Strength performance test analysis method for injection molding shell part
By combining temperature test scenarios and multiple test items in the strength performance test of injection molded shell parts, the deformation, corrosion and damage performance was analyzed, and the problem of insufficient representativeness of the test results was solved, and the comprehensiveness and accuracy analysis of injection molded shell parts was achieved. , ensuring its overall strength performance.
Patent Information
- Application Number
- CN202411178824.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The strength performance test analysis of existing injection molded shell parts is not conducted in combination with temperature test scenarios, resulting in insufficient representation and rationality of the test results, and no attention to detailed characterization, resulting in one-sidedness and inaccuracy of the strength performance analysis.
A test analysis method for strength performance of injection molded shell parts is proposed. By setting temperature test scenarios and test items, including deformation, corrosion and damage tests, recording and analyzing test data, calculating deformation bearing index, corrosion bearing index and damage bearing index, and generating performance Report to feedback results.
By combining temperature test scenarios and test projects, comprehensive and detailed analysis of the strength performance of injection molded shell parts is achieved, the representativeness and accuracy of the test results are improved, and the overall strength performance of injection molded shell parts is ensured.
Smart Images

Figure CN118961407A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of performance test analysis of injection molded shell parts, and relates to a strength performance test analysis method of injection molded shell parts. Background Art
[0002] Injection molded housing parts are plastic housing parts manufactured by injection molding process. They are widely used in the automotive industry, electronics industry, medical industry, agriculture and other fields. In order to ensure that the injection molded housing parts can meet the design requirements and customer expectations in actual use, the strength performance test analysis of the injection molded housing parts is carried out.
[0003] At present, the strength performance test analysis of injection molded shell parts is mainly carried out by setting different test items. There are still the following deficiencies: 1. When conducting the strength performance test of injection molded shell parts, the comprehensive test is not combined with the temperature test scenario, which makes the test coverage insufficient and thus cannot guarantee the representativeness and rationality of the test results.
[0004] 2. Currently, no attention is paid to the detailed characterization of injection molded housing parts, which is a broad strength performance analysis, resulting in one-sidedness in the strength performance test results, reducing the accuracy and reliability of the test results, making it difficult to discover potential problems in a timely manner, and resulting in the inability to guarantee the overall strength performance of injection molded housing parts. Summary of the invention
[0005] In view of this, in order to solve the problems raised in the above background technology, a strength performance test analysis method for injection molded housing parts is now proposed.
[0006] The purpose of the present invention can be achieved through the following technical solutions: The present invention provides an injection molded shell component strength performance test analysis method, the method comprising: step one, test scene setting: the injection molded shell component to be subjected to the injection molded shell component strength performance test is recorded as the target shell component, the temperature is used as the test scene of the target shell component, and each test temperature value is set.
[0007] Step 2: Test item setting: Set the test items for the target shell parts, including deformation test, corrosion test and destructive test.
[0008] Step 3: Test start tracking: Test each test item under the temperature test scenario on the target housing component, and record the test data of each test item under the temperature test scenario.
[0009] Step 4, strength performance analysis: according to the test data of each test item of the target shell component under the temperature test scenario, a strength performance test analysis is performed to obtain the strength performance test results, wherein the strength performance test analysis includes: Q1, performing a deformation performance analysis of the target shell component to obtain the deformation bearing index of the target shell component.
[0010] Q2. Analyze the corrosion performance of the target shell parts to obtain the corrosion bearing index of the target shell parts.
[0011] Q3. Perform a destructive performance analysis on the target shell component to obtain the destructive bearing index of the target shell component, and then use the deformation bearing index, corrosion bearing index and destructive bearing index of the target shell component as the strength performance test analysis results.
[0012] Step 5: Performance report generation feedback: Based on the strength performance test analysis results, generate a strength performance test analysis report for the target shell component and provide corresponding feedback.
[0013] Preferably, the deformation performance analysis of the target shell component includes: extracting test data of deformation tests under temperature test scenarios, and then extracting set operation indicators, actual operation indicators, set recovery time and actual recovery time of each deformation operation category during each deformation test at each test temperature.
