Finite element simulation method for bubbling of polymer liner of composite hydrogen storage cylinder

By establishing a finite element model containing defect cracks, using elastic plasticity and linear elastic fracture mechanics theory to simulate the occurrence and evolution of bubbles in the hydrogen storage cylinder of composite materials, the problem of failure to effectively study bubble damage in the prior art is solved. Accurate simulation and safety improvement of the inner shell structure of composite gas cylinders is achieved.

CN118940609AActive Publication Date: 2024-11-12ZHEJIANG UNIV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410930702.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-11
Publication Date
2024-11-12
Estimated Expiration
2044-07-11

AI Technical Summary

Technical Problem

The existing technology has failed to effectively study and solve the problem of bubble damage in the inner liner of the hydrogen storage cylinder of composite materials, resulting in the mechanical performance of the cylinder and hydrogen leakage in a high-pressure hydrogen environment, affecting safety.

Method used

Using the finite element simulation method of polymer inner liner bubble of composite hydrogen storage cylinder, the occurrence and evolution of bubbles are simulated by establishing a finite element model containing defective cracks, and using elastic plastic fracture mechanics and linear elastic fracture mechanics theory, the occurrence and evolution of bubbles are simulated, and the Effects of hydrogen permeation and increase in defect volume on the pressure in the bubble.

Benefits of technology

Accurate simulation of the bubbles in the composite gas cylinder is achieved, the test costs in high-pressure hydrogen environment is reduced, important structural design and operating conditions are provided, and the safety and service life of the gas cylinder is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118940609A_ABST
    Figure CN118940609A_ABST
Patent Text Reader

Abstract

The invention relates to a finite element simulation technology, and aims to provide a finite element simulation method for bubbling of a polymer liner of a composite hydrogen storage cylinder. Comprising the following steps: testing performance parameters of an inner container and an outer-layer composite material of the hydrogen storage cylinder; establishing a local gas cylinder hydrogen permeation model, and obtaining a relation curve of hydrogen permeation pressure changing along with the thickness of the liner; establishing a finite element model of the composite material hydrogen storage cylinder with the polymer liner containing defect cracks, and introducing a depth defect below the surface of the liner; taking bubbling of the inner container as a boundary, solving a J integral value of a defect crack front edge area by applying an elastic-plastic fracture mechanics theory, and solving a stress intensity factor of a defect crack front edge by applying a linear elastic fracture mechanics theory; in the bubbling evolution process, the influence of outward permeation of hydrogen in the defect and increase of the defect volume on pressure reduction in the bubbling is considered, and the hydrogen pressure in the bubbling is updated in each crack propagation step. The method fits the actual bubbling generation physical process, and has high accuracy.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of finite element simulation, and in particular to a finite element simulation method for bubbling a polymer liner of a composite material hydrogen storage cylinder. Background Art

[0002] The development of the hydrogen energy industry has attracted attention from countries around the world. Hydrogen energy storage and transportation is a key link in the hydrogen energy industry that connects upstream hydrogen production and downstream hydrogen use. High-pressure gaseous hydrogen storage is a relatively mature hydrogen storage solution. Composite hydrogen storage cylinders with polymer liners are widely used in scenarios such as vehicle-mounted hydrogen storage due to their lighter weight and higher hydrogen storage density.

[0003] During the service of composite hydrogen storage cylinders, high-pressure hydrogen will dissolve and diffuse in the polymer liner, occupying defects such as tiny cracks in the liner. During the rapid decompression of the cylinder, the high-pressure hydrogen accumulated in the liner will not be released in time, causing the liner material to rupture and form bubbling damage. After the liner is damaged by bubbling, its mechanical properties and hydrogen barrier properties decrease, and hydrogen is more likely to diffuse in the liner, causing hydrogen leakage in the cylinder, posing a threat to the safety of the cylinder.

[0004] Establishing a finite element simulation method for the bubbling of the polymer liner of a composite hydrogen storage cylinder is helpful to study the bubbling of the liner structure of the composite hydrogen storage cylinder and the influencing factors of the liner bubbling, which has important engineering significance for the liner structure design and the determination of the cylinder use conditions. However, the current finite element simulation research on composite hydrogen storage cylinders mainly focuses on the defects of damage, aging, fracture, penetration, etc. under high-pressure hydrogen storage environments, and no research results on the liner bubbling damage have been seen.

