Catalyst support material for ammonia synthesis
The problems of high energy consumption and CO2 emissions in the Haber-Bosch process are solved by using (MgO)x(BaO)y(Al2O3)z or (MgO)x(SrO)y(Al2O3)z as support materials and dispersing ammonia synthesis catalysts. , realizes efficient ammonia synthesis under lower conditions.
Patent Information
- Application Number
- CN202380024338.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-01
- Filing Date
- 2023-03-01
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
There are high energy consumption and CO2 emission problems in the existing ammonia synthesis process, especially in the Haber-Bosch process, and it is necessary to improve catalyst activity to achieve efficient ammonia synthesis at lower temperatures and pressures.
Using (MgO)x(BaO)y(Al2O3)z or (MgO)x(SrO)y(Al2O3)z as catalyst support materials, dispersing ammonia synthesis catalysts such as ruthenium, by optimizing the composition of the support material and the dispersion method of the catalyst, Improve the rate of ammonia synthesis.
The ammonia synthesis rate is significantly improved at lower temperatures and pressures, reducing energy consumption and CO2 emissions, and improving the efficiency of catalyst utilization.
Smart Images

Figure CN118946404A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to U.S. Provisional Patent Application No. 63 / 315,408, filed on March 1, 2022, entitled “CATALYST SUPPORT MATERIALS FOR USE IN AMMONIA SYNTHESIS,” the entire contents of which are hereby incorporated by reference herein. Technical Field
[0003] The disclosure relates to a catalyst support material for synthesizing ammonia (NH3) from nitrogen (N2) and hydrogen (H2). More specifically, the disclosure relates to a catalyst support material comprising (MgO) x (BaO) y (Al2O3) z and / or (MgO) x (SrO) y (Al2O3) z A support material on which an ammonia synthesis catalyst, such as ruthenium, may be dispersed. Background Art
[0004] It is well known that climate change driven by anthropogenic emissions of carbon dioxide (CO2) poses a threat to continued economic development and security. To mitigate this threat, both developed and developing countries are seeking energy sources that emit substantially no CO2. Although several CO2-free power generation options (e.g., wind, solar, hydroelectric, and nuclear) have been widely developed, there are few economic options for CO2-free energy sources.
[0005] Ammonia (NH3) can be burned as a fuel according to the following reaction equation (1):
[0006] 4NH3+3O2→2N2+6H2O+heat (1)
[0007] Ammonia can also be catalytically reformed to regenerate H2 and N2 reactants according to the following reaction equation (2):
[0008] 2NH3→3H2+N2 (2)
[0009] Therefore, NH3 can be used as a CO2-free fuel and / or as a hydrogen storage medium. However, almost all current NH3 production processes utilize raw materials and energy sources that generate CO2.
[0010] Previous efforts at sustainable fuel production have focused on biofuels, H2, and "artificial photosynthesis." Although ethanol and biodiesel have higher energy density than NH3, using food resources for fuel production leads to higher food prices because it shifts the allocation of farmland from food to fuel, while increasing the price of crops used for fuel production. This reallocation can lead to political instability in developing countries due to higher food prices.
[0011] Although NH3 can be considered a solution to the H2 storage density problem, hydrogen has not yet overcome its storage density challenges. NH3 has approximately twice the energy density of liquid hydrogen, but at pressures and temperatures that are easily and economically achieved (e.g., about 9 atm at about 25°C, about 1 atm at about -33°C).
[0012] Although "artificial photosynthesis" can form a closed-loop fuel cycle, CO2 must be extracted from the air to achieve it. Because nitrogen (79%) is much more abundant in the atmosphere than CO2 (0.04%), using NH3 is a more viable approach for this type of process because less air must be processed to produce the same amount of fuel. For example, for every unit of air required to produce one mole of NH3, 3,550 units of air must be processed to synthesize one mole of methane (CH4) from atmospheric CO2. In addition, commercial air separators for atmospheric N2 extraction already exist and are well known, while extracting CO2 from air is still a developing technology.
