3D printing artificial meat ink based on edible mushroom protein and preparation method of 3D printing artificial meat

By developing 3D printed artificial meat ink based on edible fungi protein, combining polysaccharides and thickeners, the rheological characteristics and printing parameters are optimized, and the problem of insufficient application of edible fungi protein in the field of artificial meat is solved, and efficient and low-cost consumption is achieved The production of artificial meat in bacterial protein meets consumers' taste and nutrition needs and reduces the pressure on animal husbandry.

CN118947811APending Publication Date: 2024-11-15ZHEJIANG UNIV OF TECH

Patent Information

Application Number
CN202410438832.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-04-12
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing artificial meat industry has challenges in raw material selection and production costs, especially the application of edible fungi protein is relatively limited, and the existing technology is difficult to meet consumers' taste and odor needs for artificial meat, and there is also the problem of low resource utilization efficiency. .

Method used

Using 3D printed artificial meat ink based on edible fungi proteins, edible fungi proteins such as yeast mushrooms and erectus mushrooms as raw materials, combined with polysaccharides and thickeners, the rheological characteristics and printing parameters are optimized, and good rheological characteristics and printing parameters are developed. 3D printed artificial meat ink with nutritional value, and 3D printing technology prepares foods with full meat.

Benefits of technology

The development of 3D printed artificial meat ink based on edible fungi protein has been achieved, which has improved production efficiency, reduced costs, met consumers' needs for taste and nutrition, and at the same time reduced the pressure on traditional animal husbandry, providing a more acceptable Sustained source of protein.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118947811A_ABST
    Figure CN118947811A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of 3D printing artificial meat, and discloses 3D printing artificial meat ink based on edible mushroom protein and a preparation method of the 3D printing artificial meat, and the 3D printing artificial meat ink comprises the following raw material components in parts by mass: 7 parts of soybean protein isolate, 2-3 parts of edible mushroom protein fiber powder, 0.5-0.8 part of a thickening agent, 1-2 parts of soy sauce and 1-2 parts of essence. 8-10 parts of water; and pigment. The edible mushroom protein fiber powder and the soybean protein isolate interact to prepare the printing ink, printability is structurally improved, the edible mushroom protein fiber powder and the soybean protein isolate cooperate with each other, food stability is improved through thickening and gelation behaviors of the two macromolecules, the proportion of the natural raw materials is adjusted, the fishy smell is weakened and eliminated, the best sensory flavor is achieved, and the edible mushroom protein fiber powder and the soybean protein isolate interact with each other to prepare the printing ink. The finished product of the 3D printing artificial meat based on the edible mushroom protein, which has nutritional and functional characteristics, is developed and obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the technical field of 3D printed artificial meat, and in particular to a 3D printed artificial meat ink based on edible fungus protein and a method for preparing 3D printed artificial meat. Background Technology

[0002] With rapid population growth and high-quality economic development, the consumption of meat products, a crucial source of protein and other nutrients for humans, is rapidly increasing globally. The surge in greenhouse gas emissions, increased arable land occupation, and exacerbated water pollution caused by meat production pose significant challenges and severe impacts on traditional animal husbandry. The process of raising animals and producing meat is often accompanied by problems such as low protein conversion efficiency, leading to underutilization of resources and substantial losses through the food chain. To meet the growing human demand for meat products, address potential food crises, and reduce the pressure on the Earth's ecology, environment, climate, and energy from meat production, "cultured meat" products have emerged and are expected to become a major trend in future food development.

[0003] The long-term intake of high-calorie foods has made obesity a modern disease. Edible fungi protein, as a high-quality protein source, can be used as a fat substitute, reducing fat intake and promoting balanced nutrition. This aligns with the future food concept that better meets human nutritional and health needs, and also better satisfies the dietary habits of the large existing vegetarian population. Edible fungi have short growth cycles and low land utilization, facilitating large-scale cultivation. While meeting the nutritional needs of a growing population, they can alleviate the problem of land resource scarcity to some extent. Furthermore, edible fungi such as king oyster mushrooms, lion's mane mushrooms, and oyster mushrooms have high-quality protein with a complete range of amino acids. Edible fungi protein isolate is comparable in nutritional value to meat protein, effectively meeting human nutritional requirements.

[0004] Most major global companies in the cultured meat industry initially chose plant-based raw materials, followed by cell-based materials. However, both have long cultivation cycles, making it difficult to obtain raw materials in large quantities. In my country, microbial protein is currently mainly used in animal feed production, with relatively limited applications in the food sector. Later, processes using a certain proportion of enoki mushrooms and white jade mushrooms to prepare meat patties have gradually emerged, but research remains largely unexplored, related technologies are immature, and current production costs are high, hindering large-scale production while maximizing cost and energy savings. Furthermore, from a sensory perspective, the taste and aroma of cultured meat need further improvement to meet consumer demands and maximize energy value. Summary of the Invention

[0005] In view of the limited research on microbial protein-based artificial meat, this invention provides a 3D printing artificial meat ink based on edible fungi protein and a method for preparing 3D printed artificial meat. The 3D printing artificial meat ink has good rheological properties and also has nutritional and functional properties.