[0014] The deformation load index of each deformation operation category at each test temperature is analyzed to obtain the deformation load index of each test temperature. , is the test temperature number, , and then calculate the deformation load index of the target shell .
[0015] Preferably, the deformation bearing index analysis of each deformation operation category at each test temperature includes: subtracting the set operation index of each deformation operation category at each test temperature from the actual operation index to obtain the operation index difference of each deformation operation category at each test temperature.
[0016] If the operation index difference of a certain deformation operation category at a certain test temperature is less than or equal to the operation index difference set as a reference for the operation category, the deformation operation category at the test temperature is recorded as a qualified operation category.
[0017] The number of qualified operation categories at each test temperature is counted, and compared with the number of deformation operation categories at each test temperature, and the ratio is taken as the qualified ratio of deformation operation categories at each test temperature, denoted as .
[0018] according to The analysis method of is similar to that of the above, and the qualified ratio of the recovery time of each test temperature is obtained, which is used as the deformation recovery efficiency of each test temperature, denoted as .
[0019] Statistics of deformation load index at each test temperature , , and Set the reference The qualified ratio of deformation operation categories and deformation recovery efficiency at each test temperature.
[0020] Preferably, the statistical deformation bearing index of the target housing component includes: constructing a deformation bearing index variation curve with the test temperature as the abscissa and the deformation bearing index as the ordinate.
[0021] The temperature and deformation load index of the first valley point as well as the temperature and deformation load index of the starting point are extracted from the deformation load index change curve and recorded as , , and .
[0022] Statistical deformation load index of target shell , , is a natural constant, and They are the reference temperature difference and deformation load index difference respectively.
[0023] Preferably, the corrosion performance analysis of the target shell component includes: extracting test data of the corrosion test under the temperature test scenario, and then extracting the set chemical corrosion degree and the actual chemical corrosion degree of the corrosion test at each test temperature and each test duration, and then calculating the corrosion bearing index of the target shell component. .
[0024] Preferably, the statistical corrosion load index of the target housing component includes: comparing the actual chemical corrosion degree with the set chemical corrosion degree at each test temperature at the same test time, obtaining the test time at which the actual chemical corrosion degree at each test temperature is greater than the set chemical corrosion degree for the first time, and taking it as the starting corrosion test time at each test temperature, recorded as .
[0025] A chemical corrosion degree variation curve for each test temperature is constructed with the test duration as the horizontal axis and the chemical corrosion degree as the vertical axis, and a chemical corrosion degree reference line is constructed in the chemical corrosion degree variation curve according to the set chemical corrosion degree for each test duration at each test temperature.
[0026] The length of the curve above the chemical corrosion reference line is extracted from the chemical corrosion change curve at each test temperature and recorded as , and the length of the chemical corrosion change curve at each test temperature is recorded as .
[0027] Statistical corrosion load index of target shell parts , , is the number of temperature tests, , To set the reference deviation curve length ratio, For setting The reference initial corrosion test duration for each test temperature.
[0028] Preferably, the destructive performance analysis of the target shell component includes: A1, extracting the test data of the destructive test under the temperature test scenario, and then extracting the internal hardness, external hardness of the target shell component at each test temperature, and the set impact damage degree, set wear amount, set surface roughness, actual impact damage degree, actual wear amount and actual surface roughness of each destructive test.
[0029] A2. According to the set impact damage degree and actual impact damage degree of each destructive test at each test temperature, the impact bearing index of the temperature test scene is calculated. .
[0030] A3. According to the set wear amount, set surface roughness, actual wear amount and actual surface roughness of each destructive test at each test temperature, the wear load index of the temperature test scene is calculated. .
[0031] A4. According to the internal hardness and external hardness of the target shell parts at each test temperature, the hardness matching index of the temperature test scene is calculated. .
[0032] A5. Calculate the damage bearing index of the target shell , , , and are the weights of the impact load index, wear load index and hardness matching index, respectively. , .