[0013] The main industrial process for producing ammonia is the Haber-Bosch process, shown in the following reaction equation (3):
[0014] N2(g)+3H2(g)→2NH3(g) (ΔH=-92.2 kJ / mol) (3)
[0015] The Haber-Bosch process requires about 31.4 gigajoules of energy per year worldwide, and as of 2017, produces about 3 tons of CO2 for every ton of NH3 produced. About two-thirds of the CO2 emissions from NH3 synthesis originate from hydrocarbon steam reforming to produce hydrogen, while the remaining one-third originates from fuel combustion to provide energy to the synthesis plant. As of 2012, about 50% of Haber-Bosch NH3 plants use natural gas as feed and fuel, while the remaining plants use coal or oil. Thus, Haber-Bosch NH3 synthesis consumes about 3% to about 5% of global natural gas production and about 1% to about 2% of global energy production. Therefore, it is desirable to provide improvements to the process for synthesizing ammonia to reduce CO2 emissions.
[0016] The Haber-Bosch reaction is usually carried out in a reactor containing an iron oxide or ruthenium catalyst at a temperature of about 300°C to about 550°C and at a pressure of about 90 bar to about 180 bar. An elevated temperature is required to achieve a reasonable reaction rate. However, as the reaction temperature increases, the reaction equilibrium becomes less favorable for the reaction product (NH3), so an elevated pressure is used to "push" the reaction according to the Le Chatelier principle. In addition, the increase in reaction pressure increases the reaction rate (that is, the rate is a function of the reactant pressure). Due to the increased power requirements of the compressor and the increased cost of equipment that can withstand high pressure, the pressurization of H2 and N2 gases is energy and economically expensive, so it is desirable to improve the catalyst activity to provide similar or better reaction rates at lower temperatures and pressures.
[0017] NH3 catalyst activity can be improved by applying the catalyst to the surface of certain carrier materials. There are at least three advantages to dispersing the catalyst on the surface of the carrier material. First, the high dispersion deposition of catalyst particles on the carrier (i.e., the particle deposition maximizes the ratio of exposed surface area to particle volume) allows more efficient use of the catalyst. Second, the carrier can supply and / or consume valence electrons from the catalyst, thereby reducing the energy barrier of adsorption, desorption or reaction of reactants or surface intermediates. Third, the carrier can provide a co-catalytic function, wherein the intermediate reaction occurs simultaneously on both the catalyst and the carrier with a reduced activation barrier (e.g., when the carrier is bound to the intermediate material, the catalyst is allowed to remove atoms (e.g., H) from the reactants).
[0018] Support materials that have been mentioned in the literature for use with NH3 catalysts include activated carbon, alumina, Al2O3, CaO, calcium amide (Ca(NH2)2), and calcium aluminum electron compounds (represented by cement chemical symbols as C12A7:e-). U.S. Patent Application Publication Nos. 2017 / 0253492 and 2020 / 0197911 also describe the use of various catalyst supports, including calcium aluminate materials such as CA, C5A3, C3A, and C (cement chemical symbols, C=CaO, A=Al2O3), both in electrically insulating and conductive forms. The entire contents of these applications are incorporated herein by reference.
[0019] In order to further facilitate the efficient production of NH3 using the above-described methods, it is highly desirable to develop improved catalysts, including improved catalyst supports. Summary of the invention
[0020] This summary is provided to introduce in simplified form a selection of concepts that will be further described below in the detailed description. This summary and the foregoing background technology are not intended to identify key aspects or essential aspects of the claimed subject matter. In addition, this summary is not intended to be used to help determine the scope of the claimed subject matter.
[0021] In some embodiments, a catalyst support material suitable for use, for example, in the synthesis of ammonia from H2 and N2 comprises (MgO) x (BaO) y (Al2O3) z , wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.5. The support material may include a material having the formula (MgO) x (BaO) y (Al2O3) z wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.5, or may include two or more materials, when their composition contents are averaged, the composition of the two or more materials has the chemical formula (MgO) x (BaO) y (Al2O3) z , wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.5. The ammonia synthesis catalyst may be dispersed on a catalyst support material. The ammonia synthesis catalyst may be, but is not limited to, ruthenium.
[0022] In some embodiments, a catalyst support material suitable for use, for example, in the synthesis of ammonia from H2 and N2 includes (MgO) x (SrO) y (Al2O3) z , wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.05 to about 0.3. The support material may include a material having the formula (MgO) x (SrO) y (Al2O3) z wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.1 to about 0.3, or may include two or more materials, when their composition contents are averaged, the composition of the two or more materials has the chemical formula (MgO) x (SrO) y (Al2O3) z, wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.05 to about 0.3. The ammonia synthesis catalyst may be dispersed on a catalyst support material. The ammonia synthesis catalyst may be, but is not limited to, ruthenium.