[0005] Therefore, the present invention intends to propose a finite element simulation method for the bubbling of the inner tank of a hydrogen storage cylinder and the bubbling evolution taking into account the factor of the hydrogen pressure drop in the bubbling, so as to provide a reference basis for practical engineering applications. Summary of the invention

[0006] The technical problem to be solved by the present invention is to overcome the deficiencies in the prior art and provide a finite element simulation method for bubbling a polymer liner of a composite material hydrogen storage cylinder.

[0007] To solve the technical problem, the solution of the present invention is:

[0008] A finite element simulation method for bubbling a polymer liner of a composite hydrogen storage cylinder is provided, comprising the following steps:

[0009] (1) The hydrogen storage cylinder used as the research object of finite element simulation includes a polymer liner and a carbon fiber composite material winding layer wrapped around the outer side of the liner; samples are taken from the hydrogen storage cylinder, and tensile, fracture mechanics and hydrogen permeation tests are performed on the liner material, and tensile and hydrogen permeation tests are performed on the carbon fiber composite material to obtain the performance parameters of the liner material and the carbon fiber composite material;

[0010] (2) Using the performance parameters of the liner material and carbon fiber composite material, a local gas cylinder hydrogen permeation model was established to obtain the relationship curve between hydrogen permeation pressure and liner thickness;

[0011] (3) Establish a finite element model of a composite hydrogen storage cylinder with a polymer liner containing defective cracks; the model is assembled from a three-dimensional model of the liner with defective cracks, a three-dimensional model of the bottle valve seat, and an outer carbon fiber winding layer, and hard contact is added between the interaction surfaces of the three models;

[0012] In the three-dimensional model of defect crack inner liner, a deep defect below the inner liner surface is introduced, and the defect type is a pore-like cavity defect or a crack defect; for the pore-like cavity defect, an initial crack penetrating through the cavity wall is further introduced;

[0013] According to the relationship curve between hydrogen permeation pressure in the liner and liner thickness, hydrogen pressure load is applied to the defects of corresponding depth in the liner, and the liner bubbling process is regarded as quasi-static crack extension;

[0014] (4) Apply the elastic-plastic fracture mechanics theory to solve the J integral value of the defect crack front area. If the solution is greater than the critical value J cr , it is considered that bubbling occurs in the liner;

[0015] The linear elastic fracture mechanics theory is further applied to solve the stress intensity factor K at the defect crack front. I If the solution is greater than the fracture toughness K of the liner material IC , which is considered as the further evolution of the bubble;

[0016] (5) During the bubble evolution process, the effects of hydrogen permeation from the defect and the increase in defect volume on the pressure drop inside the bubble are considered, and the hydrogen pressure inside the bubble is updated in each crack propagation step.

[0017] As a preferred embodiment of the present invention, the performance parameters of the liner material and the carbon fiber composite material obtained in step (1) include at least: the true stress-strain curve of the liner, elastic modulus, yield strength, Poisson's ratio, fracture toughness K IC , JR curve, liner thickness, and hydrogen diffusion coefficient and solubility coefficient of the liner and composite winding layer; further, according to the JR curve, the J integral value corresponding to the appropriate crack size is selected as the critical value J of bubbling occurrence cr .

[0018] As a preferred embodiment of the present invention, in the step (2), when establishing the hydrogen permeation model of the local gas cylinder, the shape of the local gas cylinder is selected to be a disc.

[0019] As a preferred embodiment of the present invention, in the pore-like cavity defect or crack defect in step (3), the crack propagation direction is parallel to the axis of the gas cylinder, and the crack type is contour integral; the processing mode for the singularity of the crack tip is degenerate unit control, using collapsed unit edges and repeated nodes.

[0020] As a preferred embodiment of the present invention, in the step (3), the crack front integral volume grid is a wedge-shaped unit and is arranged in a ring around the crack tip, the unit type is C3D20R, and the grid is refined around the crack front tip to form a nested integral volume form surrounding the crack front tip; the model is verified for grid independence, and the size of the innermost integral volume is continuously reduced until the obtained J integral value tends to be stable and positive.