[0033] Preferably, the impact bearing index of the statistical temperature test scenario includes: matching and comparing the set impact damage degree and the actual impact damage degree of each destructive test at each test temperature; if the set impact damage degree of a destructive test at a certain test temperature is less than or equal to the actual impact damage degree, then the destructive test at the test temperature is recorded as a qualified impact test.
[0034] The number of qualified impact tests is counted and compared with the number of test temperatures, and the ratio is used as the impact bearing index of the temperature test scenario, denoted as .
[0035] Preferably, the wear load index of the statistical temperature test scenario includes: setting the wear amount to be less than or equal to the actual wear amount as condition 1, and setting the surface roughness to be greater than the actual surface roughness as condition 2.
[0036] The destructive test that meets conditions 1 and 2 is regarded as the first wear level, the destructive test that only meets condition 1 is regarded as the second wear level, the destructive test that only meets condition 2 is regarded as the third wear level, and the destructive test that does not meet conditions 1 and 2 is regarded as the fourth wear level.
[0037] The number of first-level wear grade, second-level wear grade, third-level wear grade and fourth-level wear grade are counted and recorded as , , and , and record the number of test temperatures as .
[0038] Wear load index for statistical temperature test scenarios , , , , and are the weights of the set first wear level number ratio, second wear level number ratio, third wear level number ratio and fourth wear level number ratio, respectively. , .
[0039] Preferably, the hardness matching index of the statistical temperature test scenario includes: subtracting the corresponding internal hardness and external hardness of the target shell component at each test temperature to obtain the hardness difference of each test temperature; if the hardness difference of a certain test temperature is within a set reference hardness difference interval, the test temperature is recorded as a qualified hardness test temperature; otherwise, the test temperature is recorded as an abnormal hardness test temperature.
[0040] Count the number of hardness qualified test temperatures, recorded as .
[0041] Sort the hardness abnormal test temperatures from small to large, and extract the hardness abnormal test temperature with the first ranking as the starting hardness interference temperature, recorded as .
[0042] Statistical hardness matching index of temperature test scenario , , and They are the reference hardness qualified test temperature number ratio and the initial hardness interference temperature respectively.
[0043] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The present invention conducts a comprehensive analysis on the strength performance of the injection molded housing parts by combining various test scenarios and various test items, thereby solving the problem of the current comprehensive test not being combined with the temperature test scenario, ensuring the coverage of the test, and further ensuring the representativeness and rationality of the test results.
[0044] (2) The present invention analyzes the detailed characterization of the injection molded housing parts according to the test data of each test item under the temperature test scenario, thereby avoiding the current deficiency of not paying attention to the detailed characterization of the injection molded housing parts, achieving targeted analysis of strength performance, ensuring the comprehensiveness of performance test results, and improving the accuracy and reliability of test results, thereby facilitating the timely discovery of potential problems and ensuring the overall strength performance of the injection molded housing parts. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0046] Figure 1 It is a schematic diagram of the connection of each step of the method of the present invention.
[0047] Figure 2 It is a schematic diagram of the connection steps of the strength performance test analysis of the present invention. DETAILED DESCRIPTION
[0048] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0049] See also Figure 1 As shown, the present invention provides an injection molded shell component strength performance test analysis method, the method comprising: step one, test scene setting: recording the injection molded shell component to be subjected to the injection molded shell component strength performance test as the target shell component, taking the temperature as the test scene of the target shell component, and setting each test temperature value.
[0050] It should be added that the specific setting process of setting each test temperature value is as follows: extract the upper limit value of the adaptive temperature range of the injection molded shell component from the injection molded shell component strength performance test analysis technical specification table, and according to the pre-set temperature floating value, use the sum of the upper limit value of the adaptive temperature range and the temperature floating value as the upper limit test temperature value, and use the difference between the upper limit value of the adaptive temperature range and the temperature floating value as the lower limit test temperature value, and at the same time use the upper limit value of the adaptive temperature range as the intermediate test temperature value, and obtain each test temperature value based on this setting.
