Re-operation method of rapid annealing furnace

By regulating the cavity heating function in a rapid annealing furnace, the cavity environment is unstable and the heating lamp load is too high, and the cavity environment is restored and cost reduction is achieved.

CN118957232APending Publication Date: 2024-11-15JIANGXI ZHAO CHI SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411108548.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The temperature calibration method of the rapid annealing furnace leads to unstable cavity environment, excessive load of the heating lamp fails, and finally the cavity needs to be replaced, which is costly.

Method used

By regulating the cavity heating function of the rapid annealing furnace, using the mass production procedure to run empty-handed, and placing the preset thickness of the ITO film accompanying sheet on the loading tray, setting the process to restore the cavity environment, repeating Many times until the run-in is completed.

Benefits of technology

The environment of the cavity in the rapid annealing furnace is effectively restored, avoiding the problems of unstable cavity environment and excessive load of heating lamps, and reducing the cost of replacing the cavity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957232A_ABST
    Figure CN118957232A_ABST
Patent Text Reader

Abstract

The invention provides a recovery method of a rapid annealing furnace. The method comprises the following steps: carrying out temperature correction on a cavity heating function of the rapid annealing furnace; carrying out idle running on the rapid annealing furnace by utilizing a mass production program, and then depositing an ITO film layer with a preset thickness on an accompanying sheet for resetting the annealing furnace; placing the accompanying sheets on a carrying disc of the rapid annealing furnace one by one and carrying out setting treatment under set conditions so as to recover the environment of the inner cavity of the annealing furnace; and repeating the step of placing the accompanying sheets on the carrying disc of the rapid annealing furnace one by one for preset times and carrying out setting treatment under the set condition, and then replacing the accompanying sheets and carrying out setting treatment under the set condition again until accompanying running is completed. The problems that in the prior art, due to the temperature correction mode of a rapid annealing furnace, the cavity environment is unstable, the heating lamp loses efficacy due to too high load, finally, the cavity needs to be replaced, and cost is high are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor manufacturing equipment, and in particular to a method for resetting a rapid annealing furnace. Background Art

[0002] RTA (rapid thermal annealing) rapid annealing furnace uses halogen infrared lamp as heat source, and heats the wafer or material to 300℃-1200℃ in a very short time through extremely fast heating rate, thereby eliminating some defects inside the wafer or material and improving product performance. Rapid annealing furnace adopts advanced microcomputer control system and PID closed-loop temperature control, which can achieve extremely high temperature control accuracy and temperature uniformity, and can be configured with vacuum chamber, and can also be configured with multiple gases according to user process requirements, such as O2, N2, Ar, etc.

[0003] As the RTA is used for a long time, the quartz cover in the cavity will be covered with annealing material, and the cavity temperature will deviate. The cavity environment will also gradually change, which will eventually greatly reduce the annealing effect and cause product problems.

[0004] Currently, the cavity environment is usually restored by adjusting the oxygen flow, increasing the heating lamp load, and re-calibrating the temperature. However, if this is done for a long time, the cavity environment will become unstable, the heating lamp will fail due to excessive load, and finally the cavity will need to be replaced, which is costly. Summary of the invention

[0005] Based on this, the purpose of the present invention is to provide a rapid annealing furnace restoration method and ITO film, aiming to solve the problem in the prior art that the rapid annealing furnace temperature calibration method leads to unstable cavity environment, excessive load failure of the heating lamp, and finally the need to replace the cavity, which is costly.

[0006] The object of the present invention is to provide a method for resuming a rapid annealing furnace, the method comprising: Calibrate the temperature of the cavity heating function of the rapid annealing furnace; The rapid annealing furnace is run empty using a mass production program, and then an ITO film layer of a preset thickness is deposited on a companion sheet used for re-running the annealing furnace; Placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions to restore the environment of the cavity of the annealing furnace; Repeat the steps of placing the accompanying sheets one by one on the carrier of the rapid annealing furnace and performing the setting treatment under the setting conditions for a preset number of times, and then replace the accompanying sheets and perform the setting treatment under the setting conditions again until the accompanying process is completed.