[0021] As a preferred embodiment of the present invention, in the step (3), when a load is applied to the hydrogen pressure of the deep defect in the liner, the hydrogen pressure in the gas cylinder is the final pressure after the gas cylinder is depressurized within a period of time.

[0022] As a preferred embodiment of the present invention, in step (5), during the bubbling evolution process, the hydrogen pressure drop in the bubbling is calculated according to the following method:

[0023] (5.1) The cavity defect is approximated as a radius of r void The concentration distribution curve c(r) of hydrogen diffusion from the cavity to the outside during the pressure release period is integrated to obtain the hydrogen content entering the inner tank;

[0024] (5.2) Considering the pressure drop in the bubble caused by the increase in defect volume, the high-pressure hydrogen in the cavity is used to calculate the compressibility factor Z of the real gas using the Abel-Nobel state equation;

[0025] D1: In each calculation step, the pressure p of the bubble in the current step is first used. i Calculate the compression factor Z i , and then calculate the stress intensity factor K I ; If the crack will further expand after the calculation results are compared, the crack extension length in the next expansion step is limited to be less than the set ratio value of the current crack size;

[0026] D2: Set the volume of the cavity defect to be approximately a tiny cuboid and calculate the volume V of the cavity defect formed by bubbling;

[0027] D3: Calculate the hydrogen pressure inside the bubbling defect in the i-th crack extension step of the bubbling process;

[0028] (5.3) Repeat the calculation process of steps D1-D3 until the stress intensity factor K during bubbling is I Less than the fracture toughness K of the material IC , at which point the bubbling process ends.

[0029] Compared with the prior art, the present invention has the following beneficial effects:

[0030] 1. The present invention introduces an initial defect crack into the liner, limits the crack morphology, definition, and calculation method, and uses fracture mechanics analysis to achieve simulation of bubbling in the polymer liner of a composite gas cylinder. First, the occurrence of bubbling is determined using the elastic-plastic fracture mechanics theory, and then the linear elastic fracture mechanics theory is used to simulate the influence of the pressure reduction inside the defect on the bubbling evolution process, which fits the actual physical process of bubbling and has high accuracy.

[0031] 2. The present invention can solve the problems of high cost and limited conditions for the bubbling test of the inner liner of a composite hydrogen storage cylinder under a high-pressure hydrogen environment, and is of great significance to the design of the inner liner structure and the determination of the operating parameters of the cylinder. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 This is a diagram of the formation and evolution process of the inner bladder bubble.

[0033] Figure 2 This is a simulation diagram of the hydrogen osmotic pressure distribution when the local gas cylinder is in osmotic equilibrium.

[0034] Figure 3 This is a diagram of the integral form of the defect crack front area.

[0035] Figure 4 This is a simulation diagram of high-pressure hydrogen gas permeating outward from a spherical cavity defect.

[0036] Figure 5 This is the flow chart of the bubbling simulation algorithm.

[0037] Figure 6 This is the bubbling simulation effect diagram. DETAILED DESCRIPTION

[0038] The bubble formation and evolution process of the polymer liner of the composite hydrogen storage cylinder Figure 1 As shown, when bubbling occurs in the inner liner, the material undergoes plastic deformation at a slower rate under the action of high-pressure hydrogen in the defect. When the plastic deformation exceeds a certain degree, bubbling occurs in the inner liner to form initial cracks, which then rapidly expand under the drive of the pressure in the defect.

[0039] Based on the above bubbling evolution process, the present invention proposes a finite element simulation method for bubbling of the polymer liner of a composite hydrogen storage cylinder. First, a finite element model of a composite hydrogen storage cylinder with an initial defect crack in the polymer liner is established. By successively applying the elastic-plastic fracture mechanics theory and the linear elastic fracture mechanics theory, the prediction of the bubbling of the liner and the simulation of the evolution process after the bubbling occurs are achieved; at the same time, the influence of the drop in hydrogen pressure in the defect on the bubbling evolution process is also considered, so as to provide a reference for actual engineering.