[0051] In a specific embodiment, when the upper limit value of the adaptive temperature range of the injection molded housing is 200 degrees Celsius and the preset temperature floating value is 20 degrees Celsius, the upper limit test temperature value is 220 degrees Celsius, the lower limit test temperature value is 180 degrees Celsius, and the intermediate test temperature value is 200 degrees Celsius.
[0052] Step 2: Test item setting: Set the test items for the target shell parts, including deformation test, corrosion test and destructive test.
[0053] Step 3: Test start tracking: Test each test item under the temperature test scenario on the target housing component, and record the test data of each test item under the temperature test scenario.
[0054] The embodiment of the present invention conducts a comprehensive analysis on the strength performance of the injection molded housing parts by combining various test scenarios and various test items, thereby solving the deficiency of the current comprehensive test without combining the temperature test scenario, ensuring the coverage of the test, and further ensuring the representativeness and rationality of the test results.
[0055] See also Figure 2 As shown, step 4, strength performance analysis: according to the test data of each test item of the target shell component under the temperature test scenario, a strength performance test analysis is performed to obtain the strength performance test results, wherein the strength performance test analysis includes: Q1, performing a deformation performance analysis of the target shell component to obtain the deformation bearing index of the target shell component.
[0056] Exemplarily, the deformation performance analysis of the target shell component includes: extracting test data of deformation tests under temperature test scenarios, and then extracting set operation indicators, actual operation indicators, set recovery time and actual recovery time for each deformation operation category during each deformation test at each test temperature.
[0057] It should be supplemented that the various deformation operation categories include but are not limited to length stretching, angle bending and compression, among which the setting operation indicator of length stretching is the setting stretching length, and the actual operation indicator is the actual stretching length, the setting operation indicator of angle bending is the setting bending angle, and the actual operation indicator is the actual bending angle, and the setting operation indicator of compression is the setting compression amount, and the actual operation indicator is the actual compression amount.
[0058] It should be supplemented that the compression amount refers to the difference between the original size and the compressed size of the target housing component under the action of the compression force.
[0059] The deformation load index of each deformation operation category at each test temperature is analyzed to obtain the deformation load index of each test temperature. , is the test temperature number, , and then calculate the deformation load index of the target shell .
[0060] Furthermore, the deformation bearing index analysis of each deformation operation category at each test temperature includes: subtracting the set operation index of each deformation operation category from the actual operation index at each test temperature to obtain the operation index difference of each deformation operation category at each test temperature.
[0061] If the operation index difference of a certain deformation operation category at a certain test temperature is less than or equal to the operation index difference set as a reference for the operation category, the deformation operation category at the test temperature is recorded as a qualified operation category.
[0062] The number of qualified operation categories at each test temperature is counted, and compared with the number of deformation operation categories at each test temperature, and the ratio is taken as the qualified ratio of deformation operation categories at each test temperature, denoted as .
[0063] according to The analysis method of is similar to that of the above, and the qualified ratio of the recovery time of each test temperature is obtained, which is used as the deformation recovery efficiency of each test temperature, denoted as .
[0064] Statistics of deformation load index at each test temperature , , and Set the reference The qualified ratio of deformation operation categories and deformation recovery efficiency at each test temperature.
[0065] It should be added that and All of them are extracted from the technical specification table of injection molded housing strength performance test analysis.
[0066] Furthermore, the statistical deformation bearing index of the target housing component includes: constructing a deformation bearing index variation curve with the test temperature as the abscissa and the deformation bearing index as the ordinate.
[0067] The temperature and deformation load index of the first valley point as well as the temperature and deformation load index of the starting point are extracted from the deformation load index change curve and recorded as , , and .
[0068] Statistical deformation load index of target shell , , is a natural constant, and They are the reference temperature difference and deformation load index difference respectively.
[0069] It should be added that the reference temperature and reference deformation load index are extracted from the injection molded shell strength performance test analysis technical specification table, and the set reference temperature difference and deformation load index difference are obtained by the same analysis method as the temperature difference and deformation load index difference.