[0023] In some embodiments, a method for synthesizing NH3 from a mixture of N2 and H2 includes at least the step of exposing the mixture of N2 and H2 to a catalyst dispersed on a support material, the support material comprising: (MgO) x (BaO) y (Al2O3) z , wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.5; or (MgO) x (SrO) y (Al2O3) z , wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.05 to about 0.3. The support material may have one of the foregoing formulas by using a material having the foregoing formula, or by using two or more materials that provide a composition having the foregoing formula on average. The catalyst dispersed on the support material may be an ammonia synthesis catalyst such as, but not limited to, ruthenium.
[0024] These and other aspects of the technology described herein will be apparent after considering the detailed description and accompanying drawings herein. However, it should be understood that the scope of the subject matter claimed should be determined by the issued claims, rather than by whether a given subject matter solves any or all of the problems mentioned in the background technology or includes any features or aspects stated in the summary of the invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Non-limiting and non-exhaustive embodiments of the disclosed technology, including preferred embodiments, are described with reference to the following figures, wherein like reference numerals refer to like parts throughout the various views unless otherwise specified.
[0026] Figure 1 For (MgO) x (BaO) y (Al2O3) z ternary diagram showing that when (MgO) is used according to various embodiments described herein x (BaO) y (Al2O3) z As a support material for ammonia synthesis catalyst (MgO) x (BaO) y (Al2O3) z to achieve improved ammonia synthesis.
[0027] Figure 2 For (MgO) x (SrO) y (Al2O3) z ternary diagram showing that when (MgO) is used according to various embodiments described herein x (SrO) y (Al2O3) z As a support material for ammonia synthesis catalyst (MgO) x (SrO) y (Al2O3) z to achieve improved ammonia synthesis. DETAILED DESCRIPTION
[0028] Embodiments are described more fully below with reference to the accompanying drawings, which form a part of the embodiments and show specific exemplary embodiments in an illustrative manner. These embodiments are disclosed in full detail to enable those skilled in the art to practice the present invention. However, the embodiments can be realized in many different forms and should not be construed as being limited to the embodiments set forth herein. Therefore, the following detailed description should not be construed as restrictive.
[0029] The disclosure describes various embodiments of catalyst support materials, and in some specific embodiments, supports for use with ammonia synthesis catalysts are described. For example, the ammonia synthesis catalyst may be dispersed on the support material described herein. Any suitable method may be used to form the support material described herein. Similarly, any suitable method may be used to disperse the ammonia synthesis catalyst on the support material. Exemplary but non-limiting methods for forming the support material described herein and for dispersing the catalyst on the support material described herein are described in more detail in U.S. Patent Application Publication No. 2020 / 0197911, the entire contents of which are hereby incorporated by reference herein.
[0030] In short, without being understood in a limiting sense, the method for forming a support material as described in U.S. Patent Application Publication No. 2020 / 0197911 that can be used with the technology disclosed herein generally includes mixing the contributor materials of each component in the support material together and calcining the mixture so that the oxide form of the component included in the support material is made by the contributor material. The term "contributor" as used herein means a compound that includes a component of the final support material and is used to produce an oxide form of the component as part of the process of forming the support material. In some embodiments, the components of the support material are Mg, Ba and Al, while in other embodiments, the components of the support material are Mg, Sr and Al. Therefore, the contributors used in the method described herein will include Mg contributors, Sr contributors and Al contributors, or Mg contributors, Ba contributors and Al contributors, so that the oxide forms of these components (e.g., MgO, BaO, SrO, Al2O3) can be made from the contributor material via calcination. Any contributor material suitable for producing these oxide forms via annealing can be used. Exemplary but non-limiting contributors suitable for forming the support material described herein include:
[0031] For MgO: magnesium (metal), magnesium oxide, magnesium hydroxide, basic magnesium carbonate, magnesium acetate, magnesium carbonate, magnesium nitrate, methyl magnesium carbonate, and magnesium acetylacetonate.
[0032] For BaO: barium (metal), barium carbonate, barium acetate, barium nitrate, barium oxide, barium isopropoxide, barium hydroxide, barium peroxide, barium 2-ethylhexanoate, and barium acetylacetonate.