[0040] Part I Implementation of the Invention

[0041] The finite element simulation method for bubbling a polymer liner of a composite hydrogen storage cylinder shown in the present invention comprises the following steps:

[0042] 1. The hydrogen storage cylinder used as the research object of finite element simulation includes a polymer liner and a carbon fiber composite material winding layer wrapped around the outside of the liner. Samples are taken from the hydrogen storage cylinder, and the liner material is subjected to tensile, fracture mechanics and hydrogen permeation tests, and the carbon fiber composite material is subjected to tensile and hydrogen permeation tests to obtain the performance parameters of the liner material and the carbon fiber composite material. The obtained performance parameters include at least: the true stress-strain curve of the liner, elastic modulus, yield strength, Poisson's ratio, fracture toughness K IC , JR curve, liner thickness, and hydrogen diffusion coefficient and solubility coefficient of the liner and composite winding layer; further, according to the JR curve, the J integral value corresponding to the appropriate crack size is selected as the critical value J of bubbling occurrence cr .

[0043] 2. Use the performance parameters of the liner material and the carbon fiber composite material to establish a hydrogen permeation model for a local gas cylinder, and obtain a distribution curve of the hydrogen permeation pressure along the thickness of the liner; as an optional example, select the shape of the local gas cylinder as a disc.

[0044] 3. Establish a finite element model of a composite hydrogen storage cylinder with defective cracks in the polymer liner; the model is assembled from a three-dimensional model of the liner with defective cracks, a three-dimensional model of the bottle valve seat, and an outer carbon fiber winding layer, and hard contact is added between the interaction surfaces of the three models;

[0045] In the three-dimensional model of defect crack inner liner, a deep defect below the inner liner surface is introduced, and the defect type is a pore-like cavity defect or a crack defect; for the pore-like cavity defect, an initial crack penetrating through the cavity wall is further introduced;

[0046] In the pore-like cavity defect or crack defect, the crack propagation direction is parallel to the cylinder axis, and the crack type is the contour integral; the processing mode for the crack tip singularity is degenerate unit control, using collapsed unit edges and repeated nodes. The crack front integral volume mesh is a wedge-shaped unit and is arranged in a ring around the crack tip. The unit type is C3D20R. The mesh is refined around the crack front tip to form a nested integral volume surrounding the crack front tip; the model is verified for mesh independence, and the size of the innermost integral volume is continuously reduced until the J integral value is stable and positive.

[0047] According to the relationship curve between the hydrogen permeation pressure in the liner and the liner thickness, a hydrogen pressure load is applied to the defects of corresponding depth in the liner, and the liner bubbling process is regarded as quasi-static crack extension; the hydrogen pressure in the gas cylinder is the final pressure after the gas cylinder is depressurized within a period of time.

[0048] 4. Apply the elastic-plastic fracture mechanics theory to solve the J integral value of the defect crack front area. If the solution is greater than the critical value J cr , it is considered that bubbling occurs in the liner;

[0049] The linear elastic fracture mechanics theory is further applied to solve the stress intensity factor K at the defect crack front. I If the solution is greater than the fracture toughness K of the liner material IC , which is considered as the further evolution of the bubble;

[0050] 5. During the bubble evolution process, the influence of hydrogen permeation from the defect and the increase in defect volume on the pressure drop inside the bubble is considered, and the hydrogen pressure inside the bubble is updated in each crack propagation step.

[0051] During the bubbling evolution process, the hydrogen pressure drop in the bubble is calculated as follows:

[0052] (5.1) The cavity defect is approximated as a radius of r void The concentration distribution curve c(r) of hydrogen diffusion from the cavity to the outside during the pressure release period is integrated by formula (1) to obtain the hydrogen content entering the inner tank;

[0053]

[0054] Where: Q is the hydrogen content that penetrates into the inner liner, c(r) is the concentration distribution curve of hydrogen in the inner liner over a period of time; r is the distance from the center of the spherical cavity;

[0055] Consider this part of hydrogen that penetrates into the inner liner as an ideal gas, and calculate the pressure drop of hydrogen in the cavity caused by the hydrogen penetration amount Q during this period. If the pressure drop of hydrogen in the cavity caused by the hydrogen content Q entering the inner liner is smaller than the pressure drop calculated in (5.2), the pressure drop caused by the hydrogen in the cavity penetrating into the inner liner can be ignored.

