Resistive memory cell
By using conductive vanadium oxide V2O3 layer and titanium nitride-based electrode in nonvolatile resistive memory, combined with ion beam deposition technology, the problems of long write time and limited rewrite cycles of existing memory are solved, and the CMOS is realized The back-end integrated high-efficiency resistive memory cell has good durability and high resistance state switching capabilities.
Patent Information
- Application Number
- CN202410567292.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-09
- Filing Date
- 2024-05-09
- Publication Date
- 2024-11-12
AI Technical Summary
Existing nonvolatile resistive memory such as EEPROM and FLASH type memory has problems such as long write time, low storage point density and limited rewrite cycles. Moreover, Motex memory has a large thermal budget limitation when integrating CMOS backend, which is difficult to compatible.
Using a nonvolatile resistive memory cell based on vanadium oxide, a titanium nitride-based lower electrode and an upper electrode, the active layer is made of conductive vanadium oxide V2O3, and a conductive V2O3 layer is made through ion beam deposition technology to achieve high temperature Crystallized or partially crystallized conductive V2O3 material, suitable for CMOS back-end integration.
Bipolar switching operation between high and low resistance states is achieved, suitable for CMOS back-end processes, improves memory integration and durability, and supports more than 1000 write and erase cycles.
Smart Images

Figure CN118946158A_ABST
Abstract
Description
Technical Field
[0001] The technical field of the present invention is the technical field of resistive memory. The present invention relates to a non-volatile resistive memory cell. Background Art
[0002] Non-volatile memories of the EEPROM or FLASH type are often used for applications that need to store information even when the voltage is switched off. However, these memories have disadvantages such as long write times, a density of memory points limited by the size of the transistors used, and a limited number of rewrite cycles.
[0003] Recently, non-volatile resistive memory is a promising alternative to FLASH or EEPROM type memories.
[0004] Resistive memory is based on the use of an active medium whose resistance depends on the voltage applied across the material. In other words, a resistive memory cell has two states: the HRS state ('high resistance state') and the LRS state ('low resistance state'). The active medium is inserted between two electrodes, allowing the application of a voltage and ensuring the reading and writing of the state of the resistive memory cell.
[0005] Different types of resistive memory can be made, depending on the type of active material used: phase change material (PCRAM or 'Phase Change RAM', also known as PCM or 'Phase Change Memory'), ion conducting material (CBRAM or 'Conductive Bridging RAM'), metal oxide material (OxRAM or 'Oxide Resistive RAM'), magnetic material (MRAM or 'Magnetic RAM'), spin transfer torque magnetic material (STTRAM or 'Spin Torque Transfer RAM') or Mott insulator.
[0006] The so-called 'Mott' memory is based on the use of an active layer made of a Mott insulating material which, according to the band theory, should be conductive but which is in fact insulating due to strong electron correlations. The material can be made to transition from this Mott insulating state to a metallic state by applying pressure or an electric field. In a Mott memory, a set (SET) voltage applied to the memory electrode makes it possible to control the transition from the insulating state to the metallic state, and a reset (RESET) voltage applied to the memory electrode makes it possible to control the transition from the metallic state to the insulating state. It should be noted that Mott memories are of the non-polar type: in other words, the sign of the applied set or reset voltage is irrelevant, unlike resistive memories of the bipolar type (such as CBRAM memories), for example, for which it is necessary to reverse the sign of the potential applied to the electrodes depending on whether a set or reset operation is sought.
[0007] In Mott insulators, some of the vanadium atoms in crystalline vanadium trioxide are replaced by chromium, such as (V 1- x C x )2O3 (where x ≥ 0.011), which is a Mott insulator in which a reversible resistive switching phenomenon induced by an electrical pulse is possible. Therefore, it is used to make a Mott memory. The advantage of Mott resistive memories over other RRAM resistive memories is that they are based only on electronic transition phenomena. Unlike some other resistive memories that have an initial state (original state) in which the active material of the active storage area is insulating, Mott memories do not require an initialization step (i.e., a step during which the first electrical stress must therefore be applied to the blank memory cell in order to generate the LRS state for the first time).