[0033] For SrO: strontium (metal), strontium nitrate, strontium hydroxide, strontium isopropoxide, strontium acetate, strontium oxide, strontium aluminate, strontium carbonate, strontium tetramethylheptanedionate, strontium nitride, and strontium acetylacetonate.
[0034] For Al2O3: aluminum (metal), aluminum oxide, aluminum nitrate, aluminum hydroxide, aluminum acetylacetonate, and aluminum acetate.
[0035] Regardless of the specific manner in which the contributor materials are mixed and calcined (including any additional steps performed as part of preparing the mixture to be calcined), the support material formed by the calcining step can be in any form, such as in a powder or agglomerate form. Additional steps can be performed to change the form of the support material, such as mixing the powder or agglomerate form with any combination of binders, lubricants and / or pore formers, and forming the material into, for example, pellets, extrudates, monoliths, screens, honeycombs, or sheets.
[0036] As also discussed in more detail in U.S. Patent Application Publication No. 2020 / 0197911, when mixed, the form of the contributor material is generally not limited. In some embodiments, the contributor material is provided in powder form, which can then be mixed together to form a powder mixture. The powder mixture can be directly calcined, or additional steps can be implemented to change the form of the mixture before calcining. For example, a solvent can be added to the mixture of the contributor material to form a paste or slurry, which can then be calcined. Alternatively, the paste or slurry can then be dried to form a dry mixture, which can then be calcined. As part of the process of forming the support material, the contributor material in powder form or a mixture thereof can also be crushed and / or ball-milled to reduce the particle size of the powder material (e.g., before calcining).
[0037] The amount of each contributor used in preparing the mixture to be annealed as part of forming the support material is generally determined by the desired composition of the support material to be produced. The various contributors can be combined in different molar ratios to produce different stoichiometric support materials. Further discussion of the desired stoichiometric ratios of support materials of the present technology is provided below.
[0038] Additional aspects of the method for producing the support material (including but not limited to the temperature range for calcination, the holding / soaking time during calcination, the rate at which the temperature is increased to the calcination temperature, the rate at which the temperature is reduced when calcination is completed, the generation of conductive materials, etc.) are further described in detail in U.S. Patent Application Publication No. 2020 / 0197911 and can be used in the method for preparing the support material described herein.
[0039] Once produced, the catalyst material (such as an ammonia synthesis catalyst material) can be dispersed on the support material. In short, without being construed in a limiting sense, methods for dispersing the catalyst on the support material as described in U.S. Patent Application Publication No. 202 / 0197911 that can be used with the technology disclosed herein include incipient wetness impregnation techniques, ball milling, ion exchange, and wet impregnation. Other methods that can be used include nanoparticle dispersion, nanoparticle ligand exchange, chemical vapor deposition, and physical vapor deposition.
[0040] Having briefly described methods suitable for forming the support materials described herein, the desired composition of the support materials can now be described. In some embodiments, the support material comprises (MgO) x (BaO) y (Al2O3) z or (MgO) x (SrO) y (Al2O3) zFor each material, it has been found that when a support material having an ammonia synthesis catalyst (such as ruthenium) dispersed thereon is used, the ammonia synthesis rate is beneficially increased, provided that the values of x, y and z are within the specified ranges. x (BaO) y (Al2O3) z or (MgO) x (SrO) y (Al2O3) z The ammonia synthesis rate is increased compared to a support material wherein the values of x, y and / or z fall outside the specified range and the ammonia synthesis catalyst is dispersed thereon. In some embodiments, when the support material is (MgO) x (BaO) y (Al2O3) z , when the value of x is in the range of about 0.05 to about 0.7, the value of y is in the range of about 0.05 to about 0.6, and the value of z is in the range of about 0.3 to about 0.5, the ammonia synthesis rate is improved. In some embodiments, when the support material is (MgO) x (SrO) y (Al2O3) z When the value of x is in the range of about 0.4 to about 0.7, the value of y is in the range of about 0.05 to about 0.5, and the value of z is in the range of about 0.05 to about 0.3, the ammonia synthesis rate is improved.