[0006] The objective of this invention is achieved through the following technical solution: In a first aspect, the present invention provides a 3D printing artificial meat ink based on edible fungus protein, comprising the following raw material components by mass: 7 parts soy protein isolate, 2-3 parts edible fungus protein fiber powder, 0.5-0.8 parts thickener, 1-2 parts soy sauce, 1-2 parts flavoring, 8-10 parts water and pigment.

[0007] To alleviate pressure on the livestock industry, prevent potential food crises, improve production efficiency, and reduce waste, this invention uses edible fungi such as king oyster mushrooms, lion's mane mushrooms, and oyster mushrooms as high-quality proteins. While providing abundant essential amino acids, it can reduce fat intake, balance nutrition, and meet the future food concept of human nutrition and health needs. It can also better meet the dietary habits of some existing vegetarians.

[0008] The adhesive properties and rheological properties of 3D printing inks are important indicators of the success of developing bacterial protein-based artificial meat. The degree to which the texture closely resembles meat is another crucial indicator, directly impacting consumer purchasing decisions. This invention uses edible fungi with plump flesh and high protein content as raw materials, employing polysaccharides and thickeners to interact and link them. The thickening and gelling behaviors of these two macromolecules improve the stability of the food. Furthermore, by analyzing the relationship between rheology and printability, the invention explores the formulation parameters of 3D printing inks to further optimize their rheological properties.

[0009] Because edible fungus protein fiber powder has a higher water absorption rate than soybean protein powder, the ratio needs to be further adjusted in conjunction with moisture to achieve the best printing rheology. Therefore, the proportion of edible fungus protein fiber powder should not be too high to prevent problems such as difficulty in printing and loading (too dry and solid) or poor printing extrusion (small printing nozzle diameter, ink solidification easily clogs the nozzle).

[0010] Ultimately, this invention developed a 3D printing ink based on edible fungus protein that can be applied to the preparation of artificial meat. It has good rheological properties and is both nutritious and functional, and can leverage the two major advantages of 3D printing technology in the food industry: precise formulation and the ability to change the shape of food.

[0011] Preferably, the pigments include 0.5-1 parts of red yeast rice pigment and 0.3-0.5 parts of caramel pigment.

[0012] The addition of pigments can be further adjusted according to the color requirements of the target product.

[0013] Preferably, the thickener is carrageenan, konjac gum, or sodium alginate.

[0014] Preferably, the flavoring is a meat flavoring.

[0015] Preferably, the edible fungus protein fiber powder is made by drying and pulverizing commercially available fresh dried fungi.

[0016] This method can produce edible fungi protein powder that retains dietary fiber.

[0017] Preferably, the drying is performed under vacuum at 60-70°C for 5-10 minutes; the pulverization is performed by pulverizing and sieving to 100 mesh.

[0018] Preferably, the dried mushroom products are one or more of the following: dried king oyster mushrooms, dried lion's mane mushrooms, and dried oyster mushrooms; the dried mushroom products are 80-90% dry.

[0019] Secondly, the present invention also provides a method for preparing 3D-printed artificial meat based on edible fungus protein, comprising the following steps: (1) After the raw material components of the 3D printing artificial meat ink as described in any one of claims 1-4 are stirred and mixed evenly, the ink is loaded into an injection cylinder for 3D printing to obtain a preliminary printed product. (2) After baking the initial printed product, 3D printed artificial meat is obtained.

[0020] Preferably, the 3D printing temperature is 40-50℃, the nozzle diameter is 1.2-2.5mm, and the material extrusion rate is 25-30mm. 3 The printing speed is 30-50 mm / s, the infill density is 100%, and the printing model can be a self-built model or an online model.

[0021] Preferably, the baking temperature is 60-70℃ and the baking time is 10-15 minutes.

[0022] This method preferably employs segmented processing during baking: the oven is preheated, and the baking process is divided into segments of 5 minutes each at a preset temperature. After each segment, the product is removed and its condition is checked to prevent it from drying out and burning, thus effectively enhancing the product's shape.

[0023] As a preferred option, the 3D printing artificial meat ink undergoes rheological testing before being loaded into the injection cylinder: the mixed raw materials are placed under pressure of 103-137 kPa and temperature of 121-126℃ for high-pressure steam sterilization for 20-25 minutes, and then placed in a 45℃ water bath for 10-15 minutes. The mixed raw material paste is then placed in a texture analyzer or rheometer to determine its rheological properties in order to improve the formulation ratio.

[0024] This step is used to simulate the changes in the properties of the relevant components of ink after it has been shaped by 3D printing and is ready to eat. The mixed raw materials are placed in high-pressure steam sterilization to reach an edible state, and then kept warm in a water bath to simulate the 3D printing set temperature in this invention. This allows for a better understanding of the rheological properties of the ink after it has been shaped by 3D printing. This rheological determination step can be used to better improve the formulation ratio.