[0070] Q2. Analyze the corrosion performance of the target shell parts to obtain the corrosion bearing index of the target shell parts.
[0071] Exemplarily, the corrosion performance analysis of the target shell component includes: extracting test data of the corrosion test under the temperature test scenario, and then extracting the set chemical corrosion degree and actual chemical corrosion degree of the corrosion test at each test temperature and each test duration, and then calculating the corrosion bearing index of the target shell component. .
[0072] Furthermore, the statistical corrosion bearing index of the target shell component includes: comparing the actual chemical corrosion degree of each test temperature with the set chemical corrosion degree at the same test time, obtaining the test time at which the actual chemical corrosion degree at each test temperature is greater than the set chemical corrosion degree for the first time, and taking it as the starting corrosion test time at each test temperature, recorded as .
[0073] A chemical corrosion degree variation curve for each test temperature is constructed with the test duration as the horizontal axis and the chemical corrosion degree as the vertical axis, and a chemical corrosion degree reference line is constructed in the chemical corrosion degree variation curve according to the set chemical corrosion degree for each test duration at each test temperature.
[0074] The length of the curve above the chemical corrosion reference line is extracted from the chemical corrosion change curve at each test temperature and recorded as , and the length of the chemical corrosion change curve at each test temperature is recorded as .
[0075] Statistical corrosion load index of target shell parts , , is the number of temperature tests, , To set the reference deviation curve length ratio, For setting The reference initial corrosion test duration for each test temperature.
[0076] It should be added that the reference chemical corrosion degree for each test time at each test temperature is extracted from the technical specification table of strength performance test analysis of injection molded housing parts, and the deviation curve length ratio for the set reference is obtained by the same analysis method according to the deviation curve length ratio. , in order to facilitate analysis, The specific value can be 0.4. It is extracted from the technical specification table of strength performance test analysis of injection molded housing parts.
[0077] Q3. Perform a destructive performance analysis on the target shell component to obtain the destructive bearing index of the target shell component, and then use the deformation bearing index, corrosion bearing index and destructive bearing index of the target shell component as the strength performance test analysis results.
[0078] Exemplarily, the destructive performance analysis of the target shell component includes: A1, extracting the test data of the destructive test under the temperature test scenario, and then extracting the internal hardness, external hardness of the target shell component at each test temperature, and the set impact damage degree, set wear amount, set surface roughness, actual impact damage degree, actual wear amount and actual surface roughness of each destructive test.
[0079] It should be added that the impact damage degree refers to the various damage types and damage indicators of each damage type after the injection molded shell is subjected to an impact test. The damage types include but are not limited to cracks, breakages and deformations. The damage indicators of cracks are crack length, crack width and crack depth. The damage indicator of breakage is the area of the damaged part. The damage indicators of deformation are the area of the deformed part and the degree of deformation depression.
[0080] A2. According to the set impact damage degree and actual impact damage degree of each destructive test at each test temperature, the impact bearing index of the temperature test scene is calculated. .
[0081] Furthermore, the impact bearing index of the statistical temperature test scenario includes: A2-1, matching and comparing the set impact damage degree and the actual impact damage degree of each destructive test at each test temperature. If the set impact damage degree of a destructive test at a certain test temperature is less than or equal to the actual impact damage degree, then the destructive test at the test temperature is recorded as a qualified impact test.
[0082] A2-2. Count the number of qualified impact tests, compare it with the number of test temperatures, and use the ratio as the impact bearing index of the temperature test scenario, denoted as .
[0083] A3. According to the set wear amount, set surface roughness, actual wear amount and actual surface roughness of each destructive test at each test temperature, the wear load index of the temperature test scene is calculated. .
[0084] Furthermore, the wear load index of the statistical temperature test scenario includes: A3-1, setting the wear amount to be less than or equal to the actual wear amount as condition 1, and setting the surface roughness to be greater than the actual surface roughness as condition 2.