[0041] The values of x, y, and z provided above are stoichiometric values. It should be understood that the values of x, y, and z can be multiplied or divided by any common value and still fall within the scope of the technology described in the present invention. The values of x, y, and z provided herein represent simplified values of x, y, and z. Therefore, including (MgO) 2.1 (BaO) 0.15 (Al2O3) 0.9 The support materials can be simplified by a common factor of 3 to give (MgO) 0.7 (BaO) 0.05 (Al2O3) 0.3 , and both compositions are considered to fall within the scope of the technology described in the present invention.
[0042] In some embodiments, the support materials described herein include materials having the following chemical formula: (MgO) x (BaO) y (Al2O3) z , wherein the value of x is in the range of about 0.05 to about 0.7, the value of y is in the range of about 0.05 to about 0.6, and the value of z is in the range of about 0.3 to about 0.5; or (MgO) x (SrO)y (Al2O3) z , wherein the value of x is in the range of about 0.4 to about 0.7, the value of y is in the range of about 0.05 to about 0.5, and the value of z is in the range of about 0.05 to about 0.3. In other embodiments, the support material comprises a composition of two or more materials that averages to an overall support material having the following chemical formula: (MgO) x (BaO) y (Al2O3) z , wherein the value of x is in the range of about 0.05 to about 0.7, the value of y is in the range of about 0.05 to about 0.6, and the value of z is in the range of about 0.3 to about 0.5; or (MgO) x (SrO) y (Al2O3) z , wherein the value of x is in the range of about 0.4 to about 0.7, the value of y is in the range of about 0.05 to about 0.5, and the value of z is in the range of about 0.05 to about 0.3. In such embodiments, the composition may be composed of a compound that does not have the chemical formula (MgO) itself. x (BaO) y (Al2O3) z or (MgO) x (SrO) y (Al2O3) z and / or having the chemical formula (MgO) x (BaO) y (Al2O3) z or (MgO) x (SrO) y (Al2O3) z However, when the sum of the atomic contents of the two or more materials is averaged, the composition comprising the two or more materials has the chemical formula (MgO) x (BaO) y (Al2O3) z or (MgO) x (SrO)y(Al2O3) z , wherein the values of x, y and z fall within the aforementioned ranges. The materials used in such bulk compositions may have crystalline or amorphous forms, and thus the bulk composition may include a mixture of amorphous and crystalline materials.
[0043] In having an average to provide a chemical formula (MgO) x (BaO) y (Al2O3) zIn one non-limiting example of a bulk composition of two or more materials having a composition of (wherein the value of x is in the range of about 0.05 to about 0.7, the value of y is in the range of about 0.05 to about 0.6, and the value of z is in the range of about 0.3 to about 0.5), the composition of the structural material may have equal amounts of a chemical formula (MgO) 0.3 (BaO) 0.2 (Al2O3) 0.6 The first material has the chemical formula (MgO) 0.2 (BaO) 0.6 (Al2O3) 0.2 Although each material does not have the aforementioned chemical formula individually (because the value of z in the first material and the second material is outside the range of 0.3 to 0.5), the average value of each of the MgO, BaO and Al2O3 components provides a bulk having the chemical formula (MgO) 0.25 (BaO) 0.4 (Al2O3) 0.4 The final composition of the present invention represents a material having the aforementioned chemical formula.
[0044] Reference now Figure 1 and Figure 2 , showing the (MgO) x (BaO) y (Al2O3) z and (MgO) x (SrO) y (Al2O3) z The preferred composition range of each of the ternary diagrams can be read using any of the grid method, height method or intersection method as known to those skilled in the art. Figure 1 and Figure 2 In general, for each ternary graph, the side of the triangle opposite the vertex indicates where no compound labeled at the vertex is provided, and the amount of the compound labeled at the vertex increases as the vertex is approached from the side opposite the vertex. Thus, for example, a data point close to a vertex on the ternary graph indicates a material with a relatively high amount of the compound labeled at the vertex.
[0045] Figure 1 and Figure 2 The areas shown generally in medium gray and bounded by dashed lines on each of the ternary diagrams indicate compositions of the support material that have increased ammonia synthesis rates when an ammonia synthesis catalyst (such as ruthenium) is dispersed on the support material (at least compared to compositions falling outside of the medium gray area shown in the ternary diagram).