[0025] Compared with the prior art, the present invention has the following beneficial effects: (1) Innovative use of edible fungi protein and improved presentation of meat fibers to replace traditional plant-based and cell-based proteins.

[0026] This invention primarily uses king oyster mushrooms as the experimental subject. King oyster mushrooms, a dual-purpose edible and medicinal fungus, are not only rich in important nutrients such as polysaccharides, proteins, polyphenolic compounds, and dietary fiber, but also possess various medicinal properties. King oyster mushrooms contain many of the limiting amino acids among the essential amino acids for the human body. Compared to vegetables, king oyster mushrooms have a significantly higher protein content; and compared to soy protein isolate, they avoid the bone brittleness and kidney burden caused by excessive soy protein consumption. King oyster mushrooms are high in protein and low in fat, contain a complete range of amino acids, and contain a large amount of bioactive proteins and peptides. In terms of nutritional value, they are comparable to meat protein to a certain extent, effectively meeting nutritional needs and possessing the potential to become a future protein source.

[0027] (2) The printing ink is prepared by the interaction of protein and polysaccharide. The combination improves the printability and enhances the synergistic effect of the two. The stability of food is improved by the thickening and gelation behavior of the two macromolecules. The finished product is processed and built by extrusion, hydrogel structure design and other technologies, thereby improving the performance of 3D printing ink.

[0028] (3) Through orthogonal experiments, the 3D printing technology is improved. In addition to traditional sensory evaluation and texture analysis, the correlation between the rheological properties of printing ink and 3D printing behavior is used as a reference to optimize the texture, mechanical support, and viscoelasticity of the printing ink. The advantages of 3D printing in the food industry—precise formulation and ability to modify food shapes—are leveraged to efficiently utilize raw materials. The focus is on developing 3D printed products based on edible fungi proteins that possess both nutritional and functional properties by studying the optimal conditions and parameters for printing ink formulation and food-grade 3D printing. Simultaneously, intelligent food-grade 3D printing is used to meet the personalized design of product appearance and the diverse nutritional needs of specific consumer groups. Data is saved and shared after product design is completed, creating new advantages in the digital economy.

[0029] (4) Abandoning the traditional production process that uses a large amount of artificial seasonings to mask the fishy smell of meat, the process achieves the best sensory flavor by adjusting the ratio of natural raw materials, thereby reducing or eliminating the fishy smell. At the same time, the process utilizes a variety of pigments in combination with raw materials to restore the natural color of the products and formulate healthy and harmless combination pigments. Attached Figure Description

[0030] Figure 1 This is the curve showing the effect of different contents of king oyster mushroom protein fiber powder on product hardness and the sensory evaluation results in Example 1; Figure 2 The curves showing the effects of different types of thickeners (1: no thickener added; 2: konjac gum added; 3: gelatin added; 4: sodium alginate added; 5: carrageenan added) on the product hardness index and sensory evaluation results in Example 2. Figure 3 These are the gelatinization temperatures calculated from different protein contents of king oyster mushrooms in Example 3; Figure 4 This is a comparison of the apparent viscosity of each component under different temperature conditions in Example 4; Figure 5 These are appearance images of the extruded filament accumulation and shaping state at different printing temperatures in Example 5; Figure 6 Examples 9 show different forms of artificial meat products printed using the edible fungus protein 3D printing ink of the present invention. Detailed Implementation

[0031] The technical solution of the present invention is illustrated below with specific embodiments, but the scope of protection of the present invention is not limited thereto: This invention mainly employs single-factor orthogonal experiments, using a texture analyzer to detect the hardness of the finished product, a rheometer to measure the rheological properties of the printing ink, and combining sensory evaluation to obtain a score.

[0032] Table 1 Sensory Evaluation Table of Finished Product Effect As shown in Table 1, the sensory evaluation of the finished product involved inviting 10 food science students to form a sensory evaluation group. Before the experiment, the evaluators received targeted training and standardized evaluation criteria. Each product group was scored according to the criteria in the sensory evaluation form above, and the average score of all members was taken as the final result, which was then statistically analyzed and plotted.

[0033] (1) Study on the effect of different types of thickeners on product shaping Thickeners, as food additives, increase the viscosity of food systems and maintain their stability. In meat processing, thickeners can improve the structure, texture, water retention, and stability of meat products, while also reducing costs. This study compared four thickeners: carrageenan, gelatin, sodium alginate, and konjac gum. Using different thickeners, ingredients were weighed according to the basic formula, and the product's texture, hardness, and sensory evaluation effects were assessed to study the impact of different thickener types on product configuration. The performance of each material ratio was measured, and the results were summarized and statistically analyzed.

[0034] (2) The effect of different protein contents of edible fungi on the product Single-factor experiments were conducted using the content of edible fungal protein isolate as the main variable to compare and evaluate the hardness and sensory evaluation scores of products with different proportions, and the summarized results were obtained. The selected food raw materials, as ideal materials for extrusion 3D printing, need to possess pseudoplastic fluid properties, i.e., shear-thinning behavior, with viscosity decreasing as the shear rate increases. Simultaneously, within its linear viscoelastic region, the storage modulus must be higher than the loss modulus. The printed product should be able to form a gel / gel-like structure with a certain strength; that is, the material viscosity must be sufficiently low at high shear rates to allow flow out of the nozzle, and it must rapidly recover high viscosity after printing to support the structure after deposition.

