Optimization control method and system for production process parameters of alloy tungsten wire diamond fretsaw

By layering the monitoring and control of the pH value and temperature of the nickel-plated electrolyte in the diamond wire saw production process, the problem of low degree of refined production control is solved, and more accurate pH value control and production quality improvement is achieved.

CN118957724AInactive Publication Date: 2024-11-15JIANGSU RESOURCE FUSION SOLAR TECHNOLOGY CO LTD

Patent Information

Application Number
CN202411411691.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-11
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing diamond wire saw production process is incomplete and the degree of refined production control is low, resulting in poor production quality.

Method used

The optimization control method of alloy tungsten wire diamond wire saw production process parameters is adopted. The PH data of nickel-plating electrolyte is obtained through the preset time length. After judging the abnormal pH value, first determine whether it is caused by the abnormal temperature. If so, the cooling will be reduced and the control will be adjusted. If otherwise Adjust the pH value within the normal range through acid and alkaline solution.

Benefits of technology

Accurate pH control of nickel-plating electrolyte is achieved, production quality and control accuracy are improved, acid and alkaline liquids are saved, and the impact on tungsten wire substrate is avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957724A_ABST
    Figure CN118957724A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of diamond fretsaws, in particular to an optimal control method and system for production process parameters of an alloy tungsten wire diamond fretsaw. The method comprises the following steps: acquiring nickel plating electrolyte PH data of each nickel plating electrolyte layer in a nickel plating solution tank in a tungsten wire diamond fretsaw production line according to a preset time length based on each preset PH monitoring sensor, judging whether a nickel plating electrolyte layer with an abnormal PH value exists or not, and if the nickel plating electrolyte layer with the abnormal PH value exists, judging whether the nickel plating electrolyte layer with the abnormal PH value exists or not; if yes, electrolyte temperature data corresponding to the nickel plating electrolyte layer with the abnormal PH value are obtained, and whether the PH value is abnormal due to temperature abnormality or not is judged; if yes, the nickel plating electrolyte layer with the abnormal PH value is cooled until the PH value of the nickel plating electrolyte layer with the abnormal PH value is converted to be normal; and if not, PH adjustment is conducted till the PH value of the nickel plating electrolyte layer with the abnormal PH value is converted to be normal. According to the invention, parameter optimization of the production process of the alloy tungsten wire diamond fretsaw is realized, and the production quality and the control precision are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of diamond wire saws, and in particular to an optimization control method and system for production process parameters of alloy tungsten wire diamond wire saws. Background Art

[0002] Diamond wire saw, also known as diamond wire, refers to the method of fixing diamond abrasive on metal wire by electroplating process or resin bonding.

[0003] At present, more and more emerging technologies have been applied to the production monitoring and control of diamond wire saws. For example, the patent with publication number CN205920378U discloses a real-time monitoring system for the electroplating liquid of a diamond wire saw production line, including an electroplating liquid tank, a pH sensor, a data analysis device, and an alarm device, wherein the pH sensor is arranged inside the electroplating liquid tank, in direct contact with the electroplating liquid in the electroplating liquid tank, and is used to monitor the pH value of the electroplating liquid and output a pH value data signal; the data analysis device is connected to the pH sensor, receives the pH value data signal output by the pH sensor, and outputs a control signal after calculation and analysis; the alarm device is connected to the data analysis device, receives the control signal and alarms. The utility model adds a real-time monitoring system for the electroplating liquid to the diamond wire saw production line, which can monitor the changes in various parameters of the electroplating liquid and alarm according to the changes; it has an emergency shutdown function, which can automatically control the shutdown of the production line; it has an electroplating liquid parameter feedback adjustment device, which can automatically adjust the electroplating liquid parameters to return to normal values.

[0004] Although the technical solution in the above patent document can realize monitoring during the production process of tungsten diamond wire saws, it still has problems such as incomplete monitoring, low level of refinement of production control, and low accuracy of production process parameter monitoring and control, which in turn affects the production quality of diamond wire saws. Summary of the invention

[0005] Based on this, it is necessary to provide an optimization control method and system for the production process parameters of alloy tungsten wire diamond wire saws, which can improve the parameter control in the production process of tungsten wire diamond wire saws and achieve precise and refined control, in response to the above technical problems.

[0006] The technical solution of the present invention is as follows:

[0007] An optimization control method for production process parameters of alloy tungsten wire diamond wire saw, the method comprising: Acquire the nickel-plated electrolyte PH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on the preset time length and the preset PH monitoring sensors, and judge whether there is a nickel-plated electrolyte layer with an abnormal PH value according to the nickel-plated electrolyte PH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte PH data within one of the preset time lengths; If it is determined that there is a nickel-plated electrolyte layer with an abnormal pH value, then obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data; If the judgment is yes, an emergency temperature control instruction is generated, and a preset electrolyte cooling device is controlled according to the emergency temperature control instruction to cool the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal; If the judgment is no, an acid-base solution control instruction is generated, and the preset electrolyte PH adjustment device is controlled according to the acid-base solution control instruction to adjust the PH value of the nickel-plated electrolyte layer with abnormal PH value until the PH value of the nickel-plated electrolyte layer with abnormal PH value is converted to normal.

[0008] Optionally, judging whether there is a nickel plating electrolyte layer with an abnormal pH value according to the nickel plating electrolyte pH data includes: Extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Determine whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with an abnormal pH value.

[0009] Optionally, obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data, includes: Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with an abnormal pH value; Obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Determining whether the pH growth value is within the target pH value variation range; If the answer is yes, it is determined that the abnormal temperature causes the abnormal pH value.

