Liquid composite modified flocculant for treating desulfurization wastewater of power plant and preparation method of liquid composite modified flocculant

Through the use of liquid composite modified flocculants, the problem of poor treatment of desulfurization wastewater in power plants has been solved, and the efficient removal of COD, heavy metals and suspended matter has been achieved, the process flow has been simplified and the cost has been reduced, and the environmental protection standards have been adapted to the improvement.

CN118954738AInactive Publication Date: 2024-11-15BEIJING LIANFA MAITONG TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411312958.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-20
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing triple box process is not effective when treating power plant desulfurization wastewater, and cannot meet the current requirements of deterioration of water quality and improvement of environmental protection standards. The process is cumbersome and costly.

Method used

Liquid composite modified flocculants, including polyferrous and modified cationic flocculants, are used to remove COD, heavy metals and suspended substances in desulfurization wastewater through chemical oxidation and exchange, adsorption and flocculation of small molecules, and replace the original organic sulfur treatment and Iron/aluminum flocculant process simplifies process design and reduces the amount of agent added.

Benefits of technology

It improves the efficiency and effect of desulfurization wastewater treatment, reduces costs, simplifies the process flow, realizes efficient removal of desulfurization wastewater and heavy metal recycling, and adapts to the treatment needs of different water quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention is applicable to the technical field of water treatment, and provides a liquid composite modified flocculant for treating desulfurization wastewater of a power plant and a preparation method thereof, the liquid composite modified flocculant comprises the following components: 50-100 parts of component A polyferric, 100 parts of component B modified cationic flocculant, and an initiator; the component A is a polyferric component, and the mass part ratio of ferrous sulfate to hydrogen peroxide to concentrated sulfuric acid is 150: 90: 120; the component B is a modified cationic flocculant, and the mass ratio of epoxy chloropropane to dimethylamine to starch to NaOH to distilled water is 60: (10-20): 40: (5-10): 100. According to the liquid composite modified flocculant, on the basis of simplifying the treatment process, the dosage of chemicals is reduced, and the reaction speed and the treatment capacity are improved, so that the comprehensive treatment cost is reduced; meanwhile, through the synergistic effect of the raw materials in the chemical formula, the treatment effect and treatment efficiency of the desulfurization wastewater of the power plant are improved, various control indexes of the wastewater are greatly reduced, and great economic benefits and social benefits are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of water treatment, and in particular relates to a liquid composite modified flocculant for treating desulfurization wastewater from a power plant and a preparation method thereof. Background Art

[0002] Desulfurization wastewater is mainly the discharge water from the flue gas absorption tower during the wet desulfurization (limestone / gypsum method) of power plant boiler flue gas. In order to maintain the balance of materials in the slurry circulation system of the desulfurization device, prevent the soluble part of the flue gas, i.e., the chlorine concentration, from exceeding the specified value and ensure the quality of gypsum, a certain amount of desulfurization wastewater must be discharged from the system. The impurities contained in the desulfurization wastewater mainly include suspended solids, supersaturated sulfites, sulfates and heavy metals, many of which are the first-class pollutants that require strict control in the national environmental protection standards.

[0003] The general treatment process of desulfurization wastewater is: add lime slurry to the desulfurization wastewater to increase the pH value of the desulfurization wastewater, and make iron ions, chromium ions, zinc ions, nickel ions, manganese ions, and other heavy metal ions produce hydroxide precipitation. 2+ It can also react with some fluoride ions in wastewater to generate insoluble CaF2; 3+ Complexation generates insoluble substances. 2+ , Hg 2+ It remains in the wastewater in the form of ions, and then organic sulfide (TMT-15) is added to make it react with Pb 2+ , Hg 2+ The reaction forms insoluble sulfides that settle down. After the chemical precipitation reaction, the desulfurization wastewater still contains many small and dispersed particles and colloidal substances. Then a certain proportion of flocculants (such as polyaluminium chloride) are added to make them condense into larger particles and settle down. Then, high molecular weight polyelectrolytes are added as coagulants to neutralize the surface charge of the particles to reduce the surface tension of the particles, strengthen the growth process of the particles, and further promote the precipitation of hydroxides and sulfides, so that the fine floccules slowly become larger and easier to deposit flocs, which settle down together with the suspended matter and other impurities in the desulfurization wastewater.