[0035] The raw material mixture used in this invention exhibits shear-thinning behavior and has a certain degree of printability, but it is insufficient to print products with high precision. Further optimization of its rheological properties is needed. By changing the relative content of edible fungi protein, this invention studies the rheological properties of inks with different components, comprehensively determines the optimal formulation ratio to achieve the best rheological performance, and further narrows down the formulation range.

[0036] (3) Optimization of printing parameters, primarily based on temperature Thermally responsive materials constitute a significant proportion of 3D-printed food inks. These materials undergo a sol-gel transition during printing, leading to a decrease in their mechanical properties at high temperatures. However, their strength increases once the temperature drops below their gelation temperature (Tg). Tg is crucial for selecting the optimal printing temperature within the nozzle cavity. Setting the printing temperature above Tg ensures ink flowability, allowing for easy extrusion of thermally responsive gel inks. Furthermore, the printing temperature must guarantee an appropriate sol-gel transition rate to generate sufficient mechanical strength, enabling the ink to achieve good self-support after extrusion onto the platform.

[0037] By varying the edible fungus protein content in printing inks, the gelatinization temperatures of inks with different protein ratios were measured. This study is closely related to the extrusion and sedimentation of different protein concentrations during the 3D printing molding process. Simultaneously, printing inks used for extrusion exhibit shear-thinning properties, with viscosity decreasing due to applied shear stress. Therefore, the force required for continuous ink flow is related to its viscosity and shear-thinning properties. Based on orthogonal experimental design, a two-factor orthogonal experiment was conducted with different temperatures and protein ratios to measure and compare the apparent viscosity of inks with different compositions, thus studying the ink extrusion conditions and flow characteristics.

[0038] (4) Study on the effect of different printing parameter settings on ink extrusion plasticity 3D printing, a type of additive manufacturing technology, employs a layer-by-layer printing and stacking process, saving time and processing costs. It also allows for intelligent customization of product appearance and precise nutritional control. When using the ink of this invention to prepare 3D-printed artificial meat, the printer's basic parameter settings—nozzle diameter, extrusion speed, and printing speed—significantly affect the ink's extrusion and shaping effects. Based on orthogonal experimental design, different printing parameters were set, and the extruded filament conditions and material accumulation states under different conditions were observed and compared. This study investigated the impact of 3D food printing process parameters on the printed product, ultimately determining the optimal conditions suitable for the 3D-printed artificial meat formula of this invention.

[0039] Example 1 (The effect of different protein contents in edible fungi on the product) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Fresh dried king oyster mushrooms (commonly available dried edible fungi, 80% dry, the same below) were purchased from the market, placed in a container, and dried in a vacuum drying oven at 70℃ for 10 minutes (a microwave oven or oven can also be used, heating in the normal mode until crisp). The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh (the degree of heating in the previous step was based on the grinder being able to pulverize to below 100 mesh particle size), removing impurities to obtain king oyster mushroom protein fiber powder that retains dietary fiber.

[0040] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), with the amount of king oyster mushroom protein fiber powder added as the independent variable to set up a control group, with no addition or 2.5g, 5.0g, 7.5g, and 10.0g of king oyster mushroom protein fiber powder added respectively, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel color, and 1g meat flavoring.

[0041] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0042] (3) 3D printing The mixed raw materials are loaded into the injection cylinder, placed into the 3D printer, and the parameters are adjusted before 3D printing the finished product.

[0043] The parameters were set as follows: printing temperature 45℃, nozzle diameter 1.2mm, and material extrusion rate 25mm. 3 The printing speed is 30mm / s, the infill density is 100%, and the printing model is a self-built model (an online model can also be used).

[0044] (4) Post-processing of 3D printed products Place the printed product in an oven (or a preheated oven) at 60℃. Once the oven is preheated, process the product in 5-minute intervals, checking the condition after each interval. Bake for a total of 15 minutes to obtain the final product. Cut the product into equal-volume pieces and test their hardness using a texture analyzer. Perform sensory evaluation according to the same standards. Repeat the test three times.

[0045] Example 2 (Study on the effect of different types of thickeners on product shaping) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0046] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, with the type of thickener as the independent variable, a control group was set up with no thickener added or with 0.5g konjac gum, 0.5g gelatin, 0.5g sodium alginate, 0.5g carrageenan added, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring.

[0047] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0048] (3) 3D printing The mixed raw materials are loaded into the injection cylinder, placed into the 3D printer, and the parameters are adjusted before 3D printing the finished product.

[0049] The parameters were set as follows: printing temperature 45℃, nozzle diameter 1.2mm, and material extrusion rate 25mm.3 The printing speed is 30mm / s, the infill density is 100%, and the printing model is a self-built model.