[0056] (5.2) Considering the pressure drop in the bubble caused by the increase in defect volume, the high-pressure hydrogen in the cavity is used to calculate the compressibility factor Z of the real gas using the Abel-Nobel state equation;

[0057] D1: In each calculation step, the pressure p of the bubble in the current step is first used. i Calculate the compression factor Z i , and then calculate the stress intensity factor K I ; If the crack will further expand after the calculation results are compared, the crack extension length in the next expansion step is limited to be less than the set ratio value of the current crack size;

[0058] D2: The volume of the cavity defect is set to be approximately a tiny cuboid, and the volume V of the cavity defect formed by bubbling is calculated by formula (2);

[0059]

[0060] Where: n is the number of nodes on the crack surface, Δx j Δy j is the grid size at the central node j of a cuboid, u j is the displacement of node j;

[0061] D3: The hydrogen pressure inside the defect during the bubbling process at the i-th crack extension step is calculated by formula (3);

[0062]

[0063] Where: the superscript i represents the number of crack extension steps; p is the hydrogen pressure in the bubble; C is a constant used to modify equation (3), C = pV / ZR g T; R g is the gas constant of hydrogen; Z is the compressibility factor of hydrogen; T is the temperature; V is the volume of the cavity defect formed by bubbling;

[0064] (5.3) Repeat the calculation process of steps D1-D3 until the stress intensity factor K during bubbling is I Less than the fracture toughness K of the material IC , at which point the bubbling process ends.

[0065] Part II Specific Application Examples

[0066] In order to make the content of the present invention more clearly understood, it is described in detail below through specific embodiments in conjunction with the accompanying drawings.

[0067] In this example, the finite element simulation method for the bubbling of the polymer liner of a composite hydrogen storage cylinder specifically includes:

[0068] 1. The inner liner of the hydrogen storage cylinder is made of high-density polyethylene (HDPE) with a thickness of 6 mm; the outer side of the inner liner is wrapped with a carbon fiber composite material with a thickness of 34.9 mm. Samples were taken from the hydrogen storage cylinder to obtain the inner liner material and the carbon fiber composite material as test objects.

[0069] 2. Use conventional testing methods to conduct tensile, fracture mechanics and hydrogen permeation tests on the liner material to obtain the performance parameters of the liner material; conduct tensile and hydrogen permeation tests on the carbon fiber composite material to obtain its performance parameters. If you want to simulate the liner bubbling at different temperatures, you should test both materials at different temperatures. The final performance parameters of the test will be used to construct the finite element model, so at least they should include the true stress-strain curve of the liner material, elastic modulus, yield strength, Poisson's ratio, fracture toughness K IC , JR curve, liner thickness, and hydrogen diffusion coefficient and solubility coefficient of the liner and composite material; further, according to the JR curve, the J integral value corresponding to the appropriate crack size is selected as the critical value J for bubbling occurrence cr .

[0070] 2. Using the hydrogen diffusion coefficient and solubility coefficient of the liner material and carbon fiber composite material, a hydrogen permeation model of a local gas cylinder is established. A hydrogen permeation simulation is performed on a disc-shaped local gas cylinder to obtain the hydrogen permeation pressure distribution in the liner at steady state (e.g. Figure 2 In order to obtain the hydrogen permeation pressure at any position of the inner liner, a curve of the hydrogen permeation pressure in the inner liner changing with the thickness of the inner liner is drawn.