[0007] Furthermore, in the above-mentioned method for re-annealing the rapid annealing furnace, the thickness of the ITO film layer is 10000Å~12000Å.

[0008] Furthermore, in the above-mentioned method for restoring the rapid annealing furnace, the step of placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions to restore the environment of the cavity in the annealing furnace includes: The cavity is evacuated to a preset pressure, and then the cavity is purged with nitrogen gas at a preset flow rate; After the nitrogen purge stops, the chamber is evacuated again to a preset pressure, and the chamber is preheated after the chamber temperature is raised to a first preset temperature; The chamber is heated to a second preset temperature, a preset flow rate of oxygen is introduced for a preset time, and then an excess amount of oxygen is introduced; The vacuum pump valve is closed, and nitrogen gas with a preset flow rate is introduced for cooling. When the temperature is cooled to a third preset temperature, the carrier is removed from the cavity.

[0009] Furthermore, in the above-mentioned method for resuming the rapid annealing furnace, the preset pressure is 0.05 torr~0.1 torr.

[0010] Furthermore, in the above-mentioned method for resuming the rapid annealing furnace, the first preset temperature is 190°C to 210°C, the second preset temperature is 540°C to 560°C, and the third preset temperature is 300°C to 350°C. Furthermore, in the method for resuming the rapid annealing furnace, in the step of evacuating the cavity to a preset pressure and then purging the cavity with nitrogen at a preset flow rate, the nitrogen flow rate is 3L / min~8L / min.

[0011] Furthermore, in the method for resuming the rapid annealing furnace, the chamber is heated to a second preset temperature, a preset flow rate of oxygen is introduced for a preset time, and then an excess amount of oxygen is introduced, and the oxygen flow rate is 4 sccm to 5 sccm.

[0012] Furthermore, in the above-mentioned method for resuming the rapid annealing furnace, the vacuum pump valve is closed, a preset flow rate of nitrogen is introduced for cooling, and when the temperature is cooled to a third preset temperature, the carrier is taken out of the cavity: The flow rate of cooling nitrogen is 95~100L / min, and the cooling temperature is 300~350℃.

[0013] Furthermore, in the above-mentioned method for resuming the rapid annealing furnace, before the step of calibrating the temperature of the cavity heating function of the rapid annealing furnace, the method further includes: The quartz cover plate of the rapid annealing furnace is removed, and it is soaked in hydrochloric acid of a preset concentration and then rinsed clean; The quartz cover plate is baked in an oven to ensure that the quartz cover plate is dry, and then installed in the rapid annealing furnace.

[0014] Furthermore, in the above-mentioned method for resuming the rapid annealing furnace, the preset concentration of the hydrochloric acid is 10%, the soaking time is 4 hours, the baking temperature is 200° C., and the baking time is 2 hours.

[0015] The present invention calibrates the temperature of the cavity heating function of the rapid annealing furnace; uses the mass production program to run the rapid annealing furnace empty, and then deposits an ITO film layer of a preset thickness on the companion film used for the annealing furnace restart; places the companion films one by one on the carrier of the rapid annealing furnace and performs setting treatment under set conditions to restore the environment of the cavity in the annealing furnace; repeats the steps of placing the companion films one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions for a preset number of times, and then replaces the companion films and performs setting treatment again under set conditions until the accompanying run is completed. Instead of changing the process parameters and increasing the load of the heating lamp to put the cavity in an abnormal overload state, resulting in cavity instability. The invention solves the problem that the temperature calibration method of the rapid annealing furnace in the prior art leads to an unstable cavity environment, the heating lamp fails due to excessive load, and finally the cavity needs to be replaced, which is costly. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a flow chart of a method for resuming a rapid annealing furnace according to an embodiment of the present invention; The following specific implementation manner will further illustrate the present invention in conjunction with the above-mentioned drawings. DETAILED DESCRIPTION

[0017] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Several embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.

[0018] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.

[0019] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0020] The embodiment of the present invention proposes a method for restoring a rapid annealing furnace to solve the problem that the temperature calibration method of the rapid annealing furnace in the prior art leads to an unstable cavity environment, the heating lamp fails due to excessive load, and finally the cavity needs to be replaced, which is costly.