[0010] Optionally, judging whether there is a nickel plating electrolyte layer with an abnormal pH value according to the nickel plating electrolyte pH data further includes: If it is determined that there is no nickel plating electrolyte solution layer with abnormal pH value, then the electrolyte pH fluctuation value of the corresponding nickel plating electrolyte layer is calculated according to each of the nickel plating electrolyte pH data, wherein one nickel plating electrolyte pH data corresponds to one electrolyte pH fluctuation value; Obtain the pre-stored acceptable range of electrolyte pH fluctuation; Comparing each of the electrolyte pH fluctuation values ​​with the electrolyte pH fluctuation qualified range, and screening out the electrolyte pH fluctuation values ​​that are not within the electrolyte pH fluctuation qualified range, and setting the nickel-plating electrolyte layer corresponding to the screened electrolyte pH fluctuation value as the nickel-plating electrolyte layer with abnormal pH value fluctuation; The nickel plating electrolyte layer with abnormal pH value fluctuation is regulated according to the preset pH value fluctuation regulation steps.

[0011] Optionally, the preset time length includes multiple monitoring time points; Calculate the pH fluctuation value of the corresponding nickel plating electrolyte layer according to the pH data of the nickel plating electrolyte, including: Extracting the real-time electrolyte pH value monitored at each monitoring time point in the nickel plating electrolyte pH data; Calculating the actual pH difference between each of the real-time electrolyte pH values ​​and the pre-stored electrolyte pH intermediate value; Screening out the real-time electrolyte pH value corresponding to the actual pH difference value that is greater than or equal to the standard pH difference value, and recording it as the electrolyte marked pH value, wherein the number of the electrolyte marked pH values ​​is multiple; The electrolyte pH fluctuation value is generated according to each of the real-time electrolyte pH values ​​and each of the electrolyte marked pH values ​​based on the following formula: ; Where, F is the pH fluctuation value of the electrolyte, is the first weight coefficient, PHi is the i-th real-time electrolyte pH value in the nickel plating electrolyte pH data, PHmid is the electrolyte pH intermediate value, n is the number of real-time electrolyte pH values, PHsmax is the pre-stored standard pH maximum value, PHsmin is the pre-stored standard pH minimum value, is the second weight coefficient, PHj is the jth electrolyte marked PH value in the nickel plating electrolyte PH data, PHse is the pre-stored compensation PH value, and N is the number of electrolyte marked PH values.

[0012] Optionally, an optimization control system for production process parameters of alloy tungsten wire diamond wire saw is also provided, the system comprising: An abnormal electrolyte layer judgment module is used to obtain nickel-plated electrolyte PH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on preset time lengths and preset PH monitoring sensors, and judge whether there is a nickel-plated electrolyte layer with abnormal PH value according to the nickel-plated electrolyte PH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte PH data within one of the preset time lengths; The electrolyte temperature troubleshooting module is used to obtain electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value if it is determined that there is a nickel-plated electrolyte layer with abnormal pH value, and determine whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data; an electrolyte temperature control module, for generating an emergency temperature control instruction if the judgment is yes, and controlling a preset electrolyte cooling device to cool the nickel-plated electrolyte layer with an abnormal pH value according to the emergency temperature control instruction until the pH value of the nickel-plated electrolyte layer with an abnormal pH value is converted to normal; The electrolyte acid-base adjustment module is used to generate an acid-base solution adjustment instruction if the judgment is no, and control a preset electrolyte pH adjustment device according to the acid-base solution adjustment instruction to adjust the pH of the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal.

[0013] Optionally, the abnormal electrolyte layer judgment module is further used for: Extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Determine whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with an abnormal pH value.

[0014] Optionally, the electrolyte temperature checking module is further used for: Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with an abnormal pH value; Obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Determining whether the pH growth value is within the target pH value variation range; If the answer is yes, it is determined that the abnormal temperature causes the abnormal pH value.

[0015] Optionally, the optimization control system of the alloy tungsten wire diamond wire saw production process parameters also includes an electrolyte PH fluctuation monitoring module, which is used to: if it is determined that there is no nickel-plated electrolyte solution layer with abnormal PH value, then calculate the electrolyte PH fluctuation value of the corresponding nickel-plated electrolyte layer according to each of the nickel-plated electrolyte PH data, wherein one of the nickel-plated electrolyte PH data corresponds to one electrolyte PH fluctuation value; obtain a pre-stored electrolyte PH fluctuation qualified range; compare each of the electrolyte PH fluctuation values ​​with the electrolyte PH fluctuation qualified range, and screen out the electrolyte PH fluctuation values ​​that are not within the electrolyte PH fluctuation qualified range, and set the nickel-plated electrolyte layer corresponding to the screened electrolyte PH fluctuation value as the nickel-plated electrolyte layer with abnormal PH value fluctuation; and regulate the nickel-plated electrolyte layer with abnormal PH value fluctuation according to a preset PH value fluctuation adjustment step.

[0016] Optionally, the preset time length includes multiple monitoring time points; the electrolyte PH fluctuation monitoring module is used to: extract the real-time electrolyte PH value monitored at each monitoring time point in the nickel plating electrolyte PH data; Calculating the actual pH difference between each of the real-time electrolyte pH values ​​and the pre-stored electrolyte pH intermediate value; Screening out the real-time electrolyte pH value corresponding to the actual pH difference value that is greater than or equal to the standard pH difference value, and recording it as the electrolyte marked pH value, wherein the number of the electrolyte marked pH values ​​is multiple; The electrolyte pH fluctuation value is generated according to each of the real-time electrolyte pH values ​​and each of the electrolyte marked pH values ​​based on the following formula: ; Where, F is the pH fluctuation value of the electrolyte, is the first weight coefficient, PHi is the i-th real-time electrolyte pH value in the nickel plating electrolyte pH data, PHmid is the electrolyte pH intermediate value, n is the number of real-time electrolyte pH values, PHsmax is the pre-stored standard pH maximum value, PHsmin is the pre-stored standard pH minimum value, is the second weight coefficient, PHj is the jth electrolyte marked PH value in the nickel plating electrolyte PH data, PHse is the pre-stored compensation PH value, and N is the number of electrolyte marked PH values.