[0071] 3. In ABAQUS software, elastic and plastic material properties are assigned to the inner liner, and elastic properties of the carbon fiber in the composite material layer are assigned, and a finite element model of a composite hydrogen storage cylinder with defect cracks in the inner liner is established. The finite element model is assembled from a three-dimensional model of an inner liner with defect cracks, a three-dimensional model of a bottle valve seat, and an outer carbon fiber winding layer, and hard contact is added between the interacting surfaces of the three models. The defect type can be a pore-type cavity defect or a crack defect; if it is a pore-type cavity defect, an initial crack should be introduced through the cavity wall. Specifically, the integral volume mesh of the crack front is a wedge-shaped unit and is arranged in a ring around the crack tip. The unit type is C3D20R, and the mesh is refined around the crack front tip to form a nested integral volume form surrounding the crack front tip (such as Figure 3As shown in the figure, the mesh independence of the model is verified, and the size of the innermost integral volume is continuously reduced until the J integral value is stable and positive. The crack propagation direction is parallel to the cylinder axis, the crack type is the contour integral, and the mode for handling the singularity of the crack tip is degenerate unit control, using collapsed unit edges and repeated nodes.

[0072] According to the relationship curve between the hydrogen permeation pressure in the liner and the liner thickness, a hydrogen pressure load is applied to the defect of corresponding depth in the liner. The bubbling process of the liner is regarded as quasi-static crack extension, and the hydrogen pressure in the cylinder is the final pressure after the cylinder is depressurized within a period of time.

[0073] 4. Apply the elastic-plastic fracture mechanics theory to solve the J integral value of the defect crack front area. If the solution is greater than the critical value J cr , it is considered that the inner liner is bubbling; then, the linear elastic fracture mechanics theory is further applied to solve the stress intensity factor K at the defect crack front I If the solution is greater than the fracture toughness K of the liner material IC , which is considered as the further evolution of the bubble.

[0074] 5. During the bubble evolution process, the influence of hydrogen permeation from the defect and the increase in defect volume on the pressure drop inside the bubble is considered, and the hydrogen pressure inside the bubble is updated in each crack propagation step.

[0075] The hydrogen pressure drop in the bubble is calculated as follows:

[0076] (5.1) According to formula (1), the concentration distribution curve c(r) of hydrogen diffusion from the cavity to the outside during the pressure release period is integrated to obtain the hydrogen content entering the inner tank;

[0077]

[0078] Where: Q is the hydrogen content that penetrates into the inner liner, c(r) is the concentration distribution curve of hydrogen in the inner liner over a period of time; r is the distance from the center of the spherical cavity;

[0079] If the hydrogen permeation Q in this step causes the pressure drop of hydrogen in the cavity to differ greatly from that in (5.2), it is chosen to ignore the pressure drop in the bubble caused by the outward diffusion of hydrogen to improve the efficiency of the simulation calculation.

[0080] (5.2) Considering the pressure drop in the bubble caused by the increase in defect volume, the high-pressure hydrogen in the cavity is used to calculate the compressibility factor Z of the real gas using the Abel-Nobel state equation;

[0081] Crack propagation in bubble evolution is achieved through the following steps:

[0082] D1: Use the current bubble pressure p in each calculation step i Calculate the compression factor Z i , then calculate the stress intensity factor K I , if the crack can further expand, then the crack extension length of the next expansion step is less than 5% of the current crack size.

[0083] D2: The volume of the cavity defect is set to be approximately a tiny cuboid. Since the crack extension size is small enough, it is assumed that the pressure inside the bubble remains unchanged during the extension process. At the same time, the new crack surface displacement is calculated, and the new cavity defect volume V is obtained. i+1 , the calculation formula is shown in formula (2).

[0084]

[0085] Where: n is the number of nodes on the crack surface, Δx j Δy j is the grid size at the central node j of a cuboid, u j is the displacement of node j;

[0086] D3: Use the compression factor Z calculated in the previous step i , and obtain the new cavity defect internal pressure p i+1 , continue the next round of calculation; in the i-th crack extension step, the hydrogen pressure p inside the defect during the bubbling process i The calculation formula is shown in formula (3);

[0087]

[0088] Where: the superscript i represents the number of crack extension steps; p is the hydrogen pressure in the bubble; C is a constant used to modify equation (3), C = pV / ZR g T; R g is the gas constant of hydrogen; Z is the compressibility factor of hydrogen; T is the temperature; V is the volume of the cavity defect formed by bubbling;

[0089] (5.3) Repeat the calculation process of steps D1-D3 until the stress intensity factor K during bubbling is I Less than the fracture toughness K of the material IC , indicating that the bubbling process is over at this time.

