High-failure-possibility pipe section identification method

By establishing a three-dimensional multiphase flow simulation model and a multi-factor synergistic corrosion prediction model for pipelines, the corrosion rate was calculated and the corrosion level was determined, solving the problem of identifying multi-factor synergistic corrosion in natural gas gathering and transmission pipelines and improving pipeline safety and protection effectiveness.

CN118940487AActive Publication Date: 2024-11-12SOUTHWEST PETROLEUM UNIV

Patent Information

Application Number
CN202410969807.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-12
Estimated Expiration
2044-07-19

AI Technical Summary

Technical Problem

Existing technologies are insufficient to effectively identify and quantify the potential for multi-factor synergistic corrosion in natural gas gathering and transmission pipelines, making it difficult to control the risk of corrosion failure. In particular, corrosion prediction models have limitations under the influence of complex terrain and multiphase flow.

Method used

By establishing a three-dimensional multiphase flow simulation model for pipelines and combining it with a multi-factor synergistic corrosion prediction model, the corrosion rate along the pipeline is calculated, and a local corrosion failure criterion is established to identify pipeline sections with a high probability of corrosion failure.

Benefits of technology

It enables accurate identification of the likelihood level of corrosion failure in natural gas gathering and transmission pipelines, reduces perforation accidents caused by internal corrosion, and improves pipeline safety and protection accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118940487A_ABST
    Figure CN118940487A_ABST
Patent Text Reader

Abstract

The method comprises the following steps: performing three-dimensional multiphase flow simulation calculation on a natural gas gathering and transportation pipeline to obtain flow parameters along the pipeline, performing data acquisition, combining multiphase flow simulation parameters and data, determining an internal corrosion mechanism of the pipeline, identifying internal corrosion influence factors, and combining a multi-factor collaborative corrosion prediction model to identify a high-failure-possibility pipeline section. And finally, establishing a local corrosion failure criterion CRT (Cathode Ray Tube), and determining an internal corrosion failure possibility grade which can be used for identifying a high-corrosion failure possibility pipe section of the natural gas gathering and transportation pipeline.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of natural gas pipeline safety risk assessment, and specifically relates to a method for identifying pipe sections with high failure probability, which is mainly used for identifying pipe sections with high corrosion failure probability in natural gas gathering and transportation pipelines. Background Art

[0002] The medium transported by my country's natural gas gathering and transmission pipelines is complex, and internal corrosion and perforation accidents are prone to occur due to the synergy of multiple factors.

[0003] Internal inspection is the most accurate method to understand the internal corrosion of pipelines, but its application cost is high. Therefore, the National Association of Corrosion Engineers (NACE) proposed a direct assessment method for internal corrosion in 2002, including direct assessment method for internal corrosion of dry gas pipelines (DG-ICDA), direct assessment method for internal corrosion of crude oil pipelines (LP-ICDA), direct assessment method for internal corrosion of wet gas pipelines (WG-ICDA) and direct assessment method for internal corrosion of multiphase mixed pipelines (MP-ICDA).

[0004] Direct assessment of internal corrosion is mainly divided into pre-assessment, indirect detection, direct detection and post-assessment. Pre-assessment determines the feasibility of direct assessment of internal corrosion of pipelines through data collection, and further determines the area to be evaluated. Then, combined with the multiphase flow calculation results, corrosion rate prediction is performed, which is called indirect evaluation. Therefore, for indirect evaluation, the corrosion rate prediction result is a key parameter to improve the direct assessment of internal corrosion. In order to improve the accuracy of protection against internal corrosion of pipelines and reduce the risk of pipeline corrosion failure, the prediction of internal corrosion has become an important step. The corrosion model has also gradually developed from empirical models, semi-mechanism-semi-empirical models to mechanism models.

[0005] Due to the common multi-factor synergistic corrosion environment in industrial environments, it is difficult to construct a mechanism model. In addition, some empirical models are highly dependent on original corrosion data, have a limited scope of application, and have limitations in predicting flow corrosion in gathering and transportation pipelines.

