Magnetic control swing indirect arc ultra-narrow gap welding device and method
Through the magnetically controlled oscillation indirect arc welding device, the arc swing is driven by an external magnetic field in a thick-wall structure, and the problems of side wall arcing and poor heating effects in narrow gap welding are solved, and stable welding and efficient fusion under small gap width are achieved. .
Patent Information
- Application Number
- CN202310517933.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-12
AI Technical Summary
In thick-wall structure welding, it is difficult for the prior art to stabilize welding in a bevel with a gap width less than 10 mm, and the side wall arcing and heating effects are poor, resulting in the presence of unfusion defects.
The magnetically controlled oscillation indirect arc welding device is used to drive the arc to periodically swing back and forth on both sides of the bevel through an external magnetic field to avoid the arcing of the side wall and promote the heating of the side wall metal. The indirect arc welding workpiece is not connected to the electrical connection, and the slope is reduced. Width of the opening gap and protection and heating are achieved through ceramic nozzles and magnetron components.
The side wall arcing is effectively avoided, the wire deposition efficiency and the fusion quality of the side wall are improved, the unfusion defects are reduced, and stable welding in a narrower gap is achieved.
Smart Images

Figure CN118926658A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of welding, and more specifically to a magnetically controlled swing indirect arc ultra-narrow gap welding device and method. Background Art
[0002] In the field of thick-walled structure welding, narrow gap welding technology has become a highly anticipated emerging welding technology with its smaller groove size and higher welding efficiency. The improvement in welding efficiency is mainly attributed to the reduction in groove gap width. Reducing the groove gap width and further improving production efficiency have become important development directions for narrow gap welding technology. However, when the gap width is less than 10 mm, the arc easily climbs from the bottom of the groove to the side wall of the groove, making welding impossible. Therefore, a new ultra-narrow gap welding technology that can stably weld in narrower grooves is urgently needed.
[0003] Unlike conventional welding methods, the workpiece is not connected to electricity during indirect arc welding, and the arc is generated between the electrodes. Therefore, placing the indirect arc in a narrow gap groove for welding can avoid the problem of arc starting on the side wall, thereby further reducing the groove gap width. In addition, the energy of the arc directly acts on the melting of the welding wire, which can significantly improve the deposition efficiency of the welding wire. Dalian University of Technology has developed and studied a three-wire gas shielded indirect arc welding method, device, surfacing method and narrow gap welding method (Chinese patent application number 201510145041.4). The above method focuses on improving the melting efficiency of the welding material rather than solving the problem of arc starting on the side wall. It still welds in a groove with a gap width of more than 10 mm, and the heating effect on the side wall of the groove is poor, making it difficult to obtain a well-fused joint. Harbin Institute of Technology has developed and studied an ultra-narrow gap welding device and method for thick-walled structures based on indirect arc (Chinese patent application number 2023104846437). A non-consumable tungsten electrode and a molten welding wire are used as two electrodes for welding in a groove with a gap width of ≤6 mm. The high temperature zone of the arc can directly heat the side wall of the groove. However, during the welding process, large thick-walled structures conduct heat very quickly, and side wall unfused defects may still occur after welding. Harbin Institute of Technology has developed and studied a magnetically controlled swing arc GTAW welding device and method (Chinese patent application number 202111000615.0). The welding heat source is a conventional GTAW arc, which is suitable for welding conventional narrow gap grooves with a groove gap of >10 mm. Summary of the invention
[0004] In view of this, the main purpose of the present invention is to provide a magnetically controlled swinging indirect arc ultra-narrow gap welding device and method. On the one hand, the characteristic that the workpiece is not connected to electricity during indirect arc welding is utilized to avoid the problem of arc starting on the side wall, so that the indirect arc can be used for filling welding in the ultra-narrow gap groove of ≤6 mm. On the other hand, the indirect arc is driven by an external magnetic field to swing back and forth periodically on both sides of the groove during the welding process, which can effectively promote the arc to heat the side wall metal of the workpiece and suppress the side wall unfusion defects that are very easy to occur during the narrow gap welding of thick-walled structures.
[0005] In a first aspect of the present invention, a magnetically controlled swinging indirect arc ultra-narrow gap welding device is provided. The device comprises a wire feeding unit, a welding gun unit, a magnetic control unit and an insulating fixing plate. The insulating fixing plate is clamped on a traveling mechanism, and the wire feeding unit, the welding gun unit and the magnetic control unit are clamped on the insulating fixing plate and are insulated from each other.
[0006] Preferably, the wire feeding unit comprises a welding wire, a wire feeding tube, a ceramic nozzle, a conductive clamping block and a conductive rod. The welding wire is connected to the positive electrode of the welding power source.