[0008] Crystalline (V1-xCr) materials that can be used in Mott memories have been fabricated by physical vapor deposition (PVD) techniques such as magnetron sputtering. x )2O3 (where x ≥ 0.011): To this end, a target based on vanadium and chromium is milled with argon ions under oxygen pressure to obtain amorphous vanadium oxide that is not stoichiometric in oxygen and chromium. However, the material used in the Mott memory (V1-xCr x )2O3 (where x ≥ 0.011) must be crystalline and completely stoichiometric. Thus, the PVD deposition step is followed by an annealing step in a reducing atmosphere at a temperature greater than or equal to 500°C. This technique has some disadvantages in back-end CMOS integrated logic, where the thermal budget should not exceed 450°C. Summary of the invention
[0009] The present invention provides a solution to the previously discussed problems by providing a vanadium oxide based non-volatile resistive memory cell which is particularly easier to integrate into CMOS back-end processes.
[0010] A resistive memory cell refers to an electrical device that has a first high resistance state or HRS state or reset (RESET) state and a second low resistance state or LRS state or set (SET) state. Non-volatility resides in the fact that the memory cell retains its resistance state once the set or reset voltage is no longer applied.
[0011] More specifically, an object of the present invention is a resistive memory cell comprising:
[0012] - Titanium nitride based lower electrode,
[0013] - Upper electrode,
[0014] - an active layer having a first contact surface with the lower electrode and a second contact surface with the upper electrode, the active layer comprising a region called a local region made of a material including vanadium, titanium and oxygen extending from the first contact surface, the remainder of the active layer being made of conductive vanadium oxide V2O3.
[0015] Conductive vanadium oxide V2O3 refers to V2O3 materials with a resistivity less than or equal to 0.1 ohm.cm.
[0016] Based on the use of Mott insulator phase (V1-xCr x )2O3 (where x ≥ 0.011), the memory cell according to the invention uses an active layer made mainly of V2O3 having a single region in the layer at the interface between the active layer and the lower electrode: this region of the active layer at the lower electrode is not made of the conductive vanadium oxide V2O3 and comprises a high resistance material containing vanadium, titanium and oxygen. Surprisingly, the Applicant has found that such a cell has a resistive memory operation enabling it to switch between a high resistance HRS state and a low resistance LRS state. These reset and set operations are performed by applying a potential difference of opposite polarity between the upper and lower electrodes of the memory cell: in other words, unlike a Mott memory, the cell according to the invention has a bipolar operation.
[0017] Surprisingly, the applicant has discovered the operation of the present invention when the insulating V2O3 material for Mott memory is manufactured using the IBD (Ion Beam Deposition) technique; by using this deposition technique, the inventors have obtained a conductive V2O3 material and is therefore not suitable for Mott memory known in the prior art. However, by performing a reset / set (RESET / SET) cycle operation on a stack comprising a conductive V2O3 active layer as deposited between two electrodes, the inventors have noticed a resistive memory type operation. They also noticed that during a first initialization operation, the conductive V2O3 layer transitions from a low resistance LRS state to a high resistance HRS state, with this single high resistance local region based on titanium, oxygen and vanadium appearing in the V2O3 layer. This particular cell structure, including this region formed by a V-Ti-O alloy, confers the cell according to the present invention the action of a bipolar resistive memory cell. The structure of the cell, its operation and the mechanism for creating this local V-Ti-O region, which may be associated with the strong heating at the interface between the lower electrode and the active layer during the initialization step, will be described later. It should be noted that the IBD deposition technique enables the fabrication of crystalline or partially crystalline conductive V2O3 layers at crystallization temperatures greater than 280°C, thus being perfectly compatible with CMOS back-end integration.