[0046] First reference Figure 1 , showing the chemical formula (MgO) x (BaO)y (Al2O3) z Ternary diagram 100 of a support material, wherein region 101 represents other (MgO) than those shown on ternary diagram 100 but falling outside region 101. x (BaO) y (Al2O3) z Support material composition with improved ammonia synthesis compared to (MgO) x (BaO) y (Al2O3) z Composition of the support material. (MgO) x (BaO) y (Al2O3) z The preferred compositions of the support material generally fall within region 101, wherein in some embodiments, a linear plot line 102 extending through the middle of region 101 represents the most preferred composition. In some embodiments, linear plot line 102 is at plot point (MgO) on ternary diagram 100. 0.65 (BaO) 0.05 (Al2O3) 0.35 (exist Figure 1 Marked as 102-1) and (MgO) 0.05 (BaO) 0.55 (Al2O3) 0.40 (exist Figure 1 Other points that fall approximately on the plot line 102 include, but are not limited to, (MgO) 0.5 (BaO) 0.2 (Al2O3) 0.35 、(MgO) 0.25 (BaO) 0.4 (Al2O3) 0.37 , and (MgO) 0.15 (BaO) 0.5 (Al2O3) 0.4 However, as previously described, plot points near linear plot line 102 (e.g., at least within region 101) also provide preferred (MgO) x (BaO) y (Al2O3) z Composition of Support Material. Support material compositions that are adjacent to, but not directly on, the linear plot line 102 between points 102-1 and 102-2 should still be considered to fall within the scope of the presently described technology.
[0047] Next reference Figure 2 , showing the chemical formula (MgO) x (SrO) y (Al2O3) zTernary diagram 200 of a support material, wherein region 201 represents other (MgO) than those shown on ternary diagram 200 but falling outside region 201. x (SrO) y (Al2O3) z Support material composition with improved ammonia synthesis compared to (MgO) x (SrO) y (Al2O3) z Composition of the support material. (MgO) x (SrO) y (Al2O3) z The preferred composition of the support material falls generally within region 201, wherein in some embodiments, a linear plot line 202 extending through the middle of region 201 represents the most preferred composition. In some embodiments, linear plot line 202 is at plot point (MgO) on ternary diagram 200. 0.5 (SrO) 0.5 (Al2O3) 0.05 (exist Figure 2 Marked as 202-1) and (MgO) 0.7 (SrO) 0.05 (Al2O3) 0.3 (exist Figure 2 Other points that fall approximately on the plot line 102 include, but are not limited to, (MgO) 0.62 (SrO) 0.12 (Al2O3) 0.24 、(MgO) 0.6 (SrO) 0.3 (Al2O3) 0.13 , and (MgO) 0.58 (SrO) 0.37 (Al2O3) 0.08 However, as previously described, plot points near linear plot line 202 (e.g., at least within region 201) also provide preferred (MgO) x (SrO) y (Al2O3) z Composition of the support material. Support material compositions adjacent to, but not directly on, the linear plot line 202 between points 202-1 and 202-2 should still be considered to fall within the scope of the technology described herein. In some embodiments, a preferred support material has a composition between the plot points (MgO) and 0.6 (SrO) 0.4 (Al2O3) 0.15 Chemical formula at or near .
[0048] Once a support material having a composition as described above is formed, an ammonia synthesis catalyst can be dispersed on the support material. Any suitable catalyst known to promote the formation of ammonia from N2 and H2 or other reactants can be used. In some embodiments, the ammonia synthesis catalyst is at least one transition metal selected from Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Mo, Ru, Rh, Pd or Os. When the catalyst is dispersed on the support material, any combination of ammonia synthesis catalysts can be used.
[0049] In some embodiments, the amount of the catalyst dispersed on the support material is in the range of about 0.01 wt % to about 50 wt %, such as about 0.1 wt % to about 20 wt %, about 0.1 wt % to about 10 wt %, or about 1 wt %. Any suitable method can be used to implement the dispersion of the catalyst on the support material, including but not limited to in a manner similar to or identical to the method described in U.S. Patent Application Publication No. 2020 / 0197911. When following the method described in U.S. Patent Application Publication No. 2020 / 0197911, the dispersion is generally implemented by the following operations: (a) stirring the support material powder in a metal salt + acetone solution to disperse the salt of the desired metal on its surface; and (b) reducing the resulting material in a hydrogen-containing atmosphere to convert the catalyst metal salt into a catalyst metal. Non-limiting examples of suitable metal salts are RuCl3 hydrates for Ru dispersion and CoCl2 hexahydrates for Co dispersion. A variety of catalysts can be added to the support by using a solution containing a variety of catalyst salts, by continuous deposition and reduction of the catalyst metal, or by a combination of these two methods.