[0050] (4) Post-processing of 3D printed products The printed products were placed in an oven at 60℃. The oven was preheated and, once the preset temperature was reached, the products were processed in 5-minute intervals. After each interval, the products were removed and their condition was checked. The total baking time was 15 minutes to obtain the shaped products. The finished products were cut into equal-volume pieces and placed in a texture analyzer for hardness testing. Sensory evaluation was also conducted according to the same standards. The test was repeated three times.

[0051] Example 3 (Determination of gelatinization temperature of inks with different edible fungus protein contents) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0052] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), with the amount of king oyster mushroom protein fiber powder added as the independent variable to set up a control group, with no addition or 2.5g, 5.0g, 7.5g, and 10.0g of king oyster mushroom protein fiber powder added respectively, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel color, and 1g meat flavoring.

[0053] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0054] (3) Disinfection pretreatment of 3D printing ink The 3D printing ink was sterilized by high-pressure steam (103 kPa, 121℃) for 20 min, and then kept in a water bath at 45℃ for 10 min (simulating the 3D printing temperature set after sterilization). The mixed raw material paste was placed under a rheometer to determine its rheological properties, and the gelatinization temperature Tg of different ink formulations was calculated. The experiment was repeated three times.

[0055] Example 4 (Determination of ink rheological properties under simulated printing temperatures) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0056] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring. Weigh all raw materials and place them in a container. Stir and mix until a paste-like, slightly fluid consistency is achieved. Seal with plastic wrap and set aside.

[0057] (3) Disinfection pretreatment of 3D printing ink The 3D printing ink was sterilized by high-pressure steam (103 kPa, 121℃) for 20 min. A control group was set up with the water bath temperature as the independent variable. The water bath temperature was controlled at 35℃, 45℃, and 55℃ (simulating the 3D printing set temperature). The water bath temperature was maintained for 10 min. The mixed raw material paste was placed under a rheometer to measure its rheological properties and the changes in apparent viscosity of the printing ink at each temperature were compared.

[0058] Example 5 (Study on ink extrusion molding state at different printing temperatures) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0059] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring. Weigh all raw materials and place them in a container. Stir and mix until a paste-like, slightly fluid consistency is achieved. Seal with plastic wrap and set aside.

[0060] (3) 3D printing 3D printing ink is loaded into the injection cartridge, placed into the 3D printer, and the parameters are adjusted before 3D printing to shape the finished product. Parameter settings: A control group is set up with printing temperature as the independent variable. The printing temperature parameters are set to 35℃, 45℃, and 55℃, the nozzle diameter is 1.2mm, and the material extrusion rate is 25mm. 3The printing speed was 30 mm / s, the filling density was 100%, and the extruded filament accumulation and shaping were observed.

[0061] Example 6 (Study on the effect of different printing parameter settings—nozzle diameter on ink extrusion shaping state) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0062] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring.

[0063] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0064] (3) 3D Printing: 3D printing ink is loaded into the injection barrel, placed into the 3D printer, and the parameters are adjusted before 3D printing to shape the finished product. Parameter settings: The printing temperature is set to 45℃. A control group is set with the nozzle diameter as the independent variable. The nozzle diameters installed in the barrel are 0.84mm, 1.2mm, 2.0mm, and 3.0mm, respectively, and the material extrusion rate is 25mm. 3 The printing speed was 30 mm / s, the filling density was 100%, and the extruded filament accumulation and shaping were observed.

[0065] Example 7 (Study on the effect of different printing parameter settings - material extrusion rate on ink extrusion shaping state) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0066] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring.

[0067] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0068] (3) 3D Printing: 3D printing ink is loaded into the injection cylinder, placed into the 3D printer, and the parameters are adjusted before 3D printing to shape the finished product. Parameter settings: Printing temperature is 45℃, nozzle diameter is 1.2mm, and a control group is set with material extrusion rate as the independent variable, with the material extrusion rate set at 20mm. 3 / s, 25mm 3 / s, 30mm 3 The printing speed was 30 mm / s, the filling density was 100%, and the extruded filament accumulation and shaping were observed.

[0069] Example 8 (Study on the effect of different printing parameter settings - printing speed on ink extrusion and shaping state) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0070] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring.

[0071] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0072] (3) 3D Printing: 3D printing ink is loaded into the injection cylinder, placed into the 3D printer, and the parameters are adjusted before 3D printing to shape the finished product. Parameter settings: Printing temperature is 45℃, nozzle diameter is 1.2mm, and material extrusion rate is 25mm. 3 / s, with printing speed as the independent variable, a control group was set up with printing speed of 15mm / s, 30mm / s, 45mm / s and 60mm / s respectively, and the filling density was 100%. The extruded filament accumulation and shaping state were observed.