[0018] It should be noted that the terms 'lower' and 'upper' are of course used for a better understanding of the invention but remain relative so that the lower electrode is considered the upper electrode and the upper electrode is considered the lower electrode by inverting the memory cell while remaining within the field of application of the memory cell according to the invention.
[0019] It should be noted that the memory according to the present invention is applicable to other lower electrode materials selected from the following materials: Ta, TaN, Cu, W, Pt, Au or Ag. In this case, the local area includes Ta (in the case of Ta or TaN lower electrode), Cu (in the case of Cu lower electrode), W (in the case of W lower electrode), Pt (in the case of Pt lower electrode), Au (in the case of Au lower electrode) or Ag (in the case of Ag lower electrode) in addition to vanadium and oxygen.
[0020] Similarly, the memory according to the invention can be applied to any type of active layer made of conductive vanadium oxide. In other words, the active layer can be made of conductive V2O3, but also of conductive V6O 13 made of VO2 in its metallic rutile phase, or (i.e., a substoichiometric substitution of V2O3 in Cr relative to vanadium). More generally, all conductive VnO 2n-1 Vanadium oxides of the type vanadium oxides (where n is an integer greater than or equal to 2) have a temperature-resistance transition and become conductive above a certain temperature: they can therefore be applied to the memory according to the invention in the event that this temperature is reached during operation of the memory cell. Even more generally, all vanadium oxides that are made conductive by any possible method (temperature, electric field, laser pulse, etc.) can be applied to the method according to the invention.
[0021] In addition to the features discussed immediately above in the paragraph above, the memory cell according to the invention may have one or more additional features from the following, considered alone or in any technically possible combination:
[0022] - - The upper electrode is based on titanium nitride;
[0023] - - the local area is not in contact with the second contact surface;
[0024] - - The thickness of the active layer is between 5 nm and 200 nm;
[0025] - - the local area is in the shape of a dome whose cross section parallel to the plane of the layer decreases from the first contact surface;
[0026] - the titanium nitride-based lower electrode comprises vanadium, titanium and oxygen in a region close to the first contact surface. In this case, the local region has, for example, a mushroom shape having a dome whose cross section parallel to the plane of the layer decreases from the first contact surface;
[0027] - - The first contact surface has a diameter less than or equal to 9000 nm 2 and preferably less than or equal to 6000 nm 2 area;
[0028] - - The first contact surface is equal to the upper surface of the lower electrode and strictly smaller than the total lower surface of the active layer;
[0029] - - The lower electrode has a 'wall' type rectangular parallelepiped shape or an L shape;
[0030] - - The conductive vanadium oxide V2O3 is crystalline or partially crystalline;
[0031] - - Local areas are made of crystalline or partially crystalline material.
[0032] Another object of the invention is a method for manufacturing a memory cell, the method comprising the following steps:
[0033] - Fabrication of titanium nitride based lower electrode;
[0034] - depositing a layer made of vanadium oxide V2O3 having a first contact surface with the lower electrode;
[0035] - Manufacturing the upper electrode;
[0036] The method comprises a step known as initialization step, which consists in injecting a current through the stack formed by the lower electrode, the V2O3 layer and the upper electrode, the current density being chosen so as to create said localized area comprising vanadium, titanium and oxygen.
[0037] In addition to the features just discussed in the above paragraphs, the manufacturing method according to the invention may have one or more of the following additional features, considered alone or in any technically possible combination:
[0038] - the method comprises a heat treatment step during or after said deposition step until said vanadium oxide V2O3 layer is rendered conductive;
[0039] - the deposited layer is made of amorphous vanadium oxide V2O3;
[0040] - The current density of the initialization step is greater than or equal to 50.10 6 A / cm 2 ;
[0041] - Deposition of a layer made of vanadium oxide V2O3 using ion beam deposition technology;
[0042] - the method comprises, before the step of depositing V2O3, a step of cleaning the lower electrode by in-situ ion etching (Ar, Xe or Kr) (i.e. in the same equipment as the step of depositing V2O3, without exhaust);
[0043] - Fabrication of the upper electrode can be done in situ or after exhaust. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] These drawings are set forth by way of illustration and not for the purpose of limiting the invention.