[0090] The above algorithm flow is as follows Figure 5 shown.

[0091] In this way, two fracture mechanics models are used to simulate the bubbling of the inner liner at different stages, which fits the bubbling process and improves the simulation accuracy and applicability. The simulation effect of the bubbling of the inner liner is as follows: Figure 6 shown.

[0092] In summary, the present invention provides a finite element simulation method for bubbling of a polymer liner of a composite hydrogen storage cylinder, which divides the bubbling process into two processes: bubbling occurrence determination and bubbling evolution. First, the elastic-plastic fracture mechanics theory is used to calculate the J integral and the bubbling critical value J. cr Compare and determine whether blistering occurs, and then use linear elastic fracture mechanics theory to calculate the stress intensity factor K I The fracture toughness K of the inner liner material IC A comparison is made to determine whether the bubbling evolves further, and two pressure drop factors are taken into account: the outward diffusion of high-pressure hydrogen in the material defect and the increase in defect volume during the bubbling evolution causing the pressure drop inside the defect. This is consistent with the actual bubbling process, and the analysis results are relatively accurate and have practical engineering guidance significance.

[0093] The above embodiments are only used to illustrate the present invention, and are not used to limit the present invention. As long as they are within the essential spirit of the present invention, changes and modifications to the above embodiments will fall within the scope of the claims of the present invention.

Claims

1. A finite element simulation method for bubbling polymer liner of composite hydrogen storage cylinder, characterized in that: The following steps are involved: (1) The hydrogen storage cylinder used as the research object of finite element simulation includes a polymer liner and a carbon fiber composite material winding layer wrapped around the outer side of the liner; samples are taken from the hydrogen storage cylinder, and tensile, fracture mechanics and hydrogen permeation tests are performed on the liner material, and tensile and hydrogen permeation tests are performed on the carbon fiber composite material to obtain the performance parameters of the liner material and the carbon fiber composite material; (2) Using the performance parameters of the liner material and carbon fiber composite material, a local gas cylinder hydrogen permeation model was established to obtain the relationship curve between hydrogen permeation pressure and liner thickness; (3) Establish a finite element model of a composite hydrogen storage cylinder with a polymer liner containing defective cracks; the model is assembled from a three-dimensional model of the liner with defective cracks, a three-dimensional model of the bottle valve seat, and an outer carbon fiber winding layer, and hard contact is added between the interaction surfaces of the three models; In the three-dimensional model of defect crack inner liner, a deep defect below the inner liner surface is introduced, and the defect type is a pore-like cavity defect or a crack defect; for the pore-like cavity defect, an initial crack penetrating through the cavity wall is further introduced; According to the relationship curve between hydrogen permeation pressure in the liner and liner thickness, a hydrogen pressure load is applied to the defects of corresponding depth in the liner, and the liner bubbling process is regarded as quasi-static crack extension; (4) Apply the elastic-plastic fracture mechanics theory to solve the J integral value of the defect crack front area. If the solution is greater than the critical value J cr , it is considered that bubbling occurs in the liner; The linear elastic fracture mechanics theory is further applied to solve the stress intensity factor K at the defect crack front. I If the solution is greater than the fracture toughness K of the liner material IC , which is considered as the further evolution of the bubble; (5) During the bubble evolution process, the effects of hydrogen permeation from the defect and the increase in defect volume on the pressure drop inside the bubble are considered, and the hydrogen pressure inside the bubble is updated in each crack propagation step.

2. The method according to claim 1, characterized in that The performance parameters of the liner material and the carbon fiber composite material obtained in step (1) include at least: the true stress-strain curve of the liner, elastic modulus, yield strength, Poisson's ratio, fracture toughness K IC , JR curve, liner thickness, and hydrogen diffusion coefficient and solubility coefficient of the liner and composite winding layer; further, according to the JR curve, the J integral value corresponding to the appropriate crack size is selected as the critical value J of bubbling occurrence cr .

3. The method according to claim 1, characterized in that In the step (2), when establishing the hydrogen permeation model of the local gas cylinder, the shape of the local gas cylinder is selected to be a disc.