[0004] At present, with the development of various industries and the continuous increase in electricity consumption, the proportion of thermal power plants in the power generation industry is also increasing. Therefore, while the power plant is continuously generating electricity, a large amount of desulfurization wastewater is also generated. At present, the commonly used treatment method for desulfurization wastewater in various power plants is the three-unit process, that is, the desulfurization wastewater is treated with lime method, organic sulfur method and iron / aluminum flocculant-polyacrylamide flocculation method in succession. The three-unit process mainly plays the role of reducing the concentration of suspended matter and removing heavy metals. However, with the continuous deterioration of current water quality, the increase in the amount of treated water and the improvement of environmental protection standards, the traditional three-unit treatment process is increasingly unable to meet the current desulfurization wastewater treatment requirements, making it impossible for desulfurization wastewater to meet the discharge standards. In order to improve the treatment effect and efficiency, it is imperative to simplify the process.

[0005] Currently, the use of organic and inorganic flocculants alone in wastewater treatment has poor effects on removing heavy metals and reducing COD. In addition, the process is complicated and the cost is high. Summary of the invention

[0006] The present invention provides a method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant, aiming to solve the above-mentioned problems. The method product can replace the organic sulfur treatment process and the iron / aluminum flocculant and polyacrylamide coagulant aid treatment process in the original triple box, simplify the process design and manpower and reagent input, and at the same time reduce the amount of lime added and the consumption of hydrochloric acid neutralization. While ensuring the upgrading of desulfurization wastewater, the reaction speed is further improved compared with solid integrated reagents, the treatment efficiency is increased, the amount of reagent added is reduced, the cost is reduced, and the treatment effect of desulfurization wastewater from thermal power plants is improved. At the same time, the invented product is also widely used and has good treatment effects in the fields of water treatment, heavy metal recovery, and COD reduction.

[0007] The liquid composite modified flocculant for treating desulfurization wastewater from power plants of the present invention comprises the following components by weight:

[0008] Component A: 50-100 parts of polyferric iron, component B: 100 parts of modified cationic flocculant, initiator;

[0009] The poly-iron component of component A includes ferrous sulfate, hydrogen peroxide and concentrated sulfuric acid, wherein, by weight, ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:120. The preparation method of component A poly-iron is: under stirring conditions, hydrogen peroxide is slowly dripped into ferrous sulfate, and concentrated sulfuric acid is added to adjust the acidity, and after controlling a certain acidity and temperature for reaction, poly-iron with a higher basicity can be obtained for standby use; for the selection of the feed ratio of component A, changing the feed ratio can increase the reaction rate, and considering the cost saving and other issues from the actual production, the molar ratio of ferrous sulfate to sulfuric acid is selected to be about 1:1.25, which is the best, and can obtain poly-iron with higher quality, higher basicity and activity.

[0010] The modified cationic flocculant component B includes epichlorohydrin, dimethylamine, starch, NaOH and distilled water, wherein the weight ratio of epichlorohydrin: dimethylamine: starch: NaOH: distilled water is 60:10-20:40:5-10:100.

[0011] Preferably, the initiator is cerium sulfate with a mass fraction of 0.45%.

[0012] Preferably, the reaction temperature in the preparation method of component A polyferric is 50-60°C, and the acidity is pH 2.5-3.0. For the selection of polymerization temperature, since the basicity of polyferric increases with the increase of reaction temperature, when the reaction temperature rises to 50-60°C, the basicity of polyferric sulfate has reached a relatively high level, and the basicity changes little when the temperature continues to rise. Since this experiment is an exothermic reaction, if the temperature is too high, on the one hand, it will cause partial decomposition of the oxidant. In order to achieve the same effect, the amount of oxidant must be increased; on the other hand, high temperature will also cause the polyferric sulfate to decompose and produce precipitation, reducing the flocculation ability. Therefore, it is more appropriate to control the reaction temperature to about 50-60°C.