[0085] A3-2. The destructive test that meets conditions 1 and 2 is regarded as the first wear level, the destructive test that only meets condition 1 is regarded as the second wear level, the destructive test that only meets condition 2 is regarded as the third wear level, and the destructive test that does not meet conditions 1 and 2 is regarded as the fourth wear level.
[0086] In a specific embodiment, the order of influence of the wear levels is primary wear level > secondary wear level > tertiary wear level > quaternary wear level.
[0087] It should be added that the second-level wear grade indicates that the amount of wear is acceptable, and the third-level wear grade indicates that the surface roughness is acceptable. The amount of wear is directly related to the service life and functional integrity of the injection molded shell parts. If the amount of wear exceeds the standard, it may cause damage to the product structure or functional failure, thereby affecting its overall performance. Therefore, the second-level wear grade is set to be greater than the third-level wear grade.
[0088] A3-3. Count the number of first-level wear grade, second-level wear grade, third-level wear grade and fourth-level wear grade, and record them as , , and , and record the number of test temperatures as .
[0089] A3-4. Wear load index of statistical temperature test scenario , , , , and are the weights of the set first wear level number ratio, second wear level number ratio, third wear level number ratio and fourth wear level number ratio, respectively. , .
[0090] It should be added that the weight of the wear level number ratio is set according to the wear level. For the convenience of analysis, The specific value can be 0.4. The specific value can be 0.3. The specific value can be 0.2. The specific value can be 0.1.
[0091] A4. According to the internal hardness and external hardness of the target shell parts at each test temperature, the hardness matching index of the temperature test scene is calculated. .
[0092] Furthermore, the hardness matching index of the statistical temperature test scenario includes: A4-1, subtracting the corresponding internal hardness and external hardness of the target shell component at each test temperature to obtain the hardness difference of each test temperature. If the hardness difference of a certain test temperature is within the set reference hardness difference interval, the test temperature is recorded as the qualified hardness test temperature. Otherwise, the test temperature is recorded as the abnormal hardness test temperature.
[0093] A4-2. Count the number of hardness test temperatures that meet the test standards and record them as .
[0094] A4-3. Sort the hardness abnormal test temperatures from small to large, and extract the hardness abnormal test temperature with the first place in the ranking as the starting hardness interference temperature, recorded as .
[0095] A4-4. Hardness matching index of statistical temperature test scene , , and They are the reference hardness qualified test temperature number ratio and the initial hardness interference temperature respectively.
[0096] It should be added that the reference hardness qualified test temperature number is extracted from the injection molded shell strength performance test analysis technical specification table, and the hardness qualified test temperature number ratio of the set reference is obtained by the same analysis method according to the hardness qualified test temperature number ratio. , in order to facilitate analysis, The specific value can be 0.8. It is extracted from the technical specification table of injection molded housing strength performance test analysis.
[0097] A5. Calculate the damage bearing index of the target shell , , , and are the weights of the impact load index, wear load index and hardness matching index, respectively. , .
[0098] It should be added that the impact bearing index is directly related to the structural integrity of the injection molded housing. If the housing is broken or deformed when hit, it will affect the overall performance of the injection molded housing. The wear bearing index is crucial to ensure the reliability and durability of the injection molded housing in long-term use. The long-term impact on the performance of the injection molded housing is the hardness, which measures the ability of the material surface to resist permanent deformation or scratches, but it does not directly affect the bearing capacity of the injection molded housing. Therefore, it is set , in order to facilitate analysis, The specific value can be 0.5. The specific value can be 0.3. The specific value can be 0.2.
[0099] The embodiment of the present invention analyzes the detailed characterization of the injection molded housing parts according to the test data of each test item under the temperature test scenario, thereby avoiding the current deficiency of not paying attention to the detailed characterization of the injection molded housing parts, achieving targeted analysis of strength performance, ensuring the comprehensiveness of performance test results, and improving the accuracy and reliability of test results, thereby facilitating the timely discovery of potential problems and ensuring the overall strength performance of the injection molded housing parts.
[0100] Step 5: Performance report generation feedback: Based on the strength performance test analysis results, generate a strength performance test analysis report for the target shell component and provide corresponding feedback.