[0045] [ Figure 1 ] schematically represents a 3D view of a memory cell according to the present invention.
[0046] [ Figure 2 ] represents the behavior during 1000 write (SET) and erase (RESET) cycles of a memory cell according to the invention.
[0047] [ Figure 3 ] shows a dark field STEM image of a memory cell before initialization.
[0048] [ Figure 4 ] shows a dark field STEM image of a memory cell according to the present invention.
[0049] [ Figure 5 ]、[ Figure 6 ]、[ Figure 7 ]and[ Figure 8 ] shows energy dispersive X-ray spectroscopy (EDX) and TEM microscopic analysis of a memory cell according to the present invention.
[0050] [ Fig. 9 ]、[ Fig.10 ]、[ Fig.11 ]and[ Fig.12 ] [ Fig.13 ]、[ Fig.14 ]and[ Fig.15 ] shows the results of write (SET) and erase (RESET) cycles of cells with different contact surfaces and different active layer thicknesses according to the present invention.
[0051] [ Fig.16 ] schematically illustrates the operation of a memory cell according to the present invention.
[0052] [ Fig.17] shows a dark field STEM image and electron energy loss spectroscopy (EELS) analysis showing the absence of oxygen and vanadium in the upper portion of the lower electrode of the memory cell before initialization.
[0053] [ Fig.18 ] shows a dark field STEM image and EELS analysis showing the presence of oxygen and vanadium in the upper part of the lower electrode of a memory cell according to the present invention.
[0054] [ Fig.19 ] shows a dark field STEM image of a memory cell according to the present invention.
[0055] [ Fig. 20 ] shows Energy Dispersive X-ray spectroscopy EDX and TEM microanalysis illustrating vanadium depletion in a localized area of a memory cell according to the present invention.
[0056] The invention and its various applications will be better understood by reading the following description and viewing the accompanying drawings. DETAILED DESCRIPTION
[0057] Unless otherwise indicated, identical elements appearing in different figures have a unique reference.
[0058] [ Figure 1 ] schematically represents in three dimensions a memory cell 1 according to the invention in a reference system Oxyz, the plane Oxy defining the plane of the layer, the axis Oz defining the direction of the height of the layer, the axis Oy defining the direction of the length of the layer and the axis Ox defining the direction of the width of the layer.
[0059] The memory unit 1 comprises:
[0060] - TiN lower electrode 2;
[0061] - TiN top electrode;
[0062] - an active layer 3 , which is mainly made of conductive vanadium oxide V 2 O 3 and is crystallized or partially crystallized, but has a single local area 5 comprising titanium, vanadium and oxygen, as will be described below.
[0063] The upper surface of the active layer 3 is in contact with the lower surface of the upper electrode 4 along the contact surface S2 .
[0064] The lower surface of the active layer 3 contacts the upper surface of the lower electrode 2 along the contact surface S1 .
[0065] The lower electrode 2 has a "wall" type architecture, i.e. it forms a parallelepiped wall of length l, width L and height h: the area of the upper surface of the electrode 1xL is strictly smaller than the area of the lower surface of the active layer 3; in other words, the area of the contact surface S1 is equal to 1xL. The area of the contact surface S1 is strictly smaller than the area of the contact surface S2 (i.e. the lower electrode 2 here has a width L much smaller than the width of the upper electrode 4 and a length l less than or equal to the length of the upper electrode 4). It should be noted that the lower electrode 2 can also have other shapes, such as an L-shape with an upper first portion identical to the above-described wall and a lower second portion of parallelepiped shape parallel to the layer plane.