[0013] Regarding the selection of acidity in component A, as the pH increases, the basicity tends to decrease. The reason is that during the hydrolysis process, the coordination between oxygen ions and sulfate ions and iron ions is in a competitive relationship. 2- When the amount of ferrous sulfate is less, more hydroxide ions combine with iron ions, making the product have a higher basicity, while the amount of sulfate ions is excessive, and the product has become Fe2(S04)3, not PFS. Under the premise of ensuring the quality of the product and a certain reaction rate, when the pH of the solution is controlled at 2.5-3, the molar ratio of ferrous sulfate to sulfuric acid is 1:1.25, at which time the polyferric basicity is the highest and the reaction activity is the strongest.

[0014] Preferably, the preparation method of the modified cationic flocculant of component B is as follows: weigh dimethylamine in a three-necked flask, place the flask in an ice-water bath, slowly add epichlorohydrin to the flask with a dropping funnel under stirring, remove the ice-water bath after the addition, place it in a 40-50°C constant temperature water bath, stir and react to obtain an organic cation; weigh an appropriate amount of starch, add a certain amount of NaOH, add an appropriate amount of distilled water to the three-necked flask to prepare a suspension with a starch mass fraction of 10%, pre-gelatinize, and completely gelatinize the starch; add NaOH to promote the starch modification reaction and control the pH value of the product to be weakly alkaline; then add an initiator to the gelatinized starch, add an appropriate amount of the prepared organic cation after activation, continuously pass nitrogen for protection, and graft polymerization reaction at 55-60°C to obtain a modified cationic flocculant.

[0015] Preferably, in the preparation method of the modified cationic flocculant of component B, the starch modification reaction is promoted and the pH value of the product is controlled to be 8.0-8.5.

[0016] Selecting different amounts of dimethylamine can produce organic cations with different cationic charge densities, thereby meeting the selection requirements of various desulfurization wastewater quality; selecting a starch suspension with a mass fraction of 10% is to facilitate complete gelatinization of starch and control viscosity; selecting a 5-10 mass ratio of NaOH is to promote starch modification reactions and control the product pH value to 8.0-8.5, thereby providing suitable polymerization pH conditions for the graft polymerization reaction of the initiator added later and the appropriately prepared organic cation.

[0017] Preferably, the step of preparing the organic cation is placed in a constant temperature water bath at 40-50° C. and stirred for reaction for 2 hours.

[0018] Preferably, a suspension with a starch mass fraction of 10% is pregelatinized at 65° C. for 2 hours to completely gelatinize the starch.

[0019] Preferably, an initiator is added to the gelatinized starch, and after activation for 30 seconds, an appropriate amount of prepared organic cation is added, nitrogen is continuously passed for protection, and the graft polymerization reaction is carried out at 60° C. for 2 hours.

[0020] The above-mentioned method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises the following steps:

[0021] Weigh the raw materials of each component according to the mass ratio, adjust the pH of the modified cationic flocculant of component B to an appropriate value, stir it evenly with the polyiron of component A at 45-55℃, then add the initiator, continue stirring to make the initiator evenly distributed among the materials, stop stirring, and react with the preparations of component A and component B to obtain a new type of efficient liquid composite modified flocculant. Component A and component B are mixed at 45-55℃, which not only opens the end group of the molecular weight chain of the modified starch, but also does not further denature the modified starch, protecting its activity to the maximum extent; after being mixed evenly, add the initiator to make it evenly mixed and react primary to form charged small molecules, and with the cessation of stirring and the composite reaction at 90℃, charged molecular chains of varying sizes are formed, and the overall molecule has a dispersed network structure with small branches. Due to its special structure, it not only strengthens the electrical neutralization and coagulation effect, but also can make use of its own rigid and flexible network molecular chain's sweeping, adsorption and bridging effect to fully flocculate and purify all ions and colloids in the wastewater.