[0017] A computer device comprises a memory and a processor, wherein the memory stores a computer program, and the processor implements the steps of the above-mentioned method for optimizing the production process parameters of alloy tungsten wire diamond wire saw when executing the computer program.

[0018] A computer-readable storage medium stores a computer program, which, when executed by a processor, implements the steps of the above-mentioned method for optimizing the production process parameters of a tungsten alloy diamond wire saw.

[0019] The technical effects achieved by the present invention are as follows: The above-mentioned optimization control method and system for the production process parameters of alloy tungsten diamond wire saw, in order to finely monitor the pH value of the electrolyte, adopts data segmentation according to time periods, specifically, presetting a preset time length, and on the other hand, also stratifies the nickel-plated electrolyte in the nickel-plated solution tank in the tungsten diamond wire saw production line, specifically, delineating multiple nickel-plated electrolyte layers, so that more refined monitoring and production parameter control can be achieved by obtaining the pH value of the nickel-plated electrolyte in different layers, specifically, by obtaining the pH value of the tungsten diamond wire saw production line based on the preset pH monitoring sensors according to the preset time length. The PH data of the nickel-plated electrolyte of each nickel-plated electrolyte layer in the nickel-plated solution tank in the production line is then used to determine whether there is a nickel-plated electrolyte layer with an abnormal PH value. When it is determined that there is a nickel-plated electrolyte layer with an abnormal PH value, an acid or alkaline liquid is not directly injected to adjust the PH value, but it is first determined whether the abnormal PH value is caused by the temperature change in the nickel-plated electrolyte. Specifically, the electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal PH value is obtained, wherein the temperature-related data is collected by a technician in the field installing a temperature monitoring sensor next to the PH monitoring sensor. Then, it is determined whether the abnormal PH value is caused by abnormal temperature based on the electrolyte temperature data. Compared with the prior art, when adjusting the nickel-plated electrolyte, the effect of temperature on the PH value is ignored and the acid or alkaline liquid is directly injected for PH adjustment, which is easy to cause inaccurate adjustment. The present application takes into account the effect of temperature on the PH value and thus achieves more accurate PH regulation. When the pH value is abnormal due to temperature increase, the pH value of the nickel-plating electrolyte can be basically returned to a normal state by simply adjusting the temperature. At this time, there is no need to directly add acid or alkaline liquid to adjust the pH as in the prior art. In addition, for the case of abnormal temperature and abnormal pH value, the prior art requires the injection of acid or alkaline liquid and the temperature reduction control. In the present application, when it is determined that the pH abnormality is caused by temperature, only temperature reduction control is required, and there is no need to inject acid or alkaline liquid. On the one hand, it saves acid or alkaline liquid used to adjust the pH value, and on the other hand, it achieves precise pH value control to ensure that the pH value of the nickel-plating electrolyte will not affect the production of the tungsten wire substrate.Furthermore, when it is determined that the abnormal pH value is caused by abnormal temperature, an emergency temperature control instruction is generated, and the preset electrolyte cooling device is controlled according to the emergency temperature control instruction to cool the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal; if it is determined that the abnormal pH value is not caused by abnormal temperature, the temperature and pH value need to be regulated separately at this time, specifically, an acid-base solution control instruction is generated, and the preset electrolyte pH adjustment device is controlled according to the acid-base solution control instruction to adjust the pH of the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal, thereby taking into account the influence of temperature on pH value when abnormal pH value of the nickel-plated electrolyte layer is detected, and adjusting pH value based on this, which saves solution for adjusting pH value compared with the prior art and realizes precise control of pH value of nickel-plated electrode solution, thereby optimizing parameters of alloy tungsten wire diamond wire saw production process and improving production quality and control accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 A schematic flow chart of an optimization control method for production process parameters of alloy tungsten diamond wire saws in one embodiment; Figure 2 It is a structural block diagram of an optimization control system for production process parameters of alloy tungsten diamond wire saw in one embodiment. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0022] In one embodiment, Figure 1 As shown, a method for optimizing and controlling the production process parameters of a tungsten alloy diamond wire saw is provided, the method comprising: Step S100: Acquire the nickel-plated electrolyte pH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on the preset time length and the preset pH monitoring sensors, and determine whether there is a nickel-plated electrolyte layer with an abnormal pH value according to the nickel-plated electrolyte pH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte pH data within one of the preset time lengths; In this embodiment, the nickel-plated electrolyte layer is first delineated, which is specifically achieved by setting the installation position of the PH monitoring sensor in the nickel-plated solution tank and the data collection path of the PH monitoring sensor. The PH monitoring sensors are arranged longitudinally at equal intervals from the top of the tank wall of the nickel-plated solution tank downward. The PH monitoring sensor is also connected to a lateral pushing device, which drives the PH monitoring sensor to move linearly along the lateral direction of the nickel-plated solution tank and collects data on the PH value. The area formed by expanding outward a certain distance with the lateral movement route of the PH monitoring sensor as the center line is a nickel-plated electrolyte layer, wherein the certain distance does not need to be set and can be obtained based on the PH monitoring sensor used. Alternatively, it can be understood that the nickel-plated electrolyte layer may not have a very strict regional division, but is delineated based on the PH data monitored by each PH monitoring sensor during the movement. For example, if the number of the PH monitoring sensors is 3, the number of the nickel-plated electrolyte layers is 4. On the other hand, by setting the lateral pushing device to drive the movement of the pH monitoring sensor, it also has a part of the function of stirring the electrolyte, so that the electrolyte is more mixed. In addition, the pH data monitored based on the more mixed electrolyte can better feedback the actual pH data of the electrolyte, thereby providing accurate data for the precise control of the pH, which is conducive to the subsequent precise and refined control of the pH.