[0073] Example 9 (3D printing using a superior ink formulation) The specific preparation process of ink based on edible fungus protein for 3D printing is as follows: (1) Preparation of King Oyster Mushroom Protein Fiber Powder Commercially available fresh dried king oyster mushrooms were placed in a container and dried in a vacuum drying oven at 70℃ for 10 minutes. The dried mushrooms were then pulverized using a grinder and sieved to 100 mesh to remove impurities, yielding king oyster mushroom protein fiber powder that retains dietary fiber.

[0074] (2) Formulation of 3D printing ink 3D printing ink raw material formula: 7g soy protein (soy protein isolate), 2.5g king oyster mushroom protein fiber powder, 0.5g carrageenan, 8mL deionized water, 1g soy sauce, 0.5g red yeast rice, 0.5g caramel coloring, and 1g meat flavoring.

[0075] Weigh all ingredients and place them in a container. Stir and mix until the mixture reaches a paste-like, slightly fluid consistency. Seal with plastic wrap for later use.

[0076] (3) 3D printing The mixed raw materials are loaded into the injection cylinder, placed into the 3D printer, and the parameters are adjusted before 3D printing the finished product.

[0077] The parameters were set as follows: printing temperature 45℃, nozzle diameter 1.2mm, and material extrusion rate 25mm. 3 The printing speed is 30mm / s, the infill density is 100%, and the printing models are a self-built model and different online models.

[0078] (4) Post-processing of 3D printed products Place the printed product in an oven and set the temperature to 60℃. Preheat the oven and process it in 5-minute intervals after reaching the preset temperature. After each interval, remove the product and check its condition. Bake for a total of 15 minutes to obtain the shaped product.

[0079] The measurement results and analysis of each embodiment are as follows: (1) As Figure 1The figure shows the effect of different amounts of Pleurotus eryngii protein fiber powder on product hardness and the sensory evaluation results in Example 1. As can be seen from the figure, with the increase of Pleurotus eryngii protein fiber powder content, product hardness and sensory satisfaction show different trends. When the amount of Pleurotus eryngii protein fiber powder added is between 0g and 5g, the product hardness increases significantly. Analysis shows that increasing the initial amount of Pleurotus eryngii adds leads to an increase in the number of molecules per unit volume, enhancing the interaction between cellulose and protein macromolecules, as well as between protein and other components in the system, thus increasing product hardness. However, with further increases in the amount of Pleurotus eryngii protein fiber powder, the product hardness no longer increases and may even decrease. This may be related to the water absorption of Pleurotus eryngii protein; the protein absorbs more water, offsetting the enhanced gelation effect caused by its addition. Therefore, when the added amount exceeds 5g, the product hardness no longer increases and may even decrease, which is detrimental to self-support.

[0080] When the amount of king oyster mushroom protein fiber powder added is between 0g and 2.5g, sensory evaluation satisfaction increases with the increase of the added amount. Initially, the gel network structure formed by the isolated king oyster mushroom protein adsorbs water, sugars, and other components, giving the food a good gel texture, increasing chewiness, and retaining moisture in the product. When the amount of king oyster mushroom protein fiber powder added exceeds 2.5g, product satisfaction does not continue to increase, but instead decreases. Taking all factors into consideration, sensory evaluation should be the primary method, combined with product hardness, and an addition ratio of 2-3g is considered optimal.

[0081] (2) Figure 2 The figure shows the effect of different types of thickeners on product shaping in Example 2, referring to hardness indicators and sensory evaluation results. As can be seen from the figure, compared with the control group without thickener, the addition of carrageenan, sodium alginate, and konjac gum all resulted in a certain increase in product hardness. However, the addition of gelatin did not increase product hardness. This is because gelatin is not easily soluble in low-temperature water. In this example, low-temperature water was used to mix the raw materials, and the gelatin failed to dissolve well, thus failing to exert a thickening effect.

[0082] Compared to the absence of thickener, the components with added thickener showed no significant difference in sensory satisfaction (P>0.05). This indicates that different thickeners have a limited impact on the product's taste. According to the chart data, the product with the highest hardness (approximately 1450 grams) achieved after adding carrageenan, resulting in better shaping and the highest sensory satisfaction. Therefore, carrageenan can be considered a superior thickening ingredient for printing ink formulations.

[0083] (3) Figure 3The figure shows the gelatinization temperature results obtained from different amounts of Pleurotus eryngii protein in Example 3. As can be seen from the figure, the gelatinization temperature increases with increasing Pleurotus eryngii protein content, demonstrating the influence of the ink's thermal response characteristics on the printing temperature. The ink obtained with the optimal addition ratio (2.5g of Pleurotus eryngii protein fiber powder) in Example 1 has a gelatinization temperature closer to 45℃, providing a reference for setting the printing temperature range in Examples 4 and 5, and further explaining the extrusion and sedimentation states during printing.