[0021] See also Figure 1 , which is a flow chart of a method for resuming a rapid annealing furnace according to the present invention, and the method for resuming a rapid annealing furnace includes steps S10 to S13.

[0022] Step S10, calibrating the temperature of the cavity heating function of the rapid annealing furnace.

[0023] Among them, the cavity heating function is calibrated. The carrier has 9 positions, which can hold 5 temperature measuring TC wafers for temperature calibration. The calibration temperature is the temperature required by the production process, which is usually 550℃±5℃.

[0024] In addition, in some optional embodiments of the present invention, the step of calibrating the temperature of the cavity heating function of the rapid annealing furnace also includes: Remove the quartz cover of the RTA chamber, soak it in 8-12%, for example, 10% hydrochloric acid for 3-5 hours, for example, 4 hours, rinse it with pure water, and then bake it in an oven at 150-250°C for 2 hours to ensure that the quartz cover is dry, and then install it into the chamber.

[0025] Step S11, using a mass production program to run the rapid annealing furnace empty, and then depositing an ITO film layer of a preset thickness on a companion wafer used for re-running the annealing furnace.

[0026] Among them, the mass production program is used for dry running to test whether the machine operation alarm is triggered. The cavity is placed in a heated environment to remove impurities such as water vapor in the cavity. The dry run 3 runs makes the temperature of the cavity more stable and the cleaning more thorough.

[0027] More specifically, an ITO film layer of 10000Å~12000Å is deposited / sputtered on a clean sapphire wafer or silicon wafer (companion wafer). In the embodiment of the present invention, 45 wafers can be selected. Among them, the ITO film layer in the production process is generally 200~2000Å. Thickening is for better annealing effect, and there is no need for too many ITO film layer companion wafers, which reduces the re-machine time and the cost of companion wafers. Too thick is prone to over-temperature alarm, so 10000Å~12000Å is preferred.

[0028] Step S12, placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions to restore the environment of the cavity of the annealing furnace.

[0029] Among them, the companion sheets are placed one by one on the carrier, 9 sheets in a group, and a group can be annealed 5 times in a cycle, 45 sheets, a total of 25 runs, so that the cavity is covered with a thin layer of ITO to improve the cavity environment.

[0030] Specifically, the carrier enters the cavity and is evacuated to 0.05torr~0.1torr, so that the impurity gas in the cavity is reduced to a very small amount to avoid affecting the ITO annealing effect at high temperature; 5L / min nitrogen is introduced into the chamber for 20 seconds. At this time, the chamber is also in a vacuum environment, which can further quickly drive away the impurity gas in the chamber. Since nitrogen is an inert gas, it does not affect the ITO annealing. After nitrogen purge stops, evacuate the chamber to 0.05 torr~0.1 torr again, raise the chamber temperature to 200°C in 20 seconds, and maintain it for 50 seconds~70 seconds; The chamber temperature is raised to 540℃~560℃ in 50S. At this time, 4sccm~5sccm of oxygen is introduced and maintained for 500S~700S. The long-term high temperature and excessive oxygen introduction are to allow the molecules in the ITO film layer to fully overflow and restore the chamber environment as soon as possible. Close the vacuum pump valve and allow 95~100L / min N2 to cool. When the temperature cools to 300~350℃, the carrier is removed from the cavity and the process is completed.

[0031] Step S13, repeating the step of placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing set processing under set conditions for a preset number of times, and then replacing the companion sheets and performing set processing again under set conditions until the companion annealing is completed.

[0032] Wherein, step S11 is repeated 5 times, and a new ITO companion sheet can be replaced, until 45 companion sheets are repeated for 25 runs.

[0033] Then run 3 Runs with the original production program of the product. The 3rd Run carries the ITO companion sheet. After the process is completed, test the square resistance and transmittance data of ITO. If it meets the requirements, it can be used for production.