[0007] Preferably, the welding gun part mainly includes a welding gun, an electrode and a ceramic nozzle. The electrode is connected to the negative electrode of the welding power supply through an electrode clamp in the welding gun. A protective gas is introduced into the ceramic nozzle to protect the welding area.
[0008] Preferably, the diameters of the electrode, the ceramic nozzle, and the wire feeding tube are all smaller than the groove gap width, and can be extended into the groove for welding and protection.
[0009] Preferably, the magnetron includes a coil frame, a coil and a magnetic core. The coil frame is made of an insulating material with good rigidity and can withstand high temperatures. The enameled copper wire is wound layer by layer on the outside of the coil frame, and the copper wires between the layers are separated by insulating paper or insulating paint to ensure mutual insulation, and the two ends of the copper wire are respectively connected to the two poles of the magnetron power supply. The diameter and number of turns of the coil are adjusted according to actual needs.
[0010] Preferably, the magnetic core passes through the inner side of the coil frame and is fixed to the coil frame. The magnetic core is made of high magnetic permeability materials such as silicon steel sheets or ferrites. The shape and size of the end of the magnetic core near the arc zone are designed according to actual needs. The thickness of the end of the magnetic core should be less than the width of the groove gap to avoid contact with the side wall metal during welding.
[0011] Preferably, the upper end of the magnetic core is fixed to the insulating fixing plate by a clamping block, and the distance between the lower end and the electrode is adjusted according to demand, so as to increase the magnetic induction intensity in the arc zone as much as possible while ensuring that the magnetic core is not damaged.
[0012] Preferably, the waveform, peak value and alternating frequency of the excitation current passed into the coil are adjusted by the magnetron power supply according to requirements.
[0013] Preferably, the indirect arc is generated between the electrode and the end of the welding wire, and is driven by an external alternating magnetic field to periodically swing back and forth toward both sides of the groove to promote the melting of the side wall metal.
[0014] In a second aspect of the present invention, taking thick plate welding as an example, a method for ultra-narrow gap welding using the above-mentioned magnetically controlled swing indirect arc ultra-narrow gap welding device is provided, comprising the following steps:
[0015] Step 1: Preset a certain amount of reverse deformation on the thick plate with the groove processed and the surface cleaned, and clamp it on the welding platform through a fixture;
[0016] Step 2: Adjust the electrode end, welding wire end and magnetic core end to appropriate positions and fix them according to actual needs;
[0017] Step 3: Turn on the travel mechanism, welding power supply, magnetron power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, excitation current waveform, excitation current peak value, excitation current alternating frequency and gas flow rate of each ceramic nozzle;
[0018] Step 4: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, and start the arc after the shielding gas is introduced for a period of time in advance. After the arc is generated, turn on the external magnetic field, and the walking mechanism drives the welding gun to move to the arc-extinguishing end. During the welding process, the indirect arc periodically swings back and forth on both sides of the groove. After the end of the welding wire reaches the arc-extinguishing end, the arc is extinguished, the external magnetic field is turned off, and the gas valve is closed after the gas is delayed for a period of time, and the welding gun is moved to other designated positions. Repeat the above welding process, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The above and other objects, features and advantages of the present invention will become more apparent through the following description of the embodiments of the present invention with reference to the accompanying drawings, in which:
[0020] Figure 1 It is a schematic structural diagram of the magnetically controlled swing indirect arc ultra-narrow gap welding device of the present invention.
[0021] In the figure, 1 is a welding gun, 2 is a ceramic nozzle, 3 is an electrode, 4 is a welding wire, 5 is a wire feeding tube, 6 is a conductive clamp, 7 is a conductive rod, 8 is a conductive rod clamp, 9 is a positioning clamp, 10 is an insulating fixing plate, 11 is an assembly hole, 12 is a welding gun clamp, 13 is a magnetic core clamp, 14 is a coil frame, 15 is a coil, 16 is a magnetic core, 17 is a substrate, and 18 is a groove.
[0022] Figure 2 Schematic diagram of the indirect arc at the center of the groove and swinging to the left and right sides of the groove.
[0023] In the figure, 1 is the electrode, 2 is the indirect arc, 3 is the substrate, and 4 is the groove.
[0024] These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention. DETAILED DESCRIPTION
[0025] The present invention is described below based on examples, but the present invention is not limited to these examples. In the detailed description of the present invention below, some specific details are described in detail. It is possible for those skilled in the art to fully understand the present invention without the description of these details. In order to avoid confusing the essence of the present invention, known methods, processes, flows, and elements are not described in detail.
[0026] In addition, persons of ordinary skill in the art will appreciate that the drawings provided herein are for illustration purposes only and are not necessarily drawn to scale.
[0027] Unless the context clearly requires otherwise, throughout the specification and claims, the words "include", "comprising" and similar words should be interpreted in an inclusive sense rather than an exclusive or exhaustive sense; that is, in the sense of "including but not limited to".