[0022] Preferably, the composite reaction time of component A and component B is 90-120 minutes.

[0023] The liquid composite modified flocculant for treating desulfurization wastewater from a power plant of the present invention is added to the desulfurization wastewater for reaction. Since the pH of the wastewater is 9-10 due to the addition of gypsum in the early stage, hydrochloric acid needs to be added to lower the pH. Now the addition of the composite modified flocculant can save the amount of hydrochloric acid, and the final pH of the wastewater after treatment is 7-8.

[0024] Compared with the prior art products, the present invention has the following beneficial effects:

[0025] (1) The liquid composite modified flocculant of the present invention is mainly used in the treatment of desulfurization wastewater in power plants from three aspects: first, the reduction effect, which reduces the COD of the wastewater through small molecule chemical oxidation and exchange; second, the adsorption effect, which can adsorb heavy metals in the wastewater through the entanglement of network macromolecules, and form colloids through displacement and precipitation, and then remove them from the water; third, the flocculation effect, the synergistic effect between molecules can greatly remove suspended matter, insoluble matter and other colloids in the water, form flocs for solid-liquid separation, and reduce the content of suspended matter.

[0026] (2) The liquid composite modified flocculant of the present invention does not require the addition of other agents. On the basis of a smaller dosage, it can replace the original flocculant / coagulant aid. At the same time, it can reduce the dosage of the original lime or hydrochloric acid and reduce the operating cost of the desulfurization wastewater treatment system.

[0027] The liquid composite modified flocculant of the present invention has strong flocculation ability, faster reaction speed and better flocculation effect than the reagent used in the original process, and has a synergistic effect on the treatment of suspended matter in the desulfurization wastewater, and can achieve the upgrading and transformation of the original desulfurization wastewater treatment process. The liquid composite modified flocculant of the present invention has strong adaptability, a wide range of use, simple addition, high treatment efficiency, and is well adapted to the upgrading and transformation of the desulfurization wastewater system.

[0028] According to statistics on actual application cases of the liquid composite modified flocculant of the present invention, it can be used for desulfurization wastewater with different components and contents, with an average addition amount of 10-15 g per ton of wastewater, which is far lower than the current market demand for 100-200 g of existing flocculants.

[0029] (3) The liquid composite modified flocculant of the present invention has a stronger effect on heavy metal removal in addition to flocculation. It can remove heavy metal salts in desulfurization wastewater by entanglement and wrapping while flocculating.

[0030] (4) The liquid composite modified flocculant of the present invention, due to its special structure, not only enhances the electrical neutralization and coagulation effect, but also greatly reduces the COD and suspended matter content by virtue of the sweeping, adsorption and bridging effects of its rigid and flexible network molecular chains. DETAILED DESCRIPTION

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which the present invention belongs; the terms used in the specification of the invention herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention; the terms "including" and "having" in the specification and claims of the present invention and any variations thereof are intended to cover non-exclusive inclusions.

[0032] Example 1

[0033] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0034] The composition comprises the following components by weight: 100 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0035] Step 1: Preparation of component A polyferroic acid, wherein the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid is 150:90:120; hydrogen peroxide is slowly dripped into ferrous sulfate under stirring at 200 rad / min, and concentrated sulfuric acid is added to adjust the acidity, and the reaction is controlled at a certain acidity and temperature, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity pH to 2.5, thereby obtaining polyferroic acid with high basicity; the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity pH to 2.5, thereby obtaining polyferroic acid with high basicity.