[0023] In addition, the lateral pushing device may adopt a cylinder plus push rod structure, or other structures, and may be actually set up by technicians in the production process. This application does not make any specific limitations on this.

[0024] Step S200: if it is determined that there is a nickel-plated electrolyte layer with an abnormal pH value, then obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data; Step S300: if the judgment is yes, an emergency temperature control instruction is generated, and according to the emergency temperature control instruction, a preset electrolyte cooling device is controlled to cool the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal; In this embodiment, the electrolyte cooling device includes but is not limited to a water pipe disposed in the nickel plating solution tank, and the execution of the emergency temperature control instruction includes but is not limited to passing cold water into the water pipe to cool down or passing warm water into the water pipe to heat up. At the same time, when executing the emergency temperature control instruction, real-time PH monitoring is also performed until the PH value of the nickel plating electrolyte layer with abnormal PH value is converted to normal. Specifically, when the PH value of the electrolyte is within the pre-stored normal PH value range, it is judged to be normal, otherwise it is abnormal.

[0025] Step S400: If the judgment is no, an acid-base solution control instruction is generated, and a preset electrolyte PH adjustment device is controlled according to the acid-base solution control instruction to adjust the PH value of the nickel-plated electrolyte layer with abnormal PH value until the PH value of the nickel-plated electrolyte layer with abnormal PH value is converted to normal.

[0026] In this step, if the judgment is no, that is, it is judged that the temperature has no effect on the pH value, then a conventional acid or alkaline liquid is introduced for adjustment, specifically, the pH value of the nickel-plated electrolyte layer with abnormal pH value is adjusted by controlling a preset electrolyte pH adjustment device until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal. The electrolyte pH adjustment device includes but is not limited to an acidic or alkaline liquid injection device.

[0027] In this embodiment, in order to monitor the pH value of the electrolyte in a refined manner, data segmentation is performed according to time periods, specifically, a preset time length is pre-set. On the other hand, the nickel-plated electrolyte in the nickel-plated solution tank in the tungsten diamond wire saw production line is layered, specifically, a plurality of nickel-plated electrolyte layers are delineated. In this way, more refined monitoring and production parameter control are achieved by obtaining the pH values ​​of the nickel-plated electrolytes in different layers. Specifically, the pH values ​​of the nickel-plated electrolytes in the nickel-plated solution tank in the tungsten diamond wire saw production line are obtained based on the preset pH monitoring sensors according to the preset time length. The nickel-plated electrolyte PH data of the nickel electrolyte layer, and then judging whether there is a nickel-plated electrolyte layer with abnormal PH value according to the nickel-plated electrolyte PH data, when judging that there is a nickel-plated electrolyte layer with abnormal PH value, do not directly inject acid or alkaline liquid to adjust PH, but first judge whether the abnormal PH value is caused by the temperature change in the nickel-plated electrolyte, specifically by obtaining the electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal PH value, wherein the temperature-related data is collected by a technician in the field of technology installing a temperature monitoring sensor next to the PH monitoring sensor. Then, judging whether the abnormal PH value is caused by abnormal temperature according to the electrolyte temperature data, compared with the prior art of adjusting the nickel-plated electrolyte, ignoring the effect of temperature on PH value and directly injecting acid or alkaline liquid for PH adjustment, which is easy to cause inaccurate adjustment, the present application takes into account the effect of temperature on PH value and thus achieves more accurate PH regulation. When the pH value is abnormal due to temperature increase, the pH value of the nickel-plating electrolyte can be basically returned to a normal state by simply adjusting the temperature. At this time, there is no need to directly add acid or alkaline liquid to adjust the pH as in the prior art. In addition, for the case of abnormal temperature and abnormal pH value, the prior art requires the injection of acid or alkaline liquid and the temperature reduction control. In the present application, when it is determined that the pH abnormality is caused by temperature, only temperature reduction control is required, and there is no need to inject acid or alkaline liquid. On the one hand, it saves acid or alkaline liquid used to adjust the pH value, and on the other hand, it achieves precise pH value control to ensure that the pH value of the nickel-plating electrolyte will not affect the production of the tungsten wire substrate. Furthermore, when it is determined that the abnormal pH value is caused by abnormal temperature, an emergency temperature control instruction is generated, and the preset electrolyte cooling device is controlled according to the emergency temperature control instruction to cool the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal; if it is determined that the abnormal pH value is not caused by abnormal temperature, the temperature and pH value need to be regulated separately at this time, specifically, an acid-base solution control instruction is generated, and the preset electrolyte pH adjustment device is controlled according to the acid-base solution control instruction to adjust the pH of the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal.

[0028] Therefore, in the present invention, when an abnormal pH value of the nickel-plated electrolyte layer is detected, the influence of temperature on the pH value is considered and the pH value is regulated based on this. Compared with the prior art, the solution used to adjust the pH value is saved and the precise regulation of the pH value of the nickel-plated electrode liquid is achieved, thereby optimizing the parameters of the alloy tungsten wire diamond wire saw production process and improving the production quality and control accuracy.