[0101] The above contents are merely examples and explanations of the concept of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, they shall all fall within the protection scope of the present invention.
Claims
1. A test analysis method for the strength performance of injection molded housing parts. Features: The method includes: Step 1: Test scene setting: record the injection molded shell part to be subjected to the injection molded shell part strength performance test as the target shell part, take the temperature as the test scene of the target shell part, and set each test temperature value; Step 2: Test item setting: setting the test items of the target shell parts, including deformation test, corrosion test and destruction test; Step 3: Test start tracking: Test each test item under the temperature test scenario on the target housing component, and record the test data of each test item under the temperature test scenario; Step 4: Strength performance analysis: Based on the test data of each test item of the target shell component under the temperature test scenario, a strength performance test analysis is performed to obtain the strength performance test results, wherein the strength performance test analysis includes: Q1. Perform deformation performance analysis on the target shell component to obtain the deformation bearing index of the target shell component; Q2. Analyze the corrosion performance of the target shell parts to obtain the corrosion bearing index of the target shell parts; Q3. Perform a destructive performance analysis on the target shell component to obtain the destructive bearing index of the target shell component, and then use the deformation bearing index, corrosion bearing index and destructive bearing index of the target shell component as the strength performance test analysis results; Step 5: Performance report generation feedback: Based on the strength performance test analysis results, generate a strength performance test analysis report for the target shell component and provide corresponding feedback.
2. A strength performance test and analysis method for injection molded housing parts according to claim 1, Features: The deformation performance analysis of the target housing component includes: Extract the test data of deformation test in temperature test scenario, and then extract the setting operation index, actual operation index, setting recovery time and actual recovery time of each deformation operation category in each deformation test at each test temperature; The deformation load index of each deformation operation category at each test temperature is analyzed to obtain the deformation load index of each test temperature. , is the test temperature number, , and then calculate the deformation load index of the target shell .
3. A strength performance test and analysis method for injection molded housing parts according to claim 2, Features: The deformation bearing index analysis of each deformation operation category at each test temperature includes: The set operation index of each deformation operation category at each test temperature is subtracted from the actual operation index to obtain the operation index difference of each deformation operation category at each test temperature; If the operation index difference of a certain deformation operation category at a certain test temperature is less than or equal to the operation index difference of the reference set for the operation category, the deformation operation category at the test temperature is recorded as a qualified operation category; The number of qualified operation categories at each test temperature is counted, and compared with the number of deformation operation categories at each test temperature, and the ratio is taken as the qualified ratio of deformation operation categories at each test temperature, denoted as ; according to The analysis method of is similar to that of the above, and the qualified ratio of the recovery time of each test temperature is obtained, which is used as the deformation recovery efficiency of each test temperature, denoted as ; Statistics of deformation load index at each test temperature , , and Set the reference The qualified ratio of deformation operation categories and deformation recovery efficiency at each test temperature.
4. A strength performance test and analysis method for injection molded housing parts according to claim 2, Features: The statistical deformation load index of the target housing component includes: With the test temperature as the horizontal coordinate and the deformation bearing index as the vertical coordinate, a deformation bearing index change curve is constructed; The temperature and deformation load index of the first valley point as well as the temperature and deformation load index of the starting point are extracted from the deformation load index change curve and recorded as , , and ; Statistical deformation load index of target shell parts , , is a natural constant, and They are the reference temperature difference and deformation load index difference respectively.
5. A strength performance test and analysis method for injection molded housing parts according to claim 1, Features: The corrosion performance analysis of the target housing component includes: Extract the test data of the corrosion test under the temperature test scenario, and then extract the set chemical corrosion degree and actual chemical corrosion degree of the corrosion test at each test temperature and each test duration, and then calculate the corrosion bearing index of the target shell part .