[0084] (4) Figure 4 The figure shows the comparison results of the apparent viscosity of each component under different simulated printing temperatures in Example 4. As can be seen from the figure, all ink samples exhibit shear thinning behavior and decreased viscosity as the shear rate increases. This may be due to structural decomposition or rearrangement of the interaction between adjacent polymer chains. Further calculations and table lookups show that the consistency index K affects the extrusion behavior of the ink. An excessively high K may lead to extrusion difficulties and sample breakage, while a low consistency coefficient K is beneficial for maintaining continuous ink flow. The calculated K decreases with increasing temperature, indicating that high temperatures favor continuous extrusion. It is speculated that this may be because high temperatures hinder the formation of spirals and the resulting aggregation. Considering both gelatinization temperature and energy consumption, a temperature around 45°C can be selected as the optimal printing temperature.

[0085] (5) Figure 5 The figure shows the extruded filament accumulation and shaping state at different printing temperatures in Example 5. As can be seen from the figure, the ink printed at 35°C has a rough surface structure and is prone to clumping at the outlet, failing to deposit well onto the plane. This phenomenon is considered to be due to the temperature being lower than the gelation temperature of this formulation (measured at around 45°C in Example 3), resulting in a lower degree of ink gelation and thus poor extrudability. Excessively low temperatures may sometimes cause nozzle tip clogging. In contrast, lines printed at 55°C show a more easily extruded but softer state, even exhibiting a flowing nozzle and tailing effect. This phenomenon is considered to be because the printed structure at high temperatures requires a longer post-printing time to generate sufficient mechanical strength, which also indirectly indicates that the ink gelation characteristics change over time; while increasing the temperature, the gelation time needs to be improved. High-quality printing inks need to meet the high-temperature flow dynamics requirements of the extrusion stage to deposit well on the printing platform and spread continuously. Based on the printing forming state, a printing temperature closer to Tg (45°C) is preferred, allowing for smooth extrusion and rapid generation of sufficient mechanical strength, resulting in successful extrusion and deposition on the printer platform for self-support. In Example 5, the lines extruded at 45°C exhibit a smooth and uniform surface structure and good stacking force. This indicates that the printing temperature (40-50°C) set in this invention is close to the Tg of the ink, which will make it easier to gelatinize after extrusion, achieving smooth extrusion and stable shaping.

[0086] Table 2 (6) To ensure the molding effect and control the flowability of food materials, it is necessary to select a suitable nozzle orifice diameter. Based on the extrusion of filaments with different nozzle diameters and the material accumulation state, nozzle orifice diameters of 0.84mm are prone to clogging and poor filament extrusion. This is likely because the sieve diameter of the king oyster mushroom protein fiber powder used is relatively large (to maintain a certain fiber structure). Therefore, when the materials are fully bonded, ink particles larger than this orifice diameter are easily generated, resulting in poor extrusion and inability to extrude continuously. When printing with nozzles of 1.2mm and 2.0mm diameter, the diameter of the extruded filaments does not change significantly, and both can be continuously extruded and effectively stacked for shaping. However, considering that smaller diameter nozzles can create more delicate and intricate shapes, the 1.2mm nozzle is preferred. When using a 3.0mm nozzle, the diameter is too large, the extruded filaments exhibit a tailing effect, the printed shape begins to show breaks, and fluid jets occasionally appear, damaging the overall shaping; therefore, this nozzle is not used.

[0087] As shown in Table 2, when the nozzle orifice diameter is small, it limits the size of the extruded filament diameter. Although a smaller filament diameter results in better printing accuracy, if it is too small (0.84 mm in Example 6), nozzle clogging may occur, hindering printing. When the nozzle diameter is large (3.0 mm in Example 6), the extruded filament material may break, affecting the molding effect. When the nozzle orifice diameter is 1.2 mm, the printed sample surface is smooth, the extruded filament is relatively uniform, and there are no breakage points. Therefore, a nozzle orifice diameter of 1.2-2.5 mm is the preferred size for this invention.

[0088] Based on the extrusion filament condition and material accumulation state under different extrusion rate settings, it can be concluded that when the extrusion rate is selected as 20mm... 3 At a speed of 30mm / s, due to the slow extrusion, the nozzle, instead of being heated within the barrel, is directly exposed to room temperature. The material at the tip rapidly loses water and solidifies, easily clogging the nozzle and causing breakage in the printed shape. Material from the rear must continuously push forward to accumulate enough pressure before being forced out, resulting in poor filament output, uneven material accumulation, and the extrusion rate failing to keep up with the nozzle's movement speed. The filament is easily broken, and breakage and stacking coexist. However, as the extrusion rate increases, when set to 30mm... 3 At a speed of 1 / s, although the extrusion is faster and printing efficiency is effectively improved, the printed shape is unstable, the extruded filaments exhibit a wavy shape, and the filament lines are not fine, resulting in poor forming. There is excessive material accumulation at each printing point, making it quite thick. This may be because the extrusion volume at this rate is high, while the nozzle orifice diameter is relatively small (1.2mm in Example 8), which cannot ensure continuous and uniform movement of the extruded filaments at this rate, causing the material to be extruded in a wavy pattern. Using a 25mm nozzle... 3At an extrusion rate of / s, the extruded filaments are relatively uniform with no obvious breaks, resulting in straight-line printing and good shaping. Therefore, based on the results obtained in Example 6, a nozzle orifice diameter of 1.2-2.5mm was selected, and an extrusion rate of 25-30mm was chosen. 3 / s is the preferred value of the present invention.