[0006] At present, the difficulties in studying the multi-factor coordinated corrosion phenomenon in natural gas gathering and transportation pipelines are as follows: the transportation medium of the gathering and transportation pipelines is different at each stage, and it is necessary to trace the medium and change range that affect pipeline corrosion; the gathering and transportation pipelines are located in mountainous areas with large undulations and are affected by special gas-liquid two-phase flow, and the impact of flow on corrosion needs to be further clarified; the complex corrosion mechanism of factors such as CO2, SRB, and O2 is not yet clear, and the multi-factor coordinated corrosion mechanism needs to be studied in depth, and a corrosion prediction model needs to be established; the possibility of corrosion failure in the pipeline has not been quantified, which has become a bottleneck problem for graded corrosion control.

[0007] The present invention calculates the corrosion rate along the pipeline by performing three-dimensional multiphase flow simulation calculation on the pipeline and combining a multi-factor collaborative corrosion prediction model. The possibility of pipeline corrosion failure is determined by identifying the influencing factors of internal corrosion and calculating the internal corrosion rate. The local corrosion failure criterion CRT is established to determine the possibility level of internal corrosion failure. Summary of the invention

[0008] The present invention provides a method for identifying a pipe section with high failure probability in order to identify the high corrosion failure probability of a natural gas gathering and transportation pipeline and reduce pipeline perforation accidents caused by internal corrosion.

[0009] In order to achieve the above object, the present invention adopts the following technical solutions:

[0010] S1: Establish a three-dimensional pipeline model, perform multiphase flow simulation, calculate flow parameters along the pipeline, and collect data;

[0011] S2: Combine multiphase flow simulation parameters and data to clarify the corrosion mechanism in the pipeline;

[0012] S3: Identify the factors affecting internal corrosion by studying the internal corrosion mechanism;

[0013] S4: Combine the multi-factor synergistic corrosion prediction model to predict the internal corrosion rate;

[0014] S5: Calculate the corrosion rate along the pipeline;

[0015] S6: Establish local corrosion failure criterion CRT and determine the possibility level of internal corrosion failure.

[0016] 101: Calculating Local Corrosion Rates

[0017] 102: In the formula: CR l ——local corrosion rate, mm / a; h——pitting depth; t——time, h.

[0018] 103: Calculation of local corrosion failure criteria

[0019] 104: Where: CRT - the useful life of the pipeline under local corrosion, a (year); δ - the wall thickness of the pipeline project, mm; CR l ——Local corrosion rate, mm / a.

[0020] Based on the ratio of pipeline design wall thickness to corrosion rate, the possibility of local corrosion failure is divided into five levels, among which level 1 is "very low" failure possibility, level 2 is "low" failure possibility, level 3 is "medium" failure possibility, level 4 is "medium-high" failure possibility and level 5 is "high" corrosion failure possibility.

[0021] The method for identifying the possibility of local corrosion failure is calculated according to the following steps:

[0022] 201: When CRT ≥ 20a, the failure probability level is judged to be 1;

[0023] 202: When 20a<CRT≤10a, the failure possibility level is judged to be 2;

[0024] 203: When 10a<CRT≤5a, the failure possibility level is judged to be 3;

[0025] 204: When 5a<CRT≤3a, the failure probability level is judged to be 4;

[0026] 205: When CRT < 1a, the failure possibility level is judged to be 5. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 Flow chart for determining the possibility of internal corrosion failure of the present invention

[0028] Figure 2 This is the probability level diagram of corrosion failure in the pipeline of the present invention DETAILED DESCRIPTION

[0029] In order to better explain the present invention and facilitate understanding, the present invention is described in detail below through specific implementation modes in conjunction with the accompanying drawings.

[0030] The first step is to simulate the three-dimensional multiphase flow in the pipeline. The simulation parameters are shown in Table 1: Table 1 Pipeline simulation parameters

[0031] Calculate the corrosion rate along the pipeline:

[0032] Local corrosion rate

[0033] Where: CR l ——local corrosion rate, mm / a; h——pitting depth; t——time, h;

[0034] The corrosion rate along the line is calculated.