[0066] The active layer 3 of the memory cell 1 according to the invention can be produced in particular by depositing a crystalline or partially crystalline conductive V2O3 layer using the ion beam deposition IBD technique. The deposition comprises sputtering a vanadium target by an argon ion beam. The deposition chamber is evacuated (5x10 -8 During the deposition process, the partial pressure of oxygen is controlled and influences the degree of oxidation of the final material. The deposition takes place at room temperature and does not necessarily require a heat treatment, thus making the method for obtaining a memory cell according to the invention compatible with CMOS back-end integration. Even if a crystallization anneal is employed, it remains below 450°C, which is the maximum temperature for CMOS back-end integration.
[0067] According to another embodiment, after the IBD deposition, the V2O3 is insulating (resistivity in the order of a few ohm.cm to tens of ohm.cm) and amorphous (no diffraction peaks detected by XRD characterization). Optionally, annealing is performed at a temperature lower than 450°C and preferably greater than or equal to 280°C in order to obtain a crystalline or partially crystalline conductive V2O3 material (i.e. with a resistivity less than or equal to 0.1 ohm.cm). It should be noted that the annealing step can be performed during the fabrication of a wall-type memory cell that implements some technological steps, such as the deposition of the encapsulation dielectric at a temperature of the order of 300°C (temperature at which the amorphous IBD V2O3 crystallizes).
[0068] The preparation of the titanium nitride-based upper and lower electrodes is carried out according to techniques well known to those skilled in the art. At this stage, the active layer is made of only crystalline or partially crystalline conductive V2O3, however, it has been seen that the active layer 3 according to the invention comprises a single local area 5 containing titanium, vanadium and oxygen. Conductive V2O3 can also be obtained by other deposition techniques such as PVD deposition. Crystallized conductive V2O3 can also be used, in which part of the vanadium is replaced by chromium, as long as the V2O3 remains conductive.
[0069] In order to obtain this single local area 5, it is advisable to carry out an initialization step with the stack formed by two electrodes (the lower electrode having the shape of the wall 2) and a crystalline or partially crystalline conductive V2O3 layer. It should be understood that at this stage, called the original state (ie the blank state), the stack is in a low resistance LRS state, since the V2O3 layer is conductive. The initialization step consists in injecting a current with a high current density (preferably strictly greater than 50.10 Å) by applying a positive voltage (initialization voltage) between the first electrode and the second electrode. 6 A / cm 2 ) current. This step causes the stack to switch from its original LRS state to a high resistance HRS state and results in the appearance of Figure 1 The localized region 5 shown. The appearance of this region comprising titanium, oxygen and vanadium can be explained by the injection of a high-density current at the contact surface S1 between the first electrode 2 and the active layer 3. The area lxL of the upper surface of the wall-shaped first electrode is chosen to be small enough to cause local heating in S1 and in the region close to S1, that is, above the active region 3 and below the first electrode 2. Electrothermal simulations using the COMSOL tool show that the temperature reached at the interface between the lower wall electrode 2 and the active layer 3 can reach 2000°K: this localized heating causes the creation of a region 5 made of V-Ti-O alloy, which includes a first portion 6 in the shape of a dome extending from the first contact surface S1 and rising inside the active layer 3, and a second portion 7 located on the upper end of the lower electrode 2. In other words, the region 5 has a mushroom shape with its cap in the active region 3 and its foot at the top of the lower electrode 2.
[0070] Once this initialization operation has been performed and the V-Ti-O based region 5 has been created, the memory cell 1 behaves as a bipolar resistive memory cell. In other words, the application of a set (SET) voltage pulse will make it possible to perform a set operation and switch to the low resistance LRS state. Then, the application of a reset (RESET) voltage pulse of opposite sign to the set voltage will make it possible to switch to the high resistance HRS state. The memory cell has a non-volatile behavior such that the memory cell retains the resistance value once the set or reset voltage is no longer applied. Figure 2The behavior of a memory cell according to the invention over 1000 write (set) and erase (reset) cycles is shown, where the thickness of the active layer is 50 nm, the length 1 of the wall-type lower electrode is 100 nm and the width L is 24 nm. The set pulse is 1.2 V for 100 ns and the reset pulse with opposite polarity to the set pulse is 1.3 V for 200 ns. Good endurance performance (i.e., over 1000 set / reset cycles) is observed for the memory cell according to the invention, which switches from an LRS resistance of a few kOhm to an HRS resistance of the order of hundreds of kOhm. The endurance results show a lower dispersion of the resistance states compared to other types of resistive memories, such as CBRAM or OxRAM. Note that the set and reset pulses have amplitudes of less than 2 V and durations of less than 1 µs.