[0034] In summary, the method for resuming the rapid annealing furnace proposed in the embodiment of the present invention is to calibrate the temperature of the cavity heating function of the rapid annealing furnace; use the mass production program to run the rapid annealing furnace empty, and then deposit an ITO film layer of a preset thickness on the companion film used for resuming the annealing furnace; place the companion films one by one on the carrier of the rapid annealing furnace and perform setting treatment under set conditions to restore the environment of the cavity in the annealing furnace; repeat the steps of placing the companion films one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions for a preset number of times, and then replace the companion films and perform setting treatment again under set conditions until the accompanying run is completed. Instead of changing the process parameters and increasing the load of the heating lamp to put the cavity in an abnormal overload state, resulting in instability of the cavity. The problem of the rapid annealing furnace temperature calibration method in the prior art causing the cavity environment to be unstable, the heating lamp to fail due to excessive load, and finally the need to replace the cavity, which is costly, is solved.

[0035] In order to facilitate understanding of the present invention, the present invention will be described more fully below with reference to relevant embodiments. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.

[0036] Embodiment 1 Embodiment 1 of the present invention provides a method for resuming a rapid annealing furnace, comprising: Remove the quartz cover plate in the annealing furnace, soak it in 10% hydrochloric acid for 4 hours, rinse it with pure water, and then bake it in an oven at 200℃ for 2 hours; Calibrate the chamber heating function to 550°C and run 3 runs using the mass production program. Deposit / sputter an ITO film with a thickness of 10,000Å on a clean sapphire wafer or silicon wafer (companion wafer); Place the ITO companion sheets on the carrier one by one, 9 sheets in a group, and a group can be annealed 5 times in a cycle. The carrier enters the cavity and is evacuated to 0.05 torr; The chamber was purged with nitrogen at 5 L / min for 20 seconds. After nitrogen purging was stopped, the chamber was evacuated to 0.05 torr again. The chamber temperature was raised to 200°C over 20 seconds and maintained for 60 seconds. The chamber temperature was raised to 550°C in 50 seconds, at which time 5 sccm of oxygen was introduced, and the temperature was maintained for 600 seconds, and then excess oxygen was introduced; Close the vacuum pump valve and introduce 95L / min N2 for cooling. When the temperature cools to 300℃, the carrier is removed from the cavity and the process is completed.

[0037] Repeat the above steps 7 to 11 for 5 times, replace the new ITO companion film, and continue running for 10 runs with 18 companion films.

[0038] Embodiment 2 The embodiment of the present invention also provides a method for resuming a rapid annealing furnace. The method for resuming a rapid annealing furnace provided in the embodiment of the present invention is substantially the same as the method for resuming a rapid annealing furnace provided in the first embodiment, except that: The number of accompanying films is 27, and the run is repeated until 15 runs.

[0039] Embodiment 3 The embodiment of the present invention also provides a method for resuming a rapid annealing furnace. The method for resuming a rapid annealing furnace provided in the embodiment of the present invention is substantially the same as the method for resuming a rapid annealing furnace provided in the first embodiment, except that: The number of accompanying films is 36, and the run is repeated until 20 runs.

[0040] Embodiment 4 The embodiment of the present invention also provides a method for resuming a rapid annealing furnace. The method for resuming a rapid annealing furnace provided in the embodiment of the present invention is substantially the same as the method for resuming a rapid annealing furnace provided in the first embodiment, except that: The number of accompanying films is 45, and the runs are repeated until 25 runs.

[0041] In order to compare with the above-mentioned embodiment of the present invention, the embodiment of the present invention also provides the following comparative example.

[0042] Comparative Example 1 The comparative example of the present invention also proposes a method for resuming a rapid annealing furnace. The difference between the method for resuming a rapid annealing furnace in this comparative example and the method for resuming a rapid annealing furnace in Example 1 is that: The number of accompanying films is 54, and the run is repeated until 30 runs.

[0043] Comparative Example 2 The comparative example of the present invention also proposes a method for resuming a rapid annealing furnace. The difference between the method for resuming a rapid annealing furnace in this comparative example and the method for resuming a rapid annealing furnace in Example 1 is that: The number of accompanying films is 63, and the run is repeated until 35 runs: Please refer to the following Table 1, which shows the parameters corresponding to the above-mentioned Embodiments 1 to 4 and Comparative Examples 1 to 2 of the present invention.

