Well wall stability test damage monitoring method in low-temperature environment

By simulating the low-temperature environment in the pit and using hydraulic cylinder and refrigeration tube technology to conduct well wall stability tests, the stability monitoring problem of deep well wall in low-temperature environment is solved, and detailed deformation and damage data are provided, which is a well wall. The design provides important experimental conditions.

CN118937101APending Publication Date: 2024-11-12BEIJING CHINA COAL MINE ENG CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411182220.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In low temperature environments, stability monitoring of deep shaft walls is difficult, especially when formation pressures are directed and uneven, it is difficult for the prior art to effectively simulate and detect deformation and damage of the well walls.

Method used

By installing the support inner ring and hydraulic cylinder in the pit and laying a chiller tube on its outer layer to connect to the freezing station, it simulates the low temperature environment, produces a wellbore steel mold and concrete model, installs embedded detection sensors and acoustic emission monitoring probes, and applies hydraulic pressure The force is until the model is damaged, and the deformation and damage process are recorded.

Benefits of technology

It realizes detailed deformation and damage monitoring of the well wall structure under low temperature environment, provides important test conditions, provides practical test data for the design of the well wall concrete in deep formations, and meets different stress directions and temperatures. test requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118937101A_ABST
    Figure CN118937101A_ABST
Patent Text Reader

Abstract

The invention discloses a borehole wall stability test damage monitoring method in a low-temperature environment, which comprises the following steps of: pre-cooling a test environment, putting a wellbore steel mold into the low-temperature environment, pouring concrete, curing, dismantling the wellbore steel mold after curing to obtain a borehole wall model, applying uniform or non-uniform pressure to the borehole wall model by using a hydraulic cylinder, and monitoring the borehole wall stability test damage in the low-temperature environment. And the deformation data of the well wall model are monitored in real time. The freezing pipe is arranged to be matched with the hydraulic cylinders in all directions, so that tests at different low temperatures and in different stress directions can be carried out, stress, deformation and damage monitoring tests of the well wall under different conditions are met, research on analysis of well wall structure damage and failure mechanisms in a non-normal temperature environment at present is met, and the test efficiency is improved. Important test conditions are provided for the design of deep stratum well wall concrete under the environment, the temperature gradients of different actual stratum depths can be better simulated by arranging the spiral coil pipe, and the device better fits the actual environment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of shaft wall stability monitoring in vertical shaft engineering, and more specifically to a shaft wall stability test damage monitoring method in a low temperature environment. Background Art

[0002] The lowest temperature in winter in the western coal mining area can reach -30°, and the low temperature environment can last up to 5 months. The shaft wall at depth not only has to withstand higher formation pressure, but the ground pressure also has obvious directionality and unevenness. The deformation characteristics of the shaft wall under this special stress and low environment are more complex than those at the shallow end. Relevant studies have shown that the physical and mechanical properties of concrete will be greatly reduced at low temperatures, and the long-term stability of the deep shaft wall structure in this environment will inevitably be affected. Therefore, the long-term stability of the deep shaft wall requires more detailed research. Summary of the invention

[0003] Therefore, the technical problem to be solved by the present invention is to provide a method for monitoring damage of a wellbore stability test in a low temperature environment for conducting a wellbore test in a simulated environment.

[0004] In order to solve the above technical problems, the present invention provides the following technical solutions: a method for monitoring damage of a wellbore stability test under a low temperature environment, comprising the following steps:

[0005] Step A: Install the support inner ring in the pit, and install the hydraulic cylinder on the inner wall of the support inner ring;

[0006] Step B: Arrange a freezing pipe on the outer layer of the supporting inner ring, and connect the freezing pipe to the freezing station;

[0007] Step C: The heat preservation cover is installed on the pit by means of a crane, and the freezing station is started for pre-cooling. The freezing station inputs low-temperature brine into the freezing pipe, and the freezing medium is circulated in the freezing pipe to absorb the heat in the pit, so that the temperature in the pit drops to the design temperature;

[0008] Step D: Make the shaft steel mold according to the design size, open the insulation cover, hoist the shaft steel mold into the inner ring of the support through the crane, and fix the shaft steel mold;

