The welding wire stops swinging when it swings to the middle position of the groove. After a period of delayed gas supply, the gas valve is closed and the welding gun is moved to other designated positions. Repeat the above welding process continuously, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height.

Citation Information

Cited By

  • Self-adaptive variable-parameter composite swing welding control method and related equipment

    CN121635006A