[0071] Highlight local area 5 has passed Figure 3 and Figure 4 The scanning transmission electron microscopy (STEM) images shown in FIG. Figure 3 shows a dark field STEM image of the cell before initialization, and Figure 4 A dark field STEM image of a memory cell according to the invention is shown after an initialization step and 40 programming cycles. Figure 4 The circle represented in FIG. 1 encloses the TiN wall bottom electrode created after the initialization step. Figure 1 A specific region 5 in . This region 5 does not exist before the initialization step Figure 3 On the surface, this region 5 is a modified region of high atomic density with a dome shape of a few nanometers thick, the cross section of which parallel to the plane of the layer decreases from the first contact surface. It should be noted that this region 5 is located inside the conductive V2O3 active layer 3 and has an atomic density different from the atomic density of the conductive V2O3 part. It should also be noted that this region 5 starts from the contact surface between the active layer 3 and the lower TiN electrode 2, and then rises in the thickness of the active layer 3 without reaching the upper surface of the active layer 3, so that the region 5 is not in contact with the upper electrode 4: the local region 5 remains during the different programming cycles and can be regarded as a region in contact with the lower electrode 2 in a more overall conductive V2O3 region. The fact that the memory cell according to the invention is in a high resistance state after the initialization step indicates that the region 5 is made of a high resistance material. Therefore, the initialization step causes a change in the composition of the conductive V2O3 material in this region and the formation of a high resistance alloy based on vanadium, titanium and oxygen. This result is supported by literature data, which show that the high resistivity of the TiO2-V2O3-V2O5 alloy is about 105 Ohm.cm and is most importantly achieved by Figures 5 to 8 EDX (Energy Dispersive X-ray) spectroscopy analysis shown in FIG5 demonstrates the presence of titanium in this particular region 5 . Figures 5 to 8 Each said:
[0072] - in the right part, a TEM (Transmission Electron Microscope) image of a memory cell according to the invention;
[0073] - At the top, the diffraction pattern of the area enclosed by the rectangle in the TEM image;
[0074] - On the bottom, EDX spectrum of the area enclosed by the rectangle in the TEM image.
[0075] TEM and EDX analysis show the creation of a local area in the shape of a dome 6 comprising vanadium, titanium and oxygen. The presence of vanadium and oxygen is not surprising since this area is located in a layer originally made of V2O3. On the other hand, EDX analysis clearly shows the presence of titanium in the first wall-type electrode and also directly above the first electrode and in the Figure 1 5 . It can be noted that the amount of titanium is greater at the contact interface S1 between the active layer 3 and the lower electrode 2 , then gradually decreases until it disappears in the active layer 3 , which comprises only V2O3 on its top: this observation makes it possible to clearly identify a single area 5 that does not extend over the entire height of the active layer 3 . The presence of titanium is again evident at the upper electrode 4 .
[0076] Fig.17 and Fig.18 EELS analysis by electron energy loss spectroscopy is shown, showing the distribution of vanadium and oxygen for a stack of memory cells according to the invention before an initialization step and for a memory cell according to the invention once formed, respectively. Fig.17 and Fig.18 , top shows a transmission electron microscope image of the analyzed area: the lower electrode as well as the active layer can be seen. Fig.17 In the EELS image of the uninitialized stack (Vanadium on the bottom left and Oxygen on the bottom right), only V and O are present in the active layer. Fig.18 In FIG. 1 , an EELS image of a memory cell according to the invention (vanadium at the bottom left, oxygen at the bottom right) shows the presence of oxygen and vanadium in addition to titanium in the top 7 of the lower electrode 2. Thus, there is in fact a mushroom-shaped local region 5 (dome 6 and upper part 7 of the lower electrode) comprising vanadium, titanium and oxygen.