[0028] In the description of the present invention, it should be understood that the terms "first", "second", etc. are only used for description and cannot be understood as indicating or implying relative importance. In addition, in the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0029] Various embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. The described exemplary embodiments are intended to help understand the present invention and are not intended to limit the scope of the present invention in any way.
[0030] The present invention provides an oscillating wire indirect arc ultra-narrow gap welding device and method, which enables the end of the welding wire to periodically reciprocate toward both sides of the groove on the basis of indirect arc ultra-narrow gap welding, so as to improve the fusion state of the groove side wall. The structure and use method of the oscillating wire indirect arc ultra-narrow gap welding device of the present invention are introduced in combination with specific examples:
[0031] like Figure 1 As shown, the magnetically controlled swinging indirect arc ultra-narrow gap welding device provided by the present invention comprises a wire feeding unit, a welding gun unit, a magnetic control unit and an insulating fixing plate 10. The insulating fixing plate 10 is clamped on the walking mechanism, and the wire feeding unit, the welding gun unit and the magnetic control unit are clamped on the insulating fixing plate 10 and are insulated from each other.
[0032] The welding gun part includes a welding gun 1, an electrode 3 and a ceramic nozzle 2. The electrode 3 is made of a high melting point material such as tungsten. To avoid burning and keep the arc stable, the electrode 3 is connected to the negative electrode of the welding power supply. The ceramic nozzle 2 with inert gas is extended into the groove to protect the electrode 3, the arc and the molten pool metal.
[0033] The wire feeding unit comprises a welding wire 4, a wire feeding tube 5, a ceramic nozzle 2, a conductive clamping block 6 and a conductive rod 7. The welding wire 4 is connected to the positive electrode of the welding power source.
[0034] Preferably, the indirect arc is generated between the electrode 3 and the end of the welding wire 4, heating the end of the welding wire 4 and the metal of the workpiece 17. The diameters of the electrode 3, the ceramic nozzle 2 and the wire feeding tube 5 are all smaller than the gap width of the groove 18 and can be extended into the groove 18 for welding and protection.
[0035] Preferably, the magnetron includes a coil frame 14, a coil 15 and a magnetic core 16. The coil frame 14 is made of an insulating material with good rigidity and can withstand high temperatures. The enameled copper wire is wound layer by layer on the outside of the coil frame 14, and the copper wires between the layers are separated by insulating paper or insulating paint to ensure mutual insulation, and the two ends of the copper wire are respectively connected to the two poles of the magnetron power supply. The diameter and number of turns of the copper wire are adjusted according to actual needs. Preferably, the magnetic core 16 is made of a material with high magnetic permeability such as silicon steel sheet or ferrite, and the shape and size of the end of the magnetic core 16 near the arc zone are designed according to actual needs. The magnetic core 16 passes through the inside of the coil frame 14 and is fixed to the coil frame 14. Preferably, the thickness of the end of the magnetic core 16 should be less than the gap width of the groove 18 to avoid contact with the side wall metal during welding. Preferably, the upper end of the magnetic core 16 is fixed to the insulating fixing plate 10 by a clamp 13, and the distance between the lower end and the electrode 3 is adjusted according to needs to increase the magnetic induction intensity of the arc zone as much as possible while ensuring that the magnetic core 16 is not damaged.
[0036] Preferably, the waveform, peak value and alternating frequency of the excitation current passed into the coil 15 are adjusted by the magnetron power supply according to requirements.
[0037] like Figure 2 As shown, the indirect arc 2 swings back and forth periodically toward both sides of the groove 4 under the drive of the external alternating magnetic field, promoting the melting of the metal on the side wall of the groove 4. The figure shows schematic diagrams of the indirect arc 2 in the middle of the groove 4 and swinging to the left and right sides of the groove 4.
[0038] like Figure 1 As shown, taking thick plate welding as an example, the method for using the magnetically controlled swing indirect arc ultra-narrow gap welding device provided by the present invention is as follows:
[0039] Step 1: Grind the metal surface of the groove and surrounding area of the thick plate to be welded clean, and wipe the surface clean with volatile organic solvents such as acetone or ethanol. Preset the anti-deformation of the thick plates to be welded at a certain angle, spot weld them together, and fix them on the welding platform with a clamp;
[0040] Step 2: Adjust the end of the magnetic core, the end of the electrode and the end of the welding wire to the appropriate position according to actual needs and fix them, check and ensure that the electrode and the welding wire are in good electrical conduction with the negative and positive poles of the welding power source respectively, ensure that there is no conduction between the electrode and the welding wire, and check the shape of the electrode and the smoothness of wire feeding;
[0041] Step 3: Turn on the travel mechanism, welding power supply, magnetron power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, excitation current waveform, excitation current peak value, excitation current alternating frequency and gas flow rate of each ceramic nozzle;
[0042] Step 4: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, and start the arc after the shielding gas is introduced for a period of time in advance. After the arc is generated between the electrode and the welding wire, turn on the external magnetic field, and the walking mechanism drives the welding gun to move to the arc-extinguishing end. The indirect arc swings back and forth periodically on both sides of the groove during the welding process. When the end of the indirect arc swings to the side wall of the groove, the arc directly heats the metal on the side wall of the groove, and the molten droplets formed by the melting of the welding wire end can also directly transition to both sides of the groove. After the end of the welding wire reaches the arc-extinguishing end, the arc is extinguished, the external magnetic field is turned off, and the gas valve is closed after the gas is delayed for a period of time, and the welding gun is moved to other designated positions. Repeat the above welding process continuously, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height.