[0036] Step 2: Preparation of modified cationic flocculant of component B, wherein the mass ratio of epichlorohydrin: dimethylamine: starch: NaOH: distilled water is 60:20:40:10:100; the preparation method is to weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding, and place it in a 45°C constant temperature water bath. Stir the reaction for 2 hours to obtain an organic cation.

[0037] Weigh an appropriate amount of starch, add a certain amount of NaOH, add an appropriate amount of distilled water in a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2 hours to completely gelatinize the starch. Then add 5.5 ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30 seconds, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerization at 60°C for 2 hours to obtain a modified cationic flocculant.

[0038] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and react for 90 minutes to obtain a new and efficient liquid composite modified flocculant. See the application effect evaluation table for details.

[0039] Example 2

[0040] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0041] The composition comprises the following components by weight: 100 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0042] Step 1: Preparation of component A polyferroic acid, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:120; under stirring at 200 rad / min, slowly drip hydrogen peroxide into ferrous sulfate, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity to pH 2.5, thereby obtaining polyferroic acid with high basicity.

[0043] Step 2: Preparation of modified cationic flocculant of component B: epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:10:40:10:100 according to the mass ratio; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding, and place it in a 45°C constant temperature water bath. Stir and react for 2 hours to obtain an organic cation.

[0044] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 4.2ml of a certain mass fraction of initiator to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a modified cationic flocculant.

[0045] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and react for 90 minutes to obtain a new and efficient liquid composite modified flocculant. See the application effect evaluation table for details.

[0046] Example 3

[0047] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0048] The invention comprises the following components by weight: 50 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0049] Step 1: Preparation of component A polyferric iron, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:112; slowly drip hydrogen peroxide into ferrous sulfate under stirring at 200 rad / min, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity to pH 2.7, thereby obtaining high basicity polyferric iron;

[0050] Step 2: Preparation of modified cationic flocculant of component B: epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:15:40:8:100 by mass ratio; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding, and place in a 45°C constant temperature water bath. Stir and react for 2 hours to obtain an organic cation.

[0051] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 4.8ml of 0.45% initiator to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a new type of high-efficiency modified cationic flocculant.

[0052] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and react for 90 minutes to obtain a new and efficient liquid composite modified flocculant. See the application effect evaluation table for details.

[0053] Example 4

[0054] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0055] The invention comprises the following components by weight: 50 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0056] Step 1: Preparation of component A polyferric iron, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:107; slowly drip hydrogen peroxide into ferrous sulfate under stirring at 200 rad / min, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity to pH 3.0, thereby obtaining high basicity polyferric iron;

[0057] Step 2: Preparation of modified cationic flocculant of component B, according to the mass ratio, epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:20:40:5:100; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding and place in a 45°C constant temperature water bath. Stir and react for 2 hours to obtain an organic cation.

[0058] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 5.5ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a modified cationic flocculant.

[0059] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and react for 90 minutes to obtain a new and efficient liquid composite modified flocculant. See the application effect evaluation table for details.

[0060] Comparative Example 1

[0061] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0062] The invention comprises the following components by weight: 40 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0063] Step 1: Preparation of component A polyferroic acid, wherein component A is the preparation of polyferroic acid; wherein the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid is 150:90:120; under stirring at 200 rad / min, hydrogen peroxide is slowly dripped into ferrous sulfate, the reaction temperature is 55° C., concentrated sulfuric acid is added to adjust the acidity to pH 2.8, thereby obtaining polyferroic acid with high basicity.

[0064] Step 2: Preparation of modified cationic flocculant of component B, wherein component B is preparation of modified cationic flocculant; wherein according to the mass ratio, epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:20:40:10:100; its preparation method is to weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, and after adding, remove the ice water bath and place it in a 45°C constant temperature water bath. Stir the reaction for 2 hours to obtain an organic cation.

[0065] Weigh an appropriate amount of starch, add a certain amount of NaOH, add an appropriate amount of distilled water in a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2 hours to completely gelatinize the starch. Then add 5.5 ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30 seconds, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerization at 60°C for 2 hours to obtain a modified cationic flocculant.