[0077] Figures 9 to 15Cycling results of cells according to the invention with different contact surfaces S1 and different thicknesses of the active layer 3 are shown. These results show that the thickness of the conductive V2O3 layer has little influence on the memory behavior of the cell according to the invention: however, this thickness is preferably between 5 nm and 200 nm and even more advantageously between 10 nm and 100 nm. The contact surface S1 (ie, corresponding to the upper surface of the lower wall electrode 2) is preferably less than 6000 nm2.
[0078] Fig.16 An explanation of the operating mode of a cell according to the invention is schematically shown. The left hand side of the figure shows the stack before the initialization step in the absence of a local high resistance region 5: in this blank configuration, the stack is low resistance. After the initialization step, in order to transition from the low resistance blank state to the high resistance HRS state, a memory cell 1 according to the invention is created in the presence of a single high resistance region 5 comprising in particular Ti, V and O. The resistive memory cell can then behave as a filament resistive memory, in which the single region 5 acts as a solid electrolyte. Thus, when a positive potential is applied to the lower electrode 2, mobile titanium-based ions will move from the lower electrode 2 under the action of the electric field applied to the electrode, causing titanium metal filaments to grow within the single Ti, V and O-based region 5. When the rest of the active layer 3 is made of metal oxide, the memory cell according to the invention is subsequently transformed into a low resistance LRS state. The transition to the high resistance state HRS comprises applying a negative voltage to the lower electrode 2, causing the conductive filament to completely or partially dissolve.
[0079] It should be noted that according to another embodiment, the memory cell according to the invention is made of a stack of the TiN / V2O3 / TiN type comprising a 10 nm thick V2O3 active layer which has not yet been annealed. After initialization, the local area is formed by contact with the surface S1 of the lower electrode and the surface S2 of the upper electrode. This Fig.19 It is shown in Fig.19 A STEM scanning transmission electron microscope image of a local region 5 is shown, which extends from the surface of the lower electrode to the surface of the upper electrode.
[0080] The localized region or dome further includes a volumetric vanadium atom depletion of greater than or equal to 20% (i.e., about 40% or even more) relative to the vanadium atoms present in the volume of the remainder of the vanadium oxide active layer. The presence of voids is also observed. The vanadium atom depletion in Fig. 20 The middle panel shows, which corresponds to the initialization spectrum showing vanadium consumption at a local area ( Fig. 20 The highest spectral curve shows vanadium consumption).
[0081] Other stacks of memory cells according to the invention are made with a thickness e of the active layer, a length l and a width L of the wall-type lower electrode:
[0082] - TiN upper electrode / non-stoichiometric crystalline V2O3 active layer with a thickness e equal to 5 nm, 10 nm or 20 nm respectively, with 10% Cr substitution relative to vanadium (10 atomic % Cr relative to V+Cr or 4 atomic % Cr relative to V+Cr+O) / TiN wall-type lower electrode (with a width L of the order of 15 nm and a length l varying from 40 nm to 300 nm).
[0083] - TiN upper electrode / crystalline V2O3 active layer with 20 nm thickness / TiN lower electrode
[0084] - TiN upper electrode with thickness e of 50 nm / crystalline V2O3 active layer / TiN wall-type lower electrode (with width L of the order of 10 nm and length l varying from 40 nm to 300 nm)
[0085] - TiN upper electrode / amorphous V2O3 active layer with a thickness e of 10 nm / TiN wall-type lower electrode (with a width L of the order of 10 nm and a length l varying from 40 nm to 300 nm).