[0035] Calculation of localized corrosion failure criteria

[0036] Where: CRT - usable life of pipeline under local corrosion, a (year); δ - pipeline wall thickness, mm; CR l ——local corrosion rate, mm / a;

[0037] The useful life of the pipeline under local corrosion is calculated.

[0038] Based on the ratio of pipeline design wall thickness to corrosion rate, the possibility of local corrosion failure is divided into 5 levels:

[0039] Among them, level 1 is "very low" failure possibility, level 2 is "low" failure possibility, level 3 is "medium" failure possibility, level 4 is "medium-high" failure possibility and level 5 is "high" corrosion failure possibility.

[0040] When CRT ≥ 20a, the failure possibility level is judged to be 1;

[0041] When 20a<CRT≤10a, the failure possibility level is judged to be 2;

[0042] When 10a<CRT≤5a, the failure possibility level is judged to be 3;

[0043] When 5a<CRT≤3a, the failure possibility level is judged to be 4;

[0044] When CRT<1a, the failure possibility level is judged to be 5.

Claims

1. A method for identifying pipe sections with high failure probability, It is characterized in that The process includes the following (Figure 1): S1: Establish a three-dimensional pipeline model, perform multiphase flow simulation, calculate flow parameters along the pipeline, and collect data; S2: Combine multiphase flow simulation parameters and data to clarify the corrosion mechanism in the pipeline; S3: Identify the factors affecting internal corrosion by studying the internal corrosion mechanism; S4: Combine the multi-factor synergistic corrosion prediction model to predict the internal corrosion rate; S5: Calculate the corrosion rate along the pipeline; S6: Establish local corrosion failure criterion CRT and determine the possibility level of internal corrosion failure.

2. A method for identifying pipe sections with high failure probability according to claim 1, It is characterized in that The calculation of the local corrosion rate and failure criterion of the pipeline is calculated according to the following steps: 101: Calculating Local Corrosion Rates 102: In the formula: CR l ——local corrosion rate, mm / a; h——pitting depth; t——time, h; 103: Calculation of local corrosion failure criteria 104: Where: CRT - the useful life of the pipeline under local corrosion, a (year); δ - the wall thickness of the pipeline project, mm; CR l ——Local corrosion rate, mm / a.

3. A method for identifying pipe sections with high failure probability according to claim 1, It is characterized in that Based on the ratio of pipeline design wall thickness to corrosion rate, the local corrosion failure possibility is divided into five levels, where level 1 is "very low" failure possibility, level 2 is "low" failure possibility, level 3 is "medium" failure possibility, level 4 is "medium-high" failure possibility and level 5 is "high" corrosion failure possibility. The local corrosion failure possibility identification method is calculated according to the following steps (Figure 2): 201: When CRT ≥ 20a, the failure probability level is judged to be 1; 202: When 20a<CRT≤10a, the failure possibility level is judged to be 2; 203: When 10a<CRT≤5a, the failure possibility level is judged to be 3; 204: When 5a<CRT≤3a, the failure probability level is judged to be 4; 205: When CRT < 1a, the failure possibility level is judged to be 5.

Citation Information

Patent Citations

  • Natural gas long-distance pipeline internal corrosion simulation analysis method

    CN112069688A

  • Method for identifying corrosion high-risk section in wet natural gas pipeline

    CN112214940A

  • Localized Corrosion Monitoring Device for Limited Conductivity Fluids

    US20090184003A1

  • A system, method and article of manufacture for corrosion risk analysis and for identifying priorities for the testing and / or maintenance of corrosion susceptible structures

    WO2001080043A2

Cited By

  • Corrosion monitoring effectiveness prediction method for high-water-content crude oil gathering and transportation fluctuating pipe section

    CN121145728A

  • A method for predicting the effectiveness of corrosion monitoring of a high-water-content crude oil gathering undulating pipe section

    CN121145728B