[0043] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A magnetically controlled swinging indirect arc ultra-narrow gap welding device and method, characterized in that: The method applies an alternating transverse magnetic field to make the indirect arc swing back and forth periodically toward both sides of the groove, thereby suppressing the side wall non-fusion defect that is easily generated during the indirect arc ultra-narrow gap welding process.
2. A magnetically controlled swing indirect arc ultra-narrow gap welding device, characterized in that: The invention comprises a wire feeding part, a welding gun part, a magneto-control part and an insulating fixing plate. The insulating fixing plate is clamped on the walking mechanism, and the wire feeding part, the welding gun part and the magneto-control part are fixed on the insulating fixing plate through a clamping block and are insulated from each other.
3. The magnetically controlled swing indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The wire feeding part comprises welding wire, wire feeding tube, ceramic nozzle, conductive clamp block and conductive rod, which is clamped on the insulating fixed plate through the clamp block, and the welding wire is connected with the positive electrode of the welding power supply.
4. The magnetically controlled swing indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The welding gun part includes a welding gun, an electrode and a ceramic nozzle. The electrode is connected to the negative electrode of the welding power supply, and an indirect arc is generated between the end of the electrode and the end of the welding wire to heat the end of the welding wire and the substrate.
5. The magnetically controlled swing indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The magnetron includes a coil frame, a coil and a magnetic core. The enameled copper wire is wound layer by layer on the insulated coil frame, and insulating paint or insulating paper is used between the layers to ensure mutual insulation between the copper wires. The two ends of the copper wire are respectively connected to the two poles of the external magnetron power supply. The number of turns and diameter of the coil are adjusted according to actual needs.
6. The magnetically controlled swing indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The magnetic core passes through the inside of the coil frame and is fixed to the coil frame. The magnetic core is made of high magnetic permeability materials such as silicon steel sheets or ferrites. The size and shape of the end of the magnetic core near the arc zone are designed according to requirements. The thickness of the magnetic core is smaller than the width of the groove gap to avoid contact with the metal of the groove side wall.
7. The magnetically controlled swing indirect arc ultra-narrow gap welding device according to claim 2, characterized in that: The magnetron is clamped on the insulating fixing plate through a magnetic core clamp, and the distance between the end of the magnetic core and the electrode is adjusted according to actual needs to avoid burning or demagnetization of the magnetic core.
8. A method for welding using the magnetically controlled swing indirect arc ultra-narrow gap welding device according to any one of claims 2 to 7, characterized in that: The steps include: Step 1: Clamp the thick plate with processed grooves and cleaned surface on the welding platform, and adjust the end of the magnetic core, the end of the electrode and the end of the welding wire to the appropriate position according to actual needs and fix them; Step 2: Turn on the travel mechanism, welding power supply, magnetron power supply and cooling pump, and adjust and set the welding current, wire feeding speed, welding speed, excitation current waveform, excitation current peak value, excitation current alternating frequency and gas flow rate of each ceramic nozzle; Step 3: Move the end of the welding wire to the appropriate position above the arc-starting end at the bottom of the groove through the walking mechanism, introduce the shielding gas in advance to cover the electrode and the welding area, start the arc, and after the arc is generated, turn on the external magnetic field. The walking mechanism drives the welding gun to move to the arc-extinguishing end. The indirect arc swings back and forth periodically on both sides of the groove during the welding process. The arc is extinguished after the end of the welding wire reaches the arc-extinguishing end. At the same time, the external magnetic field is turned off, and the gas valve is closed after a period of delayed gas supply, and the welding gun is moved to other designated positions. Repeat the above welding process, fill the groove layer by layer, and complete the welding process after the transition metal fills the groove and forms a certain excess height.
Citation Information
Cited By
Magnetic control narrow-gap horizontal position welding process based on welding wire and electric arc synchronous swing and control method
CN122007551A
Magnetic control narrow gap horizontal welding process based on synchronous swing of welding wire arc and control method
CN122007551B
Electric arc and wire feeding cooperative control method and system for variable-gap groove TIG welding
CN122606097A