[0050] In some embodiments, the catalyst in oxide form can be formed by performing a calcination step in a non-reducing environment. For example, a Co / support material catalyst can be converted to a Co oxide / support material catalyst by calcining the Co / support material in an oxygen-containing atmosphere.
[0051] The support material composition with the catalyst dispersed thereon so formed can be formed into a catalyst bed by any method described in U.S. Patent Application Publication No. 2020 / 0197911 or by any other suitable method. The method described in U.S. Patent Application Publication No. 2020 / 0197911 includes, for example, using a material in powder form, extruding it (e.g., pellets), pressing it into pellets, or bonding it to a structural support. It has been found that a metal monolith with a thin layer of catalyst bonded to its surface is particularly beneficial for NH3 synthesis due to its high thermal conductivity and high catalyst utilization.
[0052] In an exemplary catalyst synthesis method, a catalyst bed or monolith is heated to 200° C. to 650° C. and a N2+H2 gas mixture is directed through the catalyst bed or monolith. The gas pressure may be in the range of 0.1 bar to 500 bar absolute pressure. The reactant input stream may be preheated before it is directed into the catalyst bed. When the N2+H2 gas mixture flows over the heated catalyst bed, a portion of it is converted into NH3. The concentration of NH3 in the product gas may vary according to temperature, pressure, gas velocity, and gas / catalyst contact time.
[0053] The thermodynamic equilibrium concentration of NH in the product stream can be increased by reducing the catalyst bed temperature, increasing the reactant pressure, or both. NH synthesis is an exothermic process, so when synthesizing NH, the temperature of the catalyst and reactant gases increases. This can be particularly important at high operating pressures because a heat removal mechanism may be required to prevent the reactor from overheating.
[0054] For a given catalyst bed volume, temperature and pressure, the proportion of incoming N2+H2 converted to NH3 can be made closer to the thermodynamic equilibrium value by reducing the NH3 flow rate to increase the residence time in the catalyst bed.
[0055] It will be appreciated from the foregoing that specific embodiments of the invention have been described herein for purposes of illustration, but that various modifications may be made without departing from the scope of the invention. Accordingly, the invention is not to be limited except as by the appended claims.
[0056] Although the present technology has been described in language specific to certain structures and materials, it should be understood that the invention defined in the appended claims is not necessarily limited to the specific structures and materials described. Instead, these specific aspects are described as forms of implementing the claimed invention. Because many embodiments of the present invention can be practiced without departing from the spirit and scope of the present invention, the present invention is subject to the following claims.
[0057] Unless otherwise stated, all numbers or expressions (such as those expressing dimensions, physical properties, etc.) used in the specification (except claims) should be understood to be modified by the term "approximately" in all cases. At the very least, without attempting to limit the application of the doctrine of equivalents to the claims, each numerical parameter modified by the term "approximately" described in the specification or claims should be interpreted at least in view of the digits of the significant digits described and by applying rounding techniques. In addition, all ranges disclosed herein should be understood to cover and provide support for claims to any and all sub-ranges or any and all single values contained therein. For example, the stated range of 1 to 10 should be considered to include and provide support for claims to any and all sub-ranges or single values between and including a minimum value of 1 and a maximum value of 10 (i.e., all sub-ranges starting with a minimum value of 1 or greater and ending with a maximum value of 10 or less (e.g., 5.5 to 10, 2.34 to 3.56, etc.) or any value from 1 to 10 (e.g., 3, 5.8, 9.9994, etc.)).
Claims
1. A catalyst support material having a chemical formula (MgO) x (BaO) y (Al2O3) z , wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.
5.
2. The catalyst support material according to claim 1, wherein (MgO) x (BaO) y (Al2O3) z The values of x, y and z are taken from the ternary diagram for MgO, BaO and Al2O3 at point (MgO) 0.65 (BaO) 0.05 (Al2O3) 0.35 With (MgO) 0.05 (BaO) 0.55 (Al2O3) 0.4 A linear plot line extending between or near data points.