[0066] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and allow the composite reaction to proceed for 90 minutes to obtain the liquid composite modified flocculant. See the application effect evaluation table for details.

[0067] Comparative Example 2

[0068] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0069] The composition comprises the following components by weight: 100 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0070] Step 1: Preparation of component A polyferric iron, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:100; slowly drip hydrogen peroxide into ferrous sulfate under stirring at 200 rad / min, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity pH to 3.5, thereby obtaining polyferric iron with low basicity;

[0071] Step 2: Preparation of modified cationic flocculant of component B: epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:10:40:10:100 according to the mass ratio; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding, and place it in a 45°C constant temperature water bath. Stir and react for 2 hours to obtain an organic cation.

[0072] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 4.8ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a modified cationic flocculant.

[0073] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and allow the composite reaction to proceed for 90 minutes to obtain the liquid composite modified flocculant. See the application effect evaluation table for details.

[0074] Comparative Example 3

[0075] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0076] The invention comprises the following components by weight: 50 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0077] Step 1: Preparation of component A polyferric iron, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:120; slowly drip hydrogen peroxide into ferrous sulfate under stirring at 200 rad / min, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity to pH 2.5, thereby obtaining high basicity polyferric iron;

[0078] Step 2: Preparation of modified cationic flocculant of component B, according to the mass ratio, epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:5:20:8:100; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding, and place it in a 45°C constant temperature water bath. Stir the reaction for 2 hours to obtain an organic cation.

[0079] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 3.5ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a modified cationic flocculant.

[0080] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value of 8.0-8.5, stir it evenly with the A component polyiron at 50°C, then add 1 ml of initiator again, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and react for 90 minutes to obtain a liquid composite modified flocculant. See the application effect evaluation table for details.

[0081] Comparative Example 4

[0082] A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant comprises:

[0083] The invention comprises the following components by weight: 50 parts of polyferric acid as component A, 100 parts of modified cationic flocculant as component B, and 0.45% of cerium sulfate as initiator by weight.

[0084] Step 1: Preparation of component A polyferric iron, according to the mass ratio of ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:100; slowly drip hydrogen peroxide into ferrous sulfate under stirring at 200 rad / min, the reaction temperature is 55°C, and concentrated sulfuric acid is added to adjust the acidity to pH 3.0, thereby obtaining polyferric iron with a lower basicity;

[0085] Step 2: Preparation of modified cationic flocculant of component B, according to the mass ratio, epichlorohydrin: dimethylamine: starch: NaOH: distilled water = 60:5:40:5:100; weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after adding and place in a 45°C constant temperature water bath. Stir and react for 2 hours to obtain an organic cation.

[0086] Weigh starch, add NaOH, add distilled water to a three-necked flask to make a 10% starch suspension, pre-gelatinize at 65°C for 2h to completely gelatinize the starch. Then add 3.5ml of initiator with a mass fraction of 0.45% to the gelatinized starch, activate for 30s, add an appropriate amount of prepared organic cations, continuously pass nitrogen for protection, and graft polymerize at 60°C for 2h to obtain a modified cationic flocculant.

[0087] Step 3: Preparation of liquid composite modified flocculant. Adjust the pH of the synthesized B component modified cationic flocculant to an appropriate value, stir it evenly with the A component polyiron at 50°C, then add the initiator, continue stirring for 30 minutes to allow the initiator to be evenly distributed among the materials, stop stirring, and allow the composite reaction to proceed for 90 minutes to obtain a liquid composite modified flocculant.

[0088] The decontamination performance of the liquid composite modified flocculant prepared by the present invention for treating desulfurization wastewater from power plants was tested and analyzed.