[0009] Step E: Put a steel mesh in the shaft steel mold, mix the concrete configured according to the design evenly, pour it into the shaft steel mold, and vibrate and compact it; at the same time, arrange the embedded detection sensor in the concrete;

[0010] Step F: Close the insulation cover, cure the concrete for 7 days at the design temperature, then remove the shaft steel formwork to obtain a shaft wall model that is the same as the actual environment;

[0011] Step G: starting the hydraulic cylinder, which extends to exert force on the well wall model, and detecting deformation data of the well wall model through the pre-buried detection sensor until the well wall model is destroyed;

[0012] Step H: Close the hydraulic cylinder and perform imaging scanning and recording on the destroyed well wall model.

[0013] In the above-mentioned method for monitoring damage of a well wall stability test under a low-temperature environment, a reserved circular hole is opened on the inner side of the wellbore steel mold, and the lead wire of the embedded detection sensor passes through the reserved circular hole.

[0014] In the above-mentioned damage monitoring method for a wellbore stability test under a low temperature environment, in step G, an acoustic emission monitoring probe is installed on the inner wall surface of the wellbore model.

[0015] In the above-mentioned method for monitoring damage of a well wall stability test under a low-temperature environment, in step A, the pit is opened on the ground, the support inner ring is made of cast concrete, an installation groove is opened on the inner wall surface of the support inner ring, the hydraulic cylinder is installed in the installation groove, and the piston rod end of the hydraulic cylinder is arranged toward the center of the support inner ring.

[0016] In the above-mentioned damage monitoring method for a well wall stability test under a low temperature environment, in step B, the freezing pipe is a spiral coil, the spiral coil is wrapped around the periphery of the supporting inner ring, and an insulation layer is arranged on the periphery of the freezing pipe.

[0017] In the above-mentioned damage monitoring method for well wall stability test under low temperature environment, the low-temperature brine in the freezing pipe circulates downward from a position close to the top of the support inner ring; the first circle of the freezing pipe is located above the support inner ring outside the pit.

[0018] In the above-mentioned damage monitoring method for a wellbore stability test under a low-temperature environment, the wellbore steel mold includes an outer mold and an inner mold, the outer mold is coaxially arranged in the inner mold, and the steel mesh and concrete are located in the space between the outer mold and the inner mold.

[0019] The above-mentioned method for monitoring damage in a wellbore stability test under a low-temperature environment, the outer mold includes a lower fixed ring, a fixed plate, an upper fixed ring and a movable plate, the lower fixed ring is fixedly connected with two or more fixed plates at equal intervals along its circumference, the bottom of the upper fixed ring is fixedly connected with two or more movable plates at equal intervals along its circumference, the fixed plate and the movable plate are both arranged along the axial direction of the lower fixed ring, the spacing between two adjacent fixed plates is equal to the width of the movable plate, the movable plate is inserted between two adjacent fixed plates to form a cylinder, and the side wall of the movable plate is tightly fitted with the side wall of the fixed plate.

[0020] In the above-mentioned damage monitoring method for well wall stability test under low temperature environment, the width of the fixed plate gradually narrows from the direction close to the lower fixed ring to the direction away from the lower fixed ring; the width of the movable plate gradually narrows from one end close to the upper fixed ring to the end away from the upper fixed ring.

[0021] In the above-mentioned method for monitoring damage of a wellbore stability test under a low-temperature environment, an open groove is provided on the fixed plate, an arc-shaped pad is installed in the open groove, and the outer wall of the arc-shaped pad is arranged corresponding to the hydraulic cylinder; in step F, when removing the wellbore steel mold, the inner mold is first removed, and then the upper fixed ring and the movable plate connected to the upper fixed ring are removed; when the hydraulic cylinder is extended, the piston rod of the hydraulic cylinder is pressed tightly against the arc-shaped pad, and the hydraulic cylinder applies a force to the wellbore model through the arc-shaped pad.