[0029] It should be noted that the present application is directed to a nickel plating solution to which a certain buffer solution is added. The buffer solution can help offset part of the pH change caused by temperature, and if the pH changes due to an increase in temperature, the pH can return to its original state if the temperature is lowered.

[0030] In another embodiment, judging whether there is a nickel plating electrolyte layer with an abnormal pH value according to the nickel plating electrolyte pH data includes: Step S111: extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Step S112: determining whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; Step S113: If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with abnormal pH value.

[0031] In this embodiment, the actual maximum pH value and the actual minimum pH value in each of the nickel-plating electrolyte PH data are first extracted, and then it is determined whether any one of the actual maximum pH value and the actual minimum pH value corresponding to each nickel-plating electrolyte PH data exceeds the pre-stored normal PH value range. That is, if the actual maximum pH value or the actual minimum pH value exceeds the pre-stored normal PH value range, the corresponding nickel-plating electrolyte PH data is judged to be abnormal, that is, the corresponding nickel-plating electrolyte layer has an abnormal PH value, that is, it is determined that the PH value of the corresponding nickel-plating electrolyte layer at this time is not conducive to the production of tungsten diamond wire saws.

[0032] Furthermore, the actual maximum pH value and the actual minimum pH value may be the last time point within the preset time length, or may be a time point distributed in the middle of the preset time length, that is, as long as there is a pH value outside the normal pH value range, it is judged to be abnormal.

[0033] In another embodiment, obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data, includes: Step S210: obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with abnormal pH value; Step S220: obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Step S230: Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Step S240: determining whether the pH growth value is within the target pH value variation range; Step S250: If the answer is yes, it is determined that the abnormal pH value is caused by abnormal temperature.

[0034] In this embodiment, the electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value is first obtained, the current temperature change difference is obtained according to the electrolyte temperature data, and the pH growth value is generated according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with abnormal pH value, the initial state pH value is the pH value corresponding to the nickel-plated electrolyte pH data at the starting time point of the preset time length, then, the actual use time of each nickel-plated electrolyte layer in the nickel-plating solution tank is obtained, and the corresponding temperature change data is obtained according to the actual use time. Since the nickel-plated electrolyte layers with different use times are affected by temperature to different degrees, the pH value change data of the nickel-plated electrolyte layers with different use times after temperature change are pre-determined and stored, that is, one actual use time corresponds to one temperature change data, for example, the change of pH value of the nickel-plated electrolyte used for 1 hour and the nickel-plated electrolyte used for 3 hours is different when the temperature changes by 5 degrees Celsius, so the influence of temperature on the electrolyte can be accurately judged by setting multiple temperature change data. Furthermore, the standard temperature variation difference is not limited to the exemplified 5 degrees Celsius, but also includes other temperatures. Different standard temperature variation differences have different effects on the pH value, so each standard temperature variation difference corresponds to a pH value variation range. Next, the current temperature variation difference is compared with each standard temperature variation difference in the corresponding temperature variation data, and the standard temperature variation difference matching the current temperature variation difference is screened out, wherein the pH value variation range corresponding to the screened standard temperature variation difference is the target pH value variation range. If it is judged that the pH growth value is within the target pH value variation range, it is judged that the pH value abnormality is caused by abnormal temperature. If it is judged that the pH growth value is not within the target pH value variation range, it can be judged that the pH value is not affected by temperature, and then the pH value control is adjusted by injecting acid or alkaline liquid.

[0035] In another embodiment, judging whether there is a nickel plating electrolyte layer with an abnormal pH value according to the nickel plating electrolyte pH data further includes: Step S510: if it is determined that there is no nickel plating electrolyte solution layer with abnormal pH value, then the electrolyte pH fluctuation value of the corresponding nickel plating electrolyte layer is calculated according to each of the nickel plating electrolyte pH data, wherein one nickel plating electrolyte pH data corresponds to one electrolyte pH fluctuation value; Step S520: obtaining a pre-stored acceptable range of pH fluctuation of the electrolyte; Step S530: comparing each of the electrolyte pH fluctuation values ​​with the electrolyte pH fluctuation qualified range, and screening out the electrolyte pH fluctuation values ​​that are not within the electrolyte pH fluctuation qualified range, and setting the nickel-plating electrolyte layer corresponding to the screened electrolyte pH fluctuation value as the nickel-plating electrolyte layer with abnormal pH fluctuation; Step S540: regulating the nickel plating electrolyte layer with abnormal pH value fluctuation according to a preset pH value fluctuation regulation step.

[0036] In this embodiment, when it is determined that there is no nickel-plated electrolyte solution layer with abnormal pH value, it means that there is no obvious pH abnormality at this time, but large pH fluctuations will also affect the production of tungsten diamond wire saws, such as causing uneven coating, rough surface or other defects. Therefore, in order to more accurately control the production process of tungsten diamond wire saws to improve production quality, the electrolyte pH fluctuation value is calculated, and then the pre-stored electrolyte pH fluctuation qualified range is obtained. Then, each electrolyte pH fluctuation value is compared with the electrolyte pH fluctuation qualified range, and the electrolyte pH fluctuation value that is not within the electrolyte pH fluctuation qualified range is screened out, and the nickel-plated electrolyte layer corresponding to the screened electrolyte pH fluctuation value is set as the nickel-plated electrolyte layer with abnormal pH fluctuation; finally, the nickel-plated electrolyte layer with abnormal pH fluctuation is regulated according to the preset pH fluctuation adjustment steps.