3. The catalyst support material according to claim 1, wherein an ammonia synthesis catalyst is dispersed on the catalyst support material.
4. The catalyst support material of claim 3, wherein the ammonia synthesis catalyst comprises ruthenium.
5. The catalyst support material according to claim 3, wherein the ammonia synthesis catalyst comprises at least one of Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Mo, Ru, Rh, Pd or Os.
6. The catalyst support material of claim 3, wherein the amount of ammonia synthesis catalyst dispersed on the catalyst support material is from about 0.5 wt% to about 20 wt% of the combination of the catalyst support material and the ammonia synthesis catalyst dispersed thereon.
7. The catalyst support material of claim 1, wherein the catalyst support material comprises two or more materials, and the average composition content of the two or more materials provides a catalyst having the chemical formula (MgO): x (BaO) y (Al2O3) z A material wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.
5.
8. A catalyst support material comprising (MgO) x (SrO) y (Al2O3) z , wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.05 to about 0.
3.
9. The catalyst support material according to claim 8, wherein (MgO) x (SrO) y (Al2O3) z MgO 0.6 (SrO) 0.4 (Al2O3) 0.15 .
10. The catalyst support material according to claim 8, wherein (MgO) x (SrO) y (Al2O3) z The values of x, y and z are taken from the ternary diagram for MgO, SrO and Al2O3 at point (MgO) 0.5 (SrO) 0.5 (Al2O3) 0.05 With (MgO) 0.7 (SrO) 0.05 (Al2O3) 0.3 A linear plot line extending between or near data points.
11. The catalyst support material according to claim 8, wherein an ammonia synthesis catalyst is dispersed on the catalyst support material.
12. The catalyst support material of claim 11, wherein the ammonia synthesis catalyst comprises ruthenium.
13. The catalyst support material of claim 11, wherein the ammonia synthesis catalyst comprises at least one of Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Mo, Ru, Rh, Pd or Os.
14. The catalyst support material of claim 11, wherein the amount of ammonia synthesis catalyst dispersed on the catalyst support material is from about 0.5 wt% to about 20 wt% of the combination of the catalyst support material and the ammonia synthesis catalyst dispersed thereon.
15. A method for synthesizing NH3 from a mixture of N2 and H2, comprising: The mixture of N2 and H2 is exposed to a catalyst support material having dispersed thereon an ammonia synthesis catalyst, the support material comprising: (MgO) x (BaO) y (Al2O3) z , wherein x is from about 0.05 to about 0.7, y is from about 0.05 to about 0.6, and z is from about 0.3 to about 0.5; or (MgO) x (SrO) y (Al2O3) z , wherein x is from about 0.4 to about 0.7, y is from about 0.05 to about 0.5, and z is from about 0.05 to about 0.
3.
16. The method according to claim 15, wherein when the support material is (MgO) x (BaO) y (Al2O3) z When (MgO) x (BaO) y (Al2O3) z The values of x, y and z are taken from the ternary diagram for MgO, BaO and Al2O3 at point (MgO) 0.65 (BaO) 0.05 (Al2O3) 0.35 With (MgO) 0.05 (BaO) 0.55 (Al2O3) 0.4 The linear plot line extending between or near the data points, and when the support material is (MgO) x (SrO) y (Al2O3) z When (MgO) x (SrO) y (Al2O3) z The values of x, y and z are taken from the ternary diagram for MgO, SrO and Al2O3 at point (MgO) 0.5 (SrO) 0.5 (Al2O3) 0.05 With (MgO) 0.7 (SrO) 0.05 (Al2O3) 0.3 A linear plot line extending between or near data points.
17. The method of claim 15, wherein the ammonia synthesis catalyst comprises ruthenium.
18. The method of claim 15, wherein the ammonia synthesis catalyst comprises at least one of Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Mo, Ru, Rh, Pd, or Os.
19. The method of claim 15, wherein the amount of ammonia synthesis catalyst dispersed on the catalyst support material is from about 0.5 wt% to about 20 wt% of the combination of the catalyst support material and the ammonia synthesis catalyst dispersed thereon.
20. The method of claim 19, wherein the amount of ammonia synthesis catalyst dispersed on the catalyst support material is about 1.0 weight percent of the combination of the catalyst support material and the ammonia synthesis catalyst disposed thereon.