[0022] The technical solution of the present invention achieves the following beneficial technical effects:

[0023] By setting up freezing pipes in conjunction with hydraulic cylinders in various positions, tests at different low temperatures and in different force directions can be carried out to meet the stress, deformation and damage monitoring tests of the well wall under different conditions. This meets the current research on the damage and destruction mechanism of the well wall structure under very low temperature environments, and provides important test conditions for the design of well wall concrete in deep formations under such environments. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A schematic cross-sectional view of the present invention;

[0025] Figure 2 A schematic diagram of the top view of the shaft steel mold of the present invention;

[0026] Figure 3 A schematic diagram of the top view of the well wall model of the present invention;

[0027] Figure 4 A schematic diagram of the movable plate of the present invention being installed on the upper fixing ring;

[0028] Figure 5 A schematic diagram of the fixing plate of the present invention being installed on the lower fixing ring;

[0029] Figure 6 Schematic diagram of the contact between the hydraulic cylinder and the arc-shaped pad of the present invention.

[0030] The reference numerals in the figure are as follows: 1-insulation layer; 2-freezing pipe; 3-support inner ring; 4-insulation cover; 5-installation groove; 6-hydraulic cylinder; 7-wellbore steel mold; 71-outer mold; 72-inner mold; 73-upper fixed ring; 74-movable plate; 75-lower fixed ring; 76-fixed plate; 77-arc pad; 8-well wall model; 9-embedded detection sensor; 10-acoustic emission monitoring probe; 11-pit; 12-crane. DETAILED DESCRIPTION

[0031] The damage monitoring method for wellbore stability test under low temperature environment in this embodiment includes the following steps:

[0032] Step A: Install the support inner ring 3 in the pit 11, and install the hydraulic cylinder 6 on the inner wall surface of the support inner ring 3. The pit 11 is opened on the ground. The support inner ring 3 is made of concrete. The inner wall surface of the support inner ring 3 is provided with a mounting groove 5. The hydraulic cylinder 6 is installed in the mounting groove 5, and the piston rod end of the hydraulic cylinder 6 is arranged toward the center of the support inner ring 3.

[0033] Step B: Arrange the freezing pipe 2 on the outer layer of the supporting inner ring 3, and connect the freezing pipe 2 to the freezing station;

[0034] Step C: The heat preservation cover 4 is hoisted on the pit 11 by the overhead crane 12, and the freezing station is started for precooling. The freezing station inputs low-temperature brine into the freezing pipe 2, and absorbs the heat in the pit 11 by circulating the freezing medium in the freezing pipe 2, so that the temperature in the pit 11 drops to the design temperature; the freezing station includes a brine pump, a brine tank and an air refrigerator, and the air refrigerator cools the brine and then inputs it into the brine tank. Under the action of the brine pump, the low-temperature brine is input into the freezing pipe 2 and circulated;

[0035] Step D: Make the shaft steel mold 7 according to the design size, open the heat preservation cover 4, hoist the shaft steel mold 7 into the support inner ring 3 through the crane 12, and fix the shaft steel mold 7;

[0036] Step E: Put a steel mesh into the shaft steel mold 7, mix the concrete configured according to the design evenly, pour it into the shaft steel mold 7, and vibrate and compact it; at the same time, arrange the embedded detection sensor 9 in the concrete, and a reserved circular hole is opened on the inner side of the shaft steel mold 7, and the lead wire of the embedded detection sensor 9 passes through the reserved circular hole;

[0037] Step F: close the heat preservation cover 4, cure the concrete for 7 days at the design temperature, then remove the shaft steel formwork 7 to obtain a shaft wall model 8 that is the same as the actual environment;

[0038] Step G: Start the hydraulic cylinder 6, which extends to apply force to the well wall model 8, and detect the deformation data of the well wall model 8 through the pre-buried detection sensor 9. An acoustic emission monitoring probe 10 is installed on the inner wall surface of the well wall model 8 to synchronously detect the deformation data until the well wall model 8 is destroyed;

[0039] Step H: closing the hydraulic cylinder 6 and performing imaging scanning and recording on the destroyed well wall model 8.