[0037] Furthermore, the pH value fluctuation adjustment step includes an electrolyte stirring control step. Specifically, when executing the electrolyte stirring control step, the nickel plating solution tank is stirred by controlling the electrolyte stirring device to fully stir the nickel plating electrolyte in the nickel plating solution tank.

[0038] In another embodiment, the pH value fluctuation adjustment step includes a production shutdown detection step. When the production shutdown detection step is executed, the tungsten diamond wire saw production line is controlled to stop production, and the nickel plating electrolyte is sampled. The sampled nickel plating electrolyte is analyzed by the production line management body, so that the production line management body can perform cause analysis.

[0039] In another embodiment, the pH value fluctuation adjustment step includes an electrolyte replacement step. When the electrolyte replacement step is performed, the tungsten diamond wire saw production line is controlled to stop production and the electrolyte is replaced with a new electrolyte.

[0040] It should be noted that the pH value fluctuation adjustment step can be one of the above steps or a combined step, such as a combination of an electrolyte agitation control step and a production shutdown detection step, that is, the electrolyte agitation control step is performed first, and then the production shutdown detection step is performed.

[0041] Of course, the above steps are only examples, and there may be other steps in actual production as long as the problem of large pH value fluctuations can be solved.

[0042] In another embodiment, the preset time length includes a plurality of monitoring time points;

[0043] Calculate the pH fluctuation value of the corresponding nickel plating electrolyte layer according to the pH data of the nickel plating electrolyte, including: Step S511: extracting the real-time electrolyte pH value monitored at each monitoring time point in the nickel plating electrolyte pH data; Step S512: Calculating the actual pH difference between each of the real-time electrolyte pH values ​​and the pre-stored electrolyte pH intermediate value; Step S513: Screening out the real-time electrolyte pH value corresponding to the actual pH difference value that is greater than or equal to the standard pH difference value, and recording it as the electrolyte marked pH value, wherein the number of the electrolyte marked pH values ​​is multiple; Step S514: Generate an electrolyte pH fluctuation value according to each of the real-time electrolyte pH values ​​and each of the electrolyte marked pH values ​​based on the following formula: ; Where, F is the pH fluctuation value of the electrolyte, is the first weight coefficient, PHi is the i-th real-time electrolyte pH value in the nickel plating electrolyte pH data, PHmid is the electrolyte pH intermediate value, n is the number of real-time electrolyte pH values, PHsmax is the pre-stored standard pH maximum value, PHsmin is the pre-stored standard pH minimum value, is the second weight coefficient, PHj is the jth electrolyte marked PH value in the nickel plating electrolyte PH data, PHse is the pre-stored compensation PH value, and N is the number of electrolyte marked PH values.

[0044] In this embodiment, in order to achieve more accurate monitoring of the pH value in the nickel-plating electrolyte layer and then make a judgment by calculating the pH fluctuation value of the electrolyte, specifically all real-time electrolyte pH values ​​and electrolyte marked pH values ​​are taken into account, and the electrolyte pH fluctuation value is comprehensively generated, so that the electrolyte pH fluctuation value is used to characterize the degree of fluctuation change of the nickel-plating electrolyte within a preset time length, and then the electrolyte pH fluctuation value is used to realize the judgment of whether the pH data of the nickel-plating electrolyte will have an abnormal trend based on the monitored pH data.

[0045] In another embodiment, if Figure 2 As shown, an optimization control system for production process parameters of alloy tungsten wire diamond wire saw is provided, and the system comprises: An abnormal electrolyte layer judgment module is used to obtain nickel-plated electrolyte PH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on preset time lengths and preset PH monitoring sensors, and judge whether there is a nickel-plated electrolyte layer with abnormal PH value according to the nickel-plated electrolyte PH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte PH data within one of the preset time lengths; The electrolyte temperature troubleshooting module is used to obtain electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value if it is determined that there is a nickel-plated electrolyte layer with abnormal pH value, and determine whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data;

[0046] an electrolyte temperature control module, for generating an emergency temperature control instruction if the judgment is yes, and controlling a preset electrolyte cooling device to cool the nickel-plated electrolyte layer with an abnormal pH value according to the emergency temperature control instruction until the pH value of the nickel-plated electrolyte layer with an abnormal pH value is converted to normal; The electrolyte acid-base adjustment module is used to generate an acid-base solution adjustment instruction if the judgment is no, and control a preset electrolyte pH adjustment device according to the acid-base solution adjustment instruction to adjust the pH of the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal.

[0047] In another embodiment, the abnormal electrolyte layer determination module is further used for: Extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Determine whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with an abnormal pH value.

[0048] In another embodiment, the electrolyte temperature checking module is further used for: Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with an abnormal pH value; Obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Determining whether the pH growth value is within the target pH value variation range; If the answer is yes, it is determined that the abnormal temperature causes the abnormal pH value.

[0049] In another embodiment, the optimization control system for the production process parameters of the alloy tungsten diamond wire saw further includes an electrolyte pH fluctuation monitoring module; The electrolyte PH fluctuation monitoring module is used for: if it is determined that there is no nickel-plated electrolyte solution layer with abnormal PH value, then the electrolyte PH fluctuation value of the corresponding nickel-plated electrolyte layer is calculated according to each of the nickel-plated electrolyte PH data, wherein one of the nickel-plated electrolyte PH data corresponds to one electrolyte PH fluctuation value; obtaining a pre-stored electrolyte PH fluctuation qualified range; comparing each of the electrolyte PH fluctuation values ​​with the electrolyte PH fluctuation qualified range, and screening out the electrolyte PH fluctuation values ​​that are not within the electrolyte PH fluctuation qualified range, and setting the nickel-plated electrolyte layer corresponding to the screened electrolyte PH fluctuation value as the nickel-plated electrolyte layer with abnormal PH value fluctuation; and regulating the nickel-plated electrolyte layer with abnormal PH value fluctuation according to a preset PH value fluctuation adjustment step.