[0044] Table 1

[0045] It can be clearly seen that the temperature of the cavity heating function of the rapid annealing furnace is calibrated; the rapid annealing furnace is run dry using the mass production program, and then an ITO film layer of a preset thickness is deposited on the companion film used for the annealing furnace restart; the companion films are placed one by one on the carrier of the rapid annealing furnace and processed under the set conditions to restore the environment of the cavity in the annealing furnace; the steps of placing the companion films one by one on the carrier of the rapid annealing furnace and processing under the set conditions are repeated for a preset number of times, and then the companion films are replaced and processed again under the set conditions until the companion run is completed. The RTA cavity environment is restored quickly and effectively, instead of changing the process parameters and increasing the heating lamp load to put the cavity in an abnormal overload state, resulting in cavity instability. The problem of the rapid annealing furnace temperature calibration method in the prior art causing the cavity environment to be unstable, the heating lamp failure due to excessive load, and finally the need to replace the cavity, which is costly, is solved.

[0046] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A method for re-operating a rapid annealing furnace. It is characterized in that The method comprises: Calibrate the temperature of the cavity heating function of the rapid annealing furnace; The rapid annealing furnace is run empty using a mass production program, and then an ITO film layer of a preset thickness is deposited on a companion sheet used for re-running the annealing furnace; Placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions to restore the environment of the cavity of the annealing furnace; Repeat the steps of placing the accompanying sheets one by one on the carrier of the rapid annealing furnace and performing the setting treatment under the setting conditions for a preset number of times, and then replace the accompanying sheets and perform the setting treatment under the setting conditions again until the accompanying process is completed.

2. The method for resuming the rapid annealing furnace according to claim 1, It is characterized in that The thickness of the ITO film layer is 10000Å~12000Å.

3. The method for resuming the rapid annealing furnace according to claim 1, It is characterized in that The step of placing the companion sheets one by one on the carrier of the rapid annealing furnace and performing setting treatment under set conditions to restore the environment of the cavity of the annealing furnace includes: The cavity is evacuated to a preset pressure, and then the cavity is purged with nitrogen gas at a preset flow rate; After the nitrogen purge stops, the chamber is evacuated again to a preset pressure, and the chamber is preheated after the chamber temperature is raised to a first preset temperature; The chamber is heated to a second preset temperature, a preset flow rate of oxygen is introduced for a preset time, and then an excess amount of oxygen is introduced; The vacuum pump valve is closed, and nitrogen gas with a preset flow rate is introduced for cooling. When the temperature is cooled to a third preset temperature, the carrier is removed from the cavity.

4. The method for resuming the rapid annealing furnace according to claim 3, It is characterized in that The preset pressure is 0.05torr~0.1torr.

5. The method for resuming the rapid annealing furnace according to claim 3, It is characterized in that The first preset temperature is 190°C~210°C, the second preset temperature is 540°C~560°C, and the third preset temperature is 300°C~350°C.

6. The method for resuming a rapid annealing furnace according to claim 3, It is characterized in that In the step of evacuating the cavity to a preset pressure and then purging the cavity with nitrogen at a preset flow rate, the nitrogen flow rate is 3L / min~8L / min.

7. The method for resuming a rapid annealing furnace according to claim 3, It is characterized in that In the step of heating the chamber to a second preset temperature, introducing a preset flow rate of oxygen for a preset time, and then introducing an excess amount of oxygen, the oxygen introduction flow rate is 4 sccm to 5 sccm.

8. The method for resuming a rapid annealing furnace according to claim 3, It is characterized in that In the step of closing the vacuum pump valve, introducing nitrogen gas with a preset flow rate for cooling, and removing the carrier from the cavity when the temperature is cooled to a third preset temperature: The flow rate of cooling nitrogen is 95~100L / min, and the cooling temperature is 300~350℃.

9. The method for resuming a rapid annealing furnace according to claim 1, It is characterized in that Before the step of calibrating the temperature of the cavity heating function of the rapid annealing furnace, the following steps are also included: The quartz cover plate of the rapid annealing furnace is removed, and it is soaked in hydrochloric acid of a preset concentration and then rinsed clean; The quartz cover plate is baked in an oven to ensure that the quartz cover plate is dry, and then installed in the rapid annealing furnace.