[0040] In step B, the freezing pipe 2 is a spiral coil, which is wrapped around the outer periphery of the supporting inner ring 3. An insulation layer 1 is arranged on the outer periphery of the freezing pipe 2. The low-temperature brine in the freezing pipe 2 circulates downward from a position close to the top of the supporting inner ring 3. By arranging the spiral coil, the temperature gradient of different actual stratum depths can be better simulated, which is more in line with the actual environment. The first circle of the freezing pipe 2 is located above the supporting inner ring 3 outside the pit 11. By arranging a circle of freezing pipes 2 located outside, the air in the environment can be cooled, which is more in line with the actual severe cold climate in the west.

[0041] The shaft steel formwork 7 comprises an outer formwork 71 and an inner formwork 72, wherein the outer formwork 71 is coaxially arranged in the inner formwork 72, and the steel mesh and concrete are located in the space between the outer formwork 71 and the inner formwork 72. The outer formwork 71 comprises a lower fixed ring 75, a fixed plate 76, an upper fixed ring 73 and a movable plate 74. More than two fixed plates 76 are fixedly connected to the lower fixed ring 75 at equal intervals along its circumference, and more than two movable plates 74 are fixedly connected to the bottom of the upper fixed ring 73 at equal intervals along its circumference. Both the fixed plates 76 and the movable plates 74 are arranged along the axial direction of the lower fixed ring 75, and the spacing between two adjacent fixed plates 76 is equal to the width of the movable plate 74. The movable plate 74 is inserted between two adjacent fixed plates 76 to form a cylinder, and the side wall of the movable plate 74 is tightly fitted with the side wall of the fixed plate 76. The width of the fixed plate 76 is from near the lower fixed ring to near the bottom. The outer wall of the arc pad 77 is arranged corresponding to the hydraulic cylinder 6, and an outer mold 71 composed of two parts is arranged. In actual use, when the mold is removed, the outer mold 71 only needs to remove the upper fixing ring 73 and the movable plate 74, and the fixed plate 76 does not need to be removed, which is convenient for mold removal. In addition, the mold designed in this way is conducive to direct contact between the mold and the supporting inner ring 3, and is conducive to direct contact between the well wall model 8 and the surrounding environment for heat exchange. In subsequent tests, the experiment can be carried out directly after the movable plate 74 is removed, and pressure is applied by connecting the hydraulic cylinder 6 with the arc pad 77, without repeated disassembly and assembly operations.

[0042] In step F, when removing the wellbore steel mold 7, first remove the inner mold 72, then remove the upper fixing ring 73 and the movable plate 74 connected to the upper fixing ring 73; when the hydraulic cylinder 6 is extended, the piston rod of the hydraulic cylinder 6 is pressed tightly against the arc pad 77, and the hydraulic cylinder 6 applies a force to the well wall model 8 through the arc pad 77.

[0043] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the claims of this patent application.

Claims

1. A damage monitoring method for wellbore stability test in a low temperature environment, characterized in that: The following steps are involved: Step A: installing the support inner ring (3) in the pit (11), and installing the hydraulic cylinder (6) on the inner wall surface of the support inner ring (3); Step B: arranging a freezing pipe (2) on the outer layer of the supporting inner ring (3), and connecting the freezing pipe (2) to a freezing station; Step C: The heat preservation cover (4) is hoisted on the pit (11) by the overhead crane (12), and the freezing station is started for precooling. The freezing station inputs low-temperature brine into the freezing pipe (2), and the freezing medium is circulated in the freezing pipe (2) to absorb the heat in the pit (11), so that the temperature in the pit (11) drops to the design temperature; Step D: making a shaft steel mold (7) according to the design dimensions, opening the heat preservation cover (4), hoisting the shaft steel mold (7) into the support inner ring (3) through the overhead crane (12), and fixing the shaft steel mold (7); Step E: a steel mesh is placed in the shaft steel mold (7), concrete configured according to the design is stirred evenly, poured into the shaft steel mold (7), and vibrated and compacted; at the same time, a pre-buried detection sensor (9) is arranged in the concrete; Step F: closing the heat preservation cover (4), curing the concrete for 7 days at the design temperature, and then removing the shaft steel formwork (7) to obtain a shaft wall model (8) identical to the actual environment; Step G: starting the hydraulic cylinder (6), the hydraulic cylinder (6) extends to exert a force on the well wall model (8), and detecting deformation data of the well wall model (8) through the pre-buried detection sensor (9) until the well wall model (8) is destroyed; Step H: closing the hydraulic cylinder (6) and performing imaging scanning and recording on the destroyed well wall model (8).