Claims
1. A resistive memory cell (1), comprising: - a lower electrode (2) based on one of the following materials: titanium nitride TiN, tantalum nitride TaN, tantalum Ta, copper Cu, tungsten W, platinum Pt, gold Au or silver Ag, - upper electrode (4), - an active layer (3), the active layer (3) having a first contact surface (S1) with the lower electrode and a second contact surface (S2) with the upper electrode, the active layer (3) comprising a region, referred to as a local region (5), made of a material comprising vanadium, oxygen and Ti if the material of the lower electrode is TiN, or Ta if the material of the lower electrode is TaN or Ta, or Cu if the material of the lower electrode is Cu, or W if the material of the lower electrode is W, or Pt if the material of the lower electrode is Pt, or Au if the material of the lower electrode is Au, or Ag if the material of the lower electrode is Ag, the local region extending from the first contact surface (S1), the remainder of the active layer being made of conductive vanadium oxide.
2. Memory unit according to the preceding claim, characterized in that The upper electrode (4) is based on titanium nitride.
3. The memory cell according to claim 1, characterized in that The local area is not in contact with the second contact surface (S2).
4. The memory unit according to claim 1, characterized in that The local area is in contact with the second contact surface (S2).
5. The memory cell according to claim 1, characterized in that The local region has a volumetric vanadium atomic depletion greater than or equal to 20% relative to the remainder of the active layer.
6. A memory cell according to any one of the preceding claims, characterized in that The thickness of the active layer is between 5 nm and 200 nm, and preferably between 10 nm and 100 nm.
7. The resistive memory cell according to claim 1, characterized in that The partial region has the shape of a dome whose cross section parallel to the plane of the layer decreases from the first contact surface.
8. The memory cell according to claim 1, characterized in that The titanium nitride-based lower electrode includes vanadium, titanium, and oxygen in a region proximate to the first contact surface.
9. The memory unit according to claim 1, characterized in that The first contact surface has a diameter less than or equal to 9000 nm 2 and preferably less than or equal to 6000 m 2 area.
10. The memory cell according to claim 1, characterized in that The first contact surface is equal to the upper surface of the lower electrode and is strictly smaller than the total lower surface of the active layer.
11. The memory cell according to claim 1, characterized in that The lower electrode has a "wall" type rectangular parallelepiped shape or an L-shape.
12. The memory cell according to claim 1, characterized in that The conductive vanadium oxide is crystalline or partially crystalline.
13. The memory cell according to claim 1, characterized in that The local area is made of a crystalline or partially crystalline material.
14. A method for producing a resistive memory cell according to any one of the preceding claims, characterized in that The method comprises the following steps: - The lower electrode is made of one of the following materials: titanium nitride TiN, tantalum nitride TaN, tantalum Ta, copper Cu, tungsten W, platinum Pt, gold Au or silver Ag; - depositing a layer made of vanadium oxide, the layer having a first contact surface with the lower electrode; - Manufacturing the upper electrode; The method comprises a step known as an initialization step, which comprises injecting a current through the stack formed by the lower electrode, the vanadium oxide layer and the upper electrode, the current density being chosen to create the local area comprising vanadium, oxygen and Ti if the material of the lower electrode is TiN, or Ta if the material of the lower electrode is TaN or Ta, or Cu if the material of the lower electrode is Cu, or W if the material of the lower electrode is W, or Pt if the material of the lower electrode is Pt, or Au if the material of the lower electrode is Au, or Ag if the material of the lower electrode is Ag.
15. Method according to the preceding claim, characterized in that The method includes a heat treatment step during or after the depositing step until the vanadium oxide layer is made conductive.
16. Method for producing a memory cell according to one of the preceding claims, characterized in that The current density of the initialization step is greater than or equal to 50.10 6 A / cm 2 .
17. Method for producing a memory cell according to one of the preceding claims, characterized in that Deposition of the layer made of vanadium oxide is carried out by means of an ion beam deposition technique.