[0050] In another embodiment, the preset time length includes multiple monitoring time points; the electrolyte pH fluctuation monitoring module is used to: extract the real-time electrolyte pH value monitored at each monitoring time point in the nickel plating electrolyte pH data; Calculating the actual pH difference between each of the real-time electrolyte pH values ​​and the pre-stored electrolyte pH intermediate value; Screening out the real-time electrolyte pH value corresponding to the actual pH difference value that is greater than or equal to the standard pH difference value, and recording it as the electrolyte marked pH value, wherein the number of the electrolyte marked pH values ​​is multiple; The electrolyte pH fluctuation value is generated according to each of the real-time electrolyte pH values ​​and each of the electrolyte marked pH values ​​based on the following formula: ; Where, F is the pH fluctuation value of the electrolyte, is the first weight coefficient, PHi is the i-th real-time electrolyte pH value in the nickel plating electrolyte pH data, PHmid is the electrolyte pH intermediate value, n is the number of real-time electrolyte pH values, PHsmax is the pre-stored standard pH maximum value, PHsmin is the pre-stored standard pH minimum value, is the second weight coefficient, PHj is the jth electrolyte marked PH value in the nickel plating electrolyte PH data, PHse is the pre-stored compensation PH value, and N is the number of electrolyte marked PH values.

[0051] In one embodiment, a computer device is also provided, including a memory and a processor, wherein the memory stores a computer program, and when the processor executes the computer program, the steps described in the above-mentioned method for optimizing the production process parameters of the alloy tungsten wire diamond wire saw are implemented.

[0052] A computer-readable storage medium stores a computer program, which, when executed by a processor, implements the steps of the above-mentioned method for optimizing the production process parameters of a tungsten alloy diamond wire saw.

[0053] Those of ordinary skill in the art can understand that all or part of the processes in the above-mentioned embodiment methods can be implemented by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to memory, storage, database or other media used in the embodiments provided in this application may include non-volatile and / or volatile memory. Non-volatile memory may include read-only memory (ROM), programmable ROM (PROM), electrically programmable ROM (EPROM), electrically erasable programmable ROM (EEPROM) or flash memory. Volatile memory may include random access memory (RAM) or external cache memory. By way of illustration and not limitation, RAM is available in many forms, such as static RAM (SRAM), dynamic RAM (DRAM), synchronous DRAM (SDRAM), double data rate SDRAM (DDRSDRAM), enhanced SDRAM (ESDRAM), synchronous link (Synchlink) DRAM (SLDRAM), memory bus (Rambus) direct RAM (RDRAM), direct memory bus dynamic RAM (DRDRAM), and memory bus dynamic RAM (RDRAM), etc.

[0054] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0055] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent of the present application shall be subject to the attached claims.

Claims

1. An optimization control method for production process parameters of alloy tungsten wire diamond wire saw, It is characterized in that The method comprises: Acquire the nickel-plated electrolyte PH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on the preset time length and the preset PH monitoring sensors, and judge whether there is a nickel-plated electrolyte layer with an abnormal PH value according to the nickel-plated electrolyte PH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte PH data within one of the preset time lengths; If it is determined that there is a nickel-plated electrolyte layer with an abnormal pH value, then obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data; If the judgment is yes, an emergency temperature control instruction is generated, and a preset electrolyte cooling device is controlled according to the emergency temperature control instruction to cool the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal; If the judgment is no, an acid-base solution control instruction is generated, and the preset electrolyte PH adjustment device is controlled according to the acid-base solution control instruction to adjust the PH value of the nickel-plated electrolyte layer with abnormal PH value until the PH value of the nickel-plated electrolyte layer with abnormal PH value is converted to normal.

2. The optimization control method for production process parameters of alloy tungsten diamond wire saw according to claim 1, It is characterized in that Judging whether there is a nickel plating electrolyte layer with an abnormal pH value according to the nickel plating electrolyte pH data includes: Extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Determine whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with an abnormal pH value.

3. The optimization control method for production process parameters of alloy tungsten diamond wire saw according to claim 1, It is characterized in that Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value, and determining whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data, including: Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with an abnormal pH value; Obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Determining whether the pH growth value is within the target pH value variation range; If the answer is yes, it is determined that the abnormal temperature causes the abnormal pH value.

4. The method for optimizing and controlling the production process parameters of the alloy tungsten wire diamond wire saw according to claim 1, It is characterized in that Judging whether there is a nickel plating electrolyte layer with abnormal pH value according to the pH data of the nickel plating electrolyte, further comprising: If it is determined that there is no nickel plating electrolyte solution layer with abnormal pH value, then the electrolyte pH fluctuation value of the corresponding nickel plating electrolyte layer is calculated according to each of the nickel plating electrolyte pH data, wherein one nickel plating electrolyte pH data corresponds to one electrolyte pH fluctuation value; Obtain the pre-stored acceptable range of electrolyte pH fluctuation; Comparing each of the electrolyte pH fluctuation values ​​with the electrolyte pH fluctuation qualified range, and screening out the electrolyte pH fluctuation values ​​that are not within the electrolyte pH fluctuation qualified range, and setting the nickel-plating electrolyte layer corresponding to the screened electrolyte pH fluctuation value as the nickel-plating electrolyte layer with abnormal pH value fluctuation; The nickel plating electrolyte layer with abnormal pH value fluctuation is regulated according to the preset pH value fluctuation regulation steps.