2. The damage monitoring method for wellbore stability test in low temperature environment according to claim 1 is characterized in that: A reserved circular hole is provided on the inner side of the shaft steel mold (7), and the lead wire of the embedded detection sensor (9) passes through the reserved circular hole.

3. The damage monitoring method for wellbore stability test in low temperature environment according to claim 1 is characterized in that: In step G, an acoustic emission monitoring probe (10) is installed on the inner wall surface of the well wall model (8).

4. The damage monitoring method for wellbore stability test in low temperature environment according to claim 1 is characterized in that: In step A, the pit (11) is opened on the ground, the support inner ring (3) is made of cast concrete, a mounting groove (5) is opened on the inner wall surface of the support inner ring (3), the hydraulic cylinder (6) is installed in the mounting groove (5), and the piston rod end of the hydraulic cylinder (6) is arranged toward the center of the support inner ring (3).

5. The damage monitoring method for wellbore stability test in low temperature environment according to claim 1 is characterized in that: In step B, the freezing pipe (2) is a spiral coil, which is wrapped around the periphery of the supporting inner ring (3), and a heat-insulating layer (1) is provided on the periphery of the freezing pipe (2).

6. The damage monitoring method for wellbore stability test in low temperature environment according to claim 5 is characterized in that: The low-temperature brine in the freezing pipe (2) circulates downward from a position close to the upper part of the supporting inner ring (3); the first circle of the freezing pipe (2) is located above the supporting inner ring (3) outside the pit (11).

7. The damage monitoring method for wellbore stability test in low temperature environment according to claim 1 is characterized in that: The shaft steel mold (7) comprises an outer mold (71) and an inner mold (72), wherein the outer mold (71) is coaxially arranged in the inner mold (72), and the steel mesh and concrete are located in the space between the outer mold (71) and the inner mold (72).

8. The damage monitoring method for wellbore stability test in low temperature environment according to claim 7 is characterized in that: The outer mold (71) comprises a lower fixed ring (75), a fixed plate (76), an upper fixed ring (73) and a movable plate (74); the lower fixed ring (75) is fixedly connected with two or more fixed plates (76) at equal intervals along its circumference; the bottom of the upper fixed ring (73) is fixedly connected with two or more movable plates (74) at equal intervals along its circumference; the fixed plates (76) and the movable plates (74) are both arranged along the axial direction of the lower fixed ring (75); the spacing between two adjacent fixed plates (76) is equal to the width of the movable plate (74); the movable plate (74) is inserted between two adjacent fixed plates (76) to form a cylinder; the side wall of the movable plate (74) is tightly fitted with the side wall of the fixed plate (76).

9. The damage monitoring method for wellbore stability test in low temperature environment according to claim 8, characterized in that: The width of the fixed plate (76) gradually narrows from a direction close to the lower fixed ring (75) to a direction away from the lower fixed ring (75); the width of the movable plate (74) gradually narrows from an end close to the upper fixed ring (73) to an end away from the upper fixed ring (73).

10. The damage monitoring method for wellbore stability test in low temperature environment according to claim 9, characterized in that: The fixed plate (76) is provided with an open groove, in which an arc-shaped pad (77) is installed, and the outer wall surface of the arc-shaped pad (77) is arranged corresponding to the hydraulic cylinder (6); in step F, when removing the wellbore steel mold (7), the inner mold (72) is first removed, and then the upper fixed ring (73) and the movable plate (74) connected to the upper fixed ring (73) are removed; when the hydraulic cylinder (6) is extended, the piston rod of the hydraulic cylinder (6) is pressed against the arc-shaped pad (77), and the hydraulic cylinder (6) applies a force to the wellbore model (8) through the arc-shaped pad (77).