6. A strength performance test and analysis method for injection molded housing parts according to claim 5, Features: The statistical target shell component corrosion bearing index includes: The actual chemical corrosion degree at each test temperature and the set chemical corrosion degree at the same test duration are compared one by one, and the test duration at which the actual chemical corrosion degree at each test temperature is greater than the set chemical corrosion degree for the first time is obtained, and is used as the starting corrosion test duration at each test temperature, recorded as ; With the test time as the horizontal axis and the chemical corrosion degree as the vertical axis, a chemical corrosion degree change curve for each test temperature is constructed, and according to the set chemical corrosion degree for each test time at each test temperature, a chemical corrosion degree reference line is constructed in the chemical corrosion degree change curve; The length of the curve above the chemical corrosion reference line is extracted from the chemical corrosion change curve at each test temperature and recorded as , and the length of the chemical corrosion change curve at each test temperature is recorded as ; Statistical corrosion load index of target shell parts , , is the number of temperature tests, To set the reference deviation curve length ratio, For setting The reference initial corrosion test duration for each test temperature.
7. A strength performance test and analysis method for injection molded housing parts according to claim 1, Features: The destructive performance analysis of the target shell component includes: A1. Extract the test data of the destructive test under the temperature test scenario, and then extract the internal hardness and external hardness of the target shell component at each test temperature, as well as the set impact damage, set wear, set surface roughness, actual impact damage, actual wear and actual surface roughness of each destructive test; A2. According to the set impact damage degree and actual impact damage degree of each destructive test at each test temperature, the impact bearing index of the temperature test scene is calculated. ; A3. According to the set wear amount, set surface roughness, actual wear amount and actual surface roughness of each destructive test at each test temperature, the wear load index of the temperature test scene is calculated. ; A4. According to the internal hardness and external hardness of the target shell parts at each test temperature, the hardness matching index of the temperature test scene is calculated. ; A5. Calculate the damage bearing index of the target shell , , , and are the weights of the impact load index, wear load index and hardness matching index, respectively. , .
8. A strength performance test and analysis method for injection molded housing parts according to claim 7, Features: The impact bearing index of the statistical temperature test scenario includes: The set impact damage degree and the actual impact damage degree of each destructive test at each test temperature are matched and compared. If the set impact damage degree of a destructive test at a certain test temperature is less than or equal to the actual impact damage degree, the destructive test at this test temperature is recorded as a qualified impact test; The number of qualified impact tests is counted and compared with the number of test temperatures, and the ratio is used as the impact bearing index of the temperature test scenario, denoted as .
9. A strength performance test and analysis method for injection molded housing parts according to claim 7, Features: The wear load index of the statistical temperature test scenario includes: The wear amount is set to be less than or equal to the actual wear amount as condition 1, and the surface roughness is set to be greater than the actual surface roughness as condition 2; The destructive test that meets conditions 1 and 2 is regarded as the first wear level, the destructive test that only meets condition 1 is regarded as the second wear level, the destructive test that only meets condition 2 is regarded as the third wear level, and the destructive test that does not meet conditions 1 and 2 is regarded as the fourth wear level; The number of first-level wear grade, second-level wear grade, third-level wear grade and fourth-level wear grade are counted and recorded as , , and , and record the number of test temperatures as ; Wear load index for statistical temperature test scenarios , , , , and are the weights of the set first wear level number ratio, second wear level number ratio, third wear level number ratio and fourth wear level number ratio, respectively. , .
10. A strength performance test and analysis method for injection molded housing parts according to claim 7, Features: The hardness matching index of the statistical temperature test scenario includes: The internal hardness and external hardness of the target housing part at each test temperature are subtracted to obtain the hardness difference at each test temperature. If the hardness difference at a certain test temperature is within the set reference hardness difference interval, the test temperature is recorded as the qualified hardness test temperature. Otherwise, the test temperature is recorded as the abnormal hardness test temperature. Count the number of hardness qualified test temperatures, recorded as ; Sort the hardness abnormal test temperatures from small to large, and extract the hardness abnormal test temperature with the first ranking as the starting hardness interference temperature, recorded as ; Statistical hardness matching index of temperature test scenario , , and They are the reference hardness qualified test temperature number ratio and the initial hardness interference temperature respectively.