[0089] Through the use of data statistics, due to the different components and contents of different desulfurization wastewater, the amount of reagent added is also different. The general amount of the reagent added is 10 to 15g of liquid composite modified flocculant per ton of wastewater. In order to verify the application effect of the above embodiments and comparative examples on desulfurization wastewater from different power plants, 1L of wastewater was taken and 0.1ml of liquid composite modified flocculant with a mass fraction of 10% was added, which is equivalent to a consumption of 10g of liquid composite modified flocculant per ton of wastewater. Table 2 shows the content of various heavy metals in the raw water of the power plant in the actual sewage of each corresponding electric field. See Table 1 for specific comparative application test effect evaluation:

[0090] Table 1: Application effect evaluation table

[0091]

[0092]

[0093] Table 2: Heavy metal content in raw water from power plants

[0094]

[0095] By comparing the indicators before and after the raw water treatment, it can be obtained that the sewage treatment effect of the liquid composite modified flocculant prepared in the embodiment of the present invention is significantly better than that of the flocculant prepared in the comparative example, and the raw water removal rate of the liquid composite modified flocculant prepared in the embodiment reaches more than 94%. The specific targeted performance is as follows:

[0096] (1) The decontamination effects of Example 1 and Comparative Example 1 can be obtained. When the ratio of component A in Comparative Example 1 is not within the required range, the removal effect of heavy metals and COD is obviously poor; when component A is prepared according to step 1, when each component is not within the required range, the treatment effect of the agent is poor, the removal rate of heavy metals and COD is greatly reduced, and the removal rate of suspended matter is low. Therefore, in terms of mass fraction, when the ratio of component A polyferric iron: component B modified cationic flocculant is within the range of 50-100:100, the decontamination effect of the prepared liquid composite modified flocculant is significantly improved.

[0097] (2) Compared with the decontamination effect of Example 3 and Comparative Example 3, when component B is prepared according to step 2, when the components are not within the required range, the treatment effect of the agent is poor, the removal rates of heavy metals and COD are reduced, and the removal of suspended matter is greatly reduced; therefore, in the preparation method of the modified cationic flocculant of component B, when the ratio of epichlorohydrin: dimethylamine: starch: NaOH: distilled water is 60:10-20:40:5-10:100 in terms of mass fractions, the decontamination effect of the prepared liquid composite modified flocculant will be significantly improved.

[0098] (3) Compared with the decontamination effects of Example 2 and Comparative Example 2, when component A in Comparative Example 2 is prepared according to step 1, when the amount of concentrated sulfuric acid is reduced, the polyiron of component A obtained is polyiron with a relatively low basicity, and the treatment effect and removal rate of the agent prepared in Example 2 are greatly reduced.

[0099] (4) Compared with the decontamination effects of the flocculants prepared in Example 4 and Comparative Example 4, the components in the preparation process of component A of Comparative Example 4 were not in the required proportions, and when component B was prepared according to step 2, the components were also not in the required range. The treatment effect and removal rate of the flocculant prepared in Comparative Example 4 were greatly reduced.

[0100] From the data results in Table 1, it can be seen that the liquid composite modified flocculant prepared by the present invention has a stronger effect on heavy metal removal in addition to flocculation. It can remove heavy metal salts in desulfurization wastewater by winding and wrapping at the same time as flocculation. Due to its special structure, it not only strengthens the electrical neutralization and coagulation effect, but also greatly reduces the COD and suspended matter content by virtue of the sweeping, adsorption and bridging effect of its rigid and flexible mesh molecular chain.

[0101] The liquid composite modified flocculant prepared by the present invention can not only reduce the amount of lime added, but also reduce the amount of hydrochloric acid added, thereby avoiding various problems caused by adding too much reagent, and can replace the addition of original organic sulfur and flocculants and coagulants, greatly simplifying the desulfurization wastewater treatment process on the basis of improving the desulfurization wastewater treatment index and promoting the desulfurization wastewater discharge to meet the standards, and has excellent treatment effects on desulfurization wastewater from power plants in various regions due to its wide adaptability. Therefore, the agent has broad application prospects and is expected to be applied to more other types of wastewater.