[0089] Based on the extrusion filament conditions and material accumulation under different printing speed settings, it was found that a nozzle movement speed of 60mm / s resulted in high printing efficiency. However, because the movement speed was much higher than the extrusion speed, there was a delay in motor extrusion. Furthermore, the high viscosity of the sample material caused uneven extrusion of the filaments, resulting in the filaments being dragged and moved before they could be properly deposited and shaped on the plane, failing to achieve proper adhesion and leading to a very unsatisfactory final molding effect, even resulting in voids and collapses. At a lower printing speed of 15mm / s, the nozzle movement was slow, and the material piled up intermittently, also resulting in breakpoints and voids, and the printing efficiency was too low. At printing speeds of 30mm / s and 45mm / s, the sample filaments were extruded smoothly without breakpoints and were relatively uniform, with no significant difference in filament accumulation and shaping. However, at a movement speed of 45mm / s, the equipment began to shake due to mechanical resonance, which limited the speed of the equipment to some extent, increased mechanical wear, and shortened the lifespan of the instrument; therefore, this speed setting was not recommended. Therefore, combining the results obtained in Example 6, a nozzle orifice diameter of 1.2-2.5 mm was selected, and the extrusion rate of 25-30 mm was selected based on the results obtained in Example 7. 3 A printing speed of 30-50 mm / s is preferred for this invention.

[0090] (9) such as Figure 6 The image shown is an illustration of the finished product printed using the edible fungus protein 3D printing ink of this invention, as described in Example 9. Food-grade 3D printing allows for intelligent design of product appearances using different models, catering to the personalized customization and diverse nutritional needs of consumers. Furthermore, data can be saved and shared after the product design is completed, creating new advantages in the digital economy. This invention leverages the two major advantages of 3D printing in the food industry: precise proportioning and the ability to modify food shapes. It can create finished products with various forms and configurations for different groups to enhance consumer focus, while also allowing for precise addition and modification of ingredients to meet the needs of diverse consumer groups.

[0091] The above are merely preferred embodiments of the present invention and do not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made using the present invention specification, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.

Claims

1. A 3D printed artificial meat ink based on edible fungus protein, characterized in that: The raw material components are as follows, calculated by weight: 7 parts of isolated soy protein, 2-3 parts of edible fungus protein fiber powder, 0.5-0.8 parts of thickener, 1-2 parts of soy sauce, 1-2 parts of flavor, 8-10 parts of water and pigment.

2. The 3D printing artificial meat ink based on edible fungus protein according to claim 1, characterized in that: The pigment comprises 0.5-1 part of monascus pigment and 0.3-0.5 part of caramel pigment.

3. The 3D printing artificial meat ink based on edible fungus protein according to claim 1, characterized in that: The thickener is carrageenan, konjac gum or sodium alginate.

4. The 3D printing artificial meat ink based on edible fungus protein according to any one of claims 1 to 3, characterized in that: The flavor is meat flavor.

5. A method for preparing 3D printed artificial meat based on edible fungus protein, characterized in that: The steps include: (1) After the raw material components of the 3D printing artificial meat ink according to any one of claims 1 to 4 are stirred and mixed evenly, they are loaded into an injection barrel for 3D printing to obtain a printed preliminary product; (2) After baking the printed product, 3D printed artificial meat is obtained.

6. The method for preparing 3D printed artificial meat based on edible fungus protein according to claim 5, characterized in that: The printing temperature of the 3D printing is 40-50°C, the nozzle diameter is 1.2-2.5mm, and the material extrusion rate is 25-30mm 3 / s, printing speed is 30-50mm / s, and filling density is 100%.

7. The method for preparing 3D printed artificial meat based on edible fungus protein according to claim 5 or 6, characterized in that: The baking temperature is 60-70° C. and the baking time is 10-15 minutes.

8. The method for preparing 3D printed artificial meat based on edible fungus protein according to claim 5, characterized in that: The edible fungus protein fiber powder is prepared by drying and crushing dried mushroom products.

9. The method for preparing 3D printed artificial meat based on edible fungus protein according to claim 8, characterized in that: The drying is performed at 60-70° C. in vacuum for 5-10 min; and the pulverizing is performed by pulverizing and sieving to 100 mesh.

10. The method for preparing 3D printed artificial meat based on edible fungus protein according to claim 8 or 9, characterized in that: The dried mushroom products are one or more of dried Pleurotus eryngii products, dried Hericium erinaceus products and dried Pleurotus ostreatus products; the dryness of the dried mushroom products is 80% to 90% dry.

Citation Information

Patent Citations

  • Meat substitute stuffing dessert and preparation method thereof

    CN104206485A

  • Composite food ink suitable for high-precision printing and 3D printing method

    CN115708539A

  • KR20200141958A

Cited By

  • 3D printing composite seasoning paste ink based on edible mushrooms and preparation method of 3D printing composite seasoning paste ink

    CN122181694A