5. The method for optimizing and controlling the production process parameters of the alloy tungsten diamond wire saw according to claim 4, It is characterized in that The preset time length includes multiple monitoring time points; Calculate the pH fluctuation value of the corresponding nickel plating electrolyte layer according to the pH data of the nickel plating electrolyte, including: Extracting the real-time electrolyte pH value monitored at each monitoring time point in the nickel plating electrolyte pH data; Calculating the actual pH difference between each of the real-time electrolyte pH values ​​and the pre-stored electrolyte pH intermediate value; Screening out the real-time electrolyte pH value corresponding to the actual pH difference value that is greater than or equal to the standard pH difference value, and recording it as the electrolyte marked pH value, wherein the number of the electrolyte marked pH values ​​is multiple; The electrolyte pH fluctuation value is generated according to each of the real-time electrolyte pH values ​​and each of the electrolyte marked pH values ​​based on the following formula: ; Where, F is the pH fluctuation value of the electrolyte, is the first weight coefficient, PHi is the i-th real-time electrolyte pH value in the nickel plating electrolyte pH data, PHmid is the electrolyte pH intermediate value, n is the number of real-time electrolyte pH values, PHsmax is the pre-stored standard pH maximum value, PHsmin is the pre-stored standard pH minimum value, is the second weight coefficient, PHj is the jth electrolyte marked PH value in the nickel plating electrolyte PH data, PHse is the pre-stored compensation PH value, and N is the number of electrolyte marked PH values.

6. An optimization control system for the production process parameters of alloy tungsten wire diamond wire saws, It is characterized in that The system comprises: An abnormal electrolyte layer judgment module is used to obtain nickel-plated electrolyte PH data of each nickel-plated electrolyte layer in the nickel-plated solution tank in the tungsten diamond wire saw production line based on preset time lengths and preset PH monitoring sensors, and judge whether there is a nickel-plated electrolyte layer with abnormal PH value according to the nickel-plated electrolyte PH data, wherein the number of the nickel-plated electrolyte layers is multiple, and each of the nickel-plated electrolyte layers corresponds to one nickel-plated electrolyte PH data within one of the preset time lengths; The electrolyte temperature troubleshooting module is used to obtain electrolyte temperature data corresponding to the nickel-plated electrolyte layer with abnormal pH value if it is determined that there is a nickel-plated electrolyte layer with abnormal pH value, and determine whether the abnormal pH value is caused by abnormal temperature according to the electrolyte temperature data; an electrolyte temperature control module, for generating an emergency temperature control instruction if the judgment is yes, and controlling a preset electrolyte cooling device to cool the nickel-plated electrolyte layer with an abnormal pH value according to the emergency temperature control instruction until the pH value of the nickel-plated electrolyte layer with an abnormal pH value is converted to normal; The electrolyte acid-base adjustment module is used to generate an acid-base solution adjustment instruction if the judgment is no, and control a preset electrolyte pH adjustment device according to the acid-base solution adjustment instruction to adjust the pH of the nickel-plated electrolyte layer with abnormal pH value until the pH value of the nickel-plated electrolyte layer with abnormal pH value is converted to normal.

7. The optimization control system for production process parameters of alloy tungsten diamond wire saw according to claim 6, It is characterized in that The abnormal electrolyte layer judgment module is also used for: Extracting the actual maximum pH value and the actual minimum pH value in each of the nickel plating electrolyte pH data, wherein one of the nickel plating electrolyte pH data corresponds to one of the actual maximum pH value and one of the actual minimum pH value; Determine whether any one of the actual maximum pH value and the actual minimum pH value corresponding to the pH data of each nickel plating electrolyte exceeds the pre-stored normal pH value range; If the answer is yes, the corresponding nickel plating electrolyte layer is determined to be a nickel plating electrolyte layer with an abnormal pH value.

8. The optimization control system for production process parameters of alloy tungsten diamond wire saw according to claim 7, It is characterized in that The electrolyte temperature checking module is also used for: Obtaining electrolyte temperature data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, obtaining a current temperature change difference according to the electrolyte temperature data, and generating a pH growth value according to the nickel-plated electrolyte pH data corresponding to the nickel-plated electrolyte layer with an abnormal pH value, wherein the pH growth value is a difference between an actual maximum pH value and an initial pH value in the pH data of the nickel-plated electrolyte with an abnormal pH value; Obtaining the actual use time of each nickel plating electrolyte layer in the nickel plating solution tank, and obtaining corresponding temperature change data according to the actual use time, wherein the temperature change data includes a plurality of standard temperature change differences, each of which corresponds to a pH value change range; Compare the current temperature change difference with each standard temperature change difference in the corresponding temperature change data, and select the standard temperature change difference that matches the current temperature change difference, wherein the pH value change range corresponding to the selected standard temperature change difference is the target pH value change range; Determining whether the pH growth value is within the target pH value variation range; If the answer is yes, it is determined that the abnormal temperature causes the abnormal pH value.

Citation Information

Patent Citations

  • Electroplating liquid supervision system for composite electroplating based on data analysis

    CN117238388A

  • Continuous surface corrosion prevention control method and system

    CN118547366A

  • Diamond wire saw production line plating solution real -time monitoring system

    CN205920378U

Cited By

  • Processing method of high-precision electrolytic superfine nickel wire

    CN120537015A

  • Intelligent control method and system for nickel plating layer thickness of diamond fretsaw

    CN122013288A