[0102] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the protection scope of the invention. Obviously, the described embodiments are only some embodiments of the present invention, rather than all embodiments. Based on these embodiments, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

Claims

1. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant, characterized in that: By mass, it includes the following components: Component A: 50-100 parts of polyferric iron, component B: 100 parts of modified cationic flocculant, initiator; The poly-iron component of component A includes ferrous sulfate, hydrogen peroxide and concentrated sulfuric acid, wherein, by weight, ferrous sulfate: hydrogen peroxide: concentrated sulfuric acid = 150:90:120; The preparation method of the polyiron of component A is as follows: under stirring conditions, hydrogen peroxide is slowly dripped into ferrous sulfate, and concentrated sulfuric acid is added to adjust the acidity. After the reaction is carried out under a certain acidity and temperature, polyiron with a high basicity can be obtained for standby use; The modified cationic flocculant component B includes epichlorohydrin, dimethylamine, starch, NaOH and distilled water, wherein the mass ratio of epichlorohydrin: dimethylamine: starch: NaOH: distilled water is 60:10-20:40:5-10:

100.

2. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 1, characterized in that: The initiator is cerium sulfate with a mass fraction of 0.45%.

3. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 2, characterized in that: In the preparation method of the A component polyiron, the reaction temperature is 50-60° C. and the acidity value is pH 2.5-3.

0.

4. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 2, characterized in that: The preparation method of the modified cationic flocculant of component B is as follows: weigh dimethylamine in a three-necked flask, place the flask in an ice water bath, slowly add epichlorohydrin into the flask with a dropping funnel under stirring, remove the ice water bath after the addition, place the flask in a constant temperature water bath pot at 40-50°C, stir and react, and obtain an organic cation; Weigh an appropriate amount of starch, add a certain amount of NaOH, add an appropriate amount of distilled water in a three-necked flask to prepare a suspension with a starch mass fraction of 10%, pre-gelatinize, and make the starch completely gelatinized; add NaOH to promote the starch modification reaction and control the pH value of the product to be weakly alkaline; Then, an initiator is added to the gelatinized starch, and after activation, an appropriate amount of prepared organic cations is added, nitrogen is continuously passed for protection, and a graft polymerization reaction is carried out at 55-60°C to obtain a modified cationic flocculant.

5. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 4, characterized in that: In the preparation method of the B component modified cationic flocculant, the starch modification reaction is promoted and the pH value of the product is controlled to be 8.0-8.

5.

6. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 4, characterized in that: The step of preparing the organic cation is placed in a constant temperature water bath at 40-50°C and stirred for reaction for 2 hours.

7. A liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 4, characterized in that: A suspension with a starch mass fraction of 10% was pregelatinized at 65°C for 2 h to completely gelatinize the starch.

8. The liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 4, characterized in that: Initiator was added to gelatinized starch, and after activation for 30 seconds, an appropriate amount of prepared organic cation was added, nitrogen was continuously passed for protection, and graft polymerization reaction was carried out at 60°C for 2 hours.

9. A method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to any one of claims 1 to 8, characterized in that: The steps include: Weigh the raw materials of each component according to the mass ratio, adjust the pH of the modified cationic flocculant of component B to an appropriate value, stir it evenly with the polyiron of component A at 45-55°C, then add the initiator, continue stirring until the initiator is evenly distributed among the materials, stop stirring, and allow the preparations of components A and B to undergo a composite reaction to obtain a new type of efficient liquid composite modified flocculant.

10. The method for preparing a liquid composite modified flocculant for treating desulfurization wastewater from a power plant according to claim 9, characterized in that: The composite reaction time of component A and component B is 90-120 minutes.

Citation Information

Patent Citations

  • Preparation method for compound flocculant and product and application thereof

    CN109052593A

  • Cationic starch and preparation method thereof

    CN110092844A

  • Producting Method of Flocculant Composition for WaterTreatment and Flocculant Composition Thereby

    KR1020010103460A