4. The method according to claim 1, characterized in that: In the pore-like cavity defect or crack defect in step (3), the crack propagation direction is parallel to the cylinder axis, and the crack type is contour integral; the processing mode for the singularity of the crack tip is degenerate unit control, using collapsed unit edges and repeated nodes.

5. The method according to claim 1, characterized in that In the step (3), the crack front integral volume grid is a wedge-shaped unit and is arranged in a ring around the crack tip. The unit type is C3D20R. The grid is refined around the crack front tip to form a nested integral volume form surrounding the crack front tip. The model is verified for grid independence, and the size of the innermost integral volume is continuously reduced until the obtained J integral value tends to be stable and positive.

6. The method according to claim 1, characterized in that In the step (3), when a load is applied to the hydrogen pressure of the deep defect in the liner, the hydrogen pressure in the gas cylinder is the final pressure after the gas cylinder is depressurized within a period of time.

7. The method according to claim 1, characterized in that In the step (5), during the bubbling evolution process, the hydrogen pressure drop in the bubbling is calculated according to the following method: (5.1) The cavity defect is approximated as a radius of r void The concentration distribution curve c(r) of hydrogen diffusion from the cavity to the outside during the pressure release period is integrated to obtain the hydrogen content entering the inner tank; (5.2) Considering the pressure drop in the bubble caused by the increase in defect volume, the high-pressure hydrogen in the cavity is used to calculate the compressibility factor Z of the real gas using the Abel-Nobel state equation; D1: In each calculation step, the pressure p of the bubble in the current step is first used. i Calculate the compression factor Z i , and then calculate the stress intensity factor K I ; If the crack will further expand after the calculation results are compared, the crack extension length in the next expansion step is limited to be less than the set ratio value of the current crack size; D2: Set the volume of the cavity defect to be approximately a tiny cuboid and calculate the volume V of the cavity defect formed by bubbling; D3: Calculate the hydrogen pressure inside the bubbling defect in the i-th crack extension step of the bubbling process; (5.3) Repeat the calculation process of steps D1-D3 until the stress intensity factor K during bubbling is I Less than the fracture toughness K of the material IC , at which point the bubbling process ends.

8. The method according to claim 7, characterized in that In the step (5.1), the hydrogen content permeating from the cavity into the inner liner is calculated according to the following formula: Where: Q is the hydrogen content that penetrates into the inner liner, c(r) is the concentration distribution curve of hydrogen in the inner liner over a period of time; r is the distance from the center of the spherical cavity; Treat this part of hydrogen that penetrates into the inner liner as an ideal gas, and calculate the pressure drop of hydrogen in the cavity caused by the hydrogen penetration amount Q during this period; if the pressure drop of hydrogen in the cavity caused by the hydrogen content Q entering the inner liner is smaller than the pressure drop calculated in (5.2), then the pressure drop caused by the penetration of hydrogen in the cavity into the inner liner can be ignored.

9. The method according to claim 7, characterized in that: In the step D2, the volume V of the cavity defect formed by bubbling is calculated according to the following formula: Where: n is the number of nodes on the crack surface, Δx j Δy j is the grid size at the central node j of a cuboid, u j is the displacement of node j.

10. The method according to claim 7, characterized in that In step D3, the hydrogen pressure inside the defect during the bubbling evolution process is calculated according to the following formula: Where: the superscript i represents the number of crack extension steps; p is the hydrogen pressure in the bubble; C is a constant used to modify equation (3), C = pV / ZR g T; R g is the gas constant of hydrogen; Z is the compressibility factor of hydrogen; T is the temperature; V is the volume of the cavity defect formed by bubbling.

Citation Information

Patent Citations

  • Passivation line equation analysis method for elastic-plastic fracture toughness test

    CN112098208A

  • Method for constructing bursting pressure model of hydrogen conveying pipeline under coupling action of hydrogen embrittlement and hydrogen corrosion

    CN116911112A

  • High-pressure hydrogen permeation test device and pressure difference test method for IV-type gas cylinder liner material

    CN117092010A

  • Fracture toughness determination using spiral-grooved cylindrical specimen and pure torsional loading